A method for adjusting the FTrPSA of the tail gas of SiC-CVD process based on the reaction of alkane and silane as the reaction circulating gas
The SiC-CVD process exhaust gas is separated and purified through full-temperature pressure swing adsorption technology, which solves the waste of resources and safety hazards in exhaust gas treatment, and realizes the recycling of exhaust gas and the improvement of deposition efficiency.
Patent Information
- Application Number
- CN202011537652.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-12-23
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2040-12-23
AI Technical Summary
Existing SiC-CVD process exhaust gas treatment methods cannot effectively utilize valuable components in the exhaust gas, resulting in high production costs and safety hazards, and it is impossible to achieve comprehensive utilization of the exhaust gas.
The full temperature range pressure swing adsorption (FTrPSA) method is used to separate and purify H2, CH4, SiH4 and other groups in the exhaust gas of the SiC-CVD process through the coupling of medium temperature pressure swing adsorption, shallow cooling pressure swing adsorption and medium and shallow cooling condensation distillation. so that it can be recycled back into the process and the C/Si ratio can be adjusted to improve deposition efficiency and quality.
It achieves comprehensive utilization of SiC-CVD process exhaust gas, reduces waste gas emissions, reduces raw material gas consumption, improves the deposition efficiency and quality of SiC crystals or films, and reduces production costs.
Smart Images

Figure CN112657314B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the recycling and reuse of tail gas in the CVD (chemical vapor deposition) growth process of silicon carbide (SiC) crystals and thin film epitaxy of the third-generation semiconductor material, which contains commonly used "carbon (C) sources" - methane (CH4) or propane (C3H8) and "silicon (Si) sources" - silane (SiH4), as well as hydrogen (H2) as a carrier gas as main components. More specifically, it relates to an adjustable method for using the tail gas of a SiC-CVD process based on the reaction of alkanes and silane as a reaction circulating gas FTrPSA (full temperature swing adsorption) method. Background Art
[0002] As a third-generation semiconductor material, silicon carbide (SiC) has been widely used in power electronic components such as power switches, frequency conversion, UPS, etc. in IT and electronic consumer products, automobiles, photovoltaics, nuclear reactors, and aerospace and military fields with harsh system working conditions due to its excellent properties such as wide bandgap, resistance to high temperature and high pressure, high frequency and high power, and radiation resistance. Among them, single crystal or epitaxial film is the key production step for the widespread application of SiC materials.
[0003] The epitaxial processes of SiC crystals or thin films include high temperature sublimation (PVT), chemical vapor deposition (CVD), liquid phase growth (LPE), molecular beam growth (MBE), electron cyclotron resonance plasma chemical vapor deposition (ECR-MPCVD), etc., and the CVD process commonly used in industry has the characteristics of low growth temperature, large production batch, good uniformity of crystals or epitaxial films, and easy operation and control. Among them, according to the different silicon (Si) sources and carbon (C) sources (called "reaction precursors") involved in the reaction, the SiC-CVD growth process can be divided into chlorine-free, chlorine-containing and C / Si-containing organic silicon compound SiC-CVD growth process. Furthermore, the exhaust gas composition generated by different growth processes is also different, and the treatment methods are also different.
[0004] In the chlorine-free SiC-CVD crystal or film epitaxial growth process based on the reaction of methane / alkane and silane, CH4 or C3H8 is usually used as the reaction precursor of "C source", SiH4 is used as the reaction precursor of "Si source", and hydrogen (H2) or inert argon (Ar) is carried into the CVD reaction chamber (furnace) to perform chemical vapor deposition reaction at a certain temperature and pressure to obtain the growth of SiC crystal or epitaxial film on the substrate. The quality of crystal or film growth depends not only on the purity of the reaction precursor, reaction temperature, pressure, feed gas (precursor) flow rate, reaction time, reaction chamber structure and other process conditions, but also on the concentration or flow ratio between the reaction precursors, such as "C / Si" feed ratio of 2~5:1, H2 concentration of 50~90%, etc. In actual operation, the appropriate ratio of "C / Si / H2" is generally achieved by adjusting the feed amount of feed gas CH4 or SiH4 or H2. In the CVD reaction process, in addition to the solid crystals or thin film epitaxial products, the gas phase still contains the reaction products H2, CH4 and a small amount of ethane (C2H6), Si powder or Si clusters or C powder and other solid tiny particles, as well as unreacted CH4, SiH4, carrier gas H2 that does not participate in the reaction, and trace or trace amounts of other impurities, such as carbon monoxide (CO), carbon dioxide (CO2), etc.
[0005] Usually, after the reaction is completed, the gas phase is discharged to form the SiC-CVD process tail gas. Since the tail gas contains toxic, harmful, flammable and explosive components such as H2, SiH4, CH4, etc., in the SiC-CVD crystal or thin film epitaxial growth process, the methods for treating the tail gas are usually dry adsorption and direct combustion. The former uses an adsorbent to adsorb SiH4, silicon clusters, ethane, propane, etc. and then directly discharges them, but it is suitable for conditions where the concentration of SiH4, ethane or propane in the tail gas is small. The latter uses the fact that each component in the tail gas is flammable and is passed through the air to oxidize SiH4, ethane / propane, etc. into non-toxic SiO2, CO2, H2O, etc., and then after water washing, spraying and absorption, it forms SiO2 slurry and is discharged, and the tail gas meets the emission standards. The combustion method is widely used in the industry due to its economy. Most of them are small-scale on-site treatment devices. However, it requires the introduction of air several times the exhaust gas flow rate to ensure that the concentration of H2, SiH4 and other highly explosive substances in the air is outside the explosion limit. Therefore, the consumption is high and there are certain safety hazards. At the same time, the combustion generates a large amount of heat and the tiny particles are very easy to explode during the combustion process. A large amount of water is required for timely spraying, resulting in secondary pollution emissions or additional treatment. In addition, a large number of valuable resources such as H2, SiH4, CH4 and C3H8 have not only failed to be effectively utilized, but their emissions also bring about a greenhouse effect. In addition, the industry also uses the adsorption method as an auxiliary method of the combustion method. When the combustion method fails to ignite or shuts down due to safety hazards, the SiC-CVD process exhaust gas will automatically switch to the adsorption method device for treatment. Both methods only treat the exhaust gas to meet emission standards and meet environmental protection requirements, but they cannot make comprehensive use of the exhaust gas, especially the raw materials that are extremely important for SiC-CVD crystal or thin film epitaxial growth processes, such as H2, SiH4, CH4 / C3H8, which cannot be reused, resulting in high production costs for crystal or thin film epitaxy.
[0006] The epitaxial growth mechanism of SiC-CVD crystals or thin films is mainly determined by the deposition or substrate surface adsorption control and gas phase reaction control to determine the crystal or thin film growth efficiency and product quality, and the concentration of CH4 / SiH4 in the gas phase reaction, the reaction conversion rate, and the partial pressure of H2 are the key factors affecting the deposition or adsorption control efficiency, which in turn have a significant impact on the deposition efficiency. Therefore, it is necessary to continuously adjust the ratio of the feed gas to achieve the most effective deposition. In view of the fact that the SiC-CVD process tail gas contains a large amount of feed gas components, the purpose of the present invention is to utilize these effective components in the tail gas, and adjust the concentration and flow rate of the effective components of the tail gas through appropriate treatment to a circulating reaction gas that can be returned to the process to meet the most suitable ratio required for the deposition reaction, which can not only save feed gas consumption, but also solve the burden of tail gas treatment. Summary of the invention
[0007] The present invention provides a method for adjusting the tail gas of SiC-CVD process based on the reaction of alkane and silane as reaction circulating gas FTrPSA (Full Temperature Range-Pressure Swing Adsorption). FTrPSA is a method based on pressure swing adsorption (PSA) and can be coupled with various separation technologies. It uses the differences in the adsorption / condensation / distillation separation coefficients and physical and chemical properties of different material components (mainly H2, CH4, SiH4) in the tail gas generated in the SiC-CVD crystal or thin film epitaxial growth process at different pressures and temperatures. It adopts medium-temperature pressure swing adsorption, shallow cold pressure swing adsorption and medium-shallow cold condensation distillation coupling, so that the adsorption and desorption in the shallow cold pressure swing adsorption concentration process are easy to match and balance the cycle operation to perform the separation and purification of the adjustable ratio of each effective component, so that the process tail gas can be directly returned to the SiC-CVD crystal or thin film epitaxial growth process as a circulating reaction gas for recycling, without consuming more raw gas or completely and clearly separating the effective components from the tail gas and returning them to the process for use. The high cost problem, thus, not only realizes the effective comprehensive utilization of SiC-CVD process tail gas and reduces waste gas emissions, but also effectively increases the deposition efficiency and quality of SiC crystal or thin film epitaxy:
[0008] A method for adjusting the tail gas of a SiC-CVD process based on the reaction of an alkane with a silane as a reaction circulating gas FTrPSA comprises the following steps:
[0009] (1) Raw gas: tail gas from a chlorine-free process in which chemical vapor deposition (CVD) is used to prepare silicon carbide (SiC) crystals or epitaxial growth on substrates using methane (CH4) or propane (C3H8) as the main carbon (C) source and silane (SiH4) as the silicon (Si) source. Its main components are hydrogen (H2), methane (CH4), silane (SiH4), a small amount of alkanes with carbon 2 or higher components (C2+), trace amounts of carbon monoxide (CO), carbon dioxide (CO2), high-silicon hydrocarbons, as well as silicon dioxide (SiO2) and carbon (C) fine particles. The pressure is normal pressure or low pressure, and the temperature is room temperature.
[0010] (2) Pretreatment: The raw gas is pressurized and sent to a pretreatment unit consisting of a dust collector, a particle filter, and an oil mist collector. Under the operating conditions of 0.2~0.3MPa pressure and room temperature, dust, particles, oil mist, some high alkanes, and high silane impurities are removed successively. The purified raw gas is subjected to heat exchange to 30~80℃ and pressurized to 0.6~1.0MPa before entering the next process - medium-temperature pressure swing adsorption process.
[0011] (3) Medium-temperature pressure swing adsorption: the purified raw gas from the pretreatment process enters a multi-tower pressure swing adsorption process consisting of at least 4 towers. The operating pressure of the adsorption tower is 0.6~1.0MPa, and the operating temperature is 30~80℃. At least one adsorption tower is in the adsorption step. The non-adsorbed phase gas flowing out from the top of the adsorption tower in the adsorption step is the intermediate gas. After heat exchange to 5~20℃, it enters the next process - shallow cold pressure swing adsorption concentration. The carbon dioxide-rich gas flowing out from the bottom of the adsorption tower in the desorption step, which mainly includes CO2, C2+ and a small amount of H2 / CH4 / SiH4, enters the subsequent medium-shallow temperature condensation process after pressurization.
[0012] (4) Shallow cold pressure swing adsorption concentration: the intermediate gas from the medium temperature pressure swing adsorption process at 5~20℃ and 0.6~1.0MPa enters a multi-tower pressure swing adsorption concentration process consisting of at least 4 towers. The operating pressure of the adsorption tower is 0.6~1.0MPa and the operating temperature is 5~20℃. At least one adsorption tower is in the adsorption step, and the other adsorption towers are in the desorption regeneration step. The non-adsorbed phase gas flowing out from the top of the adsorption tower in the adsorption step is methane hydrogen gas, which enters the next step - adsorption purification. The adsorption phase gas formed at the bottom of the adsorption tower in the desorption step is methane hydrogen gas. The concentrated gas is mixed with the purified methane and hydrogen gas from the subsequent adsorption purification according to a ratio and recycled for use as a circulating reaction gas for the SiC-CVD crystal or thin film epitaxial growth process based on the reaction of alkanes and silanes. The adsorbent of the shallow cold pressure swing adsorption concentration process adopts one or a combination of activated alumina, silica gel, activated carbon, and molecular sieves. Displacement and vacuum regeneration are used during desorption. The displacement gas comes from the crude silane gas from the subsequent medium and shallow cold distillation process to adjust the C / Si ratio in the reaction cycle gas to meet the needs of the SiC-CVD process.
[0013] (5) Adsorption purification: the methane hydrogen gas from the shallow cold pressure swing adsorption concentration process enters the adsorption purification process consisting of 2 or 3 adsorption towers after precision filtration, and is adsorbed at an operating temperature of 5~20℃ and an operating pressure of less than 1.0MPa to further purify and remove trace amounts of CO, forming purified methane hydrogen gas. A part of it is mixed with the concentrated gas from the shallow cold pressure swing adsorption concentration process in a suitable ratio and returned to the SiC-CVD crystal or thin film epitaxial growth process as a reaction circulating gas for recycling, and a part of it is used as fuel gas for heating.
[0014] (6) Medium-shallow temperature condensation. The carbon dioxide-rich gas from the medium-temperature pressure swing adsorption process is finely filtered to remove fine particles, then subjected to heat exchange to -35~-10℃ and pressurized to 1.0~2.5MPa, and enters a medium-shallow cold condenser with an operating temperature of -35~-10℃. The non-condensable gas escaping from the condenser passes through a heat exchanger to a temperature of 5~20℃, and is directly or depressurized to less than 1.0MPa, and then either returns to the shallow cold pressure swing adsorption concentration process or is used as fuel gas for heating. The condensed fluid rich in SiH4 / C3H8 and trace amounts of easily condensable impurities including carbon dioxide (CO2) flowing out of the condenser directly enters the next process - medium-shallow cold distillation.
[0015] (7) Medium-shallow cold distillation: the condensed fluid produced in the medium-shallow cold condensation process enters the medium-shallow cold distillation tower-1 with an operating temperature of -35~-10℃ and an operating pressure of 1.0~2.5MPa. A small amount of non-condensable gas of light components flows out from the top of the distillation tower-1, or is returned to the shallow cold pressure swing adsorption concentration process as feed after being cooled to 5~20℃ and reduced to less than 1MPa through a heat exchanger, or is used as fuel gas for heating. The heavy component fluid flowing out from the bottom of the distillation tower-1 enters the medium-shallow cold distillation tower-2 with an operating temperature of -35~-10℃ and an operating pressure of 1.0~2.5MPa. The top gas of crude SiH4 containing methane and hydrogen flows out from the top of the tower, which is used as the replacement gas for the shallow pressure swing adsorption concentration process to adjust the C / Si ratio in the reaction circulation gas to meet the needs of the SiC-CVD process. The heavy component enriched in C3H8 flows out from the bottom of the tower. After decarbonization (CO2), it is used as the reaction circulation gas, mixed with the concentrated gas from the shallow pressure swing adsorption concentration process, the purified methane and hydrogen gas from the adsorption purification process, and the crude silane gas from the top of the tower of this process used for the replacement gas of the shallow pressure swing adsorption concentration process in proportion, and returned to the SiC-CVD process as the reaction circulation gas for recycling.
[0016] Furthermore, the tail gas of the SiC-CVD process based on the reaction of alkanes and silanes is a reaction circulating gas FTrPSA adjustable method, characterized in that when the raw gas "C source" is only methane, there is one distillation tower in the medium-shallow cold distillation process, namely, distillation tower-1, and distillation tower-2 is omitted, that is, the condensed fluid produced from the medium-shallow temperature condensation process enters the medium-shallow cold distillation tower-1 with an operating temperature of -35~-10°C and an operating pressure of 1.0~2.5MPa, and crude SiH4 gas containing methane hydrogen flows out from the top of the distillation tower-1 as the replacement gas for the shallow cold pressure swing adsorption concentration process to adjust the C / Si ratio in the reaction circulating gas to meet the needs of the SiC-CVD process, and a small amount of heavy components enriched in CO2 flow out from the bottom of the tower for direct discharge.
[0017] Furthermore, the SiC-CVD process tail gas based on the reaction of alkanes and silanes is a reaction cycle gas FTrPSA adjustable method, characterized in that the raw gas "C source" is only methane and the CO2 content in the purified raw material is less than 10ppm. The carbon dioxide-rich desorption gas flowing out from the medium temperature pressure swing adsorption process, after adsorption and decarbonization (CO2), is used as the replacement gas of the shallow cold pressure swing adsorption concentration process to form a reaction cycle gas for recycling, and a part is used as fuel gas after being washed and oxidized by water vapor, and the intermediate gas flowing out enters the shallow cold pressure swing adsorption concentration process, thereby eliminating the medium-shallow temperature condensation and medium-shallow cold distillation processes.
[0018] Furthermore, the FTrPSA adjustable method for using the tail gas of the SiC-CVD process based on the reaction of alkanes and silane as the reaction circulating gas is characterized in that the raw gas "C source" is only methane and the CO2 content in the purified raw gas is greater than 0.1%. The purified raw gas from the pretreatment process first enters the decarbonization process for decarbonization, and an adsorption method loaded with a disposable adsorbent is used to remove the CO2 therein. The purified raw gas from which CO2 has been removed is directly entered into the shallow cold pressure swing adsorption concentration process after being subjected to heat exchange to 5~20°C and pressurized to 0.6~1.0MPa. The concentrated gas flowing out from the bottom of the adsorption tower in the desorption step is mixed with the purified methane hydrogen gas after subsequent adsorption purification according to a ratio, and is recycled and used as the circulating reaction gas for the SiC-CVD crystal or thin film epitaxial growth process based on the reaction of methane and silane, thereby eliminating the medium-temperature pressure swing adsorption, medium-shallow temperature condensation and medium-shallow cold distillation processes.
[0019] Furthermore, the SiC-CVD process tail gas based on the reaction of alkanes and silanes is a reaction cycle gas FTrPSA adjustable method, characterized in that, under the condition that the purified raw gas contains a higher concentration of C2+, the purified raw gas from the pretreatment process enters the medium-temperature pressure swing adsorption process composed of two-stage PSA after heat exchange and pressurization, wherein the purified raw gas enters from the bottom of the first PSA adsorption tower (1-stage PSA) of the medium-temperature pressure swing adsorption, and the intermediate gas of the non-adsorbed phase flowing out from the top of the 1-stage PSA tower in the adsorption stage enters the shallow cold pressure swing adsorption concentration process, and the desorbed gas flowing out from the 1-stage PSA adsorption tower in the desorption step enters from the bottom of the second PSA adsorption tower (2-stage PSA) after pressurization, and the desorbed gas flowing out from the bottom of the 2-stage PSA adsorption tower in the desorption step enters the medium-shallow temperature condensation process as a carbon dioxide-rich gas, and the non-adsorbed phase gas flowing out from the top of the 2-stage PSA adsorption tower in the adsorption step is mixed with the purified raw gas as a feed gas and returned to the 1-stage PSA adsorption tower.
[0020] Furthermore, the SiC-CVD process tail gas based on the reaction of alkanes and silanes is a reaction cycle gas FTrPSA adjustable method, characterized in that the purified raw gas contains a very high concentration of C2+ under working conditions, such as C2+ / Si ratio exceeds 5:1, the purified raw gas from the pretreatment process is subjected to heat exchange to -35~-15°C and compressed to 2.5~3.5MPa, and a shallow cold oil absorption process is used to replace the medium temperature pressure swing adsorption process, that is, the shallow cold oil absorption process consists of an absorption tower and a desorption tower, propane (C3) is used as the absorbent, and the absorption temperature is - 35~-15℃, absorption pressure is 2.5~3.5MPa, desorption temperature is room temperature, desorption pressure is atmospheric pressure or slightly positive pressure, the purified raw gas enters from the bottom of the absorption tower, and conducts reverse mass transfer with the C3 absorbent sprayed from the top of the absorption tower, the non-condensable intermediate gas escaping from the top of the absorption tower enters the subsequent shallow cold pressure swing adsorption concentration, the C2+ rich liquid flowing out from the bottom of the absorption tower enters the desorption tower, the C2+ rich gas flowing out from the top of the desorption tower directly enters the subsequent medium and shallow temperature condensation process, the absorbent C3 flows out from the bottom of the desorption tower, and after cyclic pressurization, it returns to the top of the absorption tower as absorbent for spraying absorption.
[0021] Furthermore, the SiC-CVD process tail gas based on the reaction of alkanes and silanes is a reaction cycle gas FTrPSA adjustable method, characterized in that under the condition that the silane concentration in the purified raw gas is relatively high, the purified raw gas, after being subjected to heat exchange to 5~20°C and pressurized to 0.6~1.0MPa, directly enters the shallow cold pressure swing adsorption concentration process composed of two-stage PSA, wherein the purified raw gas enters from the bottom of the first PSA adsorption tower (1-stage PSA) of the shallow cold pressure swing adsorption concentration process, the intermediate gas of the non-adsorbed phase flowing out from the top of the 1-stage PSA in the adsorption stage enters the second PSA adsorption tower (2-stage PSA), and the intermediate gas of the non-adsorbed phase flowing out from the top of the 2-stage PSA in the desorption step enters the second PSA adsorption tower (2-stage PSA). The concentrated gas flowing out from the bottom of the A adsorption tower is mixed with the purified methane and hydrogen gas after subsequent adsorption purification in a proportion and recycled for use as a circulating reaction gas for the SiC-CVD crystal or thin film epitaxial growth process based on the reaction of methane and silane. The 2nd stage PSA is desorbed by displacement and vacuum regeneration, and the displacement gas comes from the crude silane gas in the subsequent medium-shallow cold distillation process to adjust the C / Si ratio in the reaction circulating gas to meet the needs of the SiC-CVD process. The intermediate gas flowing out from the top of the 2nd stage PSA adsorption tower in the adsorption step enters the subsequent adsorption purification process, and the desorbed gas flowing out from the bottom of the 1st stage PSA adsorption tower in the desorption step is used as a carbon dioxide-rich gas and enters the medium-shallow temperature condensation process.
[0022] Furthermore, the SiC-CVD process tail gas based on the reaction of alkanes and silanes is a reaction cycle gas FTrPSA adjustable method, characterized in that the PSA adsorption tower in the desorption step in the medium-temperature pressure swing adsorption or shallow cold pressure swing adsorption concentration process includes 1 stage PSA and 2 stages PSA, and the desorption steps are equal pressure drop, sequential release, vacuuming, equal pressure increase and final filling, wherein the desorption steps for forming concentrated gas in the medium-temperature or shallow cold pressure swing adsorption process are replacement, equal pressure drop, sequential release, vacuuming, equal pressure increase and final filling, and the replacement gas comes from the crude silane gas of the subsequent process, and the final filling gas adopts the feed gas of each front-end process.
[0023] Furthermore, the SiC-CVD process tail gas based on the reaction of alkanes and silanes is a reaction cycle gas FTrPSA adjustable method, characterized in that the concentrations of CH4, C2+, and H2 in the concentrated gas are adjusted by adjusting the operation time of the adsorption and desorption steps in the medium-temperature pressure swing adsorption and shallow cold pressure swing adsorption concentration processes, the one or more combined adsorbents including aluminum oxide, silica gel, activated carbon and molecular sieves loaded in the adsorption tower and their quantities, and the switching degree of the program control valve or other valves loaded on the pipeline connecting the adsorption towers, so as to achieve proportional and The crude silane gas from the subsequent process forms a mixed gas and serves as the circulating reaction gas for the SiC-CVD crystal and thin film growth process, and enters the SiC-CVD reactor (chamber) to continue the reaction. Among them, when the operating pressure of the medium-temperature pressure swing adsorption, shallow cold pressure swing adsorption concentration or adsorption purification process is greater than 0.6MPa, the pressure changes during the adsorption and desorption cycle operation are controlled slowly and evenly through the program control valves and regulating valves on the pipelines connecting the adsorption towers to prevent the airflow from scouring the adsorption tower bed and the adsorbent from being pulverized due to excessive changes in the system pressure, so that the operation of this process system is stable and safe.
[0024] The beneficial effects of the present invention are:
[0025] (1) Through the present invention, the tail gas of the SiC-CVD crystal or thin film epitaxial growth process based on the reaction of methane and silane can be used as the circulating gas of the CVD reaction, and the deposition efficiency and quality of the SiC crystal or thin film can be greatly improved by adjusting the concentration and flow rate of each component in the circulating reaction gas, thereby realizing the comprehensive utilization of the tail gas and reducing the tail gas emission, thus filling the gap in the tail gas treatment technology of the SiC-CVD process;
[0026] (2) The present invention utilizes the physical and chemical characteristics and relative separation coefficients of H2, CH4 / C2+, and SiH4 components in the tail gas within the range of medium temperature 30-80°C, shallow cooling 5-20°C, and medium-shallow cooling -35--10°C, and selectively separates H2 / CH4 from C2+ / SiH4 through medium temperature pressure swing adsorption, shallow cooling pressure swing adsorption concentration, and medium-shallow temperature condensation and medium-shallow cooling distillation. The concentrated gas from the shallow cooling pressure swing adsorption concentration process and the silane or C2+ obtained from the medium-shallow cooling distillation, as well as the methane hydrogen gas obtained from the adsorption purification process, can be adjusted and mixed in a desired proportion, and then recycled as a reaction cycle gas for the SiC-CVD process based on the reaction of methane and silane, thereby solving the technical bottleneck of the traditional adsorption separation process that is difficult to use tail gas as a reaction cycle gas, and filling the technical gap in the comprehensive utilization of tail gas.
[0027] (3) The present invention can realize the comprehensive utilization of process tail gas as reaction circulating gas according to the concentration of CH4 / C2+, H2 and Si in the tail gas and the required ratio of circulating reaction gas, through medium temperature pressure swing adsorption or shallow cold pressure swing adsorption concentration of two-stage PSA or combination, shallow cold oil absorption replacing medium temperature pressure swing adsorption and other combinations, the adsorption and desorption cycle operation time of the adsorption tower, the type and quantity of adsorbent, and the replacement of the desorption step of the shallow cold pressure swing adsorption concentration process.
[0028] (4) The present invention does not need to completely and clearly separate the effective components in the tail gas of the SiC-CVD crystal or thin film epitaxial growth process based on the reaction of alkanes and silanes, which saves the cost of comprehensive utilization of the tail gas and the consumption of raw gas required for the process, thereby further reducing the cost of SiC crystals or epitaxial wafers obtained by the SiC-CVD process and further improving the deposition efficiency and product quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 This is a schematic diagram of the process of Example 1 of the present invention.
[0030] Figure 2 This is a schematic diagram of the process of Example 2 of the present invention.
[0031] Figure 3 This is a schematic diagram of the process of Example 3 of the present invention.
[0032] Figure 4 This is a schematic diagram of the process of Example 4 of the present invention.
[0033] Figure 5 This is a schematic diagram of the process of Example 5 of the present invention.
[0034] Figure 6 This is a schematic diagram of the process of Example 6 of the present invention.
[0035] Figure 7This is a flow chart of Example 7 of the present invention. DETAILED DESCRIPTION
[0036] In order to enable those skilled in the art to better understand the present invention, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the accompanying drawings in the embodiments of the present invention.
[0037] Example 1
[0038] like Figure 1 As shown, a method for adjusting the tail gas of SiC-CVD process based on the reaction of alkane and silane as reaction cycle gas FTrPSA, the specific implementation steps include:
[0039] (1) Raw gas: tail gas from a chlorine-free process in which propane (C3H8) is used as the main carbon (C) source and silane (SiH4) is used as the silicon (Si) source for chemical vapor deposition (CVD) to prepare silicon carbide (SiC) crystals or epitaxial growth on substrates. Its main components are hydrogen (H2), methane (CH4), silane (SiH4), a small amount of alkanes with carbon 2 or higher components (C2+), trace amounts of carbon monoxide (CO), carbon dioxide (CO2), high-silicon hydrocarbons, as well as silicon dioxide (SiO2) and carbon (C) fine particles, at normal pressure and temperature.
[0040] (2) Pretreatment: The raw gas is pressurized and sent to a pretreatment unit consisting of a dust collector, a particle filter, and an oil mist collector. Under the operating conditions of 0.2~0.3MPa pressure and room temperature, dust, particles, oil mist, some high alkanes, and high silane impurities are removed successively. The resulting purified raw gas is subjected to heat exchange to 30~80℃ and pressurized to 0.6~1.0MPa before entering the medium-temperature pressure swing adsorption process.
[0041] (3) Medium-temperature pressure swing adsorption: the purified raw gas from the pretreatment process enters a multi-tower pressure swing adsorption process consisting of 5 towers. The operating pressure of the adsorption tower is 0.6~1.0MPa, and the operating temperature is 30~80℃. One of the adsorption towers is in the adsorption step. The non-adsorbed phase gas flowing out from the top of the adsorption tower in the adsorption step is the intermediate gas. After heat exchange to 5~20℃, it enters shallow cold pressure swing adsorption concentration. The carbon dioxide-rich gas flowing out from the bottom of the adsorption tower in the desorption step, which mainly includes CO2, C2+ and a small amount of H2 / CH4 / SiH4, enters the medium-shallow temperature condensation process after pressurization.
[0042] (4) Shallow cold pressure swing adsorption concentration: the intermediate gas from the medium temperature pressure swing adsorption process at 5~20℃ and 0.6~1.0MPa enters a multi-tower pressure swing adsorption concentration process consisting of 4 towers. The operating pressure of the adsorption tower is 0.6~1.0MPa and the operating temperature is 5~20℃. One of the adsorption towers is in the adsorption step, and the other adsorption towers are in the desorption regeneration step. The non-adsorbed phase gas flowing out from the top of the adsorption tower in the adsorption step is methane hydrogen gas entering the adsorption purification process. The adsorbed phase gas formed at the bottom of the adsorption tower in the desorption step is The concentrated gas is mixed with the purified methane hydrogen gas from the subsequent adsorption purification in a proportion and recycled for use as a circulating reaction gas for the SiC-CVD crystal or thin film epitaxial growth process based on the reaction of alkanes and silanes. The adsorbent of the shallow cold pressure swing adsorption concentration process adopts a combination of activated alumina, silica gel, activated carbon, and molecular sieves. Displacement and vacuum regeneration are used during desorption. The displacement gas comes from the crude silane gas of the subsequent medium and shallow cold distillation process to adjust the C / Si ratio in the reaction cycle gas to meet the needs of the SiC-CVD process.
[0043] (5) Adsorption purification: the methane hydrogen gas from the shallow cold pressure swing adsorption concentration process enters the adsorption purification process consisting of two adsorption towers after precision filtration, and is adsorbed at an operating temperature of 5~20℃ and an operating pressure of less than 1.0MPa to further purify and remove trace amounts of CO, forming purified methane hydrogen gas. A part of it is mixed with the concentrated gas from the shallow cold pressure swing adsorption concentration process in a suitable ratio and returned to the SiC-CVD crystal or thin film epitaxial growth process as a reaction circulating gas for recycling, and a part of it is used as fuel gas for heating.
[0044] (6) Medium-shallow temperature condensation: the carbon dioxide-rich gas from the medium-temperature pressure swing adsorption process is finely filtered to remove fine particles, then subjected to heat exchange to -35~-20℃ and pressurized to 2.0~2.5MPa, and enters a medium-shallow cold condenser with an operating temperature of -35~-20℃. The non-condensable gas escaping from the condenser passes through a heat exchanger to a temperature of 5~20℃, and is depressurized to less than 1.0MPa before returning to the shallow cold pressure swing adsorption concentration process. The condensed fluid rich in SiH4 / C3H8 and trace amounts of easily condensable impurities including carbon dioxide (CO2) flowing out of the condenser directly enters the medium-shallow cold distillation.
[0045] (7) Medium-shallow cold distillation: the condensed fluid produced in the medium-shallow cold condensation process enters the medium-shallow cold distillation tower-1 with an operating temperature of -35~-2℃ and an operating pressure of 2.0~2.5MPa. A small amount of non-condensable gas of light components flows out from the top of the distillation tower-1, passes through a cold-heat exchanger to a temperature of 5~20℃ and a pressure reduction of less than 1MPa, and then returns to the shallow cold pressure swing adsorption concentration process for feeding. The heavy component fluid flowing out from the bottom of the distillation tower-1 enters the medium-shallow cold distillation tower-2 with an operating temperature of -25~-10℃ and an operating pressure of 1.5~2.5MPa, and the heavy component fluid flows out from the top of the distillation tower-2. The top gas of crude SiH4 from methane hydrogen is used as replacement gas for the shallow pressure swing adsorption concentration process to adjust the C / Si ratio in the reaction circulating gas to meet the needs of the SiC-CVD process. The heavy components enriched in C3H8 flow out from the bottom of the tower and, after decarbonization (CO2), are used as reaction circulating gas. The gas is mixed in proportion with the concentrated gas from the shallow pressure swing adsorption concentration process, the purified methane hydrogen gas from the adsorption purification process, and the crude silane gas from the top of the tower of this process used for the replacement gas of the shallow pressure swing adsorption concentration process, and the gas is returned to the SiC-CVD process as reaction circulating gas for recycling.
[0046] Example 2
[0047] like Figure 2 As shown, on the basis of Example 1, when the raw gas "C source" is only methane, there is one distillation tower in the medium-shallow cold distillation process, namely, distillation tower-1, and distillation tower-2 is omitted. That is, the condensed fluid produced in the medium-shallow temperature condensation process enters the medium-shallow cold distillation tower-1 with an operating temperature of -35~-20°C and an operating pressure of 2.0~2.5MPa, and crude SiH4 gas containing methane hydrogen flows out from the top of the distillation tower-1 as the replacement gas for the shallow cold pressure swing adsorption concentration process to adjust the C / Si ratio in the reaction cycle gas to meet the needs of the SiC-CVD process, and a small amount of heavy components enriched in CO2 flows out from the bottom of the tower for direct discharge.
[0048] Example 3
[0049] like Figure 3 As shown, based on Examples 1 and 2, under the conditions that the raw gas "C source" is only methane and the CO2 content in the purified raw material is less than 10 ppm, the carbon dioxide-rich desorption gas flowing out from the medium-temperature pressure swing adsorption process, after being adsorbed and purified to remove CO2, a part of it is used as the replacement gas of the shallow-cold pressure swing adsorption concentration process to form a reaction cycle gas for recycling, and a part of it is used as fuel gas after being washed and oxidized with water vapor, thereby eliminating the medium-shallow temperature condensation and medium-shallow cold distillation steps.
[0050] Example 4
[0051] like Figure 4As shown, on the basis of Examples 1 and 2, the raw gas "C source" is only methane and the CO2 content in the purified raw gas is greater than 0.1%, and the purified raw gas from the pretreatment process first enters the decarbonization process for decarbonization, and the CO2 therein is removed by an adsorption method loaded with a disposable adsorbent. The purified raw gas from which CO2 has been removed is directly entered into the shallow cold pressure swing adsorption concentration process after being subjected to heat exchange to 5~20°C and pressurized to 0.6~1.0MPa. The concentrated gas flowing out from the bottom of the adsorption tower in the desorption step is mixed with the purified methane hydrogen gas after subsequent adsorption purification according to a ratio, and is recycled as a circulating reaction gas for the SiC-CVD crystal or thin film epitaxial growth process based on the reaction of methane and silane, thereby eliminating the medium-temperature pressure swing adsorption, medium-shallow temperature condensation and medium-shallow cold distillation processes.
[0052] Example 5
[0053] like Figure 5 As shown, on the basis of Example 1, under the condition that the purified raw gas contains a relatively high concentration of C2+, wherein the C2+ component is mainly composed of 15% C3H8 and a small amount of ethane (C2H6), the purified raw gas enters the medium-temperature pressure swing adsorption process composed of two-stage PSA after heat exchange and pressurization, and the purified raw gas enters from the bottom of the first PSA adsorption tower (1-stage PSA) of the medium-temperature pressure swing adsorption, and the intermediate gas of the non-adsorbed phase flowing out from the top of the 1-stage PSA tower in the adsorption stage enters the shallow cold pressure swing adsorption concentration process, and the desorbed gas flowing out from the 1-stage PSA adsorption tower in the desorption step enters from the bottom of the second PSA adsorption tower (2-stage PSA) after pressurization, and the desorbed gas flowing out from the bottom of the 2-stage PSA adsorption tower in the desorption step enters the medium-shallow temperature condensation process as carbon dioxide-rich gas, and the non-adsorbed phase gas flowing out from the top of the 2-stage PSA adsorption tower in the adsorption step is mixed with the purified raw gas as feed gas and returned to the 1-stage PSA adsorption tower.
[0054] Example 6
[0055] like Figure 6As shown, based on Example 1, when the purified raw gas contains a very high concentration of C2+, for example, the C2+ / Si ratio exceeds 5:1, the purified raw gas is subjected to cold and heat exchange to -35~-15°C and compressed to 2.5~3.5MPa, and a shallow cold oil absorption process is used to replace the medium temperature pressure swing adsorption process, that is, the shallow cold oil absorption process consists of an absorption tower and a desorption tower, propane (C3) is used as the absorbent, the absorption temperature is -35~-15°C, the absorption pressure is 2.5~3.5MPa, and the desorption is The absorption temperature is normal temperature, and the desorption pressure is normal pressure. The purified raw gas enters from the bottom of the absorption tower and conducts reverse mass transfer with the C3 absorbent sprayed from the top of the absorption tower. The non-condensable intermediate gas escaping from the top of the absorption tower enters the shallow cold pressure swing adsorption concentration. The C2+-rich liquid flowing out from the bottom of the absorption tower enters the desorption tower. The C2+-rich gas flowing out from the top of the desorption tower directly enters the subsequent medium-shallow temperature condensation process. The absorbent C3 flows out from the bottom of the desorption tower, and after cyclic pressurization, it returns to the top of the absorption tower as an absorbent for spraying absorption.
[0056] Example 7
[0057] like Figure 7 As shown, based on Example 1, under the condition that the silane concentration in the purified raw gas is relatively high, the purified raw gas is subjected to heat exchange to 5-20°C and pressurized to 0.6-1.0 MPa, and then directly enters the shallow cold pressure swing adsorption concentration process composed of two-stage PSA, wherein the purified raw gas enters from the bottom of the first PSA adsorption tower (1-stage PSA) of the shallow cold pressure swing adsorption concentration process, and the non-adsorbed intermediate gas 1 flowing out from the top of the 1-stage PSA in the adsorption stage enters the second PSA adsorption tower (2-stage PSA), and the concentrated gas flowing out from the bottom of the 2-stage PSA adsorption tower in the desorption step is combined with the purified gas from the subsequent adsorption purification. The methane and hydrogen gases are mixed in proportion and recycled as circulating reaction gas for SiC-CVD crystal or thin film epitaxial growth process based on the reaction of alkanes and silanes. Displacement and vacuum regeneration are adopted during desorption of the 2nd stage PSA. The displacement gas comes from the crude silane gas in the subsequent medium-shallow cold distillation process to adjust the C / Si ratio in the reaction circulating gas to meet the needs of the SiC-CVD process. The intermediate gas 2 flowing out from the top of the 2nd stage PSA adsorption tower in the adsorption step enters the subsequent adsorption purification process. The desorbed gas flowing out from the bottom of the 1st stage PSA adsorption tower in the desorption step is used as carbon dioxide-rich gas and enters the medium-shallow temperature condensation process.
[0058] Obviously, the above-described embodiments are only a part of the embodiments of the present invention, but not all of them. Based on the embodiments recorded in the present invention, all other embodiments obtained by those skilled in the art without creative work, or structural changes made under the enlightenment of the present invention, all of which have the same or similar technical solutions as the present invention, fall within the protection scope of the present invention.
Claims
1. A FTrPSA adjustable separation method based on the reaction of alkanes and silanes with the tail gas of SiC-CVD process as reaction cycle gas, characterized in that: The steps include: (1) Raw gas, the tail gas in the chlorine-free process of preparing silicon carbide SiC crystals or epitaxial growth on substrates by chemical vapor deposition CVD using methane CH4 or propane C3H8 as the main carbon C source and silane SiH4 as the silicon Si source, its main components are hydrogen H2, methane CH4, silane SiH4, A small amount is recorded as "C2 + "C2 and above alkanes, trace amounts of carbon monoxide CO, carbon dioxide CO2, C5 and above high-silicon alkanes, as well as silicon dioxide SiO2 and carbon C fine particles, the pressure is normal pressure or a low pressure of less than or equal to 0.1MPa, and the temperature is room temperature; (2) Pretreatment: The raw gas is pressurized and sent to a pretreatment unit consisting of a dust collector, a particle filter, and an oil mist collector. Under the operating conditions of 0.2-0.3 MPa pressure and room temperature, dust, particles, oil mist, some C5 and higher alkanes, C5 and higher silane impurities are removed successively. The purified raw gas is subjected to heat exchange to 30-80°C and pressurized to 0.6-1.0 MPa before entering the next process - medium-temperature pressure swing adsorption process; (3) Medium-temperature pressure swing adsorption: the purified raw gas from the pretreatment process enters a multi-tower pressure swing adsorption process consisting of at least 4 towers. The operating pressure of the adsorption tower is 0.6-1.0 MPa, and the operating temperature is 30-80°C. At least one adsorption tower is in the adsorption step. The non-adsorbed phase gas flowing out from the top of the adsorption tower in the adsorption step is the intermediate gas. After being cooled to 5-20°C by heat exchange, it enters the next process - shallow cold pressure swing adsorption concentration. The carbon dioxide-rich gas flowing out from the bottom of the adsorption tower in the desorption step mainly includes CO2 and C2 + The components and a small amount of H2 / CH4 / SiH4 enter the subsequent medium-shallow temperature condensation process after being pressurized; (4) Shallow cold pressure swing adsorption concentration: the intermediate gas from the medium temperature pressure swing adsorption process at 5-20°C and 0.6-1.0MPa enters a multi-tower pressure swing adsorption concentration process consisting of at least 4 towers. The operating pressure of the adsorption tower is 0.6-1.0MPa and the operating temperature is 5-20°C. At least one adsorption tower is in the adsorption step, and the other adsorption towers are in the desorption regeneration step. The non-adsorbed phase gas flowing out from the top of the adsorption tower in the adsorption step is a methane-hydrogen gas composed of a mixed gas mainly composed of less than or equal to 10% methane and greater than or equal to 90% hydrogen. It enters the next process - adsorption purification. The adsorption phase gas formed at the bottom of the adsorption tower in the absorption step is a concentrated gas, which is mixed with the purified methane hydrogen gas from the subsequent adsorption purification according to a ratio and recycled as a circulating reaction gas for the SiC-CVD crystal or thin film epitaxial growth process based on the reaction of alkanes and silanes. Among them, the adsorbent of the shallow cold pressure swing adsorption concentration process adopts one or a combination of activated alumina, silica gel, activated carbon, and molecular sieves. During desorption, displacement and vacuum regeneration are adopted. The replacement gas comes from the crude silane gas of the subsequent medium and shallow cold distillation process to adjust the C / Si ratio in the reaction cycle gas to meet the needs of the SiC-CVD process. (5) Adsorption purification: the methane hydrogen gas from the shallow cold pressure swing adsorption concentration process enters the adsorption purification process consisting of two or three adsorption towers after precision filtration, and is adsorbed at an operating temperature of 5 to 20°C and an operating pressure of less than 1.0 MPa to further purify and remove trace amounts of CO, forming purified methane hydrogen gas. A portion of the gas is mixed with the concentrated gas from the shallow cold pressure swing adsorption concentration process in a suitable ratio and returned to the SiC-CVD crystal or thin film epitaxial growth process as a reaction circulating gas for recycling, and a portion of the gas is used as fuel gas for heating; (6) Medium-shallow temperature condensation: the carbon dioxide-rich gas from the medium-temperature pressure swing adsorption process is finely filtered to remove fine particles, then heat exchanged to -35 to -10°C, pressurized to 1.0 to 2.5 MPa, and enters a medium-shallow cold condenser with an operating temperature of -35 to -10°C. The non-condensable gas escaping from the medium-shallow cold condenser is passed through a heat exchanger to a temperature of 5 to 20°C, and directly or after being decompressed to less than 1.0 MPa, it is either returned to the shallow cold pressure swing adsorption concentration process or used as fuel gas for heating. The condensed fluid rich in SiH4 / C3H8 and trace amounts of easily condensable impurities including CO2 flowing out of the medium-shallow cold condenser directly enters the next process - medium-shallow cold distillation; (7) Medium-shallow cold distillation: the condensed fluid produced in the medium-shallow cold condensation process enters the distillation tower-1 with an operating temperature of -35 to -10°C and an operating pressure of 1.0 to 2.5 MPa. A small amount of non-condensable gas of light components flows out from the top of the distillation tower-1, or is returned to the shallow cold pressure swing adsorption concentration process as feed after being cooled to 5 to 20°C and reduced to less than 1 MPa through a cold-heat exchanger, or is used as fuel gas for heating. The heavy component fluid flowing out from the bottom of the distillation tower-1 enters the distillation tower-2 with an operating temperature of -35 to -10°C and an operating pressure of 1.0 to 2.5 MPa. The top gas of crude SiH4 containing methane hydrogen flows out from the top of the tower as the replacement gas for the shallow cold pressure swing adsorption concentration process to adjust the C / Si ratio in the reaction circulation gas to meet the needs of the SiC-CVD process. The heavy component enriched in C3H8 flows out from the bottom of the tower, and after decarbonization, it is used as the reaction circulation gas, mixed with the concentrated gas from the shallow cold pressure swing adsorption concentration process, the purified methane hydrogen gas from the adsorption purification process, and the crude silane gas from the top of this process used for the replacement gas of the shallow cold pressure swing adsorption concentration process in proportion, and returned to the SiC-CVD process as the reaction circulation gas for recycling.
2. The FTrPSA adjustable separation method of the SiC-CVD process tail gas based on the reaction of alkanes and silanes as claimed in claim 1, characterized in that: When the raw gas "C source" is only methane, there is one distillation tower in the medium-shallow cold distillation process, namely, distillation tower-1, and distillation tower-2 is omitted. That is, the condensed fluid produced in the medium-shallow temperature condensation process enters the distillation tower-1 with an operating temperature of -35 to -10°C and an operating pressure of 1.0 to 2.5 MPa. Crude SiH4 gas containing methane hydrogen flows out from the top of the distillation tower-1 as the replacement gas for the shallow cold pressure swing adsorption concentration process to adjust the C / Si ratio in the reaction cycle gas to meet the needs of the SiC-CVD process. A small amount of heavy components enriched in CO2 flows out from the bottom of the tower and are directly discharged.
3. The FTrPSA adjustable separation method of the SiC-CVD process tail gas based on the reaction of alkane and silane as claimed in claim 1, characterized in that: When the raw gas "C source" is only methane and the CO2 content in the purified raw material is less than 10ppm, the carbon dioxide-rich desorbed gas flowing out from the medium-temperature pressure swing adsorption process, after adsorption and decarbonization, is used as the replacement gas of the shallow-cold pressure swing adsorption concentration process to form a reaction cycle gas for recycling, and is used as fuel gas after being washed and oxidized by water vapor. The intermediate gas flowing out enters the shallow-cold pressure swing adsorption concentration process, thereby eliminating the medium-shallow temperature condensation and medium-shallow cold distillation processes.
4. The FTrPSA adjustable separation method of the SiC-CVD process tail gas based on the reaction of alkanes and silanes as claimed in claim 1, characterized in that: Under the working condition that the raw gas "C source" is only methane and the CO2 content in the purified raw gas is greater than 0.1%, the purified raw gas from the pretreatment process first enters the decarbonization process for decarbonization, and the CO2 therein is removed by an adsorption method loaded with a disposable adsorbent. The purified raw gas from which CO2 has been removed is directly entered into the shallow cold pressure swing adsorption concentration process after being subjected to heat exchange to 5-20°C and pressurized to 0.6-1.0MPa. The concentrated gas flowing out from the bottom of the adsorption tower in the desorption step is mixed with the purified methane hydrogen gas after subsequent adsorption purification according to a ratio, and is recycled as a circulating reaction gas for the SiC-CVD crystal or thin film epitaxial growth process based on the reaction of methane and silane, thereby eliminating the medium-temperature pressure swing adsorption, medium-shallow temperature condensation and medium-shallow cold distillation processes.
5. The FTrPSA adjustable separation method of the SiC-CVD process tail gas based on the reaction of alkanes and silanes as claimed in claim 1, characterized in that: The purified raw gas contains C2 + Under the working condition that the concentration is greater than or equal to 0.1-1.0%, the purified raw gas from the pretreatment process enters the medium-temperature pressure swing adsorption process composed of two-stage PSA after heat exchange and pressurization, wherein the purified raw gas enters from the bottom of the first PSA adsorption tower denoted as "1#PSA" for medium-temperature pressure swing adsorption, and the intermediate gas of the non-adsorbed phase flowing out from the top of the 1#PSA tower in the adsorption stage enters the shallow cold pressure swing adsorption concentration process, and the desorbed gas flowing out from the 1#PSA adsorption tower in the desorption step enters from the bottom of the second PSA adsorption tower denoted as "2#PSA" after pressurization, and the desorbed gas flowing out from the bottom of the 2#PSA adsorption tower in the desorption step enters the medium-shallow temperature condensation process as carbon dioxide-rich gas, and the non-adsorbed phase gas flowing out from the top of the 2#PSA adsorption tower in the adsorption step is mixed with the purified raw gas as feed gas and returned to the 1#PSA adsorption tower.
6. The FTrPSA adjustable separation method of SiC-CVD process tail gas based on the reaction of alkane and silane as claimed in claim 1, characterized in that: The purified raw gas contains C2 + Under the working condition that the concentration is greater than or equal to 1-5%, the purified raw gas from the pretreatment process is subjected to heat exchange to -35--15°C and compressed to 2.5-3.5MPa, and the medium-temperature pressure swing adsorption process is replaced by a shallow cold oil absorption process, that is, the shallow cold oil absorption process is composed of an absorption tower and a desorption tower, and propane C3H8 is used as the absorbent, the absorption temperature is -35--15°C, the absorption pressure is 2.5-3.5MPa, the desorption temperature is room temperature, and the desorption pressure is normal pressure or slightly positive pressure. The purified raw gas enters from the bottom of the absorption tower and conducts reverse mass transfer with the C3H8 absorbent sprayed from the top of the absorption tower. The non-condensable intermediate gas escaping from the top of the absorption tower enters the subsequent shallow cold pressure swing adsorption concentration, and the rich C2 + Liquid enters the desorption tower, and C2-rich liquid flows out from the top of the desorption tower. + The gas directly enters the subsequent medium-shallow temperature condensation process, and the absorbent C3H8 flows out from the bottom of the desorption tower. After circulating pressurization, it returns to the top of the absorption tower as an absorbent for spray absorption.
7. The FTrPSA adjustable separation method of SiC-CVD process tail gas based on the reaction of alkane and silane as claimed in claim 1, characterized in that: Under the condition that the silane concentration in the purified raw gas is greater than or equal to 0.1-1.0%, the purified raw gas, after being subjected to heat exchange to 5-20°C and pressurized to 0.6-1.0MPa, directly enters the shallow cold pressure swing adsorption concentration process composed of two-stage PSA, wherein the purified raw gas enters from the bottom of the first PSA adsorption tower recorded as "1#PSA" in the shallow cold pressure swing adsorption concentration process, and the non-adsorbed intermediate gas 1 flowing out from the top of the 1#PSA tower in the adsorption stage enters the second PSA adsorption tower recorded as "2#PSA", and the concentrated gas flowing out from the bottom of the 2#PSA adsorption tower in the desorption step is mixed with the gas from the subsequent adsorption tower. The purified methane and hydrogen gases are mixed according to the proportion and recycled as the circulating reaction gas for the SiC-CVD crystal or thin film epitaxial growth process based on the reaction of methane and silane. The 2#PSA is desorbed by displacement and vacuum regeneration, and the displacement gas comes from the crude silane gas in the subsequent medium-shallow cold distillation process to adjust the C / Si ratio in the reaction circulating gas to meet the needs of the SiC-CVD process. The intermediate gas 2 flowing out from the top of the 2#PSA adsorption tower in the adsorption step enters the subsequent adsorption purification process, and the desorbed gas flowing out from the bottom of the 1#PSA adsorption tower in the desorption step is used as a carbon dioxide-rich gas and enters the medium-shallow temperature condensation process.
8. The FTrPSA adjustable separation method of SiC-CVD process tail gas based on the reaction of alkane and silane as claimed in claim 1, characterized in that: The PSA adsorption tower in the desorption step in the medium-temperature pressure swing adsorption or shallow cold pressure swing adsorption concentration process includes 1#PSA and 2#PSA, and its desorption steps are equal pressure drop, sequential discharge, vacuum pumping, equal pressure increase and final filling, wherein the desorption steps for forming concentrated gas in the medium-temperature or shallow cold pressure swing adsorption process are replacement, equal pressure drop, sequential discharge, vacuum pumping, equal pressure increase and final filling, and the replacement gas comes from the crude silane gas of the subsequent process, and the final filling gas adopts the feed gas of each front-end process.
9. The FTrPSA adjustable separation method of SiC-CVD process tail gas based on the reaction of alkane and silane as claimed in claim 1, characterized in that: The concentration of CH4, C2 in the concentrated gas can be adjusted by adjusting the operation time of the adsorption and desorption steps in the medium temperature pressure swing adsorption and shallow cold pressure swing adsorption concentration process, the amount of one or more combined adsorbents including aluminum oxide, silica gel, activated carbon and molecular sieve loaded in the adsorption tower, and the opening and closing degree of the program control valve or other valves installed on the pipeline connecting the adsorption towers. + , H2 concentration, thereby forming a mixed gas in proportion with the crude silane gas from the subsequent process, and serving as the circulating reaction gas for the SiC-CVD crystal and thin film growth process, and entering the SiC-CVD reactor to continue the reaction. Among them, when the operating pressure of the medium-temperature pressure swing adsorption, shallow cold pressure swing adsorption concentration or adsorption purification process is greater than 0.6MPa, the pressure changes during the adsorption and desorption cycle operation are controlled slowly and evenly through the program control valves and regulating valves on the pipelines connecting the adsorption towers, so as to prevent the airflow from scouring the adsorption tower bed and the adsorbent from being pulverized due to excessive changes in the system pressure, so that the operation of this process system is stable and safe.