A high-strength bioactive intervertebral fusion device and a manufacturing method thereof
By adopting a high-strength bioactive intervertebral fusion cage with a multi-layer structure, combined with the design of soft materials and porous structures, the problems of insufficient biocompatibility and stability in the existing technology are solved, and bone regeneration and multi-dimensional fusion in the body are achieved. Functional, reduces the risk of wear and improves ease of operation and cost-effectiveness.
Patent Information
- Application Number
- CN202011599971.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-12-30
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2040-12-30
AI Technical Summary
Existing intervertebral fusion cages have deficiencies in biocompatibility, bone fusion, and intervertebral space stability, and the delayed inflammatory reaction and wear problems of materials are more prominent.
It adopts a high-strength bioactive intervertebral fusion device composed of an outer layer, a middle layer and an inner layer. The outer layer is made of soft material, the middle layer is a porous structure, and the inner layer is a combination of bioactive materials with a porous structure. By adjusting the porosity and pore size and pore morphological structure, combined with 3D printing technology to ensure the biocompatibility and mechanical properties of the material.
It achieves biological activity in the body, promotes bone regeneration and repair, reduces the risk of wear, has multiple functions and meets complex application requirements, is simple to operate and has low cost.
Smart Images

Figure CN112451185B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a device in the technical field of medical devices and a manufacturing method thereof, and in particular to a high-strength bioactive intervertebral fusion device and a manufacturing method thereof. Background Art
[0002] With the aging of the population, spinal degenerative diseases with neck and shoulder pain and low back and leg pain as the main symptoms are seriously affecting people's work and life. Intervertebral fusion between vertebrae is currently one of the main methods for treating spinal degenerative diseases. Through the unremitting efforts of researchers, different types of intervertebral fusion devices have been developed and gradually applied in clinical practice. The ideal intervertebral fusion device needs to be able to correct spinal deformity, restore normal physiological curvature, maintain the stability of the intervertebral space, and most importantly, promote bone fusion. However, the current fusion devices still have many shortcomings, such as poor biocompatibility of fusion device materials, intervertebral space collapse, delayed inflammatory response, etc.
[0003] With the development of disciplines such as mechanics, materials science, and tissue engineering, researchers are conducting multidisciplinary research on new intervertebral fusion devices. However, no matter how the material of the fusion device changes, it must meet the following requirements: the fusion device has no toxic side effects in the human body and has good biocompatibility; it has suitable biomechanical characteristics; it must ensure the stability of the intervertebral space and promote bone fusion; after implantation into the human body, it must have a larger fusion area with the upper and lower vertebrae and be closer to the normal physiological curvature of the human body in structure. Summary of the invention
[0004] In view of the above-mentioned deficiencies in the prior art, the present invention provides a high-strength bioactive intervertebral fusion cage and a manufacturing method thereof.
[0005] To achieve the above object, the technical solution adopted by the present invention is as follows: a high-strength bioactive intervertebral fusion device, the intervertebral fusion device is composed of three parts: an outer layer, a middle layer and an inner layer, the middle layer is wrapped inside the outer layer, and the inner layer is installed inside the middle layer;
[0006] The outer layer is a soft material, which may be hydrogel or silica gel;
[0007] The middle layer has a porous structure with completely connected internal channels, and can be made of titanium alloy or PEEK;
[0008] The inner layer is a combination of two or more porous bioactive materials with completely connected internal channels. It can be a combination of calcium magnesium silicate, silicate, or phosphate, etc., or it can be a bioactive material with some special functions, such as inhibiting tumor growth, promoting osteogenesis, and promoting vascularization.
[0009] Preferably, the middle layer of the high-strength bioactive intervertebral fusion device includes an entry port and a track, the inner layer enters the middle layer through the entry port, the inner layer is movably mounted on the track, and the entire structure of the middle layer can be hollowed out according to the needs of the application scenario. By optimizing the topological structure of the entire structure, the fusion device can be made lighter while meeting the use requirements. The function of the middle layer is to withstand external loads.
[0010] Preferably, the porosity of the intermediate layer is 30-60%, the pore size is 50-500 microns, and the pore morphology structure can be square, rectangular, parallelogram, spherical, etc.;
[0011] Preferably, the entrance and the track in the middle layer form a unit, and the unit can be one, two, or more. In actual application, the number of units is determined according to the structure of the middle layer and the required number of inner layers, and the position of the unit inside the middle layer is determined by the structure of the middle layer.
[0012] Preferably, the porosity of the inner layer of the high-strength bioactive intervertebral fusion device is 30-90%, the pore size is 200-1000 microns, the thickness is 0.3-5 mm, the pore shape structure can be a grid square, rectangle, parallelogram, etc., and the inner layer structure can be a plurality of bioactive materials.
[0013] Preferably, the outer shape of the inner layer of the high-strength bioactive intervertebral fusion device is the same as the shape of the entrance of the middle layer, which can be a triangle, a circle, etc. The outer shape of the inner layer matches the cross-sectional shape of the track, and the size of the inner layer is slightly smaller than the size of the entrance, and the inner layer can enter the interior of the middle layer through the entrance. Through the design of the special structure of the entrance, the inner layer can only reach the interior of the middle layer through the entrance in a certain position state. When the inner layer enters the interior of the middle layer, the inner layer will match the track in the middle layer to ensure that the inner layer is in a relatively stable position state in the middle layer. For example, when the shape of the inner layer is a triangle, the cross-sectional shape of the track is V-shaped, and when the shape of the inner layer is a circle, the cross-sectional shape of the track is semicircular. When multiple inner layers enter the track, the inner layer will move horizontally on the track and it is difficult to come out of the entrance, ensuring that the inner layer is always inside the middle layer.
[0014] In actual application, by wrapping the outer layer outside the middle layer, the hard material can be prevented from directly contacting the surrounding hard bone and causing wear. By adjusting the porosity, pore size and pore morphology of the middle layer, the mechanical strength of the middle layer can be adjusted. By adjusting the porosity, pore size, pore morphology of the inner layer and the porosity of the middle layer, the degradation rate of the biomaterial and the ion release rate can be controlled. By adjusting the number of inner layers or the number of materials with the same structure in a unit, the amount of ion release can be controlled to make the fusion device have better functions. By adjusting the material of the inner layer, the fusion device can have different functions or integrate multiple functions, such as inhibiting tumors, promoting vascularization, promoting bone regeneration, etc.
[0015] Preferably, the present invention relates to a method for manufacturing the above-mentioned high-strength bioactive intervertebral fusion cage, comprising the following steps:
[0016] 1) Select the material types of the middle layer, outer layer and inner layer according to the application;
[0017] 2) Design the structure of the middle layer according to the application and the material properties of the middle layer, and then use the equipment to manufacture the middle layer;
[0018] 3) Design the structure of the outer layer according to the structure of the middle layer and the material properties of the outer layer, and then manufacture the outer layer;
[0019] 4) Design the structure of the inner layer according to the application and the material properties of the inner layer, mix the inner layer material with the solvent to obtain uniformly dispersed bio-ink, and then use 3D printing equipment to manufacture multiple inner layer blanks;
[0020] 5) The inner layer blanks are placed in a high temperature furnace for high temperature calcination, and multiple inner layer structures are obtained after cooling;
[0021] 6) placing the multiple inner layer structures sequentially through the entrance of the middle layer onto the track;
[0022] 7) The intermediate layer structure containing the inner layer is wrapped with an outer layer to obtain a high-strength bioactive intervertebral fusion device.
[0023] Preferably, the calcination temperature is 950 o C-1150 o C, heating rate is 1-3 oC / min, insulation time 1-6 hours.
[0024] Compared with the prior art, the present invention has the following advantages:
[0025] 1. The high-strength bioactive intervertebral fusion device manufactured by the present invention has a soft surface structure and is not easily worn with the contact parts.
[0026] 2. The high-strength bioactive intervertebral fusion device manufactured by the present invention has good bioactivity in the body and can promote bone regeneration and repair.
[0027] 3. The present invention can manufacture a high-strength bioactive intervertebral fusion device with multiple functions to meet the complex and changeable practical application needs.
[0028] Fourth, the method for manufacturing a high-strength bioactive intervertebral fusion cage of the present invention is easy to operate and has low manufacturing cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 It is a schematic diagram of the manufacturing process of the high-strength bioactive intervertebral fusion device of the present invention;
[0030] Figure 2 It is a schematic diagram of the structure of the high-strength bioactive intervertebral fusion device of the present invention;
[0031] Figure 3 It is a partial structural schematic diagram of a high-strength bioactive intervertebral fusion device of the present invention. DETAILED DESCRIPTION
[0032] The following is a detailed description of an embodiment of the present invention. This embodiment is implemented on the premise of the technical solution of the present invention, and a detailed implementation method and a specific operation process are given, but the protection scope of the present invention is not limited to the following embodiment.
[0033] like Figure 2 As shown, the present invention provides a high-strength bioactive intervertebral fusion device, which is composed of an outer layer, a middle layer and an inner layer. The middle layer is wrapped inside the outer layer, and the inner layer is installed inside the middle layer.
[0034] The outer layer is made of soft material, which may be hydrogel or silica gel;
[0035] The above-mentioned middle layer is a porous structure with completely connected internal channels, and can be a titanium alloy or PEEK (polyetheretherketone), etc.;
[0036] The inner layer is a combination of two or more porous bioactive materials with completely connected internal pores. It can be a combination of calcium magnesium silicate, silicate, or phosphate, etc., or it can be a bioactive material with some special functions, such as inhibiting tumor growth, promoting osteogenesis, and promoting vascularization.
[0037] The middle layer of the high-strength bioactive intervertebral fusion device includes an entry port and a track. The inner layer enters the middle layer through the entry port. The inner layer is movably mounted on the track. The entire structure of the middle layer can be hollowed out according to the needs of the application. By optimizing the topological structure of the entire structure, the fusion device can be made lighter while meeting the use requirements. The function of the middle layer is to withstand external loads.
[0038] The porosity of the intermediate layer is 30-60%, the pore size is 50-500 microns, and the pore morphology can be square, rectangular, parallelogram, spherical, etc.;
[0039] The entrance and the track in the middle layer form a unit, and the unit can be one, two, or more. In actual application, the number of units is determined according to the structure of the middle layer and the required number of inner layers, and the position of the unit inside the middle layer is determined by the structure of the middle layer.
[0040] The inner layer of the high-strength bioactive intervertebral fusion device has a porosity of 30-90%, a pore size of 200-1000 microns, a thickness of 0.3-5 mm, and a pore shape structure of grid squares, rectangles, parallelograms, etc. The inner layer structure can be a plurality of bioactive materials.
[0041] The outer shape of the inner layer of the high-strength bioactive intervertebral fusion device is the same as the shape of the entrance of the middle layer, which can be a triangle, a circle, etc. The outer shape of the inner layer matches the cross-sectional shape of the track. The size of the inner layer is slightly smaller than the size of the entrance, and the inner layer can enter the middle layer through the entrance. Through the design of the entrance structure, the inner layer can only reach the middle layer through the entrance in a certain position. When the inner layer enters the middle layer, the inner layer will match the track in the middle layer to ensure that the inner layer is in a relatively stable position in the middle layer. For example, when the shape of the inner layer is a triangle, the cross-sectional shape of the track is V-shaped. When the shape of the inner layer is a circle, the cross-sectional shape of the track is semicircular. When multiple inner layers enter the track, the inner layer will move horizontally on the track and it is difficult to come out of the entrance, ensuring that the inner layer is always inside the middle layer.
[0042] In actual application, by wrapping the outer layer outside the middle layer, the hard material can be prevented from directly contacting the surrounding hard bone and causing wear. By adjusting the porosity, pore size and pore morphology of the middle layer, the mechanical strength of the middle layer can be adjusted. By adjusting the porosity, pore size, pore morphology of the inner layer and the porosity of the middle layer, the degradation rate of the biomaterial and the ion release rate can be controlled. By adjusting the number of inner layers or the number of materials with the same structure in a unit, the amount of ion release can be controlled to make the fusion device have better functions. By adjusting the material of the inner layer, the fusion device can have different functions or integrate multiple functions, such as inhibiting tumors, promoting vascularization, promoting bone regeneration, etc.
[0043] like Figure 1 FIG. 1 is a schematic diagram of a manufacturing method of a high-strength bioactive intervertebral fusion device according to the present invention, which includes the following steps:
[0044] 1) Select the material types of the middle layer, outer layer and inner layer according to the application;
[0045] 2) Design the structure of the middle layer according to the application and the material properties of the middle layer, and then use the equipment to manufacture the middle layer;
[0046] 3) Design the structure of the outer layer according to the structure of the middle layer and the material properties of the outer layer, and then manufacture the outer layer;
[0047] 4) Design the structure of the inner layer according to the application and the material properties of the inner layer, mix the inner layer material with the solvent to obtain uniformly dispersed bio-ink, and then use 3D printing equipment to manufacture multiple inner layer blanks;
[0048] 5) The inner layer blanks are placed in a high temperature furnace for high temperature calcination, and multiple inner layer structures are obtained after cooling;
[0049] 6) placing the multiple inner layer structures sequentially through the entrance of the middle layer onto the track;
[0050] 7) The intermediate layer structure containing the inner layer is wrapped with an outer layer to obtain a high-strength bioactive intervertebral fusion device.
[0051] The calcination temperature is 950 o C-1150 o C, heating rate is 1-3 oC / min, insulation time 1-6 hours.
[0052] Example 1
[0053] The manufacturing method of the intervertebral fusion cage with anti-tumor, osteogenic and vascularization promoting functions for lumbar intervertebral fusion is as follows:
[0054] 1) Titanium alloy is selected as the material of the middle layer, silicone is selected as the material of the outer layer, calcium magnesium silicate with a magnesium content of 1.6% is selected as the inner layer material A, calcium silicate material containing strontium is selected as the inner layer material B, calcium silicate material containing copper is selected as the inner layer material C, and calcium silicate material with anti-tumor drugs is selected as the inner layer material D;
[0055] 2) The outer contour of the titanium alloy middle layer is designed according to the mechanical properties required by the intervertebral fusion device and the material properties of the titanium alloy. The internal porosity is 30%, the pore diameter is 100 microns, and the pore morphology is a grid-type. There are two units in the middle layer, which are arranged at the top and bottom of the middle layer respectively. The shape of the entrance is triangular, and the cross-sectional shape of the track is V-shaped. Then, the designed middle layer structure model is imported into the metal 3D printing equipment, and the titanium alloy middle layer structure is obtained by stacking layers through the selective laser melting process;
[0056] 3) According to the upper and lower surface structures of the middle layer and the material properties of silicone, the structure of the outer layer is designed to be the same as the upper and lower surface structures of the middle layer, and the size is slightly smaller than the upper and lower surface structures of the middle layer, to ensure that the silicone can be firmly wrapped outside the middle layer, and then the silicone outer layer structure is manufactured by casting;
[0057] 4) According to the anti-tumor properties, bone regeneration properties, pro-vascularization properties and repair properties required by the application, as well as the properties of the four materials, four structures of the inner layer are designed respectively. The porosity of the inner layer A is 60%, the pore size is 500 microns, and the pore morphology is a grid square. The porosity of the inner layer B is 50%, the pore size is 400 microns, and the pore morphology is a grid square. The porosity of the inner layer C is 50%, the pore size is 400 microns, and the pore morphology is a grid square. The porosity of the inner layer D is 60%, the pore size is 700 microns, and the pore morphology is a grid square. The shapes of the four inner layers are all the same triangle as the entrance, but the size is 0.5 mm smaller than the entrance. The shape and size of the inner layer are just matched with the cross-sectional shape and size of the track. The four inner layer materials are mixed with solvents to obtain uniformly dispersed bio-inks A, B, C and D. The structural model of the inner layer is imported into the 3D printing device, and then the 3D printing device is used to stack layers to obtain inner layer blanks A, B, C and D respectively.
[0058] 5) Place the inner layer blank A in a high temperature furnace and heat it at 1150 o C high temperature calcination for 4 hours, after cooling to obtain the inner layer A, the inner layer blank B is placed in a high temperature furnace, and heated at 1100 o C was calcined at high temperature for 4 hours, and then cooled to obtain the inner layer B. The inner layer blank C was placed in a high temperature furnace and heated at 1100 o C was calcined at high temperature for 4 hours, and then cooled to obtain the inner layer C. The inner layer blank D was placed in a high temperature furnace and heated at 1100 oC is calcined at high temperature for 4 hours, and then cooled to obtain the inner layer D, and then the inner layer D is immersed in a solution containing anti-tumor drugs, and the immersion is repeated several times, and the inner layer D loaded with anti-tumor drugs is obtained after drying;
[0059] 6) Place an inner layer D onto the track through the entrance on the upper surface of the middle layer, then tilt the middle layer to allow the inner layer D to move along the track to the other end of the track, then lay the middle layer flat and allow the inner layer A to be placed onto the track through the entrance, then tilt the middle layer again to allow the inner layer A to move to the other end of the track to contact the inner layer D, and continue the operation, placing the inner layers C, B, B, C, A and D in sequence, until the eight inner layer structures are located on the track on the upper surface of the middle layer in the order of DACBBCAD, then flip the middle layer over and add the inner layer structure to the entrance on the lower surface of the middle layer, and the operation process of adding the inner layer structure on the upper surface is the same, until the track on the lower surface is filled with eight inner layer structures, and finally a middle layer with eight inner layer structures on the upper and lower surfaces is obtained;
[0060] 7) The upper surface and the outer surface of the intermediate layer obtained in step 6) are respectively wrapped with the silica gel obtained in step 3) to obtain a high-strength bioactive intervertebral fusion device. The structural schematic diagram of the key parts is shown in FIG. Figure 3 shown.
Claims
1. A high-strength bioactive intervertebral fusion cage, characterized in that: The intervertebral fusion cage is composed of an outer layer, a middle layer and an inner layer. The middle layer is wrapped inside the outer layer, and the inner layer is installed inside the middle layer. The outer layer is a soft material, such as hydrogel or silica gel; The middle layer has a porous structure, and the internal pores are completely connected, and is made of titanium alloy or PEEK; The inner layer is a combination of two or more porous bioactive materials, the internal pores are completely connected, and the inner layer is silicate, phosphate or a combination of the two, or the bioactive material has special functions, including inhibiting tumor growth, promoting angiogenesis and promoting osteogenesis; The middle layer of the high-strength bioactive intervertebral fusion device comprises an entry port and a track, the inner layer enters the middle layer through the entry port, and the inner layer is movably mounted on the track; multiple inner layer structures are sequentially placed on the track through the entry port of the middle layer; The porosity of the intermediate layer is 30-60%, the pore size is 50-500 microns, and the pore morphology is square, rectangular, parallelogram or spherical; The entrance and the track in the middle layer form a unit, and there is at least one unit; The outer shape of the inner layer of the high-strength bioactive intervertebral fusion device is the same as the shape of the entrance port of the middle layer; the outer shape of the inner layer matches the cross-sectional shape of the track, the size of the inner layer is slightly smaller than the size of the entrance port, and the inner layer can enter the interior of the middle layer through the entrance port.
2. The high-strength bioactive intervertebral fusion cage according to claim 1, characterized in that: The inner layer of the high-strength bioactive intervertebral fusion device has a porosity of 30-90%, a pore size of 200-1000 microns, a thickness of 0.3-5 mm, and a pore morphology of a grid square, rectangle or parallelogram.
3. A method for manufacturing a high-strength bioactive intervertebral fusion cage according to claim 1, characterized in that: The following steps are involved: 1) Select the material types of the middle layer, outer layer and inner layer according to the application; 2) Design the structure of the middle layer according to the application and the material properties of the middle layer, and then use the equipment to manufacture the middle layer; 3) Design the structure of the outer layer according to the structure of the middle layer and the material properties of the outer layer, and then manufacture the outer layer; 4) Design the structure of the inner layer according to the application and the material properties of the inner layer, mix the inner layer material with the solvent to obtain uniformly dispersed bio-ink, and then use 3D printing equipment to manufacture multiple inner layer blanks; 5) The inner layer blanks are placed in a high temperature furnace for high temperature calcination, and multiple inner layer structures are obtained after cooling; 6) placing the multiple inner layer structures sequentially through the entrance of the middle layer onto the track; 7) The intermediate layer structure containing the inner layer is wrapped with an outer layer to obtain a high-strength bioactive intervertebral fusion device.
4. The method for manufacturing a high-strength bioactive intervertebral fusion cage according to claim 3, characterized in that: The calcination temperature is 950°C-1150°C, the heating rate is 1-3°C / min, and the holding time is 1-6 hours.