Stage and method for manufacturing the stage
By uniformly spraying the insulating film on the stage and reducing the corner gap, the problem of insufficient voltage withstand insulating film in the prior art is solved, and the voltage withstand of the stage is increased.
Patent Information
- Application Number
- CN202080012364.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-03-01
- Filing Date
- 2020-02-25
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2040-02-25
AI Technical Summary
The existing spraying method causes gaps or gaps in the insulating film in the stage, reducing the withstand voltage, and it is difficult to meet the demand for increasing the withstand voltage in semiconductor device processing.
By uniformly spraying the insulating film on the substrate of the stage, the flat surface of the insulating film is ensured to be arranged in multiple directions, corner gaps or gaps are reduced, and alternating repeated spraying is used to form a dense insulating film, thereby improving the The voltage withstand the insulating film.
The insulation breakage voltage of the stage is significantly improved, the thickness deviation of the insulating film and the corner gap are reduced, and the voltage withstand performance of the stage is enhanced.
Smart Images

Figure CN113454761B_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present invention relate to a stage and a method for manufacturing the stage, for example, to a stage for mounting a substrate and a method for manufacturing the stage. Background Art
[0002] Semiconductor devices are mounted on almost all electronic devices and play an important role in the functions of electronic devices. Semiconductor devices are devices that utilize the semiconductor properties of silicon and the like. Semiconductor devices are formed by stacking semiconductor films, insulating films, and conductive films on a substrate and patterning these films. These films are stacked using evaporation, sputtering, chemical vapor deposition (CVD) or chemical reactions of substrates, and these films are patterned by photolithography. The photolithography process includes forming a resist on these films to be patterned, exposing the resist, forming a photoresist mask by development, partially removing these films by etching, and removing the photoresist mask.
[0003] The characteristics of the above-mentioned film depend largely on the conditions for forming the film or the conditions for patterning. One of the conditions is the voltage applied to the stage for setting the substrate (hereinafter referred to as the stage). With the miniaturization of semiconductor devices in recent years, the ratio of the diameter of the processed hole to the thickness of the processed film has become larger, so for example, the voltage applied to the stage possessed by the etching device has increased. As the voltage applied to the stage increases, it is required to improve the withstand voltage of the components possessed by the stage. The components possessed by the stage are, for example, a cooling plate, an electrostatic chuck, etc. Patent Documents 1 and 2 disclose a stage with improved withstand voltage by forming an insulating film on the surface through ceramic spraying, which is one of the spraying methods.
[0004] (Prior art literature)
[0005] (Patent Document)
[0006] Patent Document 1: Japanese Patent No. 6027407
[0007] Patent Document 2: Japanese Registered Utility Model No. 2600558 Summary of the invention
[0008] (Problems to be solved by the invention)
[0009] In the conventional spraying method, since the spraying direction is changed for each sprayed surface, a gap or void is generated at the boundary between the surfaces (hereinafter, sometimes referred to as a connection or a corner). Moreover, the withstand voltage of the sprayed insulating film is reduced due to the gap or void. Therefore, in the stage, it is a problem to increase the withstand voltage (hereinafter, sometimes referred to as the insulation breakdown voltage) of the components of the stage for spraying by reducing the gap or void in the insulating film sprayed by the spraying method.
[0010] One of the objects of the embodiments of the present invention is to provide a stage having a higher withstand voltage and a method for manufacturing the stage.
[0011] (Measures taken to solve the problem)
[0012] One embodiment of the present invention is a stage including: a substrate having a first surface and a second surface adjacent to the first surface; and an insulating film composed of a plurality of particles having flat surfaces, a portion of which is disposed along the first surface and the second surface.
[0013] In another embodiment, the substrate may include a third surface in a direction 180 degrees opposite to the first surface, and a portion of the flat surface of the insulating film may be disposed along the third surface.
[0014] In another embodiment, the surface extending from the first surface and the surface extending from the second surface may be arranged to intersect at 90 degrees.
[0015] In another embodiment, the ratio of the area of the void to the predetermined area of the insulating film may be 5% or less.
[0016] In another embodiment, the substrate may have channels for the flow of liquid.
[0017] In another embodiment, the electrostatic chuck may be disposed on an insulating film.
[0018] One of the embodiments of the present invention is a method for manufacturing a stage, which includes: a step of spraying an insulator toward a first surface from a direction perpendicular to the first surface while moving in a direction parallel to a first surface of a substrate; and a step of spraying an insulator toward a second surface from a direction perpendicular to the second surface while moving in a direction parallel to a second surface of a substrate adjacent to the first surface.
[0019] In another embodiment, the method may include: while moving in a direction parallel to a third surface of the substrate that is 180 degrees opposite to the first surface, spraying an insulator toward the third surface from a direction perpendicular to the third surface.
[0020] In another embodiment, a surface extending from the first surface and a surface extending from the second surface may be formed to intersect at 90 degrees.
[0021] In another embodiment, the step of continuously performing the steps of spraying the insulator onto the first surface and spraying the insulator onto the second surface may be included.
[0022] In another embodiment, the step of alternately and repeatedly spraying the insulator onto the first surface and spraying the insulator onto the second surface may be included.
[0023] In another embodiment, the steps of continuously performing the steps of spraying the insulator onto the third surface, spraying the insulator onto the second surface, and spraying the insulator onto the first surface may be included.
[0024] In another embodiment, the step of spraying a portion of particles included in the insulator with their flat surfaces along the first surface and the second surface may be included.
[0025] In another embodiment, the step of spraying a portion of particles included in the insulator with their flat surfaces along the third surface may be included. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1A It is a perspective view and a cross-sectional view which show the structure of the stage which concerns on one Embodiment of this invention.
[0027] Figure 1B It is a perspective view and a cross-sectional view which show the structure of the stage which concerns on one Embodiment of this invention.
[0028] Figure 1C It is a perspective view and a cross-sectional view which show the structure of the stage which concerns on one Embodiment of this invention.
[0029] Figure 2A It is a perspective view showing a method for manufacturing a stage according to one embodiment of the present invention.
[0030] Figure 2B It is a perspective view showing a method for manufacturing a stage according to one embodiment of the present invention.
[0031] Figure 2C It is a perspective view showing a method for manufacturing a stage according to one embodiment of the present invention.
[0032] Figure 3A It is a perspective view showing a method for manufacturing a stage according to one embodiment of the present invention.
[0033] Figure 3B It is a perspective view showing a method for manufacturing a stage according to one embodiment of the present invention.
[0034] Figure 3C It is a perspective view showing a method for manufacturing a stage according to one embodiment of the present invention.
[0035] Figure 4A This is a cross-sectional view for explaining a part of a corner portion of a conventional stage.
[0036] Figure 4B This is a cross-sectional view for explaining a part of a corner portion of a conventional stage.
[0037] Figure 4C This is a cross-sectional view for explaining a part of a corner portion of a conventional stage.
[0038] Figure 5A This is a cross-sectional view showing a part of a corner portion of a stage according to one embodiment of the present invention.
[0039] Figure 5B This is a cross-sectional view showing a part of a corner portion of a stage according to one embodiment of the present invention.
[0040] Fig. 6A This is a cross-sectional view showing a part of a corner portion of a stage according to one embodiment of the present invention.
[0041] Figure 6B This is a cross-sectional view showing a part of a corner portion of a stage according to one embodiment of the present invention.
[0042] Figure 7 This is an example of an image of a part of the corner of the stage according to one embodiment of the present invention captured by an electron microscope.
[0043] Fig. 8A It is a perspective view showing a method for manufacturing a stage according to one embodiment of the present invention.
[0044] Figure 8B It is a perspective view showing a method for manufacturing a stage according to one embodiment of the present invention.
[0045] Figure 8C It is a perspective view showing a method for manufacturing a stage according to one embodiment of the present invention.
[0046] Fig. 9 It is a schematic cross-sectional view of a film processing apparatus including a stage according to an embodiment of the present invention.
[0047] Fig. 10A This is an example of an image of a part of the corner of the stage according to one embodiment of the present invention captured by an electron microscope.
[0048] Fig. 10B This is an example of an image of a part of the corner of the stage according to one embodiment of the present invention captured by an electron microscope.
[0049] Fig.11 This is a diagram showing the dielectric breakdown voltage of the stage according to one embodiment of the present invention.
[0050] Fig. 12A It is a perspective view and a cross-sectional view which show the structure of the stage which concerns on one Embodiment of this invention.
[0051] Fig. 12B It is a perspective view and a cross-sectional view which show the structure of the stage which concerns on one Embodiment of this invention.
[0052] Fig. 12CIt is a perspective view and a cross-sectional view which show the structure of the stage which concerns on one Embodiment of this invention. DETAILED DESCRIPTION
[0053] Hereinafter, various embodiments of the invention disclosed in the present application will be described with reference to the drawings. However, the present invention can be implemented in various forms within the scope of the gist thereof, and should not be construed as being limited to the description of the embodiments illustrated below.
[0054] In order to make the description clearer, the drawings sometimes schematically indicate the width, thickness, shape, etc. of each part compared with the actual method, but this is only an example and does not limit the interpretation of the present invention. In this specification and each of the drawings, elements having the same functions as those described in conjunction with the existing drawings can be represented by the same reference numerals, and repeated descriptions can be omitted. In this specification and each of the drawings, elements having the same functions as those described in conjunction with the existing drawings can be represented by the same reference numerals, and repeated descriptions can be omitted.
[0055] In the present invention, when a certain film is processed to form a plurality of films, these plurality of films sometimes have different functions and effects. However, these plurality of films are films formed as the same layer in the same process, have the same layer structure, and the same material. Therefore, these plurality of films are defined as existing in the same layer.
[0056] In the present specification and drawings, when a plurality of parts of one structure are respectively distinguished and indicated, the same reference numerals are used, and hyphens and natural numbers are used.
[0057] 1. First Implementation
[0058] In this embodiment, the stage 122 according to one embodiment of the present invention will be described.
[0059] 1-1. Stage structure
[0060] FIG1 shows a cross-sectional view of the stage 122. Figure 1A and Figure 1B As shown, the stage 122 has a support plate 140 and a first insulating film 141 .
[0061] The support plate 140 has at least a first surface 440, a second surface 442 adjacent to the first surface 440, and a third surface 444. In addition, the support plate 140 has a first substrate 160 and a second substrate 162. The first substrate 160 has a first surface 440 and a second surface 442, and the second substrate 162 has a third surface 444. The first insulating film 141 is provided on the first substrate 160 and the second substrate 162 by a sputtering method. That is, the first insulating film 141 is provided on the first surface 440, the second surface 442, and the third surface 444. The second surface 442 may include all of the second surface 442-1, the second surface 442-2, the second surface 442-3, and the second surface 442-4, or may include a portion thereof. In one embodiment of the present invention, an example is shown in which the first insulating film 141 is provided on the entire third surface 444, but the first insulating film 141 may also be provided on a portion of the third surface 444.
[0062] Here, the surface of the extended first surface 440 and the surface of the extended second surface 442-1 are formed to intersect at 90 degrees or approximately 90 degrees. The surface of the extended second surface 442-1 and the surface of the extended second surface 442-2 are formed to intersect at 90 degrees or approximately 90 degrees. The surface of the extended second surface 442-2 and the surface of the extended second surface 442-3 are formed to intersect at 90 degrees or approximately 90 degrees. The surface of the extended second surface 442-3 and the surface of the extended second surface 442-4 are formed to intersect at 90 degrees or approximately 90 degrees. The surface of the extended second surface 442-4 and the surface of the extended third surface 444 are formed to intersect at 90 degrees or approximately 90 degrees. In addition, the first surface 440 and the third surface 444 are arranged in opposite directions of 180 degrees or approximately 180 degrees.
[0063] The main materials of the first substrate 160 and the second substrate 162 are metal or ceramic, for example, titanium (Ti), aluminum (Al), stainless steel or oxides thereof can be used. An opening 142 for installing a temperature sensor can also be provided on the bottom surface of the support plate 140. A thermocouple or the like can be used as the temperature sensor. In one embodiment of the present invention, an example in which the first insulating film 141 is provided on the inner wall of the opening 142 is shown, but the first insulating film 141 can also be provided on a part of the inner wall of the opening 142.
[0064] A groove (channel) 146 for circulating a medium for controlling the temperature of the substrate may also be provided inside the support plate 140 of the stage 122. As the medium, a liquid medium such as water, alcohol such as isopropyl alcohol or ethylene glycol, or silicone oil may be used. The groove 146 is formed on one or both of the first substrate 160 and the second substrate 162, and then the first substrate 160 and the second substrate 162 are joined by brazing or the like. The medium may be used in either the case of cooling the stage 122 or the case of heating.
[0065] The temperature is set to be Fig. 9 The medium controlled by the temperature controller 228 shown flows in the groove 146 , thereby controlling the temperature of the support plate 140 .
[0066] As the first insulating film 141, any known material can be used as long as it satisfies the desired withstand voltage and can be sprayed by the spraying method. For example, as the material for the first insulating film 141, one or more oxides of alkaline earth metals, rare earth metals, aluminum (Al), tantalum (Ta), and silicon (Si) can be used. Specifically, aluminum oxide (Al2O3) can be used. 2 O 3 ), magnesium oxide (MgO), etc.
[0067] The material used for the first insulating film 141 may include an inorganic insulator. Specific examples of the inorganic insulator include aluminum oxide, titanium oxide, chromium oxide, zirconium oxide, magnesium oxide, yttrium oxide, and composite oxides thereof.
[0068] As the thermal spraying method used in the specification and the like, for example, a ceramic rod flame spraying method (Rokidethermal spraying method), a plasma spraying method, or a spraying method combining these methods may be mentioned.
[0069] As an arbitrary structure, the stage 122 may also have one or more through holes 144 that penetrate the support plate 140. Fig. 9 A helium gas introduction pipe is provided in the chamber 202 shown, so that a gas with high thermal conductivity, such as helium, flows through the through hole 144. Thus, the gas flows through the gap between the stage 122 and the substrate, and the heat energy of the stage 122 can be efficiently transferred to the substrate. In addition, in one embodiment of the present invention, an example in which the first insulating film 141 is provided on the inner wall of the through hole 144 is shown, but the first insulating film 141 may also be provided on a portion of the inner wall of the through hole 144.
[0070] like Figure 1C As shown, the stage 122 may also have an electrostatic chuck 170 as a mechanism for fixing the substrate on the stage 122. The electrostatic chuck 170 may have a structure in which, for example, an electrostatic chuck electrode 172 is covered with an insulating film 174. A high voltage (from hundreds of V to thousands of V) is applied to the electrostatic chuck electrode 172, so that the substrate can be fixed under the action of the Coulomb force of the charges generated in the electrostatic chuck electrode 172 and the charges generated on the back side of the substrate and having the opposite polarity to the charges generated in the electrostatic chuck electrode 172. As an insulator, ceramics such as aluminum oxide, aluminum nitride, and boron nitride can be used. In addition, the insulating film 174 does not need to be completely insulating, and may have a certain degree of conductivity (for example, 10 9 Ω·cm to 10 12In this case, the film 174 is made by doping the ceramic with a metal oxide such as titanium oxide, zirconium oxide, or hafnium oxide. Ribs 176 for determining the position of the substrate may also be provided around the electrostatic chuck 170 .
[0071] 1-2. Manufacturing of the stage
[0072] 2 and 3 are cross-sectional views showing a first method for manufacturing the stage 122. Figure 1A , 1B Or 1C same or similar structure, the description is sometimes omitted.
[0073] The first method for manufacturing the stage 122 is described using FIG. 2 and FIG. 3. Figure 2A As shown, a support plate 140 is prepared.
[0074] Then, if Figure 2B As shown, while the sputtering machine 500 included in the sputtering device is moved in a direction parallel to the first surface 440 of the support plate 140, the first insulating film 141 is formed on at least a portion of the first surface 440. At this time, the sputtering machine 500 may also repeatedly perform an action from the end of the support plate 140 toward the approximate center of the first surface 440 of the support plate 140 and an action from the approximate center of the support plate 140 toward the end of the support plate 140, and form the first insulating film 141 on at least a portion of the first surface 440 while moving in a zigzag manner. The formation of the first insulating film 141 on the first surface 440 using the sputtering machine 500 included in the sputtering device may also be referred to as forming the first insulating film 141 on the first surface 440 by sputtering. At this time, when the direction in which the particles sputtered by the sputtering machine 500 are sprayed toward the first surface 440 is taken as the sputtering direction, the sputtering direction and the first surface 440 may be substantially perpendicular or perpendicular. In addition, the movement of the spraying machine 500 in the direction parallel to the first surface 440 can be a single direction, or as shown in FIG. Figure 2B As shown, the first insulating film 141 is formed on the first surface 440 while moving in the single direction and the 180-degree opposite directions. Thus, the first insulating film 141 can be uniformly formed on the first surface 440 .
[0075] Then, if Figure 2CAs shown, the first insulating film 141 is formed on at least a portion of the second surface 442 while the sputtering machine 500 is moved in a direction parallel to the second surface 442. At this time, the sputtering machine 500 may repeatedly move from one end of the second surface 442 (for example, the first surface 440 side) toward the other end of the second surface 442 (for example, the third surface 444 side) and from the other end of the second surface 442 toward one end of the second surface 442, and form the first insulating film 141 on at least a portion of the second surface 442 while moving in a zigzag manner. The formation of the first insulating film 141 on the second surface 442 using the sputtering machine 500 included in the sputtering device may also be referred to as forming the first insulating film 141 on the second surface 442 by sputtering. At this time, when the direction in which the particles sputtered by the sputtering machine 500 are sprayed toward the second surface 442 is taken as the sputtering direction, the sputtering direction and the second surface 442 may be substantially perpendicular or perpendicular. In addition, the movement of the spraying machine 500 in the parallel direction relative to the second surface 442 can be a single direction, or as shown in FIG. Figure 2C As shown, the first insulating film 141 is formed on the second surface 442 while moving in the single direction and the 180-degree opposite directions. Thus, the first insulating film 141 can be uniformly formed on the second surface 442 .
[0076] Then, with Figure 2B Similarly, as described in Figure 3A As shown in FIG. 1 , a first insulating film 141 is formed again on the first surface 440. Next, Figure 2C Similarly, as described in Figure 3B As shown, the first insulating film 141 is formed again on the second surface 442 .
[0077] As described above, by forming the first insulating film 141 on each surface, Figure 3C As shown in FIG. 1 , a first insulating film 141 can be provided on the support plate 140. Furthermore, for example, Figure 1C The stage 122 can be manufactured by joining the support plate 140 and the electrostatic chuck 170 as shown. The joining of the support plate 140 and the electrostatic chuck 170 can be performed by welding, screwing, or brazing, for example. Examples of the brazing material used in brazing include silver, copper, and alloys containing zinc, alloys containing copper and zinc, copper containing a trace amount of phosphorus, aluminum and alloys thereof, alloys containing titanium, copper, and nickel, alloys containing titanium, zirconium, and copper, and alloys containing titanium, zirconium, copper, and nickel.
[0078] Above, if used Figure 2A , Figure 2B , Figure 2C , Figure 3A , Figure 3B , Figure 3C as well as Figure 1A As described above, the first insulating film 141 is formed on the first surface 440 and the first insulating film 141 is formed on the second surface 442 by repeating the operation alternately, thereby the first insulating film 141 can be uniformly formed on the first surface 440 and the second surface 442 of the support plate 140. In addition, the first insulating film 141 is formed on the first surface 440 and the first insulating film 141 is formed on the second surface 442 by repeating the operation alternately, thereby the occurrence of a gap or a void at the corner of the first surface 440 and the second surface 442 can be suppressed. In addition, the first insulating film 141 formed on the first surface 440 and the first insulating film 141 formed on the second surface 442 can also be overlapped by repeating the operation alternately. By overlapping the first insulating film 141 formed on the first surface 440 and the first insulating film 141 formed on the second surface 442 , it is possible to suppress the occurrence of a gap or a void at the corner between the first surface 440 and the second surface 442 .
[0079] For example, the first insulating film 141 can also be uniformly formed on the circular support plate 140 with an approximate shape of 30 cm by repeatedly performing the following actions: moving the spray gun 500 included in the spray gun apparatus by 1 mm in a direction parallel to the first surface 440 while forming the first insulating film 141 on at least a portion of the first surface 440; and moving the spray gun 500 included in the spray gun apparatus by 1 mm in a direction parallel to the second surface 442 while forming the first insulating film 141 on at least a portion of the second surface 442.
[0080] As an arbitrary forming method, the first insulating film 141 may be formed on at least a portion of the third surface 444 while the sputtering machine 500 is moved in a direction parallel to the third surface 444. In addition, the sputtering machine 500 may repeatedly perform an action from the end of the support plate 140 toward the approximate center of the third surface 444 of the support plate 140 and an action from the approximate center of the support plate 140 toward the end of the support plate 140, and form the first insulating film 141 on at least a portion of the third surface 444 while moving in a zigzag manner. At this time, the action of forming the first insulating film 141 on at least a portion of the first surface 440, the action of forming the first insulating film 141 on at least a portion of the second surface 442, and the action of forming the first insulating film 141 on at least a portion of the third surface 444 may be repeated, thereby uniformly forming the first insulating film 141 on the first surface 440, the second surface 442, and the third surface 444 of the support plate 140.
[0081] 1-3. Comparison between the corners of the support plate of the conventional stage and the corners of the support plate 140 of the stage 122 according to one embodiment of the present invention
[0082] Fig. 4 is a cross-sectional view for explaining a part of a corner portion of a support plate included in a conventional stage. Fig. 5 and Fig. 6 are cross-sectional views showing a part of a corner portion of a support plate 140 included in a stage 122 according to an embodiment of the present invention. Figure 7 This is an example of an image of a portion of a corner portion of a support plate 140 of a stage 122 according to an embodiment of the present invention, taken by an electron microscope. The description of the configurations that are the same or similar to those in FIGS. 1 to 3 may be omitted. Figure 1B The structure of the stage 122 shown is described as an example.
[0083] exist Figure 4A , an example is shown in which the corners of the first surface 440 and the second surface 442-1 have a C-chamfered shape. Figure 4B , an example is shown in which the corners of the second surface 442-2 and the second surface 442-3 have curvature. Figure 4C , an example is shown in which the corners of the second surface 442-4 and the third surface 444 have a curvature. Conventionally, the first insulating film 141 formed on the corners of the first surface 440 and the second surface 442-1, the first insulating film 141 formed on the corners of the second surface 442-2 and the second surface 442-3, and the first insulating film 141 formed on the corners of the second surface 442-4 and the third surface 444 include a large gap or void 446. In addition, the corners of the first surface 440 and the second surface 442-1 may have a curvature, the corners of the second surface 442-2 and the second surface 442-3 may have a C-chamfered shape, and the corners of the second surface 442-4 and the third surface 444 may have a C-chamfered shape.
[0084] on the other hand, Figure 5B FIG. 1 shows an example in which the corners of the first surface 440 and the second surface 442-1 of the support plate 140 of the stage 122 according to one embodiment of the present invention have a C-chamfered shape. Figure 5B As shown, the first insulating film 141 formed on the corners of the first face 440 and the second face 442 - 1 does not include a large gap or void 446 and has a uniform film.
[0085] like Figure 5AAs shown, in the support plate 140 of the stage 122 according to one embodiment of the present invention, the first insulating film 141 formed by the sputtering method is composed of a plurality of particles 450 having a flat shape on the first surface 440. The flat surface 452 of at least a part of the plurality of particles 450 is formed by the sputtering method along a surface parallel or substantially parallel to the first surface 440. The particles sputtered by the sputtering machine 500 are particles 450. In addition, the direction 454 perpendicular or substantially perpendicular to the flat surface 452 is parallel or substantially parallel to the direction perpendicular or substantially perpendicular to the first surface 440, and is also parallel or substantially parallel to the sputtering direction in which the particles 450 sputtered by the sputtering machine 500 are sprayed toward the first surface 440.
[0086] Similar to the first surface 440, the first insulating film 141 formed by the spraying method on the second surface 442-1 is also composed of a plurality of particles 450 having a flat shape, and the flat surface 462 of at least a part of the plurality of particles 450 is formed by the spraying method in a manner along a surface parallel or substantially parallel to the second surface 442-1. In addition, the particles sprayed by the spraying machine 500 are particles 450. Furthermore, the direction 464 perpendicular or substantially perpendicular to the flat surface 462 is parallel or substantially parallel to the direction perpendicular or substantially perpendicular to the second surface 442-1, and is also parallel or substantially parallel to the spraying direction in which the particles 450 sprayed by the spraying machine 500 are sprayed toward the second surface 442-1.
[0087] Similar to the first surface 440 and the second surface 442-1, the first insulating film 141 formed by the spraying method on the surface 443 of the corner is also composed of a plurality of particles 450 having a flat shape, and the flat surface 472 of at least a part of the plurality of particles 450 is formed by the spraying method along a surface parallel or substantially parallel to the surface 443 of the corner. In addition, the particles sprayed by the spraying machine 500 are particles 450. In addition, the direction 474 perpendicular or substantially perpendicular to the flat surface 472 is parallel or substantially parallel to the direction perpendicular or substantially perpendicular to the surface 443 of the corner, and is also parallel or substantially parallel to the spraying direction in which the particles 450 sprayed by the spraying machine 500 are sprayed toward the surface 443 of the corner.
[0088] Figure 6B FIG. 1 shows an example in which the corners of the second surface 442-4 and the third surface 444 of the support plate 140 of the stage 122 according to one embodiment of the present invention have a curvature. Figure 6B As shown, the first insulating film 141 formed on the corner of the second surface 442 - 4 and the third surface 444 does not include a large gap or void 446 and has a uniform film.
[0089] like Fig. 6AAs shown, in the support plate 140 of the stage 122 of one embodiment of the present invention, on the third surface 444 set in the direction 180 degrees opposite to the first surface 440, the first insulating film 141 formed by the sputtering method is composed of a plurality of particles 450 having a flat shape. The flat surface 482 of at least a part of the plurality of particles 450 is formed by the sputtering method in a manner parallel or substantially parallel to the third surface 444. The particles sputtered by the sputtering machine 500 are particles 450. In addition, the direction 484 perpendicular or substantially perpendicular to the flat surface 482 is parallel or substantially parallel to the direction perpendicular or substantially perpendicular to the third surface 444, and is also parallel or substantially parallel to the sputtering direction in which the particles 450 sputtered by the sputtering machine 500 are sprayed toward the third surface 444.
[0090] Similar to the third surface 444, the first insulating film 141 formed by the sputtering method on the second surface 442-4 is also composed of a plurality of flat particles 450. In addition, the structure of the plurality of particles 450 formed on the second surface 442-4 is similar to that on the third surface 444. Figure 5A The structures of the plurality of particles 450 formed on the second surface 442 - 1 are the same, and thus the description thereof is omitted here.
[0091] As with the third surface 444 and the second surface 442-4, if one of the tangent planes to the points constituting the corner of the third surface 444 and the second surface 442-4 is set as a surface 491, the first insulating film 141 formed by the sputtering method on the surface 491 is also composed of a plurality of particles 450 having a flat shape, and the flat surfaces 492 of at least a part of the plurality of particles 450 are formed by the sputtering method along a surface parallel or substantially parallel to the surface 491. In addition, the particles sprayed by the sputtering machine 500 are particles 450. In addition, the direction 494 perpendicular or substantially perpendicular to the flat surface 492 is parallel or substantially parallel to the direction perpendicular or substantially perpendicular to the surface 491, and is also parallel or substantially parallel to the sputtering direction in which the particles 450 sprayed by the sputtering machine 500 are sprayed toward the surface 491 of the corner.
[0092] exist Figure 7 In FIG. 4 , the curved surface 491S and the curved surface 492S formed by the plurality of particles 450 are shown as approximate guide lines. Figure 7 As shown, the tangent planes of each point constituting the curved surface 491S and the curved surface 492S are parallel or substantially parallel. That is, the direction 494 perpendicular or substantially perpendicular to the flat surface 492 is parallel or substantially parallel to the direction perpendicular or substantially perpendicular to the tangent planes of each point constituting the curved surface 491S and the curved surface 492S, and is also parallel or substantially parallel to the direction in which the particles 450 sprayed by the spraying machine 500 are sprayed toward the corner. Figure 7In the stage according to the embodiment of the present invention shown in the figure, an example is shown in which aluminum oxide is used as the material of the first insulating film 141 and the particle size is about 25 μm.
[0093] In the stage 122 of one embodiment of the present invention, the flat surface of the particle 450 constituting at least a portion of the first insulating film 141 can be formed to be parallel or approximately parallel to the first surface 440 and the second surface 442 by alternating and repeating the following actions: while moving the spraying machine 500 in a direction parallel to the first surface 440 of the support plate 140, the first insulating film 141 is formed on the first surface 440 by spraying from a direction perpendicular to the first surface 440; and while moving the spraying machine 500 in a direction parallel to the second surface 442 adjacent to the first surface 140, the first insulating film 141 is formed on the second surface 442 by spraying from a direction perpendicular to the second surface 442.
[0094] In addition, the first insulating film 141 formed on the first surface 440 is formed overlapping with the first insulating film 141 formed on the second surface 442. As a result, the first insulating film 141 formed on the first surface 440, the second surface 442, and the corners of the first surface 440 and the second surface 442 becomes a uniform film that does not substantially contain gaps or voids. Therefore, since the first insulating film 141 is densely formed on the support plate 140, the dielectric breakdown voltage of the support plate 140 is improved. Therefore, in the stage and the method for manufacturing the stage, by applying the present invention, a stage with high withstand voltage and a method for manufacturing the stage can be provided.
[0095] 2. Second Implementation
[0096] In this embodiment, a second method for manufacturing the stage 122 according to one embodiment of the present invention will be described. The description of the same or similar structures as those in the first embodiment may be omitted.
[0097] FIG8 shows a second method for manufacturing the stage 122 according to an embodiment of the present invention. The second method for manufacturing the stage 122 is different from the first method for manufacturing the stage 122 according to the first embodiment in that the deposition machine 500 is moved continuously and in a single direction to form the first insulating film 141 on the third surface 444, the first insulating film 141 on the second surface 442, and the first insulating film 141 on the first surface 440. In the following description of the second method for manufacturing the stage 122, the differences from the first method are mainly described.
[0098] First, the steps of preparing the support plate 140 are similar to those shown in the first embodiment. Figure 2A The same, so the description is omitted here.
[0099] Then, if Fig. 8A As shown, the support plate 140 is rotated relative to an axis approximately perpendicular to the approximate center of the first surface 440 of the support plate 140, while the spraying machine 500 included in the spraying device is moved in a direction parallel to the third surface 444, while a first insulating film 141 is formed on at least a portion of the third surface 444.
[0100] Then, if Figure 8B As shown, the step of forming the first insulating film 141 on the second surface 442 by the sputtering machine 500 is performed by moving the sputtering machine 500 continuously and in a single direction from a direction parallel to the third surface 444 to a direction parallel to the second surface 442. When the first insulating film 141 is formed on the second insulating film 442 by the sputtering machine 500, the same method as the first manufacturing method of the stage 122 shown in the first embodiment can be used. The movement of the sputtering machine 500 is continuous and in a single direction, and the first insulating film 141 can be formed uniformly on the third surface 444 and the second surface 442 by forming the first insulating film 141 on the second surface 442 starting from the third surface 444.
[0101] Then, if Figure 8C As shown, the step of forming the first insulating film 141 on the first surface 440 by the sputtering machine 500 is performed by moving the sputtering machine 500 continuously and in a single direction from a direction parallel to the second surface 442 toward a direction parallel to the first surface 440. When the first insulating film 141 is formed on the first surface 440 by the sputtering machine 500, the same method as the first manufacturing method of the stage 122 shown in the first embodiment can be used. The movement of the sputtering machine 500 is continuous and in a single direction, and the first insulating film 141 can be formed uniformly on the second surface 442 and the first surface 440 by forming the first insulating film 141 on the first surface 440 starting from the second surface 442.
[0102] As described above, the first insulating film 141 can be provided on the support plate 140 by forming the first insulating film 141 on each surface. Furthermore, since the step of bonding the support plate 140 and the electrostatic chuck 170 is similar to that shown in the first embodiment, Figure 1A As described above, in the second manufacturing method, the stage 122 can be manufactured.
[0103] Above, if used Figure 2A , Fig. 8A , Figure 8B , Figure 8C as well as Figure 1AAs described above, the first insulating film 141 is formed on the third surface 444, the first insulating film 141 is formed on the second surface 442, and the first surface 440 by continuously and unidirectionally moving, thereby making it possible to form the first insulating film 141 more uniformly on the third surface 444, the second surface 442, and the first surface 440 of the support plate 140. In addition, it is possible to further suppress the occurrence of gaps or voids at the corners between the third surface 444 and the second surface 442, and the corners between the second surface 442 and the first surface 440. As a result, the first insulating film 141 formed on the third surface 444, the corners between the third surface 444 and the second surface 442, the second surface 442, the corners between the second surface 442 and the first surface 440, and the first surface 440 becomes a uniform film that does not substantially include gaps or voids. Therefore, the first insulating film 141 is densely formed on the support plate 140, so the dielectric breakdown voltage of the support plate 140 is further improved. Therefore, by applying the present invention to a stage and a method for manufacturing the stage, a stage and a method for manufacturing the stage with higher withstand voltage can be provided.
[0104] The method for manufacturing the stage of this embodiment is not limited to the above-mentioned manufacturing method.
[0105] The manufacturing method of the stage of the present embodiment may be, for example, a manufacturing method in which the first insulating film 141 is formed on the first surface 440, the first insulating film 141 is formed on the second surface 442, and the first insulating film 141 is formed on the third surface 444 while continuously and moving in a single direction. In the manufacturing method in which the first insulating film 141 is formed on the first surface 440, the first insulating film 141 is formed on the second surface 442, and the first insulating film 141 is formed on the third surface 444 while continuously and moving in a single direction, the first insulating film 141 is densely formed on the support plate 140, so that the dielectric breakdown voltage of the support plate 140 is further improved.
[0106] In addition, in the manufacturing method of the stage of the present embodiment, for example, the action of forming the first insulating film 141 on the third surface 444 may be referred to as the first spraying, and the action of continuously forming the first insulating film 141 on the second surface 442 and the first insulating film 141 on the first surface 440 may be referred to as the second spraying. Furthermore, in the manufacturing method of the stage of the present embodiment, the first spraying and the second spraying may be performed alternately, the first spraying and the second spraying may be performed alternately and repeatedly, the second spraying and the first spraying may be performed alternately, or the second spraying and the first spraying may be performed alternately and repeatedly. By alternately and repeatedly performing the first spraying and the second spraying, the deviation (unevenness) of the thickness of the insulating film of the stage can be further suppressed. As a result, a stage on which the insulating film is formed more uniformly can be provided.
[0107] In addition, in the manufacturing method of the stage of the present embodiment, the first spraying and the second spraying may be performed continuously after the first spraying and the second spraying are performed alternately, or the first spraying and the second spraying may be performed continuously and repeatedly after the first spraying and the second spraying are performed alternately and repeatedly. Similarly, in the case where the second spraying is performed first, the first spraying and the second spraying may be performed continuously after the second spraying and the first spraying are performed alternately and repeatedly, or the first spraying and the second spraying may be performed continuously and repeatedly after the second spraying and the first spraying are performed alternately and repeatedly. By performing the first spraying and the second spraying continuously after the first spraying and the second spraying are performed alternately and repeatedly, the deviation (unevenness) of the thickness of the insulating film of the stage can be further suppressed, and the occurrence of gaps or voids at the corners of the stage can be further suppressed.
[0108] 3. Third Implementation
[0109] In this embodiment, the film processing apparatus provided with the stage 122 is demonstrated as an example. The description of the structure which is the same as or similar to the 1st embodiment or the 2nd embodiment may be abbreviate|omitted.
[0110] Fig. 9 A cross-sectional view of an etching device 200 as one of the film processing devices is shown. The etching device 200 can perform dry etching on various films. The etching device 200 has a chamber 202. The chamber 202 provides a space for etching a film such as a conductor, an insulator, or a semiconductor formed on a substrate.
[0111] The chamber 202 is connected to an exhaust device 204, which can set the chamber 202 to a reduced pressure environment. The chamber 202 is also provided with an introduction pipe 206 for introducing a reaction gas, and the etching reaction gas is introduced into the chamber via a valve 208. Examples of the reaction gas include carbon tetrafluoride (CF 4 ), octafluorocyclobutane (cC 4 F 8 ), perfluorocyclopentane (cC 5 F 10 ), hexafluorobutadiene (C 4 F 6 ) and other fluorine-containing organic compounds.
[0112] A microwave source 212 may be provided at the upper portion of the chamber 202 via a waveguide 210. The microwave source 212 has an antenna for supplying microwaves, etc., and outputs high-frequency microwaves such as 2.45 GHz microwaves and 13.56 MHz radio frequency (RF) waves. The microwaves generated by the microwave source 212 are propagated to the upper portion of the chamber 202 by the waveguide 210, and are introduced into the chamber 202 via a window 214 made of quartz, ceramic, etc. The reaction gas is plasmatized by the microwaves, and the film is etched by electrons, ions, and radicals contained in the plasma.
[0113] In order to place the substrate, a stage 122 of one embodiment of the present invention is provided at the lower part of the chamber 202. The substrate is placed on the stage 122. The stage 122 is connected to a power supply 224, and a voltage equivalent to high-frequency power is applied to the stage 122, so that an electric field generated by microwaves is formed in a direction perpendicular to the surface of the stage 122 and the surface of the substrate. Magnets 216, 218, and 220 may also be provided at the upper part and side of the chamber 202. As the magnet 216, the magnet 218, and the magnet 220 may be a permanent magnet, or an electromagnet with an electromagnetic coil. The magnets 216, 218, and 220 generate a magnetic field component parallel to the stage 122 and the surface of the substrate, and due to the cooperation with the electric field generated by the microwave, the electrons in the plasma are subjected to the Lorentz force and resonate, and are bound to the surface of the stage 122 and the substrate. As a result, high-density plasma can be generated on the surface of the substrate.
[0114] For example, when the stage 122 is provided with a sheath heater, a heater power supply 230 for controlling the sheath heater is connected. A power supply 226 for an electrostatic chuck for fixing a substrate on the stage 122, a temperature controller 228 for controlling the temperature of a medium circulating inside the stage 122, and a rotation control device (not shown) for rotating the stage 122 may also be connected to the stage 122 as an arbitrary structure.
[0115] As described above, the stage 122 of one embodiment of the present invention is used in the etching device 200. By using the stage 122, the substrate can be uniformly heated and the heating temperature can be precisely controlled. In addition, by using the stage 122, the dielectric breakdown voltage of the stage can be increased. In addition, by using the stage 122, the withstand voltage of the voltage applied to the substrate can be improved. Therefore, by using the etching device 200, a contact with a high aspect ratio can be formed, or a film with a high aspect ratio can be formed. Therefore, using the etching device 200, various films provided on the substrate can be uniformly etched.
[0116] 4. Fourth Implementation
[0117] In this embodiment, the ratio of the gap or space 446 at the corner of the stage of one embodiment of the present invention and the dielectric breakdown voltage of the stage of one embodiment of the present invention are described. The description of the same or similar structures as those of the first to third embodiments may be omitted.
[0118] Fig. 10A An example of an image of a portion of a corner portion of the third surface 444 and the second surface 442 taken by an electron microscope when the stage according to one embodiment of the present invention is formed by the first manufacturing method is shown. Fig. 10B An example of an image of a portion of the corner of the third surface 444 and the second surface 442 taken by an electron microscope when the stage according to one embodiment of the present invention is formed by the second manufacturing method is shown. Fig.11 Graphs showing insulation breakdown voltages of a conventional stage, a stage according to an embodiment of the present invention manufactured by a first manufacturing method, and a stage according to an embodiment of the present invention manufactured by a second manufacturing method are shown.
[0119] like Fig. 10A and 10B As shown, gaps or voids 446 are represented by black dots. Fig. 10A and 10B No Figure 4C The large gap or space 446 in the corner of the previous stage is shown. Fig. 10A and Fig. 10B 200 μm×200 μm area 502 is shown in FIG. Fig. 10A In FIG. 5 , the area ratio of gaps or voids 446 to the area of region 502 is 4.33%. Fig. 10B , the area ratio of the gap or void 446 to the area of the region 502 is 0.49%. That is, the area ratio of the gap or void 446 to the area of the region 502 of the corner formed by the first manufacturing method and the second manufacturing method is significantly reduced compared to the conventional method.
[0120] Then, if Fig.11 As shown in the figure, the dielectric breakdown voltage of the conventional stage is 3.58 kV, the dielectric breakdown voltage of the stage according to one embodiment of the present invention manufactured by the first manufacturing method is 4.60 kV, and the dielectric breakdown voltage of the stage according to one embodiment of the present invention manufactured by the second manufacturing method is 10.37 kV. The dielectric breakdown voltage of the stage manufactured by the first manufacturing method is 1 kV higher than the dielectric breakdown voltage of the conventional stage, and the dielectric breakdown voltage of the stage manufactured by the second manufacturing method is about 3 times higher than the dielectric breakdown voltage of the conventional stage.
[0121] 5. Fifth Implementation
[0122] In this embodiment, a stage 124 according to one embodiment of the present invention will be described. Description of the same or similar structures as those of the first to fourth embodiments may be omitted.
[0123] FIG12 is a cross-sectional view of the stage 124. The structure of the stage 124 is different from the structure of the stage 122 shown in the first embodiment in that the stage 124 has a heater layer 150. In the following description of the structure of the stage 124, the differences from the structure of the stage 122 are mainly described. In addition, in the first to fourth embodiments, the stage 122 described in the first to fourth embodiments may be appropriately replaced with the stage 124 described in this embodiment.
[0124] like Fig. 12A and Fig. 12B As shown, the stage 124 has a support plate 140 on which a heater layer 150 is disposed.
[0125] In the stage 124, the temperature is adjusted from Fig. 9 The medium controlled by the temperature controller 228 shown flows in the groove 146, thereby controlling the temperature of the support plate 140. However, the temperature control response of the liquid medium is slow, and accurate temperature control is difficult. Therefore, it is preferred to roughly control the temperature of the support plate 140 using the medium and accurately control the temperature of the substrate using the heating wire 154 in the heater layer 150. In this way, not only accurate temperature control can be performed, but also the temperature adjustment of the stage 124 can be performed quickly.
[0126] The heater layer 150 mainly has three layers. Specifically, the heater layer 150 includes a second insulating film 152, a heating line 154 on the second insulating film 152, and a third insulating film 156 on the heating line 154. Fig. 12B Only one heating wire 154 may be provided in the heater layer 150, or a plurality of heating wires 154 may be provided, and each of the heating wires 154 may be provided with a plurality of heating wires 154. Fig. 9 The heater power source 230 shown is independently controlled. The heater wire 154 is electrically insulated by the second insulating film 152 and the third insulating film 156. The heater wire 154 is heated by the power supplied from the heater power source 230, thereby controlling the temperature of the stage 124.
[0127] The second insulating film 152 and the third insulating film 156 may include an inorganic insulator. The inorganic insulator has been described in the first embodiment, so the description thereof is omitted. In addition, the second insulating film 152 and the third insulating film 156 may be formed using a sputtering method. The sputtering method has been described in the first embodiment, so the description thereof is omitted.
[0128] The heating wire 154 may include a metal that generates heat by being energized. Specifically, it may include a metal selected from tungsten, nickel, chromium, cobalt, and molybdenum. The metal may be an alloy including these metals, such as an alloy of nickel and chromium, or an alloy containing nickel, chromium, and cobalt.
[0129] Preferably, the heating line 154 is formed by etching a metal film or metal foil formed by sputtering, metal organic CVD (MOCVD), vapor deposition, printing, electroplating, etc., and then placing it on the second insulating film 152. This is because, when the heating line 154 is formed by sputtering, it is difficult to ensure uniform density, thickness, and width over the entire heating line 154. On the other hand, when the metal film or metal foil is processed by etching, the heating line 154 with small deviation in these physical parameters can be formed. As a result, the temperature of the stage 124 can be precisely controlled, and the temperature distribution can be reduced.
[0130] Furthermore, the alloy has a higher volume resistivity than a metal alone, so when the layout, that is, the planar shape, of the heater wire 154 is the same, the thickness of the heater wire 154 can be increased compared to the case of using a metal alone. Therefore, the variation in the thickness of the heater wire 154 can be reduced, and a smaller temperature distribution can be achieved.
[0131] As an optional structure, the stage 124 may also have one or more through holes 144 that penetrate both the support plate 140 and the heater layer 150. In order to allow a gas with high thermal conductivity, such as helium, to flow through the through holes 144, Fig. 9 A helium gas introduction pipe is provided in the chamber 202 shown. Thus, the gas flows through the gap between the stage 124 and the substrate, and the heat energy of the stage 124 can be efficiently transferred to the substrate. In addition, in one embodiment of the present invention, an example is shown in which the first insulating film 141 is provided on the inner wall of the through hole 144, but the first insulating film 141 can also be provided on a part of the inner wall of the through hole 144.
[0132] like Fig. 12C As shown, the stage 124 may further include an electrostatic chuck 170 as a mechanism for fixing the substrate on the stage 124. Since it has been shown in the first embodiment, the description here is omitted.
[0133] As described above, the stage in one embodiment of the present invention has fewer gaps or spaces and a higher dielectric breakdown voltage than conventional stages. Therefore, by applying the manufacturing method in one embodiment of the present invention, a stage with a high withstand voltage and a method for manufacturing the stage can be provided.
[0134] As embodiments of the present invention, the above embodiments can be appropriately combined and implemented as long as they are not contradictory. In addition, those skilled in the art can add, delete or design changes to appropriate components based on the embodiments, and as long as they have the gist of the present invention, they are also included in the scope of the present invention.
[0135] Furthermore, even if there are other effects different from the effects brought about by the above-mentioned embodiments, effects that are obvious from the description of this specification or effects that are easily predicted by those skilled in the art are of course understood as effects brought about by the present invention.
[0136] (Explanation of Reference Numerals)
[0137] 100: stage; 102: chamber; 110: jacket heater; 122: stage; 124: stage; 128: temperature controller; 140: support plate; 141: first insulating film; 142: opening; 144: through hole; 146: groove (channel); 150: heater layer; 152: second insulating film; 154: heating line; 156: third insulating film; 160: first substrate; 162: second substrate; 170: electrostatic chuck; 172: electrostatic chuck electrode; 174: film; 176: rib; 200: etching device; 202: chamber; 204: exhaust device; 206: introduction pipe; 208: valve; 210: waveguide; 212: microwave source; 214: window; 2 16: magnet; 218: magnet; 220: magnet; 224: power supply; 226: power supply; 228: temperature controller; 230: heater power supply; 440: first surface; 442: second surface; 442-1: second surface; 442-2: second surface; 442-3: second surface; 442-4: second surface; 443: surface; 444: third surface; 446: gap; 450: particle; 452: flat surface; 454: direction; 462: flat surface; 464: direction; 472: flat surface; 474: direction; 482: flat surface; 484: direction; 491: surface; 491S: curved surface; 492S: curved surface; 494: direction; 500: spraying machine; 502: area.
Claims
1. A stage, comprising: a substrate having a first face, a second face adjacent to the first face, and a face forming a corner portion between the first face and the second face; as well as an insulating film disposed on the substrate, The insulating film includes a plurality of particles having flat surfaces, and is provided on the substrate such that the flat surfaces are along the first surface, the surface formed at the corner portion, and the second surface and are parallel to these surfaces.
2. The stage according to claim 1, wherein: The substrate has a third surface that is 180 degrees opposite to the first surface. The flat surface of the insulating film is provided along the third surface.
3. The stage according to claim 1, wherein: The surface extending from the first surface and the surface extending from the second surface are arranged to intersect at 90 degrees.
4. The stage according to claim 1 or 2, wherein: A ratio of the area of the voids to a predetermined area of the insulating film is 5% or less.
5. The stage according to claim 1 or 2, wherein: The substrate has channels for the flow of liquid.
6. The stage according to claim 1 or 2, wherein: An electrostatic chuck is provided on the insulating film.
7. The stage according to claim 1, wherein: The surface formed at the corner portion is a curved surface, and is provided continuously with the first surface and the second surface.
8. A method for manufacturing a stage, comprising: A step of spraying an insulator having a flat surface onto the first surface from a direction perpendicular to the first surface while moving in a direction parallel to the first surface of the substrate; A step of spraying the insulator having a flat surface toward the surface formed at the corner from a direction perpendicular to the surface formed at the corner while moving in a direction parallel to the surface formed at the corner between the first surface and a second surface of the substrate adjacent to the first surface; as well as a step of spraying the insulator having a flat surface onto the second surface from a direction perpendicular to the second surface while moving in a direction parallel to the second surface; The insulator having a flat surface is continuously sprayed onto the first surface, the surface formed at the corner, and the second surface, whereby the insulating film is provided on the substrate in such a manner that the flat surface is parallel to the first surface, the surface formed at the corner, and the second surface.
9. The manufacturing method according to claim 8, wherein: The insulator is sprayed onto the third surface from a direction perpendicular to the third surface while moving in a direction parallel to a third surface of the substrate that is 180 degrees opposite to the first surface.
10. The manufacturing method according to claim 8, wherein: A surface extending from the first surface and a surface extending from the second surface are formed to intersect at 90 degrees.
11. The manufacturing method according to claim 8, wherein: The operation of continuously spraying the insulator onto the first surface, the surface formed at the corner portion, and the second surface is repeatedly performed.
12. The manufacturing method according to claim 8, wherein: The insulating film includes a plurality of particles having flat surfaces, The plurality of particles are thermally sprayed so that the flat surfaces thereof are along the first surface, the surfaces formed at the corner portions, and the second surface.
13. The manufacturing method according to claim 9, wherein: The insulating film includes a plurality of particles having flat surfaces, The plurality of particles are sprayed so that the flat surfaces thereof are along the third surface.
14. The manufacturing method according to claim 8 or 9, wherein: The substrate has channels for the flow of liquid.
15. The manufacturing method according to claim 8 or 9, wherein: An electrostatic chuck is disposed on the substrate.
16. The manufacturing method according to claim 9, wherein: The operation of thermally spraying the insulator onto the third surface and the operation of thermally spraying the insulator onto the first surface and the second surface are repeated alternately.
17. The manufacturing method according to claim 9, wherein: The operation of thermally depositing the insulator on the third surface, the operation of thermally depositing the insulator on the second surface, and the operation of thermally depositing the insulator on the first surface are performed continuously.