Electronic components
By controlling the position and thickness of the marker in the electronic components, the maximum height does not exceed the height of the insulating film, the problem of easy peeling and insufficient visibility of the marker is solved, high visibility and peeling suppression are achieved, and installation is improved Accuracy.
Patent Information
- Application Number
- CN202011040342.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-09-30
- Filing Date
- 2020-09-28
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2040-09-28
AI Technical Summary
The markers of the existing electronic components are easily peeled off in the manufacturing process, the handling process and the installation process, and the visibility is insufficient.
By controlling the position and thickness of the marker, the maximum height (Mmax) of the marker does not exceed the maximum height (Imax) of the insulating film, so as to improve the visibility of the marker and inhibit its peeling.
High visibility of markers and stripping inhibition are achieved, and the installation accuracy of electronic components is improved.
Smart Images

Figure CN112582150B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to electronic components. Background Art
[0002] Conventionally, markers are provided on electronic components such as coil components for the purpose of identifying positions and / or directions.
[0003] Patent document 1 discloses a stacked inductor, characterized in that a spiral coil conductor is provided in a rectangular chip obtained by stacking and firing a plurality of sheet layers, and marker layers for indicating the position of the lead-out portion of the coil conductor are provided on the inner side of the upper sheet layer and the inner side of the lower sheet layer constituting the chip, respectively, each marker layer forms a rectangular shape having the same width as the chip, two sides of each marker layer on the chip side are exposed on the two side surfaces of the chip, and one side on the chip end surface side is located on the inner side at a specified distance from the chip end surface.
[0004] Prior art literature
[0005] Patent Literature
[0006] Patent Document 1: Japanese Patent Application Publication No. 2005-166745 Summary of the invention
[0007] The marking of electronic components is required to have higher visibility. In addition, it is desired that the marking is not easily peeled off during the manufacturing process of the electronic components, the conveying process of the electronic components as finished products, and the mounting process of the electronic components.
[0008] Therefore, an object of the present invention is to provide an electronic component including a marker having high visibility and suppressed peeling.
[0009] As a result of repeated studies, the present inventors have found that by controlling the position at which a marker is arranged in an electronic component and the thickness of the marker, the visibility of the marker is improved and the peeling of the marker is suppressed, thereby completing the present invention.
[0010] According to one aspect of the present invention, there is provided an electronic component comprising: a unit body (element body) having a conductor inside, an insulating film and at least one marker arranged on a surface of the unit body, and an external electrode arranged on the unit body or the insulating film.
[0011] The marker is exposed on the surface of the electronic component.
[0012] When the maximum height of the marker on the surface of the unit body where the marker is arranged is set to M max , set the maximum height of the insulating film to I max When M max and I max Satisfies the following formula:
[0013] M max ≤I max .
[0014] According to the electronic component of the present invention, the visibility of the marker can be improved and the peeling of the marker can be suppressed. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a partial cross-sectional view schematically showing the marker of the electronic component according to the first embodiment of the present invention.
[0016] Figure 2 It is a partial cross-sectional view schematically showing the maximum height of the marker and the maximum height of the insulating film.
[0017] Figure 3 It is a partial cross-sectional view schematically showing a marker of an electronic component according to a second embodiment of the present invention.
[0018] Figure 4 This is a partial cross-sectional view schematically showing a conventional marker.
[0019] Figure 5 This is an optical microscope image of a cross section of the electronic component of the present invention.
[0020] Explanation of symbols
[0021] 10 Unit
[0022] 11 Metal magnetic powder
[0023] 12 Resin
[0024] 20 Insulation film
[0025] 21 Insulation materials
[0026] 30 markers DETAILED DESCRIPTION
[0027] Hereinafter, electronic components according to embodiments of the present invention will be described in detail with reference to the drawings. However, the embodiments described below are for illustrative purposes only, and the present invention is not limited to the following embodiments.
[0028] The various numerical ranges mentioned in this specification are intended to include the lower and upper limits themselves. The words "above" and "below" of course include the numerical values themselves. Even if "above" and "below" are not attached, the numerical values themselves are also included unless otherwise specified. For example, taking the numerical range of 1 to 10 as an example, it is interpreted as including the lower limit "1" and the upper limit "10".
[0029] [First embodiment]
[0030] An electronic component according to a first embodiment of the present invention includes a unit body including a conductor therein, an insulating film and at least one marker disposed on a surface of the unit body, and an external electrode disposed on the unit body or the insulating film. Figure 1 is a partial cross-sectional view schematically showing the shape and configuration of the marker. Figure 1 As shown, the insulating film 20 and at least one marker 30 are arranged on the surface of the unit body 10. Hereinafter, the electronic component is mainly described as a coil component such as an inductor, but the electronic component of this embodiment is not limited to the coil component, and the present invention can be applied to various electronic components.
[0031] The marker 30 is exposed on the surface of the electronic component. When the maximum height of the marker 30 on the surface of the unit cell 10 on which the marker 30 is arranged is set to M max , the maximum height of the insulating film 20 is set to I max When M max and I max The following formula is satisfied.
[0032] M max ≤I max
[0033] Here, the maximum height M of the marker 30 on the surface of the unit cell 10 is max It refers to the height of the marker 30 at the position where the height of the marker 30 from the surface of the unit cell 10 is the maximum in the cross-sectional view (a cross-sectional view in a direction perpendicular to the surface of the unit cell 10 where the marker 30 is arranged). Similarly, the maximum height I of the insulating film 20 on the surface of the unit cell 10 is max It refers to the height of the insulating film 20 at the position where the height of the insulating film 20 from the surface of the unit cell 10 is the maximum in the cross-sectional view. More specifically, Figure 2 As shown, the maximum height M of the marker 30 max It refers to the height of the position where the height (distance) of the surface of the marker 30 from the surface of the unit body 10 is the maximum (indicated by the symbol (a)). Similarly, the maximum height I of the insulating film 20 max It refers to the height of the position where the height (distance) from the surface of the insulating film 20 to the surface is the maximum on the surface of the unit cell 10 where the insulating film 20 is arranged (indicated by symbol (b)). The maximum height M of the marker 30 max and the maximum height I of the insulating film 20 maxThe measurement can be performed by the following method. First, the electronic component is cut to form a cross section. The cross section is processed by ion milling. The processed cross section is observed using a scanning electron microscope (SEM). The magnification of the SEM is preferably set to about 500 to 5000 times. In the obtained SEM image, the maximum height M of the marker 30 can be measured respectively. max and the maximum height I of the insulating film 20 max And find M max and I max The value of .
[0034] In the electronic component of this embodiment, the marker 30 is exposed on the surface of the electronic component. Since the marker 30 is exposed from the insulating film 20, the marker 30 is easily identified on the surface of the electronic component, and the visibility of the marker 30 is excellent. The identification of the marker 30 can be performed, for example, by a camera and / or a sensor. In addition, in the electronic component of this embodiment, the maximum height M of the marker 30 is max is the maximum height I of the insulating film 20 max Below. For example, Figure 1 In the configuration shown, the maximum height M of the marker 30 is max The maximum height I of the insulating film 20 max same, Figure 2 In the configuration shown, the maximum height M of the marker 30 is max is smaller than the maximum height I of the insulating film 20 max Thus, the maximum height M of the marker 30 is max The maximum height I of the insulating film 20 max Same or less than I max When the marker 30 is formed, it is less susceptible to external impact and / or sliding, so the strength against external impact and / or sliding is improved, and as a result, the peeling of the marker 30 is suppressed.
[0035] In contrast, Figure 4 As shown in FIG. 1 , when the maximum height of the marker 30 is greater than the maximum height of the insulating film 20 (i.e., when the marker 30 protrudes from the surface of the insulating film 20), the marker 30 is directly exposed to impact and / or sliding from the outside. Figure 1 and Figure 2 Compared with the structure of , there is a tendency that the marker 30 is easily peeled off.
[0036] Figure 5 An optical microscope image of a cross section of the electronic component of this embodiment is shown in FIG. Figure 5 As shown, the marker 30 (white part) is exposed on the surface of the electronic component, and the maximum height M of the marker 30 is max is the maximum height I of the insulating film 20 max the following.
[0037] Hereinafter, each element constituting the electronic component of the present embodiment will be described in more detail.
[0038] (Unit 10)
[0039] The unit body 10 may be, for example, in a substantially rectangular parallelepiped shape. In this specification, a "rectangular parallelepiped" includes a cube, and a "substantially rectangular parallelepiped" also includes a rectangular parallelepiped having a rounded shape at least in one of the corners and the ridges. When the unit body 10 is in a substantially rectangular parallelepiped shape, the unit body 10 may have, for example, a length (L) of 1.1 mm to 1.6 mm, a width (W) of 0.6 mm to 1.4 mm, and a thickness (T) of 0.5 mm to 0.8 mm.
[0040] (Metal magnetic powder 11)
[0041] The unit body 10 preferably contains metal magnetic powder 11. When the unit body 10 contains metal magnetic powder 11, an insulating film 20 can be selectively formed on the surface of the unit body by the method described below. The metal magnetic material contained in the metal magnetic powder 11 can be, for example, crystalline or amorphous Fe (pure iron), Fe alloy (Fe-Si alloy, Fe-Si-Cr alloy, Fe-Si-Al alloy, Fe-Al alloy, etc.). The average particle size of the metal magnetic powder 11 is not particularly limited, and can be, for example, 1 μm to 50 μm. Figure 1 to Figure 3 As shown, the unit body 10 may contain two or more metal magnetic powders 11 having different average particle sizes, but the unit body 10 may contain only one metal magnetic powder 11. The metal magnetic powder 11 may have an insulating coating on its surface. In addition, the content of the metal magnetic powder 11 in the unit body 10 is not particularly limited, and may be, for example, 60% to 100% by weight based on the weight of the entire unit body 10.
[0042] The average particle size of the metal magnetic powder 11 can be measured by the method described below. max and I max The cross section of the electronic component is formed by the same method as the measurement method, and processed by ion milling. The processed cross section is observed with a scanning electron microscope (SEM). The magnification of the SEM is preferably set to about 500 times to 5000 times. The particle size (equivalent circle diameter) of the metal magnetic powder 11 is measured from the obtained SEM image, and the average value can be used as the average particle size of the metal magnetic powder 11. It should be noted that the average particle size of the metal magnetic powder 11 contained in the unit body 10 of the electronic component as a finished product can be considered to be substantially the same as the average particle size of the metal magnetic powder of the raw material. The average particle size of the metal magnetic powder of the raw material can be obtained by measuring the volume-based median particle size D50 using a laser diffraction / scattering method.
[0043] The content of the metal magnetic powder 11 in the unit body 10 can be measured by the following method. max and I max The cross section of the electronic component is formed by the same method as the measurement method, and processed by ion milling. For the processed cross section, time-of-flight secondary ion mass spectrometry (TOF-SIMS), X-ray photoelectron spectroscopy (XPS) or energy dispersive X-ray analysis (EDX) is implemented. When analyzing the cross section of the electronic component, carbon (C) is detected in the area where the resin exists due to the composition of the resin component. In contrast, the area where the resin does not exist contains almost no C. Therefore, the content of the metal magnetic powder 11 can be calculated based on the size of the area where C is not detected in the cross section of the electronic component.
[0044] It is preferable that the average particle size of the metal magnetic powder 11 present near the surface of the unit body 10 is smaller than the average particle size of the metal magnetic powder 11 present in the center of the unit body 10. Here, "near the surface" of the unit body 10 refers to a region that is 100 μm or less away from the surface of the unit body 10 (depth) in a direction perpendicular to the surface of the unit body 10, and "the center of the unit body 10" refers to a region that is closer to the inside than the region near the surface of the unit body 10. When the average particle size of the metal magnetic powder 11 present near the surface of the unit body 10 is smaller than the average particle size of the metal magnetic powder 11 present in the center of the unit body 10, the surface irregularities of the unit body 10 can be reduced, thereby enabling the insulating film 20 to be formed more uniformly on the surface of the unit body 10. As a result, when an external electrode is formed by plating as described later, the plating growth on the surface of the unit body 10 can be further suppressed.
[0045] (Resin 12)
[0046] The unit body 10 preferably further contains a resin 12. The type of the resin 12 is not particularly limited, and may be, for example, one or more resins selected from epoxy resins, phenolic resins, polyester resins, polyolefin resins, Si resins, acrylic resins, polyimide resins, polyvinyl butyral resins, cellulose resins, alkyd resins, and the like.
[0047] The unit cell 10 may further contain inorganic particles. The inorganic particles may be particles made of one or more materials selected from the group consisting of carbon black, borosilicate glass, TiO, ZrO2, SiO2, ZnO, and Al2O3.
[0048] (conductor)
[0049] The unit body 10 has a conductor inside. The type of conductor is not particularly limited and can be appropriately selected according to the type of electronic component. For example, when the electronic component is a coil component such as an inductor, the conductor is a coil conductor. The coil conductor is preferably composed of a metal conductor such as Ag or Cu.
[0050] (Insulating film 20)
[0051] The insulating film 20 is disposed on the surface of the unit cell 10. The insulating film 20 has at least one function of improving the moisture resistance, insulation, chemical resistance and friction resistance of the electronic component. In this specification, "insulating film" refers to a film having higher insulation than the unit cell 10 in a broad sense (i.e., a film with high resistance), and refers to a film having a volume resistivity of 10 6 The composition of the insulating film 20 is not particularly limited and can be appropriately selected according to the purpose, etc. The insulating film 20 can contain, for example, an acrylic resin, an epoxy resin, a polyimide resin, a silicone resin, a polyamide-imide resin, a polyetheretherketone resin, a fluorine resin, or an acrylic silicone resin. It should be noted that the composition of the insulating film 20 is different from that of the unit body 10.
[0052] The insulating film 20 preferably contains an inorganic filler. When the insulating film 20 contains an inorganic filler, the surface of the insulating film 20 can be given unevenness, and as a result, the glossiness of the insulating film 20 can be reduced. The glossiness of the insulating film 20 can be controlled by adjusting the particle size and content of the inorganic filler contained in the insulating film 20. By adjusting the particle size and content of the inorganic filler contained in the insulating film 20 so that the glossiness of the insulating film 20 and the glossiness of the marker 30 are different values, the recognition of the marker can be further improved. In addition, by adding a pigment as an inorganic filler to the insulating film 20, the insulating film 20 can be colored. Adding a pigment to the insulating film 20 makes the color tone of the insulating film 20 different from the color tone of the marker 30, so that the recognition of the marker 30 can be further improved. The inorganic filler contained in the insulating film 20 is preferably an inorganic particle, for example, it can be a particle composed of one or more inorganic materials selected from carbon black, borosilicate glass, TiO2, ZrO2, SiO2, ZnO and Al2O3. The average particle size (D50) and content of the inorganic filler contained in the insulating film 20 are not particularly limited. For example, the average particle size of the inorganic filler can be 1 nm to 10 μm, and the content of the inorganic filler can be 1 wt % to 30 wt % based on the total weight of the insulating film 20 .
[0053] (marker 30)
[0054] The marker 30 is arranged on the surface of the unit body 10. The marker 30 is used to make the orientation (direction) of the electronic component, the lead position of the conductor inside the unit body 10 and / or similar information recognizable from the appearance of the electronic component (for example, an identification marker for direction identification). The number, position and shape of the markers 30 provided on the electronic component are not particularly limited and can be appropriately adjusted according to the purpose, etc. The electronic component may have only one marker 30 or may have more than two markers. The marker 30 may be, for example, a circle, an ellipse or a polygon such as a triangle or a quadrilateral.
[0055] The marker 30 is preferably in contact with the unit body 10. When the marker 30 is in direct contact with the unit body 10, the contact area between the marker 30 and the unit body 10 increases, thereby improving the adhesion between the marker 30 and the unit body 10. As a result, the durability of the marker 30 against external stress is improved, and the peeling of the marker 30 is further suppressed.
[0056] Preferably, at least a portion of the outer edge of the marker 30 is covered by the insulating film 20. In other words, when viewed from a direction perpendicular to the surface of the unit body 10, preferably, at least a portion of the outer edge of the marker 30 overlaps with the insulating film 20. Here, the "outer edge" of the marker 30 refers to the outer edge of the marker 30 when viewed from a direction perpendicular to the surface of the unit body 10 on which the marker 30 is disposed. When at least a portion of the outer edge of the marker 30 is covered by the insulating film 20, the marker 30 is less susceptible to external impact and / or sliding, and the strength against external impact and / or sliding is further improved. As a result, peeling of the marker 30 is further suppressed. When at least a portion of the outer edge of the marker 30 is covered by the insulating film 20, as Figure 1 As shown, the surface of the marker 30 may be flush with the surface of the insulating film 20, as shown in FIG. Figure 2 As shown, the surface of the insulating film 20 may protrude outward from the surface of the marker 30 .
[0057] Preferably, at least a portion of the marker 30 is embedded in the unit cell 10. For example, Figure 1In the structure shown, the bottom side of the marker 30 (the side in contact with the unit body 10) is embedded in the unit body 10. When at least a portion of the marker 30 is embedded in the unit body 10, the strength of the marker 30 against external impact and / or sliding is further improved, and as a result, the peeling of the marker 30 is further suppressed. In addition, when at least a portion of the marker 30 is embedded in the unit body 10, the maximum height of the marker 30 from the surface of the unit body 10 can be reduced. When the size of the entire electronic component is the same, the lower the maximum height of the marker 30 from the surface of the unit body 10, the larger the size of the unit body 10 can be. When the electronic component is a coil component such as an inductor, the larger the size of the unit body 10 containing the metal magnetic powder, the more the inductance acquisition efficiency can be improved, and the more the magnetic properties of the coil component can be improved. Therefore, when at least a portion of the marker 30 is embedded in the unit body 10, the magnetic properties of the coil component can be improved.
[0058] The size of the marker 30 is not particularly limited and can be appropriately adjusted according to its use and the outer dimensions of the unit body 10. For example, when the unit body 10 is substantially rectangular, and the outer dimensions of the unit body 10 are length (L) 1.1 mm to 1.6 mm, width (W) 0.6 mm to 1.4 mm, and thickness (T) 0.5 mm to 0.8 mm, it is preferred that the marker 30 having a diameter or a length of one side of 0.1 mm to 0.4 mm is disposed on at least one surface of the unit body 10.
[0059] The ratio of the area of the marker 30 to the area of the surface of the unit body 10 on which the marker 30 is arranged is preferably 10% to 50%. Here, the "area" of the marker 30 refers to the area of the marker 30 when observed from a direction perpendicular to the surface of the unit body 10 on which the marker 30 is arranged, and the area of the marker 30 also includes the area of the region (outer edge portion, etc.) where the marker 30 is covered by the insulating film 20 or the insulating material 21 described later. When the area ratio of the marker 30 is 10% to 50%, the adhesion strength between the marker 30 and the unit body 10 is further improved, and the peeling of the marker 30 is further suppressed.
[0060] It is preferred that the marker 30 does not exist on the outer edge portion of the surface of the unit body 10 on which the marker 30 is arranged. In other words, it is preferred that the marker 30 is arranged on the inner side of the outer edge portion of the surface of the unit body 10 on which the marker 30 is arranged. The outer edge portion of the surface of the unit body 10 corresponds to the ridge portion of the unit body 10. The ridge portion of the unit body 10 is susceptible to external impacts and the like during the manufacturing process of the electronic component, the conveying process of the electronic component as a finished product, and the installation process of the electronic component. Therefore, when the marker 30 is arranged in a manner that does not reach the outer edge portion of the surface of the unit body 10 (i.e., the ridge portion of the unit body 10), the marker 30 is less susceptible to external impacts and the like, and as a result, the peeling of the marker 30 can be further suppressed.
[0061] It is preferable that the marker 30 is exposed on the surface of the electronic component when viewed from a direction perpendicular to the surface of the unit cell 10 on which the marker 30 is arranged. In this case, the visibility of the marker 30 is further improved.
[0062] When viewed from a direction perpendicular to the surface of the unit cell 10 on which the marker 30 is arranged, the marker 30 is preferably surrounded by the insulating film 20. As described above, the maximum height M of the marker 30 on the surface of the unit cell on which the marker 30 is arranged is max is the maximum height of the insulating film I max Therefore, the surrounding of the marker 30 is surrounded by a maximum height M of the marker 30. max Maximum height above I max When the marker 30 is surrounded by the insulating film 20, the marker 30 is less susceptible to external impact and / or sliding, so the strength against external impact and / or sliding is further improved, and as a result, the peeling of the marker 30 is further suppressed.
[0063] The marker 30 is preferably insulating. In this specification, "insulating" means in a broad sense that the marker 30 has higher insulation (i.e., higher resistance) than the unit cell 10, and in a narrow sense that the volume resistivity is 10 6 As described later, when the external electrodes are formed by plating, if the marker 30 is insulating, the plating growth on the surface of the marker 30 can be suppressed.
[0064] The marker 30 preferably contains an inorganic filler, and the inorganic filler contains one or more materials selected from borosilicate glass, TiO2, SiO2, ZnO, ZrO2 and Al2O3. More specifically, the marker 30 may contain, for example, an inorganic filler containing 10% by weight or more and less than 30% by weight of borosilicate glass, 50% by weight to 80% by weight of TiO2, and the remainder containing at least one of ZrO2 and Al2O3. The composition of the inorganic filler and the content of the marker 30 can be measured by analyzing the marker 30 using time-of-flight secondary ion mass spectrometry (TOF-SIMS), X-ray photoelectron spectroscopy (XPS), energy dispersive X-ray analysis (EDX), high-frequency inductively coupled plasma emission spectrometry (ICP-AES), high-frequency inductively coupled plasma mass spectrometry (ICP-MS) or fluorescent X-ray analysis (XRF).
[0065] When the unit body 10 contains the metal magnetic powder 11 and the marker 30 contains the inorganic filler, the average particle size of the inorganic filler contained in the marker 30 is preferably 30% to 70% of the average particle size of the metal magnetic powder 11. When the average particle size of the inorganic filler contained in the marker 30 is within the above range, the surface of the marker 30 can be smoothed, and as a result, the visibility of the marker 30 can be further improved. The average particle size of the inorganic filler can be measured in the same order as the above-mentioned method for measuring the average particle size of the metal magnetic powder 11. In addition, by adding a pigment as an inorganic filler to the marker 30, the marker 30 can be colored. By adding a pigment to the marker 30, the color tone of the marker 30 is different from the color tone of the insulating film 20, and the recognition of the marker 30 can be further improved. When the color tone of the marker 30 is different from the color tone of the insulating film 20 by adding a pigment, the pigment may be added to only one of the marker 30 and the insulating film 20, or the pigment may be added to both the marker 30 and the insulating film 20.
[0066] (External Electrode)
[0067] The shape and position of the external electrode are not particularly limited, and the shape and position of the external electrode can be selected according to the purpose, etc. The external electrode can be, for example, a so-called five-sided electrode provided on the two end faces of the unit body 10 and a part of the four faces adjacent to the two end faces, or can be an L-shaped electrode, or can be a bottom electrode. The external electrode can contain, for example, one or more metals selected from Ag, Cu, Pd, Ni and Sn. The external electrode can be formed by any method, for example, it can be formed by applying a conductive paste containing metal particles to the unit body 10 and sintering it. In addition, the external electrode can further have a plating layer.
[0068] [Second embodiment]
[0069] Next, refer to the following Figure 3 The electronic component of the second embodiment of the present invention is described. The electronic component of the second embodiment has the same structure as the electronic component of the first embodiment except that an insulating material 21 is arranged on the exposed surface of the marker 30 on the surface of the electronic component. Therefore, the insulating material 21 is mainly described below, and the description of other structures is omitted. The electronic component of the second embodiment is the same as the electronic component of the first embodiment, and the visibility of the marker can be improved and the peeling of the marker can be suppressed.
[0070] (Insulating material 21)
[0071] In the electronic component of the second embodiment, an insulating material 21 is arranged on the exposed surface of the marker 30 exposed on the surface of the electronic component. The insulating material 21 is separated from the insulating film 20. When the insulating material 21 is arranged on the exposed surface of the marker 30, the insulating material 21 can function as a buffer material for impact and / or sliding from the outside. Therefore, when the insulating material 21 is arranged on the exposed surface of the marker 30, the marker 30 is less susceptible to impact and / or sliding from the outside, and the strength of the marker 30 for impact and / or sliding from the outside can be further improved. As a result, the peeling of the marker 30 can be further suppressed. The ratio of the area occupied by the insulating material 21 can be appropriately adjusted so as not to hinder the visibility of the marker 30. In addition, the composition of the insulating material 21 can be the same as that of the insulating film 20. It should be noted that the composition of the insulating material 21 is different from that of the marker 30.
[0072] [Method for manufacturing electronic component]
[0073] The method for manufacturing an electronic component of the present invention is described below by taking the case where the electronic component is a coil component such as an inductor as an example. In particular, the method described below is only an example, and the method for manufacturing an electronic component of the present invention is not limited to the following method.
[0074] (Preparation of magnetic sheets)
[0075] Metal magnetic powder, thermosetting resin and solvent are mixed in a predetermined ratio and formed into a sheet to form a magnetic sheet. As the solvent, methyl ethyl ketone (MEK), N,N-dimethylformamide (DMF), propylene glycol monomethyl ether (PGM) and the like can be used.
[0076] (Preparation of Marking Paste)
[0077] An inorganic filler, a thermosetting resin, and a solvent are mixed in a prescribed ratio to prepare a marker paste. As a solvent, methyl ethyl ketone (MEK), N,N-dimethylformamide (DMF), propylene glycol monomethyl ether (PGM), etc. can be used. For the inorganic filler contained in the marker paste, when the total weight of the inorganic filler is set to 100 weight %, for example, it can be an inorganic filler containing 10 weight % or more and less than 30 weight % of borosilicate glass, 50 weight % to 80 weight % of TiO2, and the remaining part contains at least one of ZrO2 and Al2O3. It should be noted that the composition and average particle size of the inorganic filler contained in the marker paste can be considered to be substantially the same as the composition and average particle size of the inorganic filler contained in the marker of the electronic component as a finished product.
[0078] (Production of unit body)
[0079] Prepare a coil conductor, overlap the magnetic sheet and the coil conductor and press them, and bury the coil conductor in the magnetic sheet. When manufacturing multiple coil components at a time, prepare a base material (substrate, metal mold, film, etc.) with multiple coil conductors, overlap the magnetic sheet on it and press it, and bury the coil conductor in the magnetic sheet.
[0080] First, a plurality of coil conductors are arranged, and a magnetic sheet is overlapped on the upper surface of the coil conductors and pressurized to perform a press molding. Thus, at least a portion of the coil conductor is buried in the magnetic sheet. A marker paste is applied to the surface of the magnetic sheet by screen printing or the like, and dried to form a marker. The position and shape of the marker paste can be appropriately set according to the shape and position of the desired marker.
[0081] Next, another magnetic sheet is overlapped and pressurized on the lower surface of the coil conductor (the surface where the coil conductor is exposed from the magnetic sheet) to perform secondary pressurization. During the secondary pressurization, a portion of the marker is embedded in the magnetic sheet. In addition, the magnetic sheet overlapped and pressurized on the upper surface of the coil conductor and the magnetic sheet overlapped and pressurized on the lower surface of the coil conductor are integrally formed by the secondary pressurization.
[0082] The method of forming the marker is not limited to the above method. For example, after the primary press molding and the secondary press molding, a marker paste may be applied to the surface of the magnetic sheet and dried to form the marker, and the magnetic sheet with the marker formed thereon may be further pressurized to embed a portion of the marker in the magnetic sheet. Alternatively, a magnetic paste containing metal magnetic powder and a conductor paste containing metal powder may be sequentially laminated by screen printing or the like to form a laminate having a conductor therein, and a marker paste may be printed on the surface of the laminate and dried to form the marker, and the laminate may be pressurized to embed a portion of the marker in the laminate after the marker is formed.
[0083] Next, after the magnetic sheet with the coil conductor embedded therein is solidified, the magnetic sheet is cut (cut, etc.) according to the size of each coil component and polished (drum polishing, etc.) to obtain a unit body having a conductor (coil conductor) inside.
[0084] During the barrel grinding, a portion of the metal magnetic powder contained in the unit body adheres to the surface of the marker according to the barrel grinding processing conditions (rotation speed and / or processing time). If the metal magnetic powder adheres to the surface of the marker, an insulating material can be arranged on the surface of the marker in the insulating film forming step described later.
[0085] (Formation of Insulating Film)
[0086] Next, an insulating film is formed on the surface of the unit body. The method for forming the insulating film is not particularly limited. For example, the insulating film can be formed by the method described in Japanese Patent Publication No. 2016-178282. First, a mixed solution containing an ionizing component, a surfactant, and a resin component that ionizes the metal of the metal magnetic powder contained in the unit body is prepared. The ionizing component can be, for example, one or more selected from sulfuric acid, hydrofluoric acid, ferric fluoride, nitric acid, hydrochloric acid, phosphoric acid, and carboxylic acid. The surfactant can be, for example, an anionic surfactant such as alkylbenzene sulfonate, or a nonionic surfactant such as polyoxyethylene alkyl ether. The resin component can be, for example, one or more selected from acrylic resins, epoxy resins, polyimide resins, silicone resins, polyamide-imide resins, polyetheretherketone resins, fluorine resins, and acrylic silicone resins. The unit body is immersed in the mixed solution. The surface of the unit body is etched under the action of the ionizing component contained in the mixed solution, thereby ionizing the metal component contained in the metal magnetic powder present on the surface of the unit body. The ionized metal component reacts with the resin component in the mixed solution. The resin component in the mixed solution is neutralized by the reaction and precipitated on the surface of the unit body, and as a result, an insulating film is formed on the surface of the unit body. On the other hand, because the marker does not contain metal magnetic powder, the above-mentioned ionization and reaction of the ionized metal component and the resin component do not occur on the surface of the marker. Therefore, an insulating film can be selectively formed on the surface of the unit body where the marker is not configured. It should be noted that an insulating film is not formed on the exposed surface of the lead-out portion where the two ends of the coil conductor are led out to the surface of the unit body. This is because the constituent elements of the coil conductor (such as Cu, etc.) are noble elements compared to the metal components of the ionized unit body, and therefore are hardly ionized, and as a result, are not easy to react with the resin component.
[0087] As described above, when the unit body is roller-polished, a part of the metal magnetic powder contained in the unit body can adhere to the surface of the marker. At this time, the metal magnetic powder is ionized and the ionized metal component reacts with the resin component on the surface of the metal magnetic powder attached to the surface of the marker, and the insulating material partially adheres to the surface of the marker. As a result, in the electronic component as a finished product, the insulating material is arranged on the exposed surface of the marker. At this time, the insulating material arranged on the exposed surface of the marker can be separated from the insulating film.
[0088] Next, the unit body on which the insulating film is formed is washed with pure water or the like, and then subjected to a heat treatment. The heat treatment causes the resin component contained in the insulating film to be cross-linked via the cationic element or the resin components.
[0089] It should be noted that in addition to the above-mentioned method, the formation of the insulating film can also be implemented by the following methods, for example, after forming an insulating film on the entire surface of the unit body by an arbitrary method, the insulating film formed on the surface of the marker and the lead-out portion of the coil conductor is partially removed by laser irradiation, etc., or after waterproofing the surface of the marker and the lead-out portion of the coil conductor, an insulating film is formed on the surface of the unit body by an arbitrary method.
[0090] (Formation of External Electrodes)
[0091] The conductive paste containing metal particles is applied to the unit body formed with the insulating film to form an external electrode. The external electrode can be formed by sputtering or plating. A plating layer can be further provided on the surface of the external electrode. In this way, the electronic component (coil component) of the present invention is obtained.
[0092] More specifically, for example, when forming a five-sided electrode as an external electrode, a conductive paste is applied to both end faces of the unit body and a part of the four faces adjacent to the two end faces, and the conductive paste is sintered at a temperature at which the insulating film does not undergo thermal decomposition, thereby forming the external electrode. In this case, the external electrode is arranged on the insulating film.
[0093] As another method, for example, when an L-shaped electrode is formed as an external electrode, a laser is irradiated on the surface of the unit body in the area where the external electrode is formed, thereby removing the insulating film on the laser irradiated surface of the unit body and making the metal magnetic powder exposed on the laser irradiated surface bond with each other. Then, the external electrode is formed on the laser irradiated surface by plating (electroplating or electroless plating). In this case, the external electrode is directly arranged on the unit body.
[0094] In addition, as another method, for example, when a bottom electrode is formed as an external electrode, after forming an L-shaped electrode by the above method, an insulating film is formed on the end surface of the external electrode by spray coating or dip coating, so that the bottom electrode can be formed.
[0095] The present invention includes the following aspects, but is not limited to these aspects.
[0096] (Form 1)
[0097] An electronic component comprising:
[0098] A unit body with a conductor inside,
[0099] an insulating film and at least one marker disposed on the surface of the unit body,
[0100] External electrodes arranged on the unit cell or the insulating film,
[0101] The marker is exposed on the surface of the electronic component.
[0102] When the maximum height of the marker on the surface of the unit body where the marker is arranged is set to M max , set the maximum height of the insulating film to I max When M max and I max Satisfies the following formula:
[0103] M max ≤I max .
[0104] (Form 2)
[0105] The electronic component according to aspect 1, wherein the marker is in contact with the unit body.
[0106] (Form 3)
[0107] The electronic component according to aspect 1 or 2, wherein at least a portion of an outer edge portion of the marker is covered with an insulating film.
[0108] (Form 4)
[0109] The electronic component according to any one of aspects 1 to 3, wherein at least a part of the marker is embedded in the unit cell.
[0110] (Form 5)
[0111] The electronic component according to any one of aspects 1 to 4, wherein the unit cell contains metal magnetic powder.
[0112] (Form 6)
[0113] The electronic component according to aspect 5, wherein the average particle size of the metal magnetic powder present near the surface of the unit body is smaller than the average particle size of the metal magnetic powder present in the center of the unit body.
[0114] (Form 7)
[0115] The electronic component according to aspect 5 or 6, wherein the unit cell further contains resin.
[0116] (Form 8)
[0117] The electronic component according to any one of aspects 1 to 7, wherein the marker is insulating.
[0118] (Form 9)
[0119] An electronic component according to aspect 8, wherein the marker contains an inorganic filler containing one or more materials selected from borosilicate glass, TiO2, SiO2, ZnO, ZrO2 and Al2O3.
[0120] (Form 10)
[0121] An electronic component according to form 9, wherein the marker contains an inorganic filler containing 10 wt % or more and less than 30 wt % of borosilicate glass, 50 wt % to 80 wt % of TiO 2 , and the remainder containing at least one of ZrO 2 and Al 2 O 3 .
[0122] (Form 11)
[0123] The electronic component according to any one of aspects 1 to 10, wherein an insulating material is disposed on an exposed surface of the electronic component where the marker is exposed, and the insulating material is separated from the insulating film.
[0124] (Form 12)
[0125] The electronic component according to any one of aspects 1 to 11, wherein the insulating film contains an inorganic filler.
[0126] (Form 13)
[0127] The electronic component according to any one of aspects 1 to 12, wherein the unit body is substantially in the shape of a rectangular parallelepiped, and the outer dimensions of the unit body are 1.1 mm to 1.6 mm in length, 0.6 mm to 1.4 mm in width, and 0.5 mm to 0.8 mm in thickness,
[0128] A marker having a diameter or a side length of 0.1 mm to 0.4 mm is disposed on at least one surface of the unit body.
[0129] (Form 14)
[0130] The electronic component according to any one of aspects 1 to 13, wherein the ratio of the area of the marker to the area of the surface of the unit body on which the marker is arranged is 10% to 50%.
[0131] (Form 15)
[0132] The electronic component according to any one of aspects 1 to 14, wherein the marker is not present at an outer edge portion of the surface of the unit body on which the marker is disposed.
[0133] (Form 16)
[0134] An electronic component according to any one of forms 5 to 7, form 9 citing form 8, and form 10 citing form 9, wherein the average particle size of the inorganic filler contained in the marker is 30% to 70% of the average particle size of the metal magnetic powder, and form 8 cites any one of forms 5 to 7.
[0135] (Form 17)
[0136] The electronic component according to any one of aspects 1 to 16, wherein the marker is exposed on the surface of the electronic component when viewed from a direction perpendicular to the surface of the unit body on which the marker is arranged.
[0137] (Form 18)
[0138] The electronic component according to any one of aspects 1 to 17, wherein the marker is surrounded by an insulating film when viewed from a direction perpendicular to a surface of the unit body on which the marker is arranged.
[0139] Industrial Applicability
[0140] The electronic component of the present invention includes a marker that is excellent in visibility and is suppressed from peeling off, and thus can be mounted with high accuracy.
Claims
1. An electronic component comprising: a unit body having a conductor inside and containing metal magnetic powder, an insulating film and at least one marker arranged on the surface of the unit body, and an external electrode arranged on the unit body or the insulating film, The marker is arranged on the surface of the electronic component so as to be exposed from the insulating film in a state where at least a part of the outer edge portion overlaps with the insulating film. The insulating film has higher insulating properties than the unit cell, When the maximum height of the marker on the surface of the unit body on which the marker is arranged is set to M max , the maximum height of the insulating film is set to I max When M max and I max Satisfies the following formula: M max ≤I max .
2. The electronic component according to claim 1, wherein The average particle size of the metal magnetic powder present near the surface of the unit body is smaller than the average particle size of the metal magnetic powder present in the center portion of the unit body.
3. The electronic component according to claim 1 or 2, wherein: The unit cell further contains a resin.
4. The electronic component according to claim 1 or 2, wherein: The marker is insulating.
5. The electronic component according to claim 4, wherein The marker contains an inorganic filler, and the inorganic filler contains one or more materials selected from borosilicate glass, TiO2, SiO2, ZnO, ZrO2 and Al2O3.
6. The electronic component according to claim 5, wherein The marker contains an inorganic filler, wherein the inorganic filler contains 10 wt % or more and less than 30 wt % of borosilicate glass, 50 wt % to 80 wt % of TiO 2 , and the remainder contains at least one of ZrO 2 and Al 2 O 3 .
7. The electronic component according to claim 1 or 2, wherein: An insulating material is disposed on an exposed surface of the marker exposed on the surface of the electronic component, and the insulating material is separated from the insulating film.
8. The electronic component according to claim 1 or 2, wherein: The insulating film contains an inorganic filler.
9. The electronic component according to claim 1 or 2, wherein: The unit body is substantially in the shape of a rectangular parallelepiped, and the outer dimensions of the unit body are 1.1 mm to 1.6 mm in length, 0.6 mm to 1.4 mm in width, and 0.5 mm to 0.8 mm in thickness. The marker having a diameter or a side length of 0.1 mm to 0.4 mm is disposed on at least one surface of the unit body.
10. The electronic component according to claim 1 or 2, wherein: The ratio of the area of the marker to the area of the unit cell surface on which the marker is arranged is 10% to 50%.
11. The electronic component according to claim 1 or 2, wherein: The marker does not exist at the outer edge of the surface of the unit cell on which the marker is arranged.
12. The electronic component according to claim 5 or 6, wherein: The average particle size of the inorganic filler contained in the marker is 30% to 70% of the average particle size of the metal magnetic powder.
13. The electronic component according to claim 1 or 2, wherein: The marker is exposed on the surface of the electronic component when viewed from a direction perpendicular to the surface of the unit body on which the marker is arranged.
14. The electronic component according to claim 1 or 2, wherein: When viewed from a direction perpendicular to the surface of the unit cell on which the marker is arranged, the marker is surrounded by the insulating film.