Device and method for manufacturing thin film packaging

By using sputtering, monomer deposition and chemical vapor deposition processes in thin film packaging manufacturing equipment, combined with multiple process chambers and rotation modules, uniform control of the thickness of organic and inorganic layers is achieved, solving the problem of thickness adjustment in the existing technology Difficult problem to improve the life and production efficiency of display devices.

CN112331591BActive Publication Date: 2024-10-15SAMSUNG DISPLAY CO LTD
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202011260899.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2012-12-24
Filing Date
2013-10-10
Publication Date
2024-10-15
Estimated Expiration
2033-10-10

AI Technical Summary

Technical Problem

It is difficult to effectively adjust and uniformly control the thickness of the organic layer and the inorganic layer in the thin film packaging equipment with the existing technology, which affects the service life and production efficiency of the display device.

Method used

A thin film packaging manufacturing equipment is designed to form multi-layer films through sputtering, monomer deposition and chemical vapor deposition processes. Multiple process chambers and rotating modules are used to achieve upward and downward deposition of layers to ensure uniform thickness of each layer. stability and vacuum pressure control.

Benefits of technology

It achieves precise adjustment and uniform deposition of the thickness of the organic and inorganic layers, improves the service life and production efficiency of the display device, and enhances the stability and efficiency of the thin film packaging process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112331591B_ABST
    Figure CN112331591B_ABST
Patent Text Reader

Abstract

An apparatus and method for manufacturing thin film encapsulation include: a first cluster, configured to form a first inorganic layer on a display substrate using a sputtering process; a second cluster, configured to form a first organic layer on the first inorganic layer on the display substrate using a monomer deposition process; and a third cluster, configured to form a second inorganic layer on the first organic layer on the display substrate using a chemical vapor deposition (CVD) process or a plasma enhanced chemical vapor deposition (process).
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims priority to and the benefit of Korean Patent Application No. 10-2012-0152501, filed on Dec. 24, 2012, in the Korean Intellectual Property Office, the disclosure of which is incorporated herein by reference in its entirety. Technical Field

[0003] The present invention relates to an apparatus and a method for manufacturing a thin film package. Background Art

[0004] Recently, portable electronic devices are widely used. In addition to compact electronic devices such as mobile phones, tablet personal computers (PCs) are recently widely used as mobile electronic devices.

[0005] In order to support various functions, mobile electronic devices include display devices to provide visual information such as images to users. As components driving display devices become more compact, the size of display devices in electronic devices is gradually increasing relative to the overall size of the electronic devices, and display devices that can be bent at an angle (e.g., a predetermined angle) from a flat state are also being developed.

[0006] When the flexible display device as described above is formed, a multi-layer thin film can be used to encapsulate the light-emitting unit of the flexible display device to improve the service life of the display device. For encapsulation, an encapsulation film can be formed, and the encapsulation film can be formed by alternately stacking an organic layer and an inorganic layer. The organic layer and the inorganic layer of the encapsulation film can be formed using a variety of methods. Summary of the invention

[0007] Embodiments of the present invention provide an apparatus and method for manufacturing a thin film package, in which the thickness of an organic layer and an inorganic layer can be adjusted, and the vacuum pressure of various thin film deposition apparatuses can be uniformly maintained.

[0008] According to one aspect of the present invention, a thin film encapsulation manufacturing device is provided, including: a first cluster, configured to form a first inorganic layer on a display substrate using a sputtering process; a second cluster, configured to form a first organic layer on the first inorganic layer on the display substrate using a monomer deposition process; and a third cluster, configured to form a second inorganic layer on the first organic layer on the display substrate using a chemical vapor deposition (CVD) process or a plasma enhanced chemical vapor deposition (PECVD) process.

[0009] The first cluster, the second cluster, and the third cluster each include a plurality of process chambers.

[0010] The order of the plurality of process chambers of the first cluster, the plurality of process chambers of the second cluster, and the plurality of process chambers of the third cluster may be arranged along one direction, and the first inorganic layer, the first organic layer, and the second inorganic layer may be respectively formed in the corresponding process chambers in the same order.

[0011] At least one of the first cluster, the second cluster, and the third cluster may include a mask storage chamber.

[0012] The thin film encapsulation manufacturing apparatus may further include: a fourth cluster coupled to the third cluster and configured to form a second organic layer on the second inorganic layer delivered from the third cluster by using a monomer deposition process.

[0013] The thin film encapsulation manufacturing apparatus may further include: a fifth cluster coupled to the fourth cluster and configured to form a third inorganic layer on the second organic layer delivered from the fourth cluster by using a CVD method or a PECVD method.

[0014] The second cluster and the third cluster may be installed alternately.

[0015] The first cluster and the second cluster may form a first inorganic layer and a first organic layer, respectively, using a downward deposition method, and the third cluster may form a second inorganic layer using an upward deposition method.

[0016] The thin film encapsulation manufacturing apparatus may further include at least one of the following chambers: a channel chamber located between the first cluster and the second cluster and configured to transport the display substrate, and a rotation module chamber coupled to the second cluster and configured to align an input direction of the display substrate.

[0017] The thin film encapsulation manufacturing equipment may also include: a first plurality of channel chambers located between the first cluster and the second cluster and configured to convey the display substrate; and a first rotation module chamber configured to align the input direction of the display substrate, wherein the first plurality of channel chambers are coupled to opposite sides of the first rotation module chamber to couple the first cluster to the second cluster.

[0018] When the display substrate is transported, the internal pressures of the first cluster and one of the multiple channel chambers can be controlled to be substantially the same, the internal pressures of one of the multiple channel chambers and the rotation module chamber can be controlled to be substantially the same, the internal pressures of the rotation module chamber and another channel chamber among the multiple channel chambers can be controlled to be substantially the same, or the internal pressures of another channel chamber among the multiple channel chambers and the second cluster can be controlled to be substantially the same.

[0019] The thin film encapsulation manufacturing apparatus may further include at least one of the following chambers: a channel chamber located between the second cluster and the third cluster and configured to transport the display substrate, and a rotation module chamber coupled to the second cluster and configured to align an input direction of the display substrate.

[0020] The thin film encapsulation manufacturing equipment may also include: a second plurality of channel chambers located between the second cluster and the third cluster and configured to convey the display substrate; and a second rotation module chamber, configured to align the input direction of the display substrate, wherein the second plurality of channel chambers are coupled to opposite sides of the second rotation module chamber to couple the second cluster to the third cluster.

[0021] When the display substrate is transported, the internal pressures of the second cluster and one of the multiple channel chambers can be controlled to be substantially the same, the internal pressures of one of the multiple channel chambers and the rotation module chamber can be controlled to be substantially the same, the internal pressures of the rotation module chamber and another channel chamber among the multiple channel chambers can be controlled to be substantially the same, or the internal pressures of another channel chamber among the multiple channel chambers and the third cluster can be controlled to be substantially the same.

[0022] The thin film encapsulation manufacturing apparatus may further include: a loading cluster configured to receive the display substrate from the outside and transfer the display substrate to the first cluster.

[0023] The thin film encapsulation manufacturing apparatus may further include: an unloading cluster coupled to the third cluster and configured to remove the display substrate conveyed from the third cluster.

[0024] The unloading cluster may include a plurality of unloading chambers, and each of the unloading chambers may be configured to store one of the plurality of display substrates entering the unloading cluster when the display substrate is not present therein.

[0025] The thin film encapsulation manufacturing apparatus may further include: a rotating module chamber coupled between the third cluster and the unloading cluster and configured to reverse the display substrate withdrawn from the third cluster.

[0026] According to another aspect of the present invention, a method for manufacturing a thin film package is provided, the method comprising: forming a first inorganic layer on a display substrate using a sputtering process; forming a first organic layer on the first inorganic layer on the display substrate using a monomer deposition process; and forming a second inorganic layer on the first organic layer on the display substrate using a chemical vapor deposition (CVD) process or a plasma enhanced chemical vapor deposition (PECVD) process.

[0027] After forming the first organic layer, the display substrate may be reversed before forming the second inorganic layer.

[0028] The first inorganic layer, the first organic layer, and the second inorganic layer may be formed in a first cluster including a plurality of process chambers, in a second cluster including a plurality of process chambers, and in a third cluster including a plurality of process chambers, respectively.

[0029] The first plurality of process chambers, the second plurality of process chambers, and the third plurality of process chambers may be arranged in order along one direction, and the first inorganic layer, the first organic layer, and the second inorganic layer may be respectively formed in the corresponding process chambers in the same order.

[0030] At least one of the first cluster, the second cluster, and the third cluster may include: a mask storage chamber configured to store a mask.

[0031] The display substrate may be conveyed from the first cluster to the second cluster by at least one of: a channel chamber located between the first cluster and the second cluster and configured to convey the display substrate; and a rotation module chamber coupled to the second cluster and configured to align an input direction of the display substrate.

[0032] The method may further include coupling a first plurality of channel chambers to opposite sides of a first rotation module chamber between the first cluster and the second cluster such that the coupled first plurality of channel chambers and the coupled first rotation module chamber couple the first cluster to the second cluster.

[0033] When the display substrate is transported, the internal pressures of the first cluster and one of the multiple channel chambers can be controlled to be substantially the same, the internal pressures of one of the multiple channel chambers and the rotation module chamber can be controlled to be substantially the same, the internal pressures of the rotation module chamber and another channel chamber among the multiple channel chambers can be controlled to be substantially the same, or the internal pressures of another channel chamber among the multiple channel chambers and the second cluster can be controlled to be substantially the same.

[0034] The display substrate may be conveyed from the second cluster to the third cluster through at least one of: a channel chamber located between the second cluster and the third cluster and configured to convey the display substrate; and a rotation module chamber configured to align an input direction of the display substrate.

[0035] The method may further include coupling a second plurality of channel chambers to opposite sides of a second rotation module chamber between the second cluster and the third cluster such that the coupled second plurality of channel chambers and the coupled second rotation module chamber couple the second cluster to the third cluster.

[0036] When the display substrate is transported, the internal pressures of the second cluster and one of the multiple channel chambers can be controlled to be substantially the same, the internal pressures of one of the multiple channel chambers and the rotation module chamber can be controlled to be substantially the same, the internal pressures of the rotation module chamber and another channel chamber among the multiple channel chambers can be controlled to be substantially the same, or the internal pressures of another channel chamber among the multiple channel chambers and the third cluster can be controlled to be substantially the same.

[0037] The formation of the first organic layer and the formation of the second inorganic layer may be performed alternately a plurality of times.

[0038] The first inorganic layer and the first organic layer may be formed using a downward deposition method, and the second inorganic layer may be formed using an upward deposition method.

[0039] After forming the inorganic layer and the first organic layer, the display substrate may be reversed before forming the second inorganic layer.

[0040] The method may further include, before forming the first inorganic layer, receiving the display substrate from an outside through a loading cluster.

[0041] The method may further include removing the display substrate by unloading the cluster after forming the first inorganic layer.

[0042] The unloading cluster may include a plurality of unloading chambers, and each of the unloading chambers may be configured to store one of the plurality of display substrates entering the unloading cluster when the display substrate is not present therein.

[0043] Prior to entering the unloading cluster, the display substrate may be inverted. BRIEF DESCRIPTION OF THE DRAWINGS

[0044] The above and other features and aspects of the present invention will become more apparent by describing in detail exemplary embodiments of the present invention with reference to the accompanying drawings, in which:

[0045] Figure 1 A conceptual diagram of a thin film encapsulation manufacturing apparatus according to an embodiment of the present invention;

[0046] Figure 2 For use Figure 1 A cross-sectional view of a display substrate manufactured by a thin film encapsulation manufacturing device;

[0047] Figure 3 A conceptual diagram of a thin film encapsulation manufacturing apparatus according to another embodiment of the present invention;

[0048] Figure 4 For use Figure 3 A cross-sectional view of a display substrate manufactured by a thin film encapsulation manufacturing device;

[0049] Figure 5 A conceptual diagram of a thin film encapsulation manufacturing apparatus according to another embodiment of the present invention; and

[0050] Figure 6 For use Figure 5 A cross-sectional view of a display substrate manufactured by a thin film encapsulation manufacturing device. DETAILED DESCRIPTION

[0051] Hereinafter, the embodiments of the present invention will be described more fully with reference to the accompanying drawings. However, the inventive concept can be implemented in many different forms and should not be interpreted as being limited to the exemplary embodiments described herein. On the contrary, these embodiments are provided so that the disclosure becomes thorough and complete for those of ordinary skill in the art, and comprehensively covers the scope of the present invention. The terms used herein are only for the purpose of describing a specific embodiment and are not intended to be limited to the inventive concept. As used herein, unless otherwise indicated by cleaning, the singular form is intended to include the plural form. It will be further understood that when the terms "including" and / or "including" are used in this specification, it is to specify the presence of the features, quantities, operations, elements and / or components, rather than excluding the presence or addition of one or more other features, quantities, operations, elements, components and / or their groups. It will be understood that although the terms "first", "second", "third" can be used herein to describe a variety of elements, components, regions, layers and / or parts, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish an element, component, region, layer or part from another region, layer or part.

[0052] As used herein, the term "and / or" includes any and all combinations of one or more of the associated listed items. Expressions such as "at least one of" when preceding a list of elements, modify the entire list of elements and do not modify the individual elements of the list.

[0053] Figure 1 FIG. 1 is a conceptual diagram of a thin film encapsulation manufacturing apparatus 100 according to an embodiment of the present invention. Figure 2 For use Figure 1 sectional view of a display substrate 200 manufactured by the thin film encapsulation manufacturing apparatus 100.

[0054] Reference Figure 1 and Figure 2 The thin film encapsulation manufacturing equipment 100 may include: a loading cluster 110, a first channel chamber P1, a first cluster 120, a second channel chamber P2, a second cluster 130, a third channel chamber P3, a first rotation module chamber T1, a third cluster 140, a second rotation module chamber T2, a fourth channel chamber P4 and an unloading cluster 150.

[0055] The loading cluster 110 may receive the display substrate 200 from the outside and supply the display substrate 200 to the first cluster 120. The loading cluster 110 may include a loading chamber 112 for receiving and storing the display substrate 200. A plurality of loading chambers 112 may be included, and each of the plurality of loading chambers 112 may store the display substrate 200. Also, the loading cluster 110 may include a first transfer chamber 111 coupled to the loading chamber 112. The plurality of loading chambers 112 may be coupled to the first transfer chamber 111, respectively.

[0056] Meanwhile, the first passage chamber P1 may couple the loading cluster 110 and the first cluster 120. The first passage chamber P1 may be configured to transfer the display substrate 200 from the loading cluster 110 to the first cluster 120.

[0057] The first cluster 120 may include a second transfer chamber 121. Also, the first cluster 120 may include a first sputtering chamber 122 that is coupled to the second transfer chamber 121 and is a process chamber for performing a sputtering process. Here, a plurality of first sputtering chambers 122 may be included, and the plurality of first sputtering chambers 122 may be respectively coupled to the second transfer chamber 121. A first inorganic layer 231 may be deposited on the display substrate 200 in the first sputtering chamber 122.

[0058] Optionally, the first cluster 120 may include a first mask storage chamber 123 for storing masks required during the sputtering process. Here, the first mask storage chamber 123 may store masks and then automatically supply the masks to the first sputtering chamber 122.

[0059] Meanwhile, the second channel chamber P2 may couple the first cluster 120 and the second cluster 130 , and may be configured to transport the display substrate 200 from the first cluster 120 to the second cluster 130 .

[0060] The second cluster 130 may include a third transfer chamber 131 for temporarily storing the display substrate 200 transferred through the second passage chamber P2. Also, the second cluster 130 may include a first monomer deposition chamber 132 coupled to the third transfer chamber 131 and being a process chamber for performing a monomer deposition process. Here, a plurality of first monomer deposition chambers 132 may be included, and each first monomer deposition chamber 132 may be coupled to the third transfer chamber 131. A first organic layer 232 may be formed on the first inorganic layer 231 in the first monomer deposition chamber 132.

[0061] Optionally, the second cluster 130 may include a second mask storage chamber 133 for storing masks required during the sputtering process. Here, the second mask storage chamber 133 may store a plurality of masks and may supply the masks to the first monomer deposition chamber 132 as needed.

[0062] Meanwhile, the third passage chamber P3 and the first turning module chamber T1 may be coupled between the second cluster 130 and the third cluster 140. Here, the third passage chamber P3 is configured to convey the display substrate 200 from the second cluster 130 to the first turning module chamber T1, and the first turning module chamber T1 may be formed in the form of a flip chamber to invert (e.g., flip or reverse) and align the display substrate 200. For example, after performing downward deposition in the first and second clusters, the first turning module chamber inverts (e.g., flips or reverses) the display substrate upside down to perform upward deposition in the third cluster 140, thereby conveying the display substrate from the second cluster 130 to the third cluster 140.

[0063] The third cluster 140 may include a fourth transfer chamber 141 coupled to the first rotation module chamber T1. Here, the fourth transfer chamber 141 may also be coupled to the first chemical vapor chamber 142, which is a process chamber for laminating the second inorganic layer 233. A plurality of first chemical vapor chambers 142 may be included, and the plurality of first chemical vapor chambers 142 may be radially arranged at various intervals (e.g., predetermined intervals) in the fourth transfer chamber 141.

[0064] The second inorganic layer 233 may be formed in the first chemical vapor chamber 142 by using a conventional chemical vapor deposition (CVD) method or a plasma enhanced chemical vapor deposition (PECVD) method. However, for the convenience of description, an embodiment in which the second inorganic layer 233 is formed in the first chemical vapor chamber 142 using a conventional CVD method will be described in detail.

[0065] The third cluster 140 may be coupled to the fourth transfer chamber 141, and may include a third mask storage chamber 143 for supplying masks required in the first chemical vapor chamber 142. Here, the third mask storage chamber 143 may store masks required in a process and then supply the masks to each of the first chemical vapor chambers 142 performing the process.

[0066] Meanwhile, the second turning module chamber T2 may be coupled to the third cluster 140 formed as described above. The second turning module chamber T2 may be coupled to the fourth transfer chamber 141 and configured to transport the process-completed display substrate 200 by inverting (flipping or reversing) the display substrate 200. In detail, the second turning module chamber T2 may be formed as a flip chamber of the first turning module chamber T1 as described above.

[0067] The fourth transfer chamber P4 may be coupled to the second turning module chamber T2 . The fourth transfer chamber P4 may be configured to transfer the display substrate 200 completing the thin film encapsulation process to the unloading cluster 150 .

[0068] The unloading cluster 150 may include a fifth transfer chamber 151. Also, the unloading cluster 150 may include an unloading chamber 152 coupled to the fifth transfer chamber 151 and configured to transfer the display substrate 200 to the outside from the fifth transfer chamber 151. Here, a plurality of unloading chambers 152 may be included, and the plurality of unloading chambers 152 may be radially installed or coupled to the fifth transfer chamber 151.

[0069] Meanwhile, a method of performing a thin film encapsulation process by using the thin film encapsulation manufacturing apparatus 100 and a structure of the display substrate 200 will be described in detail hereinafter.

[0070] First, the display substrate 200 may be manufactured. In detail, the display substrate 200 may include a first substrate 210 , an encapsulation unit 230 , and a light emitting unit 220 .

[0071] The light emitting unit 220 may be formed on the first substrate 210. Here, the light emitting unit 220 includes a thin film transistor (TFT); and a passivation layer 221 covering the TFT (eg, formed on the TFT), and an organic light emitting device (OLED) may be formed on the passivation layer 221.

[0072] The first substrate 210 may be formed of a glass material, but is not limited thereto, and may also be formed of a plastic material or a metal material such as stainless steel (SUS) or titanium (Ti).

[0073] A buffer layer 222 formed of an organic compound and / or an inorganic compound may be further formed on the upper surface of the first substrate 210 and may be made of, for example, SiO x (x≥1) or SiN x (x≥1) is formed.

[0074] After an active layer 223 arranged in a pattern (e.g., a predetermined pattern) is formed on the buffer layer 222, a gate insulating layer 224 is formed on the active layer 223 and the buffer layer 222. The active layer 223 includes a source region 223a and a drain region 223c, and also includes a channel region 223b located between the source region 223a and the drain region 223c. The active layer 223 may be formed of amorphous silicon, but is not limited thereto. The active layer 223 may also be formed of an oxide semiconductor. Examples of oxide semiconductors may include oxides selected from the following materials: metal elements of Groups 4, 12, 13, and 14, such as zinc (Zn), indium (In), gallium (Ga), tin (Sn), cadmium (Cd), germanium (Ge), and hafnium (Hf), and a combination of two or more metals thereof. For example, the active layer 223 formed of a semiconductor may include GIZO [(In 2 O 3 )a(Ga 2 O3 )b(ZnO)c] (a, b and c are real numbers satisfying the conditions of a≥0, b≥0 and c>0, respectively). However, for the convenience of description, the following description will focus on the active layer 223 formed of amorphous silicon.

[0075] The active layer 223 may be formed by first forming an amorphous silicon layer on the buffer layer 222, crystallizing the amorphous silicon layer into a polysilicon layer, and patterning the polysilicon layer. Depending on the TFT type, whether the TFT is a driving TFT (not shown) or a switching TFT (not shown), the active layer 223 may include a source region 223a and a drain region 223c having impurities.

[0076] A gate electrode 225 corresponding to the active layer 223 , and an interlayer insulating layer 226 covering the gate electrode 225 are formed on the gate insulating layer 224 .

[0077] Contact holes are formed through the interlayer insulating layer 226 and the gate insulating layer 224, and a source electrode 227a and a drain electrode 227b are formed on the interlayer insulating layer 226, extending through the interlayer insulating layer 226 and the gate insulating layer 224 to contact the source region 223a and the drain region 223c, respectively.

[0078] At the same time, since the reflective layer is formed on the source / drain electrodes 227a and 227b at the same time as described above, the source / drain electrodes 227a and 227b may be formed of a high conductivity material having a thickness capable of reflecting light. For example, the source / drain electrodes 227a and 227b may be formed of a metal material such as silver (Ag), magnesium (Mg), aluminum (Al), platinum (Pt), palladium (Pd), gold (Au), nickel (Ni), neodymium (Nd), iridium (Ir), chromium (Cr), lithium (Li), calcium (Ca), or a compound of two or more thereof.

[0079] A passivation layer 221 is formed on the TFT and the reflective layer formed as described above, and a pixel electrode 228a of the OLED is formed on the passivation layer 221. The pixel electrode 228a contacts the drain electrode 227b of the TFT through a through hole H2 formed in the passivation layer 221. The passivation layer 221 may be formed of an inorganic material and / or an organic material, and may have a single layer or a structure including at least two layers, and may also be formed as a planarization layer so as to planarize its upper surface regardless of the curve of the lower layer. In addition, the passivation layer 221 may be formed of a transparent insulating material to obtain a resonance effect.

[0080] After forming the pixel electrode 228a on the passivation layer 221, the pixel defining layer 229 may be formed to cover the pixel electrode 228a and the passivation layer 221 of the organic material and / or inorganic material. The pixel defining layer 229 is opened to expose the pixel electrode 228a. That is, a portion of the pixel defining layer 229 on the pixel electrode 228a may be etched or removed to expose a portion of the surface of the pixel electrode 228a.

[0081] In addition, an organic layer 228 b and an opposing electrode 228 c are formed at least on the pixel electrode 228 a .

[0082] The pixel electrode 228 a may function as an anode electrode, and the opposing electrode 228 c may function as a cathode electrode, and the polarities of the pixel electrode 228 a and the opposing electrode 228 c may be exchanged.

[0083] The pixel electrode 228a may be formed of a material having a high work function, such as indium tin oxide (ITO), indium zinc oxide (IZO), In 2 O 3 and ZnO transparent conductors.

[0084] The opposite electrode 228c may be formed of a metal such as Ag, Mg, Al, Pt, Pd, Au, Ni, Nd, Ir, Cr, Li, Ca, and a compound or alloy of two or more thereof; in detail, the opposite electrode 228c may be formed of Mg, Ag or Al with a thin thickness to become a semi-transparent reflective layer so that light is transmitted therethrough after optical resonance. The pixel electrode 228a and the opposite electrode 228c are electrically insulated from each other by the organic layer 228b, and light is emitted in the organic emission layer by applying a voltage of opposite polarity to the organic layer 228b.

[0085] The organic layer 228b can be formed by a low molecular weight or polymer organic layer. When formed by a low molecular weight layer, the organic layer 228b can have a structure in which a hole injection layer (HIL), a hole transport layer (HTL), an organic emission layer (EML), an electron transport layer (ETL) and an electron injection layer (EIL) are stacked in a single layer or multilayer structure, and a variety of organic materials such as copper phthalocyanine (CuPc), N, N'-di (naphthalene-1-yl) -N, N'-diphenyl-benzidine (NPB), tris-8-hydroxyquinoline aluminum (Alq3) can be used. A vacuum deposition method can be used to form a low molecular weight organic layer. Here, HIL, HTL, ETL and EIL are common layers that can be commonly applied to red, green and blue pixels. Therefore, like the opposing electrode 228C, the common layer may be formed to cover the entire pixel.

[0086] For example, a polymer organic layer can generally be formed of an HTL and an EML, and here, PEDOT can be used as the HTL, and a polymer organic material such as a polyphenylenevinylene (PPV) type material or a polyfluorene type material can be used as an organic emission layer that can be formed by screen printing, inkjet printing, a fine metal mask process, a laser thermal transfer process, etc.

[0087] At the same time, the organic emission layer as described above can be formed in a variety of forms. For example, a blue organic emission layer, a green organic emission layer, and a red organic emission layer can be formed in each sub-pixel to form a single unit pixel. And, in addition to the blue, green, and red organic emission layers as described above, organic emission layers of other colors can also be formed in sub-pixels. Therefore, in addition to the blue, green, and red organic emission layers, the blue organic emission layer, the green organic emission layer, and the red organic emission layer can be stacked to form a white organic emission layer as a sub-pixel, thereby forming a single unit pixel.

[0088] In addition, although an organic emission layer formed of an additional light-emitting material in each pixel is described above, embodiments of the present invention are not limited thereto. For example, the organic emission layer may be formed in common throughout the pixel regardless of the position of the pixel. Here, the organic emission layer may be formed by vertically stacking, for example, emission materials that emit red, green, and blue light, or by mixing emission materials. Obviously, if white light can be emitted, combinations of other colors are also possible. Furthermore, a color conversion layer or filter may also be included for converting the emitted white light into another color (e.g., a predetermined color).

[0089] The organic layer 228b is not limited thereto, and other various examples of the organic layer 228b may also be applied. However, for the convenience of description, the following description will focus on sub-pixels formed by a blue organic emission layer, a green organic emission layer, and a red organic emission layer to form a single unit pixel.

[0090] Meanwhile, after preparing the first substrate 210 on which the light emitting unit 220 is formed, the first substrate 210 may be input to the thin film encapsulation manufacturing apparatus 100 to form the encapsulation unit 230. As described above, the encapsulation unit 230 may be formed by sequentially stacking the first inorganic layer 231, the first organic layer 232, and the second inorganic layer 233.

[0091] In detail, the first organic layer 232 may be formed of a polymer, and may be a single layer or a laminate formed of one of polyethylene terephthalate, polyimide, polycarbonate, epoxy resin, polyethylene, and polyacrylate. In one embodiment, the first organic layer 232 may be formed of polypropylene; in detail, the first organic layer 232 may include a monomer composition including a diacrylate monomer and a triacrylate monomer. The monomer composition may also include a monoacrylate monomer. In addition, a photoinitiator known in the art, such as a thermoplastic polyolefin (TPO), may also be included in the monomer composition, but embodiments of the present invention are not limited thereto.

[0092] The first inorganic layer 231 and the second inorganic layer 233 may be a single layer or a stacked layer including metal oxide or metal nitride. In detail, the first inorganic layer 231 and the second inorganic layer 233 may include SiNx, Al 2 O 3 、SiO 2 、TiO 2 Here, the second inorganic layer 233 may be formed to prevent or reduce penetration of moisture with respect to the light emitting unit 220 .

[0093] Meanwhile, a metal halide layer including LiF may also be included between the light emitting unit 220 and the first inorganic layer 231. The metal halide layer may prevent or reduce damage to the light emitting unit 220 when the first inorganic layer 231 is formed by using a sputtering process.

[0094] Also, the first organic layer 232 is characterized in that it has a surface smaller than that of the second inorganic layer 233. Here, the first organic layer 232 is completely covered by the second inorganic layer 233.

[0095] The method of forming the packaging unit 230 as described above will be described in detail. First, the first substrate 210 on which the light emitting unit 220 is formed may be loaded into the loading chamber 112 ( Figure 1 ). Here, various loading methods may be used. For example, the first substrate 210 on which the light emitting unit 220 is formed may be loaded into a box, and then the box may be loaded into the loading chamber 112. Also, the first substrate 210 on which the light emitting unit 220 is formed may be supplied (e.g., loaded or placed) to the loading chamber 112 by using a conveying unit such as an external robot.

[0096] Meanwhile, the first substrate 210 supplied as described above may be supplied or transferred from the loading chamber 112 to the first transfer chamber 111. Here, a robot arm or the like may be installed or coupled to the first transfer chamber 111 to move the first substrate 210. When the first substrate 210 is transferred from the loading chamber 112 to the first transfer chamber 111, the pressures of the loading chamber 112 and the first transfer chamber 111 may be adjusted to be the same before performing the transfer operation.

[0097] The first substrate 210 transferred to the first transfer chamber 111 as described above may be transferred again to the first passage chamber P1 from the first transfer chamber 111. Here, when the first substrate 210 is transferred, internal pressures of the first transfer chamber 111 and the first passage chamber P1 may be controlled to be uniform.

[0098] The first passage chamber P1 may again transfer the first substrate 210 to the second transfer chamber 121 of the first cluster 120. Here, when the first substrate 210 is transferred, internal pressures of the first passage chamber P1 and the second transfer chamber 121 may be uniformly or substantially uniformly maintained.

[0099] The first substrate 210 transported as described above can be loaded from the second transfer chamber 121 to one of the plurality of first sputtering chambers 122. Here, the plurality of first substrates 210 can be loaded into the first sputtering chamber 122 in a defined or predetermined order (e.g., in a clockwise or counterclockwise direction). For example, the order of the plurality of first sputtering chambers 122 can be specified or arranged along a direction (e.g., a predetermined direction), such as a clockwise or counterclockwise direction. And, each first sputtering chamber 122 can be assigned an identity (ID). The method of determining the order is not limited thereto, and a variety of methods can be used to determine the order of the plurality of first sputtering chambers 122. However, for the convenience of description, the following description will focus on an embodiment in which the order is determined in a desired or predetermined direction.

[0100] For example, the first substrate 210 may be loaded into the first sputtering chambers 122 numbered according to the ID given to the first substrate 210. For example, the first substrate 210 may be loaded into the first sputtering chambers 122 such that the ID of the first substrate 210 is consistent with the order of the first sputtering chambers 122.

[0101] When the first inorganic layer 231 is formed by using a sputtering process as described above, a mask for the sputtering process may be transported from the first mask storage chamber 123 to the first sputtering chamber 122 to be subjected to the sputtering process. The mask may enter at least one of a plurality of first sputtering chambers 122 to be subjected to the sputtering process. The mask may enter the first sputtering chamber 122 after or before the first substrate 210 enters the first sputtering chamber 122. Also, the embodiments of the present invention are not limited thereto, and the mask may enter simultaneously with the first substrate 210.

[0102] Meanwhile, after the first substrate 210 has entered the first sputtering chamber 122, the first sputtering chamber 122 may form a first inorganic layer 231 on the light emitting unit 220. Here, the first inorganic layer 231 is the same as described above, and thus a description thereof will be omitted.

[0103] When the first inorganic layer 231 is completely formed as described above, the first substrate 210 may be transferred from the first sputtering chamber 122 to the second transfer chamber 121. Here, pressures of the first sputtering chamber 122 and the second transfer chamber 121 may be controlled to be the same.

[0104] For example, by using a robot, the second transfer chamber 121 may transfer the first substrate 210 on which the first inorganic layer 231 is formed to the second passage chamber P2. For example, the first substrate 210 may be transferred from the second transfer chamber 121 to the second passage chamber P2 while uniformly or substantially uniformly maintaining internal pressures in the second transfer chamber 121 and the second passage chamber P2.

[0105] Meanwhile, the first substrate 210 conveyed as described above may be conveyed to the second cluster 130. Here, the first substrate 210 may be conveyed to the third transfer chamber 131 coupled to the second passage chamber P2, and when the first substrate 210 is conveyed, the pressures of the second passage chamber P2 and the third transfer chamber 131 may be maintained the same or substantially the same.

[0106] As described above, the first substrate 210 transported to the third transfer chamber 131 may be transported from the third transfer chamber 131 to the first monomer deposition chamber 132. Here, the method of transporting the first substrate 210 to one of the plurality of first monomer deposition chambers 132 may be the same as the above-described method of transporting the first substrate 210 to one of the plurality of first sputtering chambers 122. For example, the plurality of first monomer deposition chambers 132 may be numbered in the same order as the plurality of first sputtering chambers 122.

[0107] The third transfer chamber 131 and the first monomer deposition chamber 132 may be set to have the same or substantially the same pressure. The first monomer deposition chamber 132 may form the first organic layer 232 on the first inorganic layer 231. In detail, when the first substrate 210 is loaded into the first monomer deposition chamber 132, the monomer and the photoinitiator may be deposited by using a flash evaporation method, and the monomer and the photoinitiator may be polymerized by applying ultraviolet (UV) rays or heat.

[0108] When the above processes are completed, UV rays or heat may be applied to the surface on which the monomer is deposited and hardened, thereby polymerizing the monomer to form the first organic layer 232 in the form of a polymer. The first organic layer 232 is the same as described above, and thus a description thereof will be omitted.

[0109] The mask stored in the second mask storage chamber 133 and used to form the first organic layer 232 may be supplied to the first monomer deposition chamber 132. Here, a method of supplying the mask from the second mask storage chamber 133 to the first monomer deposition chamber 132 is similar to a method of supplying the mask from the first mask storage chamber 123 to the first sputtering chamber 122, and thus a description thereof will be omitted.

[0110] Meanwhile, the first substrate 210 transferred to the third transfer chamber 131 after forming the first organic layer 232 on the first inorganic layer 231 may be transferred to the third passage chamber P3 again from the third transfer chamber 131. Here, when the first substrate 210 is transferred, the internal pressures of the third passage chamber P3 and the third transfer chamber 131 may be controlled to be the same.

[0111] When the above process is completed, the first substrate 210 may be supplied from the third transfer chamber 131 to the first turning module chamber T1. Here, the first turning module chamber T1 may invert (e.g., flip or reverse) the first substrate 210 by 180 degrees. In detail, in the case of the first cluster 120 and the second cluster 130, a downward deposition method is used in which the deposition material is moved upward to deposit the first inorganic layer 231 and the first organic layer 232, and in the case of the third cluster 140, an upward deposition method is used in which the deposition material is moved downward to deposit the second inorganic layer 233. Therefore, in order to deposit upward, the first substrate 210 may be inverted (e.g., flipped or reversed) by 180 degrees.

[0112] As described above, after inverting (eg, flipping or reversing) the first substrate 210 in the first turn module chamber T1, the first substrate 210 may be supplied to the fourth transfer chamber 141. Here, internal pressures of the first turn module chamber T1 and the fourth transfer chamber 141 may be controlled to be the same or substantially the same.

[0113] Meanwhile, the first substrate 210 transferred to the fourth transfer chamber 141 may be transferred again to the first chemical vapor chamber 142. Here, internal pressures of the fourth transfer chamber 141 and the first chemical vapor chamber 142 may be controlled to be the same or substantially the same.

[0114] As described above, when the second inorganic layer 233 is deposited, the mask for the first chemical vapor chamber 142 may be supplied from the third mask storage chamber 143. Here, the process of the third mask storage chamber 143 is similar to that of the first mask storage chamber 123 or the second mask storage chamber 133, and thus a detailed description thereof will be omitted.

[0115] Meanwhile, when the deposition of the second inorganic layer 233 is completed, the display substrate 200 on which the encapsulation unit 230 is formed may be transferred to the second rotation module chamber T2 from the fourth transfer chamber 141. Here, the second rotation module chamber T2 may restore the display substrate 200 to an original state by inverting (e.g., flipping or reversing) the display substrate 200 by 180 degrees.

[0116] The display substrate 200 restored to the original state may be transferred from the second turning module chamber T2 to the fifth transfer chamber 151 through the fourth passage chamber P4. Here, when the display substrate 200 is transferred from the fourth passage chamber P4 to the fifth transfer chamber 151, it may be transferred while uniformly or substantially uniformly maintaining the internal pressures of the second turning module chamber T2 and the fourth passage chamber P4, and then finally transferred to the fifth transfer chamber 151 by uniformly or substantially uniformly maintaining the internal pressures of the fourth passage chamber P4 and the fifth transfer chamber 151.

[0117] When the above process is completed, the encapsulation unit 230 may be completely formed on the light emitting unit 220 to complete the manufacture of the display substrate 200. The display substrate 200 manufactured as described above may be loaded from the fifth transfer chamber 151 to the unloading chamber 152 and stored therein. Here, the display substrate 200 may be transported while the internal pressures of the fifth transfer chamber 151 and the unloading chamber 152 are controlled to be the same.

[0118] Meanwhile, various methods may be used to load the completed display substrate 200 into the unloading chamber 152. For example, the order for the unloading chambers 152 may be preset, or if the display panel 200 is completely loaded into a randomly selected unloading chamber 152, the display substrate 200 may be controlled to be stored in another unloading chamber 152. Also, one display substrate 200 is stored in the unloading chamber 152, and if it is determined that there is no display substrate 200, a suitable display substrate 200 may be transferred from the fifth transfer chamber 151. The suitable display substrate 200 may be selected randomly or in a predetermined order.

[0119] Therefore, the thin film encapsulation manufacturing apparatus 100 as described above can perform the thin film encapsulation process in an in-line manner, and thus can optimize the time used in the thin film encapsulation process.

[0120] Also, when forming a multi-layer thin film package, the thin film package manufacturing apparatus 100 can adjust the thickness of each layer, and since upward layer formation and downward layer formation can be performed simultaneously, the multi-layer thin film package can be easily formed.

[0121] Since the thin film encapsulation manufacturing apparatus 100 includes the loading cluster 110 and the unloading cluster 150, the thin film encapsulation may be formed in an in-line process, thereby increasing production efficiency.

[0122] Figure 3 FIG. 4 is a conceptual diagram of a thin film encapsulation manufacturing apparatus 300 according to another embodiment of the present invention. Figure 4 For use Figure 3 4 is a cross-sectional view of a display substrate 400 manufactured by the thin film encapsulation manufacturing equipment 300.

[0123] Reference Figure 3 and Figure 4The thin film encapsulation manufacturing equipment 300 may include a loading cluster (not shown), a first channel chamber P1, a first cluster 320, a second channel chamber P2, a first rotation module chamber T1, a third channel chamber P3, a second cluster 330, a fourth channel chamber P4, a second rotation module chamber T2, a fifth channel chamber P5, a third cluster 340, a sixth channel chamber P6, a third rotation module chamber T3, a seventh channel chamber P7, a fourth cluster 360, an eighth channel chamber P8, a fourth rotation module chamber T4, a ninth channel chamber P9, a fifth cluster 370, a tenth channel chamber P10, a fifth rotation module chamber T5, an eleventh channel chamber P11 and an unloading cluster (not shown).

[0124] The first channel chamber P1 to the eleventh channel chamber P11 are based on the above reference Figure 1 and Figure 2 The first to fourth passage chambers P1 to P4 are described as being formed in the same or similar manner, and the display substrate 400 may also be transported using the same or similar method, and thus a detailed description thereof will be omitted.

[0125] And the first rotating module chamber T1 to the fifth rotating module chamber T5 are based on the above reference Figure 1 and Figure 2 The described first and second turning module chambers T1 and T2 are formed in the same or similar manner, and the display substrate 400 may also be conveyed in the same or similar method by aligning or inverting (flipping or reversing) the display substrate 400, and thus a detailed description thereof will be omitted.

[0126] At the same time, loading and unloading clusters are the same as above. Figure 1 and Figure 2 The same method described is formed, and therefore its detailed description will be omitted below. In addition, the loading cluster and the unloading cluster may or may not be included in the thin film encapsulation manufacturing equipment 300, and therefore, for the convenience of description, the following description will focus on the implementation method that does not include the loading cluster and the unloading cluster.

[0127] The first cluster 320 may include a second transfer chamber 321, a first sputtering chamber 322, and a first mask storage chamber 323. The first cluster 320 is based on the reference Figure 1 and Figure 2 The same or similar method as described above is formed, and thus a detailed description thereof will be omitted.

[0128] Also, the second cluster 330 may include a third transfer chamber 331, a first monomer deposition chamber 332, and a second mask storage chamber 333. The second cluster 330 is based on the reference Figure 1 and Figure 2 The same or similar method as described above is formed, and thus a detailed description thereof will be omitted.

[0129] The third cluster 340 may include a fourth transfer chamber 341, a first chemical vapor chamber 342, and a second mask storage chamber 343. The third cluster 340 is based on the reference Figure 1 and Figure 2 The second inorganic layer 433 is formed by the same or similar method as described above, and thus a detailed description thereof will be omitted. However, for the convenience of description, the following description will focus on an embodiment in which the second inorganic layer 433 is formed in the first chemical vapor chamber 342 by using a PECVD method.

[0130] Meanwhile, the fourth cluster 360 may include a sixth transfer chamber 361, a second monomer deposition chamber 362, and a fourth mask storage chamber 363. Therefore, the fourth cluster 360 may form a second organic layer 434 on the second inorganic layer 433. The fourth cluster 360 may be formed in a similar manner to the second cluster 330, and the second organic layer 434 may be formed in the same manner as the first organic layer 432, and thus a detailed description thereof will be omitted.

[0131] The fifth cluster 370 may include a seventh transfer chamber 371, a second chemical vapor chamber 372, and a fifth mask storage chamber 373. The fifth cluster 370 may form a third inorganic layer 435 on the second organic layer 434. The fifth cluster 370 may be formed in a similar manner to the third cluster 340, and the third inorganic layer 435 may be formed in the same manner as the second inorganic layer 433, and thus a detailed description thereof will be omitted.

[0132] Meanwhile, a method of performing a thin film encapsulation process by using the thin film encapsulation manufacturing apparatus 300 and a structure of the display substrate 400 will be described in detail hereinafter.

[0133] First, the display substrate 400 may be manufactured. In detail, the display substrate 400 may include a first substrate 410, an encapsulation unit 430, and a light emitting unit 420. Here, the first substrate 410 and the light emitting unit 420 are respectively Figure 1 and Figure 2 The above-mentioned first substrate 210 and the light emitting unit 220 are the same, and thus a detailed description thereof will be omitted.

[0134] Meanwhile, after preparing the first substrate 410 on which the light emitting unit 420 is formed, the first substrate 410 may be loaded or positioned in the thin film encapsulation manufacturing apparatus 300 to form an encapsulation unit 430. Here, the encapsulation unit 430 may include at least one sandwich structure in which at least one organic layer is inserted between at least two inorganic layers. Also, the encapsulation unit 430 may include a sandwich structure in which at least one inorganic layer is inserted between at least two organic layers.

[0135] The encapsulation unit 430 may be formed by sequentially stacking the first inorganic layer 431 , the first organic layer 432 , the second inorganic layer 433 , the second organic layer 434 , and the third inorganic layer 435 as described above.

[0136] In detail, the first organic layer 432 and the second organic layer 434 may be formed of a polymer, and may be a single layer or a laminate formed of one of polyethylene terephthalate, polyimide, polycarbonate, epoxy resin, polyethylene, and polyacrylate. In one embodiment, the first organic layer 432 and the second organic layer 434 may be formed of polypropylene, and in detail, may include a monomer composition including a diacrylate monomer and a triacrylate monomer. The monomer composition may also include a monoacrylate monomer. In addition, a photoinitiator known in the art such as TPO may also be included in the monomer composition, but embodiments of the present invention are not limited thereto.

[0137] The first to third inorganic layers 431, 433, and 435 may be a single layer or a stacked layer including metal oxide or metal nitride. In detail, the first to third inorganic layers 431, 433, and 435 may include SiNx, Al 2 O 3 、SiO 2 、TiO 2 Here, the third inorganic layer 435 may be formed to prevent or reduce penetration of moisture with respect to the light emitting unit 420 .

[0138] Meanwhile, a metal halide layer including LiF may be further included between the light emitting unit 420 and the first inorganic layer 431. The metal halide layer may prevent or reduce damage to the light emitting unit 420 when the first inorganic layer 431 is formed by using a sputtering process.

[0139] Furthermore, the first organic layer 432 is characterized in that it has a smaller surface than the second inorganic layer 433, and the second organic layer 434 may also have a smaller surface area than the third inorganic layer 435. Furthermore, the first organic layer 432 is characterized in that it is completely covered by the second inorganic layer 433, and the second organic layer 434 may also be completely covered by the third inorganic layer 435.

[0140] A method of forming the encapsulation unit 430 as described above will be described in detail. By maintaining the vacuum degree or pressure of the entire thin film encapsulation manufacturing apparatus 300 at or below 5E-4Pa, masks in the first to fifth mask storage chambers 323, 333, 343, 363, and 373 can be transferred between the first sputtering chamber 322, the first monomer deposition chamber 332, the first chemical vapor chamber 342, the second monomer deposition chamber 362, and the second chemical vapor chamber 372, respectively, by using a robot arm.

[0141] When the above process is completed, the first substrate 410 on which the light emitting unit 420 is formed is installed in the first passage chamber P1, and the vacuum degree or pressure of the first passage chamber P1 is maintained at the same or substantially the same level as that of the second transfer chamber 321, and then the gate valve is opened to move the first substrate 410 to the second transfer chamber 321. Here, the first substrate 410 may be moved by using a robot.

[0142] Meanwhile, when the vacuum degree or pressure of the second transfer chamber 321 is at the same level as the vacuum degree or pressure of one of the first sputtering chambers 322 performing the sputtering process for forming the first inorganic layer 431, the gate valve is opened to move or transfer the first substrate 410 to the first sputtering chamber 322. After being loaded between the pre-installed mask and the substrate holder, the first substrate 410 is aligned by using the mark of the first substrate 410 and the opening mark of the mask by using an alignment instrument coupled with a visual unit, and then the first substrate 410 and the mask are bonded to each other.

[0143] At the same time, process gas is injected into the first sputtering chamber 322 of the sputtering process to maintain the vacuum degree or pressure in the range of 1E-1 to 1E-2 Pa, and voltage is applied to the cathode to generate plasma discharge. Here, the first substrate 410 or the cathode is transported into the first sputtering chamber 322 while the layer is formed.

[0144] During the process, when the first inorganic layer 431 reaches a target thickness, the first substrate 410 or the cathode is moved to a standby area to stop the discharge, and the gas injection operation is also stopped to control the conductance of the vacuum discharge system, thereby maintaining the vacuum degree or pressure of the first sputtering chamber 322 at the same level as that of the second transfer chamber 321. Here, the first substrate 410 and the mask are separated from each other to move the first substrate 410 to a position where it can be discharged.

[0145] When the above processes are completed, the first substrate 410 is moved from the first sputtering chamber 322 to the second transfer chamber 321. Also, when the vacuum degrees or pressures of the second transfer chamber 321 and the second passage chamber P2 are at the same or substantially the same level, the first substrate 410 is moved from the second transfer chamber 321 to the second passage chamber P2.

[0146] When the vacuum degrees or pressures of the second channel chamber P2 and the first rotation module chamber T1 are at the same or substantially the same level, the first substrate 410 is moved to the first rotation module chamber T1, and the first substrate 410 is rotated 180 degrees in the first rotation module chamber T1 to prevent or reduce changes in the input position of the first substrate 410.

[0147] Meanwhile, when the operation of the first turn module chamber T1 is completed, the vacuum degrees or pressures of the first turn module chamber T1 and the third passage chamber P3 are controlled to be the same or substantially the same, thereby moving the first substrate 410 to the third passage chamber P3.

[0148] Here, while maintaining the vacuum degrees or pressures of the third passage chamber P3 and the third transfer chamber 331 at the same or substantially the same level, the gate valve is opened to move the first substrate 410 to the third transfer chamber 331. Here, the first substrate 410 is moved by using a robot.

[0149] When the above process is completed, and the vacuum degree or pressure of the third transfer chamber 331 is at the same or substantially the same level as the vacuum degree or pressure of one of the plurality of first monomer deposition chambers 332 for performing the process of forming the first organic layer 432, the gate valve is opened to move the first substrate 410 to the first monomer deposition chamber 332. Here, after being loaded between the pre-installed mask and the substrate holder, the first substrate 410 is accurately aligned by using an alignment instrument coupled with a visual unit, by using a mark of the first substrate 410 and an opening mark of the mask, and then the first substrate 410 and the mask are bonded to each other.

[0150] A process gas for the monomer deposition process is injected into the first monomer deposition chamber 332 where the monomer deposition process is performed to maintain a vacuum degree or pressure within a range of 1E-1 to 1E-2 Pa, and a nozzle unit of a sprayer containing an evaporated organic material is turned on. Here, in the first monomer deposition chamber 332, formation and hardening of a layer are performed while conveying the first substrate 410 or the source unit.

[0151] As described above, when the first substrate 410 is loaded into the first monomer deposition chamber 332 , a monomer and a photoinitiator that may be polymerized by applying UV rays or heat may be deposited by using a flash evaporation method.

[0152] When the above processes are completed, UV rays or heat may be applied to the surface on which the monomer is deposited and hardened, thereby polymerizing the monomer to form the first organic layer 432 in the form of a polymer.

[0153] Meanwhile, during the above process, when the first organic layer 432 reaches a target thickness, the first substrate 410 or the source unit is moved to a standby area to stop the injection of the process gas, and the conductance of the vacuum discharge system is controlled to maintain the vacuum degree or pressure of the first monomer deposition chamber 332 at the same level as that of the third transfer chamber 331. Here, the first substrate 410 and the mask are separated from each other to move the first substrate 410 to a position where it can be discharged or removed.

[0154] When the vacuum degrees or pressures of the first monomer deposition chamber 332 and the third transfer chamber 331 are at the same or substantially the same level, the first substrate 410 is moved from the first monomer deposition chamber 332 to the third transfer chamber 331. Also, when the vacuum degrees or pressures of the third transfer chamber 331 and the fourth passage chamber P4 are at the same or substantially the same level, the first substrate 410 is moved or transported from the third transfer chamber 331 to the fourth passage chamber P4.

[0155] At the same time, when the vacuum degree or pressure of the fourth channel chamber P4 and the second rotation module chamber T2 is at the same or substantially the same level, the first substrate 410 is moved to the second rotation module chamber T2, and in the second rotation module chamber T2, the first substrate 410 is rotated approximately 180 degrees to prevent or reduce changes in the input position of the first substrate 410.

[0156] When the above process is completed, and when the vacuum degree or pressure of the second turn module chamber T2 and the fifth channel chamber P5 is at the same or substantially the same level, the first substrate 410 is moved to the fifth channel chamber P5. And, while the vacuum degree or pressure of the fifth channel chamber P5 and the third cluster 340 is maintained at the same level, the gate valve is opened to move the first substrate 410 to the third cluster 340. The first substrate 410 may be moved from the fourth channel chamber P4 to the fourth transfer chamber 341. Here, the first substrate 410 is moved by a robot.

[0157] As described above, when the vacuum degree or pressure of the fourth transfer chamber 341 is at the same or substantially the same level as the vacuum degree or pressure of one of the plurality of first chemical vapor chambers 342 for performing the PECVD method for forming the second inorganic layer 433 by controlling the conductance of the vacuum discharge system using the time and space division method, the gate valve is opened to move the first substrate 410 to the first chemical vapor chamber 342. After being loaded between the pre-installed mask and the substrate support, the first substrate 410 is aligned by using an alignment instrument coupled with a visual unit and by using a mark of the first substrate 410 and an opening mark of the mask, and then the first substrate 410 and the mask are bonded to each other.

[0158] Then, after completely closing the valve coupled to the high vacuum pump for controlling the conductance, Ar was injected as a discharge gas by using a plasma generation unit to keep the pressure in the range of 1 Pa to 200 Pa, and then the power was increased to 3 W / cm 2 Up to 5W / cm 2 range, thereby generating plasma.

[0159] Here, by supplying the reaction material, the reaction gas, and the transport gas using a plasma generation source, the pressure is adjusted within the range of 1 to 200 Pa. The reaction material is injected into the plasma region to form radicals (using SiN generation gas: SiH 4 / NH 3 / N 2 / H 2 / Ar). Then, in the above environment, the layer formation process is performed. Here, the layer formation speed is maintained at 200nm / min or less, and SiH is continuously supplied. 4 (50-500sccm) / NH 3 (300-2000sccm) / N 2 (300-2000sccm) of gas.

[0160] Meanwhile, during the above process, when the second inorganic layer 433 reaches the target thickness, the supply of the gas for the reaction is stopped, and the plasma power is reduced to 1 W / cm in multiple stages. 2 Then, the first substrate 410 and the mask are separated from each other to move the first substrate 410 to a position where it can be discharged. At the same time, the valve installed in the high vacuum pump for controlling the conductance is opened by using a time-division space control method, and then the vacuum degree or pressure of the first chemical vapor chamber 342 and the vacuum degree or pressure of the fourth transfer chamber 341 are maintained at the same level. Here, the first substrate 410 is moved from the first chemical vapor chamber 342 to the fourth transfer chamber 341.

[0161] Meanwhile, when the above processes are completed, the vacuum degrees or pressures of the fourth transfer chamber 341 and the sixth pass chamber P6 are at the same or substantially the same level, and the first substrate 410 is moved from the fourth transfer chamber 341 to the sixth pass chamber P6 .

[0162] Furthermore, when the vacuum degree or pressure of the sixth channel chamber P6 and the third rotation module chamber T3 is at the same or substantially the same level, the first substrate 410 is moved to the third rotation module chamber T3, and the first substrate 410 is rotated 180 degrees in the third rotation module chamber T3 to prevent or reduce the change of the input position of the first substrate 410.

[0163] Here, when the vacuum degrees or pressures of the third turn module chamber T3 and the seventh passage chamber P7 are at the same level, the first substrate 410 is moved to the seventh passage chamber P7. And, while the vacuum degrees or pressures of the seventh passage chamber P7 and the sixth transfer chamber 361 are maintained at the same level, the gate valve is opened to move the first substrate 410 to the sixth transfer chamber 361. Here, the first substrate 410 is moved by using a robot.

[0164] Meanwhile, when the vacuum degree or pressure of the sixth transfer chamber 361 is at the same or substantially the same level as the vacuum degree or pressure of one of the plurality of second monomer deposition chambers for performing a monomer deposition process for forming the second organic layer 434, the gate valve is opened to move the display substrate 200 to the second monomer deposition chamber 362. Here, the method of forming the second organic layer 434 is similar to the method of forming the first organic layer 432, and thus a detailed description thereof will be omitted.

[0165] Meanwhile, when the second organic layer 434 reaches the target thickness, the first substrate 410 or the source unit is moved to the standby area to stop the injection of the process gas, and by controlling the conductance of the vacuum discharge system, the vacuum degree or pressure of the second monomer deposition chamber 362 is maintained at the same level as that of the sixth transfer chamber 361. Here, the first substrate 410 and the mask are separated from each other to move the first substrate 410 to a position where it can be discharged.

[0166] Meanwhile, after the first substrate 410 is moved from the second monomer deposition chamber 362 to the sixth transfer chamber 361, when the vacuum degree or pressure of the sixth transfer chamber 361 and the eighth channel chamber P8 are at the same or substantially the same level, the first substrate 410 is moved from the sixth transfer chamber 361 to the eighth channel chamber P8.

[0167] Again, when the vacuum degree or pressure of the eighth channel chamber P8 and the fourth rotation module chamber T4 is at the same level, the first substrate 410 is moved to the fourth rotation module chamber T4, and the first substrate 410 is rotated 180 degrees in the fourth rotation module chamber T4 to prevent or reduce the change of the input position of the first substrate 410.

[0168] And, when the above-mentioned process is completed, and the vacuum degree or pressure of the fourth turn module chamber T4 and the ninth passage chamber P9 is at the same level, the first substrate 410 is moved to the ninth passage chamber P9. And, during the vacuum degree or pressure of the ninth passage chamber P9 and the seventh transfer chamber 371 is maintained at the same or substantially the same level, the gate valve is opened to move the first substrate 410 to the seventh transfer chamber 371. Here, the first substrate 410 is moved by using a robot.

[0169] Meanwhile, when the above-mentioned processes are completed, and by controlling the conductance of the vacuum discharge system using the time and space division method, when the vacuum degree or pressure of the seventh transfer chamber 371 is at the same or substantially the same level as the vacuum degree or pressure of one of the plurality of second chemical vapor chambers 372 for performing the PECVD method for forming the third inorganic layer 435, the gate valve is opened to move the first substrate 410 to the second chemical vapor chamber 372. Here, the method of forming the third inorganic layer 435 after aligning the first substrate 410 and the mask is similar to the above-mentioned method of forming the second inorganic layer 233, and thus a detailed description thereof will be omitted.

[0170] Meanwhile, when the process is completed as the third inorganic layer 435 reaches the target thickness, the display substrate 400 and the mask are separated to move the display substrate 400 to a position where the display substrate 400 can be discharged or removed. At the same time, a valve installed in the high vacuum pump that controls conductance by a time and space control method is opened, and then the vacuum degree or pressure of the second chemical vapor chamber 372 is maintained at the same or substantially the same level as that of the seventh transfer chamber 371.

[0171] When the above processes are completed, the display substrate 400 is transferred from the second chemical vapor chamber 372 to the seventh transfer chamber 371. And, when the vacuum degrees or pressures of the seventh transfer chamber 371 and the tenth pass chamber P10 are at the same level, the display substrate 400 is moved from the seventh transfer chamber 371 to the tenth pass chamber P10.

[0172] Meanwhile, when the above processes are completed, the display substrate 400 is transferred from the tenth channel chamber P10 to the fifth rotation module chamber T5, and the display substrate 400 may be aligned by rotating 180 degrees in the fifth rotation module chamber T5, and then transferred to the eleventh channel chamber P11.

[0173] Here, the user completes the process by moving the display substrate 400 discharged from the eleventh channel chamber P11 to the outside. The display substrate 400 in the eleventh channel chamber P11 may be taken out using a robot arm.

[0174] Therefore, by using the thin film encapsulation manufacturing apparatus 300, the thickness of each layer can be controlled when forming a multi-layer film layer stacked using an organic layer and an inorganic layer, and the vacuum degree or pressure of a plurality of thin film process devices can be maintained at the same level by using a time and space division vacuum control method, and an in-line cluster can be formed. In addition, since an in-line cluster is formed in the thin film encapsulation manufacturing apparatus 300, sputtering, flash deposition, and PECVD can be performed in an in-line manner.

[0175] Figure 5 FIG. 5 is a conceptual diagram of a thin film encapsulation manufacturing apparatus 500 according to another embodiment of the present invention. Figure 6 For use Figure 5 5 is a cross-sectional view of a display substrate 600 manufactured by a thin film encapsulation manufacturing apparatus 500 .

[0176] Reference Figure 5 and Figure 6 The thin film encapsulation manufacturing equipment 500 may include a loading cluster (not shown), a first channel chamber P1, a first cluster 520, a second channel chamber P2, a first rotation module chamber T1, a third channel chamber P3, a second cluster 530, a fourth channel chamber P4, a second rotation module chamber T2, a fifth channel chamber P5, a third cluster 540, a sixth channel chamber P6, a third rotation module chamber T3, a seventh channel chamber P7, a fourth cluster 560, an eighth channel chamber P8, a fourth rotation module chamber T4, a ninth channel chamber P9, a fifth cluster 570, a tenth channel chamber P10, a fifth rotation module chamber T5, an eleventh channel chamber P11, a sixth cluster 580, a twelfth channel chamber P12, a sixth rotation module chamber T6, a thirteenth channel chamber P13, a seventh cluster 590, a fourteenth channel chamber P14, a seventh rotation module chamber T7, a fifteenth channel chamber P15 and an unloading cluster (not shown).

[0177] Here, the first channel chamber P1 to the fifteenth channel chamber P15 are based on the above reference Figure 1 and Figure 2 The described first to fourth passage chambers P1 to P4 are formed in the same or similar manner, and the display substrate 600 may also be transported in the same or similar method, and thus a detailed description thereof will be omitted.

[0178] And the first rotating module chamber T1 to the seventh rotating module chamber T5 are based on the above reference Figure 1 and Figure 2 The described first and second turning module chambers T1 and T2 are formed in the same or similar manner, and the display substrate 600 may also be conveyed in the same or similar method by aligning or inverting (flipping or reversing) the display substrate 600, and thus a detailed description thereof will be omitted.

[0179] At the same time, loading and unloading clusters are the same as above. Figure 1 and Figure 2 The same method described is formed, and therefore its detailed description will be omitted below. In addition, the loading cluster and the unloading cluster may or may not be included in the thin film encapsulation manufacturing apparatus 500, and therefore, for the convenience of description, the following description will focus on an embodiment that does not include the loading cluster and the unloading cluster.

[0180] The first cluster 520 may include a second transfer chamber 521, a first sputtering chamber 522, and a first mask storage chamber 523. The first cluster 520 is similar to the above reference Figure 1 and Figure 2 The same or similar methods are described herein and thus a detailed description thereof will be omitted.

[0181] Also, the second cluster 530 may include a third transfer chamber 531, a first monomer deposition chamber 532, and a second mask storage chamber 533. The second cluster 530 is similar to the above reference Figure 1 and Figure 2 The same or similar methods are described herein and thus a detailed description thereof will be omitted.

[0182] The third cluster 540 may include a fourth transfer chamber 541, a first chemical vapor chamber 542, and a second mask storage chamber 543. The third cluster 540 is based on the reference Figure 1 and Figure 2 The second inorganic layer 633 is formed by the same or similar method as described above, and thus a detailed description thereof will be omitted. However, for the convenience of description, the following description will focus on an embodiment in which the second inorganic layer 633 is formed in the first chemical vapor chamber 542 by using a PECVD method.

[0183] Meanwhile, the fourth cluster 560 may include a sixth transfer chamber 561, a second monomer deposition chamber 562, and a fourth mask storage chamber 563. Therefore, the fourth cluster 560 may form a second organic layer 634 on the second inorganic layer 633. The fourth cluster 560 may be formed in a similar manner to the second cluster 530, and the second organic layer 634 may be formed in the same manner as the first organic layer 632, and thus a detailed description thereof will be omitted.

[0184] The fifth cluster 570 may include a seventh transfer chamber 571, a second chemical vapor chamber 572, and a fifth mask storage chamber 573. The fifth cluster 570 may form a third inorganic layer 635 on the second organic layer 634. The fifth cluster 570 may be formed in a similar manner to the third cluster 540, and the third inorganic layer 635 may be formed in the same manner as the second inorganic layer 233, and thus a detailed description thereof will be omitted.

[0185] Meanwhile, the sixth cluster 580 may include an eighth transfer chamber 581, a third monomer deposition chamber 582, and a sixth mask storage chamber 583. The sixth cluster 580 may form a third organic layer 636 on the third inorganic layer 635. The sixth cluster 580 may be formed in a similar manner to the second cluster 530, and the third organic layer 636 may be formed in the same manner as the first organic layer 632, and thus a detailed description thereof will be omitted.

[0186] The seventh cluster 590 may include a ninth transfer chamber 591, a third chemical vapor chamber 592, and a seventh mask storage chamber 593. The seventh cluster 590 may form a fourth inorganic layer 637 on the third organic layer 636. The seventh cluster 590 may be formed in a similar manner to the third cluster 540, and the fourth inorganic layer 637 may be formed in a similar manner to the second inorganic layer 633, and thus a detailed description thereof will be omitted.

[0187] Meanwhile, hereinafter, a method of performing a thin film encapsulation process by using the thin film encapsulation manufacturing apparatus 500 and the display substrate 600 will be described in detail.

[0188] First, the display substrate 600 may be manufactured. In detail, the display substrate 600 may include a first substrate 610, an encapsulation unit 630, and a light emitting unit 620. Here, the first substrate 610 and the light emitting unit 620 are respectively Figure 1 and Figure 2 The above-mentioned first substrate 210 and the light emitting unit 220 are the same, and thus a detailed description thereof will be omitted.

[0189] Meanwhile, after preparing the first substrate 610 on which the light emitting unit 620 is formed, the first substrate 610 may be input into the thin film encapsulation manufacturing apparatus 500 to form an encapsulation unit 630. Here, the encapsulation unit 630 may include at least one sandwich structure in which at least one organic layer is inserted between at least two inorganic layers. Also, the encapsulation unit 630 may include a sandwich structure in which at least one inorganic layer is inserted between at least two organic layers.

[0190] For example, the encapsulation unit 630 may be formed by sequentially stacking the first inorganic layer 631 , the first organic layer 632 , the second inorganic layer 634 , the third inorganic layer 635 , the third organic layer 636 , and the fourth inorganic layer 637 as described above.

[0191] In detail, the first to third organic layers 632, 634, and 636 may be formed of a polymer, and may be a single layer or a laminate formed of one of polyethylene terephthalate, polyimide, polycarbonate, epoxy resin, polyethylene, and polyacrylate. In one embodiment, the first to third organic layers 632, 634, and 636 may be formed of polypropylene, and in detail, may include a monomer composition including a diacrylate monomer and a triacrylate monomer. The monomer composition may also include a monoacrylate monomer. In addition, a photoinitiator known in the art such as TPO may also be included in the monomer composition, but embodiments of the present invention are not limited thereto.

[0192] The first to fourth inorganic layers 631, 633, 635, and 637 may be a single layer or a stacked layer including metal oxide or metal nitride. In detail, the first to fourth inorganic layers 631, 633, 635, and 637 may include SiNx, Al 2 O 3 、SiO 2 、TiO 2 Here, the fourth inorganic layer 637 may be formed to prevent or reduce penetration of moisture with respect to the light emitting unit 620 .

[0193] Meanwhile, a metal halide layer including LiF may be further included between the light emitting unit 620 and the first inorganic layer 631. The metal halide layer may prevent or reduce damage to the light emitting unit 620 when the first inorganic layer 631 is formed by using a sputtering process.

[0194] Also, the first organic layer 632 is characterized in that it has a smaller surface area than the second inorganic layer 633, and the second organic layer 634 may also have a smaller surface area than the third inorganic layer 635. The third organic layer 636 may also have a smaller surface area than the fourth inorganic layer 637.

[0195] Furthermore, the first organic layer 632 is characterized in that it is completely covered by the second inorganic layer 633 , and the second organic layer 634 may also be completely covered by the third inorganic layer 635 . Furthermore, the third organic layer 636 may be completely covered by the fourth inorganic layer 637 .

[0196] The method of forming the encapsulation unit 630 as described above will be described in detail. By maintaining the vacuum degree or pressure of the entire thin film encapsulation manufacturing apparatus 500 at or below 5E-4Pa, masks in the first to fifth mask storage chambers 523, 533, 543, 563, and 573 can be transferred between the first sputtering chamber 522, the first monomer deposition chamber 532, the first chemical vapor chamber 542, the second monomer deposition chamber 562, and the second chemical vapor chamber 572, respectively, by using a robot arm.

[0197] When the above process is completed, the first inorganic layer 631, the first organic layer 632, the second inorganic layer 633, the second organic layer 634, and the third inorganic layer 635 may be formed on the light emitting unit 620. Here, the method of forming the first inorganic layer 631, the first organic layer 632, the second inorganic layer 633, the second organic layer 634, and the third inorganic layer 635 is the same as the above reference numerals. Figure 3 and Figure 4 The method is the same as that of , and thus a detailed description thereof will be omitted.

[0198] When the above-mentioned processes are completed, the first substrate 610 may be loaded from the fifth cluster 570 into the sixth cluster 580 after passing through the tenth pass chamber P10 , the fifth turn module chamber T5 , and the eleventh pass chamber P11 .

[0199] Here, in the sixth cluster 580, the third organic layer 636 may be formed on the third inorganic layer 635 by using a flash deposition process. Here, the operation method of the sixth cluster 580 is similar to the above-described second and fourth clusters 530 and 560, and thus a detailed description thereof will be omitted.

[0200] When the above-mentioned processes are completed, the first substrate 610 may be moved from the sixth cluster 580 to the seventh cluster 590 through the twelfth pass chamber P12 , the sixth turn module chamber T6 , and the thirteenth pass chamber P13 .

[0201] Here, in the seventh cluster 590, the fourth inorganic layer 637 may be formed on the third organic layer 636. In the seventh cluster 590, the fourth inorganic layer 637 may be formed using a PECVD method. In the above case, the seventh cluster 590 operates in a similar manner to the third cluster 540 and the fifth cluster 570, and thus a detailed description thereof will be omitted.

[0202] As described above, after the fourth inorganic layer 637 is formed, the display substrate 600 may be drawn out from the seventh cluster 590 to the outside through the fourteenth passage chamber P14 , the seventh turning module chamber T7 , and the fifteenth passage chamber P15 .

[0203] Meanwhile, the encapsulation unit 630 formed as described above is not limited thereto, and the first organic layer 632 and the second inorganic layer 633 may also be alternately formed on the first inorganic layer 631 .

[0204] Therefore, by using the thin film encapsulation manufacturing apparatus 500, when a stacked multi-layer film layer is formed using an organic layer and an inorganic layer, the thickness of each layer can be controlled, and the vacuum degree or pressure of a plurality of thin film process devices can be maintained at the same level by using a time and space division vacuum control method, and an in-line cluster can be formed. In addition, as the in-line cluster is formed in the thin film encapsulation manufacturing apparatus 500, sputtering, flash deposition, and PECVD can be performed in an in-line manner.

[0205] According to an embodiment of the present invention, when a multilayer stacked thin film of an organic layer and an inorganic layer is formed, the thickness of each layer can be controlled, and a cluster of in-line clusters can be formed by uniformly maintaining the vacuum degree or pressure of a variety of thin film manufacturing equipment using a time and space division vacuum control method. In addition, according to an embodiment of the present invention, by forming an in-line cluster, sputtering, flash deposition, and plasma enhanced chemical vapor deposition (PECVD) can be performed in an in-line manner.

[0206] While the invention has been particularly shown and described with reference to exemplary embodiments thereof, it will be understood by those skilled in the art that various changes in form and details may be made therein without departing from the spirit and scope of the invention as defined by the appended claims and their equivalents.

Claims

1. A thin film encapsulation manufacturing device, include: a first cluster configured to form a first inorganic layer on an opposing electrode of a display substrate using a sputtering process; a second cluster configured to form a first organic layer on the first inorganic layer on the display substrate using a monomer deposition process; as well as a third cluster configured to form a second inorganic layer on the first organic layer on the display substrate using a chemical vapor deposition process or a plasma enhanced chemical vapor deposition process, wherein the first cluster, the second cluster, and the third cluster are arranged in an order along one direction, and the first inorganic layer, the first organic layer, and the second inorganic layer are formed in the corresponding clusters in the same order, respectively; The thin film encapsulation manufacturing equipment further includes an unloading cluster coupled to the third cluster and configured to remove the display substrate transported from the third cluster. The unloading cluster includes a transfer chamber and a plurality of unloading chambers, the plurality of unloading chambers are radially mounted or coupled to the transfer chamber, and the display substrate entering the unloading cluster is a completed display substrate, and the completed display substrate is transported from the transfer chamber to one of the plurality of unloading chambers. wherein each of the unloading chambers is configured to store the completed display substrates entering the unloading cluster randomly or in a predetermined order therein when the completed display substrates do not exist therein; wherein the first cluster and the second cluster form the first inorganic layer and the first organic layer respectively using a downward deposition method, and the third cluster forms the second inorganic layer using an upward deposition method, The thin film encapsulation manufacturing equipment further includes a first flip chamber coupled to the second cluster and the third cluster, the first flip chamber flips the display substrate and transports the display substrate from the second cluster to the third cluster, and The thin film encapsulation manufacturing equipment further includes a second inversion chamber coupled to the third cluster and the unloading cluster, and the second inversion chamber inverts the display substrate and transports the display substrate from the third cluster to the unloading cluster.

2. The thin film encapsulation manufacturing equipment according to claim 1, in, The first cluster, the second cluster, and the third cluster each include a plurality of process chambers.

3. The thin film encapsulation manufacturing equipment according to claim 2, in, The order of the multiple process chambers of the first cluster, the multiple process chambers of the second cluster, and the multiple process chambers of the third cluster are arranged along one direction, and the first inorganic layer, the first organic layer, and the second inorganic layer are respectively formed in the corresponding process chambers in the same order.

4. The thin film encapsulation manufacturing equipment according to claim 1, in, At least one of the first cluster, the second cluster, and the third cluster includes a mask storage chamber.

5. The thin film encapsulation manufacturing equipment according to claim 1, further comprising: include: A fourth cluster is coupled between the third cluster and the unloading cluster and is configured to form a second organic layer on the second inorganic layer on the display substrate using a monomer deposition process.

6. The thin film encapsulation manufacturing equipment according to claim 5, further comprising: include: A fifth cluster is coupled between the fourth cluster and the unloading cluster and is configured to form a third inorganic layer on the second organic layer on the display substrate using a chemical vapor deposition method or a plasma enhanced chemical vapor deposition method.

7. The thin film encapsulation manufacturing equipment according to claim 1, in, The second clusters and the third clusters are installed alternately.

8. The thin film encapsulation manufacturing equipment according to claim 1, further comprising at least one of the following chambers: a channel chamber located between the first cluster and the second cluster and configured to transport the display substrate; and A rotation module chamber is coupled to the second cluster and configured to align an input direction of the display substrate.

9. The thin film encapsulation manufacturing equipment according to claim 1, further comprising: include: a first plurality of channel chambers located between the first cluster and the second cluster and configured to transport the display substrate; and A first rotating module chamber is configured to align the input direction of the display substrate, Wherein, the first plurality of channel chambers are coupled to opposite sides of the first rotation module chamber to couple the first cluster to the second cluster.

10. The thin film encapsulation manufacturing equipment according to claim 9, in, When the display substrate is conveyed, the internal pressures of the first cluster and one of the first plurality of channel chambers are controlled to be the same, the internal pressures of one of the first plurality of channel chambers and the first rotation module chamber are controlled to be the same, the internal pressures of the first rotation module chamber and another channel chamber of the first plurality of channel chambers are controlled to be the same, or the internal pressures of another channel chamber of the first plurality of channel chambers and the second cluster are controlled to be the same.

11. The thin film encapsulation manufacturing equipment according to claim 1, further comprising at least one of the following chambers: a channel chamber located between the second cluster and the third cluster and configured to transport the display substrate; and A rotation module chamber is coupled to the second cluster and configured to align an input direction of the display substrate.

12. The thin film encapsulation manufacturing equipment according to claim 1, further comprising: include: a second plurality of channel chambers located between the second cluster and the third cluster and configured to transport the display substrate; and The second rotating module chamber is configured to align the input direction of the display substrate, Wherein, the second plurality of channel chambers are coupled to opposite sides of the second rotation module chamber to couple the second cluster to the third cluster.

13. The thin film encapsulation manufacturing equipment according to claim 12, in, When the display substrate is conveyed, the internal pressures of the second cluster and one of the second plurality of channel chambers are controlled to be the same, the internal pressures of one of the second plurality of channel chambers and the second rotation module chamber are controlled to be the same, the internal pressures of the second rotation module chamber and another channel chamber of the second plurality of channel chambers are controlled to be the same, or the internal pressures of another channel chamber of the second plurality of channel chambers and the third cluster are controlled to be the same.

14. The thin film encapsulation manufacturing equipment according to claim 1, further comprising: include: The loading cluster is configured to receive the display substrate from the outside and transport the display substrate to the first cluster.

15. A method for manufacturing a thin film package, include: forming a first inorganic layer on an opposite electrode of a display substrate using a sputtering process; forming a first organic layer on the first inorganic layer using a monomer deposition process; as well as forming a second inorganic layer on the first organic layer using a chemical vapor deposition process or a plasma enhanced chemical vapor deposition process, The order of the first cluster, the second cluster, and the third cluster is arranged along one direction, and in the same order: forming the first inorganic layer in the first cluster, forming the first organic layer in the second cluster, and forming the second inorganic layer in the third cluster, The method further comprises, after forming the second inorganic layer, removing the display substrate by unloading a cluster, The unloading cluster includes a transfer chamber and a plurality of unloading chambers, the plurality of unloading chambers are radially mounted or coupled to the transfer chamber, and the display substrate entering the unloading cluster is a completed display substrate, and the completed display substrate is transported from the transfer chamber to one of the plurality of unloading chambers. wherein each of the unloading chambers is configured to store the completed display substrates entering the unloading cluster randomly or in a predetermined order therein when the completed display substrates do not exist therein; wherein the first inorganic layer and the first organic layer are formed using a downward deposition method, and the second inorganic layer is formed using an upward deposition method, wherein after forming the first inorganic layer and the first organic layer, the display substrate is reversed before forming the second inorganic layer, and Wherein, after forming the second inorganic layer, the display substrate is reversed before entering the unloading cluster.

16. The method of claim 15, in, The first inorganic layer, the first organic layer, and the second inorganic layer are respectively formed in a first cluster including a first plurality of process chambers, a second cluster including a second plurality of process chambers, and a third cluster including a third plurality of process chambers.

17. The method of claim 16, in, The first plurality of process chambers, the second plurality of process chambers, and the third plurality of process chambers are arranged in order along one direction, and a first inorganic layer, a first organic layer, and a second inorganic layer are respectively formed in the corresponding process chambers in the same order.

18. The method of claim 15, in, At least one of the first cluster, the second cluster, and the third cluster includes a mask storage chamber configured to store a mask.

19. The method of claim 15, in, The display substrate is transported from the first cluster to the second cluster via at least one of the following chambers: a channel chamber located between the first cluster and the second cluster and configured to transport the display substrate; and A rotation module chamber is coupled to the second cluster and configured to align an input direction of the display substrate.

20. The method of claim 15, further comprising: include: A first plurality of channel chambers are coupled to opposite sides of a first rotation module chamber between the first cluster and the second cluster such that the coupled first plurality of channel chambers and the coupled first rotation module chambers couple the first cluster to the second cluster.

21. The method of claim 20, in, When the display substrate is conveyed, the internal pressures of the first cluster and one of the first plurality of channel chambers are controlled to be the same, the internal pressures of one of the first plurality of channel chambers and the first rotation module chamber are controlled to be the same, the internal pressures of the first rotation module chamber and another channel chamber of the first plurality of channel chambers are controlled to be the same, or the internal pressures of another channel chamber of the first plurality of channel chambers and the second cluster are controlled to be the same.

22. The method of claim 15, in, The display substrate is transferred from the second cluster to the third cluster via at least one of the following chambers: a channel chamber coupled between the second cluster and the third cluster and configured to transport the display substrate; and A rotating module chamber is configured to align with an input direction of the display substrate.

23. The method of claim 15, further comprising: include: A second plurality of channel chambers are coupled to opposite sides of a second rotation module chamber between the second cluster and the third cluster such that the coupled second plurality of channel chambers and the coupled second rotation module chambers couple the second cluster to the third cluster.

24. The method of claim 23, in, When the display substrate is conveyed, the internal pressures of the second cluster and one of the second plurality of channel chambers are controlled to be the same, the internal pressures of one of the second plurality of channel chambers and the second rotation module chamber are controlled to be the same, the internal pressures of the second rotation module chamber and another channel chamber of the second plurality of channel chambers are controlled to be the same, or the internal pressures of another channel chamber of the second plurality of channel chambers and the third cluster are controlled to be the same.

25. The method of claim 15, in, The formation of the first organic layer and the formation of the second inorganic layer are alternately performed a plurality of times, and finally the display substrate is removed by the unloading cluster.

26. The method of claim 15, further comprising: include: Before forming the first inorganic layer, the display substrate is received from the outside by a loading cluster.

Citation Information

Patent Citations

  • Apparatus for depositing a multilayer coating on discrete sheets

    CN101167160A

  • Processing device and method for processing a subtrate

    CN101431004A

  • Light-emitting device and method for manufacturing light-emitting device

    CN101467493A

  • Organic electroluminescence device and multi-color display apparatus using the same

    CN102074659A

  • Producing device

    CN1458666A