Device and method for preparing metal particles with controllable particle size
By adjusting the vibration frequency and condensate flow rate, combined with temperature and pressure detection, the controllable preparation of metal particles is achieved, and the problems of uncontrollable particle size and environmental hazards in the existing technology are solved, and the accuracy and safety of the product are improved. sex.
Patent Information
- Application Number
- CN202111494143.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-08
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2041-12-08
AI Technical Summary
The prior art is difficult to achieve controllable preparation of metal powder particle size, and there are problems of environmental hazards and biological application risks.
By adjusting the vibration frequency and the condensed water flow rate, the sealing structure of the evaporation device and the reaction device is used to combine temperature, pressure and particle size detection to adjust the heating temperature and condensed water flow rate in real time to control the particle size of the metal particles.
The controllable preparation of metal particle sizes is achieved, the accuracy and consistency of the product is improved, and environmental and biological risks are reduced.
Smart Images

Figure CN114160800B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of metal powder preparation, and in particular relates to a device and a method for preparing metal particles with controllable particle size. Background Art
[0002] In recent years, with the increasing requirements of industrial development for metal injection molding, thermal spraying, metal rapid prototyping, surface mounting and other technologies, the geometric properties of metal powders, especially the controllability of particle size, are becoming increasingly important for ensuring the accuracy and consistency of high-quality products. For example, the uniformity of metal powder particle size not only affects the output of metal injection molded parts, but also helps to ensure the reliability and consistency of the injection molding process; the controllability of metal powder particle size will significantly affect the viscosity, thereby affecting the use of adhesives, degreasing characteristics, shrinkage of blanks, sintering characteristics, final density and surface quality; in order to ensure the coating quality of plasma spraying and high-speed flame spraying, the particle size of metal powders must be within a controllable range so that the molten particles are in basically the same state when they reach the substrate, otherwise, particles that are too large will have already solidified, and particles that are too small will have already evaporated.
[0003] Common methods for preparing metal nanoparticles with controllable particle size include chemical reduction, laser ablation, electrochemistry, microwave irradiation, etc. These preparation methods use organic solvents, or rely on toxic reducing agents, stabilizers, or inevitably produce toxic byproducts, which may cause potential environmental hazards and risks in biological applications. Therefore, it is of great significance to prepare metal nanoparticles with controllable size in an environmentally friendly way.
[0004] CN01140401.9 discloses an ultrasonic atomization preparation method and device for producing spherical metal powder, including the process of prefabricating alloy ingots, vacuuming and backfilling with inert gas, smelting, ultrasonic atomization, cooling and powder collection, screening, packaging and performance testing, finished product packaging and the like; the ultrasonic energy concentrator is composed of an energy concentrator head, a variable amplitude rod, a piezoelectric ceramic sheet, metal upper and lower pressure covers and locking bolts; although it can prepare metal powder with spherical particles, it cannot achieve controllable preparation of the metal powder particle size.
[0005] Therefore, the uncontrollable particle size of the prepared metal particles has become a technical problem that needs to be urgently solved in this field. Summary of the invention
[0006] In view of the defects existing in the above-mentioned prior art, the object of the present invention is to provide an apparatus and a method for preparing metal particles with controllable particle size, and metal particles with controllable particle size can be obtained by adjusting the vibration frequency and the condensed water flow rate.
[0007] To this end, the present invention adopts the following technical solution:
[0008] In a first aspect, the present invention provides an apparatus for preparing metal particles with controllable particle size, comprising:
[0009] an evaporation device for containing a metal raw material;
[0010] A reaction device, on which a feed port connected to the evaporation device is provided, and the reaction device and the evaporation device are connected to form a sealed structure as a whole;
[0011] A detection assembly, comprising a temperature sensor for detecting the temperature of the evaporation device, a pressure sensor for detecting the pressure of the reaction device, and a particle size analyzer for detecting the particle size of metal particles in the reaction device;
[0012] a regulating assembly, comprising a heat exchanger for exchanging heat with the reaction device and a heater for heating the evaporation device;
[0013] A vibration component is arranged in the reaction device and located above the feed port, and the vibration component is used to vibrate at a set frequency when the metal vapor passes through;
[0014] A control component is signal-connected to the detection component, the adjustment component and the vibration component, and is used to select the heating temperature of the heater according to the type of the metal raw material, and to adjust the heating temperature of the heater in real time according to the detection results of the temperature sensor and the pressure sensor; and is also used to control the vibration frequency of the vibration component and the flow rate of the condensed water in the heat exchanger according to the detection results of the particle size analyzer.
[0015] Wherein, the pressure of the reaction device is 0.05-0.1MPa, and the temperature of the evaporation device is 700℃-1200℃.
[0016] Wherein, the vibration frequency of the vibration component is 5-10KHZ.
[0017] In a second aspect, the present invention further provides a method for preparing metal particles using the above-mentioned device, comprising:
[0018] The metal raw material to be prepared is placed in the evaporation device, and the control component selects the initial heating temperature of the heater to heat the metal raw material to form metal vapor;
[0019] The metal vapor enters the reaction device through the feed port, and the control component controls the condensed water in the heat exchanger to cool the metal vapor in the reaction device at a predetermined flow rate;
[0020] During the cooling process, the pressure sensor, temperature sensor and particle size analyzer transmit the test results to the control component, which processes the test results and adjusts the heating temperature of the heater, the flow rate of the condensed water in the heat exchanger and the vibration frequency of the vibration component in real time according to the processing results;
[0021] When the metal raw materials are completely evaporated and condensed, the preparation of metal particles is completed;
[0022] The control component processes the detection results, including:
[0023] Select the appropriate pre-adjusted particle size range according to the type of metal raw material to be prepared and the target particle size range;
[0024] The control component receives the particle size data of the condensed metal particles detected by the particle size analyzer, and adjusts the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger according to the preset particle size range.
[0025] Wherein, before the control component selects the initial heating temperature of the heater to heat the metal raw material, it also includes:
[0026] Inert gas is introduced into the reaction device, and vacuum treatment is performed to make the pressure in the reaction device reach the initial pressure value.
[0027] Wherein, the predetermined flow rate of the condensed water in the heat exchanger is obtained according to the initial heating temperature, the initial pressure value and the target particle size range.
[0028] The control component processes the detection result, and adjusts the heating temperature of the heater, the flow rate of the condensed water in the heat exchanger and the vibration frequency of the vibration component in real time according to the processing result, and also includes:
[0029] Obtaining a pre-adjusted temperature according to a detection result of a pressure sensor, an initial pressure value, and a detection result of a temperature sensor;
[0030] The heating temperature of the heater is adjusted according to the pre-adjusted temperature.
[0031] Wherein, when adjusting the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger according to the pre-adjusted particle size range, it includes:
[0032] Calculate the minimum absolute value of the difference between the preset particle size range and the metal particle size.
[0033] The control component starts adjusting the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger according to the minimum absolute value;
[0034] Wherein, the adjustment of the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger includes a first mode and a second mode, the first mode is to adjust the flow rate of the condensed water in the heat exchanger, and the second mode is to adjust the vibration frequency of the vibration component;
[0035] When the minimum absolute value of the difference is less than the predetermined difference, the first mode is activated; when the minimum absolute value of the difference is greater than or equal to the predetermined difference, the second mode is activated.
[0036] Wherein, when adjusting the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger according to the pre-adjusted particle size range, it includes:
[0037] Obtain the change trend of the minimum absolute value within a single time period that exceeds the preset particle size range;
[0038] The control component starts parameter adjustment of the vibration frequency of the vibration component and / or the flow rate of condensed water in the heat exchanger according to the change trend of the minimum absolute value;
[0039] The parameter adjustment of the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger includes a third mode and a fourth mode, wherein the third mode is to keep the vibration frequency and / or the adjustment parameters of the heat exchanger unchanged, and the fourth mode is to increase the amplitude of the vibration frequency and / or the adjustment parameters of the heat exchanger;
[0040] When the minimum absolute value gradually decreases, the third mode is activated; when the minimum absolute value remains unchanged or gradually increases, the fourth mode is activated.
[0041] Among them, when it is judged that the particle size of the metal particles is outside the pre-adjusted particle size range, the control component adjusts the flow rate value and adjustment time of the condensed water in the heat exchanger, as well as the vibration frequency and vibration time of the vibration component according to the amplitude exceeding the pre-adjusted particle size range and the proportion of the steam volume in the entire condensation process, so that the average particle size of the prepared metal powder is within the target particle size range.
[0042] Wherein, the target particle size range is 0.1-50 μm, and the predetermined difference is 3-5 μm.
[0043] The present invention heats the metal raw material to generate metal vapor, condenses the metal vapor through a heat exchanger, and simultaneously controls the component to adjust the heating temperature of the heater in real time according to the pressure change of the reaction device, thereby achieving a dynamic balance between temperature and pressure and increasing the anti-interference capability of the device. Furthermore, by adjusting the vibration frequency of the vibration component and the flow rate of the condensed water in the heat exchanger, the particle size of the prepared metal particles can be controlled. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] By reading the detailed description below with reference to the accompanying drawings, the above and other purposes, features and advantages of the exemplary embodiments of the present disclosure will become readily understood. In the accompanying drawings, several embodiments of the present disclosure are shown in an exemplary and non-limiting manner, and the same or corresponding reference numerals represent the same or corresponding parts, wherein:
[0045] Figure 1 is a schematic structural diagram of a device for preparing metal particles with controllable particle size according to an embodiment of the present invention;
[0046] Figure 2is a schematic diagram of a device for preparing metal particles with controllable particle size according to an embodiment of the present invention;
[0047] Figure 3 is a flow chart of preparing metal particles according to an embodiment of the present invention.
[0048] Description of reference numerals:
[0049] 1-evaporation device, 2-reaction device, 3-detection component, 31-pressure sensor, 4-regulation component, 41-heat exchanger, 42-heater, 5-vibration component, 6-control component. DETAILED DESCRIPTION
[0050] In order to make the purpose, technical scheme and advantages of the present invention clearer, the present invention will be further described in detail below with reference to the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0051] The terms used in the embodiments of the present invention are only for the purpose of describing specific embodiments, and are not intended to limit the present invention. The singular forms "a", "said" and "the" used in the embodiments of the present invention and the appended claims are also intended to include plural forms, unless the context clearly indicates other meanings, and "multiple" generally includes at least two.
[0052] It should also be noted that the term "includes", "comprising" or any other variation thereof is intended to cover non-exclusive inclusion, so that a commodity or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such commodity or device. In the absence of more restrictions, the elements defined by the sentence "comprising a ..." do not exclude the existence of other identical elements in the commodity or device including the elements.
[0053] The optional embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0054] See also Figure 1 and Figure 2 As shown, this embodiment provides a device for preparing metal particles with controllable particle size, comprising:
[0055] An evaporation device 1 for containing a metal raw material;
[0056] The reaction device 2 is provided with a feed port connected to the evaporation device 1, and the reaction device 2 and the evaporation device 1 are connected to form a sealed structure;
[0057] The detection component 3 includes a temperature sensor for detecting the temperature of the evaporation device 1, a pressure sensor 31 for detecting the pressure of the reaction device 2, and a particle size analyzer for detecting the particle size of the metal particles in the reaction device 2; wherein the particle size result of the metal particles detected by the particle size analyzer is an average particle size, which can be obtained according to the particle size distribution;
[0058] A regulating assembly 4, which includes a heat exchanger 41 for exchanging heat with the reaction device 2 and a heater 42 for heating the evaporation device 1;
[0059] A vibration component 5 is arranged in the reaction device 2, located above the feed port and at least partially covering the feed port, and the vibration component 5 is used to vibrate at a set frequency when the metal vapor passes through;
[0060] The control component 6 is signal-connected to the detection component 3, the adjustment component 4 and the vibration component 5, and is used to select the heating temperature of the heater 42 according to the type of metal raw material, and to adjust the heating temperature of the heater 42 in real time according to the detection results of the temperature sensor and the pressure sensor 31; it is also used to control the vibration frequency of the vibration component 5 and the flow rate of the condensed water in the heat exchanger 41 according to the detection results of the particle size analyzer.
[0061] In this embodiment, the heater 42 is used to heat the metal raw material in the evaporation device 1 to generate metal vapor, and the metal vapor entering the reaction device 2 is condensed through the heat exchanger 41 to form metal particles; during the condensation process, the control component 6 of this embodiment adjusts the heating temperature of the heater 42 in real time according to the pressure change of the reaction device 2, achieving a dynamic balance between temperature and pressure and increasing the anti-interference ability of the equipment. In addition, this embodiment detects the particle size results of the condensed metal particles to adjust the vibration frequency of the vibration component 5 and the flow rate of the condensed water in the heat exchanger 41, thereby achieving controllable particle size of the prepared metal particles.
[0062] The vibration component 5 in this embodiment can select different structures according to different scenarios to achieve vibration at a certain frequency when the metal vapor passes through. In an application scenario, the vibration component 5 of this embodiment may include a vibration plate that partially or completely covers the feed port and a vibration motor fixed on the vibration plate, and the vibration plate is elastically connected to the reaction device 2. Exemplarily, the vibration plate is connected to the reaction device 2 through a plurality of springs. In the actual application scenario, when the metal vapor enters the reaction device 2 through the feed port, it will pass through the vibration plate, and the vibration motor located on the vibration plate will drive the vibration plate to vibrate at a predetermined frequency. The vibration of the vibration plate will cause the passing metal vapor to condense into metal particles with a smaller particle size, so that controlling the vibration frequency of the vibration plate can make the final prepared metal powder reach a predetermined particle size.
[0063] This embodiment takes the preparation of magnesium metal particles as an example. When heating and evaporating the magnesium metal raw material, the evaporation device 1 can be heated to 700°C-1200°C by the heater 42, the pressure of the reaction device 2 can be adjusted to 0.05-0.1MPa, and the flow rate of the condensed water in the heat exchanger 41 can be adjusted to 5-25L / min; when the metal vapor passes through the vibration component 5, the vibration frequency of the vibration component 5 is 5-10KHZ. By adjusting the various parameters in the magnesium metal preparation process, the device of this embodiment can prepare ultrafine metal powder with a particle size of 0.1-50μm.
[0064] See also Figure 3 As shown, this embodiment also provides a method for preparing metal particles using the above-mentioned device, comprising:
[0065] The metal raw material to be prepared is placed in the evaporation device 1, an inert gas is introduced into the reaction device 2, and a vacuum treatment is performed so that the pressure in the reaction device 2 reaches the initial pressure value;
[0066] The control component 6 selects the initial heating temperature of the heater 42 to heat the metal raw material to form metal vapor;
[0067] The metal vapor enters the reaction device 2 through the feed port, and the control component 6 controls the condensed water in the heat exchanger 41 to cool the metal vapor in the reaction device 2 at a predetermined flow rate; wherein the predetermined flow rate of the condensed water in the heat exchanger 41 is obtained according to the initial heating temperature, the initial pressure value and the target particle size range;
[0068] During the cooling process, the pressure sensor 31, the temperature sensor and the particle size analyzer transmit the detection results to the control component 6, and the control component 6 processes the detection results and adjusts the heating temperature of the heater 42, the flow rate of the condensed water in the heat exchanger 41 and the vibration frequency of the vibration component 5 in real time according to the processing results;
[0069] When the metal raw materials are completely evaporated and condensed, the preparation of metal particles is completed;
[0070] The control component 6 processes the detection result, including:
[0071] Select the appropriate pre-adjusted particle size range according to the type of metal raw material to be prepared and the target particle size range;
[0072] The control component 6 receives the particle size data of the condensed metal particles detected by the particle size analyzer, and adjusts the vibration frequency of the vibration component 5 and / or the flow rate of the condensed water in the heat exchanger 41 according to the pre-adjusted particle size range. In actual application, this embodiment compares the particle size of the metal particles with the pre-adjusted particle size range, and if the particle size of the metal particles is outside the pre-adjusted particle size range, the vibration frequency of the vibration component 5 and / or the flow rate of the condensed water in the heat exchanger 41 is adjusted.
[0073] In this embodiment, the control component 6 processes the detection result, and adjusts the heating temperature of the heater 42, the flow rate of the condensed water in the heat exchanger 41, and the vibration frequency of the vibration component 5 in real time according to the processing result, which may specifically include:
[0074] The pre-adjusted temperature is obtained according to the detection result of the pressure sensor 31, the initial pressure value and the detection result of the temperature sensor;
[0075] The heating temperature of the heater 42 is adjusted according to the pre-adjustment temperature.
[0076] In actual application scenarios, during the continuous evaporation of metal raw materials, the detection results of the pressure sensor 31 will increase to a certain extent. When the pressure increases, the particle size of the metal particles will increase. Therefore, in order to obtain metal particles with smaller particle sizes and to control the metal particle size, it is necessary to reduce the pressure to a certain extent. In this embodiment, the heating temperature of the heater 42 is changed to achieve the purpose of adjusting the pressure.
[0077] In this embodiment, when adjusting the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger 41 according to the preset particle size range, the method includes:
[0078] Calculate the minimum absolute value of the difference between the preset particle size range and the metal particle size,
[0079] The control component 6 starts adjusting the vibration frequency of the vibration component 5 and / or the flow rate of the condensed water in the heat exchanger 41 according to the minimum absolute value;
[0080] The adjustment of the vibration frequency of the vibration component 5 and / or the flow rate of the condensed water in the heat exchanger 41 includes a first mode and a second mode. The first mode is to adjust the flow rate of the condensed water in the heat exchanger 41, and the second mode is to adjust the vibration frequency of the vibration component 5.
[0081] When the minimum absolute value of the difference is less than the predetermined difference, the first mode is activated; when the minimum absolute value of the difference is greater than or equal to the predetermined difference, the second mode is activated.
[0082] In this embodiment, the particle size of the metal particles can be finely adjusted by starting the first mode, that is, adjusting the flow rate of the condensed water in the heat exchanger 41 to achieve fine adjustment of the particle size of the metal particles, and the second mode, that is, adjusting the vibration frequency of the vibration component 5 to achieve coarse adjustment of the metal particles, so that the particle size of the metal particles finally prepared can be more accurately adjusted. In an application scenario, the predetermined difference determined by the fine adjustment and coarse adjustment in this embodiment can be within 3-5μm.
[0083] In addition, when the particle size of the metal particles of the present embodiment is outside the pre-adjusted particle size range, when the maximum value of the difference between the particle size of the metal particles and the endpoint values of the pre-adjusted particle size range is a negative value, the particle size of the metal particles is changed by adjusting the flow rate of the condensed water in the heat exchanger 41. Among them, it is necessary to make the pre-adjusted particle size range of the present embodiment within the target particle size range. For example, when the target particle size range is 0.1-50μm, the pre-adjusted particle size range can be 15-35μm. In addition, the target particle size range of the present embodiment is the range within which the particle size of the metal particles finally prepared is expected to be obtained. The pre-adjusted particle size range is the range value when adjusting according to the average particle size of the metal particles detected by the particle size analyzer. By making the average particle size of the metal particles within the pre-adjusted particle size range, the actual particle size of the prepared metal particles can be made as much as possible within the target particle size range.
[0084] In this embodiment, when the particle size of the metal particles is outside the pre-adjusted particle size range and the heat exchanger 41 and the vibration component 5 are adjusted, the following steps may be included:
[0085] Obtain the change trend of the minimum absolute value within a single time period that exceeds the preset particle size range;
[0086] The control component 6 starts adjusting the vibration frequency of the vibration component 5 and / or the flow rate of the condensed water in the heat exchanger 41 according to the variation trend of the minimum absolute value;
[0087] The parameter adjustment of the vibration frequency of the vibration component 5 and / or the flow rate of the condensed water in the heat exchanger 41 includes a third mode and a fourth mode. The third mode is to keep the vibration frequency and / or the adjustment parameters of the heat exchanger 41 unchanged, and the fourth mode is to increase the amplitude of the vibration frequency and / or the adjustment parameters of the heat exchanger 41.
[0088] When the minimum absolute value gradually decreases, the third mode is activated; when the minimum absolute value remains unchanged or gradually increases, the fourth mode is activated.
[0089] In actual application scenarios, when obtaining the changing trend of the minimum absolute value in a single time period that exceeds the preset particle size range, it can be judged by calculating the difference between the minimum absolute value at the current moment and the minimum absolute value at the previous moment in the single time period that exceeds the preset particle size range. Specifically, if the difference between the minimum absolute value at the current moment and the minimum absolute value at the previous moment in the single time period that exceeds the preset particle size range is greater than or equal to zero, the minimum absolute value is gradually increasing or unchanged, indicating that the adjusted flow rate value of the condensed water in the heat exchanger 41 and / or the vibration frequency of the vibration component 5 are not sufficient to make the particle diameter of the metal powder close to the preset particle size range. Therefore, when the flow rate value of the condensed water in the heat exchanger 41 and / or the vibration frequency of the vibration component 5 is increased, the flow rate value of the condensed water in the heat exchanger 41 and / or the vibration frequency of the vibration component 5 are further increased on the basis of the original increase; when the flow rate value of the condensed water in the heat exchanger 41 and / or the vibration frequency of the vibration component 5 are reduced, the flow rate value of the condensed water in the heat exchanger 41 and / or the vibration frequency of the vibration component 5 are further reduced on the basis of the original reduction; the amplitude of further increase and reduction can be selected according to a certain multiple relationship (for example, it can be increased or reduced by 0.2 times on the original basis). If the difference between the minimum absolute value at the current moment and the minimum absolute value at the previous moment in a single time period that exceeds the pre-adjusted particle size range is less than zero, the minimum absolute value is gradually decreasing, indicating that the adjusted flow rate value of the condensed water in the heat exchanger 41 and / or the vibration frequency of the vibration component 5 can make the particle diameter of the metal powder close to the pre-adjusted particle size range. Therefore, the flow rate value of the condensed water in the heat exchanger 41 and the vibration frequency of the vibration component 5 can be maintained to make the particle diameter of the metal powder close to the pre-adjusted particle size range.
[0090] In this embodiment, when it is determined that the particle size of the metal particles is outside the pre-adjusted particle size range, the control component 6 can adjust the flow rate value and adjustment time of the condensed water in the heat exchanger 41, as well as the vibration frequency and vibration time of the vibration component 5 according to the amplitude exceeding the pre-adjusted particle size range and the proportion of the steam volume in the entire condensation process, so that the particle size of the prepared metal particles is within the target particle size range. In actual application scenarios, if the amplitude exceeding the pre-adjusted particle size range is 7μm, the proportion of the steam volume evaporated from the metal raw material in the entire condensation process is 5%, the flow rate of the condensed water in the heat exchanger 41 is adjusted to 9L / min, the adjustment time is 10s, and the vibration frequency of the vibration component 5 is 7.8KHZ and the vibration time is 10s.
[0091] In order to facilitate the understanding of the overall solution by those skilled in the art, this embodiment describes the preparation process from the perspective of metal raw materials, which may specifically include:
[0092] The metal raw material is heated and evaporated in the evaporation device 1 to form metal vapor. When the metal vapor enters the reaction device 2, it is condensed under a certain pressure to generate metal particles. In the process of generating metal particles, it passes through the vibration component 5, and due to the vibration effect of the vibration component 5, the particle size of the metal particles will be further reduced. Among them, the vibration component 5 can have a certain vibration frequency at the beginning, and can also be started when the particle size detected by the particle size analyzer does not meet the standard. The specific operation can be selected according to the actual situation. This embodiment achieves precise control of the particle size of the metal particles by controlling the heating temperature, pressure, condensation water rate and vibration frequency.
[0093] The above introduces the preferred embodiments of the present invention, which is intended to make the spirit of the present invention clearer and easier to understand, but is not intended to limit the present invention. All modifications, substitutions, and improvements made within the spirit and principles of the present invention should be included in the scope of protection outlined by the claims attached to the present invention.
Claims
1. A method for preparing metal particles, characterized in that: Equipment for preparing metal particles with controllable particle size, comprising: an evaporation device for containing a metal raw material; A reaction device, on which a feed port connected to the evaporation device is provided, and the reaction device and the evaporation device are connected to form a sealed structure as a whole; A detection assembly, comprising a temperature sensor for detecting the temperature of the evaporation device, a pressure sensor for detecting the pressure of the reaction device, and a particle size analyzer for detecting the particle size of metal particles in the reaction device; a regulating assembly, comprising a heat exchanger for exchanging heat with the reaction device and a heater for heating the evaporation device; A vibration assembly is arranged in the reaction device and located above the feed port. The vibration assembly is used to vibrate at a set frequency when the metal vapor passes through. The vibration assembly includes a vibration plate that partially or completely covers the feed port and a vibration motor fixed on the vibration plate. The vibration plate is elastically connected to the reaction device. A control component, which is connected to the detection component, the adjustment component and the vibration component by signal, and is used to select the heating temperature of the heater according to the type of the metal raw material, and to adjust the heating temperature of the heater in real time according to the detection results of the temperature sensor and the pressure sensor; and is also used to control the vibration frequency of the vibration component and the flow rate of the condensed water in the heat exchanger according to the detection results of the particle size analyzer; Methods include: The metal raw material to be prepared is placed in the evaporation device, and the control component selects the initial heating temperature of the heater to heat the metal raw material to form metal vapor; The metal vapor enters the reaction device through the feed port, and the control component controls the condensed water in the heat exchanger to cool the metal vapor in the reaction device at a predetermined flow rate; During the cooling process, the pressure sensor, temperature sensor and particle size analyzer transmit the test results to the control component, which processes the test results and adjusts the heating temperature of the heater, the flow rate of the condensed water in the heat exchanger and the vibration frequency of the vibration component in real time according to the processing results; When the metal raw materials are completely evaporated and condensed, the preparation of metal particles is completed; The control component processes the detection results, including: Select the appropriate pre-adjusted particle size range according to the type of metal raw material to be prepared and the target particle size range; The control component receives the particle size data of the condensed metal particles detected by the particle size analyzer, and adjusts the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger according to the preset particle size range; When the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger is adjusted according to the pre-adjusted particle size range, it includes: Calculate the minimum absolute value of the difference between the preset particle size range and the metal particle size. The control component starts adjusting the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger according to the minimum absolute value; Wherein, the adjustment of the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger includes a first mode and a second mode, the first mode is to adjust the flow rate of the condensed water in the heat exchanger, and the second mode is to adjust the vibration frequency of the vibration component; When the minimum absolute value of the difference is less than the predetermined difference, the first mode is started; when the minimum absolute value of the difference is greater than or equal to the predetermined difference, the second mode is started; When the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger is adjusted according to the pre-adjusted particle size range, it also includes: Obtain the change trend of the minimum absolute value within a single time period that exceeds the preset particle size range; The control component starts parameter adjustment of the vibration frequency of the vibration component and / or the flow rate of condensed water in the heat exchanger according to the change trend of the minimum absolute value; The parameter adjustment of the vibration frequency of the vibration component and / or the flow rate of the condensed water in the heat exchanger includes a third mode and a fourth mode, wherein the third mode is to keep the vibration frequency and / or the adjustment parameters of the heat exchanger unchanged, and the fourth mode is to increase the amplitude of the vibration frequency and / or the adjustment parameters of the heat exchanger; If the difference between the minimum absolute value at the current moment and the minimum absolute value at the previous moment in a single time period that exceeds the pre-adjusted particle size range is less than zero, the minimum absolute value is gradually decreasing. When the minimum absolute value gradually decreases, the third mode is started; if the difference between the minimum absolute value at the current moment and the minimum absolute value at the previous moment in a single time period that exceeds the pre-adjusted particle size range is greater than or equal to zero, the minimum absolute value is gradually increasing or unchanged. When the minimum absolute value remains unchanged or gradually increases, the fourth mode is started.
2. The method according to claim 1, characterized in that The pressure of the reaction device is 0.05-0.1 MPa, and the temperature of the evaporation device is 700°C-1200°C.
3. The method according to claim 1, characterized in that The vibration frequency of the vibration component is 5-10KHZ.
4. The method according to claim 1, characterized in that Before the control component selects the initial heating temperature of the heater to heat the metal raw material, the control component also includes: Inert gas is introduced into the reaction device, and vacuum treatment is performed to make the pressure in the reaction device reach the initial pressure value.
5. The method according to claim 4, characterized in that The predetermined flow rate of the condensed water in the heat exchanger is obtained according to the initial heating temperature, the initial pressure value and the target particle size range.
6. The method according to claim 4, characterized in that The control component processes the detection result, and adjusts the heating temperature of the heater, the flow rate of the condensed water in the heat exchanger and the vibration frequency of the vibration component in real time according to the processing result, and also includes: Obtaining a pre-adjusted temperature according to a detection result of a pressure sensor, an initial pressure value, and a detection result of a temperature sensor; The heating temperature of the heater is adjusted according to the pre-adjusted temperature.
7. The method according to any one of claims 1 to 6, characterized in that: When it is determined that the particle size of the metal particles is outside the pre-adjusted particle size range, the control component adjusts the flow rate value and adjustment time of the condensed water in the heat exchanger, as well as the vibration frequency and vibration time of the vibration component according to the amplitude exceeding the pre-adjusted particle size range and the proportion of the steam volume in the entire condensation process, so that the average particle size of the prepared metal powder is within the target particle size range.