A small angle slope structure and manufacturing method thereof
By forming grooves in the base structure, filling sacrificial materials and depositing film layers in the micro-electromechanical system, and forming a small-angle slope structure using air pressure difference, the problem of difficulty in preparing controllable small-angle slopes in traditional etching processes is solved, and production is improved Efficiency and structural stability.
Patent Information
- Application Number
- CN202110548246.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-05-19
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2041-05-19
AI Technical Summary
In existing micro-electromechanical systems, it is difficult for traditional etching processes to prepare controllable small-angle slope structures, and the wet etching process is costly and the angle is uncontrollable.
By forming grooves in the substrate structure, filling the sacrificial material and depositing a film layer, etching to form a window to release the sacrificial material, extruding the film layer with air pressure differential to form a closed cavity, and the production of a small angle slope structure is achieved.
The stability and production efficiency of the small-angle slope structure are improved, and the problems of high perpendicularity and uncontrollable angle caused by the etching process are solved.
Smart Images

Figure CN113277466B_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the technical field of micro-electromechanical systems, and in particular to a small-angle slope structure and a manufacturing method thereof. Background Art
[0002] Micro Electro Mechanical System (MEMS) is a technology for designing, processing, manufacturing, measuring and controlling micron / nano materials. It can integrate mechanical components, optical systems, drive components and electronic control systems into a micro system as an integral unit. It uses a manufacturing process that combines microelectronics technology and micromachining technology to produce a variety of high-performance, low-cost, miniaturized sensors and actuators.
[0003] In the field of MEMS, many MEMS structures are not only made on the plane, but also designed to make vertical structures. At present, the manufacturing process of most vertical structures mainly relies on etching. In the traditional etching process, the dry etching process has a high verticality, but it is impossible to make various small-angle graphic slopes. The corrosion interface of the isotropic corrosion of the wet etching process is even more uncontrollable, and generally unstable angles will appear, and the surface is rough, which cannot be mass-produced. The anisotropic corrosion process of the wet etching process can make structures such as corrosion slopes with stable angles, but the corrosion slope is closely related to the corrosion material, and requires the use of various materials, which is costly and the angle is uncontrollable. Summary of the invention
[0004] The embodiment of the present invention provides a small-angle slope structure and a manufacturing method thereof, so as to realize a controllable small-angle slope structure and improve production efficiency.
[0005] In a first aspect, an embodiment of the present invention provides a method for manufacturing a small-angle slope structure, comprising:
[0006] Etching the substrate structure to be processed to form at least one groove in the substrate structure to be processed;
[0007] Filling at least one of the grooves with a sacrificial material so that a surface of the at least one groove is flush with a surface of the substrate structure to be processed;
[0008] Depositing a first thin film layer on the surface of the substrate structure to be processed;
[0009] Etching the first thin film layer to form a window on the first thin film layer, wherein a vertical projection of the window on the surface of the substrate structure to be processed is located within a vertical projection of the sacrificial material on the surface of the substrate structure to be processed;
[0010] The sacrificial material filled in the groove is released through the window opening to form a cavity corresponding to the groove;
[0011] Depositing a second thin film layer on the first thin film layer and filling the opening to form a planar structure with a closed cavity;
[0012] The plane structure is squeezed by using air pressure difference until it is deformed and forms a slope.
[0013] Optionally, a second thin film layer is deposited on the first thin film layer, and the opening is filled to form a planar structure with a closed cavity, including:
[0014] A second thin film layer is deposited on the first thin film layer in a vacuum environment, and the opening is filled to form a planar structure with a closed vacuum cavity.
[0015] Optionally, utilizing air pressure difference to squeeze the planar structure until it is deformed and forms a slope, comprising:
[0016] The planar structure is placed in an air pressure chamber and air pressure of a set pressure is applied to form an air pressure difference inside and outside the closed cavity and generate an extrusion force until the planar structure is deformed and forms a slope.
[0017] Optionally, the thickness of the first film layer is in the range of 0.5-5 μm, and the thickness of the second film layer is in the range of 1-5 μm.
[0018] Optionally, the first film layer and the second film layer are made of the same material, and the material of the first film layer and / or the second film layer includes an insulating material or a metal material.
[0019] Optionally, the shape obtained by cross-sectioning the groove along any plane parallel to the surface of the substrate structure to be processed includes a rectangle, a circle, and a ring.
[0020] Optionally, the openings include a plurality of openings penetrating the first film layer, and the plurality of openings are arranged in a plurality of rows or columns or in a circular arrangement.
[0021] Optionally, the aperture of the opening is less than or equal to 1 μm.
[0022] Optionally, the window opening is located at a non-bottom position of the slope.
[0023] In a second aspect, an embodiment of the present invention further provides a small-angle slope structure, including a base structure and a first film layer and a second film layer sequentially stacked on a surface of the base structure;
[0024] A groove is formed in the base structure, and the first film layer and the second film layer cover the groove in the base structure to form a closed cavity;
[0025] The first film layer is provided with a window penetrating from top to bottom, the vertical projection of the window on the surface of the substrate structure to be processed is located in the vertical projection of the groove on the surface of the substrate structure, and the second film layer fills the window and covers the first film layer;
[0026] Parts of the first film layer and the second film layer located in the area where the groove is located are recessed to form a slope.
[0027] A method for manufacturing a small-angle slope structure provided by an embodiment of the present invention comprises the following steps: etching a substrate structure to be processed to form at least one groove in the substrate structure to be processed, filling at least one groove with a sacrificial material so that the surface of the at least one groove is flush with the surface of the substrate structure to be processed, depositing a first thin film layer on the surface of the substrate structure to be processed, etching the first thin film layer, forming a window on the first thin film layer, wherein the vertical projection of the window on the surface of the substrate structure to be processed is located in the vertical projection of the sacrificial material on the surface of the substrate structure to be processed, releasing the sacrificial material filled in the groove through the window to form a cavity corresponding to the groove, depositing a second thin film layer on the first thin film layer, and filling the window to form a planar structure with a closed cavity, and utilizing an air pressure difference to extrude the planar structure until it is deformed and forms a slope, thereby solving the problem in the prior art that a controllable small-angle slope structure cannot be prepared due to the high verticality of the etching process, thereby achieving the stability of the small-angle slope structure and improving production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Other features, objects and advantages of the present invention will become more apparent from the detailed description of non-limiting embodiments made with reference to the following drawings:
[0029] Figure 1 A schematic flow chart of a method for manufacturing a small-angle slope structure provided by an embodiment of the present invention;
[0030] Figure 2 A schematic diagram of a process flow of a method for manufacturing a small-angle slope structure provided by an embodiment of the present invention;
[0031] Figure 3 A schematic structural diagram of a small-angle slope structure provided by an embodiment of the present invention;
[0032] Figure 4-Figure 6 A schematic diagram of a semi-finished product manufactured according to a method for manufacturing a small-angle slope structure provided in an embodiment of the present invention;
[0033] Figure 7 A schematic diagram of opening a window on a small-angle slope structure provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0034] In order to make the purpose, technical solution and advantages of the present invention clearer, the specific embodiments of the present invention are further described in detail below in conjunction with the accompanying drawings. It should be understood that the specific embodiments described here are only used to explain the present invention, rather than to limit the present invention.
[0035] It is also necessary to explain that in order to further illustrate the technical means and effects adopted by the present invention to achieve the predetermined purpose of the invention, the specific implementation method, structure, characteristics and effects of a small-angle slope structure and a manufacturing method thereof proposed by the present invention are described in detail below in combination with the accompanying drawings and preferred embodiments.
[0036] Figure 1 A schematic diagram of a process for manufacturing a small-angle slope structure provided by an embodiment of the present invention. Figure 1 The production method specifically comprises the following steps:
[0037] S110, etching the substrate structure to be processed to form at least one groove in the substrate structure to be processed.
[0038] Correspondingly, in order to more clearly illustrate the method for manufacturing the small-angle slope structure provided in this embodiment, a flowchart of the process preparation is used for further explanation.
[0039] Figure 2 A schematic diagram of a process flow of a method for manufacturing a small-angle slope structure provided in an embodiment of the present invention. Figure 3 A schematic structural diagram of a small-angle slope structure provided in an embodiment of the present invention.
[0040] Reference Figure 2 As shown in FIG. a), before etching the substrate structure 20 to be processed, it is necessary to perform patterning on the surface of the substrate structure 20 to be processed. For example, a pattern with alignment groove 21 marks is made on the surface of the substrate structure 20 to be processed by a photolithography mask process, and after the pattern of the groove 21 marks is defined, the mask 22 is removed.
[0041] Since the small-angle slope structure provided in this embodiment can be applied to different sensors, when the surface of the substrate structure to be processed is patterned, it is necessary to perform simulation design based on the size of the applicable sensor and the required slope, and then further use a photolithography mask process to define the pattern.
[0042] In addition, in practical applications, the substrate structure 20 to be processed should also include a sensor chip (not shown in the figure) suitable for the sensor, or the substrate structure 20 to be processed itself is a semi-finished product of the sensor chip. The sensor chip can be embedded in the substrate structure to be processed, and the material of other parts of the substrate structure to be processed can be silicon or silicon compounds except for the sensor chip.
[0043] Reference Figure 2 b), a dry etching process is used to perform etching according to the pattern defined on the surface of the substrate structure to be processed 20, and at least one groove 21 is formed in the substrate structure to be processed. Among them, when etching is performed using a dry etching process, vertical etching is performed according to the pattern defined on the surface of the substrate structure to be processed, and the side wall profile can be well controlled, and the inner wall of the formed groove 21 is also vertical. In some other embodiments, the substrate structure to be processed can also be placed in a strong alkaline KOH solution. Since the material of the substrate structure to be processed is silicon or a silicon compound, the KOH solution reacts chemically with it until the structure at the pattern defined on the surface of the substrate structure to be processed is completely corroded, and finally at least one groove 21 is formed. When the KOH solution is used for etching, the solution ratio is controlled according to the chemical reaction to form the shape required for etching. By utilizing this feature, when a slope structure is required in the sensor, a structure with a sloped inner wall of the groove 21 can be obtained by etching with a KOH solution.
[0044] S120, filling at least one groove with a sacrificial material so that a surface of the at least one groove is flush with a surface of the substrate structure to be processed.
[0045] The sacrificial layer material may be silicon dioxide or polyimide, and the growth method thereof may be a plasma enhanced chemical vapor deposition method or a spin coating method to fill the groove.
[0046] Preferably, in this embodiment, the sacrificial layer material may be silicon dioxide deposited by chemical vapor deposition. Figure 2 c), after filling at least one groove 21 with sacrificial material, a planarization process is used to keep the surface of the substrate structure 20 to be processed and the surfaces of all the grooves 21 flat. At this time, at least one groove 21 is filled with the sacrificial layer material.
[0047] It should be noted that, in this embodiment, the planarization process may be one of the conventional methods such as heat flow method, deposition method, etch-back method, etc., which is not limited here.
[0048] S130, depositing a first thin film layer on the surface of the substrate structure to be processed.
[0049] Specifically, after the substrate structure to be processed and at least one groove are planarized, Figure 2 d), a thin film is deposited on the flat surface of the substrate structure 20 to be processed by physical vapor deposition (PVD) to form a first thin film layer 23.
[0050] Among them, the PVD deposition method is a process that uses physical processes to transfer substances to the surface of a substrate. It has special properties such as high strength, wear resistance and strong heat dissipation. In practical applications, PVD deposition usually uses sputtering, vacuum evaporation, ion plating and other methods to achieve thin film deposition.
[0051] S140, etching the first thin film layer to form a window on the first thin film layer, wherein a vertical projection of the window on the surface of the substrate structure to be processed is located within a vertical projection of the sacrificial material on the surface of the substrate structure to be processed.
[0052] Before etching the first thin film layer, it is necessary to perform a patterning process on the surface of the first thin film layer to define the position and size of the window. The same patterning process as in the above step is used to make a pattern with alignment window marks on the surface of the first thin film layer. Figure 2 As shown in Figure e), after the window pattern is defined, the window 24 with the defined pattern is etched using an etching process.
[0053] Since the window 24 in this embodiment is used to release the sacrificial material filled in the above steps and fill the vacuum into the groove 21, when defining the position of the window on the surface of the first film layer, it is necessary to ensure that when the window 24 is on the surface of the first film layer 23, its vertical projection on the surface of the substrate structure 20 to be processed is located in the vertical projection of the sacrificial material on the surface of the substrate structure 20 to be processed, so as to ensure that a window 24 is provided directly above the sacrificial material filled in each groove 21, so as to facilitate the release of the sacrificial material and shorten the release path.
[0054] S150, releasing the sacrificial material filled in the groove by opening a window to form a cavity corresponding to the groove.
[0055] Specifically, refer to Figure 2 f), performing a release process to remove the sacrificial material in each groove 21, and forming a cavity groove in the substrate structure 20 to be processed.
[0056] Exemplarily, when performing the release process, release can be performed by wet etching, and the substrate structure 20 to be processed containing the sacrificial material is placed in a strong alkaline KOH solution, so that the KOH solution reacts with the sacrificial material made of silicon dioxide and is released from the window 24, thereby removing all the sacrificial materials and finally forming a cavity structure.
[0057] S160, depositing a second thin film layer on the first thin film layer and filling the openings to form a planar structure with a closed cavity.
[0058] Specifically, refer to Figure 2g), a thin film is continuously deposited on the surface of the first thin film layer 23 using the same PVD deposition method in the above steps to form a second thin film layer 25, and the opening 24 is filled while depositing the second thin film layer 25, so that a closed vacuum cavity is formed in at least one cavity groove 21 in the substrate structure to be processed.
[0059] Optionally, a second thin film layer 25 is deposited on the first thin film layer 23, and the window 24 is filled to form a planar structure with a closed cavity, including: depositing the second thin film layer 25 on the first thin film layer 23 in a vacuum environment, and filling the window 24 to form a planar structure with a closed vacuum cavity.
[0060] Since the small-angle slope structure provided in this embodiment needs to form a slope on the surface of the structure after preparation, this can be achieved by utilizing the pressure difference between the external atmospheric environment and the vacuum cavity in the groove 24. After releasing the sacrificial material, the window 24 needs to be filled while the second film layer 25 is deposited on the first film layer 23. Filling in a vacuum environment is conducive to filling the cavity with as much vacuum as possible, so that the groove 24 forms a closed vacuum cavity.
[0061] It should be noted that the first thin film layer 23 and the second thin film layer 25 have the same preparation process and the two thin film layers have the same thickness, which facilitates the use of the same deposition process to reduce the preparation process.
[0062] S170, utilizing air pressure difference to extrude the planar structure until it is deformed and forms a slope.
[0063] Specifically, refer to Figure 2 h), the structure prepared in the above steps is placed in the atmospheric environment. Due to the pressure difference between the external atmospheric environment and the vacuum cavity in the substrate structure 20 to be processed, the second film layer 25 and the first film layer 23 are squeezed by utilizing the pressure difference, so that the two film layers are concave in the vertical direction and present a slope shape with a smaller angle, thereby obtaining the small-angle slope structure required in this embodiment.
[0064] Optionally, utilizing air pressure difference to extrude the planar structure until it is deformed and forms a slope, including: placing the planar structure in an air pressure chamber and applying air pressure of a set pressure to form an air pressure difference inside and outside the closed cavity and generate an extrusion force until the planar structure is deformed and forms a slope.
[0065] It should be noted that since some sensors require a specific slope structure, when the pressure difference generated by placing the structure prepared in the above steps in the atmospheric environment is not sufficient to cause the two layers of film to deform and generate a slope, the planar structure can be placed in an air pressure chamber and air pressure of a set pressure can be applied to form an air pressure difference inside and outside the closed cavity and generate an extrusion force until the planar structure is deformed and forms a slope. This method can be used as an optional solution of this embodiment, and is not a limiting solution.
[0066] According to the above-mentioned process, the small-angle slope structure provided in this embodiment can be obtained. The specific structural diagram can be referred to as Figure 3 .
[0067] The method for manufacturing a small-angle slope structure provided in the present embodiment comprises the following steps: etching a substrate structure to be processed to form at least one groove in the substrate structure to be processed, filling at least one groove with a sacrificial material so that the surface of the at least one groove is flush with the surface of the substrate structure to be processed, depositing a first thin film layer on the surface of the substrate structure to be processed, etching the first thin film layer, forming a window on the first thin film layer, wherein the vertical projection of the window on the surface of the substrate structure to be processed is located within the vertical projection of the sacrificial material on the surface of the substrate structure to be processed, releasing the sacrificial material filled in the groove through the window to form a cavity corresponding to the groove, depositing a second thin film layer on the first thin film layer, and filling the window to form a planar structure with a closed cavity, and utilizing an air pressure difference to extrude the planar structure until it is deformed and forms a slope, thereby solving the problem in the prior art that a controllable small-angle slope structure cannot be prepared due to the high verticality of the etching process, thereby achieving the stability of the small-angle slope structure and improving production efficiency.
[0068] Optionally, the thickness of the first film layer 23 is in the range of 0.5-5 μm, and the thickness of the second film layer 25 is in the range of 1-5 μm.
[0069] Among them, when the prepared structure is placed in an atmospheric environment or an air pressure chamber, there is a pressure difference between the external atmospheric environment and the vacuum in the vacuum cavity. When the second film layer 25 and the first film layer 23 are squeezed by using this pressure difference, the two film layers are deformed and a slope phenomenon appears. The thickness of the slope is mainly controlled by the thickness of the two film layers.
[0070] It should be noted that the thickness of the second film layer is closely related to the window provided in the above embodiment, and the minimum thickness of the second film layer must be greater than the radius of the window.
[0071] Optionally, the first film layer 23 and the second film layer 25 are made of the same material, and the material of the first film layer 23 and / or the second film layer 25 includes an insulating material or a metal material.
[0072] Among them, when the materials of the first thin film layer 23 and the second thin film layer 25 are the same, commonly used insulating materials include Si, SiO2, SiN, etc., and commonly used metal materials include Al, 97% Al-3% Ti alloy, Ti, TiW and other metals. Since different materials have different inherent stiffness, when selecting insulating materials or metal materials as the materials of the thin film layer, it is mainly based on the structural angle requirements in the sensor.
[0073] It should be noted that, due to different requirements for the angle slope of the structure surface in different sensors, the materials of the first film layer 23 and the second film layer 25 may also be different. For example, when the structure surface does not need to be conductive, the material of the second film layer 25 must be an insulating material. If the structure surface needs to be conductive, the material of the second film layer 25 can first use a metal material as a lead. In the preparation process, it is preferred to select a good material, which is conducive to controlling the slope angle.
[0074] Optionally, Figure 4-Figure 6 A schematic diagram of a semi-finished product made according to a method for making a small-angle slope structure provided by an embodiment of the present invention. The shapes obtained by cross-sectioning the groove 24 along any plane parallel to the surface of the substrate structure 20 to be processed include rectangle, circle, and ring.
[0075] in, Figure 4 Schematic diagram of a rectangular shape obtained by cross-sectioning the groove 24 along any plane parallel to the surface of the substrate structure 20 to be processed, Figure 5 Schematic diagram showing that the shape of the groove 24 obtained by cross-sectioning along any plane parallel to the surface of the substrate structure 20 to be processed is circular, Figure 6 The diagram is a schematic diagram showing that the shape of the groove 24 obtained by any plane cross-section parallel to the surface of the substrate structure 20 to be processed is annular. The shape of the groove 24 obtained by the plane cross-section of the surface of the substrate structure 20 to be processed is obtained by reasonable simulation design and graphical processing is performed on the surface of the substrate structure to be processed.
[0076] It should be noted that the semi-finished product of the small-angle slope structure provided in this embodiment is obtained corresponding to step S110 in the method for manufacturing the small-angle slope structure in the above embodiment.
[0077] For example, when the shape of the groove obtained by the plane cross section of the surface of the substrate structure to be processed is a rectangle, each two grooves obtained after etching are separated by a retaining wall, and the material of the retaining wall is the material of the substrate structure to be processed. The interval between each two rectangular grooves is equal, and the retaining wall structure plays a limiting role during etching and a supporting role when the structure is extruded by using the pressure difference after forming.
[0078] Optionally, Figure 7 A schematic diagram of a window opening on a small-angle slope structure provided by an embodiment of the present invention. Figure 7 As shown, the openings include a plurality of openings 26 penetrating the first film layer, and the plurality of openings 26 are arranged in a plurality of rows or columns or in a circumferential arrangement.
[0079] Optionally, the diameter D of the opening 26 is less than or equal to 1 μm.
[0080] Optionally, refer to Figure 2In Figure h), the window is located at a non-bottom position of the slope.
[0081] Among them, refer to Figure 2 d. A window is formed after etching the first thin film layer. The window penetrates the first thin film layer and is connected to the groove in the substrate structure to be processed, which is conducive to directly filling and releasing the sacrificial material.
[0082] It should be noted that the shape of the multiple openings on the first film layer can be rectangular or circular, and the size of the openings is kept below 1 μm. In order to avoid the first film layer and the second film layer from breaking due to pressure during extrusion, the openings should be set at a non-extrusion position, that is, a position without a slope.
[0083] The embodiment of the present invention also provides a small angle slope structure, and its structural schematic diagram can be further referred to. Figure 3 The structure 300 includes a base structure 20 and a first film layer 23 and a second film layer 25 sequentially stacked on the surface of the base structure 20, a groove 21 is formed in the base structure 20, the first film layer 23 and the second film layer 25 cover the groove 21 in the base structure 20 and form a closed cavity, a window 24 is provided on the first film layer 23 which runs through from top to bottom, the vertical projection of the window 24 on the surface of the base structure 20 to be processed is located in the vertical projection of the groove 21 on the surface of the base structure 29, the second film layer 25 fills in the window 24 and covers the first film layer 23, and the first film layer 23 and the second film layer 25 are partially recessed in the area where the groove 21 is located to form a slope.
[0084] Among them, the small-angle slope structure 300 in this embodiment can be obtained according to the preparation method of the small-angle slope structure provided in the above embodiment. The structure 300 has the same or corresponding beneficial effects of the small-angle slope structure provided in the above embodiment, which will not be repeated here.
[0085] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.
Claims
1. A method for manufacturing a small-angle slope structure, characterized in that: include: Etching the substrate structure to be processed to form at least one groove in the substrate structure to be processed; Filling at least one of the grooves with a sacrificial material so that a surface of the at least one groove is flush with a surface of the substrate structure to be processed; Depositing a first thin film layer on the surface of the substrate structure to be processed; Etching the first thin film layer to form a window on the first thin film layer, wherein a vertical projection of the window on the surface of the substrate structure to be processed is located within a vertical projection of the sacrificial material on the surface of the substrate structure to be processed; The sacrificial material filled in the groove is released through the window opening to form a cavity corresponding to the groove; Depositing a second thin film layer on the first thin film layer and filling the opening to form a planar structure with a closed cavity; Using air pressure difference to squeeze the planar structure until it is deformed and forms a slope; The openings include a plurality of openings penetrating the first film layer, wherein the plurality of openings are arranged in a plurality of rows or columns or in a circumferential arrangement; and the openings are disposed at a position where the first film layer does not present a slope.
2. The method for manufacturing a small-angle slope structure according to claim 1, characterized in that: Depositing a second thin film layer on the first thin film layer and filling the openings to form a planar structure with a closed cavity, comprising: A second thin film layer is deposited on the first thin film layer in a vacuum environment, and the opening is filled to form a planar structure with a closed vacuum cavity.
3. The method for manufacturing a small-angle slope structure according to claim 1, characterized in that: The planar structure is squeezed by using air pressure difference to deform and form a slope, comprising: The planar structure is placed in an air pressure chamber and air pressure of a set pressure is applied to form an air pressure difference inside and outside the closed cavity and generate an extrusion force until the planar structure is deformed and forms a slope.
4. The method for manufacturing a small-angle slope structure according to claim 1, characterized in that: The thickness of the first film layer is in the range of 0.5-5 μm, and the thickness of the second film layer is in the range of 1-5 μm.
5. The method for manufacturing a small-angle slope structure according to claim 1, characterized in that: The first film layer and the second film layer are made of the same material, and the material of the first film layer and / or the second film layer includes an insulating material or a metal material.
6. The method for manufacturing a small-angle slope structure according to claim 1, characterized in that: The shapes obtained by cross-sectioning the groove along any plane parallel to the surface of the substrate structure to be processed include rectangle, circle and ring.
7. The method for manufacturing a small-angle slope structure according to claim 1, characterized in that: The aperture of the opening is less than or equal to 1 μm.
8. The method for manufacturing a small-angle slope structure according to claim 1, characterized in that: The window opening is located at a non-bottom position of the slope.
9. A small-angle slope structure, characterized in that: It comprises a base structure and a first film layer and a second film layer sequentially stacked on the surface of the base structure; A groove is formed in the base structure, and the first film layer and the second film layer cover the groove in the base structure to form a closed cavity; The first film layer is provided with a window penetrating from top to bottom, the vertical projection of the window on the surface of the substrate structure to be processed is located in the vertical projection of the groove on the surface of the substrate structure, and the second film layer fills the window and covers the first film layer; Parts of the first film layer and the second film layer located in the area where the groove is located are recessed to form a slope; The openings include a plurality of openings penetrating the first film layer, wherein the plurality of openings are arranged in a plurality of rows or columns or in a circumferential arrangement; and the openings are disposed at a position where the first film layer does not present a slope.