A flexible electronic paper and its preparation and application
By optimizing the materials and processes of flexible electronic paper, including the use of specific color-developing particles, electrophoretic display microcapsules and CPI films, combined with the hot-melt PS hot rolling method, the problems of insufficient bending and sealing properties of flexible electronic paper have been solved, achieving It has been widely used in smart wearable products.
Patent Information
- Application Number
- CN202111164972.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-09-30
- Publication Date
- 2024-10-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing flexible electronic paper has deficiencies in bending, thickness and sealing properties, resulting in limited bending angles and prone to pits, bubbles and warping problems, limiting its application in smart wearable products.
Adopting a structure composed of PS film, color-developing FPL, PI film, PS film, IC and FPC, through the hot-melt process and the lamination of EC glue, the particle size and shape of the color-developing particles and electrophoretic display microcapsules are optimized, and CPI is used Film and specific EC glue, combined with hot-melt PS hot rolling method, improve the bending and sealing properties of flexible electronic paper.
The realization of flexible electronic paper with a bending radius less than or equal to 2cm enhances its application potential in smart wearable products, improves display clarity and bending flexibility, while reducing material thickness and cohesion, reducing the impact on PI films. damage.
Smart Images

Figure CN113960846B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of flexible electronic paper preparation and display technology, and in particular to a flexible electronic paper and its preparation and application. Background Art
[0002] With the rapid development of Internet of Things technology, the Internet of Things ecosystem has basically taken shape. Bistable electronic paper related products, such as electronic tags, electronic table signs, electronic badges, electronic door signs, electronic bus stop signs, electronic bedside cards, electronic infusion cards and other electronic paper related products have been applied to all aspects of life. However, the electronic paper products currently used on the market are easily broken and cannot be bent due to the influence of glass lines. This makes the application of low-power electronic paper products in To C businesses such as smart wearables limited. Therefore, in order to expand the application scenarios of low-power electronic paper products, for the design of electronic paper, we have begun to focus on the development and design of flexible electronic paper.
[0003] The existing flexible electronic paper (EPD) is mainly composed of FPL (electronic paper film), PS film (polystyrene protective film), PI film (polyimide film), IC (integrated circuit chip), FPC (flexible circuit board), PI film, PI film, FPL, PS film are glued together from bottom to top by EC glue (quick ear glue), IC is fixed on FPL by IC reinforcing glue, and FPC is fixed on FPL by UV glue (ultraviolet curing glue) (as shown in the attached manual). Figure 1 As shown). Compared with hard EPD, the main difference of flexible EPD is that the etched circuit TFT of hard EPD is replaced by PI film, which is also the key factor to achieve flexibility. The existing TFT is a hard board circuit. Therefore, the production of flexible electronic paper etches the circuit on the TFT onto the PI film, thereby achieving the technical effect of flexibility, bendability and not easy to break. Among them, EC glue is mainly for sealing, but EC glue is also one of the conditions that restrict the bending of flexible electronic paper. Moreover, the EC glue currently used for electronic paper display has a high hardness. A large bending will cause the EC glue to rupture, causing water, steam, dust, etc. to enter and damage the FPL display; PS film mainly realizes the protection of FPL, IC, etc., but the thickness of the PS film currently used is nearly 300μm, which also greatly limits the flexibility and bendability of flexible electronic paper.
[0004] From the above analysis, we can see that the existing flexible electronic paper structure is limited by the PI circuit, PS film, and EC glue characteristics. The PI display can bend at a limited angle, which results in the current flexible display being thin and light, and the application scenarios that can be used are the same as those of hard screens, which greatly limits the development of flexible screens. In addition to having more stringent requirements for the thinness of the display, electronic products such as wearable products (watches / bracelets) also require the display to have greater bending characteristics. In addition, the currently designed flexible electronic paper still has problems such as pits, bubbles, and warping in terms of display. Summary of the invention
[0005] In view of the shortcomings of the prior art mentioned above, the purpose of the present invention is to provide a flexible electronic paper and its preparation and application to solve the problems of pits, bubbles, warping and other problems existing in the display of existing flexible electronic paper, as well as the shortcomings of small bending range and large overall thickness in flexibility, and to achieve the preparation of flexible electronic paper with a bending radius equal to or less than 2 cm. The flexible electronic paper of the present invention can be better used in fields requiring flexible screens such as smart wearable products (watches / bracelets).
[0006] To achieve the above-mentioned purpose and other related purposes, the first aspect of the present invention provides a flexible electronic paper, which includes, from bottom to top, a PS film (polystyrene film), a color developing FPL (electronic paper ink film), a PI film (polyimide film), a PS film (polystyrene film), and also includes an IC (integrated circuit chip) and an FPC (flexible circuit board). The IC and FPC are fixed on the PI film by IC reinforcing glue and UV glue (ultraviolet curing glue), respectively; the PS film is bonded together with the FPL and the PI film by a hot melt process, and the FPL and the PI film are bonded together by EC glue (quick ear glue).
[0007] Furthermore, the color-developing FPL is formed by injecting electrophoretic display microcapsules into transparent conductive electrodes, and the electrophoretic display microcapsules are obtained by placing color-developing particles into a capsule solution and screening with a rotating wheel; the diameter of the color-developing particles is 200nm±20nm, and the electrophoretic display microcapsules are spheres with a particle size of 20μm to 30μm.
[0008] In order to achieve better flexibility, the present invention optimizes and screens the particle size, morphology, etc. in the color-developing FPL. Particles with a diameter of 200nm±20nm are used as color-developing particles, which can enhance display clarity and improve uniformity. The electrophoresis display microcapsules are spherical structures, which can increase the bending degree of the capsules.
[0009] In the flexible electronic paper of the present invention, the color-developing particles are used to characterize the display color and display clarity of the flexible electronic paper, the microcapsule particles are used to characterize the display clarity and display transparency of the flexible electronic paper, the sealant EC glue is used to characterize the sealing degree and bending degree of the flexible electronic paper, the PS film is used to characterize the bending degree of the flexible electronic paper, and the PI film is used to characterize the bending degree and transparent display degree of the flexible electronic paper.
[0010] Furthermore, gum arabic, gelatin and chitosan are added to the capsule solution, and the mass ratio of gum arabic, gelatin and chitosan is (1-2): (1-2): (1-2), preferably 1:1:1. A certain proportion of gum arabic, gelatin and chitosan is added to the capsule solution to modify the electrophoretic display microcapsules, which can change the surface gloss and light transmittance. Finally, capsules with a particle size of 20 μm to 30 μm are selected as the electrophoretic display microcapsules of the flexible electronic paper of the present invention, which can effectively improve the overall bending flexibility and clarity of the color display FPL.
[0011] Furthermore, the color-developing particles include black color-developing particles and white color-developing particles, the black color-developing particles are carbon black, and the white color-developing particles are titanium dioxide.
[0012] Furthermore, the capsule solution is tetrachloroethylene or styrene.
[0013] Furthermore, the transparent conductive electrode is a TIO conductive film.
[0014] Furthermore, the PI film is selected from CPI (Colorless PI) film. Traditional PI film has limited toughness and bending degree, and is yellow-brown, which will affect the foldability and display effect of flexible electronic paper, while CPI film has stronger toughness, better bending property, and is a transparent film. Using CPI film as a flexible circuit board can significantly improve the bending property and display effect of flexible electronic paper.
[0015] Furthermore, the bending radius of the flexible electronic paper is equal to or less than 2 cm.
[0016] Furthermore, the thickness of the PS film is 120-130 μm, preferably 125 μm. The use of a PS film with a thickness in the above range can reduce the thickness of the flexible electronic paper and increase its flexibility, while having no adverse effects on other materials and also playing a protective role.
[0017] Furthermore, the hardness of the EC glue is Shor D 70-78, and the tensile modulus is 1800-2000; preferably, the hardness of the EC glue is Shor D 75, and the tensile modulus is 1920. Controlling the hardness and tensile modulus of the EC glue within the above range can reduce the cohesive force between the flexible electronic paper materials and enhance the overall flexibility of the flexible electronic paper.
[0018] A second aspect of the present invention provides a method for preparing the flexible electronic paper as described in the first aspect, comprising the following steps:
[0019] S1, screening out particles with a diameter of 200nm±20nm as color-developing particles through a rotating wheel;
[0020] S2, placing the color-developing particles into the capsule solution, adjusting the rotating wheel speed, and screening out electrophoresis display microcapsules with a particle size of 20 μm to 30 μm;
[0021] S3, injecting the electrophoretic display microcapsules into a transparent conductive electrode to form a color-developing FPL (electronic paper ink film);
[0022] S4, cutting the color-developing FPL (electronic paper ink film) to a desired size to prepare a flexible electronic paper (EPD), comprising the following steps: glass cutting, FPL attachment, IC Bonding, FPC Bonding, PS attachment, PI separation, and FPC serving as a bridge connecting the flexible electronic paper (EPD) and the motherboard.
[0023] Furthermore, in step S2, after the color-developing particles are placed in the capsule solution, gum arabic, gelatin and chitosan are added to the capsule solution in proportion, and then the rotating wheel speed is adjusted to screen out electrophoresis display microcapsules with a particle size of 20 μm to 30 μm.
[0024] Furthermore, in step S2, the rotating speed of the rotor is 200 to 300 revolutions per second.
[0025] Further, in step S4, the preparation of the flexible electronic paper (EPD) includes the following steps:
[0026] (1) Glass cutting: Cutting the Q panel (TFT) into small pieces of TFT, wherein the TFT includes a TFT body and a PI film;
[0027] (2) FPL attachment: attaching the FPL to the upper surface of the TFT;
[0028] (3) IC Bonding: Press the IC to the corresponding pin position of the TFT;
[0029] (4) FPC Bonding: Press the FPC to the corresponding pin position of the TFT;
[0030] (5) PS attachment: attach the PS film to the upper surface of the FPL;
[0031] (6) PI separation: The TFT body and the PI layer are separated by laser.
[0032] (7) PS attachment: Attach the PS film to the lower surface of the PI film.
[0033] Further, in step S4, PS attachment is performed by hot-melt PS hot rolling, including the following steps: placing TFT on one side and hot-melt PS film on the other side, and rolling.
[0034] Optionally, the temperature of the platform on the side where the TFT is placed is 35-38°C, preferably 36°C; the temperature of the platform on the side where the hot-melt PS film is placed is 105-115°C, preferably 110°C.
[0035] Optionally, during rolling, the roller speed is 8-12 mm / s, preferably 10 mm / s.
[0036] A third aspect of the present invention provides an application of the flexible electronic paper described in the first aspect and / or the flexible electronic paper prepared by the method described in the second aspect in the field of electronic products or display screens.
[0037] As described above, the flexible electronic paper of the present invention and its preparation and application have the following beneficial effects:
[0038] The present invention mainly improves the material properties of flexible electronic paper by controlling the particle sizes of color-developing particles and electrophoretic display microcapsules, adapting a certain proportion of gum arabic, gelatin and chitosan in the capsule solution, controlling the material selection of PI film, controlling the thickness of PS film, and controlling the hardness and tensile modulus of EC glue. At the same time, with the new preparation process, the flexibility, bendability, clarity and display effect of flexible electronic paper are further improved, the thickness is reduced, and a flexible display with a bending radius equal to or less than 2 cm is achieved, so that it can be better and more widely used in current low-power wireless display products such as smart wearables and smart military industry.
[0039] The present invention adopts a hot-melt PS hot rolling method to prepare flexible electronic paper. When the hot roller is rolling the PS process, the sealing of the flexible electronic paper can be achieved simultaneously, thereby eliminating the step of using an EC adhesive material to attach a PS film. Compared with the traditional process, the process of the present invention is used to produce and prepare flexible electronic paper, which can further reduce the cohesive force between the materials, and the prepared flexible electronic paper has lighter, thinner and softer characteristics; in addition, the hot-melt PS hot rolling method can further improve the influence of the materials on the PI film, thereby reducing the damage to the TFT circuit on the PI film due to bending. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Figure 1 It is a structural diagram of an existing flexible electronic paper display;
[0041] Figure 2 This is a structural diagram of the flexible electronic paper display screen of the present invention;
[0042] Figure 3 This is a bending display diagram of the flexible electronic paper of the present invention. DETAILED DESCRIPTION
[0043] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0044] Based on the shortcomings of existing flexible electronic paper, the present invention specifically optimizes and improves the materials used in existing flexible electronic paper, further optimizes the materials and preparation process of flexible electronic paper, and proposes a design scheme for flexible electronic paper with a bending radius equal to or less than 2 cm.
[0045] like Figure 2 As shown, the flexible electronic paper provided by the present invention includes, from bottom to top, a PS film (polystyrene film), a color-developing FPL (electronic paper ink film), a PI film (polyimide film), and a PS film (polystyrene film) laminated in sequence, wherein the PS film is laminated together with the FPL and PI films by a hot melt process, and the FPL and PI films are laminated together by EC glue (fast ear glue); the flexible electronic paper also includes an IC (integrated circuit chip) and an FPC (flexible circuit board), and the IC and FPC are fixed on the PI film by IC reinforcing glue and UV glue (ultraviolet curing glue), respectively. Among them, the color-developing particles are used to characterize the display color and display clarity of the flexible electronic paper, the electrophoretic display microcapsules are used to characterize the display clarity and display transparency of the flexible electronic paper, the sealant EC glue is used to characterize the sealing degree and bending degree of the flexible electronic paper, the PS film is used to characterize the bending degree of the flexible electronic paper, and the PI film is used to characterize the bending degree and transparent display degree of the flexible electronic paper. The hot-melt PS film does not require EC glue coating.
[0046] In another embodiment of the present invention, the color-developing FPL is formed by injecting electrophoretic display microcapsules into transparent conductive electrodes, and the electrophoretic display microcapsules are obtained by placing color-developing particles into a capsule solution and screening with a rotating wheel. Specifically, the transparent conductive electrode is a TIO conductive film, and the capsule solution is tetrachloroethylene or styrene; the color-developing particles include black color-developing particles and white color-developing particles, the black color-developing particles are carbon black, and the white color-developing particles are titanium dioxide.
[0047] In another embodiment of the present invention, the diameter of the color-developing particles is 200nm±20nm, and the electrophoresis display microcapsules are spherical with a particle size of 20μm to 30μm. In order to achieve better flexibility, the present invention optimizes and screens the particle size and morphology in the color-developing FPL. Using particles with a diameter of 200nm±20nm as color-developing particles can enhance display clarity and improve uniformity; the electrophoresis display microcapsules are spherical structures, which can increase the bending degree of the capsules.
[0048] In another embodiment of the present invention, gum arabic, gelatin and chitosan are added to the capsule solution, and the mass ratio of gum arabic, gelatin and chitosan is (1-2): (1-2): (1-2), preferably 1:1:1. A certain proportion of gum arabic, gelatin and chitosan is added to the capsule solution to modify the electrophoretic display microcapsules, which can change the surface gloss and light transmittance. Finally, capsules with a particle size of 20 μm to 30 μm are selected as the electrophoretic display microcapsules of the flexible electronic paper of the present invention, which can effectively improve the overall bending flexibility and clarity of the color display FPL.
[0049] In another embodiment of the present invention, the PI film is selected from CPI (Colorless PI) film, and the CPI film has a thickness of 1 to 4 mm, preferably a CPI film with a thickness of 3 mm. The traditional PI film has limited toughness and bending degree, and is yellow-brown, which will affect the foldability and display effect of the flexible electronic paper. The CPI film has stronger toughness, better bending, and is a transparent film. Using CPI film as a flexible circuit board can significantly improve the bending and display effect of the flexible electronic paper.
[0050] In another embodiment of the present invention, the thickness of the PS film is 120-130 μm, preferably 125 μm. The use of a PS film with a thickness in the above range can reduce the thickness of the flexible electronic paper and increase its flexibility, while having no adverse effects on other materials and also playing a protective role.
[0051] In another embodiment of the present invention, the hardness of the EC glue is Shor D 70-78, and the tensile modulus is 1800-2000; preferably, the hardness of the EC glue is Shor D 75, and the tensile modulus is 1920. Controlling the hardness and tensile modulus of the EC glue within the above range can reduce the cohesive force between the flexible electronic paper materials and enhance the overall flexibility of the flexible electronic paper.
[0052] The method for preparing the flexible electronic paper provided by the present invention comprises the following steps:
[0053] S1. Use a rotating wheel to select particles with a diameter of 200nm±20nm as color-developing particles.
[0054] S2. Put the color-developing particles into the capsule solution, adjust the rotating wheel speed to 200-300 rpm, and screen out electrophoresis display microcapsules with a particle size of 20 μm-30 μm.
[0055] S3, injecting the electrophoretic display microcapsules into the transparent conductive electrode to form a color-developing FPL (electronic paper ink film);
[0056] S4, cutting the color-developing FPL (electronic paper ink film) to the required size to prepare the flexible electronic paper (EPD), including the following steps: glass cutting, FPL attachment, IC bonding, FPC bonding, PS attachment, PI separation, FPC as a bridge connecting the flexible electronic paper (EPD) and the motherboard. Figure 2 The flexible electronic paper structure shown in the figure, the preparation process of the flexible electronic paper is as follows:
[0057] (1) Glass cutting: Cut the Q panel (TFT) into small pieces of TFT, which includes the TFT body and PI film;
[0058] (2) FPL attachment: attaching the FPL to the upper surface of the TFT;
[0059] (3) IC Bonding: Press the IC to the corresponding pin position of the TFT;
[0060] (4) FPC Bonding: Press the FPC to the corresponding pin position of the TFT;
[0061] (5) PS attachment: attach the PS film to the upper surface of the FPL;
[0062] (6) PI separation: The TFT body and the PI layer are separated by laser.
[0063] (7) PS attachment: attach the PS film to the lower surface of the PI film;
[0064] Among them, PS attachment adopts hot-melt PS hot rolling method, including the following steps: placing TFT on one side, with the platform temperature at 35-38°C; placing hot-melt PS on one side, with the platform temperature at 105-115°C, and rolling, with the roller speed of 8-12mm / s.
[0065] In another embodiment of the present invention, in step S2, after the color-developing particles are placed in the capsule solution, gum arabic, gelatin and chitosan are added to the capsule solution in proportion, and the mass ratio of gum arabic, gelatin and chitosan is (1-2): (1-2): (1-2), preferably 1:1:1; then the rotating wheel speed is adjusted to screen out electrophoretic display microcapsules with a particle size of 20μm to 30μm.
[0066] The technical solution of the present invention is further described in detail below in conjunction with specific embodiments.
[0067] Example 1
[0068] In order to achieve better flexibility, the particle size, morphology, etc. of the color-developing particles and electrophoretic display microcapsules in the FPL are optimized and screened in this embodiment.
[0069] The color-developing particles used in FPL in current flexible electronic paper are generally 200 to 300 nm in size, and the electrophoresis display microcapsules are 50 to 100 μm.
[0070] In order to achieve better flexibility, faster refresh rate and better display effect, the present embodiment miniaturizes the color-developing particles and modifies the electrophoretic display microcapsules.
[0071] The size of the color-developing particles is adjusted to about 200nm, and particles of 200nm±20nm are specifically selected as color-developing particles to enhance display clarity and improve uniformity. At the same time, the electrophoretic display microcapsules in the present invention adopt a spherical design to increase the bending degree of the capsules. At the same time, capsules with a particle size of 20μm to 30μm are prepared by adjusting the rotating speed of the rotor, and the capsules are further modified. The capsule solution is designed to be adapted to a mass ratio of (1 to 2): (1 to 2): (1 to 2) of gum arabic, gum arabic and chitosan, which can effectively improve the surface gloss and light transmittance of the capsules, and enhance the overall bending flexibility and clarity of the FPL. Among them, the optimal ratio of gum arabic, gum arabic and chitosan is 1:1:1.
[0072] Example 2
[0073] For the PS film, this embodiment verifies the design of a thinner material, reduces the thickness of the PS film from 256 μm to 125 μm, and performs combined verification.
[0074] Experiments have shown that a 125 μm thick PS film can reduce the thickness of flexible electronic paper and increase its flexibility, while having no adverse effects on other materials and also playing a protective role. Therefore, in order to improve the flexibility of flexible electronic paper and ensure the protective effect, the thickness of the PS film is controlled within the range of 120 to 130 μm in the present invention.
[0075] Example 3
[0076] In this embodiment, the hardness and shrinkage of EC glue are improved and verified. The results are shown in Table 1.
[0077] Experiments have shown that when the hardness of the EC glue is lower than 60, the flexibility of the flexible electronic paper is improved, but the sealing effect is poor, and the EC glue cannot play a sealing effect; when the hardness of the EC glue is reduced to Shor D 75 and the tensile modulus is adjusted to 1920, the flexibility of the sealing ring of the flexible electronic paper is improved to a certain extent, and when the RA reliability verification is performed at the same time, the sealing effect maintains a relatively good performance. Therefore, the present invention controls the hardness and tensile modulus of the EC glue within the range of Shor D 70-78 and 1800-2000, respectively, which can effectively reduce the cohesive force between the flexible electronic paper materials and enhance the overall flexibility of the flexible electronic paper.
[0078] Table 1. Comparison of properties of new and old EC materials
[0079]
[0080] Example 4
[0081] In the process of preparing flexible electronic paper, PS attachment adopts hot-melt PS hot rolling method, and the specific preparation process is as follows:
[0082] (1) Glass cutting: Cut the Q panel (TFT) into small pieces of TFT, which includes the TFT body and PI film.
[0083] (2) FPL attachment: Apply EC glue on the upper surface of TFT, attach FPL to the upper surface of TFT, and cure it.
[0084] (3) IC Bonding: Apply IC reinforcing glue on the TFT, press the IC to the corresponding pin position of the TFT, and cure it.
[0085] (4) FPC Bonding: Apply UV glue on the TFT, press the FPC to the corresponding pin position of the TFT, and cure it.
[0086] (5) PS attachment: Use hot melt PS hot rolling method to attach the PS film to the upper surface of FPL, as follows:
[0087] TFT is placed on one side with a platform temperature of 36°C; hot melt PS is placed on the other side with a platform temperature of 110°C, and rolling is performed with a roller speed of 10mm / s.
[0088] (6) PI separation: The TFT body and the PI layer are peeled off by laser.
[0089] (7) PS attachment: The PS film is attached to the lower surface of the PI film by hot-melt PS hot rolling method, as follows:
[0090] TFT is placed on one side with a platform temperature of 36°C; hot melt PS is placed on the other side with a platform temperature of 110°C, and rolling is performed with a roller speed of 10mm / s.
[0091] In the traditional process, EC glue is required for PS attachment, and EC glue coating and curing are required, and the edge sealing around the electronic paper can be completed in two steps; while in the new process provided by the present invention, EC glue does not need to be coated, hot-melt PS is attached, and the edge sealing around the electronic paper can be completed in one step. At the same time, compared with the traditional process, the production and preparation of flexible electronic paper using the process of the present invention can further reduce the cohesive force between the materials, so that the prepared flexible electronic paper has lighter, thinner and softer characteristics, and can further improve the influence of the materials on the PI film, thereby reducing the damage to the TFT circuit on the PI film due to bending.
[0092] Example 5
[0093] Compared with the existing flexible electronic paper, the PI film in the flexible electronic paper of this embodiment uses CPI (ColorlessPI) film as the PI circuit cover. The traditional PI film has limited toughness and bending degree, and is yellow-brown, which affects the foldability and display effect of the flexible electronic paper. Compared with the traditional PI film, the CPI film has stronger toughness, better bending, and is a transparent film. Using CPI film as a flexible circuit board can significantly improve the bending and display effect of the flexible electronic paper.
[0094] Example 6
[0095] The color-developing FPL prepared by the color-developing particles and color-developing capsule particles in Example 1, the PS film with a thickness of 125 μm in Example 2, the EC glue with a hardness of Shor D 75 and a tensile modulus of 1920 in Example 3, and the CPI film with a thickness of 3 mm are used. According to the hot-melt PS hot rolling method in Example 4, flexible electronic paper is prepared. The specific preparation process is as follows:
[0096] S1. Use a rotating wheel to select particles with a diameter of 200nm±20nm as color-developing particles.
[0097] S2. Put the color-developing particles into the capsule solution, add gum arabic, gelatin and chitosan in a mass ratio of 1:1:1 into the capsule solution, adjust the rotating wheel speed to 300 rpm, and screen out electrophoresis display microcapsules with a particle size of 20 μm to 30 μm.
[0098] S3, injecting the electrophoretic display microcapsules into a transparent conductive electrode to form a color-developing FPL (electronic paper ink film).
[0099] S4, cutting the color-developing FPL (electronic paper ink film) into a desired size to prepare a flexible electronic paper (EPD), the steps are as follows:
[0100] (1) Glass cutting: Cut the Q panel (TFT) into small pieces of TFT, which includes the TFT body and PI film.
[0101] (2) FPL attachment: Apply EC glue on the upper surface of TFT, attach FPL to the upper surface of TFT, and cure it.
[0102] (3) IC Bonding: Apply IC reinforcing glue on the TFT, press the IC to the corresponding pin position of the TFT, and cure it.
[0103] (4) FPC Bonding: Apply UV glue on the TFT, press the FPC to the corresponding pin position of the TFT, and cure it.
[0104] (5) PS attachment: Use hot melt PS hot rolling method to attach the PS film to the upper surface of FPL, as follows:
[0105] TFT is placed on one side with a platform temperature of 36°C; hot melt PS is placed on the other side with a platform temperature of 110°C, and rolling is performed with a roller speed of 10mm / s.
[0106] (6) PI separation: The TFT body and the PI layer are peeled off by laser.
[0107] (7) PS attachment: The PS film is attached to the lower surface of the PI film by hot-melt PS hot rolling method, as follows:
[0108] TFT is placed on one side with a platform temperature of 36°C; hot melt PS is placed on the other side with a platform temperature of 110°C, and rolling is performed with a roller speed of 10mm / s.
[0109] The bending display diagram of the flexible electronic paper prepared in this embodiment is as follows: Figure 3 As shown by Figure 3 It can be seen that the flexible electronic paper prepared in this embodiment can achieve a bending degree of 2 mm in radius.
[0110] Example 7
[0111] A PS film with a thickness of 120 μm, an EC glue with a hardness of Shor D 70 and a tensile modulus of 1800, and a CPI film with a thickness of 1 mm were used to prepare flexible electronic paper according to the hot-melt PS hot rolling method. The specific preparation process is as follows:
[0112] S1. Use a rotating wheel to select particles with a diameter of 200nm±20nm as color-developing particles.
[0113] S2. Put the color-developing particles into the capsule solution, add gum arabic, gelatin and chitosan in a mass ratio of 1:2:2 into the capsule solution, adjust the rotating wheel speed to 200 rpm, and screen out electrophoresis display microcapsules with a particle size of 20 μm to 30 μm.
[0114] S3, injecting the electrophoretic display microcapsules into a transparent conductive electrode to form a color-developing FPL (electronic paper ink film).
[0115] S4, cutting the color-developing FPL (electronic paper ink film) into a desired size to prepare a flexible electronic paper (EPD), the steps are as follows:
[0116] (1) Glass cutting: Cut the Q panel (TFT) into small pieces of TFT, which includes the TFT body and PI film.
[0117] (2) FPL attachment: Apply EC glue on the upper surface of TFT, attach FPL to the upper surface of TFT, and cure it.
[0118] (3) IC Bonding: Apply IC reinforcing glue on the TFT, press the IC to the corresponding pin position of the TFT, and cure it.
[0119] (4) FPC Bonding: Apply UV glue on the TFT, press the FPC to the corresponding pin position of the TFT, and cure it.
[0120] (5) PS attachment: Use hot melt PS hot rolling method to attach the PS film to the upper surface of FPL, as follows:
[0121] TFT is placed on one side with a platform temperature of 35°C; hot melt PS is placed on the other side with a platform temperature of 105°C, and rolling is performed with a roller speed of 8mm / s.
[0122] (6) PI separation: The TFT body and the PI layer are peeled off by laser.
[0123] (7) PS attachment: The PS film is attached to the lower surface of the PI film by hot-melt PS hot rolling method, as follows:
[0124] TFT is placed on one side with a platform temperature of 35°C; hot melt PS is placed on the other side with a platform temperature of 105°C, and rolling is performed with a roller speed of 8mm / s.
[0125] The flexible electronic paper produced in this embodiment can achieve a bending degree of 1.6 mm in radius.
[0126] Example 8
[0127] A PS film with a thickness of 130 μm, an EC glue with a hardness of Shor D 78 and a tensile modulus of 2000, and a CPI film with a thickness of 4 mm were used to prepare flexible electronic paper according to the hot-melt PS hot rolling method. The specific preparation process is as follows:
[0128] S1. Use a rotating wheel to select particles with a diameter of 200nm±20nm as color-developing particles.
[0129] S2. Put the color-developing particles into the capsule solution, add gum arabic, gelatin and chitosan in a mass ratio of 1:2:2 into the capsule solution, adjust the rotating wheel speed to 200 rpm, and screen out electrophoresis display microcapsules with a particle size of 20 μm to 30 μm.
[0130] S3, injecting the electrophoretic display microcapsules into a transparent conductive electrode to form a color-developing FPL (electronic paper ink film).
[0131] S4, cutting the color-developing FPL (electronic paper ink film) into a desired size to prepare a flexible electronic paper (EPD), the steps are as follows:
[0132] (1) Glass cutting: Cut the Q panel (TFT) into small pieces of TFT, which includes the TFT body and PI film.
[0133] (2) FPL attachment: Apply EC glue on the upper surface of TFT, attach FPL to the upper surface of TFT, and cure it.
[0134] (3) IC Bonding: Apply IC reinforcing glue on the TFT, press the IC to the corresponding pin position of the TFT, and cure it.
[0135] (4) FPC Bonding: Apply UV glue on the TFT, press the FPC to the corresponding pin position of the TFT, and cure it.
[0136] (5) PS attachment: Use hot melt PS hot rolling method to attach the PS film to the upper surface of FPL, as follows:
[0137] TFT is placed on one side with a platform temperature of 38°C; hot melt PS is placed on the other side with a platform temperature of 115°C, and rolling is performed with a roller speed of 12mm / s.
[0138] (6) PI separation: The TFT body and the PI layer are peeled off by laser.
[0139] (7) PS attachment: The PS film is attached to the lower surface of the PI film by hot-melt PS hot rolling method, as follows:
[0140] TFT is placed on one side with a platform temperature of 38°C; hot melt PS is placed on the other side with a platform temperature of 115°C, and rolling is performed with a roller speed of 12mm / s.
[0141] The flexible electronic paper produced in this embodiment can achieve a bending degree of 2 mm in radius.
[0142] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A flexible electronic paper, comprising, from bottom to top, a PS film, a color-developing FPL, a PI film, a PS film, and also an IC and an FPC, wherein the IC and the FPC are fixed on the PI film by IC reinforcing glue and UV glue, respectively. It is characterized in that The PS film is bonded to the FPL and PI films by a hot melt process, and the FPL and PI films are bonded to each other by EC glue; The color-developing FPL is formed by injecting an electrophoretic display microcapsule into a transparent conductive electrode. The electrophoretic display microcapsule is obtained by placing color-developing particles into a capsule solution and screening with a rotating wheel, and the rotating wheel speed is 200 to 300 revolutions per second. The diameter of the color-developing particles is 200 nm ± 20 nm, and the electrophoretic display microcapsule is a sphere with a particle size of 20 μm to 30 μm. The capsule solution contains gum arabic, gelatin and chitosan, and the mass ratio of gum arabic, gelatin and chitosan is (1-2): (1-2): (1-2); the capsule solution is tetrachloroethylene or styrene; The PI film is selected from CPI film; The thickness of the PS film is 120-130 μm; The EC glue has a hardness of Shor D 70-78 and a tensile modulus of 1800-2000; The bending radius of the flexible electronic paper is equal to or less than 2 cm.
2. The flexible electronic paper according to claim 1, Features: The color-developing particles include black color-developing particles and white color-developing particles; And / or, the transparent conductive electrode is a TIO conductive film.
3. The method for preparing the flexible electronic paper according to any one of claims 1 to 2, It is characterized in that The steps include: S1, screening particles with a diameter of 200nm±20nm as color-developing particles through a rotating wheel; S2, placing the color-developing particles into the capsule solution, adjusting the rotating wheel speed to 200-300 rpm, and screening out electrophoretic display microcapsules with a particle size of 20 μm-30 μm; S3, injecting the electrophoretic display microcapsules into a transparent conductive electrode to form a color-developing FPL; S4, cutting the color-developing FPL to a desired size to prepare flexible electronic paper, including the following steps: glass cutting, FPL attachment, IC Bonding, FPC Bonding, PS attachment, PI separation, and FPC serving as a bridge connecting the flexible electronic paper and the motherboard.
4. The preparation method according to claim 3, Features: In step S2, after the color-developing particles are placed in the capsule solution, gum arabic, gelatin and chitosan are added to the capsule solution in proportion, and then the rotating wheel speed is adjusted to screen out electrophoresis display microcapsules with a particle size of 20 μm to 30 μm.
5. The preparation method according to claim 3, Features: In step S4, PS attachment is performed by hot-melt PS hot rolling, which includes the following steps: (1) Glass cutting: Cutting the Q panel TFT into small pieces of TFT, wherein the TFT includes a TFT body and a PI film; (2) FPL attachment: attaching the FPL to the upper surface of the TFT; (3) IC Bonding: Press the IC to the corresponding pin position of the TFT; (4) FPC Bonding: Press the FPC to the corresponding pin position of the TFT; (5) PS attachment: attach the PS film to the upper surface of the FPL; (6) PI separation: The TFT body and the PI layer are separated by laser. (7) PS attachment: Attach the PS film to the lower surface of the PI film.
6. The preparation method according to claim 3, Features: In step S4, PS attachment adopts hot-melt PS hot rolling method, including the following steps: placing TFT on one side and hot-melt PS film on the other side, and rolling.
7. Application of the flexible electronic paper according to any one of claims 1 to 2 and / or the flexible electronic paper prepared according to any one of claims 3 to 6 in the field of electronic products or display screens.