A heat preservation device and method for steel ingot or steel billet in high temperature alloy forging process

Through the automatic wrapping device and self-adhesive insulation blanket, the labor intensity and uneven insulation problems of manual wrapping in traditional high-temperature alloy forging are solved, efficient heat retention and fine-grained structure formation are achieved, and the operating environment is simplified.

CN110947899BActive Publication Date: 2024-10-25JIANGSU JICUI ADVANCED METAL MATERIAL RES INST CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201911388600.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-12-30
Publication Date
2024-10-25
Estimated Expiration
2039-12-30

AI Technical Summary

Technical Problem

In the traditional high-temperature alloy forging process, artificial coating of insulation materials is labor-intensive and the working environment is harsh, resulting in long heating time, high energy consumption, and the coating is uneven and easy to fall off, making it difficult to form fine-grained or ultra-fine-grained structures.

Method used

It adopts an automatic wrapping device and a self-adhesive thermal insulation blanket, and realizes rapid automatic wrapping through adjustable joint arms and glass adhesive, reducing heat loss and reducing the difficulty of forging temperature control.

Benefits of technology

It achieves rapid and uniform heat preservation during the forging process of high-temperature alloys, reduces the risk of cracking, simplifies the operating environment, and improves the ability to form fine-grained or ultra-fine-grained structures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110947899B_ABST
    Figure CN110947899B_ABST
Patent Text Reader

Abstract

The present invention provides a heat preservation device and method for steel ingots or billets in a high-temperature alloy forging process, comprising a right arm, a left arm, a base, a heat preservation blanket and a steel ingot; the right arm and the left arm are fixed on the base, and are both composed of a plurality of joints, each of which can rotate inward within an angle of 0-180 degrees; a groove is provided on the base for supporting the heat preservation blanket, and the steel ingot can be fixed on the base, and a glass adhesive is adhered to the support heat preservation blanket, so that the heat preservation blanket can be pasted on the steel ingot. The present invention adopts an automatic sheathing device and a self-adhesive heat preservation blanket to realize rapid and automatic sheathing of the steel ingot after heating, effectively reduce heat loss, meet the fine grain and ultrafine grain structure requirements of the bar, and greatly improve the working environment of the operator.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of special material forging, and in particular relates to a heat preservation device and a method for a steel ingot or a steel billet in a high-temperature alloy forging process. Background Art

[0002] The main uses of deformable high-temperature alloys are key hot-end components in important fields such as aerospace, nuclear power energy, and petrochemicals. With the rapid development of technology, these fields have higher and higher requirements for the mechanical properties and microstructure of high-temperature alloys, and the requirements for forging processes have also increased accordingly. Due to the needs of organizational properties, such as the requirement for fine or ultrafine grains, or for some highly alloyed and difficult-to-deform high-temperature alloys, the temperature control window of the key forging process is very small, that is, the forging temperature range is small, and temperature control is one of the key points of the forging process. In the actual production process, in order to control the forging temperature, the heating temperature of the forging is selected as the upper limit of the allowable deformation temperature range, and the blank is wrapped with a jacket to slow down the heat loss during the transfer process and the hot working process to obtain a better deformation structure.

[0003] The so-called jacket wrapping is to cover the surface of the ingot or billet with insulating materials such as aluminum silicate fiber blanket to slow down the heat loss of the ingot or billet due to radiation and convection, and to prevent contact heat transfer between the mold and the ingot or billet, and to block heat transfer between the ingot or billet and the air. The method of welding the stainless steel jacket to fix the insulating material on the surface of the ingot or billet is called hard jacket; the method of fixing the insulating material on the surface of the ingot or billet by gluing is called soft jacket.

[0004] At present, the main method is to directly coat the blank manually, which has high labor intensity, poor working environment and large fluctuations in coating quality.

[0005] Patent 201610272023.7 "A method for reducing the tendency of forging cracking of high-temperature alloy materials" adopts the insulation method of wrapping the steel ingot or billet before heating. This method of wrapping before heating will result in a long heating time and high energy consumption. The heating time of the same quality wrapped steel ingot or billet is more than twice that of the unwrapped steel ingot or billet.

[0006] The insulation method used in Patent 201510269497.1 "A forging method of 500kg-grade GH3230 high-temperature alloy" is to first coat the steel ingot or billet (using a spray gun or manual brushing) and then stick the insulation material on the surface of the steel ingot or billet. This method is inconvenient to operate in a high-temperature environment and has safety hazards. The artificial coating is uneven and the wrapping material is easy to fall off.

[0007] Patent 201310359168.7 "A wrapping method for forging ultra-large nickel-based high-temperature alloy turbine disks" adopts a method of soft wrapping first and then hard wrapping, that is, the high-temperature alloy blank is first wrapped and compacted with insulation cotton, and then wrapped and fixed with stainless steel belts. Although this method is complicated, it can meet the insulation requirements of disc-shaped parts forging, but it is not applicable to cylindrical ingots or billets.

[0008] In summary, the traditional sheathing method is labor-intensive and has a harsh working environment. It will also cause the high-temperature alloy billet to be heated for too long in the furnace, consume a lot of energy, and the soft sheath will easily fall off and the clamp will be easily damaged. Summary of the invention

[0009] In order to solve the above problems, the present invention provides a heat preservation device and method for steel ingots or billets in a high-temperature alloy forging process. The heat preservation device comprises a right arm, a left arm, a base, a heat preservation blanket and a steel ingot; the right arm and the left arm are fixed on the base, each of which is composed of several joints, and each joint can rotate inward within an angle of 0-180 degrees; a groove is provided on the base for supporting the heat preservation blanket and allowing the steel ingot to be fixed on the base, and a glass adhesive is adhered to the heat preservation blanket so that the heat preservation blanket can be adhered to the steel ingot.

[0010] Furthermore, the number of joints of the right arm and the left arm is 2-6.

[0011] Furthermore, the number of joints of the right arm and the left arm is preferably 3, and they are symmetrically arranged.

[0012] Furthermore, each joint of the right arm and the left arm is driven individually by a pneumatic cylinder or a hydraulic cylinder.

[0013] Furthermore, the groove on the base is preferably V-shaped.

[0014] A heat preservation method for a heat preservation device of a steel ingot or steel billet in a high-temperature alloy forging process comprises the following steps:

[0015] Step 1: Place the steel ingot or billet in a high temperature electric furnace and heat it to 1000℃-1170℃, and keep it warm for 2.5-3 hours;

[0016] Step 2: unfold the right arm and the left arm of the heat preservation device, and lay the heat preservation blanket with the glass adhesive on the right arm and the left arm, with the side with the glass adhesive facing upward; use a special syringe to adhere the glass adhesive to the heat preservation blanket;

[0017] Step 3: After heating, the steel ingot is removed from the heating furnace and hoisted onto the groove on the heat preservation device;

[0018] Step 4: First, lift the right arm of the heat preservation device to wrap the right heat preservation blanket on the steel ingot. The heat preservation blanket is adhered to the surface of the steel ingot under the action of the glass adhesive. Then, drop the right arm and return to its original position.

[0019] Step 5: The left arm of the heat preservation device is lifted and the left heat preservation blanket is wrapped on the steel ingot. The heat preservation blanket is adhered to the surface of the steel ingot under the action of the glass adhesive. The left arm falls and returns to its original position.

[0020] Step 6: Lift the steel ingot, clamp it with a manipulator, and forge it using a fast forging machine.

[0021] The present invention adopts an automatic sheathing device and a self-adhesive thermal insulation blanket to achieve rapid and automatic sheathing of the steel ingot after heating, effectively reducing heat loss and the risk of forging cracking of difficult-to-deform alloys, and can achieve forging within a narrow temperature range to obtain fine-grained or ultrafine-grained structures, while greatly improving the working environment of operators. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a structural schematic diagram of the present invention.

[0023] Figure 2 It is a schematic diagram of the thermal insulation blanket injection glass adhesive of the present invention.

[0024] In the figure: 1—right arm; 2—left arm; 3—base; 4—thermal insulation blanket; 5—steel ingot.

[0025] Note: The double-dotted line in the middle represents the equipment's unfolded state. DETAILED DESCRIPTION

[0026] refer to Figure 1 , a heat preservation device for steel ingots or billets in a high-temperature alloy forging process, comprising a right arm 1, a left arm 2, a base 3, a heat preservation blanket 4 and a steel ingot 5; the right arm 1 and the left arm 2 are fixed on the base 3, and are both composed of a plurality of joints, each of which is made of high-temperature resistant material to meet the use requirements in a high-temperature environment, and each joint can rotate inward within an angle of 0-180 degrees; the groove on the base 3 is preferably a V-shaped groove, which is used to support the heat preservation blanket 4 and enable the steel ingot 5 to be fixed on the base 3, and a glass adhesive is adhered to the support heat preservation blanket 4 so that the heat preservation blanket 4 can be adhered to the steel ingot 5. Figure 1 In the embodiment, the number of joints of the right arm 1 and the left arm 2 is preferably 3 and symmetrically arranged. Each joint of the right arm 1 and the left arm 2 is driven individually by a cylinder or a hydraulic cylinder.

[0027] Example 1: High temperature alloy GH5188 round bar forging

[0028] 1. Place the GH5188 steel ingot with a diameter of 508mm in a high-temperature electric furnace and heat it to 1170℃, and keep it warm for 3 hours;

[0029] 2. Unfold the right arm 1 and the left arm 2 of the heat preservation device, and lay the heat preservation blanket 4 with the glass adhesive on it on the right arm 1 and the left arm 2, with the glass adhesive facing upwards; use a special syringe to adhere the glass adhesive to the heat preservation blanket 4, refer to the attached Figure 2 , the black spot is the glass adhesive;

[0030] 3. After heating, the steel ingot 5 is moved out of the heating furnace and hoisted onto the V-shaped groove on the insulation device;

[0031] 4. The right arm 1 of the heat preservation device is first lifted to wrap the right heat preservation blanket 4 onto the steel ingot 5. Under the action of the glass adhesive, the heat preservation blanket 4 is adhered to the surface of the steel ingot 5. The right arm 1 falls down and returns to its original position.

[0032] 5. The left arm 2 of the heat preservation device is lifted and the left heat preservation blanket 4 is wrapped around the steel ingot 5. The heat preservation blanket 4 is adhered to the surface of the steel ingot 5 by the action of the glass adhesive. The left arm 2 falls and returns to its original position.

[0033] 6. The steel ingot 5 is lifted off, clamped by a manipulator, and forged using a high-speed forging machine.

[0034] Example 2: Forging of fine-grained bars of high-temperature alloy GH4169

[0035] 1. Place the GH4169 steel billet with a diameter of 360 mm in a high-temperature electric furnace and heat it to 1000-1020°C, and keep it warm for 2.5 hours;

[0036] 2. Unfold the right arm 1 and the left arm 2 of the heat preservation device, and lay the heat preservation blanket 4 with the glass adhesive on it on the right arm 1 and the left arm 2, with the glass adhesive facing upwards; use a special syringe to adhere the glass adhesive to the heat preservation blanket 4, refer to the attached Figure 2 , the black spot is the glass adhesive;

[0037] 3. After heating, the steel ingot 5 is moved out of the heating furnace and hoisted onto the V-shaped groove on the insulation device;

[0038] 4. The right arm 1 of the heat preservation device is first lifted to wrap the right heat preservation blanket 4 onto the steel ingot 5. Under the action of the glass adhesive, the heat preservation blanket 4 is adhered to the surface of the steel ingot 5. The right arm 1 falls down and returns to its original position.

[0039] 5. The left arm 2 of the heat preservation device is lifted and the left heat preservation blanket 4 is wrapped around the steel ingot 5. The heat preservation blanket 4 is adhered to the surface of the steel ingot 5 by the action of the glass adhesive. The left arm 2 falls and returns to its original position.

[0040] 6. The billet is lifted off, clamped by a manipulator, and forged by a fast forging machine, with a forging deformation of 40 to 60%. Through the above process, GH4169 bars with 6 to 8 fine grains can be obtained.

Claims

1. A heat preservation method for a heat preservation device of a steel ingot or steel billet in a high temperature alloy forging process, comprising the following steps: Step 1: Place the steel ingot or billet in a high temperature electric furnace and heat it to 1000℃-1170℃, and keep it warm for 2.5-3 hours; Step 2: unfold the right arm (1) and the left arm (2) of the heat preservation device, and lay the heat preservation blanket (4) to which the glass adhesive has been adhered on the right arm (1) and the left arm (2), with the side with the glass adhesive facing upwards; the glass adhesive is adhered to the heat preservation blanket (4) using a special syringe; Step 3: After heating, the steel ingot (5) is removed from the heating furnace and hoisted onto a groove on the heat preservation device; Step 4: The right arm (1) of the heat preservation device is first lifted to wrap the right heat preservation blanket (4) onto the steel ingot (5). The heat preservation blanket (4) is adhered to the surface of the steel ingot (5) under the action of the glass adhesive, and the right arm (1) is dropped and returned to its original position. Step 5: The left arm (2) of the heat preservation device is lifted and the left heat preservation blanket (4) is wrapped around the steel ingot (5). The heat preservation blanket (4) is adhered to the surface of the steel ingot (5) under the action of the glass adhesive, and the left arm (2) is dropped and returned to its original position. Step six, the steel ingot (5) is lifted off, clamped by a manipulator, and forged by a fast forging machine. The heat preservation device for the steel ingot or billet in the high-temperature alloy forging process comprises a right arm (1), a left arm (2), a base (3), a heat preservation blanket (4), and the steel ingot (5); the right arm (1) and the left arm (2) are fixed on the base (3), and each is composed of a plurality of joints, and each joint can rotate inward within an angle of 0-180 degrees; a groove is provided on the base (3) for supporting the heat preservation blanket (4) and allowing the steel ingot (5) to be fixed on the base (3); a glass adhesive is adhered to the supporting heat preservation blanket (4) so ​​that the heat preservation blanket (4) can be adhered to the steel ingot (5).

2. The heat preservation method of a heat preservation device for a high temperature alloy forging process steel ingot or steel billet according to claim 1, characterized in that: The number of joints of the right arm (1) and the left arm (2) is 2-6.

3. The heat preservation method of a heat preservation device for a high temperature alloy forging process steel ingot or steel billet according to claim 2, characterized in that: The number of joints of the right arm (1) and the left arm (2) is preferably three, and they are symmetrically arranged.

4. The heat preservation method of a heat preservation device for a high temperature alloy forging process steel ingot or steel billet according to claim 1, characterized in that: Each joint of the right arm (1) and the left arm (2) is driven individually by a pneumatic cylinder or a hydraulic cylinder.

5. The heat preservation method of a heat preservation device for a high temperature alloy forging process steel ingot or steel billet according to claim 1, characterized in that: The groove on the base (3) is preferably V-shaped.