Millimeter wave switch chip

By using the structure of SiC substrate, AlN buffer layer and GaN layer in the millimeter wave switching chip, combining the back gate and top gate dual gate structures to form a dual HEMT channel, the millimeter wave switching chip at high frequency in the prior art is solved. The transmission difficulties under the implementation of high frequency and high power switching effects.

CN113809173BActive Publication Date: 2024-11-22SHENZHEN CHENGEN HOT VISION TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111087348.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-09-16
Publication Date
2024-11-22
Estimated Expiration
2041-09-16

Smart Images

  • Figure CN113809173B_ABST
    Figure CN113809173B_ABST
Patent Text Reader

Abstract

The present invention discloses a millimeter wave switch chip, wherein an AlN buffer layer is formed on the upper surface of a SiC substrate, a first GaN layer is formed on the upper surface of the AlN buffer layer, a portion of the lower surface of the first GaN layer is exposed through a back gate groove, and a back gate is formed on the exposed portion of the lower surface of the first GaN layer; a source ohmic contact layer is formed on the left side of the upper surface of the first GaN layer, a drain ohmic contact layer is formed on the right side of the upper surface of the first GaN layer, a first AlGaN layer, a second GaN layer and a second AlGaN layer are formed on the upper surface of the first GaN layer between the source ohmic contact layer and the drain ohmic contact layer from bottom to top, a source is formed on the upper surface of the source ohmic contact layer, a drain is formed on the upper surface of the drain ohmic contact layer, and a top gate is formed on the upper surface of the second AlGaN layer. The chip has the advantages of high switching frequency speed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of millimeter wave switch devices, and in particular to a millimeter wave switch chip with high switching frequency and speed. Background Art

[0002] Millimeter waves refer to electromagnetic waves with a frequency range of 30GHz-300GHz. In the millimeter wave frequency band, millimeter wave switches play the role of opening and closing millimeter wave signal transmission. At present, some switches in the millimeter wave frequency band are made based on PIN junctions, but millimeter wave switch chips based on this type of technology are difficult to use for space transmission. In the millimeter wave frequency band, GaN HEMT (high electron mobility transistor) can work effectively in the millimeter wave frequency band due to its two-dimensional electron gas, high electron mobility and fast speed. Based on the GaN HEMT structure, it is expected to realize a switch chip for millimeter wave transmission in the horizontal direction and in the vertical direction. Summary of the invention

[0003] The technical problem to be solved by the present invention is how to provide a millimeter wave switch chip with a high switching frequency speed.

[0004] In order to solve the above technical problems, the technical solution adopted by the present invention is: a millimeter wave switch chip, characterized in that: it includes a SiC substrate, an AlN buffer layer is formed on the upper surface of the SiC substrate, a first GaN layer is formed on the upper surface of the AlN buffer layer, a back gate groove is formed at the bottom of the chip, a portion of the lower surface of the first GaN layer is exposed through the back gate groove, and a back gate is formed on the exposed portion of the lower surface of the first GaN layer; a source ohmic contact layer is formed on the left side of the upper surface of the first GaN layer, a drain ohmic contact layer is formed on the right side of the upper surface of the first GaN layer, a first AlGaN layer, a second GaN layer and a second AlGaN layer are formed on the upper surface of the first GaN layer between the source ohmic contact layer and the drain ohmic contact layer from bottom to top, a source is formed on the upper surface of the source ohmic contact layer, a drain is formed on the upper surface of the drain ohmic contact layer, and a top gate is formed on the upper surface of the second AlGaN layer.

[0005] A further technical solution is that the back gate does not contact the SiC substrate and the AlN buffer layer.

[0006] A further technical solution is that the upper surfaces of the source ohmic contact layer, the drain ohmic contact layer and the second AlGaN layer are on the same horizontal plane.

[0007] A further technical solution is that the area of ​​the source is the same as the area of ​​the source ohmic contact layer, the area of ​​the drain ohmic contact layer is the same as the area of ​​the drain ohmic contact layer, and the area of ​​the top gate is smaller than the area of ​​the second AlGaN layer.

[0008] A further technical solution is that the thickness of the back gate is less than the sum of the thicknesses of the SiC substrate and the AlN buffer layer.

[0009] Preferably, the thickness of the SiC substrate is 25 microns to 50 microns.

[0010] Preferably, the thickness of the AlN buffer layer is 10 nm to 50 nm.

[0011] Preferably, the thickness of the first and second GaN layers is 10 nm to 50 nm, and the thickness of the first and second AlGaN layers is 15 nm to 100 nm, wherein the Al component is 30%.

[0012] Preferably, the source ohmic contact layer and the drain ohmic contact layer are made of Ti, Al, Ni and / or Au.

[0013] Preferably, the top gate and the back gate are Schottky contact electrodes, and the materials used to make them are Ti, Pt and / or Au.

[0014] The beneficial effects of the above technical solution are: the switch chip described in this application is made based on the GaN HEMT device structure, using GaN / AlGaN material structure, and using a dual HEMT communication structure to make the switch device, using a top gate and back gate dual gate structure to increase the control of the two-dimensional electron gas. It can achieve the switching effect on the millimeter wave lateral structure (gate length direction), and also achieve the switching effect on the millimeter wave in the longitudinal space (perpendicular to the gate length direction). Due to the use of a dual HEMT channel structure, the switching effect of high-power millimeter wave signals can be achieved. Based on the millimeter wave switch chip proposed in this application, the switch insertion loss is less than 3dB, and can withstand a power greater than 5W. As a space millimeter wave switch, it can be applied to the entire millimeter wave frequency band, and its switching frequency speed is high, up to 1GHz. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] The present invention will be further described in detail below in conjunction with the accompanying drawings and specific embodiments.

[0016] Figure 1 is a schematic diagram of the structure of the switch chip according to an embodiment of the present invention;

[0017] Among them: 1. SiC substrate; 2. AlN buffer layer; 3. first GaN layer; 4. back gate; 5. source ohmic contact layer; 6. drain ohmic contact layer; 7. first AlGaN layer; 8. second GaN layer; 9. second AlGaN layer; 10. source; 11. drain; 12. top gate. DETAILED DESCRIPTION

[0018] The following is a clear and complete description of the technical solutions in the embodiments of the present invention in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0019] In the following description, many specific details are set forth to facilitate a full understanding of the present invention, but the present invention may also be implemented in other ways different from those described herein, and those skilled in the art may make similar generalizations without violating the connotation of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.

[0020] like Figure 1 As shown, an embodiment of the present invention discloses a millimeter wave switch chip, comprising a SiC substrate 1, an AlN buffer layer 2 is formed on the upper surface of the SiC substrate 1, and a first GaN layer 3 is formed on the upper surface of the AlN buffer layer 2; a back gate groove is formed at the bottom of the chip, and a portion of the lower surface of the first GaN layer 3 is exposed through the back gate groove, and a back gate 4 is formed on the exposed portion of the lower surface of the first GaN layer 3, and the back gate 4 does not contact the SiC substrate 1 and the AlN buffer layer 2, and it can be seen from the figure that the thickness of the back gate 4 is less than the sum of the thickness of the SiC substrate 1 and the AlN buffer layer 2, that is, the back gate 4 does not contact the SiC substrate 1 and the AlN buffer layer 2. The back gate groove is exposed; a source ohmic contact layer 5 is formed on the left side of the upper surface of the first GaN layer 3, a drain ohmic contact layer 6 is formed on the right side of the upper surface of the first GaN layer 3, the ohmic base layer is made of metal material, and a first AlGaN layer 7, a second GaN layer 8 and a second AlGaN layer 9 are formed on the upper surface of the first GaN layer 3 between the source ohmic contact layer 5 and the drain ohmic contact layer 6 from bottom to top, a source 10 is formed on the upper surface of the source ohmic contact layer 5, a drain 11 is formed on the upper surface of the drain ohmic contact layer 6, and a top gate 12 is formed on the upper surface of the second AlGaN layer 9.

[0021] Furthermore, in this application, Figure 1 As shown, the upper surfaces of the source ohmic contact layer 5, the drain ohmic contact layer 6 and the second AlGaN layer 9 are on the same horizontal plane, so that the morphology of the chip is better. Furthermore, the area of ​​the source 10 is the same as that of the source ohmic contact layer 5 (the area refers to the area of ​​the upper surface), the area of ​​the drain 11 is the same as that of the drain ohmic contact layer 6, and the area of ​​the top gate 12 is smaller than that of the second AlGaN layer 9.

[0022] Preferably, the thickness of the SiC substrate 1 can be 25 microns to 50 microns; the thickness of the AlN buffer layer 2 can be 10nm to 50nm; the thickness of the first and second GaN layers can be 10nm to 50nm, and the thickness of the first and second AlGaN layers can be 15nm to 100nm, wherein the Al component can be 30%; the source ohmic contact layer 5 and the drain ohmic contact layer 6 can be made of Ti, Al, Ni and / or Au; the top gate 12 and the back gate 4 are Schottky contact electrodes, and the materials thereof can be Ti, Pt and / or Au. It should be noted that the thickness of the SiC substrate 1, the thickness of the AlN buffer layer 2, the thickness of the first and second GaN layers, and the thickness of the first and second AlGaN layers in the present application can also be other values, and the materials of the source ohmic contact layer 5 and the drain ohmic contact layer 6 can also be other materials, as long as they can meet the needs of the chip described in the present application.

[0023] The chip described in this application, due to the bending effect of the energy band between the AlGaN layer and the GaN layer, confines the electrons generated by the piezoelectric polarization between the interfaces to a two-dimensional space, forming a two-dimensional electron gas, and uses the concentration of the two-dimensional electron gas to absorb millimeter waves. Due to the use of two layers of two-dimensional electron gas channels, when the millimeter wave is transmitted from top to bottom, it needs to be absorbed by two layers of two-dimensional electron gas. By adjusting the voltage of the top gate 12 and the back gate 4, the electron gas concentration in the two-dimensional electron gas can be regulated. When the concentration of the two-dimensional electron gas is high, the energy of the millimeter wave signal is absorbed by the two-dimensional electron gas, and the millimeter wave switch is in the off state at this time. When the two-dimensional electron gas is exhausted by the top gate 12 and the back gate 4, the millimeter wave signal can pass through the switching device at this time, and only intrinsic absorption occurs, that is, the on state of the millimeter wave switch, and the insertion loss of the millimeter wave signal can be generated at this time.

[0024] The epitaxial structure of the chip described in this application can be obtained by MOCVD or MBE, and the manufacturing process of the source, drain and top gate is very mature. The back gate in this solution needs to polish the SiC layer and AlN buffer layer on the back and remove part of the SiC layer and part of the AlN buffer layer by gas etching, and then make the back gate on the back of the first GaN layer.

[0025] In summary, the switch chip described in this application is made based on the GaN HEMT device structure, adopts the GaN / AlGaN material structure, and adopts a dual HEMT communication structure to make the switch device, and adopts a top gate and back gate dual gate structure to increase the control of the two-dimensional electron gas. It can not only achieve the switching effect on the millimeter wave lateral structure (gate length direction), but also achieve the switching effect on the millimeter wave in the longitudinal space (perpendicular to the gate length direction). Due to the use of the dual HEMT channel structure, the switching effect of high-power millimeter wave signals can be achieved. Based on the millimeter wave switch chip proposed in this application, the switch insertion loss is less than 3dB, and it can withstand a power greater than 5W. As a space millimeter wave switch, it can be applied to the entire millimeter wave frequency band, and its switching frequency speed is high, up to 1GHz.

Claims

1. A millimeter wave switch chip, characterized in that: The invention comprises a SiC substrate (1), an AlN buffer layer (2) is formed on the upper surface of the SiC substrate (1), a first GaN layer (3) is formed on the upper surface of the AlN buffer layer (2), a back gate groove is formed at the bottom of the chip, a portion of the lower surface of the first GaN layer (3) is exposed through the back gate groove, and a back gate (4) is formed on the exposed portion of the lower surface of the first GaN layer (3); a source ohmic contact layer (5) is formed on the left side of the upper surface of the first GaN layer (3), and the upper surface of the first GaN layer (3) is A drain ohmic contact layer (6) is formed on the right side of the source ohmic contact layer (5), a first AlGaN layer (7), a second GaN layer (8) and a second AlGaN layer (9) are formed on the upper surface of the first GaN layer (3) between the source ohmic contact layer (5) and the drain ohmic contact layer (6) from bottom to top, a source (10) is formed on the upper surface of the source ohmic contact layer (5), a drain (11) is formed on the upper surface of the drain ohmic contact layer (6), and a top gate (12) is formed on the upper surface of the second AlGaN layer (9); The upper surfaces of the source ohmic contact layer (5), the drain ohmic contact layer (6) and the second AlGaN layer (9) are on the same horizontal plane; the area of ​​the source (10) is the same as that of the source ohmic contact layer (5), the area of ​​the drain (11) is the same as that of the drain ohmic contact layer (6), and the area of ​​the top gate (12) is smaller than that of the second AlGaN layer (9); The back gate (4) is not in contact with the SiC substrate (1) and the AlN buffer layer (2); the thickness of the back gate (4) is less than the sum of the thicknesses of the SiC substrate (1) and the AlN buffer layer (2); the thickness of the SiC substrate (1) is 25 micrometers to 50 micrometers; the thickness of the AlN buffer layer (2) is 10 nm to 50 nm; the thickness of the first and second GaN layers is 10 nm to 50 nm, and the thickness of the first and second AlGaN layers is 15 nm to 100 nm, wherein the Al component is 30%; the source ohmic contact layer (5) and the drain ohmic contact layer (6) are made of Ti, Al, Ni and / or Au; the top gate (12) and the back gate (4) are Schottky contact electrodes, and the materials used to make them are Ti, Pt and / or Au; Due to the bending effect of the energy band between the AlGaN layer and the GaN layer, the chip confines the electrons generated by the piezoelectric polarization between the interfaces within a two-dimensional space, forming a two-dimensional electron gas, and utilizing the concentration of the two-dimensional electron gas to absorb the millimeter wave; due to the use of two layers of two-dimensional electron gas channels, when the millimeter wave is transmitted from top to bottom, it needs to be absorbed by the two layers of two-dimensional electron gas, and the electron gas concentration in the two-dimensional electron gas is regulated by adjusting the voltage of the top gate (12) and the back gate (4); when the concentration of the two-dimensional electron gas is high, the energy of the millimeter wave signal is absorbed by the two-dimensional electron gas, and the millimeter wave switch is in the off state at this time; when the two-dimensional electron gas is exhausted by the top gate (12) and the back gate (4), the millimeter wave signal can pass through the switch device, and the millimeter wave switch is in the on state, and the insertion loss of the millimeter wave signal can be generated at this time.