Method for manufacturing a rewiring structure

By using phase shift mask and double exposure technology in integrated fan-out packages, the problem of redistribution circuit structures that are difficult to manufacture submicron scale spacing in the prior art is solved, and a combination of high resolution and wide focus depth is achieved. Meets the needs of high-density packaging.

CN111128768BActive Publication Date: 2024-11-15TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201911043962.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-10-02
Filing Date
2019-10-30
Publication Date
2024-11-15
Estimated Expiration
2039-10-30

AI Technical Summary

Technical Problem

The prior art is difficult to manufacture redistribution circuit structures with submicron scale spacing in integrated fan-out packages, especially in the problem of improving image contrast and optical resolution while maintaining a wide focal depth.

Method used

Using phase shift mask and double exposure technology, exposure is performed through an I-line step lithography machine, using numerical apertures equal to or less than 0.18, to form a conductive pattern with submicron scale spacing, and to adjust the seed layer and conductivity through the etching process. The shape of the pattern is to achieve the manufacturing of the redistribution circuit structure.

Benefits of technology

It realizes improving optical resolution on I-line exposure tools, extends the critical size of rewiring conductive patterns to submicron scale, exceeds the capabilities of traditional I-line exposure tools, and meets the needs of high-density packaging.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111128768B_ABST
    Figure CN111128768B_ABST
Patent Text Reader

Abstract

The embodiment of the present invention discloses a method for manufacturing a redistribution wiring structure, and one of the methods includes the following steps. A seed layer is formed on a tube core and an encapsulation body encapsulating the tube core. A photoresist material is formed on the seed layer. Using a numerical aperture equal to or less than 0.18, the photoresist material is exposed to an I-line wavelength in an I-line stepper lithography machine through a phase shift mask. The photoresist material is developed to form a photoresist layer, and the photoresist layer includes a photoresist pattern and an opening between the photoresist patterns. A conductive material is formed in the opening. The photoresist pattern is removed to form a conductive pattern. By using the conductive pattern as a mask, the seed layer is partially removed to form a seed layer pattern below the conductive pattern, wherein the redistribution conductive pattern includes the seed layer pattern and the conductive pattern, respectively.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] An embodiment of the present invention relates to a method for manufacturing a redistribution wiring structure. Background Art

[0002] The semiconductor industry has experienced rapid growth due to the continued increase in the integration density of various electronic components (i.e., transistors, diodes, resistors, capacitors, etc.). In large part, this increase in integration density comes from the repeated reduction of the minimum feature size, which enables more smaller components to be integrated into a given area. These smaller electronic components also require smaller packages that utilize a smaller area compared to previous packages. Some smaller types of packages for semiconductor components include quad flat packages (QFP), pin grid array (PGA) packages, ball grid array (BGA) packages, and the like.

[0003] Currently, integrated fan-out packages are becoming increasingly popular due to their compactness. Integrated fan-out packages typically include a redistribution wiring structure located above a molded integrated circuit device to provide access to the integrated circuit device. In order to meet the demand for smaller size and higher packaging density, the manufacturing method of the redistribution wiring structure has become an important issue in this field. Summary of the invention

[0004] A method for manufacturing a redistribution wiring structure according to an embodiment of the present invention comprises the following steps. A seed layer is formed on a tube core and an encapsulation body encapsulating the tube core. A first photoresist material is formed on the seed layer. The first photoresist material is exposed to an I-line wavelength in an I-line stepper lithography machine through a phase-shift mask using a numerical aperture equal to or less than 0.18. The first photoresist material is developed to form a first photoresist layer, wherein the first photoresist layer includes a plurality of first photoresist patterns and a plurality of first openings between the plurality of first photoresist patterns. A first conductive material is formed in the plurality of first openings. The first photoresist layer is removed to form a plurality of first conductive patterns. The seed layer is partially removed using the plurality of first conductive patterns as a mask to form a plurality of seed layer patterns below the plurality of first conductive patterns, wherein a plurality of redistribution conductive patterns respectively include the plurality of seed layer patterns and the plurality of first conductive patterns. BRIEF DESCRIPTION OF THE DRAWINGS

[0005] The various aspects of the present invention will be best understood by reading the following detailed description in conjunction with the accompanying drawings. It should be noted that, in accordance with standard practice in the industry, various features are not drawn to scale. In fact, the key dimensions of various features may be arbitrarily increased or decreased for clarity of discussion.

[0006] Figures 1A to 1H is a schematic cross-sectional view illustrating a manufacturing process of a package according to some embodiments of the present invention.

[0007] FIG. 2A to FIG. 2F is a cross-sectional view showing a manufacturing process of a redistribution wiring structure according to some embodiments of the present invention.

[0008] FIG. 3A to FIG. 3F is a cross-sectional view showing a manufacturing process of a redistribution wiring structure according to some embodiments of the present invention. DETAILED DESCRIPTION

[0009] The following disclosure provides many different embodiments or examples for implementing the different features of the provided subject matter. Specific examples of components and arrangements are described below to simplify the present invention. Of course, these are only examples and are not intended to be limiting. For example, the following description in which a second feature is formed on or on a first feature may include an embodiment in which the second feature is formed to be in direct contact with the first feature, and may also include an embodiment in which an additional feature may be formed between the second feature and the first feature so that the second feature may not be in direct contact with the first feature. In addition, the present invention may reuse reference numbers and / or letters in various examples. This repetition is for the purpose of brevity and clarity, rather than indicating the relationship between the various embodiments and / or configurations discussed by itself.

[0010] Additionally, for ease of description, spatially relative terms such as "beneath," "below," "lower," "on," "over," "overlying," "above," "upper," etc. may be used herein to describe the relationship of one element or feature shown in the figures to another (other) element or feature. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations), and the spatially relative descriptors used herein may be interpreted accordingly.

[0011] The advanced lithography processes, methods, and materials described in the current disclosure can be used in many applications, including fin-type field effect transistors (FinFETs). For example, fins can be patterned to produce relatively tight spacing between features, which is well suited for the above disclosure. In addition, spacers used in forming fins of FinFETs can be processed according to the above disclosure.

[0012] Figures 1A to 1His a schematic cross-sectional view showing a manufacturing process of a package according to some embodiments of the present invention. Figure 1A , a carrier C is provided. A stripping layer DB and a dielectric layer DI are stacked in a sequential order on the carrier C. In some embodiments, the stripping layer DB is formed on the upper surface of the carrier C, and the stripping layer DB is between the carrier C and the dielectric layer DI. The carrier C is, for example, a glass substrate. On the other hand, in some embodiments, the stripping layer DB is a light-to-heat conversion (LTHC) release layer formed on the glass substrate. In some embodiments, the dielectric layer DI is, for example, a polymer, such as polyimide, benzocyclobutene (BCB), polybenzoxazole (PBO), etc. In some alternative embodiments, the dielectric layer DI may include a non-organic dielectric material, such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, etc. However, the materials of the stripping layer DB, the carrier C, and the dielectric layer DI are for illustration only, and the present invention is not limited thereto.

[0013] A plurality of conductive pillars 102 and a plurality of tube cores 104 are arranged on the dielectric layer DI. The tube core 104 is mounted on the dielectric layer DI on which the conductive pillars 102 are formed. In some embodiments, a die attach film (DAF) (not shown in the figure) is located between the tube core 104 and the dielectric layer DI, and is used to attach the tube core 104 to the dielectric layer DI. The tube core 104 is arranged in an array and surrounded by the conductive pillars 102. The tube core 104 is, for example, a semiconductor tube core. Each of the tube cores 104 includes an active surface 104a, a plurality of pads 104b distributed on the active surface 104a, a passivation layer 104c covering the active surface 104a, a plurality of conductive pillars 104d and a protective layer 104e. The pad 104b is partially exposed by the passivation layer 104c. The conductive pillar 104d is disposed on the pad 104b and electrically connected to the pad 104b, and the protective layer 104e covers the conductive pillar 104d and the passivation layer 104c. For example, the conductive pillar 104d is a copper pillar or other suitable metal pillar. In some embodiments, the protective layer 104e may be a polybenzoxazole (PBO) layer, a polyimide (PI) layer or other suitable polymer. In some alternative embodiments, the protective layer 104e may be made of an inorganic material. Figure 1A As shown in , the top surface of the die 104 is lower than the top surface of the conductive pillar 102. However, the present invention is not limited thereto. In some alternative embodiments, the top surface of the die 104 may be substantially coplanar with the top surface of the conductive pillar 102 or higher than the top surface of the conductive pillar 102.

[0014] Reference Figure 1B, an insulating material 106 is formed on the dielectric layer DI to encapsulate the conductive pillar 102 and the tube die 104. In some embodiments, the insulating material 106 is a molding compound formed by a molding process. The conductive pillar 102 and the protective layer 104e of the tube die 104 are encapsulated by the insulating material 106. In other words, the conductive pillar 102 and the protective layer 104e of the tube die 104 are not exposed and are fully protected by the insulating material 106. In some embodiments, the insulating material 106 may include epoxy resin or other suitable materials.

[0015] Reference Figure 1C , grinding the insulating material 106 and the protective layer 104e of the tube core 104 until the top surface of the conductive pillar 104d is exposed. After grinding the insulating material 106, an encapsulation 106' is formed on the dielectric layer DI. During the aforementioned grinding process, a portion of the protective layer 104e is also ground to form the protective layer 104e'. In some embodiments, during the aforementioned grinding process of the insulating material 106 and the protective layer 104e, a portion of the conductive pillar 104d and a portion of the conductive pillar 102 are ground until the top surface of the conductive pillar 104d and the top surface of the conductive pillar 102 are exposed. In other words, the encapsulation 106' exposes at least a portion of the tube core 104 and at least a portion of the conductive pillar 102. In some embodiments, the encapsulation 106' can be formed by mechanical grinding, chemical mechanical polishing (CMP), or another suitable mechanism.

[0016] The encapsulation body 106' encapsulates the sidewalls of the die 104, and the encapsulation body 106' is penetrated by the conductive pillar 102. In other words, the die 104 and the conductive pillar 102 are embedded in the encapsulation body 106'. It should be noted that although the die 104 and the conductive pillar 102 are embedded in the encapsulation body 106', the encapsulation body 106' exposes the top surface of the die 104 and the conductive pillar 102. In other words, the top surface of the conductive pillar 102, the top surface of the protection layer 104e', and the top surface of the conductive pillar 104d are substantially coplanar with the top surface of the encapsulation body 106'.

[0017] In some embodiments, after forming the encapsulant 106' to encapsulate the die 104, the entire package may experience global warping, for example, due to differences in the coefficient of thermal expansion (CTE) and stiffness between the die 104 and the encapsulant 106'. The global warping may cause a height variation (difference) that may range from 10 μm to 20 μm across the top surface of the entire package. In some embodiments, individual dies 104 may experience local warping, and this may cause a height variation (difference) across the top surface of the individual dies 104. However, in some embodiments, after the above-mentioned grinding process, the height variation due to local warping may range from 3 μm to 5 μm, which may be negligible.

[0018] Reference Figure 1D After forming the encapsulation body 106' and the protection layer 104e', a dielectric layer 108 is formed on the top surface of the conductive pillar 102, the top surface of the encapsulation body 106', the top surface of the conductive pillar 104d, and the top surface of the protection layer 104e'. In some embodiments, the dielectric layer 108 is, for example, a polymer, such as polyimide, benzocyclobutane (BCB), polybenzoxazole (PBO), etc. In some alternative embodiments, the dielectric layer 108 may include a non-organic dielectric material, such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, etc. Then, a plurality of through holes 110 are formed in the dielectric layer 108, wherein each of the through holes 110 is electrically connected to one of the conductive pillars 104d of the tube core 104 or one of the conductive pillars 102. In some embodiments, a plurality of openings (not shown in the figure) are formed in the dielectric layer 108, and then the through holes 110 are respectively formed in the openings. In some embodiments, the top surface of the conductive pillar 104d and the top surface of the conductive pillar 102 are in contact with the via 110. In some embodiments, for example, the via 110 is a copper via or other suitable metal via. In some embodiments, for example, the via 110 may include a seed layer and a conductive layer on the seed layer.

[0019] Reference Figure 1E A redistribution wiring structure 112 electrically connected to the through hole 110 is formed on the top surface of the dielectric layer 108. Figure 1EAs shown in , the redistribution wiring structure 112 includes a plurality of redistribution conductive patterns 112a and a plurality of interlayer dielectric layers 112b that are alternately stacked. In some embodiments, the redistribution conductive pattern 112a is electrically connected to a through hole 110 embedded in the dielectric layer 108, wherein the top surface of the through hole 110 is in contact with the bottommost redistribution conductive pattern 112a of the redistribution wiring structure 112. In addition, the topmost redistribution conductive pattern 112a includes a plurality of pads. In some embodiments, the aforementioned pads include a plurality of under-ball metallurgy (UBM) patterns 112a1 for ball mounting and / or at least one connecting pad 112a2 for passive component mounting. The number of under-ball metal patterns 112a1 and connecting pads 112a2 is not limited in the present invention.

[0020] The formation of the redistribution wiring structure 112 will be described in detail below. FIG. 2A to FIG. 2F It is to show some embodiments according to the present invention Figure 1E FIG. 1 is a cross-sectional view of the manufacturing process of the redistribution wiring structure 112 shown in FIG. FIG. 2A to FIG. 2F The diagrams shown in the figure are for illustrative purposes only. FIG. 2A to FIG. 2F The proportions, sizes and shapes shown may not reflect the exact Figure 1D However, like elements are denoted by like reference numerals to establish FIG. 2A to FIG. 2F and Figure 1E The correlation between them.

[0021] Currently, in order to cover the high topography and high warpage characteristics of packages such as integrated fan-out (INFO) packages or INFO ultra-high density (UHD) packages, I-line and low numerical aperture (NA) of 0.18 or less are applied to obtain a wider depth of focus (DOF). However, low NA causes low image contrast, and the pitch resolution (also called "minimum pitch") is correspondingly limited, that is, the pitch is greater than 2μm. In other words, by using I-line and low NA, it is difficult to obtain conductive lines with critical dimensions of submicron scale (e.g., 1μm or less). In detail, the "pitch" is the sum of the line width and the space width, and the "minimum pitch (also called pitch resolution)" is the pitch that can be resolved by a projection optical exposure device with a predetermined wavelength λ and numerical aperture NA. It is known that the pitch resolution is determined by the Rayleigh formula: R = k1(λ / NA), where R is the resolution of the pattern, NA is the numerical aperture, λ is the wavelength of the light used for exposure, and k1 is a constant. Depth of focus (DOF) is defined as DOF ​​= k2(λ / (NA) 2 ), where k2 is a constant, NA is the numerical aperture, and λ is the wavelength of the light used for exposure. As previously described, high DOF is obtained by using I-line and low NA, however, this can adversely affect the pitch resolution. In some embodiments, in order to reduce the pitch without changing the exposure conditions of I-line and low NA, a phase shift mask is used or the constant k1 in the Rayleigh formula is adjusted to improve the pitch resolution. In other words, image contrast and optical resolution are improved while maintaining a wide DOF. Therefore, under the exposure conditions of I-line and low NA, the critical dimension of the pattern can be reduced to a sub-micron scale. In other words, the optical resolution is improved and exceeds the capabilities of current I-line exposure tools.

[0022] Reference Figure 2A , providing a substrate SUB. The substrate SUB has a first region R1 and a second region R2. In some embodiments, the substrate SUB may be Figure 1DAs shown in the figure, a carrier C, a peeling layer DB, a dielectric layer DI, a conductive column 102, a tube core 104, an encapsulation body 106', a dielectric layer 108 and a through hole 110 are included. However, the present invention is not limited to this. Subsequently, a seed layer 210 is formed on the substrate SUB. In some embodiments, the seed layer 210 is formed on the top surface of the through hole 110 and the dielectric layer 108. In some embodiments, the seed layer 210 is in contact with the top surface of the through hole 110 and the dielectric layer 108. In some embodiments, the material of the seed layer 210 may, for example, include copper, copper alloy or other suitable material selections. In some embodiments, the seed layer 210 is formed by a sputtering method, a deposition method (such as physical vapor deposition) or other applicable methods. In some embodiments, for example, the seed layer 210 may have a thickness of about 0.01 μm to about 1 μm.

[0023] In some embodiments, a photoresist material 220 may be formed on the seed layer 210, and a phase shift mask PSM may be disposed corresponding to and on the photoresist material 220. In some embodiments, the photoresist material 220 is a positive photoresist. In an alternative embodiment, for example, the photoresist material 220 may be a negative photoresist. In some embodiments, an I-line stepper lithography machine (not shown in the figure, also referred to as an I-line scanner) is provided. The I-line stepper lithography machine is an I-line type lithography optical system that uses ultraviolet light (UV) with an exposure wavelength of 365nm. For example, the optical lithography system may include a light source, light, a focusing lens, a photomask, a mask carrier, a projection lens, and a package carrier. However, there may be other configurations and inclusions or omissions of the system. The light source includes a radiation source that provides light with a single wavelength of 365nm. For example, a mercury lamp may be used, which is operable to provide an I-line (e.g., 365nm) wavelength. In some embodiments, Figure 2A The package shown is arranged on a package carrier. In some embodiments, for example, the photomask is a phase shift mask PSM. For example, the phase shift mask PSM may be an alternating aperture phase shift mask (alt-PSM), an attenuating PSM (att-PSM) or other suitable phase shift masks. In some embodiments, the phase shift mask PSM includes a plurality of patterns MP and a plurality of openings OP between the patterns MP. The pattern MP may be designed to form a rewiring conductive pattern 112a, such as a through hole, a conductive line or other possible conductive pattern. In some embodiments, the phase shift mask PSM includes a plurality of patterns (not shown in the figure) designed to form a rewiring conductive pattern 112a (such as a through hole, a conductive line or other possible conductive pattern).

[0024] Reference Figure 2B, performing an exposure step, that is, using an exposure condition to expose the photoresist material 220 to the I-line wavelength in the I-line stepper through the phase shift mask PSM. Then, the photoresist material 220 is developed to form a photoresist layer 220', thereby transferring the pattern MP of the phase shift mask PSM to the photoresist layer 220'. In some embodiments, the photoresist layer 220' includes a plurality of photoresist patterns 222a, 222b and a plurality of openings 224a, 224b between the photoresist patterns 222a, 222b. In some embodiments, the exposure condition is that in the Rayleigh formula, λ is the wavelength of the I line (for example, 365nm), NA is equal to or less than 0.18, and the constant k1 is a positive constant equal to or less than 0.49. In some embodiments, by using the exposure condition, the pitch P of the photoresist layer 220' corresponding to the region R1 can be equal to or less than 2μm. The pitch P (also referred to as the minimum pitch) is the sum of the width W1 (i.e., line width) of the photoresist pattern 222a and the width W2 (i.e., space width) of the opening 224a. In some embodiments, for example, when the constant k1 is a positive constant equal to or less than 0.39, the pitch P is 1.6 μm. In some embodiments, for example, the width of the photoresist pattern 222a may be 0.5 μm, and the width of the opening 224a may be 1.1 μm. In some alternative embodiments, the pitch may be equal to or less than 1.4 μm. For example, when the constant k1 is a positive constant equal to or less than 0.35, the pitch may be 1.4 μm. In some embodiments, as required, the pitch of the photoresist layer 220' corresponding to other regions (e.g., region R2 in which the photoresist pattern 222b is disposed) may be greater than 2 μm. In some embodiments, for example, the openings 224a, 224b are disposed corresponding to the through hole 110 and may be disposed directly above the through hole 110.

[0025] Reference Figure 2C , the conductive material 230 is partially filled into the openings 224a, 224b of the photoresist layer 220'. In some embodiments, for example, the top surface of the conductive material 230 is lower than the top surface of the photoresist layer 220'. However, in some alternative embodiments, the top surface of the conductive material 230 may be substantially coplanar with the top surface of the photoresist layer 220'. In some embodiments, the conductive material 230 may be formed by a plating process. The plating process is, for example, electroplating, electroless plating, immersion plating, etc. The conductive material 230 is, for example, copper, a copper alloy, etc. In some embodiments, the seed layer 210 and the conductive material 230 include the same material. For example, the seed layer 210 and the conductive material 230 are made of the same material.

[0026] Reference Figure 2D, then remove the photoresist layer 220' to present a plurality of conductive patterns 232a, 232b, and expose a portion of the seed layer 210. Because the conductive patterns 232a, 232b originate from the openings 224a, 224b, the conductive patterns 232a, 232b also have the same configuration. That is, the pitch P (also referred to as the minimum pitch) is the sum of the line width W2 of the conductive pattern 232a and the spacing width W1 between the conductive patterns 232a. The pitch P may be equal to or less than 2μm. In some embodiments, for example, the photoresist layer 220' is removed by a stripping process. A portion of the seed layer 210 is covered by the conductive patterns 232a, 232b, and a portion of the seed layer 210 between the conductive patterns 232a, 232b is exposed. In some embodiments, for example, the conductive patterns 232a, 232b may be conductive lines.

[0027] like Figure 2D and Figure 2E As shown in , in some embodiments, additional patterns may be formed over the conductive patterns 232a, 232b. For example, an additional conductive pattern 252 may be formed in the second region R2. Figure 2D After forming the conductive patterns 232a and 232b, a photoresist layer 240 is formed on the seed layer 210 and the conductive patterns 232a and 232b for additional patterning. In some embodiments, for example, the photoresist layer 240 has an opening 242 to expose the conductive pattern 232b. In some embodiments, for example, the width of the opening 242 is less than the line width of the conductive pattern 232b. Then, the conductive material 250 is partially filled into the opening 242 of the photoresist layer 240. In some embodiments, for example, the top surface of the conductive material 250 is lower than the top surface of the photoresist layer 240. In some embodiments, the conductive material 250 can be formed by a plating process. The plating process is, for example, electroplating, electroless plating, immersion plating, etc. The conductive material 250 is, for example, copper, a copper alloy, etc.

[0028] Reference Figure 2E , and then, the photoresist layer 240 is subsequently removed to present a conductive pattern 252 in the second region R2. In some embodiments, for example, the conductive pattern 252 may be a through hole. In some embodiments, for example, the photoresist layer 240 is removed by a stripping process. In some embodiments, for example, the width of the conductive pattern 252 may be substantially the same as the width of the conductive pattern 232a. In some alternative embodiments, the formation of the conductive pattern 252 may be omitted.

[0029] Reference Figure 2F, thereafter, by using the conductive patterns 232a, 232b as mask layers, the seed layer 210 is partially removed to form a plurality of seed layer patterns 210a, 210b under the conductive patterns 232a, 232b, respectively. In detail, for example, portions of the seed layer 210 exposed by the conductive patterns 232a, 232b are selectively removed by wet etching or dry etching. It should be noted that, inevitably, the material of the conductive patterns 232a, 232b, 252 may be partially removed during the etching process of the seed layer 210. Specifically, the width and / or height of the conductive patterns 232a, 232b, 252 may be reduced, thereby obtaining a plurality of remaining conductive patterns 232a', 232b', 252'. In some embodiments, the remaining conductive patterns 232a' have a post-etching line width W2' that is smaller than the line width W2, the spacing width W1' between the conductive patterns 232a' is larger than the spacing width W1, and the pitch P is (W1'+W2'), which is equal to (W1+W2). In other words, the pitch P remains substantially the same before and after the etching process of the seed layer 210, such as FIG. 2E to FIG. 2F As shown in . In some embodiments, by controlling the line width and the space width of the photoresist layer 220' corresponding to the region R1 and the etching process conditions of the seed layer 210, the desired line width of the conductive pattern 232a' can be obtained. For example, the line width W2' and the space width W1' can be equal to half of the pitch P, respectively. In an embodiment where the pitch P is 1.6 μm, the line width W2' and the space width W1' can be 0.8 μm, respectively. In other words, the critical dimension is a sub-micron scale.

[0030] like Figure 2F As shown in , the sidewalls of the conductive patterns 232a', 232b' are substantially flush with the sidewalls of the seed layer pattern 210a. Through the aforementioned etching process, the sidewalls of the conductive patterns 232a', 232b' are substantially aligned with the sidewalls of the seed layer pattern 210a. The conductive patterns 232a', 232b' and the seed layer pattern 210a thereunder constitute conductive structures 234A, 234B that can be used as conductive lines or through holes. The conductive pattern 252' can be used as a through hole. In some embodiments, a dielectric layer 236 can be formed to cover the conductive structures 234A, 234B and the conductive pattern 252', and, for example, the dielectric layer 236 can be used as one of the interlayer dielectric layers 112b. In some embodiments, by adjusting the constant k1 using a phase shift mask PSM or adjusting the constant k1 using other means, the critical dimension of the conductive structure 234A can be reduced to a submicron scale.

[0031] In some embodiments, the redistribution wiring structure 112 is a multi-layer structure (eg, Figure 1E In this case, FIG. 2A to FIG. 2FThe steps shown in can be repeated several times to present the redistribution wiring structure 112. In some embodiments, the redistribution wiring structure 112 includes at least one redistribution pattern 112a having a conductive structure 234A, and other redistribution patterns 112a can have any one of the conductive structures 234A, 234B and the conductive pattern 252' or other suitable structures.

[0032] It should be noted that FIG. 2A to FIG. 2F The steps shown in the Figure 1E The above steps may be used for redistribution wiring structures located at other locations in the package. In some embodiments, the width of the lower redistribution conductive pattern 112a near the tube core 104 may be smaller than that near the conductive terminal 114 ( Figure 1F 104d) because the size of the conductive pillar 104d is much smaller than the size of the conductive terminal 114. Therefore, in some embodiments, the aforementioned photolithography may be applied to form the lower redistribution conductive pattern 112a. In some embodiments, for example, the redistribution conductive pattern 112a having the conductive structure 234A may contact the through hole 110. In some alternative embodiments, for example, the through hole 110 may be formed by applying the aforementioned photolithography.

[0033] Return to reference Figure 1F After forming the redistribution wiring structure 112, a plurality of conductive terminals 114 are placed on the under ball metal pattern 112a1, and a plurality of passive components 116 are installed on the connection pads 112a2. In some embodiments, the conductive terminals 114 may be placed on the under ball metal pattern 112a1 by a ball planting process or other suitable process, and the passive components 116 may be installed on the connection pads 112a2 by a welding process, a reflow process, or other suitable process.

[0034] Reference Figure 1G After the conductive terminals 114 and the passive components 116 are mounted on the redistribution wiring structure 112, the dielectric layer DI formed on the bottom surface of the encapsulation body 106' is peeled off from the peeling layer DB, so that the dielectric layer DI is separated from the carrier C. In other words, the carrier C is removed. In some embodiments, the peeling layer DB (for example, the LTHC release layer) can be irradiated by UV laser, so that the dielectric layer DI adhered to the bottom surface of the encapsulation body 106' is peeled off from the carrier C. Figure 1F As shown in , the dielectric layer DI is then patterned to form a plurality of contact openings O to partially expose the conductive pillars 102. The number of the contact openings O corresponds to the number of the conductive pillars 102. In some embodiments, the contact openings O of the dielectric layer DI are formed by a laser drilling process, a mechanical drilling process, or other suitable processes.

[0035] Reference Figure 1HAfter forming contact openings O in the dielectric layer DI, a plurality of conductive terminals 118 are placed in the contact openings O, and the conductive terminals 118 are electrically connected to the conductive pillars 102. Herein, the formation of the integrated fan-out (INFO) package array is substantially completed. Figure 1H As shown in , after forming the conductive terminals 114 and the conductive terminals 118, the INFO package array is cut to form a plurality of INFO packages 10 having a double-sided terminal design. In some embodiments, the cutting process or the singulation process generally involves cutting using a rotating blade or a laser beam. In other words, the cutting or singulation process is, for example, a laser cutting process, a mechanical cutting process, or other suitable processes. In some alternative embodiments, the INFO package 10 may be stacked with other electronic devices (e.g., another INFO package, a memory device, a ball grid array (BGA), or a wafer). For example, another package (e.g., an IC package) may be stacked on the INFO package 10 and electrically connected to the INFO package 10 through the conductive terminals 118 to produce a package-on-package (POP) structure.

[0036] FIG. 3A to FIG. 3F It is to show some embodiments according to the present invention Figure 1E FIG. 1 is a cross-sectional view of the manufacturing process of the redistribution wiring structure 112 shown in FIG. FIG. 3A to FIG. 3F The diagrams shown in the figure are for illustrative purposes only. FIG. 3A to FIG. 3F The proportions, sizes and shapes shown may not reflect the exact Figure 1E However, like elements are denoted by like reference numerals to establish FIG. 3A to FIG. 3F and Figure 1E The correlation between them.

[0037] Reference Figure 3A , a substrate SUB is provided, and a seed layer 210 is formed on the substrate SUB. Then, a photoresist material 220 may be formed on the seed layer 210. The structures and materials of the substrate SUB, the seed layer 210, and the photoresist material 220 are similar to Figure 2A and 2B , and therefore the details are omitted herein.

[0038] In some embodiments, in order to form sub-micron-scale spacing, a double exposure method is used. The double exposure method consists of two separate exposures on the same photoresist layer using two different photomasks. Double exposure can define the minimum size feature twice with a twice-enlarged line-to-space ratio, and thus improve the lithography resolution.

[0039] Thereafter, a first mask M1 is disposed on the photoresist material 220. Then, a first exposure step is performed, that is, the photoresist material 220 in the first region 220a is exposed to the I-line wavelength in the I-line stepper through the first mask M1. In some embodiments, the NA is equal to or less than 0.18. In some embodiments, the first mask M1 has a plurality of patterns MP1 and a plurality of openings OP1 between the patterns MP1, and the openings OP1 are disposed corresponding to the first region 220a. In some embodiments, for example, the ratio of the width of the pattern MP1 to the width of the opening OP1 is substantially 3:1.

[0040] Reference Figure 3B , a second mask M2 is set on the photoresist material 220. Then, a second exposure step is performed, that is, the photoresist material 220 in the second area 220b is exposed to the I-line wavelength in the I-line stepper through the second mask M2. In some embodiments, NA is equal to or less than 0.18. In some embodiments, the second mask M2 has a plurality of patterns MP2 and a plurality of openings OP2 between the patterns MP2, and the openings OP2 are arranged corresponding to the second area 220b. In some embodiments, for example, the ratio of the width of the pattern MP2 to the width of the opening OP2 is substantially 3:1. In some embodiments, the pitch of the second mask M2 is equal to the pitch of the first mask M1. In some embodiments, the first area 220a and the second area 220b are arranged alternately.

[0041] Reference Figure 3C , the photoresist material 220 is developed to form a photoresist layer 220', thereby transferring the pattern MP1 of the first mask M1 and the pattern MP2 of the second mask M2 to the photoresist layer 220'. In some embodiments, the photoresist layer 220' includes a plurality of photoresist patterns 222 and a plurality of openings 224 in the regions 220a, 220b between the photoresist patterns 222. For example, the openings 224 correspond to the openings OP1, OP2. In some embodiments, by using double exposure, the pitch P of the photoresist layer 220' may be equal to or less than 2 μm. The pitch P is the sum of the width W1 (i.e., line width) of the photoresist pattern 222 and the width W2 (i.e., space width) of the opening 224. In some embodiments, for example, the width W1 of the photoresist pattern 222 may be substantially equal to the width W2 of the opening 224.

[0042] Reference Figure 3D, the conductive material 230 is partially filled into the opening 224 of the photoresist layer 220'. In some embodiments, for example, the top surface of the conductive material 230 is lower than the top surface of the photoresist layer 220'. However, in some alternative embodiments, the top surface of the conductive material 230 may be substantially coplanar with the top surface of the photoresist layer 220'. In some embodiments, the conductive material 230 may be formed by a plating process. The plating process is, for example, electroplating, electroless plating, immersion plating, etc. The conductive material 230 is, for example, copper, a copper alloy, etc. In some embodiments, the seed layer 210 and the conductive material 230 include the same material. For example, the seed layer 210 and the conductive material 230 are made of the same material.

[0043] Reference Figure 3E , the photoresist layer 220' is then removed to present a plurality of conductive patterns 232, and a portion of the seed layer 210 is exposed. Since the conductive patterns 232 originate from the openings 224, the conductive patterns 232 also have the same configuration. In some embodiments, for example, the photoresist layer 220' is removed by a stripping process. In some embodiments, the pitch P is the sum of the line width W2 of the conductive pattern 232 and the spacing width W1 between the conductive patterns 232.

[0044] Reference Figure 3F , thereafter, by using the conductive pattern 232 as a mask, the seed layer 210 is partially removed to form a plurality of seed layer patterns 210a respectively under the conductive pattern 232. In detail, for example, the portion of the seed layer 210 exposed by the conductive pattern 232 is selectively removed by wet etching or dry etching. It should be noted that, inevitably, the material of the conductive pattern 232 may be partially removed during the etching process of the seed layer 210. Specifically, the width W2 and / or the height of the conductive pattern 232 may be reduced, thereby obtaining a plurality of conductive patterns 232'. The conductive pattern 232' and the seed layer pattern 210a thereunder constitute a conductive structure 234 that may be used as a conductive line or a via. In some embodiments, the conductive pattern 232' has a post-etching line width W2' that is less than the line width W2, the spacing width W1' between the conductive patterns 232' is greater than the spacing width W1, and the pitch P is (W1'+W2'), which is equal to (W1+W2). In other words, the pitch P is constant before and after the etching process of the seed layer 210. In some embodiments, for example, the pitch P is equal to or less than 2 μm. In some embodiments, for example, the pitch P is equal to or less than 1.4 μm. In some embodiments, the line width and the space width may be equal to half of the pitch P, and may be, for example, 0.7 μm. In some embodiments, through double exposure and pitch splitting, the critical dimension of the rewiring conductive pattern can be extended to a sub-micron scale, which exceeds the capabilities of current I-line exposure tools. Therefore, a fine pitch is achieved.

[0045] In some embodiments, the redistribution wiring structure 112 is a multi-layer structure (eg, Figure 1E In this case, FIG. 3A to FIG. 3F The steps shown in the figure may be repeated several times to present the redistribution wiring structure 112. In some embodiments, the redistribution wiring structure 112 includes at least one redistribution pattern 112a having a conductive structure 234, and other redistribution patterns 112a may have other suitable structures.

[0046] Conventionally, due to the high topography and high warpage characteristics of packages such as INFO packages or INFO UHD packages, an exposure tool with I-line and low NA of 0.18 or less is required to obtain a wider DOF, which causes low image contrast and limits spacing resolution. In some embodiments, by using a phase-shift mask, adjusting the constant k1 in the Rayleigh formula, or using double exposure, the image contrast and optical resolution are improved while maintaining a wide DOF with I-line and low NA. Therefore, the lithography performance and process window are significantly improved, and a large DOF and high resolution are obtained. In other words, the optical resolution is improved and exceeds the capabilities of current I-line exposure tools. Therefore, the critical dimensions of the rewiring conductive pattern can be extended to sub-micron scales. In addition, the aforementioned lithography can be applied to other elements that need to be formed using I-line and low NA by an I-line exposure tool.

[0047] According to some embodiments of the present invention, a method for manufacturing a redistribution wiring structure includes the following steps. A seed layer is formed on a tube core and an encapsulation body encapsulating the tube core. A first photoresist material is formed on the seed layer. Using a numerical aperture equal to or less than 0.18, the first photoresist material is exposed to an I-line wavelength in an I-line stepper lithography machine through a phase-shift mask. The first photoresist material is developed to form a first photoresist layer, wherein the first photoresist layer includes a plurality of first photoresist patterns and a plurality of first openings between the plurality of first photoresist patterns. A first conductive material is formed in the plurality of first openings. The first photoresist layer is removed to form a plurality of first conductive patterns. Using the plurality of first conductive patterns as a mask, the seed layer is partially removed to form a plurality of seed layer patterns below the plurality of first conductive patterns, wherein a plurality of redistribution conductive patterns respectively include the plurality of seed layer patterns and the plurality of first conductive patterns.

[0048] In some embodiments, a line width of the plurality of first conductive patterns is equal to or less than 1 μm.

[0049] In some embodiments, a line width of the plurality of first conductive patterns is equal to or less than 0.7 μm.

[0050] In some embodiments, the seed layer is partially removed by an etching process, and the plurality of first conductive patterns are partially removed by the etching process.

[0051] In some embodiments, the method further includes: forming a second photoresist layer over the first conductive material and the first photoresist layer, wherein the second photoresist layer includes at least one second opening; forming a second conductive material in the at least one second opening; removing the second photoresist layer to form at least one second conductive pattern; and forming a dielectric layer, wherein the at least one second conductive pattern is disposed in the dielectric layer.

[0052] In some embodiments, the seed layer is partially removed by an etching process, and the plurality of first conductive patterns and the at least one second conductive pattern are partially removed by the etching process.

[0053] In some embodiments, the first photoresist layer and the second photoresist layer are removed simultaneously.

[0054] In some embodiments, the die includes a conductive pillar thereon, and one of the plurality of seed layer patterns contacts the conductive pillar.

[0055] According to an alternative embodiment of the present invention, a method for manufacturing a redistribution wiring structure includes the following steps. A seed layer is formed on a tube core and an encapsulation body encapsulating the tube core. A first photoresist material is formed on the seed layer. Using the conditions in the Rayleigh formula R=k1(λ / NA), the first photoresist material is exposed to the I-line wavelength in the I-line stepper lithography machine through a mask, where R is the resolution of the pattern, NA is the numerical aperture, λ is the wavelength of the light used for exposure, and k1 is a positive constant equal to or less than 0.49. The first photoresist material is developed to form a first photoresist layer, wherein the first photoresist layer includes a plurality of first photoresist patterns and a plurality of first openings between the plurality of first photoresist patterns. A first conductive material is formed in the plurality of first openings. The first photoresist layer is removed to form a plurality of first conductive patterns. Using the plurality of first conductive patterns as a mask layer, the seed layer is partially removed to form a plurality of seed layer patterns below the plurality of first conductive patterns, wherein the plurality of redistribution conductive patterns respectively include the plurality of seed layer patterns and the plurality of first conductive patterns.

[0056] In some embodiments, k1 is a positive constant equal to or less than 0.35.

[0057] In some embodiments, a line width of the plurality of first conductive patterns is equal to or less than 1 μm.

[0058] In some embodiments, a line width of the plurality of first conductive patterns is equal to or less than 0.7 μm.

[0059] In some embodiments, the seed layer is partially removed by an etching process, and the plurality of first conductive patterns are partially removed by the etching process.

[0060] In some embodiments, after performing the etching process, widths of the plurality of first conductive patterns are reduced, and intervals between the plurality of first conductive patterns are increased.

[0061] In some embodiments, the die includes a conductive pillar thereon, and one of the plurality of seed layer patterns contacts the conductive pillar.

[0062] According to some alternative embodiments of the present invention, a method for manufacturing a redistribution wiring structure includes the following steps. A seed layer is formed on a tube core and an encapsulation body encapsulating the tube core. A photoresist material is formed on the seed layer. A first exposure is performed by using a numerical aperture equal to or less than 0.18, and a first portion of the photoresist material is exposed to an I-line wavelength in an I-line stepper lithography machine through a first mask. A second exposure is performed by using a numerical aperture equal to or less than 0.18, and a second portion of the photoresist material is exposed to the I-line wavelength in the I-line stepper lithography machine through a second mask, wherein the first portion and the second portion are alternately arranged. The photoresist material is developed to form a photoresist layer, wherein the photoresist layer includes a plurality of photoresist patterns and a plurality of openings between the plurality of photoresist patterns. A conductive material is formed in the plurality of openings. The photoresist layer is removed to form a plurality of conductive patterns. The seed layer is partially removed by using the plurality of conductive patterns as a mask to form a plurality of seed layer patterns under the plurality of conductive patterns, wherein the plurality of redistribution conductive patterns respectively include the plurality of seed layer patterns and the plurality of conductive patterns.

[0063] In some embodiments, a line width of the plurality of conductive patterns is equal to or less than 1 μm.

[0064] In some embodiments, a line width of the plurality of conductive patterns is equal to or less than 0.7 μm.

[0065] In some embodiments, the seed layer is partially removed by an etching process, and the plurality of conductive patterns are partially removed by the etching process.

[0066] The features of several embodiments are summarized above so that those skilled in the art can better understand the various aspects of the present invention. Those skilled in the art should understand that they can easily use the present invention as a basis for designing or modifying other processes and structures to implement the same purposes and / or achieve the same advantages as the embodiments described herein. Those skilled in the art should also recognize that these equivalent constructions do not depart from the spirit and scope of the present invention, and they can make various changes, substitutions and modifications to them without departing from the spirit and scope of the present invention.

Claims

1. A method for manufacturing a redistribution wiring structure, the method comprising: forming a seed layer over the die; forming a first photoresist material on the seed layer; exposing the first photoresist material to an I-line wavelength in an I-line stepper through a phase shift mask using a numerical aperture equal to or less than 0.18; developing the first photoresist material to form a first photoresist layer, wherein the first photoresist layer includes a plurality of first photoresist patterns and a plurality of first openings between the plurality of first photoresist patterns; forming a first conductive material in the plurality of first openings; forming a second photoresist layer on the first conductive material, wherein the second photoresist layer comprises at least one second opening; forming a second conductive material in the at least one second opening; removing the first photoresist layer and the second photoresist layer to form a plurality of first conductive patterns and at least one second conductive pattern; locally removing the seed layer using the plurality of first conductive patterns as a mask to form a plurality of seed layer patterns under the plurality of first conductive patterns; as well as A dielectric layer is formed, wherein the at least one second conductive pattern is disposed in the dielectric layer. 2 . The method according to claim 1 , wherein a line width of the plurality of first conductive patterns is equal to or less than 1 μm. 3 . The method according to claim 1 , wherein a line width of the plurality of first conductive patterns is equal to or less than 0.7 μm. 4 . The method according to claim 1 , wherein the seed layer is partially removed by an etching process, and the plurality of first conductive patterns are partially removed by the etching process. 5 . The method according to claim 1 , wherein the seed layer is partially removed by an etching process, and the plurality of first conductive patterns and the at least one second conductive pattern are partially removed by the etching process. The method of claim 1 , wherein the first photoresist layer and the second photoresist layer are removed simultaneously. 7 . The method of claim 1 , wherein the die includes a conductive pillar thereon, and one of the plurality of seed layer patterns contacts the conductive pillar. The method of claim 1 , further comprising forming an encapsulation body encapsulating the die.

9. The method according to claim 1, wherein the plurality of first conductive patterns are located in the dielectric layer.

10. A method for manufacturing a redistribution wiring structure, the method comprising: forming a seed layer over the die; forming a first photoresist material on the seed layer; Using the condition in the Rayleigh formula R=k1(λ / NA), exposing the first photoresist material to an I-line wavelength in an I-line stepper through a mask, where R is the resolution of the pattern, NA is the numerical aperture, λ is the wavelength of light used for exposure, and k1 is a positive constant equal to or less than 0.49; developing the first photoresist material to form a first photoresist layer, wherein the first photoresist layer includes a plurality of first photoresist patterns and a plurality of first openings between the plurality of first photoresist patterns; forming a first conductive material in the plurality of first openings; removing the first photoresist layer to form a plurality of first conductive patterns; as well as The seed layer is partially removed by an etching process using the plurality of first conductive patterns as a mask layer to form a plurality of seed layer patterns under the plurality of first conductive patterns, wherein the etching process simultaneously partially removes the plurality of first conductive patterns. The method according to claim 10 , wherein k1 is a positive constant equal to or less than 0.

35. 12 . The method according to claim 10 , wherein a line width of the plurality of first conductive patterns is equal to or less than 1 μm. 13 . The method according to claim 10 , wherein a line width of the plurality of first conductive patterns is equal to or less than 0.7 μm. 14 . The method of claim 10 , wherein after performing the etching process, widths of the plurality of first conductive patterns are reduced and intervals between the plurality of first conductive patterns are increased. 15 . The method of claim 10 , wherein the die includes a conductive pillar thereon, and one of the plurality of seed layer patterns contacts the conductive pillar. The method of claim 10 , wherein the mask is a phase-shift mask.

17. A method for manufacturing a redistribution wiring structure, the method comprising: forming a seed layer over the die; forming a photoresist material on the seed layer; Performing a first exposure, exposing a first portion of the photoresist material to an I-line wavelength in an I-line stepper lithography machine through a first mask; Performing a second exposure, exposing a second portion of the photoresist material to the I-line wavelength in the I-line stepper lithography machine through a second mask, wherein the first portion and the second portion are alternately arranged; developing the photoresist material to form a photoresist layer, wherein the photoresist layer includes a plurality of photoresist patterns and a plurality of openings between the plurality of photoresist patterns; forming a conductive material in the plurality of openings; removing the photoresist layer to form a plurality of conductive patterns; as well as The seed layer is partially removed by an etching process using the plurality of conductive patterns as a mask to form a plurality of seed layer patterns under the plurality of conductive patterns, wherein the etching process partially removes the plurality of conductive patterns at the same time. The method according to claim 17 , wherein a line width of the plurality of conductive patterns is equal to or less than 1 μm. 19 . The method according to claim 17 , wherein a line width of the plurality of conductive patterns is equal to or less than 0.7 μm.

20. The method of claim 17, wherein exposing the second portion of the photoresist material to an I-line wavelength through a second mask is performed using a numerical aperture equal to or less than 0.

18.

21. A method for manufacturing a redistribution wiring structure, the method comprising: forming a first photoresist material; exposing the first photoresist material through a phase shift mask; developing the first photoresist material to form a first photoresist layer, wherein the first photoresist layer includes a plurality of first photoresist patterns and a plurality of first openings between the plurality of first photoresist patterns; forming a first conductive material in the plurality of first openings; forming a second photoresist layer on the first conductive material, wherein the second photoresist layer comprises at least one second opening; forming a second conductive material in the at least one second opening; removing the first photoresist layer and the second photoresist layer to form a plurality of first conductive patterns and at least one second conductive pattern; as well as A dielectric layer is formed, wherein the at least one second conductive pattern is disposed in the dielectric layer.

22. The method of claim 21, wherein exposing the first photoresist material is performed using an I-line wavelength in an I-line stepper and a numerical aperture equal to or less than 0.

18. 23 . The method according to claim 21 , wherein a line width of the plurality of first conductive patterns is equal to or less than 1 μm. 24 . The method according to claim 21 , wherein a line width of the plurality of first conductive patterns is equal to or less than 0.7 μm.

25. The method of claim 21, further comprising: forming a seed layer, wherein the first photoresist material is formed on the seed layer; as well as The seed layer is partially removed using the plurality of first conductive patterns as a mask to form a plurality of seed layer patterns under the plurality of first conductive patterns. 26 . The method of claim 25 , wherein the seed layer is partially removed by an etching process, and the plurality of first conductive patterns are partially removed by the etching process. 27 . The method according to claim 25 , wherein the seed layer is partially removed by an etching process, and the plurality of first conductive patterns and the at least one second conductive pattern are partially removed by the etching process.

28. The method of claim 21, wherein the first photoresist layer and the second photoresist layer are removed simultaneously.

29. The method according to claim 21, wherein the plurality of first conductive patterns are located in the dielectric layer.

30. A method for manufacturing a redistribution wiring structure, the method comprising: forming a first photoresist material over the seed layer; exposing the first photoresist material through a mask; developing the first photoresist material to form a first photoresist layer, wherein the first photoresist layer includes a plurality of first photoresist patterns and a plurality of first openings between the plurality of first photoresist patterns; forming a first conductive material in the plurality of first openings; removing the first photoresist layer to form a plurality of first conductive patterns; as well as The seed layer is partially removed by an etching process using the plurality of first conductive patterns as a mask layer to form a plurality of seed layer patterns under the plurality of first conductive patterns, wherein the etching process simultaneously partially removes the plurality of first conductive patterns.

31. A method according to claim 30, wherein exposing the first photoresist material is performed by exposing at an I-line wavelength in an I-line stepper lithography machine using the condition in the Rayleigh formula R=k1(λ / NA), where R is the resolution of the pattern, NA is the numerical aperture, λ is the wavelength of the light used for exposure, and k1 is a positive constant equal to or less than 0.

49. 32 . The method according to claim 30 , wherein a line width of the plurality of first conductive patterns is equal to or less than 1 μm. 33 . The method according to claim 30 , wherein a line width of the plurality of first conductive patterns is equal to or less than 0.7 μm. 34 . The method of claim 30 , wherein after performing the etching process, widths of the plurality of first conductive patterns are reduced and intervals between the plurality of first conductive patterns are increased.

35. The method of claim 30, wherein the mask is a phase-shift mask.

36. A method for manufacturing a redistribution wiring structure, the method comprising: forming a seed layer over the die; forming a photoresist material on the seed layer; Performing a first exposure to expose a first portion of the photoresist material through a first mask; Performing a second exposure to expose a second portion of the photoresist material through a second mask, wherein the first portion and the second portion are alternately arranged; developing the photoresist material to form a photoresist layer, wherein the photoresist layer includes a plurality of photoresist patterns and a plurality of openings between the plurality of photoresist patterns; forming a conductive material in the plurality of openings; removing the photoresist layer to form a plurality of conductive patterns; as well as The seed layer is partially removed by an etching process using the plurality of conductive patterns as a mask to form a plurality of seed layer patterns under the plurality of conductive patterns, wherein the etching process partially removes the plurality of conductive patterns at the same time. 37 . The method according to claim 36 , wherein a line width of the plurality of conductive patterns is equal to or less than 1 μm. The method according to claim 36 , wherein a line width of the plurality of conductive patterns is equal to or less than 0.7 μm.