A micro-disk cavity with integrated waveguide on chip and preparation method thereof
By setting up an extended cavity on the silicon oxide wafer and optimizing the waveguide structure, the problem of large transmission loss of the microdisk cavity is solved, the quality factor and output optical power of the microdisk cavity are improved, and its performance in nonlinear optical applications is enhanced.
Patent Information
- Application Number
- CN202110357339.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-04-01
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2041-04-01
AI Technical Summary
In the prior art, the transmission loss of the microdisk cavity of the integrated waveguide on chip is relatively large, which affects its application in nonlinear optics and other aspects.
By setting the second expansion cavity and the first expansion cavity on the silicon oxide wafer, the output loss of light in the silicon-based substrate is reduced, and the coupling of the waveguide structure and the microdisk cavity is optimized. The microdisk cavity is prepared by a dry etching process to form a Microdisk cavity to improve quality factor.
The transmission loss of light in the silicon oxide waveguide structure is reduced, the quality factor of the microdisk cavity and the power of the output light are improved, and the performance of the microdisk cavity with the integrated waveguide on chip in nonlinear optics.
Smart Images

Figure CN112925059B_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to optical technology, and in particular to a micro-disk cavity with an on-chip integrated waveguide and a preparation method thereof. Background Art
[0002] An optical microcavity is a tiny device that can confine light within a certain size of space and time. Due to its high quality factor Q and small mode volume, it can greatly enhance the interaction between light and matter. Therefore, optical microcavities play an important role in nonlinear optics, lasers, coherent optical communications, and sensing. Integrating optical waveguides for coupling on optical microcavities will effectively promote the development of all-optical integrated photonic devices.
[0003] The transmission loss of the micro-disk cavity of the on-chip integrated waveguide formed in the prior art is relatively large. Summary of the invention
[0004] The present invention provides a micro-disk cavity with an on-chip integrated waveguide and a preparation method thereof, which reduces the transmission loss of light in the waveguide structure and improves the quality factor of the micro-disk cavity.
[0005] In a first aspect, an embodiment of the present invention provides a micro-disk cavity with an on-chip integrated waveguide, the micro-disk cavity comprising:
[0006] An oxidized silicon wafer; the oxidized silicon wafer comprises a silicon-based substrate and a silicon oxide semiconductor layer;
[0007] The silicon oxide semiconductor layer includes a functional area and a non-functional area; the functional area includes a waveguide structure, a micro-disk structure and a first opening located in the micro-disk structure; the non-functional area includes a second opening; the micro-disk structure and the first opening constitute a micro-disk cavity;
[0008] A first extension cavity and a second extension cavity; the first extension cavity extends from the first opening into the silicon-based substrate along a direction perpendicular to the plane of the silicon-based substrate; the second extension cavity extends from the second opening into the silicon-based substrate along a direction perpendicular to the plane of the silicon-based substrate; the first extension cavity is connected to the second extension cavity; the vertical projections of the waveguide structure and the micro-disk structure on the silicon-based substrate are located in a connected structure formed by the first extension cavity and the second extension cavity.
[0009] Optionally, the thickness of the silicon oxide semiconductor layer at the non-opening position of the functional area is greater than the thickness of the silicon oxide semiconductor layer in the non-functional area.
[0010] Optionally, the waveguide structure is a linear waveguide structure;
[0011] Alternatively, the waveguide structure is a curved waveguide structure; and the vertical distance from each point on the curved waveguide structure to the micro-disk structure is a fixed value.
[0012] Optionally, a spacing distance L between the waveguide structure and the micro-disk structure satisfies: 0 μm≤L≤10 μm.
[0013] Optionally, the first opening is located in a central area of the micro-disk structure.
[0014] Optionally, the second opening is located at a side of the waveguide structure away from the micro-disk structure.
[0015] Optionally, a size of the first extended cavity at a contact surface between the silicon-based substrate and the silicon oxide semiconductor layer is larger than a size of the first opening;
[0016] A size of the second extended cavity at a contact surface between the silicon-based substrate and the silicon oxide semiconductor layer is larger than a size of the second opening.
[0017] In a second aspect, an embodiment of the present invention further provides a method for preparing a micro-disk cavity with an on-chip integrated waveguide, the method for preparing the micro-disk cavity with an on-chip integrated waveguide as described in the first aspect, the method comprising:
[0018] Providing a silicon oxide wafer; the silicon oxide wafer comprises a silicon-based substrate and a silicon oxide semiconductor layer; the silicon oxide semiconductor layer comprises a functional area and a non-functional area;
[0019] Etching the non-functional area of the silicon oxide semiconductor layer using a dry etching process, so that the functional area of the silicon oxide semiconductor layer forms a waveguide structure and a micro-disk structure;
[0020] The silicon oxide semiconductor layer in the micro-disk structure and the silicon oxide semiconductor layer in a part of the non-functional area are etched by a dry etching process to form a first opening in the micro-disk structure and a second opening in the non-functional area; the micro-disk structure and the first opening constitute a micro-disk cavity;
[0021] The silicon-based substrate is etched using the first opening structure and the second opening structure as masks to form a first extension cavity and a second extension cavity; the first extension cavity is connected to the second extension cavity; and the vertical projections of the waveguide structure and the micro-disk structure on the silicon-based substrate are located in the connecting structure formed by the first extension cavity and the second extension cavity.
[0022] Optionally, etching the silicon-based substrate using the first opening structure and the second opening structure as masks to form a first extended cavity and a second extended cavity comprises:
[0023] The silicon-based substrate is etched by an etching process using the first opening structure and the second opening structure as masks respectively, so as to form a first extended cavity and a second extended cavity; the size of the first extended cavity at the contact surface between the silicon-based substrate and the silicon oxide semiconductor layer is larger than the size of the first opening; the size of the second extended cavity at the contact surface between the silicon-based substrate and the silicon oxide semiconductor layer is larger than the size of the second opening;
[0024] Wherein, the reactants of the etching process include at least one of xenon difluoride, potassium hydroxide, tetramethylammonium hydroxide, or a mixture of nitric acid, hydrofluoric acid and acetic acid.
[0025] Optionally, the dry etching process includes a reactive plasma etching process or an inductively coupled plasma etching process.
[0026] The technical solution reduces the output loss of light in the silicon-based substrate by setting a second extended cavity, thereby reducing the transmission loss of light in the silicon oxide waveguide structure; at the same time, by setting a first extended cavity, the output loss of light coupled from the waveguide structure to the micro-disk cavity in the silicon-based substrate is reduced, and the quality factor of the micro-disk cavity is improved, thereby improving the power of the output light of the micro-disk cavity of the entire on-chip integrated waveguide, solving the problem of large transmission loss of the micro-disk cavity of the on-chip integrated waveguide in the prior art, and facilitating its application in nonlinear aspects. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 is a schematic structural diagram of a micro-disk cavity with an on-chip integrated waveguide provided by an embodiment of the present invention;
[0028] Figure 2 is a schematic diagram of a top view of a micro-disk cavity with an on-chip integrated waveguide provided by an embodiment of the present invention;
[0029] Figure 3 is along Figure 2 Schematic diagram of the cross-sectional structure of the micro-disk cavity with integrated waveguide on chip obtained by the A'B' section line;
[0030] Figure 4 is a schematic diagram of a top view of another micro-disk cavity with integrated waveguide on a chip provided by an embodiment of the present invention;
[0031] Figure 5 It is a schematic flow chart of a method for preparing a micro-disk cavity with an on-chip integrated waveguide provided by an embodiment of the present invention;
[0032] Figure 6-11 It is a process diagram of a micro-disk cavity with an on-chip integrated waveguide provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0033] The present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only parts related to the present invention, rather than all structures, are shown in the accompanying drawings.
[0034] Figure 1 is a schematic structural diagram of a micro-disk cavity with an on-chip integrated waveguide provided by an embodiment of the present invention, Figure 2 is a schematic diagram of a top view of a micro-disk cavity with an on-chip integrated waveguide provided by an embodiment of the present invention; Figure 3 is along Figure 2 Schematic diagram of the cross-sectional structure of the micro-disk cavity with integrated waveguide on chip obtained by the A'B' section line; Figure 1-3 As shown, the micro-disk cavity comprises: an oxidized silicon wafer 10; the oxidized silicon wafer 10 comprises a silicon-based substrate 11 and a silicon oxide semiconductor layer 12; the silicon oxide semiconductor layer 12 comprises a functional area A and a non-functional area B; the functional area A comprises a waveguide structure 121, a micro-disk structure 122 and a first opening 123 located in the micro-disk structure 122; the non-functional area B comprises a second opening 124; the micro-disk structure 122 and the first opening 123 constitute a micro-disk cavity 125; a first extension cavity 111 and a second extension cavity 112; the first extension cavity 111 extends from the first opening 123 to the silicon-based substrate 11 in a direction perpendicular to the plane where the silicon-based substrate 11 is located; the second extension cavity 112 extends from the second opening 124 to the silicon-based substrate 11 in a direction perpendicular to the plane where the silicon-based substrate 11 is located; the first extension cavity 111 is connected to the second extension cavity 112; the vertical projections of the waveguide structure 121 and the micro-disk structure 122 on the silicon-based substrate 11 are located in the connected structure composed of the first extension cavity 111 and the second extension cavity 112.
[0035] Among them, the micro-disk cavity with integrated waveguide on chip first couples light to the micro-disk cavity 125 through the waveguide structure 121. When the light meets certain conditions, the light coupled into the micro-disk cavity 125 resonates in the micro-disk cavity 125, which plays an important role in nonlinear optics, lasers, coherent optical communications, sensing and other aspects.
[0036] Specifically, when light is coupled to the micro-disk cavity 125 through the waveguide structure 121, part of the light will leak into the silicon-based substrate 11 due to the low refractive index of the waveguide structure 121 made of silicon oxide semiconductor, resulting in high material absorption loss; the technical solution forms a second extended cavity 112 by setting a second opening 124, so that when light is transmitted in the silicon oxide waveguide structure 121, there is air with a lower refractive index below, and the light will not be absorbed by the silicon-based substrate 11, which greatly reduces the output loss of light in the waveguide structure 121; at the same time, the first extended cavity 111 is set to reduce the output loss of light coupled to the micro-disk cavity 125 in the corresponding silicon-based substrate 11, thereby improving the quality factor of the micro-disk cavity 125, thereby improving the power of the output light of the micro-disk cavity of the entire on-chip integrated waveguide, thereby improving the non-optical characteristics of the output light of the micro-disk cavity of the on-chip integrated waveguide. Optionally, the second opening 124 is located on the side of the waveguide structure 121 away from the micro-disk structure 123.
[0037] Optional, see Figure 3 , the thickness of the silicon oxide semiconductor layer at the non-opening position of the functional area A is greater than the thickness of the silicon oxide semiconductor layer in the non-functional area B.
[0038] Wherein, the silicon oxide semiconductor layer 12 includes a silicon oxide semiconductor support layer and a silicon oxide semiconductor functional layer;
[0039] The silicon oxide semiconductor support layer is located between the silicon-based substrate and the silicon oxide semiconductor functional layer; the waveguide structure 121 and the micro-disk structure 122 of the functional area A are prepared by etching the silicon oxide semiconductor functional layer through the same dry etching process; the second opening 124 of the non-functional area B is made by etching the silicon oxide semiconductor support layer.
[0040] The first opening 123 of the functional area A is made by etching the silicon oxide semiconductor support layer and the silicon oxide semiconductor functional layer corresponding to the micro-disk structure 122; thus, the thickness of the silicon oxide semiconductor layer at the non-opening position of the functional area A is greater than the thickness of the silicon oxide semiconductor layer of the non-functional area B, that is, the waveguide structure 121 and the micro-disk structure 122 of the functional area are arranged on one side of the silicon oxide semiconductor support layer, so that after the first extension cavity 111 and the second extension cavity 112 are formed, the silicon oxide semiconductor support layer can play a role in supporting the waveguide structure 121 and the micro-disk cavity 122.
[0041] Optional, see Figure 1-3 , the waveguide structure 121 is a linear waveguide structure; the coupling point between the linear waveguide structure and the micro-disk structure 122 is a fixed point, and the coupling mode between the waveguide structure 121 and the micro-disk cavity 125 is unique.
[0042] Optional, Figure 4 FIG. 1 is a schematic diagram of a top view of another micro-disk cavity with integrated waveguide on a chip provided by an embodiment of the present invention; Figure 4 As shown, the waveguide structure 121 is a curved waveguide structure; the vertical distance from each point on the curved waveguide structure 121 to the micro-disk structure 122 is a fixed value, and the coupling points between the curved waveguide structure and the micro-disk structure 122 are multiple vertical distance points, so that the waveguide structure 121 and the micro-disk cavity 125 are coupled in various ways, the coupling efficiency between the waveguide structure 121 and the micro-disk cavity 125 is high, and more light is coupled into the micro-disk cavity 125, which can improve the light output energy of the micro-disk cavity 125 of the on-chip integrated waveguide. It should be noted that the waveguide structure 121 only needs to realize the coupling function with the micro-disk cavity 125, and the specific shape of the waveguide structure 121 is not specifically limited here.
[0043] Optional, see Figure 2 , the spacing distance L between the waveguide structure 121 and the micro-disk structure 122 satisfies:
[0044] 0μm≤L≤10μm.
[0045] Among them, when the interval distance between the waveguide structure 121 and the micro-disk structure 122 is large, the light output by the waveguide structure 121 will have some loss and cannot be completely transmitted to the micro-disk structure 122, thereby affecting the output light energy of the micro-disk cavity 125; if the interval distance between the waveguide structure 121 and the micro-disk structure 122 is small, the difficulty of the preparation process of the entire integrated waveguide will increase. Preferably, the interval distance L between the waveguide structure 121 and the micro-disk structure 122 satisfies the above range, which can improve the coupling efficiency between the waveguide structure 121 and the micro-disk structure 122, thereby improving the energy of the light output by the micro-disk cavity 125, and can also reduce the difficulty of the preparation process of the micro-disk cavity of the entire on-chip integrated waveguide.
[0046] Optional, see Figure 1-4 , the first opening 123 is located in the central area of the micro-disk structure 122. The size of the first extended cavity 111 at the contact surface between the silicon-based substrate 11 and the silicon oxide semiconductor layer 12 is larger than the size of the first opening 123; the size of the second extended cavity 112 at the contact surface between the silicon-based substrate 11 and the silicon oxide semiconductor layer 12 is larger than the size of the second opening 124.
[0047] Among them, since the intrinsic loss of the silicon-based substrate 11 is relatively large, the second extended cavity 112 corresponding to the second opening 124 is etched, and the vertical projection of the waveguide structure 121 on the plane where the silicon-based substrate 11 is located is located in the second extended cavity 112, thereby reducing the additional loss caused by the silicon-based substrate 11 and reducing the transmission loss of light in the waveguide structure 121; at the same time, the silicon-based substrate 11 corresponding to the first opening 123 is etched to form the first extended cavity 111, and the vertical projection of the micro-disk cavity 125 on the plane where the silicon-based substrate 11 is located is located in the first extended cavity 111, further reducing the additional loss caused by the silicon-based substrate 11, reducing the transmission loss of the light coupled to the micro-disk cavity 125, and improving the quality factor of the micro-disk cavity 125, thereby improving the power of the micro-disk cavity output light of the entire on-chip integrated waveguide.
[0048] Based on the same inventive concept, an embodiment of the present invention further provides a method for preparing a micro-disk cavity with an on-chip integrated waveguide, which is used to prepare the micro-disk cavity with an on-chip integrated waveguide provided by an embodiment of the present invention. Figure 5 FIG. 1 is a flow chart of a method for preparing a micro-disk cavity with an on-chip integrated waveguide provided by an embodiment of the present invention. Figure 5 As shown, the preparation method comprises:
[0049] S110, providing a silicon monoxide wafer;
[0050] The silicon oxide wafer may be a commercial silicon oxide wafer, and the silicon oxide wafer includes a silicon-based substrate and a silicon oxide semiconductor layer; the silicon oxide semiconductor layer includes a functional area and a non-functional area.
[0051] S120, etching the non-functional area of the silicon oxide semiconductor layer using a dry etching process, so that the functional area of the silicon oxide semiconductor layer forms a waveguide structure and a micro-disk structure;
[0052] in, Figure 6-11 FIG. 1 is a process diagram of a micro-disk cavity with an on-chip integrated waveguide provided by an embodiment of the present invention, referring to Figure 6-8 , provide a silicon oxide wafer, the silicon oxide wafer includes a silicon-based substrate 11 and a silicon oxide semiconductor layer 12; apply photoresist on the silicon oxide semiconductor layer 12; use a mask plate with a preset pattern as a mask, perform photolithography and development on the photoresist to obtain a defined waveguide structure photoresist pattern 31 and a micro-disk structure 122 photoresist pattern 32; then use the waveguide structure photoresist pattern 31 and the micro-disk structure photoresist pattern 32 as masks, and partially etch the silicon oxide semiconductor layer 12 by reactive plasma etching or inductively coupled plasma etching to form a waveguide structure 121 and a micro-disk structure 122.
[0053] It should be noted that, compared with wet etching, since the corrosion through chemical reaction is isotropic, the size of the actual micro-disk structure 122 after the reaction will be smaller than the size of the photoresist pattern 32 of the micro-disk structure; this will lead to the complication of the process of coupling and preparing the waveguide structure 121 on one side of the micro-disk structure 122. The present technical solution etches the silicon oxide semiconductor layer 12 through a dry etching process. Compared with the wet etching process, the dry etching process is anisotropic, that is, the reaction speed is different in each direction, and the reaction speed can be flexibly controlled, so that the etching accuracy of the micro-disk structure 122 of the integrated waveguide structure 121 becomes higher, and the preparation of the micro-disk structure 122 of the integrated waveguide structure 121 is precisely controlled.
[0054] In addition, compared with the prior art, the waveguide structure 121 and the micro-disk structure 122 of different material layers are prepared by two wet etching methods. In this solution, the waveguide structure 121 and the micro-disk structure 122 are prepared in the same dry etching process, which simplifies the process of process preparation and does not require precise overlay during the preparation process. In addition, the waveguide structure 121 and the micro-disk structure 122 are both made of silicon oxide semiconductor material, which makes it easier to achieve phase matching.
[0055] S130, etching the silicon oxide semiconductor layer in the micro-disk structure and the silicon oxide semiconductor layer in a part of the non-functional area by a dry etching process to form a first opening in the micro-disk structure and a second opening in the non-functional area; the micro-disk structure and the first opening constitute a micro-disk cavity;
[0056] Among them, refer to Figure 9-10 , a photoresist is coated on the waveguide structure 121 and the micro-disk structure 122, and then a mask of a preset shape is used as a mask to perform photolithography and development on the photoresist to expose the silicon oxide semiconductor layer 12 corresponding to the micro-disk structure 122 and the silicon oxide semiconductor layer 12 in the non-functional area, and then the portion of the silicon oxide semiconductor layer 12 corresponding to the micro-disk structure 122 is etched to form a first opening 123 in the micro-disk structure 122, the first opening 123 penetrates the silicon oxide semiconductor layer 12, and the first opening 123 and the micro-disk structure 122 constitute a micro-disk cavity 125, that is, a micro-disk cavity of an on-chip integrated waveguide is formed; at the same time, the silicon oxide semiconductor layer 12 in the non-functional area is partially etched in the same dry etching process to form a second opening 124 in the non-functional area. In this way, the silicon oxide semiconductor layer 12 at the corresponding micro-disk structure 122 and part of the silicon oxide semiconductor layer 12 in the non-functional area are etched by reactive plasma etching or inductively coupled plasma etching. Since the dry etching process has anisotropy, the etching accuracy of the micro-disk cavity 125 and the second opening 124 of the integrated waveguide structure 121 is improved.
[0057] S140, etching the silicon-based substrate using the first opening and the second opening as masks respectively to form a first extended cavity and a second extended cavity;
[0058] Specifically, refer to Fig.11 , using the first opening 123 and the second opening 124 as masks, respectively, using at least one of xenon difluoride, potassium hydroxide, tetramethylammonium hydroxide, or a mixture of nitric acid, hydrofluoric acid and acetic acid to etch the silicon-based substrate 11 to form a first extension cavity 111 and a second extension cavity 112. Wherein, the size of the first extension cavity 111 at the contact surface between the silicon-based substrate 11 and the silicon oxide semiconductor layer 12 is larger than the size of the first opening 123; the size of the second extension cavity 112 at the contact surface between the silicon-based substrate 11 and the silicon oxide semiconductor layer 12 is larger than the size of the second opening 124; the first extension cavity 111 is connected to the second extension cavity 112; the vertical projections of the waveguide structure 121 and the micro-disk structure 122 on the silicon-based substrate 11 are located in the connected structure formed by the first extension cavity 111 and the second extension cavity 112. Since the intrinsic loss of the silicon-based substrate 11 is relatively large, the first extended cavity 111 is formed by wet etching the silicon-based substrate 11, which reduces the additional loss of the input light in the silicon-based substrate 11 and reduces the transmission loss of the input light in the waveguide structure 121. At the same time, the second extended cavity 112 is formed by etching the silicon-based substrate 11, which further reduces the additional loss of the light coupled to the micro-disk cavity 125 in the silicon-based substrate 11 and improves the quality factor of the micro-disk cavity 125. In this way, the power of the output light of the micro-disk cavity of the entire on-chip integrated waveguide is improved, which is beneficial to its application in nonlinear optics.
[0059] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.
Claims
1. A microdisk cavity with integrated waveguide on a chip, characterized in that: include: An oxidized silicon wafer; the oxidized silicon wafer comprises a silicon-based substrate and a silicon oxide semiconductor layer; The silicon oxide semiconductor layer includes a functional area and a non-functional area; the functional area includes a waveguide structure, a micro-disk structure and a first opening located in the micro-disk structure; the non-functional area includes a second opening; the micro-disk structure and the first opening constitute a micro-disk cavity; a first extension cavity and a second extension cavity; the first extension cavity extends from the first opening into the silicon-based substrate along a direction perpendicular to the plane where the silicon-based substrate is located; the second extension cavity extends from the second opening into the silicon-based substrate along a direction perpendicular to the plane where the silicon-based substrate is located; the first extension cavity is connected to the second extension cavity; the vertical projections of the waveguide structure and the micro-disk structure on the silicon-based substrate are located in the connected structure formed by the first extension cavity and the second extension cavity; The non-functional area of the silicon oxide semiconductor layer is etched by a dry etching process, so that the functional area of the silicon oxide semiconductor layer forms a waveguide structure and a micro-disk structure; The silicon oxide semiconductor layer in the micro-disk structure and a portion of the silicon oxide semiconductor layer in the non-functional area are etched using a dry etching process to form a first opening in the micro-disk structure and a second opening in the non-functional area.
2. The micro-disk cavity with integrated waveguide on chip according to claim 1, characterized in that: The thickness of the silicon oxide semiconductor layer at the non-opening position of the functional area is greater than the thickness of the silicon oxide semiconductor layer in the non-functional area.
3. The micro-disk cavity with integrated waveguide on chip according to claim 1, characterized in that: The waveguide structure is a linear waveguide structure; Alternatively, the waveguide structure is a curved waveguide structure; and the vertical distance from each point on the curved waveguide structure to the micro-disk structure is a fixed value.
4. The micro-disk cavity with integrated waveguide on chip according to claim 3, characterized in that: A spacing distance L between the waveguide structure and the micro-disk structure satisfies: 0 μm≤L≤10 μm.
5. The micro-disk cavity with integrated waveguide on chip according to claim 1, characterized in that: The first opening is located in a central region of the micro-disk structure.
6. The micro-disk cavity with integrated waveguide on chip according to claim 1, characterized in that: The second opening is located at a side of the waveguide structure away from the micro-disk structure.
7. The micro-disk cavity with integrated waveguide on a chip according to claim 1, characterized in that: The size of the first extended cavity at the contact surface between the silicon-based substrate and the silicon oxide semiconductor layer is larger than the size of the first opening; A size of the second extended cavity at a contact surface between the silicon-based substrate and the silicon oxide semiconductor layer is larger than a size of the second opening.
8. A method for preparing a micro-disk cavity with an on-chip integrated waveguide, characterized in that: A micro-disk cavity for preparing an on-chip integrated waveguide as claimed in any one of claims 1 to 7, the preparation method comprising: Providing a silicon oxide wafer; the silicon oxide wafer comprises a silicon-based substrate and a silicon oxide semiconductor layer; the silicon oxide semiconductor layer comprises a functional area and a non-functional area; Etching the non-functional area of the silicon oxide semiconductor layer using a dry etching process, so that the functional area of the silicon oxide semiconductor layer forms a waveguide structure and a micro-disk structure; The silicon oxide semiconductor layer in the micro-disk structure and the silicon oxide semiconductor layer in a part of the non-functional area are etched by a dry etching process to form a first opening in the micro-disk structure and a second opening in the non-functional area; the micro-disk structure and the first opening constitute a micro-disk cavity; The silicon-based substrate is etched using the first opening and the second opening as masks to form a first extension cavity and a second extension cavity; the first extension cavity is connected to the second extension cavity; the vertical projections of the waveguide structure and the micro-disk structure on the silicon-based substrate are located in the connected structure formed by the first extension cavity and the second extension cavity.
9. The preparation method according to claim 8, characterized in that: The silicon-based substrate is etched using the first opening and the second opening as masks to form a first extended cavity and a second extended cavity, comprising: The silicon-based substrate is etched by an etching process using the first opening and the second opening as masks respectively, so as to form a first extended cavity and a second extended cavity; the size of the first extended cavity at the contact surface between the silicon-based substrate and the silicon oxide semiconductor layer is larger than the size of the first opening; the size of the second extended cavity at the contact surface between the silicon-based substrate and the silicon oxide semiconductor layer is larger than the size of the second opening; Wherein, the reactants of the etching process include at least one of xenon difluoride, potassium hydroxide, tetramethylammonium hydroxide, or a mixture of nitric acid, hydrofluoric acid and acetic acid.
10. The preparation method according to claim 8, characterized in that: The dry etching process includes a reactive plasma etching process or an inductively coupled plasma etching process.