Production technology of nanometer modified polyolefin resin film

A polyolefin resin and production process technology, applied in the field of nano-material modified polyolefin resin film, can solve the problems of poor barrier performance, high oxygen transmission rate, insufficient material rigidity, etc., to prolong shelf life and improve barrier performance Effect

CN101550251AInactive Publication Date: 2009-10-07浙江富陵控股集团有限公司 +2
0 Cites 15 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Publication Date
2009-10-07
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 1
    Figure 1
  • Figure 2
    Figure 2
  • Figure 3
    Figure 3
Patent Text Reader

Abstract

The invention discloses a production technology of nanometer modified polyolefin resin film, In the technology, un-stretched polypropylene film production process comprises: preparing modified nanometer silica, preparing modified nanometer montmorillonite, adding the prepared modified silica and modified montmorillonite into polypropylene homopolymers, adding dispersant, high speed banburing, melting, extruding and granulating to obtain parent material, melting the parent material, extruding, quenching, thickness measuring, corona treating, winding, cutting and packaging; and the production process of bidirectional stretched polypropylene film comprises an extra step of bidirectional stretching after the quenching step; wherein the weight percentages of the added substances are: modified silica 2%, modified montmorillonite 1.5%, F800E polypropylene homopolymers 93.5% and dispersant 3%. The invention solves problems of poor obstructing performance, relatively high oxygen transmittance, no antibacterial effect and insufficient rigidity of material existing in present CPP and BOPP films in our country; can prolong the shelf life of packing.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention relates to a production process of nanometer material modified polyolefin resin film. Background technique

[0002] Polypropylene resin has become the fastest-growing variety among general-purpose resins, especially polyolefin film, which accounts for 40% of the entire plastic product industry due to its rich source of raw materials, low price, easy processing and molding, excellent product comprehensive performance and wide range of uses. about. The traditional polyolefin film process steps are to melt and extrude the polypropylene masterbatch, then undergo rapid cooling, thickness measurement, corona treatment, winding, slitting and packaging. The annual production capacity of BOPP in my country has reached 1.5 million tons, and that of CPP has reached 220,000 tons. Nevertheless, polyolefin films also have some disadvantages. For example, polyolefin films cannot be used for the packaging of electronic products such as electronic integ...

Examples

Embodiment 1

[0019] The production process of a kind of unstretched nano-material modified polyolefin resin film (CPP) of the present embodiment, this process comprises 1) the preparation of modified nano silicon dioxide, the preparation of modified nano silicon dioxide adopts particle size = 50nm nano-SiO 2 Particles and titanate coupling agent NDZ-101, first dissolve the weighed isopropyl dioleic acid acyloxy (dioctyl phosphate acyloxy) titanate coupling agent with xylene solvent, and then mix with nano-SiO 2 The particles were thoroughly mixed until uniform, and put into an oven to dry to remove the solvent, wherein the drying temperature was 110° C., and the drying time was 2 hours. The addition of titanate coupling agent is nano-SiO 2 5% by weight of particles.

[0020] 2) The preparation of modified nano-montmorillonite uses nano-montmorillonite particles with a particle size of 50nm and a titanate coupling agent NDZ-101. First, the weighed titanate coupling agent is dissolved in ...

Embodiment 2

[0024] A kind of production technology of biaxially stretched nanomaterial modified polyolefin resin film (BOPP) of the present embodiment, this technology comprises 1) the preparation of modified nano silicon dioxide, the preparation of modified nano silicon dioxide adopts particle diameter = 50nm nano-SiO 2 Particles and titanate coupling agent NDZ-101, first dissolve the weighed isopropyl dioleic acid acyloxy (dioctyl phosphate acyloxy) titanate coupling agent with xylene solvent, and then mix with nano-SiO 2 The particles were thoroughly mixed until uniform, and put into an oven to dry to remove the solvent, wherein the drying temperature was 110° C., and the drying time was 2 hours. The addition of titanate coupling agent is nano-SiO 2 5% by weight of particles.

[0025] 2) The preparation of modified nano-montmorillonite adopts nano-montmorillonite particles with a particle size of 50nm and titanate coupling agent NDZ-101. Name?) dissolved, then fully mixed with nano...