A high saturation magnetic induction intensity iron-based alloy strip and preparation method thereof

By processing iron-based alloys in vacuum induction furnaces and resistance molten salt furnaces, combined with rapid cooling and low-temperature cryogenic cooling, the problem of low performance of existing iron-based amorphous nanocrystalline soft magnetic alloy thin strips is solved, and high saturation magnetic induction is achieved Strength and simple low-cost preparation process, suitable for industrial production.

CN114496441BActive Publication Date: 2024-10-29SHANXI RAY WHEAT ELECTRONICS TECH
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202210043287.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-14
Publication Date
2024-10-29
Estimated Expiration
2042-01-14

AI Technical Summary

Technical Problem

The existing iron-based amorphous nanocrystalline soft magnetic alloy thin strips have low overall performance, complex preparation processes and high costs, making them difficult to be suitable for industrial production.

Method used

The preparation method of iron-based alloy strips with high saturation magnetic induction intensity includes smelting and remelting in a vacuum induction furnace to form alloy strips, and performing pulse power supply treatment in a resistance molten salt furnace, combining rapid cooling, low-temperature cryogenics and Aging treatment controls the grain refinement and uniform distribution of chemical components of the alloy and reduces internal stress.

Benefits of technology

It improves the magnetic properties and thermal stability of the alloy, simplifies the preparation process, reduces production costs, is suitable for industrial production, and significantly improves the soft magnetic properties of the material.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114496441B_ABST
    Figure CN114496441B_ABST
Patent Text Reader

Abstract

The present invention relates to a high saturation magnetic flux density iron-based alloy strip and a preparation method thereof, wherein the mass composition is: Nb 0.5-0.9%, Cr 0.8-1.4%, In 0.02-0.06%, Al 0.5-0.9%, Pb 0.04-0.07%, Be 0.09-0.12%, Nd 0.1-0.6%, Au 0.03-0.04%, Si 0.3-0.8%, B 3-5%, Fe remainder. The high saturation magnetic flux density iron-based alloy strip prepared by the present invention has the advantages of good thermal stability and good magnetic properties. The preparation method of the present invention has a simple process, low production cost, and is suitable for industrial production. The material prepared by the present invention can be applied to magnetic devices in the fields of information and communication.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of functional materials, and in particular to an iron-based alloy strip with high saturation magnetic induction intensity and a preparation method thereof. Background Art

[0002] Chinese patent application number CN201510674626.5 discloses an iron-based amorphous nanocrystalline soft magnetic alloy ribbon, whose composition is as shown in FeaSibBcPdCueMef, wherein a, b, c, d, e and f respectively represent the contents of Fe, Si, B, P, Cu and Me in the alloy ribbon in terms of atomic mass fractions, 80≤a≤90, 0.5≤b≤5, 5≤c≤12, 1≤d≤9, 0.3≤e≤2, 0.3≤f≤3, a+b+c+d+e+f=100; however, the comprehensive performance of this material is not high. Summary of the invention

[0003] The object of the present invention is to provide a high saturation magnetic induction intensity iron-based alloy strip material in view of the above technical defects, which has the advantages of good thermal stability and good magnetic properties.

[0004] Another object of the present invention is to provide a method for preparing an iron-based alloy strip with high saturation magnetic induction intensity, which has a simple process, low production cost and is suitable for industrial production.

[0005] In order to achieve the above-mentioned invention object, the technical solution provided by the present invention is:

[0006] A high saturation magnetic induction intensity iron-based alloy strip, which comprises the following components in terms of weight percentage:

[0007] Nb 0.5-0.9%, Cr 0.8-1.4%, In 0.02-0.06%, Al 0.5-0.9%, Pb 0.04-0.07%, Be 0.09-0.12%, Nd 0.1-0.6%, Au 0.03-0.04%, Si 0.3-0.8%, B 3-5%, Fe balance. The method for preparing a high saturation magnetic induction intensity iron-based alloy strip comprises the following steps:

[0008] 1) First, the ingredients are prepared according to the above alloy composition, and the purity of Nb, Cr, In, Al, Pb, Be, Nd, Au, and Fe in the raw materials is greater than 99.9%;

[0009] 2) placing the raw materials in a vacuum induction furnace for smelting at a smelting temperature of 1510-1560° C. to obtain a master alloy, and then placing the raw materials in a remelting tubular crucible in a vacuum induction forming furnace for remelting at a remelting temperature of 1510-1530° C.; the bottom of the remelting tubular crucible is placed 2-4 mm above the rim of the rotating wheel of the forming furnace; when the master alloy is melted, opening the valve on the upper part of the remelting tubular crucible, the molten master alloy is sprayed from the through hole at the bottom of the crucible to the rotating rim of the forming furnace under nitrogen pressure to form a continuous alloy strip;

[0010] 3) Then, molten salt is prepared in a resistance molten salt furnace, wherein the molten salt components include AgCl, NaCl, NaF, BeF2, Mg2B2O5·H2O, NdCl3, powdered SiO2 and silicon carbide powder; the above molten salt components are all pure substances with a purity of 99.99%, wherein the particle size of the powdered substances used is 270-300 mesh;

[0011] 4) When the temperature of the resistance molten salt furnace reaches 680-740℃, keep the temperature constant for 20-25min, and start to immerse the alloy strip in the molten salt; turn on the DC power supply and use pulse power supply; the alloy strip moves at a uniform speed in the molten salt, and the residence time of each point of the alloy strip in the molten salt is kept for 25-30 minutes; after the alloy strip is taken out of the molten salt, the strip is rolled up by the strip take-up machine, and the material preparation is completed;

[0012] 5) The alloy strip is then placed in a liquid nitrogen atmosphere for low temperature treatment and kept warm; then placed at room temperature for static treatment; then placed under heating conditions and kept warm; then cooled to room temperature along with the furnace.

[0013] In step 2), a through hole is provided at the bottom of the remelting tubular crucible, and the upper part of the remelting tubular crucible is connected to a nitrogen system via a valve, and the pressure of the nitrogen system is 1.5 to 1.7 atmospheres.

[0014] In step 3), the inner diameter of the remelting crucible is 12-14 mm, the height is 250-280 mm, the diameter of the through hole at the bottom of the remelting crucible is 1.3-1.5 mm; the linear speed of the rotating wheel is 25-27 m / s; the thickness of the obtained alloy strip is 300-350 μm, and the width is 3-5 mm.

[0015] In step 4), when preparing molten salt in a resistance molten salt furnace, first dry each substance at 150-180°C for 6-8h, weigh each component according to the weight ratio of AgCl, NaCl, NaF, BeF2, Mg2B2O5·H2O, and NdCl3 of 0.1:1:3:(0.05-0.09):0.32:0.010, add a mixture of powdered SiO2 and powdered silicon carbide accounting for 5-9% of the mass fraction of the molten salt medium, grind and mix for use; the alloy strip is the anode, and the cathode of the resistance molten salt furnace is silicon steel containing 4.5% Si and having a thickness of 0.8-1.5mm.

[0016] Among them, the weight ratio of SiO2 to silicon carbide is 1:(0.1-0.3).

[0017] In step 5), the average current density is controlled to be 60-70 mA / cm2; the alloy strip moves at a constant speed in the molten salt, and the travel speed is 0.07-0.11 m / min.

[0018] In step 6), the alloy strip is placed in a liquid nitrogen atmosphere for low temperature treatment at a temperature of -130°C to -150°C for 15 to 18 minutes; then placed at room temperature for 1 to 2 hours; then placed at 180 to 220°C for 2 to 4 hours, and then cooled to room temperature with the furnace.

[0019] Compared with the prior art, the present invention has the following beneficial effects:

[0020] In the high saturation magnetic flux density iron-based alloy strip of the present invention, Si, Be and Nd can prevent the growth of grains during heat treatment, refine the grains, thereby improving the resistivity and reducing the loss. Al and the second transition series Nb can effectively inhibit the growth of grains, which is conducive to obtaining a finer and more uniform grain structure, and can also improve the thermal stability of the magnet. The first transition series Cr inhibits the growth of particles at the intersection of grains and refines the grains, thereby inhibiting the enhancement of the stray field around them, thereby improving the magnetic properties. In, Pb, Au and B work together to improve the amorphous forming ability.

[0021] The alloy of the present invention adopts a combination of rapid cooling, low-temperature deep cooling, aging treatment and alloying during solidification, which not only effectively reduces the phase size in the alloy, ensures the uniform distribution of chemical components in the material, and ensures the magnetic properties of the alloy, but also greatly reduces the internal stress caused by rapid cooling through gradient treatment, and also ensures the mechanical properties of the alloy.

[0022] The product obtained by the present invention has excellent soft magnetic properties. No heavy rare earth elements are used in the preparation, and the rare elements used are trace, and the cost of other raw materials is relatively low; in addition, the alloy is quickly cooled during the preparation process, which ensures the uniformity of the alloy composition, structure and performance, and ensures the quality of the alloy. The alloy preparation process is simple, the process is simple, the produced alloy has good performance, and is very convenient for industrial production. The material prepared by the present invention can be applied to magnetic devices in the fields of information, communication, etc. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is an electron microscope image of the organizational structure of the high saturation magnetic induction intensity iron-based alloy strip of the present invention. DETAILED DESCRIPTION

[0024] The present invention will be further described below in conjunction with specific embodiments.

[0025] A high saturation magnetic induction intensity iron-based alloy strip, whose components are as follows by weight percentage: Nb 0.5-0.9%, Cr 0.8-1.4%, In 0.02-0.06%, Al 0.5-0.9%, Pb 0.04-0.07%, Be 0.09-0.12%, Nd 0.1-0.6%, Au 0.03-0.04%, Si 0.3-0.8%, B 3-5%, Fe balance.

[0026] Its preparation method is:

[0027] First, the ingredients are prepared according to the above alloy components, and the purity of Nb, Cr, In, Al, Pb, Be, Nd, Au, and Fe in the raw materials is greater than 99.9%.

[0028] The raw materials are placed in a vacuum induction furnace for melting at a temperature of 1510-1560°C to obtain a master alloy, which is then placed in a remelting tubular crucible in a vacuum induction forming furnace for remelting at a temperature of 1510-1530°C; a through hole is provided at the bottom of the remelting tubular crucible, and the upper part of the remelting tubular crucible is connected to a nitrogen system via a valve, and the pressure of the nitrogen system is 1.5-1.7 atmospheres.

[0029] The bottom of the remelting crucible is placed 2 to 4 mm above the rim of the forming furnace wheel. When the master alloy is melted, the valve on the top of the remelting crucible is opened, and the molten master alloy is sprayed from the through hole at the bottom of the crucible to the rotating rim of the forming furnace wheel under nitrogen pressure to form a continuous alloy belt; the inner diameter of the remelting crucible is 12 to 14 mm, the height is 250 to 280 mm, and the through hole diameter at the bottom of the remelting crucible is 1.3 to 1.5 mm. The linear speed of the wheel is 25 to 27 m / s; the thickness of the obtained alloy belt is 300 to 350 μm and the width is 3 to 5 mm.

[0030] Then prepare molten salt in a resistance molten salt furnace: AgCl, NaCl, NaF, BeF2, Mg2B2O5·H2O, NdCl3, powdered SiO2, and silicon carbide powder are all pure substances with a purity of 99.99%. First, dry each substance at 150-180℃ for 6-8h, weigh each component according to the weight ratio of AgCl, NaCl, NaF, BeF2, Mg2B2O5·H2O, and NdCl3 of 0.1:1:3: (0.05-0.09):0.32:0.010, add 5-9% (mass fraction) of SiO2 and silicon carbide powder mixture in the molten salt medium, grind and mix well for use. The weight ratio of SiO2 to silicon carbide in the powder mixture is 1:0.1-0.3. The particle size of the powder substance is 270-300 mesh.

[0031] The cathode of the resistance molten salt furnace is silicon steel containing 4.5% Si and has a thickness of 0.8-1.5mm.

[0032] When the furnace temperature reaches 680-740℃, keep the temperature constant for 20-25min, and start to immerse the alloy strip in the molten salt. Connect the DC power supply, use pulse power supply, and control the average current density to 60-70mA / cm2. The alloy strip moves at a constant speed in the molten salt, and the travel speed is 0.07-0.11m / min. Keep the alloy strip in the molten salt for 25-30 minutes at each point. After the alloy strip is taken out of the molten salt, it is rolled up by the take-up machine, and the material preparation is completed.

[0033] The alloy strip is then placed in a liquid nitrogen atmosphere for low-temperature treatment at a temperature of -130°C to -150°C for 15 to 18 minutes; then placed at room temperature for 1 to 2 hours; then placed at 180 to 220°C for 2 to 4 hours, and then cooled to room temperature with the furnace.

[0034] Figure 1 The microstructure of the high saturation magnetic flux density iron-based alloy strip of the present invention is shown in Table 1. The microstructure is uniform and dense. The solution in patent CN201510674626.5 is used as a comparative example to measure the saturation magnetic flux density T of the present invention and the comparative example at 450°C. The measurement results are shown in Table 1.

[0035] Examples 1 to 3 in Table 1 all use the above preparation method to prepare high saturation magnetic flux density iron-based alloy strips, wherein the weight percentage of each component varies. The measurement results show that the material prepared by the present invention has good comprehensive performance. The percentage of raw materials used in Examples 4 and 5 is outside this range, and the performance is inferior to the solution of the present invention, but better than the comparative example.

[0036] Table 1

[0037]

[0038]

[0039] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Any technician familiar with the profession, without departing from the scope of the technical solution of the present invention, according to the technical essence of the present invention, any simple modification, equivalent replacement and improvement made to the above embodiment still falls within the protection scope of the technical solution of the present invention.

Claims

1. A method for preparing a high saturation magnetic induction intensity iron-based alloy strip, characterized in that: The following steps are involved: 1) First, the ingredients are prepared according to the alloy composition, which includes the following components according to the weight percentage: Nb 0.5-0.9%, Cr 0.8-1.4%, In 0.02-0.06%, Al 0.5-0.9%, Pb 0.04-0.07%, Be0.09-0.12%, Nd 0.1-0.6%, Au 0.03-0.04%, Si 0.3-0.8%, B 3-5%, Fe balance; the purity of Nb, Cr, In, Al, Pb, Be, Nd, Au, Fe in the raw materials is greater than 99.9%; 2) placing the raw materials in a vacuum induction furnace for smelting at a smelting temperature of 1510-1560° C. to obtain a master alloy, and then placing the raw materials in a remelting tubular crucible in a vacuum induction forming furnace for remelting at a remelting temperature of 1510-1530° C.; the bottom of the remelting tubular crucible is placed 2-4 mm above the rim of the rotating wheel of the forming furnace; when the master alloy is melted, opening the valve on the upper part of the remelting tubular crucible, the molten master alloy is sprayed from the through hole at the bottom of the crucible to the rotating rim of the forming furnace under nitrogen pressure to form a continuous alloy strip; 3) Then, a molten salt is prepared in a resistance molten salt furnace, wherein the molten salt components include AgCl, NaCl, NaF, BeF2, Mg2B2O5·H2O, NdCl3, powdered SiO2 and silicon carbide powder; the above molten salt components are all pure substances with a purity of 99.99%, wherein the particle size of the powdered substances used is 270-300 meshes; 4) When the temperature of the resistance molten salt furnace reaches 680-740 ℃, keep the temperature constant for 20-25 minutes, and start to immerse the alloy strip in the molten salt; connect the DC power supply and use pulse power supply; the alloy strip moves at a uniform speed in the molten salt, and the residence time of each point of the alloy strip in the molten salt is kept for 25-30 minutes; after the alloy strip is taken out of the molten salt, the strip is rolled up by the strip take-up machine, and the material preparation is completed; 5) The alloy strip is then placed in a liquid nitrogen atmosphere for low temperature treatment and kept warm; then placed at room temperature for static treatment; then placed under heating conditions and kept warm; then cooled to room temperature along with the furnace.

2. The method for preparing a high saturation magnetic induction intensity iron-based alloy strip according to claim 1, characterized in that: In step 2), a through hole is provided at the bottom of the remelting tubular crucible, and the upper part of the remelting tubular crucible is connected to a nitrogen system via a valve, and the pressure of the nitrogen system is 1.5 to 1.7 atmospheres.

3. The method for preparing a high saturation magnetic induction intensity iron-based alloy strip according to claim 1, characterized in that: In step 2), the inner diameter of the remelting crucible is 12-14 mm, the height is 250-280 mm, the diameter of the through hole at the bottom of the remelting crucible is 1.3-1.5 mm; the linear speed of the rotating wheel is 25-27 m / s; the thickness of the obtained alloy strip is 300-350 μm, and the width is 3-5 mm.

4. The method for preparing a high saturation magnetic induction intensity iron-based alloy strip according to claim 1, characterized in that: In step 3), when preparing molten salt in a resistance molten salt furnace, first dry each substance at 150-180 ° C for 6-8 h, weigh each component according to the weight ratio of AgCl, NaCl, NaF, BeF2, Mg2B2O5·H2O, and NdCl3 of 0.1:1:3: (0.05-0.09): 0.32:0.010, add a mixture of powdered SiO2 and powdered silicon carbide accounting for 5-9% of the mass fraction of the molten salt medium, grind and mix well for use; the alloy strip is the anode, and the cathode of the resistance molten salt furnace is silicon steel containing 4.5% Si and having a thickness of 0.8-1.5 mm.

5. The method for preparing a high saturation magnetic induction intensity iron-based alloy strip according to claim 4, characterized in that: in, The weight ratio of SiO2 to silicon carbide is 1:(0.1-0.3).

6. The method for preparing a high saturation magnetic induction intensity iron-based alloy strip according to claim 1, characterized in that: In step 5), the average current density is controlled to be 60-70 mA / cm2; the alloy strip moves at a constant speed in the molten salt, and the travel speed is 0.07-0.11 m / min.

7. The method for preparing a high saturation magnetic induction intensity iron-based alloy strip according to claim 1, characterized in that: In step 5), the alloy strip is placed in a liquid nitrogen atmosphere for low-temperature treatment at a temperature of -130°C to -150°C for 15 to 18 minutes; then placed at room temperature for 1 to 2 hours; then placed at 180 to 220°C for 2 to 4 hours, and then cooled to room temperature with the furnace.

Citation Information

Patent Citations

  • Fe-based amorphous and nanocrystalline soft magnetic alloy ribbon and preparation method thereof

    CN105261435A

  • Soft magnetic material and preparation method thereof

    CN107424707A

  • Ferrous alloy permanent magnet powder and its making method

    CN1303108A