Method for manufacturing optical fingerprint device

By using a light-transmitting material to cover the pad area and form a light-transmitting structure and microlens in optical fingerprint devices, the problem of poor uniformity of the light-transmitting layer in the prior art is solved, improving signal accuracy and production efficiency, and reducing costs.

CN113707676BActive Publication Date: 2024-11-26GALAXYCORE SHANGHAI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010441471.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-05-22
Publication Date
2024-11-26
Estimated Expiration
2040-05-22

AI Technical Summary

Technical Problem

In the current manufacturing of optical fingerprint devices, the poor uniformity of the light-transmitting layer, light-blocking layer, and infrared cut-off filter film leads to low signal accuracy, high process difficulty, limited production capacity, and high manufacturing cost.

Method used

The pad area is covered with a light-transmitting material, and a light-transmitting structure and microlens are formed through an imprinting process. Combined with a light-blocking structure and an infrared cut-off filter film, the difficulty of the pad opening process is reduced, and production efficiency and structural reliability are improved.

Benefits of technology

It improves the uniformity of incident light, enhances the accuracy of pixel units in receiving optical signals, reduces manufacturing costs, and improves the recognition performance of optical fingerprint devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113707676B_ABST
    Figure CN113707676B_ABST
Patent Text Reader

Abstract

The present invention provides a method for manufacturing an optical fingerprint device, wherein the optical fingerprint device comprises an image sensor chip having a pad area and a photosensitive area, wherein the pad area is covered with a light-transmitting material and then the light-transmitting material on the pad area is pressed away, thereby reducing the difficulty of a pad opening process, improving production efficiency, increasing production capacity, and reducing manufacturing costs; a light-transmitting material is used to form a light-transmitting structure located above a photosensitive unit of the image sensor to replace the light-transmitting layer in the prior art, thereby improving structural reliability, improving the uniformity of incident light, improving the accuracy of a pixel unit in receiving an optical signal, and improving the recognition performance of the optical fingerprint device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for manufacturing an optical fingerprint device. Background Art

[0002] The current fingerprint recognition solutions include optical technology, silicon technology (capacitive / radio frequency), ultrasonic technology, etc. Among them, optical fingerprint recognition technology has been widely used in portable electronic devices.

[0003] Optical fingerprint recognition technology uses optical imaging equipment based on the principle of total reflection of light (FTIR). Light shines on the surface of the light-transmitting layer (such as organic or inorganic glass) with fingerprints pressed on it, and the reflected light is captured by the image sensor. The amount of reflected light depends on the depth of the fingerprint ridges and valleys pressed on the glass surface, as well as the oil and moisture between the skin and the glass. After the light passes through the glass and reaches the center of the valley, it is totally reflected at the interface between the glass and the air, and the light is reflected to the image sensor, while the light directed to the ridge is not totally reflected, but is absorbed by the contact surface between the ridge and the glass or diffusely reflected to other centers, thus forming an image of the fingerprint on the image sensor.

[0004] Since a larger microlens is required to increase the energy of the incident light and achieve higher image quality, in the prior art, it is often necessary to set a thicker light-transmitting layer (more than 50μm) above the pixel unit and a thicker light-blocking layer (for example, 15-50μm) between the pixel units in order to solve the problem of incident light entering the adjacent pixel units of the image sensor and causing signal crosstalk. In addition, an infrared cut-off filter film is also required above the pixel unit to reduce the infrared light in the incident light entering the image sensor to cause noise crosstalk and image distortion, thereby improving the optical performance of the optical fingerprint device. However, it should be noted that the light-transmitting layer, light-blocking layer, and infrared cut-off filter film all need to avoid the pad area of ​​the image sensor to avoid affecting the electrical connection performance of the pad area.

[0005] However, the reliability of setting a light-transmitting layer above the pixel unit by using a film-sticking method is poor, and the uniformity of the film in the hole is also difficult to control, so that the incident light passing through the light-transmitting layer often has a problem of poor uniformity, thereby affecting the accuracy of the optical signal received by the pixel unit of the image sensor, and further affecting the recognition performance of the optical fingerprint device.

[0006] In addition, in the prior art, the light-transmitting layer, light-blocking layer, and infrared cutoff filter film corresponding to the pad area are often removed through an etching process to achieve the purpose of opening the pad area of ​​the image sensor. The process is relatively difficult, the etching efficiency is relatively low, the production capacity is very limited, and the manufacturing cost is relatively high. Summary of the invention

[0007] The purpose of the present invention is to provide a method for manufacturing an optical fingerprint device, reduce process difficulty, improve production efficiency, increase production capacity, reduce manufacturing cost, improve structural reliability, improve the uniformity of incident light, improve the accuracy of pixel units receiving optical signals, and improve the recognition performance of optical fingerprint devices.

[0008] Based on the above considerations, the present invention provides a method for manufacturing an optical fingerprint device, comprising the following steps: the optical fingerprint device comprises an image sensor chip having a pad area and a photosensitive area, and the pad area is covered with a light-transmitting material and then the light-transmitting material on the pad area is pressed away, thereby reducing the difficulty of the pad opening process.

[0009] Preferably, a light blocking structure is provided in the photosensitive area, the light-transmitting material is used to form a light-transmitting structure located above the photosensitive unit of the image sensor and a microlens is formed on the light-transmitting structure, and a mold for pressing away the light-transmitting material on the pad area positions the distance from the surface of the microlens to the surface of the light-blocking structure.

[0010] Preferably, when forming the microlenses, transparent side walls are formed between the microlenses at the same time, and then a light blocking layer is formed on the transparent side walls.

[0011] Preferably, a first wafer formed with a plurality of image sensor chips is provided, the light blocking structure is arranged on the first wafer, and the light blocking structure is formed by a second wafer.

[0012] Preferably, the light-transmitting structure and the microlens are integrally formed by embossing.

[0013] Preferably, a light-transmitting structure is first formed by embossing or coating, and after the light-transmitting structure is planarized, a microlens is formed on the light-transmitting structure by embossing or coating.

[0014] Preferably, the light-transmitting material is photosensitive adhesive, silicon dioxide or an organic material.

[0015] Preferably, the method for manufacturing the optical fingerprint device further comprises: forming an infrared cutoff filter film between the light blocking structure and the first wafer.

[0016] Preferably, the light blocking structure is made of a material that is opaque to visible light.

[0017] Preferably, the light-blocking structure is formed by a second wafer or an organic light-blocking material.

[0018] Preferably, the method for manufacturing the optical fingerprint device further comprises covering the surface and side walls of the light-blocking structure with an anti-reflection layer.

[0019] The manufacturing method of the optical fingerprint device of the present invention comprises an image sensor chip having a pad area and a photosensitive area. The pad area is covered with a light-transmitting material and then the light-transmitting material on the pad area is pressed away, thereby reducing the difficulty of the pad opening process, improving production efficiency, increasing production capacity, and reducing manufacturing costs. A light-transmitting material is used to form a light-transmitting structure located above a photosensitive unit of the image sensor to replace the light-transmitting layer in the prior art, thereby improving structural reliability, improving the uniformity of incident light, improving the accuracy of the pixel unit in receiving optical signals, and improving the recognition performance of the optical fingerprint device. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Other features, objects and advantages of the present invention will become more apparent from the following detailed description of non-limiting embodiments with reference to the accompanying drawings.

[0021] Figure 1-Figure 7 The figure is a schematic diagram of a method for manufacturing an optical fingerprint device according to a preferred embodiment of the present invention.

[0022] In the drawings, the same or similar reference numerals denote the same or similar devices (modules) or steps throughout different drawings. DETAILED DESCRIPTION

[0023] The present invention provides a method for manufacturing an optical fingerprint device, wherein the optical fingerprint device comprises an image sensor chip having a pad area and a photosensitive area, wherein the pad area is covered with a light-transmitting material and then the light-transmitting material on the pad area is pressed away, thereby reducing the difficulty of a pad opening process, improving production efficiency, increasing production capacity, and reducing manufacturing costs; a light-transmitting material is used to form a light-transmitting structure located above a photosensitive unit of the image sensor to replace the light-transmitting layer in the prior art, thereby improving structural reliability, improving the uniformity of incident light, improving the accuracy of a pixel unit in receiving an optical signal, and improving the recognition performance of the optical fingerprint device.

[0024] In the following specific description of the preferred embodiments, reference will be made to the attached drawings which constitute a part of the present invention. The attached drawings show by way of example specific embodiments that can implement the present invention. The illustrative embodiments are not intended to be exhaustive of all embodiments according to the present invention. It will be appreciated that other embodiments may be utilized, and structural or logical modifications may also be made without departing from the scope of the present invention. Therefore, the following specific description is not restrictive, and the scope of the present invention is limited by the appended claims.

[0025] The present invention is described in detail below with reference to specific embodiments.

[0026] See also Figure 1, a first wafer 200 having a plurality of image sensors formed thereon is provided. The image sensors include a pad area 202 and a photosensitive area 203 , and the pad area 202 and the photosensitive area 203 are separated by a dotted line in the figure.

[0027] See also Figure 2 , providing a second wafer 206 for forming a light-blocking structure. Preferably, the light-blocking structure is formed of a material that is opaque to visible light. Those skilled in the art will appreciate that using the second wafer to form a light-blocking structure is only a preferred embodiment of the present invention, and according to process and application requirements, the light-blocking structure may also be formed of other organic opaque materials such as black glue.

[0028] Preferably, before the second wafer 206 is combined with the first wafer 200, an infrared cut-off filter film 201 is formed on the surface of the second wafer 206. Preferably, a peeling process or a jig blocking method can be used to make the infrared cut-off filter film 201 avoid the portion corresponding to the pad area 202 of the image sensor.

[0029] Those skilled in the art will understand that the infrared cut-off filter 201 being located on the surface of the second wafer 206 is only a preferred embodiment of the present invention, and according to process and application requirements, the infrared cut-off filter 201 may also be disposed at other locations between the second wafer 206 and the first wafer 200 (e.g., the surface of the first wafer 200 ), or above the second wafer 206 .

[0030] See also Figure 3 Preferably, the second wafer 206 is formed on the first wafer 200 by bonding or oxide layer bonding, and the second wafer is thinned and etched to form a light-blocking structure 206, and the light-blocking structure 206 has a gap 213 in the area corresponding to the photosensitive unit of the image sensor. Preferably, an anti-reflection layer can also be covered on the surface and sidewall of the light-blocking structure 206 to reduce the reflection of light by the light-blocking structure 206.

[0031] See also Figure 4-Figure 6 , a light-transmitting material 207 is used to fill the gap 213 to form a light-transmitting structure 210 located above the photosensitive unit of the image sensor and a microlens 208 is formed on the light-transmitting structure 210. Preferably, the light-transmitting material is a photosensitive adhesive, silicon dioxide (SOG material) or an organic material. Specifically, the gap 213 is first filled by embossing (such as nano-imprinting) or coating to form the light-transmitting structure 210, the light-transmitting material 207 protruding from the gap 213 is flattened, and then the microlens 208 is formed on the light-transmitting structure 210 by embossing or coating. In other preferred embodiments not shown, the light-transmitting structure 210 and the microlens 208 can also be integrally formed by embossing.

[0032] Since the pad area 202 of the image sensor is exposed when the second wafer is etched to form the light blocking structure 206, the light-transmitting material 207 will cover the pad area 202 when the gap 213 is filled. Subsequently, a die (not shown) may be used, and the portion of the die corresponding to the pad area 202 is raised, and the raised portion is pressed above the pad area 202 (see FIG. Figure 4 The die is preferably formed by pressing the light-transmitting material 207 on the pad area 202 in the direction of the arrow in the figure) so as to press away the light-transmitting material 207 on the pad area 202 (the light-transmitting material 207 pressed away will enter the gap 213 of the adjacent light-blocking structure 206 or the image sensor cutting path area not shown), thereby reducing the thickness of the light-transmitting material 207 on the pad area 202 (it is best to completely press away the light-transmitting material 207 on the pad area 202 so that the pad area 202 is completely exposed) to reduce the difficulty of the pad opening process. In addition, the stamper partially positions the distance from the surface of the microlens 208 to the surface of the light-blocking structure 206 corresponding to the photosensitive area 203 to ensure the shape and size of the microlens, thereby making the imaging more accurate and clear. Preferably, the stamper can be integral or split.

[0033] Preferably, when forming the microlenses 208, transparent side walls 211 between the microlenses 108 can be formed simultaneously, and then a light blocking layer 209 such as a black plastic material can be formed on the transparent side walls 211 to further reduce signal interference caused by light crosstalk. In other preferred embodiments not shown, the light blocking layer 209 can also be directly formed between the microlenses 208.

[0034] See also Figure 7 After forming the light-transmitting structure 210 and the microlens 208, the first wafer 200 is thinned. If there is still a small amount of light-transmitting material 207 remaining on the pad area 202, the small amount of light-transmitting material 207 is removed by an etching process to expose the pad area 202. Compared with the prior art of removing a thicker light-transmitting layer by an etching process, the difficulty of the pad opening process is reduced, the production efficiency is improved, the production capacity is increased, and the manufacturing cost is reduced. In addition, since a light-transmitting material is used to form a light-transmitting structure located above the photosensitive unit of the image sensor, replacing the light-transmitting layer in the prior art, the structural reliability is improved, the uniformity of the incident light is improved, the accuracy of the pixel unit receiving the optical signal is improved, and the recognition performance of the optical fingerprint device is improved.

[0035] It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, in any case, the embodiments should be considered exemplary and non-restrictive. Furthermore, it is apparent that the term "comprising" does not exclude other elements and steps, and the wording "a" does not exclude the plural. Multiple elements stated in a device claim may also be implemented by one element. The words first, second, etc. are used to indicate names and do not indicate any particular order.

Claims

1. A method for manufacturing an optical fingerprint device, characterized in that: The steps include: The optical fingerprint device comprises an image sensor chip having a pad area and a photosensitive area, a light-blocking structure is arranged in the photosensitive area, the light-blocking structure has a gap in the area corresponding to the photosensitive unit of the image sensor, a light-transmitting material is used to fill the gap, and the light-transmitting material is embossed to integrally form a light-transmitting structure located above the photosensitive unit of the image sensor and a microlens located on the light-transmitting structure; When the light-transmitting material is used to fill the gap, the light-transmitting material also covers the pad area, and a die is used, wherein the portion of the die corresponding to the pad area is convex, and the convex portion is pressed above the pad area to press away the light-transmitting material on the pad area, thereby reducing the difficulty of the pad opening process; The portion of the stamper corresponding to the photosensitive area positions the distance from the surface of the microlens to the surface of the light blocking structure.

2. The method for manufacturing an optical fingerprint device according to claim 1, characterized in that: When forming the microlenses, transparent side walls between the microlenses are simultaneously formed, and then a light blocking layer is formed on the transparent side walls.

3. The method for manufacturing an optical fingerprint device according to claim 1, characterized in that: A first wafer formed with a plurality of image sensor chips is provided, and the light blocking structure is arranged on the first wafer, and the light blocking structure is formed by a second wafer.

4. The method for manufacturing an optical fingerprint device according to claim 1, characterized in that: The light-transmitting material is photosensitive adhesive, silicon dioxide or organic material.

5. The method for manufacturing an optical fingerprint device according to claim 3, characterized in that: Also includes: An infrared cut-off filter film is formed between the light blocking structure and the first wafer.

6. The method for manufacturing an optical fingerprint device according to claim 1, characterized in that: The light blocking structure is made of a material that is opaque to visible light.

7. The method for manufacturing an optical fingerprint device according to claim 6, characterized in that: The light blocking structure is formed by a second wafer or an organic light blocking material.

8. The method for manufacturing an optical fingerprint device according to claim 1, characterized in that: It also includes covering the surface and sidewalls of the light blocking structure with an anti-reflection layer.