SiC film single body structure
By using a negative mold base material with opposite concavities and convexities in the SiC film monomer structure for vapor deposition, a high-precision functional surface is formed, and a stacked SiC layer is formed through lamination, which solves the problem of the SiC film monomer structure in the existing technology. The problem of inconsistent shape and insufficient strength of the body when the base material is uneven is achieved, and high-precision consistency and strength improvement of the functional surface and the shape of the base material are achieved.
Patent Information
- Application Number
- CN201980002150.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-02-28
- Filing Date
- 2019-08-28
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2039-08-28
AI Technical Summary
When the base material of the existing SiC film monomer structure has unevenness, the functional surface is inconsistent with the shape of the base material, resulting in uneven film thickness distribution, affecting product accuracy and strength. Especially in narrow areas, there is a problem of thickening of the film thickness, making it difficult to Improves strength by increasing film thickness.
A negative mold substrate with opposite concavities and convexities is used for vapor deposition to form the SiC layer on the functional surface to ensure that the functional surface is consistent with the shape of the substrate with high precision, and the strength is improved by increasing the film thickness. The CVD method is used to form the SiC layer in the pores on the surface of the substrate. A SiC layer is formed, stacked to form a stacked SiC layer, and unnecessary parts of the base material are removed to form a high-precision SiC film single-piece structure.
It achieves high-precision consistency between the functional surface of the SiC film monomer structure and the shape of the substrate, and increases the strength of the structure by increasing the film thickness, ensuring the high quality and precision of the product, and is suitable for complex shapes and fine structures.
Smart Images

Figure CN111868885B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to SiC film forming technology, and in particular to a structure composed of a SiC film monomer. Background Art
[0002] Due to its good environmental resistance and high chemical stability, there is an increasing demand for film monomer structures made of SiC, especially in the field of semiconductor device manufacturing, as fixtures such as wafer boats, tubes and dummy wafers used at ultra-high temperatures when manufacturing semiconductors.
[0003] In the past, this SiC film monomer structure was formed by the film forming process and substrate removal process disclosed in Patent Document 1. The details are as follows. First, in the film forming process, a SiC film is formed on the surface of a substrate composed of carbon (graphite) or the like by a CVD (Chemical Vapor Deposition) method, and its thickness is controlled by the film forming time, the number of film layering, etc.
[0004] Next, in the substrate removal step, the substrate is burned off by heating the film-formed blank in a high-temperature oxidizing atmosphere. By performing such treatment, a SiC film single body structure having a shape consistent with the outer shape of the substrate is produced.
[0005] Prior art literature
[0006] Patent Literature
[0007] Patent Document 1: Japanese Patent Application Publication No. 2001-158666 Summary of the invention
[0008] Technical problem to be solved by the invention
[0009] In the SiC film monomer structure formed in the above manner, the functional surface is a vapor deposition surface formed by the CVD method. The thickness of the vapor-deposited film will also vary depending on the location of the substrate and the position of the substrate. Therefore, in the case where the substrate has bumps and depressions, it is particularly necessary to predict the adhesion of the film during vapor deposition, that is, the state of the film of the SiC film monomer structure after completion, to determine the shape of the substrate, and there will be a deviation between the desired shape and the finished shape. In addition, when using a substrate with a complex surface shape, the film thickness tends to become thinner in narrow parts and deep parts. This difference in product precision and film thickness distribution often has a greater impact on its function depending on the product's use.
[0010] Furthermore, there is a risk that a desired gap cannot be obtained in a narrow portion due to an increase in the film thickness, and there is also a problem that it is difficult to improve the strength by increasing the film thickness.
[0011] Therefore, an object of the present invention is to solve the above-mentioned problems and to provide a SiC film single body structure in which the shape of the functional surface of the SiC film single body structure can be matched with the shape of the substrate with high accuracy and the strength can be improved by increasing the film thickness.
[0012] Means for solving technical problems
[0013] The SiC film monomer structure of the present invention for achieving the above-mentioned purpose is a film monomer structure formed by laminating a SiC layer on the concave-convex surface of a substrate having concave-convex shapes by a vapor deposition type film forming method, and is characterized in that a negative mold substrate having concave-convex shapes opposite to the shape of a desired structure is used for the substrate, and the SiC layer constitutes a functional surface on the contact surface in contact with the negative mold substrate in the first SiC layer formed by contacting the concave-convex surface of the negative mold substrate.
[0014] In addition, in the SiC film single structure having the above characteristics, the smoothness of the functional surface and the non-functional surface on both the front and back sides of any specific part is higher than the smoothness of the non-functional surface. By having such characteristics, after the SiC film single structure is formed, surface treatment such as grinding is not required. Therefore, even for complex and fine structures, high-quality products can be provided.
[0015] Furthermore, in the SiC film single body structure having the above characteristics, when the formed surface has a corner, the ridgeline of the corner of the functional surface is sharper than that of the non-functional surface. With such characteristics, the accuracy required for a mold or the like can be reliably obtained.
[0016] Effects of the Invention
[0017] According to the SiC film single body structure having the above characteristics, the functional surface of the SiC film single body structure is not affected by the film thickness. In addition, since the functional surface is not affected by the film thickness, the strength can be improved by increasing the film thickness. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a diagram showing the structure of a SiC film single body structure according to an embodiment.
[0019] Figure 2 It is a diagram for explaining the manufacturing process of the SiC film single body structure according to the embodiment.
[0020] Figure 3 It is a diagram showing a modification example in the configuration of the SiC film single body structure. DETAILED DESCRIPTION
[0021] Hereinafter, the embodiment of the SiC film monomer structure of the present invention will be described in detail with reference to the accompanying drawings. Note that the embodiment shown below is a part of the preferred mode for implementing the present invention, and even if a part of the structure is changed within the scope of the invention, it can be regarded as a part of the present invention.
[0022] [structure]
[0023] In the present embodiment, the SiC film single body structure 10 is configured by providing the SiC film with strength sufficient to be independent. Figure 1 The form shown is a wafer boat as a jig for manufacturing semiconductor wafers, but this is to show that the SiC film single structure 10 of the embodiment can be applied not only to a planar structure but also to a form having projections and depressions, and the form and application are not limited.
[0024] Figure 1 The SiC film single body structure 10 shown in the figure has one main surface having a function as a wafer boat, that is, a slit 16 for supporting the wafer 50, as a functional surface 12. Figure 1 As shown in the partially enlarged schematic diagram surrounded by a circle in FIG, a plurality of micro protrusions 12b that are difficult to obtain by mechanical processing are provided on the functional surface 12 of the SiC film monomer structure 10 of the embodiment. By providing such micro protrusions 12b on the functional surface 12, the contact area between the supporting material (e.g., the wafer 50) and the SiC film monomer structure 10 can be reduced. Therefore, when the heating or cooling process is performed, the wafer 50 will not stick to the SiC film monomer structure 10. In addition, the temperature difference between the portion exposed to the gas environment and the contact portion can be suppressed.
[0025] Regarding the corners 12a and 14a, the corner 12a of the functional surface 12 has a very sharp ridgeline, whereas the corresponding portion (corner 14a) of the non-functional surface 14 has a gentler ridgeline than the corresponding portion of the functional surface 12 .
[0026] This is because, as described in detail later, the functional surface 12 of the SiC film single structure 10 and the substrate 30 (see Figure 2 ) contact structure, a shape consistent with its bare surface shape is obtained. Therefore, the shape of the functional surface 12 can be made consistent with the shape of the substrate 30 with high precision.
[0027] [Manufacturing process]
[0028] Reference Figure 3 The manufacturing process of the SiC film single body structure 10 of this structure of this embodiment is described. First, Figure 2As shown in (A), a substrate 30 having a concavoconvex shape opposite to the shape of the desired structure, i.e., a negative mold substrate 30, is prepared. The substrate 30 can be prepared using a porous member having micropores formed on the surface, such as graphite, as a constituent material. Note that a mask 32 is applied to the lower end side of the substrate 30 so that it can be set on the reference surface.
[0029] Then, if Figure 2 As shown in (B), the first SiC layer 20 is formed on the surface of the substrate 30 by a vapor deposition type film forming method. Note that the so-called vapor deposition type film forming method may be, for example, a film forming method based on a CVD method. Here, there are countless pores on the surface of the graphite constituting the substrate 30. The first SiC layer 20 formed by the CVD method is also formed in the pores existing on the surface of the substrate 30. The first SiC layer 20 formed in the pores thus constitutes a micro-protrusion 12b provided on the functional surface 12.
[0030] After the first SiC layer 20 is formed, Figure 2 As shown in (C), the stacking is performed based on the first SiC layer 20, and the stacked SiC layer 22 is formed. Here, there is no need to set a structural difference between the first SiC layer 20 and the stacked SiC layer 22 stacked thereon, but the first SiC layer 20 is formed on the surface of the substrate 30. Therefore, the first SiC layer 20 obtains a highly accurate shape of the properties and shape of the bare surface of the substrate 30.
[0031] After the stacked SiC layer 22 has reached a thickness sufficient to obtain a desired strength, Figure 2 As shown in (D), the substrate 30 on which the SiC layer (the first SiC layer 20 and the stacked SiC layer 22) is formed is removed from the reference surface, and the unnecessary portion ( Figure 2 (D) The part above the dotted line is cut off and removed. Figure 2 As shown in (E), after removing unnecessary parts, the substrate 30 is removed. When graphite is used as the substrate 30, the substrate 30 can be removed by placing the entire substrate 30 with the SiC layer formed thereon in a high-temperature oxidizing environment and heating it.
[0032] The graphite heated in the high temperature oxidizing environment is converted into gas as CO 2 and burns off. Therefore, even a complex shape or a fine shape that is difficult to remove by machining can be removed from the base material 30 .
[0033] By removing the substrate 30 in the above manner, as Figure 2 As shown in (F), a SiC film single body structure 10 is formed.
[0034] [Effect]
[0035] Thus, the SiC film single structure 10 of the embodiment is formed by sequentially stacking the stacked SiC layers 22 based on the first SiC layer 20 constituting the functional surface 12. Therefore, the shapes of the functional surface 12 of the SiC film single structure 10 and the substrate 30 are highly accurately matched. In addition, since the shape accuracy is not affected by the film thickness, the SiC film single structure 10 can also seek to improve the strength by increasing the film thickness.
[0036] [Modifications]
[0037] As described above, in the SiC film single structure 10 of the present embodiment, the functional surface 12 is not affected by the film thickness. Figure 3 As shown, even if the thickness of the SiC film is increased and the width of the groove formed on the non-functional surface 14 is narrowed, the functional surface 12 can maintain the desired accuracy. Therefore, it is possible to provide a SiC film single structure 10 that has high operating accuracy even when a heavy object is placed or held.
[0038] In addition, when a metal with a smooth bare surface is used as the substrate 30, a surface treatment (such as sandblasting) is performed to make the surface have micro-concavities and convexities, thereby forming a functional surface 12 with micro-protrusions similar to the above-mentioned embodiment. Note that when a metal is used as the substrate 30, the substrate 30 can be removed by dissolving the substrate 30 with a chemical solution.
[0039] Industrial Applicability
[0040] In the above-mentioned embodiment, the CVD method is cited as a vapor deposition type film forming method for explanation. Compared with the vacuum evaporation type PVD (Physical Vapor Deposition) method and the MBE (Molecular Beam Epitaxy) method, the vapor deposition based on the CVD method can achieve uniform film thickness. Therefore, as a method for manufacturing a conventional SiC film monomer structure using the final stacked surface to constitute a functional surface, it was once an effective means. However, the SiC film monomer structure 10 of the embodiment is formed by stacking a stacked SiC layer 22 based on the first SiC layer 20 constituting the functional surface 12. Therefore, even if a film forming technology based on a vacuum evaporation type film forming method such as the PVD method or the MBE method is applied, a high-precision product can be manufactured.
[0041] In the above embodiment, a wafer boat is described as an example of the SiC film single structure 10. However, the SiC film single structure 10 can be used in various applications such as a wafer holder and a susceptor.
[0042] Description of Reference Numerals
[0043] 10…………SiC film single body structure
[0044] 12………Functional aspects
[0045] 12a...corner
[0046] 12b…………Small protrusions
[0047] 14………Non-functional surface
[0048] 14a………corner
[0049] 16... Slit
[0050] 20………First SiC layer
[0051] 22……Laminated SiC layer
[0052] 30………Base material
[0053] 32.....Shield
[0054] 50...Chip
Claims
1. A SiC film monomer structure, which is a film monomer structure formed by laminating a SiC layer on a concave-convex surface of a substrate having concave-convex surfaces by a vapor deposition type film forming method, characterized in that: A negative mold substrate having a concave-convex shape opposite to the shape of the desired structure is used for the substrate. The SiC layer forms a functional surface on a contact surface with the negative mold base material in the first SiC layer formed in contact with the concavo-convex surface of the negative mold base material, The functional surface has protrusions formed due to the porous material characteristics of the substrate.
2. The SiC film monomer structure according to claim 1, characterized in that: A SiC layer constituting a non-functional surface is stacked on the side of the first SiC layer opposite to the functional surface.
3. The SiC film monomer structure according to claim 2, characterized in that: When the formation surface has a corner, the ridge line of the corner of the functional surface is sharper than that of the non-functional surface.