A method and device for determining the position of butterfly defects in CMP process
By dividing the chip layout into regions and establishing a grid, the location of butterfly defects in the CMP process can be determined, solving the problem of inaccurate positioning in existing technologies and achieving higher product yield and planarization effect.
Patent Information
- Application Number
- CN202110818227.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-07-20
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2041-07-20
AI Technical Summary
Existing technologies cannot accurately determine the specific location of butterfly defects in CMP processes, leading to a decrease in chip manufacturing yield, especially at nanometer/deep submicron process nodes where the impact is more significant.
The blank areas of the chip layout are divided into rectangular and/or triangular regions. Sensitive areas are identified and primary and secondary meshes are established. The location of butterfly defects is determined by equivalent parameter extraction and CMP simulation. Redundant metal filling is performed to avoid local defects.
It improves the accuracy of determining the location of butterfly defects, reduces local defects on the chip surface, and enhances the planarization effect and product yield of the CMP process.
Smart Images

Figure CN113486626B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of integrated circuit design for manufacturability, and in particular to a method and device for determining a butterfly defect position in a CMP process. Background Art
[0002] In the large-scale integrated circuit manufacturing process, CMP (Chemical Mechanical Polishing) is a planarization process that combines chemical and mechanical actions, and is the main means of global planarization of the chip surface.
[0003] Due to the different removal rates of different materials in the CMP process, there are two main defects: dishing and erosion. The dishing defect is particularly prominent in the node process below 45nm, directly affecting the performance of the device and the yield of the chip. At present, the dishing defect is mainly solved by the redundant metal filling technology (dummy fill). This technology fills redundant metal in the places where defects may occur to make the layout density uniform, thereby reducing the occurrence of dishing defects.
[0004] A butterfly defect is a local defect, that is, a depression appears in the metal line. The size of the butterfly defect is represented by the height difference between the dielectric layer and the lowest point in the metal line. The current redundant metal filling method cannot accurately determine the specific location of the butterfly defect. As the chip manufacturing process gradually enters the nano / deep submicron process node, the impact of butterfly defects is getting bigger and bigger, which will lead to chip tape-out failure or a decrease in product yield. Summary of the invention
[0005] In order to solve the above technical problems, the present application provides a method and device for determining the position of a butterfly defect in a CMP process, which can accurately determine the specific position of the butterfly defect for redundant metal filling, thereby improving product yield.
[0006] In a first aspect, an embodiment of the present application provides a method for detecting butterfly defect locations in a CMP process, comprising:
[0007] Divide the blank area of the chip layout into a number of rectangular and / or triangular areas;
[0008] The blank area corresponding to the distance between the metal wires being greater than or equal to the first preset value is taken as the sensitive area;
[0009] A primary grid and a secondary grid are established according to the sensitive area; the lengths of the primary grid and the secondary grid are equal to the length of the sensitive area; the area of the secondary grid is greater than the area of the primary grid;
[0010] Extracting equivalent parameters according to the structural information of the primary grid and the secondary grid;
[0011] The chip layout is subjected to CMP simulation according to the equivalent parameters, and the location and structural information of the butterfly defect are determined from the simulation results.
[0012] Optionally, establishing a primary grid and a secondary grid according to the sensitive area includes:
[0013] The length of the sensitive area is used as the primary grid length, and the width of the sensitive area plus a second preset value is used to obtain the primary grid width, and a primary grid is established;
[0014] The length of the sensitive area is used as the secondary grid length, and the primary grid width is added with a third preset value to obtain the secondary grid width, and the secondary grid is established.
[0015] Optionally, the extracting equivalent parameters according to the structural information of the primary grid and the secondary grid includes:
[0016] Equivalently converting the metal wires in the primary grid into two equivalent metal wires with equal widths and symmetrically distributed along the sensitive area, and calculating the width of one of the equivalent metal wires;
[0017] The metal wire density of the peripheral area is calculated; the peripheral area is the area between the primary grid and the secondary grid; the metal wire density is the ratio of the area of the metal wires in the peripheral area to the area of the peripheral area;
[0018] Equivalent parameters are calculated based on the width of the equivalent metal wire, the metal wire density, the total perimeter of the metal wire in the secondary grid and the width of the sensitive area; the equivalent parameters include equivalent line width and equivalent spacing.
[0019] Optionally, the calculating to obtain a width of the equivalent metal line includes:
[0020] Calculate the total area of the metal wires in the primary grid;
[0021] The total area is divided by the length of the primary grid to obtain the total width of the equivalent metal line, and the width of one equivalent metal line is half of the total width of the equivalent metal line.
[0022] Optionally, the method further includes:
[0023] Redundant metal filling is performed according to the position and structure information of the butterfly defect.
[0024] In a second aspect, an embodiment of the present application provides a device for determining a location of a butterfly defect in a CMP process, comprising:
[0025] A division unit, used to divide the blank area of the chip layout into a plurality of rectangular and / or triangular areas;
[0026] A sensitive area determination unit, configured to take a blank area corresponding to a distance between metal wires greater than or equal to a first preset value as a sensitive area;
[0027] A grid establishment unit, used to establish a primary grid and a secondary grid according to the sensitive area; the length of the primary grid and the secondary grid is equal to the length of the sensitive area; the area of the secondary grid is greater than the area of the primary grid;
[0028] An equivalent parameter extraction unit, used for extracting equivalent parameters according to the structural information of the primary grid and the secondary grid;
[0029] The simulation unit is used to perform CMP simulation on the chip layout according to the equivalent parameters, and determine the location and structural information of the butterfly defect from the simulation results.
[0030] Optionally, the grid establishing unit includes:
[0031] A primary grid establishing unit, used to take the length of the sensitive area as the primary grid length, add the width of the sensitive area to a second preset value to obtain the primary grid width, and establish the primary grid;
[0032] The secondary grid establishing unit is used to use the length of the sensitive area as the secondary grid length, add the primary grid width to a third preset value to obtain the secondary grid width, and establish the secondary grid.
[0033] Optionally, the equivalent parameter extraction unit includes:
[0034] An equivalent metal line extraction unit, used to convert the metal lines in the primary grid into two equivalent metal lines with equal widths and symmetrically distributed along the sensitive area, and calculate the width of one of the equivalent metal lines;
[0035] A metal wire density calculation unit, used to calculate the metal wire density of the peripheral area; the peripheral area is the area between the primary grid and the secondary grid; the metal wire density is the ratio of the area of the metal wires in the peripheral area to the area of the peripheral area;
[0036] The equivalent parameter extraction subunit is used to calculate the equivalent parameters according to the width of the equivalent metal wire, the metal wire density, the total perimeter of the metal wire in the secondary grid and the width of the sensitive area; the equivalent parameters include the equivalent line width and the equivalent spacing.
[0037] Optionally, the equivalent metal line extraction unit includes:
[0038] A metal wire area calculation unit, used to calculate the total area of the metal wires in the primary grid;
[0039] The equivalent metal line width calculation unit is used to divide the total area by the length of the first-level grid to obtain the total width of the equivalent metal line, and the width of one equivalent metal line is half of the total width of the equivalent metal line.
[0040] Optionally, the device further comprises:
[0041] The redundant metal filling unit is used to perform redundant metal filling according to the position and structure information of the butterfly defect.
[0042] Compared with the prior art, this application has at least the following advantages:
[0043] The present application provides a method and device for determining the position of butterfly defects in a CMP process, wherein a blank area of a chip layout is divided into a plurality of rectangular and / or triangular areas. Since the distance between metal lines is greater than or equal to a first preset value, the possibility of butterfly defects is relatively high. Therefore, the blank area corresponding to the distance between metal lines being greater than or equal to the first preset value is used as a sensitive area. A primary grid and a secondary grid are established based on the sensitive area. The length of the primary grid and the secondary grid is equal to the length of the sensitive area. Equivalent parameters are extracted based on the structural information of the primary grid and the secondary grid. CMP simulation is performed on the chip layout based on the equivalent parameters, and the position and structural information of the butterfly defects are determined from the simulation results. Since the primary grid and the secondary grid are established based on the sensitive area, the specific position of the butterfly defects in the CMP process can be determined more accurately, thereby effectively avoiding defects in local areas of the chip surface and realizing the flattening of the CMP grinding process. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0045] Figure 1 A flow chart of a method for determining a butterfly defect position in a CMP process provided by an embodiment of the present application is shown;
[0046] Figure 2 A structural diagram of a chip layout division provided by an embodiment of the present application is shown;
[0047] Figure 3 A schematic diagram of a device for determining a butterfly defect position in a CMP process provided by an embodiment of the present application is shown. DETAILED DESCRIPTION
[0048] In order to make the above-mentioned objects, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail below with reference to the accompanying drawings.
[0049] In the following description, many specific details are set forth to facilitate a full understanding of the present application, but the present application may also be implemented in other ways different from those described herein, and those skilled in the art may make similar generalizations without violating the connotation of the present application. Therefore, the present application is not limited to the specific embodiments disclosed below.
[0050] As described in the background art, in the large-scale integrated circuit manufacturing process, CMP (Chemical Mechanical Polishing) is a planarization process that combines chemical and mechanical actions and is the main means of global planarization of the chip surface.
[0051] Due to the different removal rates of different materials in the CMP process, there are two main defects: dishing and erosion. The dishing defect is particularly prominent in the node process below 45nm, directly affecting the performance of the device and the yield of the chip. At present, the dishing defect is mainly solved by the redundant metal filling technology (dummy fill). This technology fills redundant metal in the places where defects may occur to make the layout density uniform, thereby reducing the occurrence of dishing defects.
[0052] A butterfly defect is a local defect, that is, a depression appears in the metal line. The size of the butterfly defect is represented by the height difference between the dielectric layer and the lowest point in the metal line. The current redundant metal filling method cannot accurately determine the specific location of the butterfly defect. As the chip manufacturing process gradually enters the nano / deep submicron process node, the impact of butterfly defects is getting bigger and bigger, which will lead to chip tape-out failure or a decrease in product yield.
[0053] In order to solve the above technical problems, the present application provides a method and device for determining the position of butterfly defects in a CMP process, dividing the blank area of the chip layout into a number of rectangular and / or triangular areas. Since the distance between metal lines is greater than or equal to a first preset value, the possibility of butterfly defects is relatively high. Therefore, the blank area corresponding to the distance between metal lines is greater than or equal to the first preset value is used as a sensitive area, and a primary grid and a secondary grid are established according to the sensitive area. The length of the primary grid and the secondary grid is equal to the length of the sensitive area. Equivalent parameters are extracted according to the structural information of the primary grid and the secondary grid. CMP simulation is performed on the chip layout according to the equivalent parameters, and the position and structural information of the butterfly defect are determined from the simulation results. Since the primary grid and the secondary grid are established according to the sensitive area, the specific position of the butterfly defect in the CMP process can be determined more accurately, so that the defects in the local area of the chip surface can be effectively avoided, and the flattening of the CMP grinding process can be achieved.
[0054] In order to better understand the technical solution and technical effects of the present application, specific embodiments will be described in detail below with reference to the accompanying drawings.
[0055] Exemplary Methods
[0056] See also Figure 1 FIG. 1 is a flow chart of a method for determining a butterfly defect position in a CMP process provided by an embodiment of the present application, and the specific steps include:
[0057] S101: Divide the blank area of the chip layout into a plurality of rectangular and / or triangular areas.
[0058] In the embodiment of the present application, the chip layout is an integrated circuit layout including a metal structure, and the metal structure may be a metal wiring layer or a metal interconnection layer. The layout may be a layout provided in an electronic design automation file format, such as a layout provided in a GDS format.
[0059] First, the chip layout can be read in to obtain the internal structural information of the chip layout. The internal structural information of the chip layout can include the area, height, length, width and other information of the metal wire and dielectric layer. Figure 2 As shown, the blank area of the chip layout can be divided into several rectangular and / or triangular areas. The figure only shows the blank area of the chip layout divided into rectangular areas St i In other layouts, when the blank area cannot be completely divided by a rectangle, the blank area can be divided by a triangle, which is not specifically limited in the embodiments of the present application.
[0060] S102: A blank area corresponding to a distance between metal lines greater than or equal to a first preset value is used as a sensitive area.
[0061] In the embodiment of the present application, since the possibility of CMP butterfly defects is high when the distance between the metal lines is greater than or equal to the first preset value, the blank area corresponding to the distance between the metal lines being greater than or equal to the first preset value can be used as the sensitive area Sti, see Figure 2 As shown, that is, the size of S1 is greater than or equal to the first preset value, and the blank area with a width of S1 is used as the sensitive area Sti.
[0062] It should be noted that the size of the first preset value can be determined by the CMP process conditions and the CMP simulation results, and is not specifically limited in the embodiments of the present application, and can be set by those skilled in the art according to actual conditions.
[0063] S103: establishing a primary grid and a secondary grid according to the sensitive area; the lengths of the primary grid and the secondary grid are equal to the length of the sensitive area; and the area of the secondary grid is greater than the area of the primary grid.
[0064] In the embodiment of the present application, after the sensitive area is determined, since the metal wires near the sensitive area have a certain influence on the formation of the butterfly defect, a primary grid and a secondary grid can be established according to the sensitive area, and the length of the primary grid and the secondary grid is equal to the length of the sensitive area, and the area of the secondary grid is greater than the area of the primary grid. The size of the primary grid and the secondary grid is set according to the size of the sensitive area, so that the position of the butterfly area can be determined more accurately, avoiding the current stage where the fixed grid cannot adapt well to the sensitive area due to the fixed size of the fixed grid. The final simulation result is the average value of the chip layout structure information, and the specific position of the butterfly defect cannot be accurately determined in the end.
[0065] See also Figure 2 As shown, it is a schematic diagram of the primary grid and the secondary grid established according to the sensitive area in an embodiment of the present application, wherein the length GL1 of the primary grid and the length GL2 of the secondary grid are equal to the length GL0 of the sensitive area, and the area of the secondary grid is larger than the area of the primary grid.
[0066] Optionally, the width of the sensitive area can be added to the second preset value to obtain the primary grid width, thereby establishing a primary grid, that is, the primary grid width GW1 is equal to the sum of the width S1 of the sensitive area and the second preset value △S1; the primary grid width GW1 can be added to the third preset value △S2 to obtain the secondary grid width GW2. It should be noted that the embodiment of the present application does not specifically limit the size of the second preset value △S1 and the third preset value △S2, which can be set by those skilled in the art according to actual conditions.
[0067] S104: Extracting equivalent parameters according to the structural information of the primary grid and the secondary grid.
[0068] In an embodiment of the present application, after the primary grid and the secondary grid are established, equivalent parameter extraction can be performed based on the structural information of the primary grid and the secondary grid. First, the structural information of the central area within the primary grid can be simplified, that is, the metal lines within the primary grid can be equivalent to two equivalent metal lines with equal widths and symmetrically distributed along the sensitive area, and the width W1 of any one of the equivalent metal lines can be calculated.
[0069] Optionally, the total area of the metal wires in the first-level grid ∑A can be calculated 1i , the total area ∑A 1i The total width of the equivalent metal line is obtained by dividing the length GL1 of the first-level grid. The width W1 of an equivalent metal line is half of the total width of the equivalent metal line.
[0070] Right now Among them, A 1i It is the area where the i-th metal wire in the primary grid intersects with the primary grid.
[0071] Optionally, the metal wire density ρ of the peripheral area can be calculated. The peripheral area is the area between the primary grid and the secondary grid. The metal wire density ρ is the ratio of the area of the metal wires in the peripheral area to the area of the peripheral area.
[0072] Right now Among them, S total is the total area of metal wires in the secondary grid.
[0073] Optionally, equivalent parameters can be calculated based on the equivalent metal wire width W1, the metal wire density ρ, the total perimeter Pe of the metal wires in the secondary grid and the sensitive area width S1, and the equivalent parameters include the equivalent line width W3 and the equivalent spacing S3.
[0074] Specifically, the contact mechanics theory can be used to introduce the pressure P on the upper surface of the central area of the secondary grid: up and the pressure P on the lower surface down The formula is used to calculate the equivalent line width and equivalent spacing.
[0075] in
[0076] Where C1 and C2 are constants.
[0077] Since there are various complex and irregular metal line structures inside the secondary grid, a set of equivalent parameters, namely, equivalent line width and equivalent spacing, must be input in the actual CMP simulation process.
[0078] Therefore, it is also necessary to introduce the upper and lower surface pressure formulas of the standard structure (ie, the metal wires inside the grid are equivalent to a set of equivalent line width W3 and equivalent spacing S3) for calculation.
[0079]
[0080]
[0081] In addition, formula (1) = (3), (2) = (4), and by solving this set of equations, the equivalent line width S3 and the equivalent spacing S4 can be obtained.
[0082] S105: Perform CMP simulation on the chip layout according to the equivalent parameters, and determine the location and structural information of the butterfly defect from the simulation results.
[0083] In the embodiment of the present application, after the equivalent parameters are calculated, the equivalent parameters can be used to perform CMP simulation on the chip layout, so as to determine the location and structural information of the butterfly defect from the simulation results.
[0084] Specifically, a CMP simulation may be performed first to determine whether a CMP local butterfly defect is generated. If a butterfly defect is generated, the defect position and corresponding structural information are further marked.
[0085] Optionally, redundant metal filling can be performed based on the location and structural information of the butterfly defect. Redundant metal filling refers to adding metal structure in the area with low metal structure density in the layout. The added metal structure is not used for the actual connection of the device, but is to improve the uniformity of the metal structure in the layout. In this way, the generation of defects can be reduced in the CMP process and the flatness of the chip surface after the CMP process can be improved.
[0086] The present application provides a method for determining the position of butterfly defects in a CMP process, dividing the blank area of a chip layout into a plurality of rectangular and / or triangular areas, and since the distance between metal lines is greater than or equal to a first preset value, the possibility of butterfly defects is relatively high, therefore, the blank area corresponding to the distance between metal lines being greater than or equal to the first preset value is taken as a sensitive area, and a primary grid and a secondary grid are established according to the sensitive area, and the length of the primary grid and the secondary grid is equal to the length of the sensitive area, and equivalent parameters are extracted according to the structural information of the primary grid and the secondary grid, and CMP simulation is performed on the chip layout according to the equivalent parameters, and the position and structural information of the butterfly defects are determined from the simulation results. Since the primary grid and the secondary grid are established according to the sensitive area, the specific position of the butterfly defects in the CMP process can be determined more accurately, so that the defects in the local area of the chip surface can be effectively avoided, and the flattening of the CMP grinding process can be achieved.
[0087] Exemplary Devices
[0088] See also Figure 3 FIG. 1 is a schematic diagram of a device for determining a butterfly defect position in a CMP process provided by an embodiment of the present application, comprising:
[0089] A division unit 301 is used to divide the blank area of the chip layout into a plurality of rectangular and / or triangular areas;
[0090] A sensitive area determination unit 302, configured to take a blank area corresponding to a distance between metal wires greater than or equal to a first preset value as a sensitive area;
[0091] A grid establishment unit 303 is used to establish a primary grid and a secondary grid according to the sensitive area; the length of the primary grid and the secondary grid is equal to the length of the sensitive area; the area of the secondary grid is greater than the area of the primary grid;
[0092] An equivalent parameter extraction unit 304, configured to extract equivalent parameters according to the structural information of the primary grid and the secondary grid;
[0093] The simulation unit 305 is used to perform CMP simulation on the chip layout according to the equivalent parameters, and determine the location and structural information of the butterfly defect from the simulation results.
[0094] Optionally, the grid establishing unit 303 includes:
[0095] A primary grid establishing unit, used to take the length of the sensitive area as the primary grid length, add the width of the sensitive area to a second preset value to obtain the primary grid width, and establish the primary grid;
[0096] The secondary grid establishing unit is used to use the length of the sensitive area as the secondary grid length, add the primary grid width to a third preset value to obtain the secondary grid width, and establish the secondary grid.
[0097] Optionally, the equivalent parameter extraction unit 304 includes:
[0098] An equivalent metal line extraction unit, used to convert the metal lines in the primary grid into two equivalent metal lines with equal widths and symmetrically distributed along the sensitive area, and calculate the width of one of the equivalent metal lines;
[0099] A metal wire density calculation unit, used to calculate the metal wire density of the peripheral area; the peripheral area is the area between the primary grid and the secondary grid; the metal wire density is the ratio of the area of the metal wires in the peripheral area to the area of the peripheral area;
[0100] The equivalent parameter extraction subunit is used to calculate the equivalent parameters according to the width of the equivalent metal wire, the metal wire density, the total perimeter of the metal wire in the secondary grid and the width of the sensitive area; the equivalent parameters include the equivalent line width and the equivalent spacing.
[0101] Optionally, the equivalent metal line extraction unit includes:
[0102] A metal wire area calculation unit, used to calculate the total area of the metal wires in the primary grid;
[0103] The equivalent metal line width calculation unit is used to divide the total area by the length of the first-level grid to obtain the total width of the equivalent metal line, and the width of one equivalent metal line is half of the total width of the equivalent metal line.
[0104] Optionally, the device further comprises:
[0105] The redundant metal filling unit is used to perform redundant metal filling according to the position and structure information of the butterfly defect.
[0106] The present application provides a device for determining the position of butterfly defects in a CMP process, dividing the blank area of a chip layout into a plurality of rectangular and / or triangular areas, and since the distance between metal lines is greater than or equal to a first preset value, the possibility of butterfly defects is relatively high, therefore, the blank area corresponding to the distance between metal lines being greater than or equal to the first preset value is used as a sensitive area, and a primary grid and a secondary grid are established according to the sensitive area, and the length of the primary grid and the secondary grid is equal to the length of the sensitive area, and equivalent parameters are extracted according to the structural information of the primary grid and the secondary grid, and CMP simulation is performed on the chip layout according to the equivalent parameters, and the position and structural information of the butterfly defects are determined from the simulation results. Since the primary grid and the secondary grid are established according to the sensitive area, the specific position of the butterfly defects in the CMP process can be determined more accurately, so that the defects in the local area of the chip surface can be effectively avoided, and the flattening of the CMP grinding process can be achieved.
[0107] Each embodiment in this specification is described in a progressive manner, and the same or similar parts between the embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. In particular, for the device embodiment, since it is basically similar to the method embodiment, the description is relatively simple, and the relevant parts can be referred to the partial description of the method embodiment.
[0108] The above is only a preferred implementation of the present application. Although the present application has been disclosed as a preferred embodiment, it is not intended to limit the present application. Any technician familiar with the art can use the above disclosed methods and technical contents to make many possible changes and modifications to the technical solution of the present application without departing from the scope of the technical solution of the present application, or modify it into an equivalent embodiment of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiments based on the technical essence of the present application without departing from the content of the technical solution of the present application still falls within the scope of protection of the technical solution of the present application.
Claims
1. A method for determining the location of a butterfly defect in a CMP process, characterized in that: include: Divide the blank area of the chip layout into a number of rectangular and / or triangular areas; The blank area corresponding to the distance between the metal wires being greater than or equal to the first preset value is taken as the sensitive area; Establishing a primary grid and a secondary grid according to the sensitive area; the length of the primary grid and the secondary grid is equal to the length of the sensitive area; The area of the secondary grid is greater than the area of the primary grid; Extracting equivalent parameters according to the structural information of the primary grid and the secondary grid; Perform CMP simulation on the chip layout according to the equivalent parameters, and determine the location and structural information of the butterfly defect from the simulation results; The step of establishing a primary grid and a secondary grid according to the sensitive area includes: The length of the sensitive area is used as the primary grid length, and the width of the sensitive area plus a second preset value is used to obtain the primary grid width, and a primary grid is established; The length of the sensitive area is used as the secondary grid length, and the primary grid width is added with a third preset value to obtain the secondary grid width, and the secondary grid is established.
2. The method according to claim 1, characterized in that The extracting equivalent parameters according to the structural information of the primary grid and the secondary grid includes: Equivalently converting the metal wires in the primary grid into two equivalent metal wires with equal widths and symmetrically distributed along the sensitive area, and calculating the width of one of the equivalent metal wires; The metal wire density of the peripheral area is calculated; the peripheral area is the area between the primary grid and the secondary grid; the metal wire density is the ratio of the area of the metal wires in the peripheral area to the area of the peripheral area; Equivalent parameters are calculated based on the width of the equivalent metal wire, the metal wire density, the total perimeter of the metal wire in the secondary grid and the width of the sensitive area; the equivalent parameters include equivalent line width and equivalent spacing.
3. The method according to claim 2, characterized in that The calculating of the width of the equivalent metal line includes: Calculate the total area of the metal wires in the primary grid; The total area is divided by the length of the primary grid to obtain the total width of the equivalent metal line, and the width of one equivalent metal line is half of the total width of the equivalent metal line.
4. The method according to claim 3, characterized in that The method further comprises: Redundant metal filling is performed according to the position and structure information of the butterfly defect.
5. A device for determining the location of a butterfly defect in a CMP process, characterized in that: include: A division unit, used to divide the blank area of the chip layout into a plurality of rectangular and / or triangular areas; A sensitive area determination unit, configured to take a blank area corresponding to a distance between metal wires greater than or equal to a first preset value as a sensitive area; A grid establishment unit, used to establish a primary grid and a secondary grid according to the sensitive area; the length of the primary grid and the secondary grid is equal to the length of the sensitive area; The area of the secondary grid is greater than the area of the primary grid; An equivalent parameter extraction unit, used for extracting equivalent parameters according to the structural information of the primary grid and the secondary grid; A simulation unit, used for performing CMP simulation on the chip layout according to the equivalent parameters, and determining the location and structural information of the butterfly defect from the simulation results; The grid establishing unit comprises: A primary grid establishing unit, used to take the length of the sensitive area as the primary grid length, add the width of the sensitive area to a second preset value to obtain the primary grid width, and establish the primary grid; The secondary grid establishing unit is used to use the length of the sensitive area as the secondary grid length, add the primary grid width to a third preset value to obtain the secondary grid width, and establish the secondary grid.
6. The device according to claim 5, characterized in that The equivalent parameter extraction unit comprises: An equivalent metal line extraction unit, used for converting the metal lines in the primary grid into two equivalent metal lines with equal widths and symmetrically distributed along the sensitive area, and calculating the width of one of the equivalent metal lines; A metal wire density calculation unit, used to calculate the metal wire density of the peripheral area; the peripheral area is the area between the primary grid and the secondary grid; the metal wire density is the ratio of the area of the metal wires in the peripheral area to the area of the peripheral area; The equivalent parameter extraction subunit is used to calculate the equivalent parameters according to the width of the equivalent metal wire, the metal wire density, the total perimeter of the metal wire in the secondary grid and the width of the sensitive area; the equivalent parameters include the equivalent line width and the equivalent spacing.
7. The device according to claim 6, characterized in that The equivalent metal line extraction unit comprises: A metal wire area calculation unit, used to calculate the total area of the metal wires in the primary grid; The equivalent metal line width calculation unit is used to divide the total area by the length of the first-level grid to obtain the total width of the equivalent metal line, and the width of one equivalent metal line is half of the total width of the equivalent metal line.
8. The device according to claim 7, characterized in that The device also includes: The redundant metal filling unit is used to perform redundant metal filling according to the position and structure information of the butterfly defect.