Method for manufacturing a semi-hole plate with partial hard gold plating where leads cannot be pulled

By first electroplating copper thick on the half-hole plate and making a nickel-thick gold layer in advance, then tin plating, milling half-holes and etching, combining dry film exposure technology and gold depositing steps, the problem of being unable to design leads is solved, and local Mass production and process simplification of gold-plated half-porous plates.

CN110267464BActive Publication Date: 2024-11-05SHENZHEN JIEXING INTELLIGENT MANUFACTURING TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201910482861.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-06-04
Publication Date
2024-11-05
Estimated Expiration
2039-06-04

AI Technical Summary

Technical Problem

In the prior art, the partially thick gold-plated half-porous plate design cannot be designed, resulting in mass production due to the inability to design leads, and the burrs are poor, requiring manual repair, which is time-consuming and easy to scrap.

Method used

The copper thickness is first electroplating, and the nickel-thick gold layer is made in advance, and the surface treatment is carried out for tin plating, milling half holes, etching and solder resist characters are carried out for surface treatment. The nickel-thick gold is plated at local locations through dry film exposure technology, combining the deposited gold and the film removal Steps to realize the production of partially hard gold-plated half-well plates.

Benefits of technology

It realizes the production of partially hard gold-plated half-well plates without pulling the leads, simplifies the process, reduces the need for manual repairs, and facilitates mass production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110267464B_ABST
    Figure CN110267464B_ABST
Patent Text Reader

Abstract

The present invention provides a method for manufacturing a semi-hole plate with partial hard gold plating where leads cannot be pulled, comprising: firstly, the electroplated copper thickness meets the requirements, and a nickel-thick gold layer is made in advance. Then, tin plating is performed, a semi-hole is milled, a pattern is etched, and a surface treatment is performed after solder mask characters are applied. Due to the adoption of the above technical scheme, the present invention can manufacture a semi-hole plate with partial hard gold plating when leads cannot be pulled, and is convenient for mass production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of circuit board manufacturing, and in particular to a method for manufacturing a semi-hole board with partial hard gold plating where leads cannot be pulled. Background Art

[0002] New markets drive the development of new technologies, and the development of science and technology promotes the diversification of printed circuit design. Half-hole boards with partial thick gold plating usually use the method of full-board gold plating + partial thick gold plating, but burrs at the half-hole position need to be repaired manually, which is time-consuming and material-consuming and easy to be scrapped after repair. The design of leads can be partially plated with thick gold, but in most cases, it is impossible to design leads, so similar designs cannot be mass-produced. Summary of the invention

[0003] The present invention provides a method for manufacturing a semi-hole plate that is partially hard-gold plated and cannot pull leads, so as to solve at least one of the above-mentioned technical problems.

[0004] To solve the above problems, as one aspect of the present invention, a method for manufacturing a semi-hole plate with partial hard gold plating where leads cannot be pulled is provided, comprising: firstly, the electroplated copper thickness meets the requirements, and a nickel-thick gold layer is made in advance. Then, tin plating is performed, a semi-hole is milled, a pattern is etched, and surface treatment is performed after solder mask characters are applied.

[0005] Preferably, the method specifically includes: firstly, the electroplated copper thickness meets the requirements, and then partially nickel-plated with thick gold, after the nickel-thick gold is made, the film is exposed to make a dry film pattern, and then the half hole is milled after direct tinning, and then etching is performed, so that the local position of the circuit pattern is plated with thick gold in advance, and after the solder mask and characters are made, if the surface treatment is OSP, then OSP is performed normally. If it is immersion gold, it is necessary to use dry film to selectively cover the hard gold position, and then the immersion gold is retreated; the method specifically includes the following steps:

[0006] Step 1, cutting;

[0007] Step 2, drilling: drilling machine processing is performed on the board to prepare for the conduction of the inner and outer layers in the subsequent process;

[0008] Step 3, copper deposition / negative film electroplating: remove the drilling dirt in the hole through the previous desmearing process to make the hole clean, and then activate the colloidal palladium adsorbed on the surface and in the hole, and an oxidation-reduction reaction occurs in the copper deposition tank to form a copper layer; then, the copper thickness of the hole / surface copper is thickened to the customer's required standard through electroplating;

[0009] Step 4, external light imaging: at a certain temperature and pressure, a dry film is pasted on the board surface, and then the film is aligned, and finally the dry film not shielded by the film is irradiated with ultraviolet light on the exposure machine to react, forming the required circuit pattern on the board surface, and then the film not irradiated by light is dissolved by the developer in the developing section, exposing the area that needs to be plated with nickel thick hard gold;

[0010] Step 5, nickel-thick gold plating: deposit nickel and gold layers of customer-required thickness in nickel and gold baths by electroplating:

[0011] Step 6, film removal: remove the dry film on the board to expose the metal layer:

[0012] Step 7, external light imaging 2: The working principle is similar to external light imaging, exposing the circuit layer, including the nickel-plated thick gold layer;

[0013] Step 8, tin plating: In the tin bath, a layer of metal tin is plated on the conductive area of ​​the board through the principle of electroplating for anti-etching protection;

[0014] Step 9, milling half hole: mill the specified inner groove according to customer requirements, and the remaining half hole:

[0015] Step 10, outer layer etching: Under the action of alkali solution, the film is removed to expose the copper surface to be etched. In the etching tank, copper reacts with copper ions to produce cuprous to achieve etching. In the detinning tank, nitric acid reacts with the tin surface to remove the tinned layer and expose the copper surface of the circuit pad.

[0016] Step 11, Solder Mask / Characters:

[0017] Solder mask: Use a screen printing net to print the solder mask on the board surface and pre-bake to remove the volatilization to form a semi-cured film layer. Through the alignment exposure, the solder mask cross-links in the illuminated areas, and the unexposed areas are developed under the action of alkali solution. At high temperature, the solder mask is completely cured and attached to the board surface;

[0018] Characters: The production method is similar to solder mask;

[0019] Step 12, external light imaging 3: The working principle is similar to external light imaging. This time, the nickel-thick gold area is covered with a dry film, and the area that needs to be immerged gold is exposed to facilitate immersion gold.

[0020] Step 13, immersion gold: deposit a layer of metal nickel and gold on the copper surface through chemical replacement reaction;

[0021] Step 14, film stripping 2: Similar to the working principle of film stripping, the dry film on the board is stripped clean to expose the thick gold layer of electroplated nickel.

[0022] Due to the adoption of the above technical solution, the present invention can manufacture a semi-hole plate partially plated with hard gold when the lead wire cannot be pulled, and is convenient for mass production. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 The schematic diagram of step 3 is schematically shown;

[0024] Figure 2 The schematic diagram of step 4 is schematically shown;

[0025] Figure 3 The schematic diagram of step 5 is schematically shown;

[0026] Figure 4 The schematic diagram of step 6 is schematically shown;

[0027] Figure 5 The schematic diagram of step 7 is schematically shown;

[0028] Figure 6 The schematic diagram of step 8 is schematically shown;

[0029] Figure 7 The schematic diagram of step 9 is schematically shown;

[0030] Figure 8 The schematic diagram of step 10 is schematically shown;

[0031] Fig. 9 The schematic diagram of step 12 is schematically shown;

[0032] Fig.10 A schematic diagram of step 13 is schematically shown. DETAILED DESCRIPTION

[0033] The embodiments of the present invention are described in detail below with reference to the accompanying drawings, but the present invention can be implemented in many different ways as defined and covered by the claims.

[0034] The invention belongs to the field of printed circuit board manufacturing, and in particular relates to the manufacturing of a semi-hole board with partial hard gold plating where leads cannot be drawn.

[0035] The present invention firstly makes the electroplated copper thickness meet the requirements, and makes a nickel thick gold layer in advance. Then, tinning is performed, half holes are milled, patterns are etched, and surface treatment is performed after solder resist characters are formed. In this way, a half-hole plate with partial nickel thick gold plating that cannot design leads is manufactured.

[0036] The present invention firstly makes the electroplated copper thickness meet the requirements, and then partially nickel-plated with thick gold. After the nickel-thick gold is made, the film is exposed to make a dry film pattern, and then a half hole is milled directly after tinning, and then etching is performed. In this way, the local position of the circuit pattern is plated with thick gold in advance. After the solder mask and characters are made, if the surface treatment is OSP, then OSP is performed normally. If it is immersion gold, it is necessary to use dry film to selectively cover the hard gold position, and then the immersion gold can be retreated.

[0037] The present invention discloses a method for manufacturing a semi-hole plate with partial nickel thick gold plating where leads cannot be designed, and the process is as follows: cutting—(inner layer circuit manufacturing—lamination)—drilling—copper deposition—negative film electroplating—external light imaging—nickel thick gold plating—film stripping—external light imaging 2—external light inspection—tinning—milling plate holes—external layer etching—external layer AOI—solder mask—characters—external light imaging 3—gold deposition—film stripping 2—post-process.

[0038] The above process is described in detail below:

[0039] 1. Cutting

[0040] The copper clad laminate is cut into designed size by a cutting machine.

[0041] 2. Drilling

[0042] According to the customer's requirements, drilling machine processing is performed on the board to prepare for the conduction of the inner and outer layers in the subsequent process

[0043] 3. Copper plating / negative electroplating

[0044] Through the previous desmearing process, the drilling dirt in the hole is removed to make the hole clean. After activation, the colloidal palladium is adsorbed on the surface and in the hole, and an oxidation-reduction reaction occurs in the copper sink to form a copper layer. Then, the copper thickness of the hole / surface copper is thickened to the customer's required standard through electroplating.

[0045] 4. External light imaging.

[0046] Under certain temperature and pressure, a dry film is pasted on the board surface, and then aligned with a film. Finally, ultraviolet light is used on an exposure machine to make the dry film not masked by the film react and form the required circuit pattern on the board surface. Then, the film not irradiated by light is dissolved by the developing solution in the developing section, exposing the area that needs to be plated with thick nickel and hard gold.

[0047] 5.Nickel-plated thick gold

[0048] Nickel and gold layers of customer-required thickness are deposited by electroplating in nickel and gold baths.

[0049] 6. Film removal

[0050] Remove the dry film on the board to expose the metal layer.

[0051] 7. External light imaging 2

[0052] The working principle is similar to external light imaging, exposing the circuit layer, including the nickel-plated thick gold layer

[0053] 8.Tin plating

[0054] In the tin bath, a layer of metal tin is plated on the conductive area of ​​the board through the principle of electroplating for anti-etching protection.

[0055] 9. Milling half hole

[0056] According to customer requirements, the specified inner groove is dug out, leaving half a hole.

[0057] 10. Outer layer etching

[0058] Under the action of alkali solution, the film is removed to expose the copper surface to be etched. In the etching tank, copper reacts with copper ions to produce cuprous to achieve etching. In the tin stripping tank, nitric acid reacts with the tin surface to remove the tin plating layer and expose the copper surface of the circuit pad.

[0059] 11. Solder mask / characters

[0060] Solder mask: Use a screen printing net to print solder mask on the board surface, and then pre-bake to remove the volatilization to form a semi-cured film layer. Through the alignment exposure, the solder mask cross-links in the illuminated areas, and the unexposed areas are developed under the action of alkali solution. At high temperature, the solder mask is completely cured and attached to the board surface.

[0061] Characters: The production method is similar to solder mask.

[0062] 12. External light imaging 3

[0063] The working principle is similar to external light imaging. This time, the nickel-thick gold area is covered with a dry film. The area that needs to be immersing gold is exposed to facilitate immersion gold.

[0064] 13. Immersion Gold

[0065] Through chemical replacement reaction, a layer of metal nickel and gold is deposited on the copper surface.

[0066] 14. Stripping 2

[0067] The working principle is similar to film stripping, which removes the dry film on the board and exposes the thick gold layer of electroplated nickel.

[0068] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A method for manufacturing a semi-hole plate with partial hard gold plating where leads cannot be pulled, characterized in that: include: First, the electroplated copper thickness meets the requirements, and a nickel thick gold layer is made in advance, and then tinning is performed, half a hole is milled, and a pattern is etched out, and surface treatment is performed after solder mask characters are applied; specifically, the electroplated copper thickness meets the requirements, and then nickel thick gold is plated locally. After the nickel thick gold is applied, the film is exposed to make a dry film pattern, and a half hole is milled directly after tinning, and then etching is performed. In this way, the local position of the circuit pattern is plated with thick gold in advance, and after solder mask and characters are made, the surface treatment is OSP, then OSP is performed normally, and if it is immersion gold, the hard gold position needs to be selectively covered with dry film, and the film can be removed after immersion gold; The specific steps include: Step 1, cutting; Step 2, drilling: drilling machine processing is performed on the board to prepare for the conduction of the inner and outer layers in the subsequent process; Step 3, copper deposition / negative film electroplating: remove the drilling dirt in the hole through the previous desmearing process to make the hole clean, and then activate the colloidal palladium adsorbed on the surface and in the hole, and an oxidation-reduction reaction occurs in the copper deposition tank to form a copper layer; then, the copper thickness of the hole / surface copper is thickened to the customer's required standard through electroplating; Step 4, external light imaging: at a certain temperature and pressure, a dry film is pasted on the board surface, and then the film is aligned, and finally the dry film not shielded by the film is irradiated with ultraviolet light on the exposure machine to react, forming the required circuit pattern on the board surface, and then the film not irradiated by light is dissolved by the developer in the developing section, exposing the area that needs to be plated with nickel thick hard gold; Step 5, nickel-thick gold plating: deposit nickel and gold layers of customer-required thickness in nickel and gold baths by electroplating: Step 6, film removal: remove the dry film on the board to expose the metal layer: Step 7, external light imaging 2: The working principle is similar to external light imaging, exposing the circuit layer, including the nickel-plated thick gold layer; Step 8, tin plating: In the tin bath, a layer of metal tin is plated on the conductive area of ​​the board through the principle of electroplating for anti-etching protection; Step 9, milling half hole: mill the specified inner groove according to customer requirements, and the remaining half hole: Step 10, outer layer etching: Under the action of alkali solution, the film is removed to expose the copper surface to be etched. In the etching tank, copper reacts with copper ions to produce cuprous to achieve etching. In the detinning tank, nitric acid reacts with the tin surface to remove the tinned layer and expose the copper surface of the circuit pad. Step 11, Solder Mask / Characters: Solder mask: Use a screen printing net to print the solder mask on the board surface and pre-bake to remove the volatilization to form a semi-cured film layer. Through the alignment exposure, the solder mask cross-links in the illuminated areas, and the unexposed areas are developed under the action of alkali solution. At high temperature, the solder mask is completely cured and attached to the board surface; Characters: The production method is similar to solder mask; Step 12, external light imaging 3: The working principle is similar to external light imaging. This time, the nickel-thick gold area is covered with a dry film, and the area that needs to be immerged gold is exposed to facilitate immersion gold. Step 13, immersion gold: deposit a layer of metal nickel and gold on the copper surface through chemical replacement reaction; Step 14, film stripping 2: Similar to the working principle of film stripping, the dry film on the board is stripped clean to expose the thick gold layer of electroplated nickel.