A AB axis cradle structure and processing method thereof
By adopting a combined structure of steel shell and aluminum core in the AB axis platform, combined with split processing and inline, the problem of low elastic deformation and processing success rate of the cradle structure in the prior art is solved, and the structural rigidity and Improved accuracy ensures high-quality processing results.
Patent Information
- Application Number
- CN202110647417.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-06-10
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2041-06-10
AI Technical Summary
The cradle structure in the existing AB axis platform is prone to elastic deformation after processing, with low processing success rate and unsmooth surface. Moreover, due to the characteristics of slender rods, it is difficult to meet the requirements of high precision and high rigidity.
Using a combination structure of steel shell and aluminum core, the aluminum core is embedded in the steel shell through the principle of interference fit and heating expansion, and combined with the embedding of the left and right end covers, the structural rigidity is enhanced by split processing and inlay to ensure that It is not easy to deform when the fixture is loosened, and the increase in internal stress is avoided when the part is removed later.
It improves the rigidity and processing success rate of the AB axis cradle structure, ensures the outer roundness and dimensional tolerance, avoids elastic deformation and increase in internal stress, and improves the accuracy and processing quality of the overall parts.
Smart Images

Figure CN113245864B_ABST
Abstract
Description
[Technical field]
[0001] The invention relates to the technical field of AB axis platforms, in particular to an AB axis cradle structure applied to an AB axis platform. [Background Technology]
[0002] At present, the most difficult part to process in the existing AB axis (also called the fourth and fifth axis of the machine tool), the B axis fixing seat (also called the cradle), is mostly processed in one piece. In the 3C industry, while pursuing overall lightness, it is also necessary to achieve high precision, especially the concentricity of the shaft holes on both sides, which is generally required to be around 0.01mm. The main shortcomings are as follows:
[0003] (1) Under the same structural conditions, the rigidity of aluminum is lower than that of steel. Even if the precision requirements are met after processing, the cradle will undergo elastic deformation when the load increases during later use;
[0004] (2) Without changing the structure, the processing scrap rate is high, and some processors cannot even do it;
[0005] (3) When processing the two ends, due to the large ratio of the cradle length to the diameter, this structure belongs to the category of slender rods, and the knife vibration phenomenon will occur during processing. At the same time, the processed surface is not smooth and the processing knife marks are deep. [Summary of the invention]
[0006] The purpose of the present invention is to solve the above-mentioned deficiencies and provide an AB axis cradle structure with enhanced structural rigidity. When it is lifted up from the two end holes, it is not easy to cause the overall deformation when the clamp is loosened, and it will not cause an increase in internal stress due to the subsequent cutting of other parts.
[0007] In order to achieve the above purpose, an AB axis cradle structure is designed, including a steel shell 1, an aluminum core 2, a left end cover 3 and a right end cover 4. The steel shell 1 is a cylindrical shape with open left and right ends and a circular ring-shaped cross section. A semicircular groove 5 is dug in the middle of the steel shell 1. The aluminum core 2 is an aluminum core shaft with a semicircular cross section. A rectangular groove 6 is dug inside the aluminum core 2 and passes through the axial direction. The outer cylindrical surface of the aluminum core 2 is matched and connected with the inner cylindrical surface of the steel shell 1. The aluminum core 2 is nested in the steel shell 1, and an interference fit is adopted between the aluminum core 2 and the steel shell 1. The inner cylindrical surfaces of the circular rings at the left and right ends of the steel shell 1 are respectively matched and connected with the outer cylindrical surfaces of the left end cover 3 and the right end cover 4. The left end cover 3 and the right end cover 4 are embedded at both ends of the steel shell 1 and an interference fit is adopted between the steel shell 1.
[0008] Furthermore, the steel housing 1 is made of stainless steel.
[0009] Furthermore, the aluminum core 2 is made of aluminum rod.
[0010] Furthermore, threaded holes, through holes and pin holes are processed on the left end cover 3 and the right end cover 4.
[0011] The present invention also provides a processing method for an AB axis cradle structure, comprising the following steps: before the steel shell 1 is embedded, the outer circle and end face are turned by a lathe, the inner circle is processed by a boring machine, and the outer dimensions are cut out by a laser processing method; the inner circle size and end size of the aluminum core 2 and the inner circle size of the steel shell 1 are finely processed, the steel shell 1 is heated, and according to the principle of thermal expansion, the aluminum core 2 is pressed into the steel shell 1, and after cooling, the aluminum core 2 is nested in the steel shell 1, and the area where the steel shell 1 and the aluminum core 2 cooperate is within half of the circle; the outer circle and end face sizes of the left end cover 3 and the right end cover 4 are finely processed by a lathe, and the internal contour is processed by NC and the inner circle is roughly processed, and threaded holes, through holes and pin holes are made, and the left end cover 3 and the right end cover 4 are embedded in the two ends of the steel shell 1 in the same way.
[0012] Furthermore, the aluminum core 2 is made of an integral aluminum rod, and the outer circle and end face are precision-turned, and a margin of several millimeters is left on the left end face, and no margin is left on the right end face.
[0013] Furthermore, taking the right end face of the steel shell 1 as the axial reference, the right end cover 4 is first pressed into the steel shell 1 by means of interference fit and heating the steel shell 1, and then the temperature of the steel shell 1 is continued to be maintained, and the aluminum core 2 is pressed into the steel shell 1. After cooling, the size of the remaining left end face of the aluminum core 2 is measured, and the excess amount is processed by a lathe. Then, the steel shell 1 is heated again, and the left end cover 3 is pressed into the steel shell 1; after the embedding is completed, the concentric holes of the left and right end covers 3 and 4 are processed based on the outer circle of the steel shell 1, and the inner holes are processed after positioning through the outer circle; then, the excess part of the aluminum core 2 is processed according to the contour of the steel shell 1, and after axial support and fixation on the turning and milling machine, the mounting surface is finally processed.
[0014] Compared with the prior art, the present invention adopts the structure and processing method of aluminum-embedded steel, and the embedded aluminum core adopts split processing and embedding. On the one hand, the structural rigidity is enhanced, and when it is lifted up from the holes at both ends, it is not easy to cause the overall deformation when the clamp is loosened, thereby increasing the success rate of processing and avoiding the problem of elastic deformation of the cradle when the load increases in later use in the traditional structure; on the other hand, the split processing of the present invention can ensure the roundness and dimensional tolerance of the outer circle, and will not cause an increase in internal stress due to the subsequent cutting of other parts, thereby ensuring the accuracy of the overall parts, and is worthy of popularization and application. [Drawings]
[0015] Figure 1 is an exploded view of the present invention;
[0016] Figure 2 It is a front structural schematic diagram of the present invention;
[0017] Figure 3 yes Figure 2 Left view of
[0018] Figure 4 yes Figure 2 Right view of;
[0019] Figure 5 yes Figure 2 Middle AA section view;
[0020] Figure 6 It is a schematic diagram of the front structure of the aluminum core in the present invention;
[0021] Figure 7 yes Figure 6 A schematic diagram of the side structure of
[0022] Figure 8 yes Figure 6 A schematic diagram of a top view structure;
[0023] Fig. 9 It is a front structural schematic diagram of the steel housing in the present invention;
[0024] Fig.10 yes Fig. 9 A schematic diagram of the side structure of
[0025] Fig.11 yes Fig. 9 Middle CC section view;
[0026] Fig.12 It is a structural schematic diagram of the outer side surface of the left end cover in the present invention;
[0027] Fig.13 It is a structural schematic diagram of the inner side of the left end cover in the present invention;
[0028] Fig.14 yes Fig.12 Middle EE section view;
[0029] Fig.15 It is a structural schematic diagram of the outer side surface of the right end cover in the present invention;
[0030] Fig.16 It is a structural schematic diagram of the inner side of the right end cover in the present invention;
[0031] Fig.17 yes Fig.15 Middle DD section view;
[0032] In the figure: 1, steel shell 2, aluminum core 3, left end cover 4, right end cover 5, semicircular groove 6, rectangular groove. [Specific implementation method]
[0033] The present invention is further described below in conjunction with the accompanying drawings:
[0034] As shown in the accompanying drawings, the present invention provides an AB axis cradle structure, comprising a steel shell 1, an aluminum core 2, a left end cover 3 and a right end cover 4. The steel shell 1 is made of stainless steel, and the aluminum core 2 is processed from an aluminum rod. The steel shell 1 is a cylindrical shape with open left and right ends and a circular ring-shaped cross section. A semicircular groove 5 is dug in the middle of the steel shell 1. The aluminum core 2 is an aluminum core shaft with a semicircular cross section. A rectangular groove 6 is dug inside the aluminum core 2 and penetrates along the axial direction. The outer cylindrical surface of the aluminum core 2 is matched and connected with the inner cylindrical surface of the steel shell 1. The aluminum core 2 is nested in the steel shell 1, and an interference fit is adopted between the aluminum core 2 and the steel shell 1. The inner cylindrical surfaces of the circular rings at the left and right ends of the steel shell 1 are respectively matched and connected with the outer cylindrical surfaces of the left end cover 3 and the right end cover 4. The left end cover 3 and the right end cover 4 are embedded in the two ends of the steel shell 1, and an interference fit is adopted between the steel shell 1; the left end cover 3 and the right end cover 4 are processed with threaded holes, through holes and pin holes.
[0035] The present invention is used in conjunction with a linear module and is applied to an AB axis platform. The cradle structure mainly includes a steel shell, a left end cover, a right end cover and an aluminum core. The steel shell and the aluminum core are connected by nesting. The processing method is to first fine-machine the inner circle size and end size of the aluminum core, and the inner circle size of the steel shell, using interference fit. Specifically, the steel shell is heated, and according to the principle of thermal expansion, the aluminum core is pressed into the steel shell. After cooling, the aluminum core will be nested in the steel shell. Since the area where the steel shell and the aluminum core cooperate is within half of the circle, even if the excess part of the aluminum core is cut off in the later processing, the aluminum core will not be transferred out. The end covers at both ends are embedded in the two ends of the steel shell in the same way. First, the outer circle and end face are fine-machined, and the inner circle and contour size are roughly machined. At the same time, the outer circle is embedded by interference fit.
[0036] The steel shell material is made of stainless steel. Before embedding, the outer circle and end face of the steel shell are turned by lathe, the inner circle is processed by boring machine, and the outer dimensions are cut by laser processing. The aluminum core uses an integral aluminum rod to finely turn the outer circle and end face. At this time, the left end face size has a few millimeters of margin, and the right end face has no margin. The left and right end covers are finely processed by lathe for the outer circle and end face size, and the internal contour is processed by NC, and the inner circle is rough-processed to make threaded holes, through holes and pin holes. Taking the right end face of the steel shell as the axial reference, the right end cover is pressed into the steel shell by interference fit and heating the steel shell, and then the temperature of the steel shell is maintained, and the aluminum core is pressed into the steel shell. After cooling, the size of the remaining left end face of the aluminum core is measured, and the excess amount is processed by lathe, and then the steel shell is heated again, and the left end cover is pressed into the steel shell. After embedding, the outer circle of the steel shell is used as the reference to process the concentric holes of the two end caps. At this time, because the rough processing is completed in the early stage, it is only necessary to locate the outer circle and then process the inner hole in the later stage. Then, the excess part of the aluminum core is processed according to the contour of the steel shell. At this time, it can be fixed axially on the turning and milling machine to finally process the installation surface; because the shell is made of steel, the structural rigidity is greater than the original integrated aluminum parts, which ensures the success rate of processing.
[0037] The cradle of the present invention adopts the processing technology of aluminum embedded in steel, and the embedded aluminum core adopts split processing and embedding, so the structural rigidity is enhanced. When it is lifted from the holes at both ends, it is not easy to cause the whole to deform when the clamp is loosened. At the same time, the success rate of processing is increased; and the split processing ensures the roundness and dimensional tolerance of the outer circle, and will not cause an increase in internal stress due to the subsequent cutting of other parts, thereby ensuring the accuracy of the overall parts.
[0038] The present invention is not limited to the above-mentioned embodiments, and any other changes, modifications, substitutions, combinations, and simplifications made without departing from the spirit and principles of the present invention shall be equivalent replacement methods and shall be included in the protection scope of the present invention.
Claims
1. A method for processing an AB axis cradle structure, characterized in that: The following steps are involved: Before the steel shell (1) is embedded, the outer circle and end face are machined by lathe, the inner circle is machined by boring machine, and the outer dimensions are cut by laser processing; the inner circle size and end size of the aluminum core (2) and the inner circle size of the steel shell (1) are finely machined, the steel shell (1) is heated, and according to the principle of thermal expansion, the aluminum core (2) is pressed into the steel shell (1), and after cooling, the aluminum core (2) is nested in the steel shell (1), and the matching area between the steel shell (1) and the aluminum core (2) is within half of the circle; the outer circle and end face size of the left end cover (3) and the right end cover (4) are finely machined by lathe, and the internal contour and the inner circle are roughly machined by NC, and the threaded holes, through holes and pin holes are made, and the left end cover (3) and the right end cover (4) are embedded in the two ends of the steel shell (1) in the same way; The AB axis cradle structure comprises a steel shell (1), an aluminum core (2), a left end cover (3) and a right end cover (4); the steel shell (1) is a cylindrical shape with open left and right ends and a circular ring-shaped cross section; a semicircular groove (5) is dug in the middle of the steel shell (1); the aluminum core (2) is an aluminum core shaft with a semicircular cross section; a rectangular groove (6) is dug inside the aluminum core (2) and passes through along the axial direction; the outer cylindrical surface of the aluminum core (2) is matched and connected with the inner cylindrical surface of the steel shell (1); the aluminum core (2) is nested in the steel shell (1). , and an interference fit is adopted between the aluminum core (2) and the steel shell (1); the inner circular surfaces of the circular rings at the left and right ends of the steel shell (1) are respectively matched and connected with the outer circular surfaces of the left end cover (3) and the right end cover (4); the left end cover (3) and the right end cover (4) are embedded in the two ends of the steel shell (1) and an interference fit is adopted between the steel shell (1); the steel shell (1) is made of stainless steel; the aluminum core (2) is made of aluminum rod; the left end cover (3) and the right end cover (4) are both processed with threaded holes, through holes and pin holes.
2. The method according to claim 1, characterized in that: The aluminum core (2) is made of an integral aluminum rod, and its outer circle and end face are precision-turned, with a margin of several millimeters left on the left end face and no margin left on the right end face.
3. The method according to claim 1, characterized in that: The right end face of the steel shell (1) is used as an axial reference, and the right end cover (4) is first pressed into the steel shell (1) by means of interference fit and heating the steel shell (1). Then, the temperature of the steel shell (1) is maintained and the aluminum core (2) is pressed into the steel shell (1). After cooling, the size of the remaining left end face of the aluminum core (2) is measured, and the excess amount is processed by a lathe. Then, the steel shell (1) is heated again and the left end cover (3) is pressed into the steel shell (1). After the embedding is completed, the concentric holes of the left end cover (3) and the right end cover (4) are processed based on the outer circle of the steel shell (1), and the inner hole is processed after positioning by the outer circle. Then, the excess part of the aluminum core (2) is processed according to the contour of the steel shell (1), and after axial support and fixation on the turning and milling machine, the installation surface is finally processed.