A high-extension ironing wire and its preparation method and application
By setting alternating gaps on the sewing thread and filling the hot melt thread, the problem of sewing thread not getting longer after high temperature ironing in the prior art is solved, and the sewing thread extends synchronously with the fabric and is smooth and wrinkle-free clothing effect.
Patent Information
- Application Number
- CN202111344622.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-11-15
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2041-11-15
AI Technical Summary
The existing clothing fabrics become longer after ironing at high temperatures, while the sewing threads do not grow longer, resulting in wrinkles and unevenness in the clothing, affecting the beauty.
Highly extended sewing thread made of polyester staple fiber, polyester silk or nylon material, forms a circular sewing thread by twisting or unifying thread, and alternate gaps are set axially, and hot melt thread is filled at the gap to form " The cross-section of the bow" shape ensures that the wire can extend synchronously during high temperature ironing.
The sewing thread extends synchronously with the fabric after high-temperature ironing, avoiding wrinkles and unevenness of the clothing and improving the aesthetics of the clothing.
Smart Images

Figure CN113981582B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an ironing high-extension wire and a preparation method and application thereof, belonging to the technical field of clothing ironing modification. Background Art
[0002] Currently, many clothing fabrics on the market will become longer after high-temperature ironing, while the sewing threads on the market do not change much after ironing. As a result, the fabrics become longer, but the sewing threads do not become longer, resulting in wrinkles, unevenness, and unsightly appearance of the clothing after ironing. Summary of the invention
[0003] The purpose of the present invention is to overcome the shortcomings of the prior art and to propose an ironing high-extension thread and a preparation method and application thereof. The extension thread is used for sewing clothes. The extension thread can become longer after high-temperature ironing and has good sewing performance.
[0004] The technical solution of the present invention is:
[0005] An ironing high-extension thread, the material of the ironing high-extension thread is polyester staple fiber, polyester silk, nylon, the ironing high-extension thread is a circular sewing thread formed by twisting polyester staple fiber, the ironing high-extension thread is a circular sewing thread formed by paralleling polyester silk, the ironing high-extension thread is a circular sewing thread formed by paralleling nylon after spinning, the circular sewing thread has left and right alternating notches along the axial direction, the left and right alternating notches are respectively called left notches and right notches, the opening direction of the left notch faces left, and the opening direction of the right notch faces right, that is, the cross section of the sewing thread after the left notch and the right notch are opened is a "bow" shape;
[0006] The left notch is formed by chemicals or laser etching;
[0007] The right notch is formed by chemicals or laser etching;
[0008] Assume that the radius of the circular sewing line is r; the distance between the left notch and the right notch (the distance between the bottom end of the adjacent left notch and the top end of the right notch or the distance between the top end of the adjacent left notch and the bottom end of the right notch) is r;
[0009] The length of the left notch is r, and the height of the left notch is r;
[0010] The length of the right notch is r, and the height of the right notch is r;
[0011] The left notch is filled with a hot melt line;
[0012] The right notch is filled with a hot melt line;
[0013] The hot melting temperature of the hot melt line is 70°C.
[0014] A method for preparing an ironing high-extension wire, the method comprising the steps of:
[0015] In the first step, the polyester staple fibers are twisted to form a circular sewing thread;
[0016] In the second step, the circular sewing line formed in the first step is provided with left and right alternate notches along the axial direction to form a left notch and a right notch;
[0017] The third step is to fill the left and right notches formed in the second step with hot melt lines to obtain ironing high extension lines.
[0018] An application of an ironing high-extension thread, comprising the steps of: using the prepared ironing high-extension thread to sew fabric clothing, the hot melt thread melts when the fabric clothing is ironed at 70-100°C, and the ironing high-extension thread extends synchronously with the fabric clothing as the fabric clothing extends, so that the clothing is flat and wrinkle-free.
[0019] Beneficial Effects
[0020] After the garment fabric is sewn, the ironing high-extension line of the present invention will extend synchronously with the garment fabric as the garment fabric extends after being ironed at high temperature, so that the garment is smooth, wrinkle-free, smooth and beautiful. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a schematic structural diagram of the ironing high-extension wire of the present invention. DETAILED DESCRIPTION
[0022] The present invention will be further described below in conjunction with the accompanying drawings and embodiments.
[0023] Example 1
[0024] like Figure 1 As shown, an ironing high-extension thread is made of polyester staple fibers. The ironing high-extension thread is a circular sewing thread formed by twisting the polyester staple fibers. The circular sewing thread has left and right alternating notches along the axial direction. The left and right alternating notches are respectively called left notches and right notches. The opening direction of the left notch faces left, and the opening direction of the right notch faces right, that is, the cross section of the sewing thread after the left notch and the right notch are opened is a "bow" shape;
[0025] The left notch is formed by chemical corrosion;
[0026] The right side notch is formed by chemical corrosion;
[0027] Assume that the radius of the circular sewing line is r; the distance between the left notch and the right notch (the distance between the bottom of the left notch and the top of the right notch) is r;
[0028] The length of the left notch is r, and the height of the left notch is r;
[0029] The length of the right notch is r, and the height of the right notch is r;
[0030] The left notch is filled with a hot melt line;
[0031] The right notch is filled with a hot melt line;
[0032] The hot melting temperature of the hot melt line is 70°C.
[0033] A method for preparing an ironing high-extension wire, the method comprising the steps of:
[0034] In the first step, the polyester staple fibers are twisted to form a circular sewing thread;
[0035] In the second step, the circular sewing line formed in the first step is provided with left and right alternate notches along the axial direction to form a left notch and a right notch;
[0036] The third step is to fill the left and right notches formed in the second step with hot melt lines to obtain ironing high extension lines.
[0037] An application of an ironing high-extension thread, comprising the steps of: using the prepared ironing high-extension thread to sew fabric clothing, the hot melt thread melts when the fabric clothing is ironed at 80°C, the ironing high-extension thread extends synchronously with the fabric clothing as the fabric clothing extends, and the clothing is flat and wrinkle-free.
[0038] Example 2
[0039] An ironing high-extension thread, the material of the ironing high-extension thread is polyester silk, the ironing high-extension thread is a circular sewing thread formed by paralleling polyester silk, the circular sewing thread has left and right alternating notches along the axial direction, the left and right alternating notches are respectively called left notches and right notches, the opening direction of the left notch faces left, and the opening direction of the right notch faces right, that is, the cross section of the sewing thread after the left notch and the right notch are opened is a "bow" shape;
[0040] The left notch is formed by laser etching;
[0041] The right notch is formed by laser etching;
[0042] Assume that the radius of the circular sewing line is r; the distance between the left notch and the right notch (the distance between the bottom of the left notch and the top of the right notch) is r;
[0043] The length of the left notch is r, and the height of the left notch is r;
[0044] The length of the right notch is r, and the height of the right notch is r;
[0045] The left notch is filled with a hot melt line;
[0046] The right notch is filled with a hot melt line;
[0047] The hot melting temperature of the hot melt line is 70°C.
[0048] A method for preparing an ironing high-extension wire, the method comprising the steps of:
[0049] In the first step, the polyester staple fibers are twisted to form a circular sewing thread;
[0050] In the second step, the circular sewing line formed in the first step is provided with left and right alternate notches along the axial direction to form a left notch and a right notch;
[0051] The third step is to fill the left and right notches formed in the second step with hot melt lines to obtain ironing high extension lines.
[0052] An application of an ironing high-extension thread, comprising the steps of: using the prepared ironing high-extension thread to sew fabric clothing, the hot melt thread melts when the fabric clothing is ironed at 85°C, the ironing high-extension thread extends synchronously with the fabric clothing as the fabric clothing extends, and the clothing is flat and wrinkle-free.
[0053] Example 3
[0054] An ironing high-extension thread, the material of the ironing high-extension thread is nylon, the ironing high-extension thread is a circular sewing thread formed by spinning and paralleling nylon, the circular sewing thread has left and right alternating notches along the axial direction, the left and right alternating notches are respectively called left notches and right notches, the opening direction of the left notch faces left, and the opening direction of the right notch faces right, that is, the cross section of the sewing thread after the left notch and the right notch are opened is a "bow" shape;
[0055] The left notch is formed by chemicals or laser etching;
[0056] The right notch is formed by chemicals or laser etching;
[0057] Assume that the radius of the circular sewing line is r; the distance between the left notch and the right notch (the distance between the bottom of the left notch and the top of the right notch) is r;
[0058] The length of the left notch is r, and the height of the left notch is r;
[0059] The length of the right notch is r, and the height of the right notch is r;
[0060] The left notch is filled with a hot melt line;
[0061] The right notch is filled with a hot melt line;
[0062] The hot melting temperature of the hot melt line is 70°C.
[0063] A method for preparing an ironing high-extension wire, the method comprising the steps of:
[0064] In the first step, the polyester staple fibers are twisted to form a circular sewing thread;
[0065] In the second step, the circular sewing line formed in the first step is provided with left and right alternate notches along the axial direction to form a left notch and a right notch;
[0066] The third step is to fill the left and right notches formed in the second step with hot melt lines to obtain ironing high extension lines.
[0067] An application of an ironing high-extension thread, comprising the steps of: using the prepared ironing high-extension thread to sew fabric clothing, the hot melt thread melts when the fabric clothing is ironed at 90°C, the ironing high-extension thread extends synchronously with the fabric clothing as the fabric clothing extends, and the clothing is flat and wrinkle-free.
[0068] The contents not described in detail in this specification belong to the prior art known to professional and technical personnel in this field.
[0069] The above description shows and describes several preferred embodiments of the present invention, but as mentioned above, it should be understood that the present invention is not limited to the form disclosed herein, and should not be regarded as excluding other embodiments, but can be used in various other combinations, modifications and environments, and can be modified within the scope of the invention concept described herein through the above teachings or the technology or knowledge of the relevant field. Changes and variations made by those skilled in the art do not depart from the spirit and scope of the present invention, and should be within the scope of protection of the claims attached to the present invention.
Claims
1. An ironing high extension line, characterized in that: The ironing high extension line is a circular sewing line with left and right alternating notches along the axial direction; the left and right alternating notches are respectively called left notches and right notches, the opening direction of the left notches is leftward, and the opening direction of the right notches is rightward, that is, the cross section of the sewing line after the left notches and the right notches are opened is a "bow" shape; The length of the left notch is consistent with the radius of the circular sewing line, the height of the left notch is consistent with the radius of the circular sewing line, the length of the right notch is consistent with the radius of the circular sewing line, the height of the right notch is consistent with the radius of the circular sewing line, and the distance between the bottom end of the adjacent left notch and the top end of the right notch is consistent with the radius of the circular sewing line; The left notch is formed by chemicals or laser etching; The right notch is formed by chemicals or laser etching; The left notch is filled with a hot melt line; The right notch is filled with a hot melt line; The hot melt temperature of the hot melt line is 70°C. Sewing fabric garments using the prepared iron-on high-extension thread; When the fabric garment is ironed at 70-100°C, the hot melt line melts, and the ironing high extension line extends synchronously with the fabric garment as the fabric garment extends.
2. The high-extension ironing wire according to claim 1, characterized in that: The material of the ironing high-extension thread is polyester staple fiber, polyester silk or nylon.
3. The high-extension ironing wire according to claim 2, characterized in that: When the material of the ironing high-extension thread is polyester staple fiber, the ironing high-extension thread is a circular sewing thread formed by twisting the polyester staple fiber.
4. The high-extension ironing wire according to claim 2, characterized in that: When the material of the ironing high-extension line is polyester silk, the ironing high-extension line is a circular sewing line formed by parallel lines of polyester silk.
5. The high-extension ironing wire according to claim 2, characterized in that: When the material of the ironing high-extension line is nylon, the ironing high-extension line is a circular sewing line formed by spinning and doubling the nylon.
6. A method for preparing an ironing high-extension wire according to any one of claims 1 to 5, characterized in that The steps of the method include: The first step is to process polyester staple fiber, polyester silk or nylon into a circular sewing thread; In the second step, the circular sewing line formed in the first step is provided with left and right alternate notches along the axial direction to form a left notch and a right notch; The third step is to fill the left and right notches formed in the second step with hot melt lines to obtain ironing high extension lines.
7. The method for preparing an ironing high-extension wire according to claim 6, characterized in that: When the material of the ironing high-extension line is polyester staple fiber, the ironing high-extension line is a circular sewing line formed by twisting the polyester staple fiber; When the material of the ironing high-extension line is polyester silk, the ironing high-extension line is a circular sewing line formed by paralleling polyester silk; When the material of the ironing high-extension line is nylon, the ironing high-extension line is a circular sewing line formed by spinning and doubling the nylon; The left notch is formed by chemicals or laser etching; The right notch is formed by chemicals or laser etching; The left notch is filled with a hot melt line; The right notch is filled with a hot melt line; The hot melt temperature of the hot melt line is 70°C.
Citation Information
Patent Citations
BE566146A
Seam-slippage-preventing stitching method for light and thin fabric
CN103478948A
Method for improving wrinkling of seam positions of ready-made garments
CN110101154A
Sewing thread for down coat
CN205398844U
Ironing high extension line
CN216585404U