Flip chip bonding structure and circuit substrate thereof
By designing the T-line structure in the overcrystal package, the width of the connection segment is reduced, the problems of solder overflow and bridge short circuit are solved, and the product yield and packaging reliability are improved.
Patent Information
- Application Number
- CN202010554734.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-12-31
- Filing Date
- 2020-06-17
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2040-06-17
AI Technical Summary
During the overcrystal packaging process, wide lines cause solder overflow and bridge short circuits, especially during the hot pressing process, solder flows along the line to bumps, resulting in overflow and short circuits, reducing product yield .
A T-line structure is designed, in which the width of the connecting segment is reduced to reduce the amount of solder flowing to the branch segment. By adjusting the width and length of the main segment, the connecting segment and the branch segment, the flow direction and amount of solder are controlled to avoid Overflow and short circuit.
It effectively avoids solder overflow and bridge short circuits, improves product yield, and controls solder flow and bonding, ensuring the reliability of the package.
Smart Images

Figure HDA0002543812860000011 
Figure HDA0002543812860000021 
Figure HDA0002543812860000031
Abstract
Description
Technical Field
[0001] The invention relates to a flip chip bonding structure, in particular to a flip chip bonding structure with a T-shaped circuit. Background Art
[0002] Flip chip packaging technology mostly uses thermal compression to soften the solder to join the chip and substrate. During the thermal compression process, the softened solder will flow along the circuit toward the bump. However, when the bump is adjacent to a circuit with a wider line width, the solder on the circuit will be softened by heat at a faster rate and flow toward the bump, resulting in excessive solder overflow around the bump, and even bridging short circuits, which reduces the yield. Summary of the invention
[0003] The object of the present invention is to provide a flip chip bonding structure with a T-shaped circuit, which effectively avoids the occurrence of a bridge short circuit due to solder overflow by reducing the width of the T-shaped circuit connection section.
[0004] The present invention discloses a flip chip bonding structure, which includes a circuit substrate, a chip and a solder layer. The circuit substrate has a carrier, a plurality of inner pins and at least one T-shaped circuit. The surface of the carrier defines an inner bonding area, the inner bonding area includes a first inner bonding area and a second inner bonding area. The inner pin is located in the first inner bonding area, and the T-shaped circuit is located in the second inner bonding area. The T-shaped circuit has a main line segment, a connecting segment and a branch line segment. The main line segment connects the connecting segment and extends along a transverse direction. The branch line segment connects the connecting segment and extends toward the first inner bonding area along a longitudinal direction. The main line segment has a first width along the longitudinal direction, and the connecting segment has a second width along the longitudinal direction, and the second width is smaller than the first width. The chip is arranged in the inner bonding area and has a plurality of first bumps and at least one second bump. The solder layer is located between the circuit substrate and the chip. The first bump is bonded to the inner pin by the solder layer, and the second bump is bonded to the branch line segment by the solder layer.
[0005] Preferably, the branch line segment extends along the longitudinal direction toward one of the inner pins.
[0006] Preferably, the branch line segment extends along the longitudinal direction to between two adjacent inner pins.
[0007] Preferably, the branch line segment has a first end and a second end, the first end is connected to the connecting segment, the second end is engaged with the second protrusion, and the line width of the first end is greater than the line width of the second end.
[0008] Preferably, the branch line segment has a third width along the transverse direction, and a ratio of the second width to the third width is not less than 0.5.
[0009] Preferably, the second protrusion has a fourth width along the lateral direction, and a ratio of the second width to the fourth width is less than 2.
[0010] Preferably, the second width and the fourth width are the same.
[0011] Preferably, the connecting section has a first length along the transverse direction, the second protrusion has a second length along the longitudinal direction, and the ratio of the first length to the second length is not less than 4.
[0012] Preferably, there is a straight-line distance between the connecting section and the second protrusion, and a ratio of the straight-line distance to the second width is not less than 3.
[0013] Preferably, the thickness of the solder layer is not greater than 0.30 μm.
[0014] The present invention further discloses a circuit substrate, which includes a carrier, a plurality of inner pins and at least one T-shaped circuit. The carrier has a surface, which defines an inner bonding area. The inner bonding area includes a first inner bonding area and a second inner bonding area. The inner pins are located in the first inner bonding area, and the T-shaped circuit is located in the second inner bonding area. The T-shaped circuit has a main line segment, a connecting segment and a branch line segment. The main line segment connects the connecting segment and extends along the transverse direction. The branch line segment connects the connecting segment and extends along the longitudinal direction toward the first inner bonding area. The branch line segment is used to connect a bump. The main line segment has a first width along the longitudinal direction, and the connecting segment has a second width along the longitudinal direction. The second width is smaller than the first width.
[0015] Preferably, the branch line segment extends along the longitudinal direction toward one of the inner pins.
[0016] Preferably, the branch line segment extends along the longitudinal direction to between two adjacent inner pins.
[0017] Preferably, the branch line segment has a first end and a second end, the first end is connected to the connecting segment, the second end is used to engage the bump, and the line width of the first end is greater than the line width of the second end.
[0018] Preferably, the branch line segment has a third width along the transverse direction, and a ratio of the second width to the third width is not less than 0.5.
[0019] Preferably, it further comprises a solder layer, wherein the solder layer is formed on the branch line segment, and the branch line segment is bonded to the bump via the solder layer.
[0020] Preferably, the thickness of the solder layer is not greater than 0.30 μm.
[0021] When the circuit substrate and the chip are joined, the solder layer will be softened by heat and flow from different directions to the bump joint on the branch segment. Therefore, the present invention reduces the width of the connection segment and reduces the amount of solder flowing from the connection segment to the branch segment to avoid solder overflowing from the bump joint and causing a bridging short circuit. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 : A top view of a carrier according to a preferred embodiment of the present invention.
[0023] Figure 2 : A top view of a flip chip bonding structure according to a preferred embodiment of the present invention.
[0024] Figure 3 : A partial top view of the inner bonding area of the circuit substrate according to a preferred embodiment of the present invention.
[0025] Figure 4 : A partial top view of the inner bonding area of the circuit substrate according to a preferred embodiment of the present invention.
[0026] Figure 5 : A partial top view of the inner bonding area of the circuit substrate according to a preferred embodiment of the present invention.
[0027] Figure 6 : A partial top view of the inner bonding area of the circuit substrate according to a preferred embodiment of the present invention.
[0028] Figure 7 : A partial top view of the inner bonding area of the circuit substrate according to a preferred embodiment of the present invention.
[0029] Figure 8 :along Figure 7 Section view along line AA.
[0030]
Main component symbol description
[0031] 100: Circuit board 110: Carrier board
[0032] 111: Surface 112: External bonding area
[0033] 113: Inner joint area 113a: First inner joint area
[0034] 113b: second inner bonding area 120: outer lead
[0035] 130: inner pin 140: T-type circuit
[0036] 141: Main line segment 142: Connecting segment
[0037] 143: branch line segment 143a: first end
[0038] 143b: second end 200: chip
[0039] 210: first bump 220: second bump
[0040] 300: solder mask 400: solder layer
[0041] 500: Encapsulation colloid D1: Horizontal direction
[0042] D2: Longitudinal direction I: Flip chip bonding structure
[0043] L1: first length L2: second length
[0044] LD: Straight distance W1: First width
[0045] W2: second width W3: third width
[0046] W4: fourth width DETAILED DESCRIPTION
[0047] See also Figures 1 to 3 The present invention discloses a flip chip bonding structure I, which can be a chip on film packaging structure (Chip on Film, COF), a chip on glass packaging structure (Chip on Glass, COG) or other flip chip packaging structures. The flip chip bonding structure I includes a circuit substrate 100 and a chip 200. The circuit substrate 100 has a carrier 110, a plurality of external pins 120 and a plurality of internal pins 130. The carrier 110 can be made of polyimide (PI), polyethylene terephthalate (PET) The carrier 110 is made of PET, glass, ceramic, metal or other materials. The carrier 110 has a surface 111. The outer pins 120 and the inner pins 130 are formed on the surface 111. The surface 111 defines two outer bonding areas 112 and an inner bonding area 113. The outer bonding areas 112 are respectively located on both sides of the carrier 110. The inner bonding area 113 is located between the outer bonding areas 112. The outer pins 120 are located in the outer bonding areas 112, and the inner pins 130 are located in the inner bonding areas 113.
[0048] See also Figure 2 and Figure 3 Preferably, the flip-chip bonding structure I further has a solder mask 300, which covers the surface 111 of the carrier 110 and exposes the outer bonding area 112 and the inner bonding area 113. The chip 200 is arranged in the inner bonding area 113. In the present embodiment, the chip 200 is bonded to the inner pin 130 by means of a thermal compression bonding technique, and the outer pin 120 is used to bond to an external device (not shown).
[0049] See also Figure 3 and Figure 4 The inner bonding area 113 includes a first inner bonding area 113a and a second inner bonding area 113b, the inner pin 130 is located in the first inner bonding area 113a, and the circuit substrate 100 also has at least one T-shaped circuit 140, the T-shaped circuit 140 is located in the second inner bonding area 113b, there is no electrical connection between the T-shaped circuit 140 and the inner pin 130, and it is used for grounding or connecting to a power source. Preferably, the inner bonding area 113 includes two first inner bonding areas 113a, the first inner bonding areas 113a are located on both sides, and the second inner bonding area 113b is located between the first inner bonding areas 113a, the inner pins 130 are arranged along the edges of both sides of the inner bonding area 113, and the T-shaped circuit 140 is located between the inner pins 130 on both sides. Preferably, the inner pins 130 and the T-shaped circuit 140 are formed by a patterned copper foil substrate.
[0050] See also Figure 3 and Figure 4 , which is an embodiment of the present invention, the T-shaped line 140 has a main line segment 141, a connecting segment 142 and a branch line segment 143, the main line segment 141 connects the connecting segment 142 and extends along the lateral direction D1, the branch line segment 143 connects the connecting segment 142 and extends toward the first inner bonding area 113a along the longitudinal direction D2, and the branch line segment 143 is used to bond the bump of the chip 200. In this embodiment, the connecting segment 142 and the branch line segment 143 are perpendicular to each other, but the present invention is not limited to this, and the angle between the connecting segment 142 and the branch line segment 143 can be greater than, less than or equal to 90 degrees.
[0051] Preferably, the circuit substrate 100 has a plurality of T-shaped circuits 140 , the main line segments 141 of each T-shaped circuit 140 are connected to each other along the transverse direction D1 , and the branch line segments 143 of each T-shaped circuit 140 extend toward the first inner bonding area 113 a along the longitudinal direction D2 .
[0052] Figure 5 , Figure 6 and Figure 7 The branch line segment 143 of different embodiments, Figure 5 The branch line segment 143 shown extends along the longitudinal direction D2 toward one of the inner pins 130 , but is not connected to the inner pin 130 . Figure 6 The branch line segment 143 shown extends along the longitudinal direction D2 to between two adjacent inner pins 130 . Figure 7The branch line segment 143 shown has a first end 143a and a second end 143b, wherein the first end 143a is connected to the connecting segment 142, and the second end 143b is used to engage the bump of the chip 200, wherein the line width of the first end 143a is greater than the line width of the second end 143b to avoid breakage between the connecting segment 142 and the branch line segment 143, and preferably, the second end 143b is located between two adjacent inner pins 130.
[0053] See also Figures 3 to 8 The chip 200 has a plurality of first bumps 210 and at least one second bump 220. The flip chip bonding structure I further has a solder layer 400. The solder layer 400 is located between the circuit substrate 100 and the chip 200. The first bump 210 is bonded to the inner lead 130 by the solder layer 400. The second bump 220 is bonded to the branch line segment 143 by the solder layer 400. Preferably, the thickness of the solder layer 400 is not greater than 0.30 μm. More preferably, the thickness of the solder layer 400 is not greater than 0. 20μm. In the present embodiment, the circuit substrate 100 includes the solder layer 400. The solder layer 400 is formed on the inner pin 130 and the main line segment 141, the connecting segment 142 and the branch line segment 143 of the T-type circuit 140. The thickness is 0.16μm±0.4μm. When the chip 200 and the circuit substrate 100 are joined, the inner pin 130 is joined to the first bump 210 through the solder layer 400, and the branch line segment 143 is joined to the second bump 220 through the solder layer 400.
[0054] See also Figure 7 In the present embodiment, the second end 143 b of the branch line segment 143 is used to engage the second bump 220 , so when the chip 200 is engaged with the circuit substrate 100 , the second end 143 b is engaged with the second bump 220 via the solder layer 400 .
[0055] See also Figure 8 Preferably, the flip chip bonding structure I further has a packaging colloid 500, and the packaging colloid 500 is filled between the circuit substrate 100 and the chip 200. The packaging colloid 500 can be an underfill, but the present invention is not limited thereto.
[0056] The solder layer 400 will be softened by heat and become fluid during the thermal pressing process. When the second bump 220 is connected to the branch segment 143, the solder layer 400 located on the T-type line 140 will flow from different directions to the joint of the second bump 220 to increase the incidence of overflow. In order to avoid bridging short circuits, the present invention performs wiring design for the T-type line 140.
[0057] See also Figure 4The main line segment 141 has a first width W1 along the longitudinal direction D2, and the connecting segment 142 has a second width W2 along the longitudinal direction D2. The second width W2 is smaller than the first width W1. By reducing the width of the connecting segment 142, the amount of solder flowing from the connecting segment 142 to the branch line segment 143 is effectively reduced, thereby preventing excessive solder from flowing to the second bump 220 and causing overflow. Preferably, the branch line segment 143 has a third width W3 along the transverse direction D1, and the ratio of the second width W2 to the third width W3 is not less than 0.5. When the ratio is between 0.5 and 1 Indicates that the second width W2 is smaller than the third width W3. When the ratio is equal to 1 Indicates that the second width W2 is equal to the third width W3, when the ratio is greater than 1 It means that the second width W2 is greater than the third width W3 . In this embodiment, the line width of the branch line segment 143 is the same as the line width of the inner lead 130 .
[0058] See also Figure 5 The second protrusion 220 has a fourth width W4 along the transverse direction D1, and the ratio of the second width W2 to the fourth width W4 is less than 2. The ratio can be between 1 and 2 That is, the second width W2 is greater than the fourth width W4, but less than twice the fourth width W4, and the ratio may be equal to 1. The second width W2 and the fourth width W4 are made the same, and the ratio can also be between 0 and 1. The second width W2 is smaller than the fourth width W4. When designing wiring, the width of the connecting section 142 can be determined according to the width of the second bump 220, so that the ratio of the second width W2 to the fourth width W4 is smaller than 2.
[0059] See also Figure 6 The connecting section 142 has a first length L1 along the transverse direction D1, and the second protrusion 220 has a second length L2 along the longitudinal direction D2, and the ratio of the first length L1 to the second length L2 is not less than 4. The length of the connecting segment 142 is made not less than 4 times the length of the second protrusion 220. Therefore, the length of the connecting segment 142 that needs to be reduced in width can be determined according to the length of the second protrusion 220. In the present embodiment, the branch segment 143 is located at the center of the connecting segment 142, that is, the shortest distance from the branch segment 143 to both ends of the connecting segment 142 is the same, but the present invention is not limited to this. The branch segment 143 can be selectively biased toward one end of the connecting segment 142 according to different wiring design requirements.
[0060] See also Figure 6, there is a straight-line distance LD between the edge of the connecting section 142 and the edge of the second bump 220, and the straight-line distance LD is the shortest distance between the connecting section 142 and the second bump 220. When the thickness of the solder layer 400 increases, it is necessary to increase the ratio of the straight-line distance LD to the second width W2, that is, the ratio of the straight-line distance LD to the second width W2 must be proportional to the thickness of the solder layer 400 to avoid excessive solder flowing to the junction between the branch line section 143 and the second bump 220 during the hot pressing process, thereby causing a bridge short circuit. Preferably, when the thickness of the solder layer 400 is 0.16 μm, the ratio of the straight-line distance LD to the second width W2 must be not less than 3 The straight distance LD is greater than or equal to 3 times the second width W2. When the thickness of the solder layer 400 is 0.18 μm, the ratio of the straight distance LD to the second width W2 must be no less than 4. The straight-line distance LD is greater than or equal to 4 times the second width W2.
[0061] In order to prevent excessive amount of the solder layer 400 from flowing from the T-shaped line 140 to the second bump 220, the present invention reduces the width of the connecting section 142, thereby reducing the amount of solder flowing from the connecting section 142 to the branch section 143, and can selectively adjust the width and length of the connecting section 142 and the distance between it and the second bump 220 according to different needs, so as to significantly reduce the occurrence rate of bridging short circuits due to solder overflow, thereby effectively improving product yield.
[0062] The protection scope of the present invention shall be determined by the scope of the patent application. Any changes and modifications made by anyone familiar with this technology without departing from the spirit and scope of the present invention shall fall within the protection scope of the present invention.
Claims
1. A flip chip bonding structure, It is characterized in that It contains: A circuit substrate, comprising a carrier, a plurality of inner pins and at least one T-shaped circuit, wherein an inner bonding area is defined on a surface of the carrier, wherein the inner bonding area comprises a first inner bonding area and a second inner bonding area, wherein the inner pins are located in the first inner bonding area, wherein the T-shaped circuit is located in the second inner bonding area, wherein the T-shaped circuit comprises a main line segment, a connecting segment and a branch line segment, wherein the main line segment connects the connecting segment and extends along a transverse direction, wherein the branch line segment connects the connecting segment and extends toward the first inner bonding area along a longitudinal direction, wherein the main line segment has a first width along the longitudinal direction, wherein the connecting segment has a second width along the longitudinal direction, wherein the second width is smaller than the first width; A chip is disposed in the inner bonding area, the chip having a plurality of first bumps and at least one second bump; as well as The solder layer is located between the circuit substrate and the chip. The first bump is connected to the inner lead through the solder layer, and the second bump is connected to the branch line segment through the solder layer.
2. The flip chip bonding structure according to claim 1, It is characterized in that The branch line segment extends along the longitudinal direction toward one of the inner pins.
3. The flip chip bonding structure according to claim 1, It is characterized in that The branch line segment extends along the longitudinal direction to between two adjacent inner pins.
4. The flip chip bonding structure according to claim 1, It is characterized in that The branch line segment has a first end and a second end, the first end is connected to the connection segment, the second end is connected to the second bump, and the line width of the first end is greater than the line width of the second end.
5. The flip chip bonding structure according to claim 1, It is characterized in that The branch line segment has a third width along the transverse direction, and a ratio of the second width to the third width is not less than 0.
5.
6. The flip chip bonding structure according to claim 1, It is characterized in that The second protrusion has a fourth width along the transverse direction, and a ratio of the second width to the fourth width is less than 2.
7. The flip chip bonding structure according to claim 6, It is characterized in that The second width and the fourth width are the same.
8. The flip chip bonding structure according to claim 6, It is characterized in that The connecting section has a first length along the transverse direction, the second protrusion has a second length along the longitudinal direction, and the ratio of the first length to the second length is not less than 4.
9. The flip chip bonding structure according to claim 1, It is characterized in that There is a straight-line distance between the connecting section and the second protrusion, and a ratio of the straight-line distance to the second width is not less than 3.
10. The flip chip bonding structure according to claim 1, It is characterized in that The thickness of the solder layer is no more than 0.30 μm.
11. A circuit substrate, It is characterized in that It contains: A carrier having a surface, the surface defining an inner bonding area, the inner bonding area including a first inner bonding area and a second inner bonding area; A plurality of inner pins located in the first inner bonding area; as well as At least one T-shaped line is located in the second inner joining area, the T-shaped line has a main line segment, a connecting segment and a branch line segment, the main line segment connects the connecting segment and extends along the transverse direction, the branch line segment connects the connecting segment and extends toward the first inner joining area along the longitudinal direction, the branch line segment is used to engage the protrusion, the main line segment has a first width along the longitudinal direction, the connecting segment has a second width along the longitudinal direction, and the second width is smaller than the first width.
12. The circuit substrate according to claim 11, It is characterized in that The branch line segment extends along the longitudinal direction toward one of the inner pins.
13. The circuit substrate according to claim 11, It is characterized in that The branch line segment extends along the longitudinal direction to between two adjacent inner pins.
14. The circuit substrate according to claim 11, It is characterized in that The branch line segment has a first end and a second end, the first end is connected to the connection segment, the second end is used to engage the bump, and the line width of the first end is greater than the line width of the second end.
15. The circuit substrate according to claim 11, It is characterized in that The branch line segment has a third width along the transverse direction, and a ratio of the second width to the third width is not less than 0.
5.
16. The circuit substrate according to claim 11, It is characterized in that The invention further comprises a solder layer, wherein the solder layer is formed on the branch line segment, and the branch line segment is connected to the bump through the solder layer.
17. The circuit substrate according to claim 16, It is characterized in that The thickness of the solder layer is no more than 0.30 μm.