Micro light emitting diode backplane and preparation method thereof
By forming a double-layer protective structure of nanoparticles and polyelectrolyte layers on the side walls of micro-LEDs, the problem of easy peeling of the side wall protective layer is solved, the bonding force is enhanced, the risk of leakage is reduced, and a more stable side wall is achieved Protect.
Patent Information
- Application Number
- CN202210028457.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-01-11
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2042-01-11
AI Technical Summary
In the existing technology, the sidewall protective layer of the micro light-emitting diode is easy to peel off, and the bonding force between the organic film and the GaN sidewall is not good, making it difficult to solve the edge leakage current problem.
A nanoparticle layer and a polyelectrolyte layer are provided on the side wall of the micro light-emitting diode. The nanoparticle layer is composed of gallium or gallium oxide, with a particle diameter of 50 to 300 nanometers. The polyelectrolyte layer is composed of polydiallyldimethylammonium chloride. , polypropylene It is composed of sodium phosphate, polydimethyl diallyl ammonium chloride and acrylic acid-vinyl pyridine copolymer, and uses electrostatic layer-by-layer assembly technology to form a double-layer sidewall protective layer to ensure the electrical properties of the nanoparticle layer and the polyelectrolyte layer. On the contrary, it enhances the adhesion force.
It effectively prevents the peeling and cracking of the side wall protective layer of micro-LEDs, reduces the risk of leakage, and improves the stability and protection effect of the side wall.
Smart Images

Figure CN114420716B_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the field of display technology, and in particular, relates to a micro light emitting diode backplane and a preparation method thereof. Background Art
[0002] In recent years, Mini-LED / Micro-LED display technology has become a hot spot for major panel manufacturers due to its outstanding advantages and rapid development. Compared with current LCD and OLED display devices, both have the advantages of fast response, high color gamut, high PPI, low energy consumption, ultra-high number of partitions for precise dimming, and ultra-high contrast.
[0003] In the prior art, in order to reduce the sidewall leakage current of micro light-emitting diode devices (Mirco-LEDs), the sidewalls of Mirco-LEDs are usually protected. Common sidewall protection methods include depositing inorganic insulating layers such as SiO2, SiN, MgO and Gd2O3, which have a high interface trap density with GaN and cannot effectively solve the edge leakage current problem. The sidewall protection solution of a simple organic film has a poor bonding strength with the GaN sidewall, and is easy to peel off and produce cracks.
[0004] Therefore, the prior art has defects and is in urgent need of improvement. Summary of the invention
[0005] The embodiment of the present application provides a micro-light emitting diode back plate and a preparation method thereof, so that the side wall protection layer of the micro-light emitting diode is not easy to peel off.
[0006] In a first aspect, an embodiment of the present application provides a micro light emitting diode backplane, comprising:
[0007] Back panel;
[0008] Micro light emitting diodes, the micro light emitting diodes are arranged in an array on the back panel;
[0009] A first contact electrode, the first contact electrode is disposed on a first surface of the micro light emitting diode away from the back plate;
[0010] a second contact electrode, the second contact electrode being disposed on a second surface of the micro-LED opposite to the first surface;
[0011] a bonding metal layer, the bonding metal layer being disposed between the second contact electrode and the back plate;
[0012] Wherein, a nanoparticle layer is arranged on the side of the micro light emitting diode, and a polyelectrolyte layer is also arranged on the nanoparticle layer.
[0013] Optionally, the nanoparticle layer consists of gallium nanoparticles or gallium oxide nanoparticles.
[0014] Optionally, the particle diameters of the gallium nanoparticles and the gallium oxide nanoparticles are 50 to 300 nanometers.
[0015] Optionally, the nanoparticle layer and the polyelectrolyte layer have opposite electrical properties.
[0016] Optionally, the polyelectrolyte layer is composed of at least one of polydiallyldimethylammonium chloride, sodium polyacrylate, polydimethyldiallylammonium chloride and acrylic acid-vinylpyridine copolymer.
[0017] In a second aspect, an embodiment of the present application provides a method for preparing a micro light emitting diode backplane, comprising:
[0018] A nanoparticle solution is coated on a preformed first intermediate product, and the nanoparticle solution is air-dried to obtain a nanoparticle layer, wherein the first intermediate product comprises a transient substrate, a magnetron layer, and a metal electrode material layer stacked in sequence from bottom to top, an array of micro-light emitting diodes is arranged on the metal electrode material layer, and a photoresist protective layer is arranged on each of the micro-light emitting diodes;
[0019] Etching the nanoparticle layer between adjacent micro-light emitting diodes to obtain a nanoparticle layer located on the side of the micro-light emitting diodes;
[0020] Etching the metal electrode material layer between adjacent micro-light emitting diodes to obtain a second contact electrode between the micro-light emitting diodes and the magnetron layer;
[0021] coating a polyelectrolyte solution on the nanoparticle layer, and air-drying the polyelectrolyte solution to obtain a polyelectrolyte layer;
[0022] Stripping the photoresist protective layer, and transferring the micro light emitting diode and the second contact electrode to a back plate with a bonding metal layer;
[0023] A first contact electrode is deposited on the micro light emitting diode to obtain a micro light emitting diode backplane.
[0024] Optionally, before the step of coating the nanoparticle solution on the preformed first intermediate product, the step further includes:
[0025] forming an epitaxial material layer and a metal electrode material layer on a substrate from bottom to top;
[0026] Inverting the substrate, and controlling the metal electrode material layer to be bonded and connected to the transient substrate through the magnetron layer;
[0027] The substrate is peeled off to form a photoresist protection layer arranged in an array on the epitaxial material layer;
[0028] The epitaxial material layer is etched to remove the epitaxial material layer not protected by the photoresist protection layer, thereby forming micro light emitting diodes arranged in an array and obtaining the first intermediate product.
[0029] Optionally, the epitaxial material layer is composed of gallium nitride.
[0030] Optionally, before the step of controlling the metal electrode material layer to be bonded and connected to the transient substrate by the magnetron layer, the method further includes:
[0031] The polyurethane compound is used as a continuous phase, and ferroferric oxide particles are heated to a molten state of 100° C. and added to the polyurethane compound, and the mass of the added ferroferric oxide particles is controlled to account for 1% to 20% of the total mass to form a magnetron layer.
[0032] Optionally, the nanoparticle layer and the polyelectrolyte layer have opposite electrical properties.
[0033] The micro-LED backplane provided in the embodiment of the present application includes: a backplane; micro-LEDs, which are arranged in an array on the backplane; a first contact electrode, which is arranged on a first surface of the micro-LED away from the backplane; a second contact electrode, which is arranged on a second surface of the micro-LED opposite to the first surface; a bonding metal layer, which is arranged between the second contact electrode and the backplane; wherein a nanoparticle layer is arranged on the side of the micro-LED, and a polyelectrolyte layer is also arranged on the nanoparticle layer. The present application forms a double-layer sidewall protection layer on the sidewall of the micro-LED by arranging a nanoparticle layer and a polyelectrolyte layer on the sidewall of the micro-LED, and defines that the electrical properties of the nanoparticle layer and the polyelectrolyte layer are opposite, so as to increase the adhesion between the polyelectrolyte layer and the nanoparticle layer, so that the sidewall protection layer of the micro-LED is not easy to peel off. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 It is a schematic diagram of the preparation process of the micro light emitting diode backplane provided in the embodiment of the present application.
[0035] Figure 2 This is a schematic diagram of the structure of the first intermediate product provided in an embodiment of the present application.
[0036] Figure 3 This is a schematic diagram of the first intermediate state when preparing the first intermediate product provided in an embodiment of the present application.
[0037] Figure 4 A schematic diagram of the second intermediate state when preparing the first intermediate product provided in an embodiment of the present application.
[0038] Figure 5 This is a schematic diagram of the third intermediate state when preparing the first intermediate product provided in an embodiment of the present application.
[0039] Figure 6 A molecular schematic diagram of the polyurethane compound provided in the embodiments of the present application.
[0040] Figure 7 This is a schematic diagram of the structure of the second intermediate product provided in an embodiment of the present application.
[0041] Figure 8 This is a schematic diagram of the structure of the third intermediate product provided in an embodiment of the present application.
[0042] Fig. 9 This is a schematic diagram of the structure of the fourth intermediate product provided in an embodiment of the present application.
[0043] Fig.10 This is a schematic diagram of the structure of the fifth intermediate product provided in an embodiment of the present application.
[0044] Fig.11 This is a schematic diagram of the structure of the sixth intermediate product provided in an embodiment of the present application.
[0045] Fig.12 A schematic diagram of the structure of a micro light emitting diode backplane provided in an embodiment of the present application. DETAILED DESCRIPTION
[0046] The technical solutions in the embodiments of the present application will be described clearly and completely below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present application.
[0047] In the prior art, in order to reduce the sidewall leakage current of micro light-emitting diode devices (Mirco-LEDs), the sidewalls of Mirco-LEDs are usually protected. Common sidewall protection methods include depositing inorganic insulating layers such as SiO2, SiN, MgO and Gd2O3, which have a high interface trap density with GaN and cannot effectively solve the edge leakage current problem. The sidewall protection solution of a simple organic film has a poor bonding strength with the GaN sidewall, and is easy to peel off and produce cracks.
[0048] In order to prevent the sidewall protective layer of the micro-LED from peeling off and cracking, the present invention provides a method for preparing a micro-LED backplane. Figure 1 , Figure 1 : is a schematic diagram of the preparation process of the micro-light emitting diode backplane provided in the embodiment of the present application. The preparation method of the micro-light emitting diode backplane includes:
[0049] Step 101: coating a nanoparticle solution on a preformed first intermediate product, and air-drying the nanoparticle solution to obtain a nanoparticle layer.
[0050] Among them, see Figure 2 , Figure 2 A schematic diagram of the structure of the first intermediate product provided in an embodiment of the present application. The first intermediate product 100 includes a transient substrate 11, a magnetron layer 12, and a metal electrode material layer 13 stacked in sequence from bottom to top, an array of micro-light emitting diodes 14 are arranged on the metal electrode material layer 13, and a photoresist protective layer 15 is arranged on each of the micro-light emitting diodes 14.
[0051] In some embodiments, before the step of coating the nanoparticle solution on the preformed first intermediate product, the method further comprises:
[0052] (1) forming an epitaxial material layer and a metal electrode material layer in sequence from bottom to top on a substrate;
[0053] (2) inverting the substrate, and controlling the metal electrode material layer to be bonded and connected to the temporary substrate through the magnetron layer;
[0054] (3) peeling off the substrate, and forming an array-arranged photoresist protection layer on the epitaxial material layer;
[0055] (4) Etching the epitaxial material layer to remove the epitaxial material layer not protected by the photoresist protection layer, forming an array of micro light emitting diodes, and obtaining a first intermediate product.
[0056] Among them, see Figures 3 to 5 , Figure 3 A schematic diagram of a first intermediate state when preparing a first intermediate product provided in an embodiment of the present application; Figure 4 A schematic diagram of a second intermediate state when preparing a first intermediate product provided in an embodiment of the present application; Figure 5 This is a schematic diagram of the third intermediate state when preparing the first intermediate product provided in an embodiment of the present application.
[0057] Specifically, the epitaxial material layer 141 and the metal material layer 131 are sequentially deposited on the substrate 21, and then the entire substrate is inverted so that the substrate 21 is at the top, and the epitaxial material layer 141 and the metal material layer 131 are sequentially arranged downward. The metal material layer 131 is controlled to be bonded and connected to the temporary substrate 11 through the magnetron layer 12. Then the topmost substrate 21 is peeled off to expose the epitaxial material layer 141. A photoresist protective layer 15 is arrayed on the exposed epitaxial material layer 141 to obtain Figure 5 The third intermediate state when preparing the first intermediate product is shown. Finally, the epitaxial material layer 141 is etched to remove the epitaxial material layer 141 not protected by the photoresist protection layer 15, forming an array of micro-light-emitting diodes 14, and obtaining the following Figure 2 A first intermediate product 100 is shown.
[0058] In some embodiments, the epitaxial material layer 141 is composed of gallium nitride.
[0059] In some embodiments, before the step of controlling the metal electrode material layer to be bonded and connected to the transient substrate by the magnetron layer, the method further includes:
[0060] The polyurethane compound is used as a continuous phase, and ferroferric oxide particles are heated to a molten state of 100° C. and added to the polyurethane compound, and the mass of the added ferroferric oxide particles is controlled to account for 1% to 20% of the total mass to form a magnetron layer.
[0061] The above-mentioned magnetically controlled organic-inorganic composite material is prepared by using a polyurethane compound as a continuous phase and adding 1% to 20% of unmodified commercial ferroferric oxide particles to the mixture in a molten state at 100°C. Figure 6 , Figure 6 A molecular schematic diagram of a polyurethane compound provided in an embodiment of the present application. The polyurethane compound is synthesized from three components: terminal hydroxylated polyolefin diol, diphenylmethane diisocyanate, and 4-(2-aminoethyl)morpholine. Due to the presence of multiple hydrogen bonds in polyurethane X, the organic-inorganic composite material itself has good adhesion. When the organic-inorganic composite material is placed in an oscillating magnetic field, the ferroferric oxide particles therein will couple with the magnetic field to generate a hysteresis thermal effect, causing the temperature of the organic-inorganic composite material to rise, further weakening the hydrogen bonds between the polyurethane molecules, thereby achieving debonding of the organic-inorganic composite material from the adhered surface.
[0062] Among them, see Figure 7 , Figure 7A schematic diagram of the structure of the second intermediate product provided in an embodiment of the present application. A nanoparticle solution is coated on the first intermediate product and air-dried to obtain a nanoparticle layer 16. The process of coating the nanoparticle solution may be coating the entire surface of the first intermediate product 100 or coating point-to-point without the photoresist protective layer 15, etc., which is not limited here.
[0063] Specifically, the nanoparticle solution is composed of gallium (Ga) nanoparticles or gallium oxide (Ga2O3) nanoparticles, and the transparent metal Ga / Ga2O3 nanoparticle solution is prepared by laser-induced oxidation: Ga / Ga2O3 nanoparticles with diameters ranging from 50 to 300 nm are manufactured by using femtosecond laser to ablate a Ga film immersed in a certain solution. A femtosecond laser amplifier (Legend, Coherent) with a pulse duration of 100 fs and a repetition rate of 1 kHz is used in the ablation process. The femtosecond laser beam is focused on the Ga film with a spot diameter of about 40 mm using an objective lens with a focal length of 25 cm. The Ga NPs ejected from the Ga film after femtosecond laser irradiation are uniformly dispersed in the solvent.
[0064] Among them, Ga / Ga2O3 nanoparticles carry positive or negative charges, and the positive or negative charge can be adjusted by pH.
[0065] Step 102 : etching the nanoparticle layer between adjacent micro-light emitting diodes to obtain the nanoparticle layer located on the side of the micro-light emitting diodes.
[0066] Among them, see Figure 8 , Figure 8 The schematic diagram of the structure of the third intermediate product provided in the embodiment of the present application is that the nanoparticle layer 16 located between adjacent micro-LEDs 14 is etched away by dry etching or wet etching to retain the nanoparticle layer 16 located on the side of the micro-LEDs 14 .
[0067] Step 103: etching the metal electrode material layer between adjacent micro-LEDs to obtain a second contact electrode between the micro-LEDs and the magnetron layer.
[0068] Among them, see Fig. 9 , Fig. 9 The schematic diagram of the structure of the fourth intermediate product provided in the embodiment of the present application is as follows: The metal material layer 131 between adjacent micro-LEDs 14 is etched away by dry etching or wet etching to retain the second contact electrode 13 (lower contact electrode) between the micro-LED 14 and the magnetron layer 12.
[0069] Step 104 : coating a polyelectrolyte solution on the nanoparticle layer, and air-drying the polyelectrolyte solution to obtain a polyelectrolyte layer.
[0070] Among them, see Fig.10 , Fig.10 A schematic diagram of the structure of the fifth intermediate product provided in the embodiment of the present application is shown in FIG. 1 . A polyelectrolyte solution is coated on the nanoparticle layer 16 , and the polyelectrolyte solution is air-dried to obtain a polyelectrolyte layer 17 .
[0071] Specifically, the polyelectrolyte layer is composed of at least one of polydiallyldimethylammonium chloride, sodium polyacrylate, polydimethyldiallylammonium chloride and acrylic acid-vinylpyridine copolymer.
[0072] The electrical properties of the nanoparticle layer and the polyelectrolyte layer are opposite to each other, so as to increase the adhesion between the polyelectrolyte layer and the nanoparticle layer, thereby forming a strong protective layer material.
[0073] Step 105 , peeling off the photoresist protective layer, and transferring and aligning the micro light emitting diode and the second contact electrode to the back plate with the bonding metal layer.
[0074] Among them, see Fig.11 , Fig.11 A schematic diagram of the structure of the sixth intermediate product provided in an embodiment of the present application. After the photoresist protective layer 15 is peeled off, the micro-LEDs are transferred in batches to the backplane 32 having the bonding metal layer 31 .
[0075] Specifically, the bonding metal layers 31 on the back plate 32 are arranged in an array, and the spacing between adjacent bonding metal layers 31 is the same as the spacing between adjacent micro-LEDs 14 , so as to ensure that one micro-LED 14 corresponds to one bonding metal layer 31 .
[0076] Step 106: deposit a first contact electrode on the micro-LED to obtain a micro-LED backplane.
[0077] Among them, see Fig.12 , Fig.12 A schematic diagram of the structure of a micro-LED backplane provided in an embodiment of the present application: A first contact electrode 33 is deposited on the micro-LED 14 to form an upper contact electrode of the micro-LED 14 .
[0078] Among them, the coating method of the nanoparticle solution and the coating method of the polyelectrolyte solution can both adopt layer-by-layer assembly technology (Layer-by-Layer, LBL). The layer-by-layer assembly technology is a process that utilizes a layer-by-layer alternating deposition method to spontaneously associate layers with each other to form a complete structure, stable performance, and a molecular aggregate or supramolecular structure with a certain specific function by means of weak interactions between molecules in each layer (such as electrostatic attraction, hydrogen bonds, coordination bonds, etc.). In this embodiment, the electrostatic layer-by-layer assembly technology is mainly used, that is, the electrostatic interaction between ions is used as the driving force for film formation.
[0079] The preparation method of the micro-LED backplane provided in the embodiment of the present application includes: providing a first intermediate product, coating a nanoparticle solution on the first intermediate product, and air-drying the nanoparticle solution to obtain a nanoparticle layer, wherein the first intermediate product includes a transient substrate, a magnetron layer, and a metal electrode material layer stacked in sequence from bottom to top, and arrayed micro-LEDs are arranged on the metal electrode material layer, and a photoresist protective layer is arranged on the micro-LED; etching the nanoparticle layer located between adjacent micro-LEDs to obtain a nanoparticle layer located on the side of the micro-LED; etching the metal electrode material layer located between adjacent micro-LEDs to obtain a second contact electrode located between the micro-LED and the magnetron layer; coating a polyelectrolyte solution on the nanoparticle layer, and air-drying the polyelectrolyte solution to obtain a polyelectrolyte layer; peeling off the photoresist protective layer, and transferring the micro-LED and the second contact electrode to a backplane with a bonding metal layer; depositing a first contact electrode on the micro-LED to obtain a micro-LED backplane. In this way, by preparing a nanoparticle layer and a polyelectrolyte layer on the side of the micro-light-emitting diode, a double-layer sidewall protection layer is formed on the side wall of the micro-light-emitting diode, and the electrical properties of the nanoparticle layer and the polyelectrolyte layer are limited to be opposite, so as to increase the adhesion between the polyelectrolyte layer and the nanoparticle layer, so that the sidewall protection layer of the micro-light-emitting diode is not easy to peel off and crack, thereby reducing the risk of leakage.
[0080] Based on this, an embodiment of the present application further provides a micro light emitting diode backplane, comprising:
[0081] Back plate 32;
[0082] Micro light emitting diodes 14, wherein the micro light emitting diodes 14 are arranged in an array on the back plate 32;
[0083] A first contact electrode 33, wherein the first contact electrode 33 is disposed on a first surface of the micro light emitting diode 14 away from the back plate 32;
[0084] A second contact electrode 13, wherein the second contact electrode 13 is disposed on a second surface of the micro-LED 14 opposite to the first surface;
[0085] A bonding metal layer 31, wherein the bonding metal layer 31 is disposed between the second contact electrode 13 and the back plate 32;
[0086] A nanoparticle layer 16 is disposed on the side of the micro-LED 14 , and a polyelectrolyte layer 17 is further disposed on the nanoparticle layer 16 .
[0087] In some embodiments, the nanoparticle layer consists of gallium nanoparticles or gallium oxide nanoparticles.
[0088] The nanoparticle solution is composed of gallium (Ga) nanoparticles or gallium oxide (Ga2O3) nanoparticles, and the transparent metal Ga / Ga2O3 nanoparticle solution is prepared by laser induced oxidation method.
[0089] In some embodiments, the particle diameter of the gallium nanoparticles and the gallium oxide nanoparticles is 50 to 300 nanometers.
[0090] Specifically, Ga / Ga2O3 nanoparticles with diameters ranging from 50 to 300 nm were fabricated by ablating Ga thin films immersed in a certain solution using femtosecond lasers. A femtosecond laser amplifier (Legend, Coherent) with a pulse duration of 100 fs and a repetition rate of 1 kHz was used in the ablation process. The femtosecond laser beam was focused on the Ga film with a spot diameter of about 40 mm using an objective lens with a focal length of 25 cm. The Ga NPs ejected from the Ga film after femtosecond laser irradiation were uniformly dispersed in the solvent.
[0091] In some embodiments, the nanoparticle layer and the polyelectrolyte layer have opposite electrical properties to increase the adhesion between the polyelectrolyte layer and the nanoparticle layer.
[0092] The electrical properties of the nanoparticle layer and the polyelectrolyte layer are opposite to each other, so as to increase the adhesion between the polyelectrolyte layer and the nanoparticle layer, thereby forming a strong protective layer material.
[0093] In some embodiments, the polyelectrolyte layer is composed of at least one of polydiallyldimethylammonium chloride, sodium polyacrylate, polydimethyldiallylammonium chloride, and acrylic acid-vinylpyridine copolymer.
[0094] The micro-LED backplane provided in the embodiment of the present application includes: a backplane; micro-LEDs, which are arranged in an array on the backplane; a first contact electrode, which is arranged on a first surface of the micro-LED away from the backplane; a second contact electrode, which is arranged on a second surface of the micro-LED opposite to the first surface; a bonding metal layer, which is arranged between the second contact electrode and the backplane; wherein a nanoparticle layer is arranged on the side of the micro-LED, and a polyelectrolyte layer is also arranged on the nanoparticle layer. The present application forms a double-layer sidewall protection layer on the sidewall of the micro-LED by arranging a nanoparticle layer and a polyelectrolyte layer on the sidewall of the micro-LED, and defines that the electrical properties of the nanoparticle layer and the polyelectrolyte layer are opposite to each other, so as to increase the adhesion between the polyelectrolyte layer and the nanoparticle layer, so that the sidewall protection layer of the micro-LED is not easy to peel off and cracks are not easy to form, thereby reducing the risk of leakage.
[0095] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.
[0096] The above is a detailed introduction to the micro-light emitting diode backplane and the preparation method thereof provided in the embodiments of the present application. Specific examples are used herein to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method of the present application and its core idea. At the same time, for technicians in this field, according to the ideas of the present application, there will be changes in the specific implementation methods and application scopes. In summary, the content of this specification should not be understood as a limitation on the present application.
Claims
1. A micro light emitting diode backplane, characterized in that: include: Back panel; Micro light emitting diodes, the micro light emitting diodes are arranged in an array on the back panel; A first contact electrode, the first contact electrode is disposed on a first surface of the micro light emitting diode away from the back plate; a second contact electrode, the second contact electrode being disposed on a second surface of the micro-LED opposite to the first surface; a bonding metal layer, the bonding metal layer being disposed between the second contact electrode and the back plate; A nanoparticle layer is arranged on the side of the micro light emitting diode, and a polyelectrolyte layer is also arranged on the nanoparticle layer. The electrical properties of the nanoparticle layer and the polyelectrolyte layer are opposite.
2. The micro light emitting diode backplane according to claim 1, characterized in that: The nanoparticle layer consists of gallium nanoparticles or gallium oxide nanoparticles.
3. The micro light emitting diode backplane according to claim 2, characterized in that: The particle diameters of the gallium nanoparticles and the gallium oxide nanoparticles are 50 to 300 nanometers.
4. The micro light emitting diode backplane according to claim 1, characterized in that: The polyelectrolyte layer is composed of at least one of polydiallyldimethylammonium chloride, sodium polyacrylate, polydimethyldiallylammonium chloride and acrylic acid-vinylpyridine copolymer.
5. A method for preparing a micro light emitting diode backplane, characterized in that: include: A nanoparticle solution is coated on a preformed first intermediate product, and the nanoparticle solution is air-dried to obtain a nanoparticle layer, wherein the first intermediate product comprises a transient substrate, a magnetron layer, and a metal electrode material layer stacked in sequence from bottom to top, an array of micro-light emitting diodes is arranged on the metal electrode material layer, and a photoresist protective layer is arranged on each of the micro-light emitting diodes; Etching the nanoparticle layer between adjacent micro-light emitting diodes to obtain a nanoparticle layer located on the side of the micro-light emitting diodes; Etching the metal electrode material layer between adjacent micro-light emitting diodes to obtain a second contact electrode between the micro-light emitting diodes and the magnetron layer; Coating a polyelectrolyte solution on the nanoparticle layer and air-drying the polyelectrolyte solution to obtain a polyelectrolyte layer, wherein the nanoparticle layer has opposite electrical properties to the polyelectrolyte layer; Stripping the photoresist protective layer, and transferring the micro light emitting diode and the second contact electrode to a backplane with a bonding metal layer; A first contact electrode is deposited on the micro light emitting diode to obtain a micro light emitting diode backplane.
6. The method for preparing a micro light emitting diode backplane according to claim 5, characterized in that: Before the step of coating the nanoparticle solution on the preformed first intermediate product, the method further comprises: forming an epitaxial material layer and a metal electrode material layer in sequence from bottom to top on a substrate; Inverting the substrate, and controlling the metal electrode material layer to be bonded and connected to the transient substrate through the magnetron layer; The substrate is peeled off to form a photoresist protection layer arranged in an array on the epitaxial material layer; The epitaxial material layer is etched to remove the epitaxial material layer not protected by the photoresist protection layer, thereby forming micro light emitting diodes arranged in an array and obtaining the first intermediate product.
7. The method for preparing a micro light emitting diode backplane according to claim 6, characterized in that: The epitaxial material layer is composed of gallium nitride.
8. The method for preparing a micro light emitting diode backplane according to claim 6, characterized in that: Before the step of controlling the metal electrode material layer to be bonded and connected to the transient substrate by the magnetron layer, the method further includes: A polyurethane compound is used as a continuous phase, ferroferric oxide particles are heated to a molten state of 100° C. and added to the polyurethane compound, and the mass of the added ferroferric oxide particles is controlled to account for 1% to 20% of the total mass to form a magnetron layer.
Citation Information
Patent Citations
Pixel structure and manufacturing method
CN106784203A
Micro light-emitting diode backboard and manufacturing method thereof
CN111725363A
Light emitting diode device and preparation method thereof
CN112382711A
Light emitting diode and light emitting module
CN113903840A
Semiconductor element and manufacturing method of the same
JP2013197336A