A special-shaped PBN and quartz combined crucible
By designing a combination crucible of irregularly shaped PBN and quartz, the problem of uneven heat flow caused by the difference in thermal conductivity between PBN and quartz crucibles was solved, achieving a flat growth interface for semiconductor materials and improved thermal stress distribution, resulting in large-size crystals with low dislocation density.
Patent Information
- Application Number
- CN202011048268.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-29
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2040-09-29
AI Technical Summary
Existing PBN crucibles and quartz crucibles suffer from uneven heat flow due to differences in thermal conductivity during semiconductor material growth, resulting in uneven growth interfaces, easy formation of fine twins, and thermal stress concentration, which affects the uniformity and integrity of the crystal.
By using a combination of irregularly shaped PBN and quartz crucibles, a vacuum zone and a specific heat exchange path are formed through the combination of the quartz crucible and the PBN crucible, a suitable temperature gradient is created, radial heat exchange is reduced, and thermal stress distribution is improved.
This method achieves a flat growth interface for semiconductor materials, reduces the probability of fine twins and polycrystalline formation, improves the uniformity and integrity of crystals, and yields large-size crystals with low dislocation density.
Smart Images

Figure CN112195506B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of semiconductor material production, in particular to a special-shaped PBN and quartz combined crucible. Background Art
[0002] Vertical temperature gradient solidification (VGF) and vertical Bridgman method (VB) are the main production methods for compound semiconductor gallium arsenide (GaAs) and indium phosphide (InP) materials on the market. After a long period of development, PBN crucibles and quartz crucibles are used in the current production process. The thermal conductivity of PBN crucible along the crucible wall is 62.8W / (m·K). -1 , the high thermal conductivity causes the gap between the PBN crucible and the quartz crucible to have a great influence on the heat conduction of the temperature field.
[0003] When the PBN crucible and the quartz crucible are similar in shape and fit closely together, a large amount of heat flow is conducted away through the PBN crucible wall and the quartz crucible, generating a large radial heat flow, thereby resulting in a more concave growth interface shape of the semiconductor material. The concave growth interface of semiconductor materials is prone to produce small twins at the edge, which is not conducive to the growth of large-sized crystals. In addition, the substrate impurity concentration obtained from the crystals on the same horizontal plane is distributed in concentric circles with poor uniformity, and the inflection point from the PBN crucible and the quartz crucible seed crystal cavity to the tapered part produces large thermal stress, the crystal rod and the processed substrate are prone to cracking and fragmentation, and the concentration of thermal stress is prone to produce polycrystalline with high dislocation density. When the two are completely separated, the latent heat of phase change becomes the main factor affecting the shape of the growth interface, and the growth interface also presents a concave melt shape, but the PBN crucible is completely separated from the quartz crucible, and the overall thermal stress is relatively uniform. When the PBN crucible and the quartz crucible seed crystal cavity are closely fitted, and the cone angle and equal diameter positions are separated, the growth interface tends to be flat, which is conducive to obtaining large-sized crystals with low dislocation density and high uniformity, but the stress concentration problem in the seed crystal cavity and the cone angle position is still difficult to solve.
[0004] However, in the current industrial mass production of GaAs and InP materials on the market, the gap between the PBN crucible and the quartz crucible has not been taken seriously. The shapes of the two are basically similar, and the gap between them cannot be well controlled. Summary of the invention
[0005] In view of this, the purpose of the present invention is to provide a special-shaped PBN and quartz combination crucible. Through the combination of the special-shaped quartz crucible and the PBN crucible, during the growth process of compound semiconductor crystals, a vacuum zone is formed around the initial seed crystal melting start to the end of crystal growth, which can enable the semiconductor material to obtain a flat growth interface and effectively improve the crystal thermal stress concentration phenomenon, thereby obtaining large-sized, low-dislocation-density, and well-uniform crystals.
[0006] The present invention solves the above technical problems by the following technical means:
[0007] A special-shaped PBN and quartz combined crucible comprises a quartz crucible, a PBN crucible and a quartz cap, wherein the quartz crucible comprises a coating cavity and a quartz crucible seed crystal cavity, the PBN crucible comprises a raw material cavity and a PBN crucible seed crystal cavity, the PBN crucible and the quartz cap are both arranged in the inner cavity of the quartz crucible, the quartz cap is arranged at an end close to an opening of the quartz crucible, and the opening of the quartz cap faces the PBN crucible; the quartz crucible seed crystal cavity comprises a first seed crystal cavity segment and a second seed crystal cavity segment, the second seed crystal cavity segment is tightly fitted with the outer wall of the PBN crucible seed crystal cavity, and a spacing area is arranged between the first seed crystal cavity segment and the coating cavity of the quartz crucible and the PBN crucible.
[0008] The inner wall of the second seed crystal cavity section of the present invention is tightly fitted with the outer wall of the PBN crucible seed crystal cavity, which can timely guide away the latent heat of phase change in the crystal growth process and shape a suitable temperature gradient. The melting depth is within the relative position of the PBN crucible seed crystal cavity and the first seed crystal cavity section of the quartz crucible. A spacing zone is provided between the first seed crystal cavity section and the coating cavity of the quartz crucible and the PBN crucible. After vacuuming, the quartz crucible and the PBN crucible at the spacing zone are in a vacuum state, ensuring that the radial heat exchange from the initial growth interface to the end of growth during the seed crystal welding process is mainly heat radiation, with less heat exchange and low heat conduction efficiency; the heat is mainly formed in the axial direction as a heat exchange system dominated by melt→growth interface→crystal→seed crystal→low-temperature zone at the bottom of the single crystal furnace, ensuring that the growth interface is flat during the growth process and the overall thermal stress is average, and semiconductor material crystals with large size, low dislocation density, good uniformity and average thermal stress can be obtained.
[0009] Furthermore, a first step is provided on the inner wall of the quartz crucible, and a second step is provided on the inner wall of the PBN crucible, and the outer wall of the second step is closely fitted with the inner wall of the first step. The first step and the second step are closely fitted, firstly, the PBN crucible can be placed on the inner wall of the quartz crucible, so that the quartz crucible can bear the weight of the PBN crucible, and secondly, the inner wall of the quartz crucible and the outer wall of the PBN crucible can form an annular sealing belt, so that the outer wall of the raw material chamber of the PBN crucible and the interior of the quartz crucible form a spacing area.
[0010] Further, the quartz crucible's covering cavity includes a first quartz crucible segment and a second quartz crucible segment, the first quartz crucible segment, the second quartz crucible segment, the first seed crystal cavity segment and the second seed crystal cavity segment are sequentially connected and their diameters are sequentially reduced, and the first step is arranged at the connection between the first quartz crucible segment and the second quartz crucible segment; the PBN crucible also includes a first PBN crucible segment, the first PBN crucible segment, the raw material cavity and the PBN crucible seed crystal cavity are sequentially connected and their diameters are sequentially reduced, and the second step is arranged at the connection between the first PBN crucible segment and the raw material cavity. Such a shape is similar to the shape of the existing PBN crucible and quartz crucible, which is conducive to the growth of crystals.
[0011] Furthermore, a quartz crucible conical section is provided between the second quartz crucible section and the first seed crystal chamber section, and a PBN crucible seed conical section is provided between the raw material chamber and the PBN crucible seed crystal chamber. Such a shape is similar to the shape of the existing PBN crucible and quartz crucible, which is conducive to the growth of crystals.
[0012] Furthermore, the height of the first PBN crucible section is smaller than the height of the first quartz crucible section, so that space can be left in the quartz crucible for placing the quartz cap.
[0013] Furthermore, the outer diameter of the quartz cap is larger than the inner diameter of the PBN crucible, so that the quartz cap can be prevented from damaging the PBN crucible during the vacuuming process.
[0014] Furthermore, the PBN crucible is movably arranged in the quartz crucible, so that the PBN crucible can be disassembled from the quartz crucible for easy cleaning and recycling.
[0015] Beneficial effects of the present invention:
[0016] The inner wall of the second seed crystal cavity section of the present invention is tightly fitted with the outer wall of the PBN crucible seed crystal cavity, which can timely guide away the latent heat of phase change in the crystal growth process and shape a suitable temperature gradient. The melting depth is within the relative position of the PBN crucible seed crystal cavity and the first seed crystal cavity section of the quartz crucible. A spacing zone is provided between the first seed crystal cavity section and the coating cavity of the quartz crucible and the PBN crucible. After vacuuming, the quartz crucible and the PBN crucible at the spacing zone are in a vacuum state, ensuring that the radial heat exchange from the initial growth interface to the end of growth during the seed crystal welding process is mainly heat radiation, with less heat exchange and low heat conduction efficiency. Compared with the prior art, the present invention can effectively improve the degree of depression of the growth interface during the crystal growth process, obtain a relatively flat growth interface, reduce the probability of generating fine twins at the edge of the crystal and polycrystals at the inflection point of the seed crystal and the crystal cone, improve the crystallization rate and crystal uniformity, and at the same time improve the thermal stress distribution state of the crystal, reduce the probability of generating chipping, fragments, etc. during substrate processing, and obtain large-sized crystals with low dislocation density. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a structural schematic diagram of a special-shaped PBN and quartz combined crucible of the present invention.
[0018] Among them, the quartz crucible 1, the PBN crucible 2, the quartz cap 3, the first quartz crucible segment 101, the second quartz crucible segment 102, the quartz crucible conical segment 103, the first seed crystal cavity segment 104, the second seed crystal cavity segment 105, the first PBN crucible segment 201, the raw material cavity 202, the PBN crucible seed conical segment 203, the PBN crucible seed crystal cavity 204, the sealing ring 4, and the spacer 5. DETAILED DESCRIPTION
[0019] The present invention will be described in detail below with reference to the accompanying drawings:
[0020] like Figure 1 As shown:
[0021] A special-shaped PBN and quartz combined PBN crucible comprises a quartz crucible 1, a PBN crucible 2 and a quartz cap 3, wherein the PBN crucible 2 and the quartz cap 3 are both movably placed in the inner cavity of the quartz crucible 1; the quartz crucible 1 comprises, from top to bottom, a first quartz crucible segment 101, a second quartz crucible segment 102, a quartz crucible tapered segment 103, a first seed crystal cavity segment 104 and a second seed crystal cavity segment 105 which are integrally formed in sequence, and the diameters of the first quartz crucible segment 101, the second quartz crucible segment 102, the first seed crystal cavity segment 104 and the second seed crystal cavity segment 105 are successively reduced; the PBN crucible 2 comprises, from top to bottom, a first PBN crucible segment 201, a raw material cavity 202, a PBN crucible seed tapered segment 203 and a PBN crucible seed crystal cavity 204 which are integrally formed in sequence, and the diameters of the first PBN crucible segment 201, the raw material cavity 202 and the PBN crucible seed crystal cavity 204 are successively reduced.
[0022] A first step is formed at the connection between the first quartz crucible segment 101 and the second quartz crucible segment 102 of the quartz crucible 1, and a second step is formed at the connection between the first PBN crucible segment 201 and the raw material chamber 202 of the PBN crucible 2. The outer wall of the second step fits tightly with the inner wall of the first step to form a sealing ring 4. The quartz cap 3 is arranged at one end close to the opening of the quartz crucible 1, and the opening of the quartz cap 3 faces downward, and the outer diameter of the quartz cap 3 is larger than the inner diameter of the PBN crucible 2.
[0023] The inner wall of the second seed crystal cavity section 105 of the quartz crucible 1 is tightly fitted with the outer wall of the PBN crucible seed crystal cavity 204 , and a spacing area 5 is provided between the first seed crystal cavity section 104 of the quartz crucible 1 , the quartz crucible conical section 103 , the second quartz crucible section 102 and the outer wall of the PBN crucible 2 .
[0024] The method of use of the present invention is as follows:
[0025] When in use, first clean the quartz crucible 1, quartz cap 3, PBN crucible 2, raw materials and seed crystals, then place the quartz crucible 1 horizontally, and put the PBN crucible 2 into the quartz crucible 1. Note that when placing the PBN crucible 2, the quartz crucible 1 is in a horizontal state and the quartz crucible 1 and the PBN crucible 2 are combined first to avoid damage to the PBN crucible 2 due to combination after loading.
[0026] Then, the seed crystal is loaded into the PBN crucible seed crystal cavity 204 of the PBN crucible 2, the raw material is loaded into the raw material cavity 202 of the PBN crucible 2, and the quartz cap 3 is loaded into the quartz crucible 1. After vacuuming, the quartz crucible 1 and the quartz cap 3 are welded and sealed with an oxyhydrogen flame. The PBN crucible 2, which is a combination of the quartz crucible 1 and the PBN crucible 2, is then placed in a single crystal furnace, and the heating element of the single crystal furnace is controlled to heat up to completely melt the raw material. After the temperature stabilizes, the seed crystal is started to be welded, and the melting depth is between the second seed crystal cavity section 105. The inner wall of the second seed crystal cavity section 105 of the present invention is closely fitted with the outer wall of the PBN crucible seed crystal cavity 204, which can timely guide away the latent heat of phase change during the crystal growth process, shape a suitable temperature gradient, and the melting depth is within the relative position of the PBN crucible seed crystal cavity 204 and the first seed crystal cavity section 104 of the quartz crucible 1. A spacing area 5 is provided between the first seed crystal cavity section 104 of the quartz crucible 1, the conical section 103 of the quartz crucible, the second quartz crucible section 102 and the PBN crucible 2. After vacuuming, the spacing area 5 is located at the position of the There is a vacuum state between the quartz crucible 1 and the PBN crucible 2, ensuring that the radial heat exchange from the initial growth interface to the end of growth during the seed crystal welding process is mainly heat radiation, with less heat exchange and low heat conduction efficiency; the heat is mainly formed in the axial direction with the melt → growth interface → crystal → seed crystal → low temperature zone at the bottom of the single crystal furnace as the dominant heat exchange system, ensuring that the growth interface is flat during the growth process and the overall thermal stress is average, so that semiconductor material crystals with large size, high low dislocation density, good uniformity and average thermal stress can be obtained.
[0027] Finally, after a period of constant temperature, single crystal growth begins, and after growth is completed, the temperature is lowered and the furnace is taken out of the furnace.
[0028] The above embodiments are only used to illustrate the technical solutions of the present invention and are not intended to limit the present invention. Although the present invention is described in detail with reference to the preferred embodiments, it should be understood by those skilled in the art that the technical solutions of the present invention may be modified or replaced by equivalents without departing from the purpose and scope of the technical solutions of the present invention, which should be included in the scope of the claims of the present invention. The techniques, shapes, and structural parts not described in detail in the present invention are all known technologies.
Claims
1. A special-shaped PBN and quartz combination crucible, comprising a quartz crucible, a PBN crucible and a quartz cap, wherein the quartz crucible comprises a coating cavity and a quartz crucible seed cavity, and the PBN crucible comprises a raw material cavity and a PBN crucible seed cavity. Features: The PBN crucible and the quartz cap are both arranged in the inner cavity of the quartz crucible, the quartz cap is arranged at an end close to the opening of the quartz crucible, and the opening of the quartz cap faces the PBN crucible; the seed crystal cavity of the quartz crucible includes a first seed crystal cavity section and a second seed crystal cavity section, the second seed crystal cavity section is tightly fitted with the outer wall of the seed crystal cavity of the PBN crucible, and a spacing area is arranged between the first seed crystal cavity section and the coating cavity of the quartz crucible and the PBN crucible; a first step is arranged on the inner wall of the quartz crucible, and a second step is arranged on the inner wall of the PBN crucible, and the outer wall of the second step is in contact with the first seed crystal cavity section and the coating cavity of the quartz crucible. The inner wall of a step is tightly fitted; the coating cavity of the quartz crucible includes a first quartz crucible segment and a second quartz crucible segment, the first quartz crucible segment, the second quartz crucible segment, the first seed crystal cavity segment and the second seed crystal cavity segment are connected in sequence and their diameters are reduced in sequence, and the first step is arranged at the connection between the first quartz crucible segment and the second quartz crucible segment; the PBN crucible also includes a first PBN crucible segment, the first PBN crucible segment, the raw material cavity and the PBN crucible seed crystal cavity are connected in sequence and their diameters are reduced in sequence, and the second step is arranged at the connection between the first PBN crucible segment and the raw material cavity.
2. A special-shaped PBN and quartz combination crucible according to claim 1, Features: A quartz crucible tapered section is provided between the second quartz crucible section and the first seed crystal chamber section, and a PBN crucible tapered section is provided between the raw material chamber and the PBN crucible seed crystal chamber.
3. A special-shaped PBN and quartz combination crucible according to claim 2, Features: The height of the first PBN crucible segment is smaller than the height of the first quartz crucible segment.
4. A special-shaped PBN and quartz combination crucible according to claim 3, Features: The outer diameter of the quartz cap is greater than the inner diameter of the PBN crucible.
5. A special-shaped PBN and quartz combination crucible according to claim 4, Features: The PBN crucible is movably arranged in the quartz crucible.