A manufacturing process for quartz glass microneedle coating and a quartz glass microneedle device

CN113332587BActive Publication Date: 2024-11-26SHENZHEN XUMEI TECH CO LTD
View PDF 0 Cites -1 Cited by

Patent Information

Application Number
CN202110571936.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-05-25
Publication Date
2024-11-26
Estimated Expiration
2041-05-25

Smart Images

  • Figure CN113332587B_ABST
    Figure CN113332587B_ABST
Patent Text Reader

Abstract

The present invention discloses a manufacturing process for quartz glass microneedle coating and a quartz glass microneedle device, and specifically relates to the technical field of quartz glass microneedles. The specific steps are as follows: Step 1: First, a non-through hole-shaped groove is made on the front side of a silicon wafer by deep silicon dry etching; Step 2: Use thermal oxidation to cause vapor deposition on the front and back sides of the silicon wafer and the inner wall of the hole to form a thick oxide layer; Step 3: Use a glue coating photolithography method to form corrosion window patterns on the front and back sides of the silicon wafer. The present invention sets a manufacturing process for quartz glass microneedle coating. After coating, the surface smoothness of the quartz glass microneedle is increased, so that when the quartz glass microneedle enters the epidermis of the skin during use, it can quickly and effectively separate from the cell tissue of the epidermis after effectively cleaning the skin, avoiding bacterial growth and preventing secondary pollution damage to the skin. The use effect is good, and it can effectively avoid inflammation and acne after the skin is used, and black spots on the facial skin are grown, and the use safety is strong.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of quartz glass microneedles, and in particular to a manufacturing process for coating a quartz glass microneedle and a quartz glass microneedle device. Background Art

[0002] Nano-microneedles on the market are currently made of stainless steel and ordinary single-crystal silicon wafers. Although stainless steel has the advantage of being cheap, its material hardness and brittleness during processing make it impossible to achieve the minimum size of 80 nanometers for the microneedle head, resulting in the inability to reach the requirement of piercing the epidermis of the skin. Although single-crystal silicon can currently meet the 80-nanometer size requirement for the needle tip, its surface roughness is too low, making it difficult for epidermal cells and proteins to effectively separate from the nano-microneedle wafer. When the nano-microneedles are working, the cells and proteins in the epidermis of the skin are exposed to air pollution and oxidation and then enter the skin, which can easily cause inflammation of sensitive skin and acne, and leave black spots on the face.

[0003] Moreover, when using existing nano-microneedles, they often need to be picked up by hand for installation and operation, which is not only easy to cause puncture injuries, but also easy to cause bacterial growth and cross infection, and has low safety in use. Summary of the invention

[0004] To this end, the present invention provides a quartz glass microneedle coating manufacturing process and a quartz glass microneedle device. Through the setting of the quartz glass microneedle coating manufacturing process, after coating, the surface smoothness of the quartz glass microneedle is improved, so that when the quartz glass microneedle enters the epidermis of the skin during use, it can be quickly and effectively separated from the cell tissue of the epidermis after effectively cleaning the skin, thereby avoiding bacterial growth and preventing secondary pollution damage to the skin. The use effect is good, and the skin inflammation and acne after use can be effectively avoided, and the facial skin can be protected from black spots. The use safety is strong and the practicability is strong, so as to solve the problems of bacterial growth and pigmentation during use caused by the excessive size of the nano-microneedles in the market and the low surface roughness in the prior art.

[0005] In order to achieve the above object, the present invention provides the following technical solution: a manufacturing process of quartz glass microneedle coating, the specific steps are as follows:

[0006] Step 1: First, a non-through hole-shaped groove is made on the front side of the silicon wafer by deep silicon dry etching;

[0007] Step 2: Use thermal oxidation to cause vapor deposition on the front and back surfaces of the silicon wafer and the inner wall of the hole to form a thick oxide layer;

[0008] Step 3: Forming etching window patterns on the front and back sides of the silicon wafer respectively by using a photolithography method;

[0009] Step 4: Remove the silicon dioxide in the window by dry or wet etching to expose the substrate silicon;

[0010] Step 5: remove the photoresist, and etch the silicon wafer with a single crystal silicon anisotropic etching solution to form a micro-needle structure on the upper surface of the silicon wafer and a groove structure on the lower surface, so that the hole-shaped groove penetrates the micro-needle structure on the front side of the silicon wafer, and the bottom of the hole-shaped groove is connected to the groove structure on the back side of the silicon wafer to form a cone shape;

[0011] Step 6: Use an environmentally friendly coating process to coat the silicon wafer and the microneedles on the front of the silicon wafer with a thin film.

[0012] Furthermore, the silicon wafer type in step 1 is an N-type 100 silicon wafer.

[0013] Furthermore, in step 2, the main component of the thick oxide layer is silicon dioxide.

[0014] Furthermore, in the dry method in step 4, ammonia and hydrofluoric acid vapor are used to react with silicon dioxide to generate ammonium fluorosilicate, and the ammonium fluorosilicate is heated to 95-203° C. to volatilize it and expose the substrate silicon.

[0015] Furthermore, the wet etching in step 4 uses an etching solution containing hydrofluoric acid.

[0016] Furthermore, the tip of the cone in step five reaches 30-80 nm.

[0017] Furthermore, the environmentally friendly coating process in step six is ​​plasma enhanced chemical vapor deposition coating, and the coating process is: first, the silicon wafer microneedle is transferred to the reaction chamber, and then silane and nitrogen are mixed at a volume flow ratio of 1:1-15 to form a gas phase, and the gas phase is introduced into the reaction chamber three times. During the three depositions, the deposition temperature of the reaction chamber is adjusted to 180-620°C, the deposition chamber pressure is adjusted to 450-3040mTorr, and the deposition time is controlled to 35-500s. Finally, a three-layer silicon oxynitride film is obtained on the surface of the silicon wafer microneedle, and the total film thickness is 5-10nm.

[0018] Furthermore, in the environmentally friendly coating process in step six, the coating colors include: 18K gold, purple sapphire, sapphire blue and other process colors.

[0019] The present invention also includes a quartz glass microneedle device, including a diamond-shaped glass shell, a rear outer wall of the diamond-shaped glass shell is provided with a fixing thread, a stepped mounting cavity is provided inside the diamond-shaped glass shell, a microneedle fixing connecting rod is slidably connected in the stepped mounting cavity, a sliding cavity is provided in the microneedle fixing connecting rod, a push rod is slidably connected in the sliding cavity, a spring is elastically installed between the front wall of the rear end of the push rod and the middle of the stepped mounting cavity, and a quartz glass microneedle is fixedly connected to the front wall of the microneedle fixing connecting rod.

[0020] The present invention has the following advantages:

[0021] 1. The present invention sets a manufacturing process for quartz glass microneedle coating. Compared with the prior art, after coating, the surface smoothness of the quartz glass microneedle is improved, so that when the quartz glass microneedle enters the epidermis of the skin during use, it can quickly and effectively separate from the cell tissue of the epidermis after effectively cleaning the skin, thereby avoiding bacterial growth and secondary pollution damage to the skin. The use effect is good, and the skin inflammation and acne after use can be effectively avoided, and the facial skin can be protected from black spots. The use safety is strong and the practicability is strong;

[0022] 2. Compared with the prior art, the present invention, through the setting of the quartz glass microneedle device, can fix the quartz glass microneedle on the front wall of the microneedle fixing connecting rod when the quartz glass microneedle needs to be used to clean the skin. When the position of the quartz glass microneedle needs to be moved, the push rod can be pushed to slide in the sliding cavity to compress or pull the spring, and the microneedle fixing connecting rod can be controlled to extend and retract forward and backward in the stepped installation cavity, thereby controlling the front and rear position of the quartz glass microneedle to make the quartz glass microneedle work, which can avoid direct contact between the hands and the quartz glass microneedle, prevent bacterial infection and breeding, and has a simple structure, low manufacturing cost, convenient operation, high safety, strong applicability, and is easy to promote. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the implementation of the present invention or the technical solution in the prior art, the following briefly introduces the drawings required for the implementation or the prior art description. Obviously, the drawings in the following description are only exemplary, and for ordinary technicians in this field, other implementation drawings can be derived from the provided drawings without creative work.

[0024] The structures, proportions, sizes, etc. illustrated in this specification are only used to match the contents disclosed in the specification so as to facilitate understanding and reading by persons familiar with the technology. They are not used to limit the conditions under which the present invention can be implemented, and therefore have no substantial technical significance. Any structural modification, change in proportion or adjustment of size shall still fall within the scope of the technical contents disclosed in the present invention without affecting the effects and purposes that can be achieved by the present invention.

[0025] Figure 1 This is a process flow chart of the quartz glass microneedle coating manufacturing process of the present invention;

[0026] Figure 2 This is a three-dimensional diagram of the overall structure of the quartz glass microneedle device of the present invention;

[0027] Figure 3 This is a top view of the structure of the quartz glass microneedle device of the present invention;

[0028] Figure 4 Schematic diagram of the top view of the quartz glass microneedle device of the present invention;

[0029] Figure 5 This is a top view of the structure of the quartz glass microneedle device of the present invention;

[0030] Figure 6 This is a three-dimensional diagram of the diamond-shaped glass shell structure of the present invention;

[0031] Figure 7 A three-dimensional diagram of the microneedle fixing connecting rod structure of the present invention;

[0032] Figure 8 It is a three-dimensional diagram of the top rod structure of the present invention;

[0033] Fig. 9 A three-dimensional diagram of the spring structure of the present invention;

[0034] Fig.10 This is a three-dimensional diagram of the quartz glass microneedle structure of the present invention;

[0035] Fig.11 It is a rear stereoscopic diagram of the matching structure of the diamond-shaped glass shell and the microneedle fixing connecting rod of the present invention.

[0036] In the figure: 1. Diamond-shaped glass shell; 2. Fixed thread; 3. Stepped mounting cavity; 4. Microneedle fixing connecting rod; 5. Sliding cavity; 6. Push rod; 7. Spring; 8. Quartz glass microneedle. DETAILED DESCRIPTION

[0037] The following is a description of the implementation of the present invention by specific embodiments. People familiar with the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0038] Embodiment 1:

[0039] Refer to the instruction manual Figure 1 The present invention provides a manufacturing process for quartz glass microneedle coating, and the specific steps are as follows:

[0040] Step 1: Prepare a silicon wafer of N-type 100, and use deep silicon dry etching to make a non-through hole-shaped groove on the front side of the silicon wafer;

[0041] Step 2: Use thermal oxidation to cause vapor deposition on the front and back surfaces of the silicon wafer and the inner wall of the hole to produce a silicon dioxide film, thereby forming a thick oxide layer;

[0042] Step 3: Forming etching window patterns on the front and back sides of the silicon wafer respectively by using a photolithography method;

[0043] Step 4: using ammonia gas and hydrofluoric acid vapor to react with silicon dioxide to generate ammonium fluorosilicate, and heating the ammonium fluorosilicate to 95°C to volatilize it, exposing the substrate silicon;

[0044] Step 5: Remove the photoresist and etch the silicon wafer with a single crystal silicon anisotropic etching solution to form a micro-needle structure on the upper surface of the silicon wafer and a groove structure on the lower surface, so that the hole-shaped groove penetrates the micro-needle structure on the front side of the silicon wafer, and the bottom of the hole-shaped groove is connected to the groove structure on the back side of the silicon wafer to form a cone shape, and the needle tip at the top of the cone reaches 80nm;

[0045] Step six: Use plasma enhanced chemical vapor deposition coating process to coat the silicon wafer and the microneedles on the front of the silicon wafer with a thin film. The coating process is as follows: first, transfer the silicon wafer microneedles to the reaction chamber, then mix silane and nitrogen at a volume flow ratio of 1:1 to form a gas phase, and introduce the gas phase into the reaction chamber three times. During the three depositions, the deposition temperature of the reaction chamber is adjusted to 180°C, the deposition chamber pressure is adjusted to 450mTorr, and the deposition time is controlled to 35s. Finally, a three-layer silicon oxynitride film is obtained on the surface of the silicon wafer microneedles. The total film thickness is 5nm and the color is 18K gold.

[0046] Embodiment 2:

[0047] Refer to the instruction manual Figure 1 The present invention provides a manufacturing process for quartz glass microneedle coating, and the specific steps are as follows:

[0048] Step 1: Prepare a silicon wafer of N-type 100, and use deep silicon dry etching to make a non-through hole-shaped groove on the front side of the silicon wafer;

[0049] Step 2: Use thermal oxidation to cause vapor deposition on the front and back surfaces of the silicon wafer and the inner wall of the hole to produce a silicon dioxide film, thereby forming a thick oxide layer;

[0050] Step 3: Forming etching window patterns on the front and back sides of the silicon wafer respectively by using a photolithography method;

[0051] Step 4: using ammonia gas and hydrofluoric acid vapor to react with silicon dioxide to generate ammonium fluorosilicate, and heating the ammonium fluorosilicate to 152°C to volatilize it, exposing the substrate silicon;

[0052] Step 5: Remove the photoresist and etch the silicon wafer with a single crystal silicon anisotropic etching solution to form a micro-needle structure on the upper surface of the silicon wafer and a groove structure on the lower surface, so that the hole-shaped groove penetrates the micro-needle structure on the front side of the silicon wafer, and the bottom of the hole-shaped groove is connected to the groove structure on the back side of the silicon wafer to form a cone shape, and the needle tip at the top of the cone reaches 50nm;

[0053] Step six: Use plasma enhanced chemical vapor deposition coating process to coat the silicon wafer and the microneedles on the front of the silicon wafer with a thin film. The coating process is as follows: first, the silicon wafer microneedles are transferred to the reaction chamber, and then silane and nitrogen are mixed at a volume flow ratio of 1:7 to form a gas phase, and the gas phase is introduced into the reaction chamber three times. During the three depositions, the deposition temperature of the reaction chamber is adjusted to 360°C, the deposition chamber pressure is adjusted to 1290mTorr, and the deposition time is controlled to 285s. Finally, a three-layer silicon oxynitride film is obtained on the surface of the silicon wafer microneedles. The total film thickness is 7nm and the color is amethyst.

[0054] Embodiment 3:

[0055] Refer to the instruction manual Figure 1 The present invention provides a manufacturing process for quartz glass microneedle coating, and the specific steps are as follows:

[0056] Step 1: Prepare a silicon wafer of N-type 100, and use deep silicon dry etching to make a non-through hole-shaped groove on the front side of the silicon wafer;

[0057] Step 2: Use thermal oxidation to cause vapor deposition on the front and back surfaces of the silicon wafer and the inner wall of the hole to produce a silicon dioxide film, thereby forming a thick oxide layer;

[0058] Step 3: Forming etching window patterns on the front and back sides of the silicon wafer respectively by using a photolithography method;

[0059] Step 4: using ammonia and hydrofluoric acid vapor to react with silicon dioxide to generate ammonium fluorosilicate, heating the ammonium fluorosilicate to 203°C to volatilize it, exposing the substrate silicon;

[0060] Step 5: Remove the photoresist and etch the silicon wafer with a single crystal silicon anisotropic etching solution to form a micro-needle structure on the upper surface of the silicon wafer and a groove structure on the lower surface, so that the hole-shaped groove penetrates the micro-needle structure on the front side of the silicon wafer, and the bottom of the hole-shaped groove is connected to the groove structure on the back side of the silicon wafer to form a cone shape, and the needle tip at the top of the cone reaches 30nm;

[0061] Step six: Use plasma enhanced chemical vapor deposition coating process to coat the silicon wafer and the microneedles on the front of the silicon wafer with a thin film. The coating process is as follows: first, the silicon wafer microneedles are transferred to the reaction chamber, and then silane and nitrogen are mixed at a volume flow ratio of 1:10 to form a gas phase, and the gas phase is introduced into the reaction chamber three times. During the three depositions, the deposition temperature of the reaction chamber is adjusted to 530°C, the deposition chamber pressure is adjusted to 2960mTorr, and the deposition time is controlled to 470s. Finally, a three-layer silicon oxynitride film is obtained on the surface of the silicon wafer microneedles. The total film thickness is 9nm and the color is sapphire blue.

[0062] Embodiment 4:

[0063] Refer to the instruction manual Figure 1The present invention provides a manufacturing process for quartz glass microneedle coating, and the specific steps are as follows:

[0064] Step 1: Prepare a silicon wafer of N-type 100, and use deep silicon dry etching to make a non-through hole-shaped groove on the front side of the silicon wafer;

[0065] Step 2: Use thermal oxidation to cause vapor deposition on the front and back surfaces of the silicon wafer and the inner wall of the hole to produce a silicon dioxide film, thereby forming a thick oxide layer;

[0066] Step 3: Forming etching window patterns on the front and back sides of the silicon wafer respectively by using a photolithography method;

[0067] Step 4: Use an etching solution containing hydrofluoric acid to react with silicon dioxide to remove silicon dioxide and expose the substrate silicon;

[0068] Step 5: Remove the photoresist and etch the silicon wafer with a single crystal silicon anisotropic etching solution to form a micro-needle structure on the upper surface of the silicon wafer and a groove structure on the lower surface, so that the hole-shaped groove penetrates the micro-needle structure on the front side of the silicon wafer, and the bottom of the hole-shaped groove is connected to the groove structure on the back side of the silicon wafer to form a cone shape, and the needle tip at the top of the cone reaches 40nm;

[0069] Step six: Use plasma enhanced chemical vapor deposition coating process to coat the silicon wafer and the microneedles on the front of the silicon wafer with a thin film. The coating process is as follows: first, the silicon wafer microneedles are transferred to the reaction chamber, and then silane and nitrogen are mixed at a volume flow ratio of 1:15 to form a gas phase, and the gas phase is introduced into the reaction chamber three times. During the three depositions, the deposition temperature of the reaction chamber is adjusted to 620°C, the deposition chamber pressure is adjusted to 3040mTorr, and the deposition time is controlled to 500s. Finally, a three-layer silicon oxynitride film is obtained on the surface of the silicon wafer microneedles. The total thickness of the film is 10nm and the color is amethyst.

[0070] Embodiment 5:

[0071] 150 nano-microneedle users were selected, and 30 people were divided into a group. They used the quartz glass microneedles prepared in Examples 1-4 and ordinary nano-microneedles sold on the market to clean their skin within 90 days, and the following data were obtained:

[0072] Microneedle tip size (nm) Surface roughness#timg# (IT15) Microneedle Color Microneedle contact with the skin surface Bacterial growth and pigmentation Example 1 85 0.006 18K Gold Good separation Slight bacterial growth and no pigmentation Example 2 57 0.004 purple sapphire color Completely out of touch No bacteria growth Example 3 39 0.002 Sapphire blue Completely out of touch No bacteria growth Example 4 50 0.005 purple sapphire color Fully detached No bacteria growth Control group 130 0.2 Silver Adhesion cells Melanin deposition after severe bacterial growth

[0073] It can be seen from the above table that the quartz glass microneedles of Examples 1-4 can all effectively clean the skin, but the improvement degree of Example 3 is the greatest. After coating, the surface smoothness of the quartz glass microneedles is high, so that when the quartz glass microneedles enter the epidermis of the skin during use, they can quickly and effectively separate from the cell tissue of the epidermis after effectively cleaning the skin, avoiding bacterial growth and causing secondary pollution damage to the skin. The use effect is good, and it can effectively prevent the skin from getting inflamed and acne after use, and black spots on the facial skin. It is safe to use and practical.

[0074] Embodiment 6:

[0075] Refer to the instruction manual Figure 2-11 The present invention also includes a quartz glass microneedle device, including a diamond-shaped glass shell 1, a fixing thread 2 is provided on the rear outer wall of the diamond-shaped glass shell 1, a stepped mounting cavity 3 is provided inside the diamond-shaped glass shell 1, a microneedle fixing connecting rod 4 is slidably connected in the stepped mounting cavity 3, a sliding cavity 5 is provided in the microneedle fixing connecting rod 4, a push rod 6 is slidably connected in the sliding cavity 5, a spring 7 is elastically installed between the front wall of the rear end of the push rod 6 and the middle of the stepped mounting cavity 3, and a quartz glass microneedle 8 is fixedly connected to the front wall of the microneedle fixing connecting rod 4.

[0076] The specific implementation scenario is as follows: when the quartz glass microneedle 8 needs to be used to clean the skin, the quartz glass microneedle 8 can be fixedly installed on the front wall of the microneedle fixing connecting rod 4. When the position of the quartz glass microneedle 8 needs to be moved, the push rod 6 can be pushed to slide in the sliding cavity 5 to compress or pull the spring 7, and control the microneedle fixing connecting rod 4 to extend and retract forward and backward in the stepped installation cavity 3, thereby controlling the front and rear position of the quartz glass microneedle 8 to make the quartz glass microneedle 8 work, which can avoid direct contact between the hands and the quartz glass microneedle 8, and avoid bacterial infection and breeding. It has a simple structure, low manufacturing cost, convenient operation, high safety, strong applicability, and is easy to promote. This implementation method specifically solves the problem that in the prior art, nano-microneedles often need to be picked up and installed by hand when used, which is not only easy to get stabbed, but also easy to cause bacterial breeding, cross infection, and low safety of use.

[0077] Although the present invention has been described in detail above by general description and specific embodiments, it is obvious to those skilled in the art that some modifications or improvements can be made to the present invention. Therefore, these modifications or improvements made without departing from the spirit of the present invention all belong to the scope of protection claimed by the present invention.

Claims

1. A manufacturing process for quartz glass microneedle coating, characterized by: The specific steps are as follows: Step 1: First, a non-through hole-shaped groove is made on the front side of the silicon wafer using deep silicon dry etching; Step 2: Use thermal oxidation to vapor-deposit the front and back surfaces of the silicon wafer and the inner wall of the hole to form a thick oxide layer; Step 3: Forming etching window patterns on the front and back of the silicon wafer using a resist photolithography method; Step 4: Remove the silicon dioxide in the window by dry or wet etching to expose the substrate silicon; The dry method uses ammonia and hydrofluoric acid vapor to react with silicon dioxide to generate ammonium fluorosilicate, which is then heated to 95-203°C to volatilize and expose the substrate silicon. Step 5: Remove the photoresist and etch the silicon wafer with a single-crystal silicon anisotropic etching solution to form a microneedle structure on the upper surface of the silicon wafer and a groove structure on the lower surface. The hole-shaped groove penetrates the microneedle structure on the front of the silicon wafer, and the bottom of the hole-shaped groove is connected to the groove structure on the back of the silicon wafer to form a cone shape. The needle tip at the top of the cone reaches 30-80nm. Step 6: Use an environmentally friendly coating process to coat the silicon wafer and the microneedles on the front of the silicon wafer with a thin film; The environmentally friendly coating process is plasma-enhanced chemical vapor deposition coating. The coating process is as follows: first, the silicon wafer microneedles are transferred to the reaction chamber, and then silane and nitrogen are mixed at a volume flow ratio of 1:15 to form a gas phase, and the gas phase is introduced into the reaction chamber three times. During the three depositions, the deposition temperature of the reaction chamber is adjusted to 180-620°C, the deposition chamber pressure is adjusted to 450-3040mTorr, and the deposition time is controlled to 35-500s. Finally, a three-layer silicon oxynitride film is obtained on the surface of the silicon wafer microneedles, and the total film thickness is 5-10nm.

2. The manufacturing process of a quartz glass microneedle coating according to claim 1, characterized in that: The silicon wafer type in step 1 is an N-type 100 silicon wafer.

3. The manufacturing process of a quartz glass microneedle coating according to claim 1, characterized in that: In step 2, the thick oxide layer is mainly composed of silicon dioxide.

4. The manufacturing process of a quartz glass microneedle coating according to claim 1, characterized in that: The wet etching in step 4 uses an etching solution containing hydrofluoric acid.

5. The manufacturing process of a quartz glass microneedle coating according to claim 1, characterized in that: In the environmentally friendly coating process in step six, the coating colors are: 18K gold, purple sapphire and sapphire blue.

6. A process for manufacturing a quartz glass microneedle coating according to any one of claims 1 to 5, characterized in that: The invention also includes a quartz glass microneedle device, comprising a diamond-shaped glass shell (1), a fixing thread (2) being provided on the rear outer wall of the diamond-shaped glass shell (1), a stepped mounting cavity (3) being provided inside the diamond-shaped glass shell (1), a microneedle fixing connecting rod (4) being slidably connected inside the stepped mounting cavity (3), a sliding cavity (5) being provided inside the microneedle fixing connecting rod (4), a push rod (6) being slidably connected inside the sliding cavity (5), a spring (7) being elastically provided between the front wall of the rear end of the push rod (6) and the middle of the stepped mounting cavity (3), and a quartz glass microneedle (8) being fixedly connected to the front wall of the microneedle fixing connecting rod (4).