Method for manufacturing wireless communication device, wireless communication device, and assembly of wireless communication device

By forming the circuit and the antenna on two film substrates in the RFID inlay and attaching them with high precision, and using the organic semiconductor layer, the problem of damage of the RFID inlay under bending pressure in the existing technology is solved, and a flexible, low-cost Cost-effective and efficient manufacturing of wireless communication devices.

CN113015979BActive Publication Date: 2024-10-29TORAY INDUSTRIES INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN201980074204.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-12-13
Publication Date
2024-10-29
Estimated Expiration
2039-12-13

AI Technical Summary

Technical Problem

Existing RFID inlays are easily damaged when bending or pressure is applied, resulting in poor tag operation, and high-density combinations of drive circuits and antennas are difficult to achieve, resulting in low production efficiency and high costs.

Method used

Using a manufacturing method that forms circuits and antennas on two film substrates respectively, and achieves high-precision bonding through alignment marks and tension adjustment, organic semiconductors and carbon materials are used to form semiconductor layers to achieve the manufacturing of flexible wireless communication devices.

Benefits of technology

It realizes the connection between the RFID circuit and the antenna with strong bending resistance and pressure resistance, reduces the production cost and the number of processes, improves the position accuracy and production efficiency, and achieves small-area inlay design.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113015979B_ABST
    Figure CN113015979B_ABST
Patent Text Reader

Abstract

The subject of the present invention is to provide a wireless communication device with simple process, good positional accuracy, low cost and flexibility. The main purpose of the present invention is a wireless communication device and a manufacturing method thereof, wherein the manufacturing method is a method for manufacturing a wireless communication device by laminating a first film substrate having at least a circuit formed thereon and a second film substrate having an antenna formed thereon, wherein the circuit includes a transistor, and the transistor is formed by a process including the following processes: a process of forming a conductive pattern on the first film substrate; a process of forming an insulating layer on the film substrate having the conductive pattern formed thereon; and a process of applying a solution containing an organic semiconductor and / or a carbon material on the insulating layer and drying it to form a semiconductor layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for manufacturing a wireless communication device and the wireless communication device. Background Art

[0002] In recent years, wireless communication devices using RFID (Radio Frequency Identification) technology have been developed as contactless tags. In an RFID system, wireless communication is performed between a wireless transceiver called a reader / writer and an RFID tag.

[0003] RFID tags are made by embedding, processing, and labeling an RFID inlay, which consists of a drive circuit including transistors, capacitors, etc., and an antenna for wireless communication with a reader / writer. The antenna set in the tag receives the carrier sent from the reader / writer, thereby driving the circuit to operate.

[0004] RFID tags have already been partially introduced into IC cards such as transportation cards, product tags, etc., and are expected to be used in various applications such as logistics management, product management, and pickpocket prevention.

[0005] Therefore, the RFID inlay is required to be flexible and can be manufactured at low cost. As a method of manufacturing the RFID inlay, a method of forming the RFID drive circuit and the antenna on the same substrate can be cited. However, in this method, since the size of the antenna is large, the RFID drive circuit must be formed in the part without the antenna, so the RFID drive circuit cannot be formed at a high density. Therefore, the production efficiency is low, which becomes the main reason for the cost increase.

[0006] Therefore, the following method is being studied: after forming the RFID driving circuit and antenna at high density on different substrates, the substrate on which the RFID driving circuit is formed is divided into multiple sections containing one or more RFID chips, and the antenna is attached to the antenna substrate (for example, refer to patent document 1).

[0007] Prior art literature

[0008] Patent Literature

[0009] Patent Document 1: Japanese Patent Application No. 2005-520266 Summary of the invention

[0010] Problems to be solved by the invention

[0011] However, the method described in Patent Document 1 uses an RFID inlay in which an IC chip is mounted. In this case, there is a problem that the wafer used in the IC chip is hard, and if bending or pressure is applied, the substrate such as the film or the IC chip is damaged, resulting in malfunction of the RFID tag.

[0012] In view of the above problems, an object of the present invention is to provide a method for manufacturing a wireless communication device that is resistant to bending, pressure, and friction and can accurately fit the connection between an RFID circuit and an antenna.

[0013] Means for solving problems

[0014] The present invention is made in view of the above-mentioned problems and is a wireless communication device and a manufacturing method thereof, wherein the manufacturing method is a method for manufacturing the wireless communication device by bonding a first film substrate having at least a circuit formed thereon and a second film substrate having an antenna formed thereon, wherein:

[0015] The circuit comprises a transistor,

[0016] The transistor is formed by a process including the following steps:

[0017] forming a conductive pattern on the first film substrate;

[0018] forming an insulating layer on the film substrate having the conductive pattern formed thereon; and

[0019] A step of applying a solution containing an organic semiconductor and / or a carbon material on the insulating layer and drying the solution to form a semiconductor layer.

[0020] Effects of the Invention

[0021] According to the present invention, a flexible wireless communication device can be obtained. In addition, in the case of a configuration in which a circuit and a part of an antenna overlap, a small area of ​​an inlay can be achieved. Furthermore, by the manufacturing method of the present invention, a wireless communication device can be manufactured with a small number of steps, good position accuracy and low cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] [ Figure 1A ] is a schematic diagram showing an example of a method for manufacturing a wireless communication device according to an embodiment of the present invention.

[0023] [ Figure 1B ] is a schematic cross-sectional view of the bonding portion of the first film substrate and the second film substrate.

[0024] [ Figure 1C ] is a schematic diagram showing the position offset between the RFID circuit and the antenna.

[0025] [ Figure 2] is a schematic top view showing the first film substrate on which the RFID circuit is formed.

[0026] [ Figure 3 ] is a schematic top view showing the second film substrate on which the antenna circuit is formed.

[0027] [ Figure 4A ] is a schematic top view of a wireless communication device according to an embodiment of the present invention.

[0028] [ Figure 4B ] is a schematic cross-sectional view showing the connection portion between the RFID circuit and the antenna.

[0029] [ Figure 5 ] is a schematic cross-sectional view showing an example of a method for manufacturing an RFID circuit.

[0030] [ Figure 6 ] is a schematic diagram showing an example of a method for manufacturing a wireless communication device according to an embodiment of the present invention.

[0031] [ Figure 7 ] is a schematic diagram showing an example of a method for manufacturing a wireless communication device according to an embodiment of the present invention.

[0032] [ Figure 8 ] is a schematic diagram showing an example of a method for manufacturing a wireless communication device according to an embodiment of the present invention.

[0033] [ Fig. 9 ] is a schematic diagram showing an example of a method for manufacturing a wireless communication device according to an embodiment of the present invention.

[0034] [ Fig.10 ] is a schematic diagram showing an example of a method for manufacturing a wireless communication device according to an embodiment of the present invention.

[0035] [ Fig.11 ] is a schematic top view showing an example of a wireless communication device according to an embodiment of the present invention.

[0036] [ Fig. 12A ] is a schematic top view showing an example of the overlapping portion of the circuit and the antenna.

[0037] [ Fig. 12B ] is a schematic cross-sectional view showing an example of the overlapping portion of the circuit and the antenna.

[0038] [ Fig. 12C ] is a schematic cross-sectional view showing an example of the overlapping portion of the circuit and the antenna.

[0039] [ Fig.12D ] is a schematic cross-sectional view showing an example of the overlapping portion of the circuit and the antenna. DETAILED DESCRIPTION

[0040] Hereinafter, the mode for implementing the present invention will be described in detail. It should be noted that the present invention is not limited to the following embodiment.

[0041] In the present invention, the circuit refers to a circuit composed of an electronic circuit and a connecting part, wherein the electronic circuit is composed of a transistor, a capacitor, an electrode wiring, etc., and the connecting part is a connecting part that electrically connects the electronic circuit to the antenna using a connecting pad and an antenna coil. Specifically, it refers to a circuit that includes at least one of a rectifier circuit, a demodulation circuit, a logic circuit, a modulation circuit, and a storage circuit used in RFID, a transceiver, a wireless microphone, a sensor module for IoT, an RF remote control, a lighting control system, a keyless entry system, etc. In addition, an antenna refers to a device that sends information to a reader / writer by receiving radio waves from a reader / writer and driving the circuit. As a circuit composed of an electronic circuit (the electronic circuit is composed of a transistor, a capacitor, an electrode wiring, etc.) and a connecting part (the connecting part is a connecting part that electrically connects the electronic circuit to the antenna using a connecting pad and an antenna coil), there is an RFID circuit. The following takes the RFID circuit as an example to illustrate the method for implementing the present invention.

[0042] (Implementation Method 1)

[0043] Figure 1A This is a schematic diagram showing an outline of a method for manufacturing a wireless communication device according to Embodiment 1 of the present invention. In Embodiment 1, a process of bonding a first film substrate 100 having an RFID circuit 110 formed thereon and a second film substrate 200 having an antenna 210 formed thereon are schematically shown. Figure 1B This is a schematic diagram of the lamination portion as viewed from the lateral direction.

[0044] As the material used for the first film substrate, any material can be used as long as at least the surface on which the electrode system is arranged is an insulating film. Organic materials such as polyimide, polyvinyl alcohol, polyvinyl chloride, polyethylene terephthalate, polyvinylidene fluoride, polysiloxane, polyvinylphenol (PVP), polyester, polycarbonate, polysulfone, polyethersulfone, polyethylene, polypropylene, polyphenylene sulfide, polyparaxylene, cellulose, etc. can be suitably used, but are not limited to these.

[0045] As the material used for the second film substrate, any material can be used as long as the surface on which the antenna is arranged is an insulating film, and the same material as the first film substrate, paper, etc. can be used.

[0046] The RFID circuit 110 is formed in an array of two rows in the longitudinal direction of the first film substrate 100. The RFID circuit 110 includes a transistor. As the transistor, an organic field effect transistor is preferably used.

[0047] The antenna 210 is formed in an array shape of two rows in the longitudinal direction of the second film substrate 200. The number of rows of these arrays is not particularly limited, but one or more rows is preferred.

[0048] The laminating nip roller 404 is a roller for laminating the first film substrate 100 and the second film substrate 200 by applying pressure. The laminating feed roller 403 is a roller for conveying the two substrates at a predetermined speed after laminating. The laminating and conveying are performed by the above rollers.

[0049] Figure 2 1 is a schematic top view showing a first film substrate on which an RFID circuit is formed. An RFID circuit 110, an alignment mark 120, and an upper electrode wiring 131 are formed on the first film substrate 100. The upper electrode wiring 131 is included in the RFID circuit 110 and is a connection wiring connected to an antenna. Figure 2 In order to facilitate understanding, the state where only one RFID circuit 110 is formed is shown, but it is of course not limited to this number. The same applies to the alignment mark 120 and the upper electrode wiring 131. The method of forming the RFID circuit will be described later.

[0050] Figure 3 2 is a schematic top view showing the second film substrate on which the antenna is formed. The second film substrate 200 is provided with an antenna 210, an alignment mark 220, and an antenna wiring 230. The antenna wiring 230 is a part of the antenna 210 and is a connection wiring connected to the RFID circuit 110. Figure 3 In order to facilitate understanding, only one antenna 210 is shown, but the number is not limited to this. The same applies to the alignment mark 220 and the antenna wiring 230.

[0051] As a method for forming the antenna 210, the following known methods can be cited: a method of using a punch to process a metal foil such as copper foil or aluminum foil into an antenna and transfer it to a substrate (hereinafter referred to as a punch method); a method of etching the metal foil adhered to a substrate such as a plastic film using an anti-etching layer formed on the metal foil as a mask; a method of printing a conductive paste on a substrate such as a plastic film in a pattern corresponding to the antenna and curing it by heat or light (hereinafter referred to as a printing method); a method of etching a metal film formed by vapor deposition using an anti-etching layer formed on the metal film as a mask; and the like.

[0052] The material used for the antenna is not particularly limited, and Ag, Au, Cu, Pt, Pb, Sn, Ni, Al, W, Mo, Cr, Ti, carbon, or indium can be used. As the metal foil material used in the punching method, Cu and Al are preferred from the viewpoints of cost and antenna performance, and as the metal material contained in the conductive paste used in the printing method, Ag is preferred from the viewpoints of cost and antenna performance.

[0053] By forming a coating film on the second film substrate 200 using a photosensitive paste and then forming a pattern corresponding to electrodes and wirings using a photolithography method, an antenna substrate with wirings and electrodes can be formed.

[0054] Figure 4A It shows that Figure 2 The first film substrate shown in Figure 3 Schematic top view of a wireless communication device manufactured by laminating the first film substrate 100 with the second film substrate 200. The surface of the RFID circuit 110 formed on the first film substrate 100 is laminated with the surface of the antenna 210 formed on the second film substrate 200. The lamination is performed by aligning the positions of the alignment marks 120 and 220. In addition, as shown in FIG. Figure 4A As shown in the partially enlarged view of the interior of the RFID circuit 110 shown in , the antenna wiring 230 on the second film substrate is connected to the upper electrode wiring 131 on the first film substrate.

[0055] Figure 4B yes Figure 4A A schematic cross-sectional view of the dotted line XY portion. Figure 4B In the embodiment, a TFT portion 140, which is one of the operating portions of the circuit, and an electrode portion that is a connection portion with the antenna are formed on the first film substrate. In the electrode portion, a pattern (contact hole) that is an opening portion is formed on the insulating layer 112 in order to achieve conduction from the lower electrode wiring 130. Furthermore, the upper electrode wiring 131 is connected to the antenna wiring 230. The upper electrode wiring 131 and the antenna wiring 230 may be directly connected, or may be connected after a conductive paste is applied to the connection portion, or may be connected after a non-conductive paste is applied to at least a portion between the upper electrode wiring 131 and the antenna wiring 230. In this way, by making the RFID circuit 110 on the first film substrate 100 and the antenna 210 on the second film substrate 200 face each other and directly bonded, there is no need to use a wire, a conductive tape, etc., so that bonding with less unevenness can be achieved.

[0056] return Figure 1A It should be noted that the circuit 110 formed on the lower side of the first film substrate 100 is originally depicted with dotted lines, but is shown with solid lines for easy understanding. The wireless communication device manufactured by bonding the first film substrate 100 and the second film substrate 200 is also shown with solid lines. A plurality of wireless communication devices (an aggregate of wireless communication devices) are manufactured on the two film substrates bonded in this way.

[0057] The alignment camera 405 provided in the process of bonding the first film substrate and the second film substrate measures and detects the positional deviation between the first film substrate 100 and the second film substrate 200 in the conveying direction. Alignment marks ( Figure 1A The above positional offset is detected based on their relative offset.

[0058] As long as the alignment mark can be detected within the camera field of view, the size and shape are not specified. In addition, as long as the positional offset can be detected based on the overlap between the RFID circuit 110 and the antenna 210, the alignment mark may not be provided.

[0059] The alignment camera may be of any type and form as long as it can detect the alignment mark, and examples thereof include an area array camera, a line scan camera, etc. In addition, a flash light may be used to periodically capture the image.

[0060] exist Figure 1A In the present invention, the positional deviation of the first film substrate 100 and the second film substrate 200 is detected after lamination, but it can also be detected before lamination. For example, in order to detect the alignment marks of each substrate before the first film substrate 100 and the second film substrate 200 pass through the lamination position, two alignment cameras are set on the upstream side of the lamination position. Then, the position of each substrate before lamination is detected by each camera, and the distance from each detection position to the lamination position is calculated, thereby calculating the positional deviation amount.

[0061] The positional deviation correction can be performed on a regular basis, but usually an allowable range of the positional deviation is set and the correction is performed when it is exceeded. The allowable range of the positional deviation is set according to the size of the connection part of the RFID circuit and the connection part of the antenna.

[0062] The correction of the positional deviation is preferably performed by changing the conveying tension of the first film substrate or the second film substrate according to the amount of the positional deviation. The change in conveying tension can be performed by using, for example, Figure 1A The tension adjustment is realized by the tension adjustment nip roller 402 and the tension adjustment feed roller 401 shown in the figure, but any mechanism capable of changing the tension is acceptable and the tension adjustment is not limited to the above-mentioned rollers.

[0063] exist Figure 1A In the composition of Figure 1CAs shown in the figure, when the alignment mark 220 of the second film substrate is offset relative to the alignment mark 120 of the first film substrate in the conveying direction 500 and bonded, the rotation speed of the tension adjustment feed roller 401 is slowed down relative to the rotation speed of the bonding feed roller 403, so that only the second film substrate 200 is stretched, and a tension that does not return to the original level even after stretching is generated. In this way, the second film substrate 200 can be plastically deformed to adjust the positional offset.

[0064] How much the rotation speed of the tension adjustment feed roller 401 is slowed down according to the positional deviation is determined by the physical properties such as the glass transition temperature and thickness of the second film substrate and the degree of plastic deformation due to temperature.

[0065] In the case of a film that is difficult to stretch, in order to facilitate stretching, the following method can be used: Figure 1A The film substrate is heated by heater 406 as shown. In particular, by making the temperature higher than the softening point of the second film substrate, a significant stretching effect can be obtained. However, if the temperature deviation is large, it will be partially stretched or wrinkled, so it can be set after confirming the temperature distribution and temperature accuracy. As a heating method, known methods such as hot air, infrared rays, and heating rollers can be cited.

[0066] As a control method for correcting the positional deviation, for example, the following control is performed: when a positional deviation of more than 100 μm is detected, the conveying is performed with a tension 10N higher than the set tension, and when the positional deviation is restored to less than 100 μm, the tension is restored to the set tension. In the above control, the tension is increased when the positional deviation exceeds a certain threshold, and the threshold of the positional deviation used to change the tension can be set in several stages. Considering that the detection of the positional deviation includes measurement errors, the positional deviation used in the control is preferably an average value obtained by multiple detections. In addition, regarding the change of tension, instead of setting a threshold for the positional deviation as described above, the tension can be changed little by little in accordance with the positional deviation.

[0067] Furthermore, by setting the conveying speeds of the first film substrate 100 and the second film substrate 200 after passing the laminating feed roller 403 to be the same, it is possible to eliminate the possibility of positional displacement or peeling due to shearing after lamination.

[0068] exist Figure 1A In the example, the tension of the second film substrate 200 is adjusted, but the tension of the first film substrate 100 may also be adjusted.

[0069] exist Figure 1A and Figure 1BIn the example of , the surface of the RFID circuit side of the first film substrate is bonded to the surface of the antenna side of the second film substrate. That is, the surfaces of the two substrates are bonded to each other. Thus, the RFID circuit and the antenna can be directly connected to supply power. In addition, even if the first film substrate 100 or the second film substrate 200 is damaged by friction during processing, wireless communication can be performed as long as the damage does not reach the inner surface.

[0070] It should be noted that the method of laminating the first film substrate and the second film substrate is not limited to the above-mentioned method. Specifically, the back side of any substrate can be laminated to the surface of the other substrate, or the back sides of the two substrates can be laminated to each other. In the case of these methods, power is supplied by a known non-contact coupling method such as a coupling method using electrostatic capacitance and a coupling method using electromagnetic induction, thereby enabling wireless communication.

[0071] However, from the viewpoints of stability of wireless communication, scratch resistance during the manufacturing process, etc., it is more preferable to bond the surface of the first film substrate on the RFID circuit side to the surface of the second film substrate on the antenna side.

[0072] Figure 5 1 is a schematic cross-sectional view showing an example of a method for manufacturing a transistor which is one of the elements constituting the RFID circuit 110 .

[0073] first, Figure 5 In (a), a lower conductive film 150 is formed on the first film substrate 100. As a method for forming the lower conductive film 150, a resistance heating evaporation method, an electron beam method, a sputtering method, a plating method, a CVD method, etc. can be cited. In addition, the following method can be cited: a paste containing a conductor and a photosensitive organic component is applied to the substrate by a known coating method such as an inkjet method, a printing method, an ion plating method, a doctor blade coating method, a slot die coating method, a screen printing method, a rod coating method, a casting method, a printing transfer method, a dip-pull method, etc., and then the coated film is dried to remove the solvent.

[0074] As a material of the lower conductive film 150 , silver, copper, and gold are preferable from the viewpoint of conductivity, and silver is more preferable from the viewpoint of cost and stability.

[0075] Next, Figure 5In (b), the lower conductive film 150 is patterned to form the gate electrode 111 and the lower electrode wiring 130 including the connection portion with the antenna. Patterning based on known photolithography is preferred. In the case where the lower conductive film 150 is not photosensitive, known patterning using a photoresist can be used. In the case where a paste containing a conductor and a photosensitive organic component is applied to a substrate to form the lower conductive film 150, the photosensitive conductive film can be photolithographically processed. Thus, the gate electrode 111 and the lower electrode wiring 130 as a conductive pattern are formed on the first film substrate 100.

[0076] Next, Figure 5 In (c), a gate insulating layer 112 is formed on the gate electrode 111 and the lower electrode wiring 130 including the connection portion with the antenna. The material used for the gate insulating layer is not particularly limited, and examples thereof include inorganic materials such as silicon oxide and aluminum oxide; organic materials such as polyimide, polyvinyl alcohol, polyvinyl chloride, polyethylene terephthalate, polyvinylidene fluoride, polysiloxane, and polyvinylphenol (PVP); or a mixture of inorganic material powder and organic material.

[0077] The method for preparing the gate insulating layer is not particularly limited, and for example, the following method can be cited: the raw material composition is applied to a substrate having a gate electrode formed thereon and dried, and the coating film thus obtained is subjected to heat treatment as required. As the coating method, known coating methods such as a doctor blade coating method, a slit die coating method, a screen printing method, a rod coating method, a casting method, a printing transfer method, a dip-pull method, and an inkjet method can be cited.

[0078] Next, Figure 5 In (d), the gate insulating layer 112 on the lower electrode wiring 130 is removed to form a contact hole. This is performed on the portion connecting the lower electrode wiring and the upper electrode wiring. Figure 5 When the gate insulating layer 112 is obtained using a paste containing a photosensitive organic component in the step (c), the contact hole can be formed by patterning using a photolithography method.

[0079] Next, Figure 5 In (e), an upper conductive film 160 containing a conductor and a photosensitive organic component is formed on the gate insulating layer 112. By making the organic binder contain a photosensitive organic component, electrode pattern processing based on photolithography can be performed without using a resist, which can further improve productivity. As a method for forming the upper conductive film 160, the following method can be cited: after coating by a known coating method such as a doctor blade coating method, a slit die coating method, a screen printing method, a rod coating method, a casting method, a printing transfer method, a dip pulling method, an ink jet method, etc., the coated film is dried to remove the solvent.

[0080] Next, Figure 5In (f), the upper conductive film 160 is patterned to form the source electrode 114, the drain electrode 115, and the upper electrode wiring 131 including the connection portion with the antenna. These are exposed from the back through the first film substrate 100 using the gate electrode 111 as a mask, so that the source electrode 114 and the drain electrode 115 can be aligned with high precision without alignment. However, it is also possible to Figure 5 The gate electrode 111 and the lower electrode wiring 130 in (b) are formed in the same manner.

[0081] Finally, in Figure 5 (g) An organic semiconductor layer 113 is formed between the source electrode 114 and the drain electrode 115. The material used for the organic semiconductor layer is an organic semiconductor and / or a carbon material. As carbon materials, carbon nanotubes (CNTs), graphene, fullerene, etc. can be cited. From the aspects of adaptability to coating processes and high mobility, CNTs are preferred. Furthermore, CNTs (hereinafter referred to as CNT complexes) having a conjugated polymer attached to at least a portion of the surface have excellent dispersion stability in the solution and can obtain high mobility, so they are particularly preferred.

[0082] As a method for forming the organic semiconductor layer 113, a dry method such as resistance heating evaporation, electron beam, sputtering, CVD, etc. can also be used. From the perspective of manufacturing cost and suitability for a large area, a coating method is preferably used. As a coating method, known coating methods such as a scraper coating method, a slit die coating method, a screen printing method, a rod coating method, a casting method, a printing transfer method, an immersion pull method, and an inkjet method can be cited. It should be noted that step (g) can be implemented before steps (e) and (f). In this way, an organic semiconductor layer 113 is formed on the gate insulating layer 112.

[0083] (Implementation Method 2)

[0084] Figure 6 1 is a schematic diagram showing an outline of a method for manufacturing a wireless communication device according to Embodiment 2 of the present invention. In Embodiment 2, the conveying directions of the first film substrate 100 and the second film substrate 200 are the same, and they are conveyed intermittently in the longitudinal direction so as to face each other. That is, both are conveyed for a certain amount and then temporarily stopped. When stopped, the first film substrate 100 is fixed by a film conveying fixture 409. The conveying tension is cut off by the tension adjustment feed roller 401a and the tension adjustment clamp roller 402a, and the tension adjustment feed roller 401b, the tension adjustment clamp roller 402b, and the conveying fixture are lowered while the first film substrate 100 is relaxed.

[0085] After the descent, the first film substrate 100 and the second film substrate 200 are in a state of being close to each other, and the positional deviation of both sides is detected by the alignment camera 405. The positional deviation is confirmed at at least two points of the alignment marks of the first film substrate 100 and the second film substrate 200, and the positions in the longitudinal direction and the short side direction are aligned. The positional alignment is performed, for example, by moving the stage 407 while the second film substrate 200 is adsorbed on the stage 407.

[0086] The first film substrate 100 is further lowered, and after the first film substrate 100 is placed on the second film substrate 200, the film cutter 408 is used to only (half) cut the first film substrate 100. Thus, the first film substrate 100 is divided into a single sheet containing a plurality of RFID circuits. Then, the clamping of the film conveying clamp 409 is released, and the tension adjustment feed roller 401b, the tension adjustment clamp roller 402b, and the conveying clamp 409 are raised. The second film substrate 200 is conveyed and passed through the bonding feed roller 403 and the bonding clamp roller 404, thereby clamping the first film substrate 100 and the second film substrate 200 and bonding them.

[0087] Figure 6 The structure is an example, and other structures may be used as long as it includes a process of cutting any film substrate when the conveyance stops, a process of detecting the positional deviation of the first film substrate and the second film substrate, a position alignment process, and a bonding process.

[0088] (Implementation method 3)

[0089] Figure 7 Schematic diagram showing an outline of a method for manufacturing a wireless communication device according to Embodiment 3 of the present invention. Embodiment 3 is manufactured through the same steps as Embodiment 2 except that the first film substrate 100 and the second film substrate 200 are arranged orthogonally.

[0090] Due to the influence of longitudinal and transverse stretching in the film manufacturing process, for example, the thermal shrinkage of the PET film in the longitudinal direction is often greater than that in the short-side direction. Therefore, by making the first film substrate and the second film substrate orthogonal to each other, the longitudinal direction of each is bonded to the short-side direction, and thus the positional deviation is often reduced compared to bonding the longitudinal directions to each other.

[0091] (Implementation 4)

[0092] Figure 81 is a schematic diagram showing an outline of a method for manufacturing a wireless communication device according to Embodiment 4 of the present invention. In Embodiment 4, a step of dividing a first film substrate 100 into two or more pieces and a step of adjusting the interval of the divided first film substrate in a direction perpendicular to the conveying direction to the interval of the antenna array in the substrate width direction of the second film substrate are added to Embodiment 1, and a tension adjustment feed roller 401 and a tension adjustment clamping roller 402 corresponding to each of the divided first film substrates 100 are provided.

[0093] The position of the divided first film substrate in the short-side direction is controlled using, for example, “EPC” (registered trademark, Edge Position Control), thereby enabling alignment in the short-side direction in addition to positional deviation in the longitudinal direction.

[0094] According to the manufacturing method described above, the circuit 110 formed in an array on the first film substrate and the antenna 210 formed in an array on the second film substrate can be aligned even when the array pitches in the film width direction are different.

[0095] (Implementation 5)

[0096] Fig. 9 Schematic diagram showing an outline of a method for manufacturing a wireless communication device according to Embodiment 5 of the present invention. Embodiment 5 is manufactured through the same steps as Embodiment 4 except that the first film substrate 100 and the second film substrate 200 are arranged orthogonally.

[0097] (Implementation 6)

[0098] Fig.10 1 is a schematic diagram showing an outline of a method for manufacturing a wireless communication device according to Embodiment 6 of the present invention. In Embodiment 6, although the second film substrate 200 has the same shape as Embodiment 2, the first film substrate 100 is a single sheet, which is different. The RFID circuit is formed in an array of one or more rows in the longitudinal direction of the single-sheet first film substrate.

[0099] The second film substrate 200 is intermittently transported in the longitudinal direction. When stopped, the first film substrate 100 is transported to the second film substrate and fixed by the film transport fixture 409. As long as it is a mechanism that can stop after transporting the first film substrate 100 to the second film substrate, other structures can be used. For example, a mechanism that can absorb a part or the entire surface of the first film substrate can be provided, and after picking up the first film, it is transported to the second substrate.

[0100] After the first film substrate and the second film substrate stop, the first film substrate 100 and the second film substrate 200 are close to each other and the positional deviation of both sides is detected by the alignment camera 405. The positional deviation is confirmed at at least two points of the alignment marks of the first film substrate 100 and the second film substrate 200, and the positions in the longitudinal direction and the short side direction are aligned. The positional alignment is performed by moving the film conveying clamp 409.

[0101] The first film substrate 100 is further lowered and placed on the second film substrate 200. Then, the clamping of the film conveying clamp 409 is released and the film conveying clamp 409 is raised. The second film substrate 200 is conveyed and passed through the laminating feed roller 403 and the laminating clamp roller 404, thereby clamping the first film substrate 100 and the second film substrate 200 and laminating them.

[0102] In all embodiments, a step of applying a conductive paste to the connection portion between the RFID circuit 110 formed on the first film substrate 100 and the antenna 210 formed on the second film substrate 200 may be provided before lamination. In addition, a step of applying a non-conductive paste to at least a portion between the first film substrate 100 and the second film substrate 200 may be provided.

[0103] As the conductive paste, silver paste, carbon paste, indium paste, etc. can be used, and as the non-conductive paste, a known paste including urethane resin, epoxy resin, and acrylic resin can be used.

[0104] Examples of the method for applying the conductive paste and the non-conductive paste include known methods such as screen printing, bar coating, printing transfer, inkjet, and dispenser methods.

[0105] (Implementation 7)

[0106] Fig.11 1 is a schematic plan view showing an outline of a wireless communication device according to Embodiment 7 of the present invention. Embodiment 7 is characterized in that a circuit 110 and a part of an antenna 210 are designed to overlap intentionally. Fig. 12A yes Fig.11 Schematic cross-sectional view of the overlapped portion 300 of the circuit and the antenna shown in FIG. Fig. 12AAs shown, the lower electrode wiring 130, which is a part of the circuit, is configured to overlap with the antenna 210, thereby reducing the area of ​​the overlapping portion. In addition, the overlapping portion can be used as a wiring connecting the circuit and the antenna, and can also be used as a parallel plate capacitor. In this case, a parallel plate capacitor can be made using the lower electrode wiring 130, the insulating layer 112, and the antenna 210. The electrostatic capacitance is determined by the overlapping area of ​​the lower electrode wiring 130 and the antenna 210, and the dielectric constant of the insulating layer. As for the shape of the overlap between the lower electrode wiring 130 and the antenna 210, a rectangle is used as an example, but it can be any shape. In addition, the materials and formation methods of each layer are as shown in Implementation 1.

[0107] In the present invention, it is important to include the following steps: forming a circuit including an organic semiconductor layer using an organic semiconductor and / or a carbon material on a film substrate. In the case of inorganic semiconductors, after forming a circuit on a wafer, the circuit is formed into a chip of several mm square and mounted, so it is difficult to obtain the effect of the present invention in terms of structure and size.

[0108] (Implementation 8)

[0109] Fig. 12B , Fig. 12C and Fig.12D 1 is a schematic cross-sectional view showing an outline of a wireless communication device according to an eighth embodiment of the present invention. In the eighth embodiment, an insulating adhesive layer 170 as an adhesive is formed in contact with the antenna 210. Therefore, a parallel plate capacitor using any of the lower electrode wiring 130 and the insulating layer 112, the upper electrode wiring 131, the adhesive layer 170, and the antenna 210 can be formed to connect the wiring. Although the adhesive layer 170 is described as a single layer, the same effect can be obtained even if a plurality of adhesive layers 170 having different dielectric constants are used. Fig. 12B It can be considered that the parallel plate capacitor is formed with the adhesive layer 170 between the antenna 210 and the upper electrode wiring 131, and the parallel plate capacitor is formed with the insulating layer 112 between the upper electrode wiring 131 and the lower electrode wiring 130. Fig. 12C In this way, a parallel plate capacitor can be manufactured in which the insulating layer 112 and the adhesive layer 170 are formed between the antenna 210 and the lower electrode wiring 130. Fig.12D That way, it can be made into Fig. 12B The parallel plate capacitor has the same structure but has a smaller shape of the lower electrode wiring 130 so that the area of ​​the parallel plate is different.

[0110] Furthermore, by forming a part or the entire surface of the adhesive layer 170 on any one of the first film substrate 100 and the second film substrate 200 and laminating them using any of the manufacturing methods in Embodiments 1 to 6, a flexible substrate with few irregularities can be obtained, thereby obtaining a wireless communication circuit with strong resistance to bending and pressure. Furthermore, since positional displacement is detected and lamination is performed with high precision, the deviation of the electrostatic capacitance of the parallel plate capacitor formed in the overlapping portion 300 of the circuit and the antenna can also be reduced.

[0111] The adhesive layer is formed of a known resin such as a urethane resin, an epoxy resin, or an acrylic resin, and may contain a known insulating material such as silicon dioxide, titanium oxide, or granular glass.

[0112] In addition, although the parallel plate capacitor is used as an example in the seventh and eighth embodiments, from the perspective of reducing the area of ​​the inlay, a portion of the circuit may overlap with the antenna, and components other than the antenna may be used for the capacitance and resistance of the circuit.

[0113] As a modified example, a peeling layer may be formed in advance between the second film substrate and the antenna, and after lamination by any of the methods in Embodiments 1 to 6, the second film substrate may be peeled off to transfer the antenna to the circuit side.

[0114] The method for manufacturing an RFID wireless communication device of the present invention can be used to manufacture an RFID tag as an inlay. The form of the RFID tag is not particularly limited, and examples thereof include a seal label, a price tag, and a package with an RFID tag.

[0115] As a method for producing a seal label, there can be mentioned, for example, a method including at least the following two steps.

[0116] (1) A step of manufacturing an RFID inlay by laminating a PET film (first film substrate) on which an RFID circuit is formed and an antenna film (second film substrate) formed using the PET film using the method described in the present invention.

[0117] (2) Of the front and back surfaces of the RFID inlay, an adhesive is applied to the surface not bonded to the first film substrate (i.e., the back surface), a release paper is laminated to the back surface, and a surface sheet capable of being printed with characters or the like is laminated to the surface formed with the first film substrate (i.e., the front surface) using an adhesive material, followed by a scraping process.

[0118] As a method for producing a price tag, for example, there can be mentioned a method including at least the following two steps.

[0119] (1) A step of manufacturing an RFID inlay by laminating a PET film (first film substrate) on which an RFID circuit is formed and an antenna film (second film substrate) formed of paper using the method described in the present invention.

[0120] (2) A step of laminating a surface paper printed with a price, a product name, etc., on the surface (ie, the front surface) on which the first film substrate is formed, using an adhesive material.

[0121] As a method for producing a package package with an RFID tag, for example, there can be mentioned a method including at least the following two steps.

[0122] (1) A process of manufacturing an RFID inlay by laminating a packaging film (first film substrate) having an RFID circuit formed thereon and an antenna film (second film substrate) formed using a PET film using the method described in the present invention. It should be noted that, as the packaging film, for example, a label film of a PET bottle can be cited, on which a product name, a product image, etc. are printed. In this case, the antenna pattern can be formed by a printing method using a conductive paste when printing the product name and the product image.

[0123] (2) A step of laminating a surface paper printed with a price, a product name, etc., on the surface (ie, the front surface) on which the first film substrate is formed, using an adhesive material.

[0124] Description of Reference Numerals

[0125] 100: 1st film substrate

[0126] 110: RFID circuit

[0127] 111: Gate electrode

[0128] 112: Insulation layer

[0129] 113: Organic semiconductor layer

[0130] 114: Source electrode

[0131] 115: Drain electrode

[0132] 120: Alignment mark

[0133] 130: Lower electrode wiring

[0134] 131: Upper electrode wiring (connection part)

[0135] 140: TFT Department

[0136] 150: Lower conductive film

[0137] 160: Upper conductive film

[0138] 170: Adhesive layer

[0139] 200: 2nd film substrate

[0140] 210: Antenna

[0141] 220: Alignment mark

[0142] 230: Antenna wiring (connection part)

[0143] 300: The overlapping part of the circuit and the antenna

[0144] 401, 401a, 401b: Feed rollers for tension adjustment

[0145] 402, 402a, 402b: Nipples for tension adjustment

[0146] 403: Feed roller for lamination

[0147] 404: Lamination roller

[0148] 405: Alignment Camera

[0149] 406: Heater

[0150] 407: Carrier

[0151] 408: Membrane cutting knife

[0152] 409: Membrane transport fixture

[0153] 500: Arrow indicating the conveying direction of the first film substrate and the second film substrate

Claims

1. A method for manufacturing a wireless communication device, comprising laminating a first film substrate having at least a circuit formed thereon and a second film substrate having at least an antenna formed thereon, in, The circuit comprises a transistor, The transistor is formed by a process including the following steps: forming a conductive pattern on the first film substrate; forming an insulating layer on the film substrate having the conductive pattern formed thereon; and A step of coating a solution containing an organic semiconductor and / or a carbon material on the insulating layer and drying the solution to form a semiconductor layer, The circuit is formed into an array of more than one row in the length direction of the first film substrate, the antenna is formed into an array of more than one row in the length direction of the second film substrate, the first film substrate and the second film substrate are transported in the length direction, and the bonding is continuously performed, The bonding process includes the following steps: a step of measuring the positional deviation of the first film substrate and the second film substrate in the conveying direction; and a step of correcting the position of the first film substrate or the second film substrate according to the positional deviation. The positions of the first film substrate and the second film substrate are corrected by changing the conveyance tension of the first film substrate or the second film substrate according to the positional deviation amount.

2. The method for manufacturing a wireless communication device according to claim 1, comprising the following steps: The step of measuring the positional deviation amount in the conveying direction by using an alignment camera; and The step of correcting the positional deviation amount by changing the conveyance tension of the first film substrate or the second film substrate.

3. The method for manufacturing a wireless communication device according to claim 1 or 2, comprising the following steps: The first film substrate is divided into at least two steps in a conveying direction; and A step of adjusting the interval between the divided film substrates in a direction perpendicular to the conveying direction to the interval between the antenna columns in the substrate width direction of the second film substrate.

4. The method for manufacturing a wireless communication device according to claim 1 or 2, in, On the first film substrate or the second film substrate, a conductive paste is applied to a connection portion between the circuit and the antenna, and then the bonding is performed.

5. The method for manufacturing a wireless communication device according to claim 1 or 2, in, The bonding is performed after a non-conductive paste is applied to at least a portion between the circuit and the antenna on the first film substrate or the second film substrate.

6. The method for manufacturing a wireless communication device according to claim 1 or 2, in, The circuit-side surface of the first film substrate and the antenna-side surface of the second film substrate are bonded together.

7. The method for manufacturing a wireless communication device according to claim 1 or 2, in, The circuit is an RFID circuit.

Citation Information

Patent Citations

  • method for manufacturing rfid labels

    JP2005520266A

  • Method for producing reversible thermosensitive recording medium, production apparatus for the same, and reversible thermosensitive recording medium

    CN102205756A

  • Tape supply device

    JP2006298572A

  • IC mounted module, its manufacturing method, and manufacturing facility

    JP2007108983A

  • Semiconductor film and semiconductor element using the same, and dispersion liquid

    JP2018093198A