A method for manufacturing a super junction planar gate power MOSFET

The manufacturing method of superjunction planar gate power MOSFET through 4-layer photomask and self-alignment technology solves the problems of high cost and high cycle time in the existing technology, realizes the optimization of on-resistance and gate charge, and meets the DC requirements. -Application requirements for DC transformers.

CN114188399BActive Publication Date: 2024-10-11SHENZHEN GUBANG SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111469699.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-03
Publication Date
2024-10-11
Estimated Expiration
2041-12-03

AI Technical Summary

Technical Problem

Existing superjunction power MOSFET devices require multiple photomasks during the manufacturing process, resulting in high manufacturing cycle and cost, and it is difficult to balance the on-resistance and gate charge, affecting the quality factor and efficiency of the device.

Method used

The superjunction planar gate power MOSFET manufacturing method using a 4-layer photomask is used to form p-pillars through self-alignment technology and in-situ selective epitaxial growth. Combined with the planar gate structure, the on-resistance and gate charge are optimized. Reduce photomask alignment errors and improve manufacturing efficiency and yield.

Benefits of technology

It achieves lower on-resistance and gate charge, obtains better quality factor, reduces manufacturing cost and manufacturing cycle, and is suitable for upper and lower MOSFET tube applications of DC-DC transformers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114188399B_ABST
    Figure CN114188399B_ABST
Patent Text Reader

Abstract

The present invention proposes a method for manufacturing a superjunction planar gate power MOSFET that only requires 4 layers of photomasks. The manufacturing method can obtain low on-resistance and lower gate charge. Therefore, a better quality factor (FOM) can be obtained. The main difference from the traditional vertical VDMOS manufacturing method is that the p-column of the superjunction is formed in the n-epitaxial layer by in-situ selective epitaxial growth (insitu-SEG), so that the doping concentration of the p-column and the n-type epitaxial layer achieves charge balance, and the planar gate length can also be minimized to reduce channel resistance and gate charge. In addition, compared with the existing manufacturing method that generally requires 6 layers of photomasks, the present invention can also improve manufacturing efficiency and reduce manufacturing costs.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of semiconductor device and process manufacturing, and relates to a method for manufacturing a planar gate MOSFET, and in particular to a method for manufacturing a super junction planar gate power MOSFET. Background Art

[0002] Superjunction power MOSFET is a majority-carrier conductive unipolar device with no minority-carrier storage effect, fast switching speed, high working efficiency, and low switching loss. At the same time, the on-resistance of superjunction MOSFET devices is small, which effectively reduces the on-state power consumption of the device. Superjunction MOSFET effectively solves the contradiction between breakdown voltage and on-resistance, and has the characteristics of high breakdown voltage and low on-resistance, and is widely used in switching power supplies and synchronous rectification circuits.

[0003] An important application area of ​​superjunction power MOSFET is DC converter. In DC converter, in order to obtain higher conversion efficiency, both conduction and switching power consumption need to be reduced. The current 30V channel power MOSFET can achieve an on-resistance (Rdson) as low as 7mΩ-mm. 2 . However, compared with the planar gate structure LDMOS, since its gate and drain / source have more overlap, it has a higher gate charge (QG). On the other hand, the planar gate structure LDMOS has a higher on-resistance than the trench MOSFET. Therefore, in order to obtain better performance indicators, such as the quality factor (FOM, FOM is the product of the on-resistance Rdson and the gate charge QG), it is necessary to balance the on-resistance and gate charge to obtain a lower quality factor (FOM). For the typical application of DC converters, namely DC-DC, since the power consumption of the lower MOSFET tube is mainly the on-power consumption, it is expected that the lower MOSFET tube has a low on-resistance. However, for the upper MOSFET tube, the switching power consumption is its main power consumption, which requires a lower quality factor (FOM). Therefore, a power MOSFET with both lower on-resistance and better quality factor (FOM) is needed to meet the needs of both the upper and lower MOSFET tubes.

[0004] In addition, the industry knows that fewer photomasks mean shorter manufacturing cycles and more competitive manufacturing costs. However, existing super junction devices, including super junction MOSFET and shielded poly gate MOSFET, generally require six photomasks or more, which leads to high manufacturing cycles and costs for existing devices. In addition to the cycle and cost not being reduced, more photomasks will lead to greater alignment errors during the photomask patterning (i.e., photolithography), which will also affect the yield of the finished product, further pushing up the cost. Summary of the invention

[0005] In the present invention, in view of the problems existing in the prior art, a method for manufacturing a super junction planar gate power MOSFET that only requires 4 layers of photomasks is proposed. Compared with the prior art that uses 6 photomasks, the use of photomasks is reduced, thereby greatly improving the manufacturing efficiency and significantly reducing the manufacturing cost. In addition, the source contact metal layer (source contact) of the present invention adopts a self-alignment technology to avoid the alignment error between the contact metal layer and the source, thereby avoiding the device failure that may be caused by this, and thus improving the yield.

[0006] In the present invention, MOSFET has a super junction structure. The super junction structure can provide low on-resistance, and the planar gate structure provides lower gate charge. Combining these two characteristics, a better flat figure of merit (FOM) can be obtained. Therefore, the device prepared by the manufacturing method of the super junction planar gate power MOSFET proposed in the present invention is suitable for upper and lower MOSFET tubes for DC-DC transformer applications. The main difference from the traditional vertical VDMOS manufacturing method is that the p-column of the super junction is formed in the n-epitaxial layer by in-situ selective epitaxial growth (insitu-SEG), and the doping concentration of the p-column and the n-type epitaxial layer is thus charged balanced, and the planar gate length can also be minimized to reduce the channel resistance and gate charge.

[0007] A method for manufacturing a super junction planar gate power MOSFET comprises the following steps:

[0008] (1) growing an epitaxial layer on a substrate;

[0009] (2) forming a first mask after growing a first oxide layer on the epitaxial layer;

[0010] (3) etching a plurality of deep trenches in the epitaxial layer;

[0011] (4) removing the first mask and the first oxide layer, and selectively growing an epitaxial layer in situ in the deep trench to form a p-column;

[0012] (5) forming a stacked structure on the surface of the epitaxial layer and the P column; the stacked structure sequentially comprises a gate oxide layer, a polysilicon gate layer and a second oxide layer;

[0013] (6) forming a second mask on the surface of the second oxide layer, wherein the epitaxial layer is divided into a first region and a second region; the second mask on the first region has a first groove and a second groove; the second mask on the second region is a complete mask without grooves; etching the stacked structure in the first region by an etching process, etching the second oxide layer, the gate polysilicon layer and the gate oxide layer in sequence, thereby extending the first groove and the second groove downward to expose the upper surface of the p-column and the upper surface of the epitaxial layer;

[0014] (7) removing the second mask and forming a third oxide layer by a deposition process; the third oxide layer completely covers the upper surfaces of the polysilicon gate layer, the p-column, and the epitaxial layer;

[0015] (8) etching the third oxide layer on the first region to form a third trench; the third trench exposes the upper surface of the p-column and the upper surface of the epitaxial layer, and forms an oxide layer sidewall on the side of the stacked structure consisting of the gate oxide layer and the polysilicon gate layer;

[0016] (9) performing an ion implantation process to form a p+ ion implantation region and an n+ ion implantation region in the p column and the epitaxial layer;

[0017] (10) performing an ion diffusion process to form a p+ ion diffusion region and an n+ ion diffusion region; the ion diffusion process is a thermal annealing process. Further, the p+ ion diffusion region is aligned to the edge of the gate oxide layer in the lateral direction, so that the projection of the gate oxide layer in the vertical direction is located within the p+ ion diffusion region;

[0018] (11) etching the p+ ion diffusion region and the n+ ion diffusion region to form a fourth trench; the fourth trench is formed by completely etching the n+ ion diffusion region and partially etching the p+ ion diffusion region in a vertical direction through the etching process;

[0019] (12) spin coating a photoresist on the entire surface of the third oxide layer and patterning the photoresist in the second region to form an opening, and the photoresist after forming the opening serves as a third mask; wherein the opening exposes the upper surface of the third oxide layer;

[0020] (13) using the third mask as protection, etching the third oxide layer to expose the upper surface of the polysilicon gate layer;

[0021] (14) sputtering to form a metal layer; the metal layer completely covers the third oxide layer and completely fills the fourth trench;

[0022] (15) patterning a fourth mask on the metal layer, wherein the fourth mask is retained only at locations where the source electrode and the gate electrode are to be formed;

[0023] (16) etching the metal layer to form a source electrode and a gate electrode;

[0024] (17) A metal layer is formed on the back side of the n+ substrate as a drain electrode.

[0025] The deep trenches in step (3) have a width of 0.4 microns and a depth of 1.2 microns, and the spacing between each deep trench is 1.4 microns.

[0026] Among them, in step (6), the first trench is located directly above the p-column and has a width of 0.8 microns; the width of the stacked structure composed of the patterned gate oxide layer, the gate polysilicon layer and the second oxide layer is 0.3 microns; the width of the second trench formed between the two above-mentioned stacked structures is 0.4 microns. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1-15 A schematic diagram of a method for manufacturing a super junction planar gate power MOSFET proposed in the present invention.

[0028] in,

[0029] Figure 1 A cross-sectional view of growing an epitaxial layer on a substrate.

[0030] Figure 2a and Figure 2b They are a cross-sectional view and a stereoscopic view respectively showing the formation of a channel on the epitaxial layer through the first mask.

[0031] Figure 3a and Figure 3b They are a cross-sectional view and a stereoscopic view of etching the epitaxial layer to form a trench, respectively.

[0032] Figure 4a and Figure 4b They are a cross-sectional view and a stereoscopic view of the in-situ selective epitaxial growth of a P-type structure in a trench, respectively.

[0033] Figure 5a and Figure 5b They are the cross-sectional view and stereoscopic view of the gate oxide layer, polysilicon layer and insulating oxide layer formed after in-situ selective growth of the P-type structure.

[0034] Figure 6a and Figure 6b They are a cross-sectional view and a stereoscopic view respectively of forming a gate through an etching process using a second mask.

[0035] Figure 7a and7b They are a cross-sectional view and a stereoscopic view of depositing an oxide layer on the gate, respectively.

[0036] Figure 8a and Figure 8b They are a cross-sectional view and a stereoscopic view respectively showing etching of a deposited oxide layer to form a side wall.

[0037] Fig. 9 Schematic diagram of the process of ion implantation into the epitaxial layer to form source and body electrodes.

[0038] Fig.10 A schematic diagram of an annealing process performed after an ion implantation process to facilitate ion diffusion.

[0039] Figure 11a-11b They are the cross-sectional view and stereoscopic view of etching the source and body electrodes after the ion diffusion process.

[0040] Figures 11c-11d A three-dimensional view showing the formation of a gate electrode opening.

[0041] Fig.12a and Figure 12b for Fig.11a -d etching process followed by a metal sputtering process to form a cross-sectional view and a three-dimensional view of the metal layer.

[0042] Fig.13 It is a three-dimensional view of forming a fourth mask on the metal layer.

[0043] Fig.14 This is a three-dimensional view after the gate electrode and source electrode are formed.

[0044] Fig.15 It is a three-dimensional view of the MOSFET device structure after the drain electrode is formed.

[0045] The markings in the accompanying drawings are explained as follows. It should be particularly noted that the present invention includes multiple cross-sectional views and stereoscopic views. In order to make the drawings simpler and clearer, the figure markings of the same structure are only marked in the cross-sectional views.

[0046] 100: n+ substrate; 101: n- epitaxial layer; 102: first oxide layer; 103: p-column; 104: gate oxide layer; 105: polysilicon gate layer; 106: second oxide layer; 107: third oxide layer; 108: p+ ion implantation region; 109: n+ ion implantation region; 1081: p+ ion diffusion region; 1091: n+ ion diffusion region; 1082: body electrode; 1092: source region; 110: metal layer; 111: gate electrode; 112: source electrode; 11: first mask; 12: second mask; 13: third mask; 14: fourth mask; 1001: first trench; 1002: second trench; 1003: third trench; 1004: fourth trench; 1301: opening; 1: gate electrode; 2: source electrode; 3: drain electrode; 201: deep trench. DETAILED DESCRIPTION

[0047] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.

[0048] The manufacturing method of the super junction planar gate power MOSFET proposed by the present invention is as follows Figure 1-13 shown.

[0049] See also Figure 1 First, an epitaxial layer (epi) is grown on a substrate. In the present invention, the substrate is an n+ substrate 100, and the epitaxial layer is an n- epitaxial layer 101. Typical substrate materials and epitaxial layer materials are, for example, silicon. The epitaxial growth method used is a vapor phase epitaxial growth method. According to the reaction type, the vapor phase epitaxy of silicon can be divided into a hydrogen reduction method and a direct thermal decomposition method. The hydrogen reduction method uses hydrogen to reduce a vapor phase silicon-containing precursor at a high temperature (e.g., 1200°C) to produce silicon atoms for epitaxial growth on the substrate surface. The direct thermal decomposition method is based on SiH 4 The direct thermal decomposition reaction of the feed gas can achieve epitaxial growth of silicon at a relatively low temperature (eg, 650°C).

[0050] See also Figure 2a and Figure 2b , a first oxide layer 102 is grown on the n-epitaxial layer 101. The first oxide layer 102 can be formed by chemical vapor deposition (CVD), and its material is silicon oxide, silicon nitride, a stack structure of silicon oxide-silicon nitride (ON) or a stack structure of silicon oxide-silicon nitride-silicon oxide (ONO). In the present invention, silicon oxide is preferably used. After the first oxide layer 102 is formed, a photoresist is spin-coated on its surface. The photoresist can be a positive photoresist or a negative photoresist. In the present invention, a positive photoresist is used. The photoresist is patterned by a photolithography mask template to form a first mask 11, and then the first oxide layer 102 is etched to partially expose the upper surface of the n-epitaxial layer 101, forming a Figure 2a and Figure 2b The structure shown.

[0051] See also Figure 3a and Figure 3b , using the first mask 11 as an etching mask, an etching process is used to etch the n-epitaxial layer 101, thereby forming a plurality of vertically steep deep grooves 201 in the n-epitaxial layer 101. The etching process adopted in the present invention is a plasma etching process. In addition, optionally, the photoresist can be removed in advance before the above-mentioned etching process, that is, the first mask 11 is removed. After removing the first mask 11, the remaining first oxide layer 102 actually serves as a hard mask for the etching process. Furthermore, pre-removing the photoresist used as the first mask 11 can prevent the photoresist from producing polymers attached to the side walls of the deep grooves 201 during the plasma etching process, thereby causing the side walls to be uneven or introduce defects due to the attachment of the polymers. In addition, it should be noted that Figure 3a and Figure 3b Only the case where the first mask 11 is not removed is shown, and the case where etching is performed after the first mask 11 is removed is not shown. Figure 3a and Figure 3b The process can be clearly understood based on the above. In the present invention, the deep trench has a width of 0.4 micrometers and a depth of 1.2 micrometers, and the spacing between each deep trench is 1.4 micrometers.

[0052] See also Figure 4a and 4b After forming the deep trench, the first mask 11 and the first oxide layer 102 are removed. The first oxide layer 102 can be removed by chemical method. For example, when the first oxide layer 102 is silicon oxide, it can be removed by wet method of hydrofluoric acid solution. Thereafter, in-situ selective epitaxial growth (in-situ SEG) is used to form a p-column 103 in the deep trench 201. In the present invention, the material of the p-column 103 is p-type doped silicon. In-situ selective epitaxial growth is to supply silicon source gas and n / p-type dopant gas in situ, thereby growing an n / p-type epitaxial layer.

[0053] See also Figure 5a and 5bAfter the p-column 103 is selectively epitaxially grown in situ, a gate oxide layer 104, a polysilicon gate layer 105 and a second oxide layer 106 are sequentially formed on the surface of the n-epitaxial layer 101 and the p-column 103. The gate oxide layer 104 is formed by a thermal oxidation process. The thermal oxidation process can form a dense oxide layer, thereby meeting the gate's requirements for the oxide layer. Both the polysilicon gate layer 105 and the second oxide layer 106 can be formed by chemical vapor deposition. The second oxide layer 106 and the first oxide layer 102 can be made of the same material. Optionally, before the stacking structure of the gate oxide layer 104, the polysilicon gate layer 105 and the second oxide layer 106 is formed after the p-column 103 is selectively grown in situ, the surface of the n-epitaxial layer 101 can also be planarized.

[0054] See also Figure 6a and 6b , a photoresist is spin-coated on the second oxide layer 106, and the photoresist is patterned through a photolithography mask to form a second mask 12. From a three-dimensional perspective, see Figure 6b The second mask 12 is divided into two parts. The first part located in the first area 301 is patterned so as to be used as an etching protection mask for forming the first trench 1001 and the second trench 1002. The second part of the second mask 12 located in the second area 302 is completely retained in the photolithography process to protect the second oxide layer 106 in the gate area. The second mask 12 is used as an etching protection layer, and the second oxide layer 106, the gate polysilicon layer 105 and the gate oxide layer 104 in the first area 301 are etched in sequence by an etching process, so as to form a plurality of trenches, such as Figure 6a and 6b As shown. The first trench 1001 formed directly above the p-column 103 has a width of 0.8 microns. The width of the stacked structure formed by the patterned gate oxide layer 104, the gate polysilicon layer 105 and the second oxide layer 106 is 0.3 microns. In addition to the first trench 1001 directly above the p-column 103, the width of the second trench 1002 formed between the two stacked structures is 0.4 microns.

[0055] See also Figure 7a and 7b After forming the structure of the first trench 1001 and the second trench 1002, the second mask 12 is removed (the structure after removing the second mask 12 is as shown in FIG. Figure 6b As shown in FIG. 1 , a third oxide layer 107 is then formed by chemical vapor deposition. The third oxide layer 107 covers the first trench 1001 and the second trench 1002 and covers the stacked structure composed of the gate polysilicon layer 105 and the gate oxide layer 104.

[0056] See also Figure 8a and Figure 8b, the third oxide layer 107 is etched to form a third trench 1003, thereby completely exposing the upper surface of the p-column 103 and a portion of the surface of the n-epitaxial layer 101 in the first region 301. After the etching process of the third oxide layer 107, the third oxide layer 107 also partially covers the upper surface of the gate polysilicon layer 105 and the sidewall of the stacked structure composed of the gate polysilicon layer 105 and the gate oxide layer 104.

[0057] See also Fig. 9 , using the third oxide layer 107 after the etching process as a mask and performing an ion implantation process. In the ion implantation process, p-type ion implantation is first performed to form a p+ ion implantation region 108 in the p-column 103 and the n-epitaxial layer 101 exposed by the third trench 1003, and then n-type ion implantation is performed to further form an n+ ion implantation region 109 in the p+ ion implantation region 108. The p+ ion implantation region 108 and the p-column will serve as the body electrode (i.e., the body electrode) of the device; the n+ ion implantation region 109 will serve as the source of the device.

[0058] See also Fig.10 After the ion implantation process is performed, the ion diffusion process is immediately performed. The ion diffusion process uses a high-temperature thermal annealing process. The high-temperature annealing process can further diffuse the implanted doping ions to form a p+ ion diffusion region 1081 and an n+ ion diffusion region 1091. The p+ ion diffusion region 1081 diffuses to the edge of the gate oxide layer 104 in the lateral direction of the device, so that the projection of the gate oxide layer 104 in the vertical direction is slightly longer (~0.1um) than the p+ ion diffusion region 1081. In addition, high-temperature thermal annealing can also repair lattice damage caused by the ion implantation process, such as Fig.10 shown.

[0059] See also Fig.11a , 11b After the ion diffusion process, the third oxide layer 107 is used as a self-aligned etching hard mask, and the p-column 103 and the n-epitaxial layer 101 exposed by the third trench 1003 in the first region 301 are etched by a dry etching process to form a fourth trench 1004. The fourth trench 1004 is formed by completely etching the n+ ion diffusion region 1091 and partially etching the p+ ion diffusion region 1081 in the vertical direction of the third trench 1003 by the etching process; the body electrode 1082 and the source region 1092 are formed after this etching process. Fig.11c and Fig.11d ,exist Fig.11b After the etching process shown in Fig.11bThe entire device surface shown in FIG. 1 is spin-coated with photoresist, and then the photoresist is patterned to form an opening 1301 in the photoresist. The opening 1301 exposes the upper surface of the third oxide layer 107. The patterned photoresist is used as a third mask 13. Then, the etching process is performed again with the third mask 13 as protection, so that the third oxide layer 107 is etched away to expose the upper surface of the polysilicon gate layer 105. After etching the third oxide layer 107, the third mask 13 is removed. After removing the third mask 13, the structure of the upper surface of the polysilicon gate layer 105 is exposed as shown in FIG. Fig.11d shown.

[0060] See also Fig.12a and 12b ,exist Fig.11a After the etching process of -c, a sputtering process is used to form a metal layer 110. The metal layer 110 completely fills the third trench 1003 and the fourth trench 1004, and completely covers the upper surface of the third oxide layer 107. The metal layer can be formed by different metal materials. In the present invention, metal aluminum is used to form the metal layer 110.

[0061] See also Fig.13 , spin-coat photoresist on the metal layer 110 , and after patterning, retain the photoresist at the position where the source and the gate need to be formed as the fourth mask 14 .

[0062] See also Fig.14 The fourth mask 14 is used as an etching mask, and the metal layer 110 is etched by an etching process, so that the gate metal and the source metal are separated. After the etching process is completed, the fourth mask 14 is removed, and the gate electrode 1 and the source electrode 2 are formed on the surface of the device.

[0063] See also Fig.15 A metal layer is formed on the back side of the n+ substrate 100, and the metal layer serves as the drain electrode 3 of the MOSFET.

[0064] So far, the manufacturing method of the super junction planar gate power MOSFET proposed in the present invention has been fully introduced. The present invention completes the manufacturing of MOSFET with only 4 layers of photomasks, and obtains MOSFET devices with low on-resistance and low gate charge, which can meet the application of DC converters such as DC-DC.

[0065] The above description is only the best specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by any technician familiar with the technical field within the technical scope disclosed by the present invention should be covered within the protection scope of the present invention.

Claims

1. A method for manufacturing a super junction planar gate power MOSFET, characterized in that: The steps include: Growing an epitaxial layer on a substrate; forming a first mask after growing a first oxide layer on the epitaxial layer; etching to form a plurality of deep trenches in the epitaxial layer; The first mask and the first oxide layer are removed, and an epitaxial layer is selectively grown in situ in the deep trench to form a p-column; a stacked structure including a gate oxide layer, a polysilicon gate layer and a second oxide layer is formed on the surface of the epitaxial layer and the p-column in sequence; forming a second mask on the surface of the second oxide layer, wherein the epitaxial layer is divided into a first region and a second region; the second mask on the first region has a first groove and a second groove; etching the stacked structure in the first region by an etching process to expose the upper surface of the p column and the upper surface of the epitaxial layer; removing the second mask and forming a third oxide layer by a deposition process; etching the third oxide layer on the first region to form a third trench; Performing an ion implantation process to form a p+ ion implantation region and an n+ ion implantation region in the p column and the epitaxial layer; performing an ion diffusion process to form a p+ ion diffusion region and an n+ ion diffusion region; Etching the p+ ion diffusion region and the n+ ion diffusion region to form a fourth trench; Spin-coating a photoresist on the entire surface of the third oxide layer and patterning the photoresist in the second region to form an opening, and using the photoresist after the opening as a third mask; etching the third oxide layer to expose the upper surface of the polysilicon gate layer with the third mask as protection; Sputtering to form a metal layer; Patterning a fourth mask on the metal layer; The metal layer is etched to form a source electrode and a gate electrode; and a metal layer is formed on the back side of the n+ substrate as a drain electrode.

2. The method for manufacturing a super junction planar gate power MOSFET according to claim 1, characterized in that: The deep trenches have a width of 0.4 micrometers and a depth of 1.2 micrometers, and a spacing between each deep trench is 1.4 micrometers.

3. The method for manufacturing a super junction planar gate power MOSFET according to claim 1, wherein: In the formation of the second mask, the first trench is located directly above the p-column and has a width of 0.8 microns; the width of the stacked structure composed of the patterned gate oxide layer, the gate polysilicon layer and the second oxide layer is 0.3 microns; the width of the second trench formed between the two stacked structures is 0.4 microns.

4. The method for manufacturing a super junction planar gate power MOSFET according to claim 1, wherein: In the step of forming the third trench, the third trench exposes the upper surface of the p-column and the upper surface of the epitaxial layer, and forms an oxide layer sidewall on the side of the stacked structure composed of the gate oxide layer and the polysilicon gate layer.

5. The method for manufacturing a super junction planar gate power MOSFET according to claim 1, wherein: The ion diffusion process is a thermal annealing process; the p+ ion diffusion region is aligned to the edge of the gate oxide layer in the lateral direction, so that the projection of the gate oxide layer in the vertical direction is located in the p+ ion diffusion region.

6. The method for manufacturing a super junction planar gate power MOSFET according to claim 1, wherein: In the step of forming the fourth trench, the fourth trench is formed after completely etching the n+ ion diffusion region and partially etching the p+ ion diffusion region in a vertical direction.

7. The method for manufacturing a super junction planar gate power MOSFET according to claim 6, characterized in that: in, The entire surface of the third oxide layer is spin-coated with photoresist and patterned in the photoresist in the second region to form an opening, wherein the opening exposes the upper surface of the third oxide layer.

8. The method for manufacturing a super junction planar gate power MOSFET according to claim 7, characterized in that: in, In the step of etching the third oxide layer to expose the upper surface of the polysilicon gate layer, the metal layer completely covers the third oxide layer and completely fills the fourth trench.

9. The method for manufacturing a super junction planar gate power MOSFET according to claim 7, characterized in that: In the step of forming the fourth mask, the fourth mask remains only at positions where the source electrode and the gate electrode are to be formed.