Coating equipment
By using independent process lines and multiple side-by-side coating lines in the coating equipment of SHJ solar cells, combining hot wire chemical vapor deposition method and transfer parts, the cross-contamination problem between the coating processes is solved and the solar panels is improved Photoelectric conversion efficiency and reduce equipment costs.
Patent Information
- Application Number
- CN202011616393.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-12-30
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2040-12-30
AI Technical Summary
In the intrinsic amorphous silicon thin film and doped amorphous silicon thin film production process of SHJ solar cells, there is a problem of cross-contamination between the coating processes, resulting in a degradation of performance.
A coating equipment was designed to coat the substrate by using independent process lines in the hot wire chemical vapor deposition method to prevent cross-contamination between the P-type doped silicon-based film and other coating processes. Multiple process lines were used The coating is carried out side by side, and the efficiency is improved using multiple hot wire coating sources, and the substrate is efficiently transported and flipped through the transfer components.
It effectively prevents cross-contamination between coating processes, improves the photoelectric conversion efficiency of solar panels, reduces the number of process chambers, and reduces equipment costs.
Smart Images

Figure CN112708868B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of but not limited to solar panel manufacturing technology, and in particular to a coating device. Background Art
[0002] In the process of manufacturing intrinsic amorphous silicon thin films and doped amorphous silicon thin films of SHJ solar cells, there are usually two known methods, plasma enhanced chemical vapor deposition (PECVD) and hot wire chemical vapor deposition (HWCVD).
[0003] In the known technology, it is believed that the performance of solar panels will be degraded when they are affected by water vapor, oxygen, dust, etc. in the air, and therefore an integrated process line is designed to simultaneously complete the coating stacking of the single-sided intrinsic amorphous silicon thin film and the doped (n or p) amorphous silicon thin film of the solar panel. However, this integrated process line has the technical problem of cross contamination between different coating processes. Summary of the invention
[0004] The present invention aims to solve the technical problems existing in the known technologies to at least a certain extent. To this end, the present invention proposes a coating device that can effectively reduce the technical problem of cross contamination between coating processes.
[0005] According to an embodiment of one aspect of the present invention, a coating device can be used to coat a substrate in a hot wire chemical vapor deposition method, and the coating device includes at least two process lines for coating the substrate, and the process lines are connected by a transmission device. Among the process lines, a first process line is included, and in the first process line, a first coating chamber is only provided as a coating chamber for coating a P-type doped silicon-based thin film on one side of the substrate.
[0006] The coating equipment according to the present invention has at least the following beneficial effects: since an independent process line (i.e., the first process line) is used to coat a P-type doped silicon-based thin film on one side of a substrate, cross contamination between the coating of a P-type doped silicon-based thin film on one side of the substrate and other coating processes can be prevented.
[0007] In some embodiments, the process line further includes a second process line, wherein the second process line is provided with a second coating chamber for coating an n-type doped silicon-based thin film on the other side of the substrate.
[0008] In some embodiments, the second process line is further provided with a third coating chamber for coating an intrinsic amorphous silicon thin film on one side of the substrate, and a fourth coating chamber for coating an intrinsic amorphous silicon thin film on the other side of the substrate, and the third coating chamber and the fourth coating chamber are respectively provided at the front end of the second coating chamber.
[0009] In some embodiments, the process lines are respectively configured to coat each side of a plurality of the substrates arranged side by side at intervals.
[0010] In some embodiments, a first coating source is disposed in the first coating chamber, and the first coating source includes a plurality of hot wires disposed along the transmission direction of the substrate; the substrate includes two pieces, and when the substrate is coated with a P-type doped silicon-based thin film, the two substrates are respectively located on both sides of the first coating source.
[0011] In some embodiments, a second coating source is disposed in the second coating chamber, and the second coating source includes a plurality of hot wires disposed along the transmission direction of the substrate; the substrate includes two pieces, and when the substrate is coated with an n-type doped silicon-based thin film, the two substrates are respectively located on both sides of the second coating source.
[0012] In some embodiments, one of the third coating chamber and the fourth coating chamber is provided with a third coating source, and the third coating source includes a plurality of hot wires arranged along the transmission direction of the substrate; the substrate includes two pieces, and when an intrinsic amorphous silicon thin film is coated on one side of the substrate, the two substrates are respectively located on both sides of the third coating source.
[0013] In some embodiments, the other one of the third coating chamber and the fourth coating chamber is provided with two fourth coating sources, the two fourth coating sources are arranged side by side, and the two fourth coating sources respectively include a plurality of hot wires arranged along the transmission direction of the substrate; the substrate includes two pieces, and when the intrinsic amorphous silicon thin film is coated on the other side of the substrate, the two substrates are respectively located on the outside of the two fourth coating sources.
[0014] In some embodiments, it also includes: a first tray, loaded with the substrate located at the first process line; a second tray, loaded with the substrate located at the second process line; and a transfer unit, arranged between the second process line and the first process line, transferring the substrate loaded on the second tray to the first tray.
[0015] In some embodiments, the first tray is a shielded tray, and the second tray is a hollow tray. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a schematic diagram of an embodiment of the coating equipment of the present invention.
[0017] Figure 2 is a schematic diagram of the first tray.
[0018] Figure 3 is a schematic diagram of the second tray.
[0019] Figure 4 It is a schematic diagram of an embodiment of a product involved in the coating equipment of the present invention. DETAILED DESCRIPTION
[0020] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0021] In the description of the present invention, it should be understood that descriptions involving orientations, such as up, down, front, back, left, right, etc., and orientations or positional relationships indicated are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0022] In the description of the present invention, "several" means one or more, "more" means more than two, "greater than", "less than", "exceed" etc. are understood as not including the number itself, and "above", "below", "within" etc. are understood as including the number itself. If there is a description of "first" or "second", it is only used for the purpose of distinguishing the technical features, and cannot be understood as indicating or implying the relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.
[0023] In the description of the present invention, unless otherwise clearly defined, terms such as setting, installing, connecting, etc. should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above terms in the present invention based on the specific content of the technical solution.
[0024] In addition, in the following Figure 1 In the description, the front-to-back direction can also be understood as the order of the coating process. For example, the position of the device in the previous process is understood as "front", and the position of the device in the next process is understood as "back". The direction parallel to the paper surface is understood as the "horizontal direction", and the direction perpendicular to the paper surface is understood as the "vertical direction".
[0025] Figure 11 is a schematic diagram of an embodiment of a coating device 100. According to an embodiment of the present invention, the coating device 100 can be used for coating a substrate 201 (see FIG. 1 ) in a hot wire chemical vapor deposition method. Figure 4 , described later), the coating equipment 100 includes at least two process lines 101 for coating the substrate 201, the process lines 101 are connected by a transmission device 102, the process lines 101 include a first process line 103, and in the first process line 103, only a first coating chamber 104 for coating a P-type doped silicon-based film 203 on one side of the substrate 201 is provided as a coating chamber.
[0026] In this embodiment, since an independent process line (i.e., the first process line 103) is used to coat the P-type doped silicon-based film 203 on one side of the substrate 201, cross contamination between the coating of the P-type doped silicon-based film 203 on one side of the substrate 201 and other coating processes can be prevented.
[0027] Figure 4 Schematic diagram of a solar cell panel 200 manufactured by the coating device 100. Figure 4 Specifically, the substrate 201 used for coating can be, for example, an n-type single crystal silicon base layer of a solar cell panel 200. One side of the two sides of the n-type single crystal silicon base layer has, from the base layer toward the outside, an intrinsic amorphous silicon thin film 202, a P-type doped silicon-based thin film 203, a TCO layer 204 (transparent conductive layer), and an electrode 205 in sequence. The other side of the two sides of the n-type single crystal silicon base layer has, in sequence, an intrinsic amorphous silicon thin film 202, an n-type doped silicon-based thin film 206, a TCO layer 204, and an electrode 205. In addition, the material and shape of the substrate 201 are not particularly limited as long as they can be used as the material and shape of the solar cell panel 200.
[0028] Although it is believed in the known technology that the solar panel 200 will suffer performance degradation when it is affected by water vapor, oxygen, dust, etc. in the air. However, after demonstration, the inventors have not found that water vapor, oxygen, dust, etc. in the air have an impact on the solar panel 200 that is sufficient to cause its performance degradation. In addition, in actual production, the production environment of the solar panel 200 can be ensured by strengthening the management of the production workshop, such as producing the solar panel 200 in a dust-free workshop. In contrast, since the doped (p) amorphous silicon thin film coating stack has a more serious pollution on other thin film coatings, the inventors have fully demonstrated that it is more realistic to control the cross-contamination problem between coating processes. Therefore, in this embodiment, by making the coating process of coating the P-type doped silicon-based thin film 203 on the substrate 201 be completed on a different process line 101 relative to other coating processes such as coating the intrinsic amorphous silicon thin film 202 and the n-type doped silicon-based thin film 206, cross contamination between the coating process of the P-type doped silicon-based thin film 203 and other coating processes can be avoided, thereby improving the photoelectric conversion efficiency of the solar cell panel 200.
[0029] Specifically, in addition to the first coating chamber 104, the first process line 103 may also include, for example, a first feed chamber 105, a first heating chamber 106, a first discharge chamber 107, and a transmission device 102 for transmitting the substrate 201 therebetween. The first feed chamber 105, the first heating chamber 106, the first coating chamber 104, and the first discharge chamber 107 are arranged in sequence from front to back. The first feed chamber 105 is connected to other process lines 101 (such as the second process line 108 described below) through the transmission device 102. The first heating chamber 106 is arranged behind the first feed chamber 105 to heat the substrate 201 to be coated. The first coating chamber 104 is arranged behind the first heating chamber 106 to coat the preheated substrate 201 with a P-type doped silicon-based thin film 203. The first discharge chamber 107 is arranged behind the first coating chamber 104 to discharge the substrate 201 coated with the P-type doped silicon-based thin film 203. The transmission device 102 may be, for example, a roller line, which is used to transmit a tray (for example, the first tray 109 described later) loaded with the substrate 201 between the first feeding chamber 105, the first heating chamber 106, the first coating chamber 104, and the first discharging chamber 107. Each chamber is connected in sequence by, for example, a vacuum lock (not shown) known to those skilled in the art. In addition, each chamber may be equipped with a heating device and a heat preservation device. Electric partitions 110 are respectively provided at the connection points of each chamber to make each chamber independent of each other.
[0030] In some embodiments, in order to achieve coating of a doped (n) amorphous silicon film on the other side of the substrate 201, the process line 101 further includes a second process line 108, and the second process line 108 is provided with a second coating chamber 111 for coating an n-type doped silicon-based film 206 on the other side of the substrate 201. Specifically, the second process line 108 is independent of the first process line 103. For example, the second process line 108 is provided with a second discharge chamber 112 (described below) behind the second coating chamber 111. After the coating of the n-type doped silicon-based film 206 is completed in the second coating chamber 111, the substrate 201 is discharged through the second discharge chamber 112.
[0031] In order to realize the transfer of the substrate 201 from the second process line 108 to the first process line 103, a transfer unit 113, for example, including a six-axis robot for clamping the substrate 201, may be provided between the second process line 108 and the first process line 103, and the transfer unit 113 transfers the substrate 201 from the second process line 108 to the first process line 103. Specifically, the first process line 103 includes a first tray 109 for loading the substrate 201 located in the first process line 103, and the second process line 108 includes a second tray 114 for loading the substrate 201 located in the second process line 108. After the second tray 114 loaded with the substrate 201 is discharged through the second discharge chamber 112, the transfer unit 113, for example, a six-axis robot, clamps the substrate 201 on the second tray 114 and transfers it to the first tray 109.
[0032] In some embodiments, the second process line 108 is further provided with a third coating chamber 115 for coating an intrinsic amorphous silicon film 202 on one side of the substrate 201, and a fourth coating chamber 116 for coating an intrinsic amorphous silicon film 202 on the other side of the substrate 201, and the third coating chamber 115 and the fourth coating chamber 116 are respectively provided at the front end of the second coating chamber 111. As described above, since one side of the substrate 201 is coated with the intrinsic amorphous silicon film 202 and the P-type doped silicon-based film 203 from the inside to the outside, and the other side is coated with the intrinsic amorphous silicon film 202 and the n-type doped silicon-based film 206 from the inside to the outside, therefore, before the coating of the n-type doped silicon-based film 206 and the P-type doped silicon-based film 203 is completed, the intrinsic amorphous silicon film 202 needs to be coated on both sides of the substrate 201.
[0033] In addition, the second process line 108 may also include, for example, a second feed chamber 117, a second heating chamber 118, a second discharge chamber 112, and a transmission device 102 for transmitting the substrate 201 therebetween, in addition to the second coating chamber 111, the third coating chamber 115, and the fourth coating chamber 116. The second feed chamber 117, the second heating chamber 118, the fourth coating chamber 116, the third coating chamber 115, the second coating chamber 111, and the second discharge chamber 112 are arranged in sequence from front to back. The second feed chamber 117 is arranged at the front end of the second process line 108, and is connected to the loading device (not shown) of the substrate 201 through the transmission device 102. The second heating chamber 118 is arranged behind the second feed chamber 117 to heat the substrate 201 to be coated. The fourth coating chamber 116 and the third coating chamber 115 are arranged behind the second heating chamber 118 to coat the intrinsic amorphous silicon thin film 202 on the preheated substrate 201. The positions of the third coating chamber 115 and the fourth coating chamber 116 are not particularly limited, as long as they are disposed between the second coating chamber 111. The second coating chamber 111 is disposed behind the third coating chamber 115 and the fourth coating chamber 116. The second discharge chamber 112 is disposed behind the second coating chamber 111 to discharge the substrate 201 coated with the n-type doped silicon-based thin film 206.
[0034] In addition, although the above describes an example in which the intrinsic amorphous silicon thin film 202 on both sides of the substrate 201 and the n-type doped silicon-based thin film 206 on one side of the substrate 201 are integrated in one process line (i.e., the second process line 108), it is not limited to this. These coating processes can also be completed on multiple different process lines. In addition, although the above describes an example in which two coating chambers (the third coating chamber 115 and the fourth coating chamber 116) are used to complete the coating of the intrinsic amorphous silicon thin film 202 on both sides of the substrate 201, it is not limited to this. It is also possible to use only one coating chamber to complete the coating of the intrinsic amorphous silicon thin film 202 on both sides of the substrate 201.
[0035] In some embodiments, in order to improve production efficiency and reduce the number of coating chambers, the process line 101 (i.e., the first process line 103 and the second process line 104) are respectively configured to coat each side of a plurality of spaced and arranged substrates 201. Specifically, for example, coating of one side of a plurality of substrates 201 is completed in each coating chamber.
[0036] The following is a detailed description of each coating chamber for completing the coating of each side of the two substrates 201.
[0037] In some embodiments, a first coating source 119 is disposed in the first coating chamber 104, and the first coating source 119 includes a plurality of hot wires 120 disposed along the transmission direction of the substrate 201. When coating the substrate 201 with a P-type doped silicon-based thin film 203, two substrates 201 are respectively located on both sides of the first coating source 119. Specifically, the hot wires 120 as the first coating source 119 are not particularly limited as long as they can achieve non-directional heating and coat the substrates 201 located on both sides thereof. For example, they can be tungsten wires commonly used in hot wire chemical vapor deposition methods, which are used to heat the reaction gas to the process temperature of coating on the surface of the substrate 201. The heating of these hot wires 120 is non-directional, and the substrates 201 located on both sides thereof can be processed simultaneously. Therefore, the hot wires 120 in the first coating chamber 104 can simultaneously coat the opposite sides of the substrates 201 located on both sides thereof. The first coating source 119 may include three groups of hot wires 120 or four groups of hot wires 120, thereby improving the efficiency of coating. The multiple groups of hot wires 120 of the first coating source 119 may be spaced along the transmission direction (front-back direction) of the substrate 201, and each hot wire 120 may be arranged to extend in the vertical direction (vertical coating, i.e., the coating surface of the substrate 201 is perpendicular to the horizontal direction), or have a certain inclination angle relative to the vertical direction. In addition, each hot wire 120 of the first coating source 119 may also be arranged to extend in the horizontal direction (horizontal coating, i.e., the coating surface of the substrate 201 is parallel to the horizontal direction), or have a certain inclination angle relative to the horizontal direction. It should be noted that, here, the horizontal direction may be understood as a direction parallel to the ground (the paper surface in the attached figure), and the vertical direction may be understood as a direction of gravity (perpendicular to the paper surface in the attached figure). In addition, as long as it can be judged by the naked eye, the length direction of the hot wire 120 extends approximately in the vertical direction, or approximately in the horizontal direction.
[0038] Figure 2 is a schematic diagram of the first tray 109 carrying the substrate 201 in a vertical state, referring to Figure 2 And continue to refer to Figure 1 In addition, in order to prevent the first coating source 119 from causing contamination, plating around, etc. on the other side of the substrate 201 when coating one side of the two substrates 201, the first tray 109 of the first process line 103 may use a shielding tray. Specifically, the shielding tray is not particularly limited as long as it can prevent the coating material from contaminating the other side of the substrate 201. For example, a first receiving groove 122 for accommodating the substrate 201 may be opened on the first substrate 121 of the first tray 109, and the receiving groove 122 is configured not to penetrate the first substrate 121. In this way, it is possible to prevent the other side of the substrate 201 from being contaminated when coating the P-type doped silicon-based thin film 203 on one side of the substrate 201.
[0039] In some embodiments, a second coating source 123 is disposed in the second coating chamber 111, and the second coating source 123 includes a plurality of hot wires 120 disposed along the transmission direction of the substrate 201. When the substrate 201 is coated with an n-type doped silicon-based thin film 206, the two substrates 201 are respectively located on both sides of the second coating source 123. Specifically, the second coating source 123 can be arranged with reference to the first coating source 119, which will not be described in detail here. In addition, it should be noted that, since only one coating source is disposed in each of the first coating chamber 104 and the second coating chamber 111, and the opposite side of the substrate 201 located on both sides thereof is coated, the substrate 201 needs to be turned over before the substrate 201 is transferred from the second coating chamber 111 to the first coating chamber 104. Specifically, the transfer unit 113 may also include a turning mechanism (not shown) for turning over the substrate 201, and the turning mechanism may use a turning mechanism known to those skilled in the art, which will not be described in detail here.
[0040] In some embodiments, one of the third coating chamber 115 and the fourth coating chamber 116 is provided with a third coating source 124, and the third coating source 124 includes a plurality of hot wires 120 arranged along the transmission direction of the substrate 201. When the intrinsic amorphous silicon thin film 202 is coated on one side of the substrate 201, the two substrates 201 are respectively located on both sides of the third coating source 124. Specifically, the third coating chamber 115 can be adjacent to the second coating chamber 111, and the third coating source 124 is arranged in the third coating chamber 115. In addition, the third coating source 124 can be arranged with reference to the first coating source 119, and will not be described in detail here.
[0041] In addition, one of the third coating chamber 115 and the fourth coating chamber 116 is provided with two fourth coating sources 125, the two fourth coating sources 125 are arranged side by side, and the two fourth coating sources 125 respectively include a plurality of hot wires 120 arranged along the transmission direction of the substrate 201. When the intrinsic amorphous silicon thin film 202 is coated on the other side of the substrate 201, the two substrates 201 are respectively located outside the two fourth coating sources 125. Specifically, the fourth coating chamber 116 can be located in front of the third coating chamber 115, and the fourth coating source 125 is arranged in the fourth coating chamber 116. In the fourth coating chamber 116, according to the needs of the process, the two fourth coating sources 125 can be distributed at intervals along the horizontal direction of the fourth coating chamber 116, or can be distributed along the vertical direction of the fourth coating chamber 116. In addition, when the two fourth coating sources 125 are coating the side of the substrate 201 opposite thereto, the two fourth coating sources 125 can either coat the side of the substrate 201 opposite thereto at the same time or coat the side of the substrate 201 one after another. Those skilled in the art can control the fourth coating sources 125 by controlling the opening or closing of the control system as needed.
[0042] Figure 3 is a schematic diagram of the second tray 114 carrying the substrate 201 in a vertical state, referring to Figure 3 , and continue to refer to Figure 1 In addition, in the second process line 108, in order to coat both sides of the substrate 201, the second tray 114 is set as a hollow tray. Specifically, as long as the second tray 114 can achieve double-sided coating of the substrate 201, the hollowing method is not particularly limited. For example, in addition to the second accommodating groove 126 for accommodating the substrate 201, a through notch 127 can be opened on the second base plate 127 of the second tray 114, thereby enabling double-sided coating of the substrate 201.
[0043] It should be noted that in the above embodiments, the shapes and structures of the components that are not described in detail can be considered to be well known to those skilled in the art. For example, the configuration of the vacuum system for controlling the vacuum pressure in each coating chamber, the configuration of the ultrapure gas system for controlling the gas in each coating chamber, the installation method of the vacuum lock, the installation method of the electric partition 110, the installation method of the heating components and the insulation components in each chamber, etc., can be installed by those skilled in the art according to actual needs.
[0044] The following is a description of the process of manufacturing a solar panel 200 using the coating device 100 of the above embodiment. Specifically, the coating device 100 is used to manufacture a double-sided intrinsic amorphous silicon film 202 and a doped amorphous silicon film stack (a p-type doped silicon-based film 203 and an n-type doped silicon-based film 206) on both sides (hereinafter also referred to as the left side and the right side) of an n-type single crystal silicon base layer (hereinafter referred to as substrate 201).
[0045] Specifically, the coating equipment 100 is roughly U-shaped, including a second process line 108, a first process line 103, and a transfer part 113 connecting the rear end of the second process line 108 and the front end of the first process line 103. The second process line 108 includes, from front to back, a second feeding chamber 117, a second heating chamber 118, a fourth coating chamber 116, a third coating chamber 115, a second coating chamber 111, and a second discharging chamber 112. The chambers are isolated by an electric partition 110. The chambers are connected by a transmission device 102 such as a roller line. The transmission device 102 simultaneously transmits two second trays 114 side by side in the left and right directions. The second tray 114 is a hollow tray, and each second tray 114 carries a substrate 201. The substrate 201 is placed on the second tray 114 in a direction perpendicular to the horizontal plane. The first process line 103 includes, from front to back, a first feeding chamber 105, a first heating chamber 106, a first coating chamber 104, and a first discharging chamber 107. The chambers are isolated by an electric partition 110. The chambers are connected by a transmission device 102 such as a roller line. The transmission device 102 simultaneously transmits two first trays 109 arranged side by side in the left and right directions. The first tray 109 is a shielded tray, and each first tray 109 carries a substrate 201 from a second tray 114. The substrate 201 is placed on the first tray 109 in a direction perpendicular to the horizontal plane. In addition, the vacuum system, gas system, heating system (heating component and insulation component) of the coating equipment 100 are not shown in the figure.
[0046] After the second tray 114 enters the second process line 108 from the second feed chamber 117, it is preheated in the second heating chamber 118 and enters the fourth coating chamber 116. In the fourth coating chamber 116, two substrates 201 are located between two fourth coating sources 125 in the left-right direction. The fourth coating source 125 on the right coats the intrinsic amorphous silicon thin film 202 on the right side of the substrate 201 on the right, and the fourth coating source 125 on the left coats the intrinsic amorphous silicon thin film 202 on the left side of the substrate 201 on the left.
[0047] After the fourth coating chamber 116 completes coating on one side of the two substrates 201, the transfer device 102 transfers the second tray 114 to the third coating chamber 115. In the third coating chamber 115, the two substrates 201 are respectively located on both sides of the third coating source 124 in the left and right directions. The third coating source 124 coats the intrinsic amorphous silicon thin film 202 on the left side of the right substrate 201 and the right side of the left substrate 201.
[0048] After the fourth coating chamber 116 and the third coating chamber 115 finish coating the intrinsic amorphous silicon thin film 202 on both sides of the substrate 201, the transfer device 102 transfers the second tray 114 to the second coating chamber 111. In the second coating chamber 111, the two substrates 201 are respectively located on both sides of the second coating source 123 in the left and right directions, and the third coating source 124 coats the left side of the right substrate 201 with an n-type doped silicon-based thin film 206 and the right side of the left substrate 201 with an n-type doped silicon-based thin film 206.
[0049] After the second coating chamber 111 completes coating of the n-type doped silicon-based thin film 206 on one side of each substrate 201, the transfer device 102 transfers the second tray 114 to the second discharge chamber 112. After the vacuum in the second discharge chamber 112 is broken, the transfer unit 113 obtains the substrate 201 from the second tray 114, turns it over, and places it on the first tray 109.
[0050] After the first tray 109 obtains the substrate 201, the transmission device 102 of the first process line 103 transmits the first tray 109 to the first feeding chamber 105 and the first heating chamber 106 respectively. After the first heating chamber 106 completes preheating, the transmission device 102 transmits the first tray 109 to the first coating chamber 104. In the first coating chamber 104, the two substrates 201 are respectively located on both sides of the left and right directions of the first coating source 119, and the first coating source 119 respectively coats the left side surface of the substrate 201 on the right with a P-type doped silicon-based film 203, and coats the right side surface of the substrate 201 on the left with a P-type doped silicon-based film 203.
[0051] After the first coating chamber 104 completes coating of the P-type doped silicon-based thin film 203 on one side of each substrate 201, the transmission device 102 transfers the first tray 109 to the first discharge chamber 107. Thus, the double-sided intrinsic amorphous silicon thin film 202 is coated on the n-type monocrystalline silicon base layer (substrate 201) of the solar cell panel 200, and the n-type doped silicon-based thin film 206 is coated on one side and the P-type doped silicon-based thin film 203 is coated on the other side.
[0052] Therefore, the coating equipment 100 of the present invention uses an independent process line 101 (i.e., the first process line 103) to coat the P-type doped silicon-based thin film 203 on one side of the substrate 201. Therefore, cross contamination between the coating of the P-type doped silicon-based thin film 203 on one side of the substrate 201 and other coating processes can be prevented, thereby improving the photoelectric conversion efficiency of the solar cell panel 200.
[0053] In addition, the coating device 100 of the present invention can coat multiple substrates 201 at the same time, thereby reducing the number of process chambers and lowering the equipment cost.
[0054] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.
Claims
1. A coating device for coating a substrate of a solar panel in a hot wire chemical vapor deposition method, characterized in that: The coating equipment comprises at least two mutually independent process lines for coating the substrate, the process lines are connected by a transmission device, and the process lines include: A first process line, wherein in the first process line, only a first coating chamber for coating a P-type doped silicon-based thin film on one side of the substrate is provided as a coating chamber; a second process line, wherein the second process line is provided with a second coating chamber for coating an n-type doped silicon-based thin film on the other side of the substrate; A first tray, loading the substrate located in the first process line; A second tray, loading the substrate located at the second process line; The transfer unit is disposed between the second process line and the first process line, and transfers the substrate loaded on the second tray to the first tray after the second tray loaded with the substrate is unloaded.
2. The coating device according to claim 1, characterized in that: The second process line is also provided with a third coating chamber for coating an intrinsic amorphous silicon thin film on one side of the substrate, and a fourth coating chamber for coating an intrinsic amorphous silicon thin film on the other side of the substrate. The third coating chamber and the fourth coating chamber are respectively arranged at the front end of the second coating chamber.
3. The coating device according to claim 2, characterized in that: The first process line and the second process line are respectively configured to coat one side of a plurality of substrates arranged side by side at intervals.
4. The coating device according to claim 3, characterized in that: A first coating source is disposed in the first coating chamber, and the first coating source includes a plurality of hot wires disposed along a transmission direction of the substrate; The substrate comprises two pieces. When the substrate is coated with a P-type doped silicon-based thin film, the two substrates are respectively located on two sides of the first coating source.
5. The coating device according to claim 3, characterized in that: A second coating source is disposed in the second coating chamber, and the second coating source includes a plurality of hot wires disposed along a transmission direction of the substrate; The substrate comprises two pieces. When the substrate is coated with an n-type doped silicon-based thin film, the two substrates are respectively located on two sides of the second coating source.
6. The coating device according to claim 3, characterized in that: One of the third coating chamber and the fourth coating chamber is provided with a third coating source, and the third coating source includes a plurality of hot wires arranged along the transmission direction of the substrate; The substrate comprises two pieces. When an intrinsic amorphous silicon thin film is plated on one side of the substrate, the two substrates are respectively located on two sides of the third film-plating source.
7. The coating device according to claim 6, characterized in that: The other of the third coating chamber and the fourth coating chamber is provided with two fourth coating sources, the two fourth coating sources are arranged side by side, and the two fourth coating sources respectively include a plurality of hot wires arranged along the transmission direction of the substrate; The substrate comprises two pieces. When the intrinsic amorphous silicon thin film is plated on the other side of the substrate, the two substrates are respectively located outside the two fourth coating sources.
8. The coating device according to claim 1, characterized in that: The first tray is a shielded tray, and the second tray is a hollow tray.
Citation Information
Patent Citations
Coating device and coating equipment
CN211112215U
Coating equipment
CN214458304U
Metal organic chemical vapor deposition apparatus having satellite n-type and p-type doping chambers
US20110220025A1