A method for upward layered filling mining
Through technologies such as high-strength tailings cement and emulsified explosives, safe, efficient and environmentally friendly mining of upward-level mining has been achieved, and the problems of low efficiency and environmental damage of existing mining methods have been solved, thereby improving ore recovery and mining services have been improved. Year.
Patent Information
- Application Number
- CN202111114564.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-09-23
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2041-09-23
AI Technical Summary
The existing upward stratified mining methods are inefficient and insufficient in production capacity, complex and unsafe mining process, low ore recovery rate, and underground mining causes damage to the surface environment.
High-strength tailings glued bodies are used for stratified mining of intercolumns and mine rooms, rock mass is crushed by rock drilling and blasting, and high-strength tailings glued bodies are used for backfilling and support, combining emulsified explosives and non-electric ring detonation networks, Achieve safe and efficient mining operations.
It improves mining efficiency and production capacity, reduces workers' labor intensity, increases ore recovery rate, reduces the damage to the surface environment by underground mining, and realizes the resource utilization of phosphorus tailings, and improves the service life of mines.
Smart Images

Figure CN114000878B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an upward layered filling mining method, belonging to the technical field of mineral mining methods. Background Art
[0002] The upward layered filling mining method is a filling mining method that mines chambers, blocks or pans upward in layers during mining, first extracts ore from each layer, and then fills the goaf outside the working space required for the next layer after extraction. The working space of this mining method is located under the ore roof, and is suitable for mining ore bodies of various thicknesses and shapes with stable ore, medium-stable surrounding rock, steep inclination and inclination. At present, the upward layered mining method adopts the horizontal hole and upward fan-shaped hole mining method, that is, first drill the rock and blast the top to form a rock drilling space, then drill the blasthole with horizontal holes and upward fan-shaped holes, charge, blast, and mine, and then continue to drill the blasthole with horizontal holes and upward fan-shaped holes, charge, blast, and mine, and so on. A layered mining field needs more than ten cycles of rock drilling, charging, blasting, and mining to be completed. The defects of this horizontal hole mining method are: first, the footage of each blasting is small and the amount of blasted ore is small, resulting in low mining production efficiency and production capacity; second, the rate of large blocks of ore falling is high and the block size is uneven. After the recovery blasting, the roof of the mining area is irregular, and the workload of prying and protecting the roof is large; third, the operation cycle of each process of rock drilling, charging, blasting and mining must be organized in batches in the stratified mining area, which makes the production organization and management complicated. Summary of the invention
[0003] The purpose of the present invention is to provide an upward layered filling mining method, which innovates mining technology so that operations such as rock drilling, blasting, and mining can be carried out in an approach road or a rock drilling tunnel, with good operation safety, high degree of mechanization, low labor intensity of workers, high operation efficiency, large production capacity, and high ore recovery rate.
[0004] In order to solve the above technical problems, the present invention adopts the following technical solutions:
[0005] An upward layered filling mining method includes the following steps: S100: crushing the rock mass by rock drilling and blasting; S200: mining: first mining the lowest layer of ore, the mine room is arranged along the vein direction, the width of the pillar is 12 meters, the width of the mine room is 18 meters, the height of the pillar and the mine room is equal to 15 meters, and the length of the pillar and the mine room is equal to the horizontal thickness of the ore body; first mining the pillar, after mining the pillar, fill the pillar with a high-strength tailings cement, and then mine the mine room, after mining the current layer, mining upward layer by layer by the above method. In this scheme, the pillars are mined first because the load capacity of the high-strength tailings cement is better than that of the original ore body, and the performance is more stable. In the process of mining the pillars, the original ore body of the mine room plays a supporting role; after the pillars are mined, the high-strength tailings cement is backfilled, and the mine room is mined after the backfilling is completed. In the process of mining the mine room, the high-strength tailings cement plays a major supporting role. Through calculation, it is known that the bearing capacity ratio of the original ore body and the high-strength tailings cementation body is 2:3, so the width ratio of the mine room and the pillar is 3:2. At present, the conventional mine room and pillar are both 15 meters, so the width of the pillar is designed to be 12 meters and the width of the mine room is 18 meters.
[0006] In the aforementioned upward layered filling mining method, step S200 also includes the following contents: a segmented tunnel is arranged along the strike of each layer, and the segmented tunnels are connected through stone gates and slope tunnels; a through-vein tunnel is set in the middle of each ore block, and the through-vein tunnel is constructed from the segmented tunnel to the top plate of the ore body, and each through-vein tunnel also serves as a mining exit tunnel for the upper segment and a rock drilling tunnel for the lower segment.
[0007] In the aforementioned upward layered filling mining method, the step S200 also includes the following contents: a cutting tunnel is arranged along the direction in the vein of the ore body roof, which also serves as a return air tunnel, and a cutting skylight is arranged in the vein in the direction of each ore block roof, which also serves as a return air shaft; the upper layered through-vein tunnel is used as a downward fan-shaped deep-hole rock drilling tunnel, and the lower layered through-vein tunnel is used as a channel for shoveling and transporting ore out of the mine; after the filling is completed, the high-strength tailings cementation body reaches a maintenance cycle of 28 days, and the upper layered rock drilling tunnel is used as a channel for shoveling and transporting the upper layer out of the mine.
[0008] In the aforementioned upward layered filling mining method, step S200 also includes the following contents: during the blasting of the mining area, the collapsed ore remains in the mining area, providing temporary support for the ore rock or filling body on both sides; the mining area is blasted once to remove the ore until the mining is completed; the residual ore in the mining area chamber is cleaned up by a remote-controlled shovel loader to avoid direct entry of personnel into the empty area for operation; large pieces of ore are transported to the nearby loading access for secondary crushing, and the ore size is controlled below 500 mm.
[0009] In the aforementioned upward layered filling mining method, the step S100 also includes the following contents: using a drilling trolley to drill downward vertical parallel deep holes in the vein-penetrating tunnel, with a hole diameter of 100 mm and a row spacing of 2 m; using a drilling trolley to construct downward fan-shaped holes in the segmented vein-penetrating tunnel, with a hole diameter of 100 mm, a row spacing of 2 to 2.5 m, and a hole bottom distance of 2.1 to 2.5 m.
[0010] In the above-mentioned upward layered filling mining method, the step S100 also includes the following contents: the downward fan-shaped hole retreats from the middle slot area to the ore-loading access road of the mine room to collapse the ore in stages; the emulsion explosive matrix and the sensitizer are mixed in the hole to form the emulsion explosive; the blasthole adopts a non-coupled intermittent filling charging structure, each row of holes is charged and blasted at one time, 2 to 5 rows are blasted each time, and the pushing distance is 6 to 12m; the amount of explosives for each blast is controlled within Below, the maximum single-shot charge is controlled within 100kg; when charging the downward fan-shaped holes, a length of 1.5 to 2m is left between the charge surface and the hole mouth without charging. After the charge is loaded, it is blocked with gun mud with a blocking length of not less than 50cm, and the outer mouth of the gun hole is then blocked with a wooden plug or river sand.
[0011] In the aforementioned upward layered filling mining method, the step S100 also includes the following contents: a non-electric annular detonating network is used, an explosive bag is placed at the bottom of the blasthole and two same-segment differential detonators are inserted; the end of the detonating cord is led out of the hole, and then all the same-segment differential detonating cords are divided into two bundles, which are respectively tied to auxiliary short detonating cords, and the auxiliary short detonating cords are respectively tied to the main detonating cord; the leading end of the main detonating cord is glued to the instantaneous detonator, and finally the exciting detonating cord is led to a safe distance and detonated with a detonator, and the detonation point is greater than or equal to 200m from the blasting operation site.
[0012] In the aforementioned upward layered filling mining method, the high-strength tailings cementing body includes water, cement, aggregate and tailings, and the weight ratio of water, cement, aggregate and tailings is 1:4:3:13. The mixed raw materials are used to fill the segmented, layered bottom pillars, top pillars, single pillars, boundary pillars and mine room tops; the weight ratio of water, cement, aggregate and tailings is 1:6:11:26, and the mixed raw materials are used to fill the layered and segmented mine room recovery filling and pillar recovery retaining wall areas with a span of more than 15 meters; the weight ratio of water, cement, aggregate and tailings is 1:8:24:44, and the mixed raw materials are used to fill the layered or segmented area above the pillar recovery retaining wall with a span of less than 15 meters; the weight ratio of water, cement, aggregate and tailings is 1:10:23:72, and the mixed raw materials are used to fill the layered or segmented area above the pillar recovery retaining wall with a span of more than 30 meters and the empty area where no mining activities are carried out.
[0013] In the above-mentioned upward layered filling mining method, the high-strength tailings cementing body includes water, cement, ultrafine phosphorus slag powder, aggregate and tailings, and the weight ratio of water, cement, ultrafine phosphorus slag powder, aggregate and tailings is 10:28:12:30:130. The mixed raw materials are used to fill single ore pillars, boundary ore pillars and mine room tops with a segmentation of less than 15 meters; the weight ratio of water, cement, ultrafine phosphorus slag powder, aggregate and tailings is 10:42:18:110:260. The mixed raw materials are used to fill the stratified or segmented span of less than 15 meters in the mine room and the pillar recovery. Mining retaining wall area; the weight ratio of water, cement, ultrafine phosphate slag powder, aggregate and tailings is 10:56:24:240:440, and the mixed raw materials are used to fill the area above the pillar mining retaining wall with a span of less than 15 meters in the layer or segment; the weight ratio of water, cement, ultrafine phosphate slag powder, aggregate and tailings is 1:7:3:23:72, and the mixed raw materials are used to fill the area above the pillar mining retaining wall with a span of less than 15 meters in the layer or segment, the area above the pillar mining retaining wall with a span of more than 30 meters in the layer or segment, and the empty area where no mining activities are carried out.
[0014] In the aforementioned upward layered filling mining method, before filling with high-strength tailings cement, an expansion layer is laid at the bottom, and the expansion layer is composed of the following raw materials in parts by weight: 10 parts of water, 72 parts of cement, and 7 parts of calcium aluminate. The thickness of the expansion layer is 20 cm.
[0015] Compared with the prior art, the mining technology of the present invention is innovative, so that operations such as rock drilling, blasting, and mining can be carried out in the approach or rock drilling chamber, with good operation safety; high degree of mechanization, low labor intensity of workers; high operation efficiency, large production capacity, and high ore recovery rate. In addition, this method has the following advantages: 1. Layered mining, strong flexibility, can better adapt to changes in the morphology of the ore body, and has a strong promotion significance in mines of the same type. 2. The phosphorus tailings filling technology is adopted to digest the phosphorus tailings, reduce a series of problems such as the occupation of land by tailings discharge and the environmental pollution caused by tailings storage. 3. The filling mining technology is adopted to reduce the damage to the surface environment caused by underground mining; 4. The filling treatment of the empty area makes mining safer, increases the ore recovery rate to 89.5%, and also extends the service life of the mine. 5. Comprehensively utilize water resources to realize the ecological and circular utilization of water resources. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 , Figure 2 and Figure 3 It is a schematic diagram of the upward layering mining method;
[0017] Figure 4 It is a schematic diagram of a partial filling position of the present invention;
[0018] Figure 5 It is another partial filling position schematic diagram of the present invention;
[0019] Figure 6 is a filling process flow chart of an embodiment of the present invention;
[0020] Figure 7 It is the aggregate distribution frequency diagram of each particle size interval under aggregate and Fuller grading;
[0021] Figure 8 It is the particle size characteristic curve of underground waste rock as aggregate.
[0022] Figure markings: 1-slope tunnel, 2-middle section transport tunnel, 3-segmented tunnel, 4-stone gate, 5-mine exit tunnel, 6-cutting skylight also serving as return air shaft, 7-return air tunnel, 8-high-strength tailings cementation body, 9-filling retaining wall, 10 blast hole.
[0023] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments. DETAILED DESCRIPTION
[0024] Embodiment 1: A method for upward layered filling mining, comprising the following steps:
[0025] S100: Rock mass is broken by rock drilling and blasting. In the vein tunnel, a rock drilling trolley is used to drill downward vertical parallel deep holes with a hole diameter of 100mm and a row spacing of 2m. In the segmented vein drilling tunnel, a rock drilling trolley is used to construct downward fan-shaped holes with a hole diameter of 100mm, a row spacing of 2m, and a hole bottom distance of 2.1m. The downward fan-shaped holes retreat from the middle trough area to the ore loading access road of the mine room and collapse the ore laterally in batches; the emulsion explosive matrix and sensitizer are mixed in the hole to form an emulsion explosive; the blast hole 10 adopts a non-coupled intermittent filling charging structure, and each row of holes is charged and blasted at one time, with 2 rows blasted each time and a pushing distance of 6m; the amount of explosives for each blast is controlled within Below, the maximum single-shot charge is controlled within 100kg; when charging the downward fan-shaped holes, a length of 1.5m is left between the charge surface and the hole mouth without charging. After the charge is loaded, it is blocked with gun mud with a blocking length of not less than 50cm, and the outer mouth of the gun hole 10 is blocked with a wooden plug or river sand.
[0026] A non-electric annular detonating network is used, with an explosive pack placed at the bottom of blasthole 10 and two same-section differential detonators inserted; the end of the detonating cord is led out of the hole, and then all the same-section differential detonating cords are divided into two bundles and tied to auxiliary short detonating cords respectively, and the auxiliary short detonating cords are then tied to the main detonating cord respectively; the leading end of the main detonating cord is glued to the instantaneous detonator, and finally the exciting detonating cord is led to a safe distance and detonated with a detonator, and the detonation point is greater than or equal to 200m from the blasting operation site.
[0027] S200: Ore discharge: During the blasting of the mining area, the collapsed ore remains in the mining area, providing temporary support for the ore rock or filling body on both sides; the mining area is blasted once for ore discharge until the mining is completed; the residual ore in the mining area chamber is cleaned up by remote-controlled scrapers to avoid direct entry of personnel into the open area for operation; large pieces of ore are transported to the nearby loading access for secondary crushing, and the ore size is controlled below 500mm.
[0028] First, the lowest layer of ore is mined, and the ore room is arranged along the vein direction. The length and width of the pillars are both equal to 12 meters, the length and width of the ore room are both equal to 18 meters, and the height of the pillars and the ore room is equal to 15 meters; first, the pillars are mined, and after the pillars are mined, the pillars are filled with high-strength tailings cement 8, and then the ore room is mined. After the current layer is mined, the above method is used to mine upward layer by layer. The middle section transport roadway 2 plays the role of connecting the segmented transport roadway 3, connecting the segmented transport roadway 3.
[0029] A segmented tunnel 3 is arranged along the strike of each layer, and the segmented tunnel 3 is connected to the slope tunnel 1 through a stone gate 4; a through-vein tunnel is set in the middle of each ore block, and the through-vein tunnel is constructed from the segmented tunnel 3 to the top plate of the ore body, and each through-vein tunnel also serves as the upper segment mine exit tunnel 5 and the lower segment rock drilling tunnel. A cutting tunnel along the strike is arranged in the vein of the top plate of the ore body, which also serves as the return air tunnel 7, and a cutting skylight is arranged in the vein of the top plate of each ore block, which also serves as the return air shaft 6; the upper layer through-vein tunnel is used as a downward fan-shaped deep hole rock drilling tunnel, and the lower layer through-vein tunnel is used as a channel for shoveling and transporting ore out of the mine; after filling is completed, the high-strength tailings cementation body 8 reaches a maintenance period of 28 days, and the upper layer rock drilling tunnel is used as the upper layer shoveling and transporting channel out of the mine.
[0030] The high-strength tailings cementitious body 8 comprises water, cement, aggregate and tailings, wherein the weight ratio of water, cement, aggregate and tailings is 1:4:3:13, and the mixed raw materials are used to fill the segmented, layered bottom pillars, top pillars, single pillars, boundary pillars and mine room tops; the weight ratio of water, cement, aggregate and tailings is 1:6:11:26, and the mixed raw materials are used to fill the mine room recovery filling and pillar recovery retaining wall areas with a span of more than 15 meters in the layers and segments; the weight ratio of water, cement, aggregate and tailings is 1:8:24:44, and the mixed raw materials are used to fill the areas above the pillar recovery retaining wall with a span of less than 15 meters in the layers or segments; the weight ratio of water, cement, aggregate and tailings is 1:10:23:72, and the mixed raw materials are used to fill the areas above the pillar recovery retaining wall with a span of more than 30 meters in the layers or segments, and the empty areas where no mining activities are carried out.
[0031] Before filling with the high-strength tailings binder 8, an expansion layer is laid at the bottom. The expansion layer is composed of the following raw materials by weight: 10 parts of water, 72 parts of cement, and 7 parts of calcium sulfonate. The thickness of the expansion layer is 20 cm. The high-strength tailings binder 8 will reduce in volume after the water evaporates. To address this problem, an expansion layer is involved. The expansion layer is located under the high-strength tailings binder 8, which can neutralize the volume reduction of the high-strength tailings binder 8 due to the evaporation of water. The expansion agent is not stirred in the high-strength tailings binder 8 to prevent the expansion agent from not being stirred evenly in the high-strength tailings binder 8, affecting the test effect. The high-strength tailings binder 8 and the expansion layer can be implemented at the same time, and the high-strength tailings binder 8 is directly filled above the expansion layer. After the filling is completed, a filling retaining wall 9 is piled up at the end of the filling to prevent the high-strength tailings binder 8 from overflowing.
[0032] Embodiment 2: An upward layered filling mining method comprises the following steps:
[0033] S100: Rock mass is broken by rock drilling and blasting. In the vein tunnel, a rock drilling rig is used to drill downward vertical parallel deep holes with a hole diameter of 100mm and a row spacing of 2m. In the segmented vein drilling tunnel, a rock drilling rig is used to construct downward fan-shaped holes with a hole diameter of 100mm, a row spacing of 2.5m, and a hole bottom distance of 2.5m. The downward fan-shaped holes retreat from the middle trough area to the ore loading access road of the mine room and collapse the ore in stages. The emulsion explosive matrix and sensitizer are mixed in the hole to form an emulsion explosive. The blast hole 10 adopts a non-coupled intermittent filling charging structure, and each row of holes is charged and blasted at one time. 5 rows are blasted each time, and the push distance is m; the amount of explosives for each blast is controlled within Below, the maximum single-shot charge is controlled within 100kg; when charging the downward fan-shaped holes, the charge surface is left 2m away from the hole mouth without charging. After the charge is loaded, it is blocked with gun mud with a blocking length of not less than 50cm, and the outer mouth of the gun hole is then blocked with a wooden plug or river sand.
[0034] A non-electric annular detonating network is used, with an explosive pack placed at the bottom of blasthole 10 and two same-section differential detonators inserted; the end of the detonating cord is led out of the hole, and then all the same-section differential detonating cords are divided into two bundles and tied to auxiliary short detonating cords respectively, and the auxiliary short detonating cords are then tied to the main detonating cord respectively; the leading end of the main detonating cord is glued to the instantaneous detonator, and finally the exciting detonating cord is led to a safe distance and detonated with a detonator, and the detonation point is greater than or equal to 200m from the blasting operation site.
[0035] S200: Ore discharge: During the blasting of the mining area, the collapsed ore remains in the mining area, providing temporary support for the ore rock or filling body on both sides; the mining area is blasted once for ore discharge until the mining is completed; the residual ore in the mining area chamber is cleaned up by remote-controlled scrapers to avoid direct entry of personnel into the open area for operation; large pieces of ore are transported to the nearby loading access for secondary crushing, and the ore size is controlled below 500mm.
[0036] The lowest layer of ore is mined first, and the mine chamber is arranged along the vein direction. The length and width of the pillars are both equal to 12 meters, the length and width of the mine chamber are both equal to 18 meters, the height of the pillars and the mine chamber is both equal to 15 meters, and the length of the pillars and the mine chamber is equal to the horizontal thickness of the ore body; the pillars are mined first, and then the pillars are filled with high-strength tailings cementation, and then the mine chamber is mined. After mining the current layer, mining is carried out layer by layer upwards using the above method.
[0037] The ramp tunnel 1 serves to connect the middle transport tunnel 2 and the segmented tunnel 3. A segmented tunnel 3 is arranged along the strike of each layer, and the segmented tunnel 3 is connected to the ramp tunnel 1 through a stone gate 4; a through-vein tunnel is set in the middle of each ore block, and the through-vein tunnel is constructed from the segmented tunnel 3 to the top plate of the ore body, and each through-vein tunnel also serves as the upper segmented mine exit tunnel 5 and the lower segmented rock drilling tunnel. A cutting tunnel along the strike is arranged in the vein of the top plate of the ore body, which also serves as the return air tunnel 7, and a cutting skylight is arranged in the vein of the top plate of each ore block, which also serves as the return air shaft 6; the upper layer through-vein tunnel serves as a downward fan-shaped deep-hole rock drilling tunnel, and the lower layer through-vein tunnel serves as a channel for shoveling and transporting ore out of the mine; after filling is completed, the high-strength tailings cementation body 8 reaches a maintenance cycle of 28 days, and the upper layer rock drilling tunnel serves as the upper layer shoveling and transporting channel out of the mine.
[0038] The high-strength tailings cement body 8 includes water, cement, ultrafine phosphorus slag powder, aggregate and tailings. The weight ratio of water, cement, ultrafine phosphorus slag powder, aggregate and tailings is 10:28:12:30:130. The mixed raw materials are used to fill single ore pillars with a length of less than 15 meters, boundary ore pillars and mine room tops; the weight ratio of water, cement, ultrafine phosphorus slag powder, aggregate and tailings is 10:42: The weight ratio of water, cement, ultrafine phosphate slag powder, aggregate and tailings is 10:56:24:240:440, and the mixed raw materials are used to fill the area above the pillar mining retaining wall with a span of less than 15 meters in the layer or segment; the weight ratio of water, cement, ultrafine phosphate slag powder, aggregate and tailings is 1:7:3:23:72, and the mixed raw materials are used to fill the area above the pillar mining retaining wall with a span of less than 15 meters in the layer or segment, the area above the pillar mining retaining wall with a span of more than 30 meters in the layer or segment, and the empty area where no mining activities are carried out.
[0039] Before filling with the high-strength tailings binder 8, an expansion layer is laid at the bottom. The expansion layer is composed of the following raw materials by weight: 10 parts of water, 72 parts of cement, and 7 parts of calcium aluminate. The thickness of the expansion layer is 20 cm. The high-strength tailings binder 8 will lose volume after the water evaporates. To address this problem, an expansion layer is involved. The expansion layer is located under the high-strength tailings binder 8, which can neutralize the volume loss of the high-strength tailings binder 8 due to the evaporation of water. The expansion agent is not stirred in the high-strength tailings binder 8 to prevent the expansion agent from not being stirred evenly in the high-strength tailings binder 8, affecting the effect. The high-strength tailings binder 8 and the expansion layer can be implemented at the same time, and the high-strength tailings binder 8 is directly filled above the expansion layer. When preparing for filling, a filling retaining wall 9 is built at the end of the mining tunnel 5 to prevent the high-strength tailings binder 8 from overflowing.
[0040] Normally, the filling design is to design the material mix ratio according to the filling strength requirements of the mining method, and select the appropriate concentration range to adapt to pipeline transportation. The filling strength is designed according to the requirements of the mining method and is the basis; whether the filling slurry can achieve stable pipeline transportation is the key. At present, most filling mines use pipeline transportation to transport the filling slurry, so the fluidity of the filling slurry must meet the requirements of pipeline transportation. Under the premise of determining the filling multiple, ensuring that the filling slurry is smoothly transported to the underground goaf by gravity or pumping is a prerequisite for filling. Cost is a prerequisite for filling design and determines whether it can be "affordable". The filling cost is a relatively high part of the mining cost in mines that adopt the filling mining method, and the cost of filling materials is the main factor constituting the filling cost. Therefore, when a mine selects filling materials, it must first ensure that the filling materials have a wide source and low cost; the selection of solid industrial waste such as tailings, underground waste rock, and ultrafine phosphorus slag as filling materials is not only low-cost, but also can solve the sewage discharge problem of mining enterprises. Therefore, this type of industrial solid waste should be the first choice for filling materials; secondly, it can be adapted to local conditions and use natural materials such as underground waste rock to reduce solid waste discharge and storage. At the same time, through experimental research on filling materials and filling slurry mix ratios, choosing cheap filling materials that meet production conditions and choosing a reasonable filling slurry mix ratio is an effective way to reduce filling costs. Slurry concentration is a link that affects the mix ratio, strength, pipeability, homogeneity of the filling body, stability, plasticity, rheology, etc. In actual mining production, the fewer types of filling materials, the less construction and land occupation of surface storage silos, the smaller the construction investment scale, the simpler the corresponding filling slurry system, and the easier it is to control the proportion of filling slurry; otherwise, the entire slurry station process is complex and the control is cumbersome, and the fluctuation of various material feeds has a greater impact on the quality of the slurry. Therefore, under the premise of meeting other principles, a simple slurry proportion and slurry system should be designed. Only under the premise of large filling scale, rich filling material sources and full consideration of comprehensive technical and economic indicators, can more material matching methods be selected.
[0041] Aggregate gradation refers to the distribution of aggregate particle sizes from the finest material to medium and coarse particles. Generally speaking, aggregate gradation should be good so that fine particles can fill the gaps between coarse particles, which helps to reduce the void ratio in the aggregate skeleton. These gaps are filled with cementitious materials such as cement paste. After hardening, the loose aggregate particles are connected into a whole, that is, concrete as hard as rock.
[0042] The commonly used grading theories at present mainly include the maximum density curve theory and the quantum interference theory. The former mainly describes the particle size distribution of continuous grading and is used to calculate continuous grading, while the latter can be used to calculate continuous grading and discontinuous grading. The existing grading algorithms are all developed based on the maximum density curve theory, which only emphasizes that the grading reaches the maximum density without considering whether the skeleton structure is formed. Therefore, the grading designed by this method is difficult to form a skeleton dense structure.
[0043] The maximum density curve theory is an ideal curve proposed through experiments. After experiments, WB Fuller proposed that the solid particles are arranged regularly according to the particle size, and the coarse and fine particles are matched, so that the mixture with the maximum density and the smallest voids can be achieved. Initial studies believed that the particle grading of fine aggregate is an elliptical curve, and the coarse aggregate is a straight line tangent to the elliptical curve. The grading curve composed of these two parts can achieve the maximum density. Later, after improvements, a simplified "parabola maximum density ideal curve" was proposed, which believed that the closer the particle grading curve is to the parabola, the greater the density. The expression is:
[0044]
[0045] Where P x —The passing percentage of a certain aggregate particle size d that you want to calculate, %;
[0046] D—maximum particle size of aggregate, mm.
[0047] Concrete industry tests and applications have shown that aggregates that meet Fuller's ideal gradation are particularly suitable for mixing low-fluidity concrete mixtures, which have the characteristics of tightly packed particles. During on-site construction, this type of concrete requires high-efficiency vibration equipment for pouring and construction.
[0048] To this end, Bolomey suggested introducing parameter A to modify the ideal gradation curve. Parameter A needs to take into account workability requirements and aggregate type (natural aggregate or artificial aggregate). If A = 0, the Bolomey formula is the same as the Fuller formula.
[0049]
[0050] D max ——Refers to the aperture size of the sieve through which all aggregates pass or at most 5% fail in the screening test.
[0051] As the workability of the concrete changes from dry to high flow and the aggregate changes from spherical natural aggregate to angular crushed stone, the parameter A also increases from 8 to 14. The increase in the value of A means an increase in the amount of fine particles passing the 5 mm sieve.
[0052] In the selection of filling materials, a lot of work has been done on the experimental research of filling mortar strength. From the perspective of technology and economy, the mine has selected tailings, yellow phosphorus slag and underground waste rock with rich reserves as filling materials. Ultrafine phosphorus slag powder is made by grinding yellow phosphorus slag into powder. It has strong bonding ability and can be used as raw material for cement production.
[0053]
[0054] According to the above table, the aggregate distribution frequency diagram of each particle size range under the aggregate and Fuller grading is drawn as follows Figure 7 shown.
[0055] It can be seen that the particle size distribution of aggregates is characterized by "fewer coarse and fine particles and more intermediate particles". In fact, the aggregate particle size distribution index is 0.5, which meets the fuller's requirements for grading. The aggregate particle size distribution is good and the density is high, but it can be seen that the aggregate is very fine, and the aggregate is basically below 200 mesh. If aggregates are used alone for filling, the excessively fine particles will inevitably lead to an increase in the consumption of filling cement, which is not conducive to the development of the strength of the cemented filling body. Therefore, although the aggregate grading index is very ideal, coarse aggregates must be mixed into the filling process to reduce cement consumption and strengthen the filling body strength.
[0056] Underground waste rock has many corners and rough surface texture. When mixing, the friction between adjacent particles is very strong. At the same time, it has a large surface area to volume ratio, and more cement slurry is needed to completely cover the surface of the particles. The influence of underground waste rock crushing aggregate on the design of filling slurry mix ratio mainly includes particle shape, texture and aggregate gradation. According to the safety technical standards for cemented filling, the maximum particle size of cemented filling aggregate should not exceed 1 / 5 of the conveying pipe diameter. The conveying pipe diameter of phosphate mines is mostly 100mm inner diameter steel pipe or plastic pipe. Therefore, the maximum particle size of underground waste rock should not exceed 20mm. Underground waste rock is crushed by jaw crusher until the crushed particle size meets the design requirements. The gradation or particle size distribution of underground waste rock aggregate is an important property of aggregate, which determines the packing density of aggregate, the amount of filling cement, and the pipe transportability. Through testing and analysis, the aggregate size gradation of underground waste rock crushing aggregate is shown in the following table:
[0057]
[0058] The particle size characteristic curve of underground waste rock as aggregate is as follows: Figure 8 shown.
[0059] The grading curve of underground waste rock crushed aggregate is shown in the figure above. The grading index of underground waste rock crushed aggregate n = 0.41 is less than the Fuller grading index (n = 0.41). Obviously, the coarse particle content of underground waste rock crushed aggregate is large, and the stacking density is large. Under the condition of high water-cement ratio, the slurry is prone to water seepage during pipeline transportation (whether pump pressure or gravity transportation) and causes pipe blockage. In addition, large particles are prone to sedimentation during pipeline transportation, which is not conducive to pipeline transportation. It must be matched with fine materials to improve grading, increase the filling effect and aggregate density.
[0060] In general, filling aggregates account for more than 60% of the mass of the filling entity, and cement costs account for more than 70% of the filling material costs. Therefore, the simple and necessary principle to reduce the filling cost is "add more aggregates to the filling body, add less cement and self-flowing filling". According to the current filling practice results at home and abroad: under high-concentration pipeline filling conditions, as long as the volume concentration of the slurry is increased by 1%, the amount of cement can be reduced by 5-10% under the same strength conditions. Good grading is the premise of "adding more aggregates", so further research is needed to reasonably prepare the filling slurry and select the filling concentration.
[0061] The aggregate particle size distribution index is 0.5, which meets the fuller's requirements for grading, and the aggregate is basically below 200 mesh. Using aggregate alone for filling is not conducive to the development of the strength of the cemented filling body. Therefore, although the aggregate grading index is very ideal, coarse aggregate must be mixed into the filling process to reduce cement consumption and strengthen the filling body strength.
[0062] The gradation index of underground waste rock crushing aggregate is n=0.41, which is less than Fuller gradation index (n=0.41). Large particles in underground waste rock filling are prone to sedimentation, which is not conducive to pipeline transportation. It must be mixed with fine materials to improve gradation, increase gap filling effect and aggregate density.
[0063] From the perspective of quantitative analysis, the packing density (Φ) of cemented filling aggregate in mines refers to the ratio of the solid volume in the aggregate bulk system to the total volume of the bulk system, and the porosity (ω) of the aggregate bulk system refers to the ratio of the void volume in the aggregate bulk system to the total volume of the bulk system. According to the definition of packing density and porosity, Φ = 1-ω. The relationship between the void ratio ε and the porosity ω is: ε = ω / (1-ω). Assume that the filling aggregate bulk system is a mixture of coarse aggregate 1 and fine aggregate 2, and define the various parameters of the filling aggregate bulk system as follows:
[0064] (1) x is the ratio of coarse aggregate in the two aggregates, that is, the ratio of the mass of aggregate 1 to the mass of mixed aggregate;
[0065] (2) m----total mass of mixed aggregate, kg;
[0066] (3) m1: the mass of aggregate 1 (coarse aggregate) in the two mixed aggregates, kg;
[0067] (4) m2 – the mass of aggregate 2 (fine aggregate) in the two mixed aggregates, kg;
[0068] (5) k-----The mass ratio of aggregate 1 to aggregate 2 in the two mixed aggregates.
[0069] (6)ρ-----density of mixed aggregate,
[0070] (7)ρ1----density of aggregate 1,
[0071] (8)ρ2----density of aggregate 2,
[0072] (9)Φ-----mixed aggregate packing density;
[0073] (10) ----The packing density of aggregate 1 (coarse aggregate) in a certain mixing state;
[0074] (11) Φ1--packing density of aggregate 1;
[0075] (12) Φ2----packing density of aggregate 2;
[0076] (13) ω-----Porosity of mixed aggregate;
[0077] (14)ω2----porosity of aggregate 2;
[0078] (15)ω1----Porosity of aggregate 1.
[0079] The mathematical model of the density of mixed stacking of two aggregates is established as follows:
[0080] (1) According to the meaning of ρ, ρ1, ρ2, and x parameters, we have the following equation:
[0081] 1 / ρ=x / ρ1+(1-x) / ρ2 (3)
[0082] (2) Based on the property that the solid volume of the two aggregates remains unchanged before and after mixing, the following formula can be established:
[0083]
[0084] (3) According to the parameter meaning of x, its value range is: 0≤x≤1, then There are several situations:
[0085] ① Boundary condition 1: When x = 1, that is, when there is no aggregate 2, from formula 4) we get:
[0086] ② Boundary condition 2: When x = 0, that is, when there is no aggregate 1, from equation (4), we get: Φ = Φ2;
[0087] ③ When x is very small, that is, when aggregate 2 has an absolute advantage, aggregate 1 cannot form a skeleton structure and its pores are completely filled with aggregate 2. At this time, the porosity of aggregate 1 can be regarded as zero, that is, ω1 = 0. That is, aggregate 1 does not form a skeleton structure in the mixture, but is completely "suspended" in aggregate 2. This state is quantitatively expressed as follows:
[0088]
[0089] Substituting (5) into (4) we can immediately obtain:
[0090]
[0091] ④ When x is very large, that is, when aggregate 1 accounts for an absolute majority, aggregate 1 forms a complete skeleton structure in the mixture, and aggregate 2 is only used to "fill the gaps". Aggregate 2 fills the gaps of aggregate 1 from part to all. This state is quantitatively expressed as follows:
[0092]
[0093]
[0094] in:
[0095] In summary, the two mixture packing density model functions can be established as follows:
[0096]
[0097] The symbols in the formula have the same meaning as before.
[0098] From the model function of the density of the two mixtures, it can be seen that the density of the mixed aggregate Φ of the two aggregates is a single-valued function of the proportion of the two mixed aggregates. The density of the coarse aggregate 1 in the mixed aggregate bulk system, the density of the fine aggregate 2, the density of the two mixed aggregates, the density of the coarse aggregate 1, and the density of the fine aggregate 2 can all be measured experimentally.
[0099] In terms of slurry properties, tailings-aggregate cemented filling slurry is a low-grade multiphase mixture. In an ideal filling slurry, its components are evenly dispersed and filled with each other. For tailings aggregates, which account for the vast majority of the volume in the slurry, good grading can not only reduce segregation and improve the workability of the slurry mixture, but also increase the interlocking ability between tailings particles. The majority of the aggregates are quasi-round particles, and the particle size distribution is relatively uniform. The extremely fine flocculent material adheres to the surface of the coarse particles, and the appropriate ratio is used to determine the maximum density.
[0100] According to formula (8), the maximum point of the packing density of the tailings-aggregate mixture can be calculated, that is, when tailings: aggregate ≈ 0.7:0.3, Φ = 0.76961.
[0101] When the proportion of tailings crushed aggregate is less than 0.6, the density of the mixture increases with the increase of the amount of coarse tailings particles. As the amount of tailings crushed aggregate increases, the amount of coarse particles also gradually increases, and the "skeleton" effect is obvious, resulting in a further increase in the density of the mixture. As the amount of coarse tailings aggregate increases further, the amount of aggregate gradually decreases, and the density of the mixture also shows a downward trend.
[0102] The calculated results of the aggregate packing density have the same trend as the measured results. The results show that the packing density reaches the maximum when the coarse aggregate accounts for 60%. The measured packing density at this time is 0.73, and then the packing density begins to decrease. In the mixed filling material, with the increase of fine aggregate, the porosity of the aggregate gradually decreases. When the fine aggregate reaches 60%, the aggregate pores are the smallest. The maximum packing density means that the filling slurry at this time should have the maximum bonding strength under the same conditions.
[0103] Cemented filling is a means to control ground pressure. Only under pressure can it generate resistance to react to the surrounding rock. Due to the use of open-pit mining, the surrounding rock of the stope has completed the stress redistribution process such as stress release and transfer during the mining process. Even if high elastic modulus and high-strength filling materials are used, they will not immediately produce a supporting effect on the surrounding rock of the stope. Therefore, the supporting role of the cemented filling is mainly manifested in bearing the loose ground pressure of the stope.
[0104] Taking into account the cohesion of the cemented filling body, the internal friction angle, the contact conditions between the cemented filling body and the surrounding rock, and the lateral pressure of the surrounding rock on the cemented filling body, the equilibrium equation of the three-dimensional wedge of the cemented filling body was established using the limit equilibrium analysis method, and the vertical stress distribution solution of the cemented filling body was obtained:
[0105]
[0106] In the formula: K Approximate calculations;
[0107] β—the angle between the sliding surface at the bottom of the filling body and the horizontal plane, °;
[0108]
[0109] C j —Cohesion between cemented filling and surrounding rock, MPa;
[0110] It is approximately between 0.6 and 1.
[0111] The remaining parameters are the same as before.
[0112] The Lupin wedge sliding model can not only reflect the influence of the height and length of the filling body on the required strength of the filling body, but also reflect the influence of the strength characteristics of the filling body (cohesion and internal friction angle) and the interaction between the filling body and the surrounding rock on the required strength of the filling body. This model is the result of the study of the mechanical properties of cement-bonded filling bodies, and has good applicability to cement-bonded filling bodies under self-supporting conditions. Professor Cai Sijing used the Lupin wedge sliding model to calculate the required strength of the cemented ore pillars under the self-supporting state of the Mount Isa Mine. The calculation results are closest to the measured results of the Mount Isa Mine, and the calculation results are higher than the measured results, which verifies the applicability of the model under self-supporting conditions.
[0113] The Origin software custom function was used to fit the aggregate triple-link high-pressure consolidation test results, and the functional relationship between aggregate density and height was established. By analyzing the mechanical equilibrium state of the micro-element at any height of the aggregate filling body in the stope, the equivalent substitution relationship between the self-weight stress of the aggregate and the height was established. The equivalent substitution relationship was brought into the functional relationship between the aggregate and the pressure, and the relationship between the aggregate density and the height was obtained, which satisfies the power function characteristics:
[0114] ρ h =iρ 0砂 (h+j) l
[0115] in:
[0116]
[0117]
[0118] The relationship between the density of mineral aggregate and height can be described as:
[0119] ρ h2 =1.2ρ 02 (h+0.0246) 0.0492
[0120] By using the above formula and the actual dimensions of each part of the mine, it is possible to calculate the proportion of cementing agent to be used in each part.
[0121] The test results show that: ① Grading analysis of tailings + aggregate mixture: The particle size distribution of three different ratios of tailings and aggregate mixtures all meet the Fuller grading theory model, among which the Talbol grading index n = 0.25 when the tailings and aggregates are mixed at a ratio of 5:5 is the largest, followed by n = 0.23 when the tailings and aggregates are mixed at a ratio of 4:6, and n = 0.21 when the tailings and aggregates are mixed at a ratio of 3:7. This is consistent with the Talbol grading theory, indicating that only the mixture of 5:5 among the three ratios has a good packing density. ②Grading analysis after mixing ultrafine phosphorus slag + aggregate: The gradations all conform to the Talbol gradation equation, and the fitting coefficients of the curves are all high. The fitting indexes of ultrafine phosphorus slag aggregate 3:7, 4:6, and 5:5 are 0.23, 0.26, and 0.31, respectively. Among them, the one closest to the Fuller index is ultrafine phosphorus slag aggregate 5:5, indicating that under this ratio, the yellow phosphorus slag aggregate mixture has the optimal packing density, the smallest porosity, and the maximum bonding strength under the same conditions.
[0122] The strength of the cementitious body is closely related to the aggregate packing density in unit volume of slurry, the volume concentration of slurry, and the water-cement ratio, and is linearly related to the aggregate packing density; and has a negative power exponential relationship with the water-cement ratio. The model regression results show that among the factors affecting the strength of the cementitious body (3 days, 7 days, and 28 days), the aggregate packing density (determined by grading) is the primary factor, and W / C is the secondary factor affecting the strength.
[0123] Combining the previous research results, this study proposed a new strength prediction model. The advantage of the model is that it comprehensively considers the effects of aggregate, cement and water on strength and is conducive to regression analysis.
[0124]
[0125] From the results of strength test, in the tailings-aggregate cemented filling slurry, the slurry of 5:5 to 3:7 can meet the strength requirements at a lime-sand ratio of 1 / 6. At a lime-sand ratio of 1 / 8, only tailings and aggregates at a ratio of 5:5 and 4:6 can meet the requirements. Phosphorus slag ultrafine powder-aggregate can meet the cementing strength requirements at lime-sand ratios of 1 / 6 and 1 / 8. From the perspective of cementing strength optimization, the lower the cement content, the more filling costs can be saved. In the distribution of filling costs, the unit price of phosphorus slag ultrafine powder is higher than that of tailings. Therefore, the conclusion is to use a cemented filling slurry with a mass concentration of 71% of tailings-aggregate 5:5 and tailings-aggregate 11:6 and a lime-sand ratio of 1 / 8.
[0126] The physical strength of the bonding material reaching the specified index is a necessary condition for application in actual situations, while the lateral force of the bonding material is the basis for calculating the different weight ratios of raw materials for different size environments.
[0127] Finite element analysis was performed on the stability of the cemented backfill. The monitoring results and the finite element analysis results were combined to obtain a semi-empirical formula as shown in formula (10), which is used to describe the relationship between the required strength of the cemented backfill and the exposed height, width, length and internal friction angle. Under the geological and ore body geometric conditions, the cemented backfill can be self-supporting even if it is exposed to the air on one side and has a tailings backfill on the other side under the lateral force.
[0128]
[0129] Where: σ—Required strength of cemented filling body, MPa;
[0130] γ—bulk density of cemented filling body, MN / m3;
[0131] —friction angle of cemented filling body, °;
[0132] H—maximum self-supporting height of cemented filling, m;
[0133] L—length of cemented filling body; m;
[0134] W—width of cemented filling body; m.
[0135] Formula (10) summarizes the calculation formula of the strength of cemented filling body, which is related to the structural dimensions (length, width, height) and strength characteristics (internal friction angle) based on full consideration of practical experience. This formula provides a research idea for the strength design of cemented filling body under the premise of meeting the safety production requirements.
[0136] Analysis of formula (10) revealed that: (1) The relationship between the internal friction angle and strength of the cemented filling body in formula (1) is inconsistent with the strength characteristics of the cemented filling body. The required strength of the cemented filling body in formula (10) decreases as the internal friction angle of the cemented filling body increases. However, based on the relationship between the Mohr limit stress circle and the Coulomb-Navier strength curve, the relationship between the uniaxial compressive strength of the cemented filling body and the internal friction angle can be deduced as shown in formula (11). Under the condition of a certain cohesion in the cemented filling body, when the internal friction angle is hour, is a monotonically increasing function. The strength of the cemented filling increases with the increase of the internal friction angle. (2) Formula (10) can meet the stability requirements under the condition that the cemented filling body is open on one side and has the tailings filling body side pressure on the other side. However, there is no parameter in the formula that can characterize the tailings side pressure. That is, the formula is used to calculate the required strength of the cemented filling body under the condition of self-supporting conditions and one side is open and the other side is tailings filling body. The results are consistent. (3) The shear resistance between the cemented filling body and the surrounding rock can transfer the self-weight stress of the cemented filling body to the surrounding rock, forming an arch effect. There is no parameter in the formula that can characterize this shear resistance. In summary, formula (10) provides a convenient and fast calculation method for the strength design of the cemented filling body, and can meet the requirements of safe production. In terms of the problems existing in the model and the differences in mines, this formula is not suitable for designing the strength of cemented filling bodies in other mines.
[0137]
[0138] The essence of geotechnical mechanics analysis method is to analyze the mechanical model of cemented filling body with the help of research results or analysis methods in geotechnical mechanics, and derive the strength calculation formula of cemented filling body. Based on the different understandings of the interaction between filling body and surrounding rock, the model can be divided into four categories: arch effect, wedge sliding theory (limit equilibrium analysis method), overburden bearing theory and surrounding rock-support action principle.
[0139] Under the condition that other parameters remain unchanged, the required strength of the cemented filling increases with the increase of height. As the height of the cemented filling increases, the gravity of the cemented filling, the height of the top plate balance arch (the weight of the loose rock on the top of the cemented filling), and the lateral pressure of the tailings on the cemented filling all increase, resulting in an increase in the sliding force on the sliding surface of the cemented filling. Although the shear resistance (T s ) also increases with the increase of the height of the cemented filling body, but its increasing rate is lower than the increasing rate of the sliding force on the sliding surface of the cemented filling body. Therefore, the cemented filling body is prone to shear failure along the sliding surface, resulting in instability of the cemented filling body. In order to ensure the stability of the filling body, the strength of the cemented filling body needs to be increased.
[0140] The uniaxial compressive strength required for the cemented filling body. As shown in the table
[0141]
[0142]
[0143] For upward filling bodies, a safety factor of 1.5 to 2.0 is generally considered. After considering the safety factor, the bonding strength requirement for the two-step method is 1.62MPa, and the bonding strength requirement for the Lupin model is 0.74MPa. From the perspective of bonding strength, it is obvious that the bonding strength required for the first step is higher, which is mainly due to the lateral pressure of the surrounding tailings filling body in the first step. The increase in the bonding strength requirement means an increase in the unit consumption of cement. In fact, because the two-step mining method does not require full bonding, it only increases the strength of the cemented ore pillar. From the perspective of the filling cost of the entire segment, the overall cost can be reduced.
[0144] The non-cemented tailing sand filling body will slide down along the sliding surface and collapse without restraint. Therefore, the pressure of the non-cemented tailing sand on the cemented filling body is active pressure. Maximum principal stress is the weight of tailings overlying the unit body; the minimum principal stress σ 3砂 It is the stress between non-cemented tailing sand and cemented backfill, and is the lateral pressure of non-cemented tailing sand on cemented backfill.
[0145] Usually, after the uncemented tailings are dehydrated in the stope, they can be regarded as loose media, and the cohesive force of the tailings is assumed to be zero. At this time, it is assumed that the unit volume on the contact surface between the tailings and the cemented filling is 1砂 and σ 3砂 If the unit cell is in a state of limit equilibrium under stress conditions, then in the rectangular coordinate system composed of normal stress and shear stress, the strength curve of the unit cell is tangent to the stress Mohr circle.
[0146] The triangular relationship between AB and OB is:
[0147]
[0148]
[0149] or
[0150]
[0151] Formula (12) is processed as follows:
[0152]
[0153] According to the following trigonometric relationship:
[0154] sin A-sin B=2cos[(A+B) / 2]sin[(AB) / 2]
[0155] sin A+sin B=2 sin[(A+B) / 2]cos[(AB) / 2] (14)
[0156] According to the trigonometric function relationship shown in formula (14), formula (14) can be rewritten as:
[0157]
[0158]
[0159] According to the following trigonometric relationship:
[0160]
[0161]
[0162] According to the trigonometric function relationship shown in formula (16), formula (16) can be rewritten as:
[0163]
[0164]
[0165]
[0166]
[0167]
[0168] Considering the compression characteristics of tailings in the stope, the lateral pressure of tailings filling body of any height on the cemented filling body can be obtained:
[0169]
[0170] Formula (18) is the calculation formula for the lateral pressure of tailings on cemented backfill.
[0171] Considering the contact area between the graded tailings and the cemented backfill, the resultant force of the graded tailings on the lateral pressure of the cemented backfill is:
[0172]
[0173] Formula (19) is the calculation formula for the resultant pressure of tailings on the side of cemented backfill.
[0174] Taking the Dahongshan Copper Mine as an example, the tailings self-weight compaction model (17) is substituted into the calculation formula (19) of the lateral pressure to analyze the relationship between the lateral pressure of graded tailings on the cemented filling body and the height under the condition of a stope height of 60m. The internal friction angle of graded tailings is 20°, and the calculation process of the lateral pressure of tailings on the cemented filling body is as follows:
[0175]
[0176] ρ h1 =1.027ρ01 (h+0.6116) 0.05272
[0177]
[0178]
[0179] The lateral pressure of graded tailings on the cemented filling body increases with the increase of height, and is distributed in a triangle over the entire height of the cemented filling body. Compared with the lateral pressure calculated by using the density of graded tailings in a naturally loose state, the lateral pressure calculated by this method is larger.
[0180] Taking the Weng'an Daxin Beidoushan Phosphate Mine as an example, the calculation formula (19) of the tailings self-weight compaction model (17) shows the relationship between the change of the tailings' lateral pressure on the cemented backfill body with height under the conditions of a mining site height of 60m and a length of 20m. The internal friction angle of the tailings is 20°, and the calculation process of the tailings' lateral pressure on the cemented backfill body is as follows:
[0181]
[0182] ρ h1 =1.027ρ 01 (h+0.6116) 0.05272
[0183]
[0184]
[0185] The combined lateral pressure of graded tailings on the cemented filling increases with the increase of height, and the growth rate of the combined force of tailings on the cemented filling also increases. Compared with the combined force calculated by using the density of graded tailings in a natural loose state, the combined lateral pressure calculated by this method is larger. According to formula (20), it can be calculated that the use of cementing materials with different weight ratios in different application environments can meet the strength requirements and have the lowest cost.
[0186] In the above embodiment, the coarse aggregate size is greater than or equal to 15 mm and less than or equal to 20 mm, the tailings are below 200 mesh, the ultrafine phosphorus slag powder is below 100 mesh, the weight ratio of tailings to ultrafine phosphorus slag powder is 4:6, the fine aggregate concentration is equal to 0.45%, and the tailings slurry density is equal to
[0187] The preparation, curing and strength determination of compressive strength specimens were carried out in accordance with the provisions of JGJ / T70-2009 "Standard for Test Methods of Basic Properties of Building Mortar". The specimens were prepared into 70.7mm*70.7mm*70.7mm standard test blocks, the curing temperature was (14±3) degrees Celsius, and the relative humidity was (73±5)%. Sampling was carried out according to the amount of empty space in the filling mine room. Every 2000m 3 Sampling was performed once, with 9 test blocks in 3 groups each time. Random sampling was performed every 1-2 hours during the filling process, with 3 test blocks at a time.
[0188] The weight ratio of water, cement, aggregate and tailings is 1:4:3:13. The mixed raw materials are used to fill the subdivision, high-layer bottom pillar, top pillar, single pillar, boundary pillar and mine room top. According to the test, the compressive strength at 28 days is greater than 2MPa under this ratio.
[0189] The weight ratio of water, cement, aggregate and tailings is 1:6:11:26. The mixed raw materials are used to fill the mine room with a depth of more than 15 meters in the layers and sections and the retaining wall area of the pillars. According to the test, the compressive strength at 28 days is greater than 1.4MPa under this ratio.
[0190] The weight ratio of water, cement, aggregate and tailings is 1:8:24:44. The mixed raw materials are used to fill the area above the pillar mining retaining wall with a span of more than 15 meters in the layer or segment. According to the test, the compressive strength at 28 days is greater than 0.8MPa under this ratio.
[0191] The weight ratio of water, cement, aggregate and tailings is 1:10:23:72. The mixed raw materials are used to fill the area above the pillar mining retaining wall with a span of more than 30 meters in the layer or segment, and the open area without mining activities. According to the test, the compressive strength at 28 days is greater than 0.5MPa under this ratio.
[0192] The weight ratio of water, cement, ultrafine phosphorus slag powder, aggregate and tailings is 10:28:12:30:130. The mixed raw materials are used to fill single pillars with a low segmentation of less than 15 meters, boundary pillars, and mine room roofs. According to tests, the compressive strength at this ratio is greater than 1.7MPa at 28 days.
[0193] The weight ratio of water, cement, ultrafine phosphorus slag powder, aggregate and tailings is 10:42:18:110:260. The mixed raw materials are used to fill the mine room with a span of less than 15 meters in the layer or segment and the pillar mining retaining wall area. According to the test, the compressive strength at 28 days is greater than 1.2MPa under this ratio.
[0194] The weight ratio of water, cement, ultrafine phosphorus slag powder, aggregate and tailings is 10:56:24:240:440. The mixed raw materials are used to fill the area above the pillar mining retaining wall with a span of less than 15 meters in the layer or segment. According to the test, the compressive strength at 28 days is greater than 0.7MPa under this ratio.
[0195] The weight ratio of water, cement, ultrafine phosphorus slag powder, aggregate and tailings is 1:7:3:23:72. The mixed raw materials are used to fill the area above the pillar mining retaining wall with a span of less than 15 meters in the layer or segment, the area above the pillar mining retaining wall with a span of more than 30 meters in the layer or segment, and the open area without mining activities. According to the test, the compressive strength at 28 days at this ratio is greater than 0.5MPa.
[0196] Cement unit price From the unit price of cementitious materials, the unit price of cement in one cubic meter of filling slurry is 81.6 to 79.2 yuan, compared with the 1 / 6 lime-sand ratio (91.2 yuan / m 3 ) The cement cost per cubic meter of filling slurry can be reduced by 11.8%.
Claims
1. An upward layered filling mining method, characterized in that: The steps include: S100: rock mass is broken by rock drilling and blasting; in the vein tunnel, a rock drilling rig is used to drill downward vertical parallel deep holes with a hole diameter of 100 mm and a row spacing of 2 m; in the segmented vein drilling tunnel, a rock drilling rig is used to construct downward fan-shaped holes with a hole diameter of 100 mm, a row spacing of 2 to 2.5 m, and a hole bottom distance of 2.1 to 2.5 m; the downward fan-shaped holes are retreated from the middle trough area to the ore loading access road of the mine room to collapse the ore in stages; emulsion explosive matrix and sensitizer are mixed in the hole to form emulsion explosive; the blast hole (10) adopts a non-coupled intermittent filling charging structure, each row of holes is charged and blasted at one time, 2 to 5 rows are blasted each time, and the pushing distance is 6 to 12m; the amount of explosives for each blast is controlled below 1.5 tons, and the maximum amount of explosives for a single shot is controlled within 100kg; when charging the downward fan-shaped hole, a length of 1.5 to 2m is left from the surface of the explosive to the hole mouth without charging, and after charging, the explosives are blocked with gun mud, the blocking length of which is not less than 50cm, and the outer mouth of the blast hole (10) is blocked with a wooden plug or river sand; a non-electric annular detonating network is adopted, an explosive bag is placed at the bottom of the blast hole (10) and two same-segment differential detonators are inserted; the end of the detonating cord is led out of the hole, and then all the same-segment differential detonating cords are divided into two bundles, which are respectively tied to the auxiliary short detonating cords, and the auxiliary short detonating cords are respectively tied to the main detonating cords; Glue the lead end of the main detonating cord to the instantaneous detonator, and finally lead the detonating cord to a safe distance and detonate it with a detonator. The distance between the detonation point and the blasting operation site should be greater than or equal to 200m; S200: Mining: first mine the lowest layer of ore, and arrange the mine room along the vein direction. The width of the pillar is 12 meters, the width of the mine room is 18 meters, the height of the pillar and the mine room is equal to 15 meters, and the length of the pillar and the mine room is equal to the horizontal thickness of the ore body; first mine the pillar, and after mining the pillar, fill the pillar with a high-strength tailings cement (8), and then mine the mine room. After mining the current layer, mine upward layer by layer using the above method; the step S200 also includes the following contents: each layer is arranged along the strike of a segmented tunnel (3), and the segmented tunnel (3) is divided into The segment tunnel (3) is connected to the slope tunnel (1) through a stone gate (4), and the middle transport tunnel (2) serves to connect the segment tunnels (3); a through-vein tunnel is set in the middle of each ore block, and the through-vein tunnel is constructed from the segment tunnel (3) to the top plate of the ore body. Each through-vein tunnel also serves as the mining tunnel (5) of the upper segment and the rock drilling tunnel of the lower segment; a cutting tunnel is arranged along the strike direction in the vein of the top plate of the ore body, which also serves as the return air tunnel (7); a through-vein tunnel is arranged in the vein in the top plate direction of each ore block. A cutting shaft also serves as a return air shaft (6); the upper layer through-vein tunnel serves as a downward fan-shaped deep-hole rock drilling tunnel, and the lower layer through-vein tunnel serves as a channel for shoveling and transporting ore out of the mine; a filling retaining wall (9) is built at the end of the filling. After the filling is completed, the high-strength tailings cementation body (8) reaches a maintenance cycle of 28 days, and the upper layer rock drilling tunnel serves as a channel for shoveling and transporting the upper layer out of the mine; during the blasting of the mining area, the collapsed ore remains in the mining area to provide temporary support for the ore rock or filling body on both sides; the mining area blasting The ore is removed after one crushing until the mining is completed; the residual ore in the mining chamber is cleaned by a remote-controlled scraper to avoid direct personnel entering the empty site for operation; large pieces of ore are transported to the nearby loading access for secondary crushing, and the ore size is controlled to be less than 500 mm; before filling with a high-strength tailings cementing body (8), an expansion layer is laid on the bottom, the expansion layer is composed of the following raw materials by weight: 10 parts of water, 72 parts of cement, and 7 parts of calcium sulfate, and the thickness of the expansion layer is 20 cm; The high-strength tailings cement (8) comprises water, cement, ultrafine phosphorus slag powder, aggregate and tailings, wherein the weight ratio of water, cement, ultrafine phosphorus slag powder, aggregate and tailings is 10:28:12:30:130, and the mixed raw materials are used to fill single ore pillars with a length of less than 15 meters, boundary ore pillars, and mine room roofs; The weight ratio of water, cement, ultrafine phosphorus slag powder, aggregate and tailings is 10:42:18:110:
260. The mixed raw materials are used to fill the mine room with a span of less than 15 meters in the layer or segment and the pillar mining retaining wall area; The weight ratio of water, cement, ultrafine phosphate slag powder, aggregate and tailings is 10:56:24:240:
440. The mixed raw materials are used to fill the area above the pillar mining retaining wall with a span of less than 15 meters in the layer or segment; the weight ratio of water, cement, ultrafine phosphate slag powder, aggregate and tailings is 1:7:3:23:
72. The mixed raw materials are used to fill the area above the pillar mining retaining wall with a span of less than 15 meters in the layer or segment, the area above the pillar mining retaining wall with a span of more than 30 meters in the layer or segment, and the empty area where no mining activities are carried out.