Method for stirring liquid metal in electric arc furnace
Patent Information
- Application Number
- CN202080078178.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-09-19
- Filing Date
- 2020-09-15
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2040-09-15
AI Technical Summary
The temperature homogenization of liquid metal in existing electric arc furnaces is insufficient, leading to problems such as uneven element concentrations, process parameter errors, local temperature peaks, and premature component wear. Moreover, the role of the electromagnetic stirrer is not related to the steps of the melting cycle, limiting the liquid state. The best fusion of metals.
Arrange at least two electromagnetic stirrers in the electric arc furnace to generate mutually inconsistent and consistent electromagnetic fields to adjust the direction of the mixing force of the liquid metal in different steps, ensure uniform stirring and temperature homogenization of the steel, and optimize melting and refining in the furnace efficiency.
Through this method, the temperature and chemical composition uniformity of the liquid metal is achieved, the total energy consumption of the electric arc furnace is optimized and the cycle time is reduced, and the service life of the furnace components is extended.
Smart Images

Figure CN114729781B8_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for electromagnetically stirring liquid metal in an electric arc furnace, which can be used in the processing of melting metal materials with substantially continuous charging. Background Technology
[0002] Equipment for melting continuously charged metallic materials is known, comprising an electric arc furnace having at least one container or shell in which the metallic charge is melted.
[0003] The electric arc furnace also includes a covered top with holes for electrode passages, through which the electrodes enter the shell to allow the arc to be triggered, thereby allowing the metal charge to melt. The top also has holes for extracting flue gas, while the bottom or sides of the shell typically have devices for discharging molten metal.
[0004] An electric arc furnace is associated with a device for supplying metallic materials, which can be a continuous charging system.
[0005] Continuous charging schemes typically use a charging system with a basket to perform the initial start-up charge with the furnace closed, so as to generate a large amount of metal material at the bottom of the furnace to be melted at the beginning of the cycle. Usually, once the material is completely melted, the process of continuously charging scrap into the furnace begins.
[0006] In the most common configuration, the electric arc furnace has an eccentric discharge port at the bottom of the shell, known as "eccentric bottom discharge" or EBT. Alternatively, there may be a discharge trough at the bottom of the shell for extracting molten metal from the shell during the discharge step.
[0007] The discharge step follows the refining step, during which specific elements are introduced into the molten metal to improve its quality or impart desired properties, depending on the formulation of the steel to be obtained.
[0008] One of the most common drawbacks of this type of melting process is the lack of uniformity in the temperature of the molten metal within the shell.
[0009] A lack of temperature uniformity in molten metal can lead to problems such as unwanted concentrations of certain elements, incorrect measurement of process parameters, localized temperature spikes, premature wear of components, or other issues known in the art.
[0010] To address these issues, electromagnetic stirrers are known to be used, which are typically positioned below the bottom of the furnace or, at most, associated with its sidewalls.
[0011] For example, document WO 2018 / 145754 describes an electric arc furnace having an electromagnetic stirrer located approximately at the center below the bottom of the outer shell, and having an electromagnetic stirring axis intersecting a vertical plane passing through the center of the outer shell and the center of the discharge hole or discharge chute.
[0012] Document EP 2616560 B1 is also known, which describes an electric arc furnace equipped with two electromagnetic stirrers that are opposite each other relative to the central axis of the furnace.
[0013] US 3,409,726 is also known, which generally states that the direction of movement of molten metal can be easily reversed by reversing the polarity of the direct current or the excitation current of the electromagnet passing through the molten metal. US'726 describes the use of a magnetic pole with the center of the bottom of the casing as the axis, or, in addition to the central magnetic pole, the use of three magnetic poles arranged radially and equidistantly on the circumference of the electric furnace.
[0014] JP 62-73591 describes a magnetic stirring device for an electric arc furnace. The device includes an electromagnetic stirrer that can move below the furnace to present a variable position according to different steps of the melting cycle.
[0015] Schemes that use a stirrer to stir molten metal in a furnace typically do not provide a correlation between the role of the stirrer itself and the steps of the melting cycle.
[0016] This can lead to excessive wear on the inner wall of the casing, where the liquid metal has a higher velocity and defines a dead zone where the liquid metal tends to stagnate, rather than optimally blending with the surrounding liquid metal.
[0017] Therefore, there is a need to improve a method for electromagnetically stirring liquid metal in an electric arc furnace that can overcome the shortcomings of existing technologies.
[0018] In particular, one object of the present invention is to improve a method for electromagnetically stirring liquid metal in an electric arc furnace, which prevents uneven wear on the furnace walls and bottom, ensures uniform temperature of the liquid metal, and improves the efficiency of the melting and refining steps within the furnace.
[0019] The applicant has designed, tested and implemented the present invention to overcome the disadvantages of the prior art and to obtain these and other objectives and advantages. Summary of the Invention
[0020] The invention is set forth and its features are described in the independent claims. The dependent claims describe other features of the invention or variations of the main inventive concept.
[0021] In accordance with the above objectives, the present invention relates to a method for electromagnetically stirring liquid metal associated with the melting period in an electric arc furnace, the method providing at least one charging step (during which metal charge is introduced into the furnace), a melting step in the electric arc furnace, and a refining step of the liquid metal.
[0022] According to one aspect of the invention, this electromagnetic stirring is applied in a continuously charged electric arc furnace, wherein at least two electromagnetic stirrers arranged at or below the furnace bottom generate at least one first electromagnetic field along a first electromagnetic stirring axis and at least one second electromagnetic field along a second electromagnetic stirring axis.
[0023] According to one aspect of the invention, in at least a first step of the furnace cycle, a first electromagnetic field and a second electromagnetic field generate a mixed force on the liquid metal with inconsistent directions, and in at least a second step of the furnace cycle, the electromagnetic fields generate forces on the liquid metal with consistent directions.
[0024] In the description herein and below, the term “inconsistent” means that the axis of the mixing force generated by the first electromagnetic stirrer points in the opposite direction to the axis of the mixing force generated by the second electromagnetic stirrer; on the other hand, the term “consistent” means that the axes of the mixing forces generated by the two electromagnetic stirrers point in the same direction, i.e., they have the same direction.
[0025] In this way, when the axes of force are not aligned (or are opposite), the steel is stirred generally toward the entire periphery of the shell, and the steel moves in a basically circular and tangential manner relative to the refractory wall of the shell.
[0026] On the other hand, when the axes of the electromagnetic forces are aligned, the two agitators cause the steel to move toward the same peripheral area of the furnace, and the steel bounces off the periphery and returns toward the center.
[0027] By differentiating the mixing effects associated with the melting process, in addition to obtaining liquid metal with very uniform thermophysical and chemical composition properties, the total energy consumption of the electric arc furnace can be optimized and the total cycle time reduced. Attached Figure Description
[0028] These and other aspects, features, and advantages of the present invention will become apparent from the following description of some embodiments, which are given by way of non-limiting example with reference to the accompanying drawings, wherein:
[0029] - Figure 1 This is a cross-sectional schematic diagram of an electric arc furnace to which the electromagnetic stirring method of the present invention is applicable;
[0030] - Figure 2 and Figure 3 These are schematic diagrams of the stirring method according to the present invention;
[0031] - Figures 4a-4f This is a schematic diagram of a possible alternative arrangement of the electromagnetic stirrer in an electric arc furnace to which the electromagnetic stirring method of the present invention is applicable.
[0032] For ease of understanding, the same reference numerals have been used to denote the same common elements in the drawings where possible. It should be understood that elements and features of one embodiment can be readily incorporated into other embodiments without further explanation. Detailed Implementation
[0033] We will now refer in detail to possible embodiments of the invention, one or more of which are illustrated in the accompanying drawings. Each example is provided by way of illustration and should not be construed as limiting the invention. For example, features shown or described, as long as they are part of one embodiment, may be changed or adopted in other embodiments, or associated with other embodiments to produce other embodiments. It should be understood that the invention should include all such modifications and variations.
[0034] Before describing these embodiments, we must also clarify that this specification is not limited to its application to the details of the construction and arrangement of the components described below using the accompanying drawings. This specification may provide other embodiments and may be obtained or performed in various other ways. We must also clarify that the wording and terminology used herein are for descriptive purposes only and should not be considered limiting.
[0035] The embodiments described in the accompanying drawings relate to an electric arc furnace, generally indicated by reference numeral 10, in which liquid metal L is mixed using an electromagnetic stirring method according to the present invention.
[0036] The electric arc furnace 10 can be of the type powered by alternating current (AC) and characterized by the presence of three or more electrodes 14 between which an electric arc strikes to ignite and / or continue the melting process, or powered by direct current (DC) and characterized by the presence of one or two electrodes 14 arranged in the center, which perform the function of a cathode that cooperates with an anode located at the bottom of the electric arc furnace 10 to generate an electric arc.
[0037] Although the accompanying drawings described herein refer to an electric arc furnace 10 of the type powered by alternating current (AC), it is clear that the concepts described below also apply to an electric arc furnace 10 of the type powered by direct current (DC).
[0038] according to Figure 1 The embodiment shown includes an electric arc furnace 10 in its basic part a container or shell 11, and a covering element or top 12 arranged above and covering the shell 11.
[0039] For the electric arc furnace 10, there is a related device 13 to continuously supply the metal charge 25, which may include, for example, scrap S.
[0040] The feeding device 13 is adapted to move the metal charge 25 according to the determined feeding axis Z.
[0041] According to some embodiments, the supply device 13 can be arranged laterally, see Figure 1-3 The metal charge 25 is introduced from the side of the electric arc furnace 10, or from the top through a hole formed in the top 12.
[0042] The metal charge 25 is positioned on the feeding device 13 in a known manner and can have a defined size that can be highly variable.
[0043] Holes for accommodating and / or positioning electrodes 14 are formed in the top 12, and these holes are adapted to generate an electric arc to melt the metal charge present in the casing 11.
[0044] The top 12 and the electrode 14 are associated with lifting and rotating devices adapted to lift (or even lift each other independently) the top 12 and the electrode 14.
[0045] The outer shell 11 is provided with a bottom or furnace bottom 15 and sidewalls 16 made of at least part of refractory material to withstand the high temperature and highly reactive environment reached during the melting process.
[0046] The bottom 15 may be provided with an eccentric discharge port 17, also known as an "eccentric bottom discharge" (EBT), or alternatively or additionally, a discharge trough for extracting molten metal from the housing 11 during the discharge step.
[0047] The housing 11 is mounted on a bracket not visible in the accompanying drawings and is typically provided with an actuation device to rotate the housing 11 itself about a defined axis of rotation.
[0048] The furnace 10 also includes a liner 18, which has a lower edge 19 arranged on the upper edge of the outer casing 11.
[0049] The lining 18, typically consisting of a cooling plate, extends substantially along with the walls of the housing 11, and the top 12 is arranged above it to enclose the latter.
[0050] The lining 18 is provided with a first hole 20 and a second hole. The supply device 13 is positioned through the first hole 20 to supply the metal charge 25, and the slag discharge operation can be performed through the second hole.
[0051] Inside the outer casing 11, below the first hole 20, there is a charging area 28 where newly introduced metal charge 25 accumulates.
[0052] The charging zone 28 is located on the periphery of the electric arc furnace 10 where the electrode 14 is located.
[0053] The second orifice can be selectively accessed / inaccessible via the slag discharge gate 22, which is typically located opposite the discharge orifice 17. Figure 2-3 .
[0054] According to some embodiments, such as Figure 2 and Figure 3 As shown, the electric arc furnace 10 has two electromagnetic stirrers 23 and 24 below the outer shell 11, which are configured to generate mixing forces F1 and F2 in the liquid metal L inside the outer shell 11 during the smelting process.
[0055] As can be seen from the attached figures, the electromagnetic stirrers 23 and 24 can be arranged in a relative and mirror-symmetrical manner to form a pair of electromagnetic stirrers relative to the central plane P.
[0056] The electric arc furnace 10 includes a power supply 26 configured to power electromagnetic stirrers 23 and 24, and a control unit 27 operatively connected to the power supply 26 to control the drive of the electromagnetic stirrers 23 and 24.
[0057] According to some embodiments, each electromagnetic stirrer 23, 24 includes a body made of magnetic material, around which a coil of conductive material is wound. The coil is configured to be powered by a power supply 26 to generate a magnetic field in the direction of the axis of electromagnetic stirring of the electromagnetic stirrer 23, 24.
[0058] According to some embodiments, the control unit 27 may also be operatively associated with the power supply device 13 and the electrode 14.
[0059] The first electromagnetic stirrer 23 is energized to generate a first electromagnetic field along the first electromagnetic stirring axis X1.
[0060] The second electromagnetic stirrer 24 is energized to generate a second electromagnetic field along the second electromagnetic stirring axis X2.
[0061] According to another embodiment, as shown in FIG4, there may be more than two electromagnetic stirrers 123, 124, so as to generate a corresponding number of electromagnetic fields along the electromagnetic stirring axis X.
[0062] According to some embodiments, the electromagnetic stirrers 123, 124 can be arranged to form a pair of electromagnetic stirrers, for example, two pairs. Figure 4a , 4d ) or more, for example, three pairs ( Figure 4e ).
[0063] Alternative embodiments may provide an offset relative to the center plane P ( Figure 4d ) or alignment ( Figure 4e Pairs of opposing electromagnetic stirrers 123 are arranged.
[0064] According to other embodiments, a pair of electromagnetic stirrers 123, 124 can be positioned at different distances relative to the central plane P. Figure 4d ).
[0065] In other embodiments, different pairs of electromagnetic stirrers 123, 124 may have different distances from the central plane P. Figure 4a ).
[0066] Other embodiments may provide an odd number of electromagnetic stirrers 123, 124, such as 3 or 5. Figure 4b , 4c ).
[0067] In embodiments providing an odd number of electromagnetic stirrers 123, 124, at least two stirrers can be arranged as opposing pairs relative to the central plane P. Figure 4b ).
[0068] According to some embodiments, one or more electromagnetic stirrers 123, 124 can be arranged substantially aligned with the central plane P. Figure 4b , 4c ).
[0069] Some embodiments may provide a central plane P that asymmetrically divides the number of electromagnetic stirrers 123, 124. Figure 4c ).
[0070] In other embodiments, the electromagnetic stirrers 123, 124 may be arranged such that their stirring axis X is inclined relative to the central plane P, for example, orthogonal. Figure 4f ).
[0071] According to another embodiment not shown here, the electric arc furnace 10 may be equipped with electromagnetic stirrers 123, 124, whose stirring axes X are oriented differently relative to each other.
[0072] According to some embodiments, the dimensions of the electromagnetic stirrers 123, 124 may be appropriately determined relative to the dimensions of the housing 11 and / or the desired arrangement.
[0073] Some embodiments not shown here may provide an electric arc furnace 10 equipped with electromagnetic stirrers 123, 124 of different sizes relative to each other.
[0074] According to some embodiments, the first electromagnetic stirring axis X1 and the second electromagnetic stirring axis X2 are parallel to each other with respect to the central plane P.
[0075] The central plane P is vertical and passes through the center of the bottom 15 of the housing 11 and through the discharge hole 17, or alternatively through the discharge trough.
[0076] The central plane P can be a plane of symmetry with respect to at least the outer shell 11.
[0077] According to some embodiments, the housing 11 has a top planar cross-section, which may have a curved shape, for example defined by one or more curves appropriately selected from the group consisting of circles, parabolas, ellipses, and straight lines.
[0078] According to some embodiments, the housing 11 has an elongated curved shape in the direction of the discharge hole 17, so that the discharge hole 17 is located very far from the center of the housing 11.
[0079] Refer to examples Figure 2-3 A method for using liquid metal L in an electromagnetic stirring electric arc furnace 10 is described.
[0080] The melting process is carried out in the electric arc furnace 10, which includes at least one charging step, during which metal charge 25 is introduced and melted and added to the previously melted liquid metal L, and the subsequent step is to refine the liquid metal L in the electric arc furnace 10.
[0081] In the method according to the invention for electromagnetically stirring liquid metal in a continuously charged electric arc furnace 10, a first electromagnetic field along a first electromagnetic stirring axis X1 and a second electromagnetic field along a second electromagnetic stirring axis X2 are generated.
[0082] According to one aspect of the present invention, in a first step, the first electromagnetic field and the second electromagnetic field generate mixed forces F1 and F2 on the liquid metal L with inconsistent directions, and in a second step, these electromagnetic fields generate forces F1 and F2 on the liquid metal L with consistent directions.
[0083] In a favorable configuration, the first step is a loading step and the second step is a refining step.
[0084] According to some embodiments, such as Figure 2-3 As shown, during at least one charging step and during the refining step, the first electromagnetic stirring axis X1 and the second electromagnetic stirring axis X2 are parallel to each other with respect to the central vertical plane P, which passes through the center of the electric arc furnace 10 and through the discharge hole 17 of the electric arc furnace 10.
[0085] According to some embodiments, during at least one loading step, mixing forces F1 and F2 define the liquid metal flow L along a counterclockwise peripheral direction, see [link to embodiment]. Figure 2 .
[0086] In other words, during the loading step described above, the axes of the mixing forces F1 and F2 generated by the first electromagnetic stirrer 23 and the second electromagnetic stirrer 24 are oriented in opposite (or inconsistent) directions. Figure 2 In the diagram, the opposite direction of the generated force is represented by F3 for electromagnetic stirrer 23 and F4 for electromagnetic stirrer 24.
[0087] In this way, the steel is stirred mainly toward the entire periphery of the outer shell 11, and the movement of the liquid metal L is basically circular and tangential to the refractory wall of the outer shell 11.
[0088] In other embodiments, the mixing forces F1 and F2 define the liquid metal flow L (not shown) in a clockwise peripheral direction.
[0089] The positions of the magnetic stirrers 23 and 24, and the opposite and inconsistent directions of their stirring actions, are defined by their respective electromagnetic stirring axes X1 and X2, allowing the metal charge 25 to be introduced and accumulated in the corresponding charging zone 28 in an optimal manner. Due to the direction of the stirring force, the newly introduced metal charge 25 is gradually incorporated into the previous charge, thereby promoting temperature uniformity and corresponding to the area of the discharge port 17 located further away from the center of the electric arc furnace 10.
[0090] Furthermore, the construction and actuation mode of the electromagnetic stirrers 23 and 24 allow for a more uniform velocity distribution, preventing eddies and / or instabilities in the liquid metal L-flow.
[0091] In this configuration, the liquid metal flow L, being substantially circular and tangential to the sidewall 16 of the housing 11, exhibits a reduced radial component of momentum. This helps limit erosion of the sidewall 16 and thus reduces the need for frequent maintenance and repair interventions.
[0092] According to some embodiments, during the refining step, the mixing forces F1 and F2 have a consistent orientation, that is, the electromagnetic stirrers 23 and 24 are powered such that the axis of the generated electromagnetic force (in) Figure 3 (The electromagnetic stirrer 23 is represented by arrow F5, and the electromagnetic stirrer 24 is represented by arrow F4.) They have the same direction and orientation.
[0093] In this situation, both agitators 23 and 24 promote the movement of molten metal L towards the same peripheral area of furnace 10, particularly towards the eccentric discharge port 17. Then, the molten metal L rebounds at the periphery and returns towards the center, moving along the direction of the slag discharge gate 22. Figure 3 .
[0094] This also allows for temperature homogenization in the central region of the housing 11, during which the liquid metal L flows at a faster rate relative to the sidewalls 16 of the housing 11 during the loading step, with almost no mixing.
[0095] According to some embodiments, during at least one loading step and refining step, control unit 27 sends a control signal to power supply unit 26, which supplies power to first electromagnetic stirrer 23 with a first current and to second electromagnetic stirrer 24 with a second current to generate the aforementioned first electromagnetic field and second electromagnetic field, respectively, which are appropriately oriented in opposite (or opposite) directions or in the same direction (i.e., having the same orientation) depending on one or the other of the steps.
[0096] According to some embodiments, the control unit 27 can receive a charging signal from the supply device 13 that is proportional to the amount of metal charge 25 introduced into the electric arc furnace 10, and send an operation signal to the power supply device 26 to limit a first current and a second current based on the amount of metal charge 25 introduced.
[0097] The greater the amount of metal charge 25 introduced, the greater the current intensity, because the respective mixing forces F1 and F2 must stir a larger amount of liquid metal L.
[0098] This allows for automatic adjustment of the stirring action of electromagnetic stirrers 23 and 24, ensuring a perfect and uniform mixture of liquid metal L at all times.
[0099] According to some embodiments, the first current and the second current may have the same intensity during at least one charging step and refining step.
[0100] According to another embodiment, the first current and the second current may have different intensities during at least one charging step and refining step.
[0101] In particular, during the charging step, a current with a greater intensity than that during the refining step can be provided.
[0102] In fact, the presence of partially melted and / or solid metal charge 25 requires mixing forces F1 and F2 to be greater than the mixing forces required to stir the liquid metal L at the end of the melting process and during the refining step.
[0103] The intensity of the current can be adjusted in connection with and / or according to the amount of metal charge 25 introduced, in relation to the above charging and refining steps, allowing for optimization of the total energy consumption of the electric arc furnace 10.
[0104] Obviously, modifications and / or additions can be made to the above method for electromagnetically stirring liquid metal in an electric arc furnace without departing from the scope and domain of the present invention.
[0105] It is equally clear that, although the invention has been described with reference to some specific examples, those skilled in the art will certainly be able to implement many other equivalent forms of the method for electromagnetically stirring liquid metal in an electric arc furnace, which, having the features described in the claims, are all within the scope of protection defined by the claims.
[0106] In the following claims, the reference numerals in parentheses serve only for ease of reading: they shall not be regarded as limiting factors relating to the field of protection claimed in the particular claim.
Claims
1. A method for electromagnetically stirring liquid metal in a continuously charged electric arc furnace (10), wherein at least one first electromagnetic field along a first electromagnetic stirring axis (X1) and at least one second electromagnetic field along a second electromagnetic stirring axis (X2) are generated by electromagnetic stirrers (23, 24; 123, 124), characterized in that... In the first step of the furnace cycle, the first electromagnetic field and the second electromagnetic field generate mixed forces (F1, F2) with inconsistent directions on the liquid metal (L), and in the second step of the furnace cycle, the electromagnetic fields generate forces (F1, F2) with consistent directions on the liquid metal (L), and the first step is a charging step and the second step is a refining step.
2. The method according to claim 1, characterized in that... During the at least one charging step and during the refining step, the first electromagnetic stirring axis (X1) and the second electromagnetic stirring axis (X2) are parallel to each other with respect to the vertical center plane (P), which passes through the center of the electric arc furnace (10) and through the discharge port (17) of the electric arc furnace (10).
3. The method according to any one of the preceding claims, characterized in that... During the at least one loading step, the mixing forces (F1, F2) define the flow of liquid metal (L) in a counterclockwise peripheral direction.
4. The method according to any one of the preceding claims, characterized in that... During the at least one loading step, the mixing forces (F1, F2) define the flow of liquid metal (L) in a clockwise peripheral direction.
5. The method according to any one of the preceding claims, characterized in that... During the refining step, the mixing forces (F1, F2) define a flow of liquid metal (L) along the direction of the discharge orifice (17) and subsequently in the opposite direction toward the central region of the electric arc furnace (10).
6. The method according to any one of the preceding claims, characterized in that... During the at least one loading step and the refining step, the control unit (27) sends a control signal to the power supply unit (26), which supplies power to at least one first electromagnetic stirrer (23) with a first current and to at least one second electromagnetic stirrer (24) with a second current, so as to generate appropriately oriented first electromagnetic fields and second electromagnetic fields respectively according to one or the other of the steps.
7. The method according to claim 6, characterized in that... The control unit (27) receives a charging signal from the supply device (13) that is proportional to the amount of metal charge (25) introduced into the electric arc furnace (10), and sends the operation signal to the power supply device (26) such that the first current and the second current have an intensity proportional to the amount of metal charge (25) introduced.
8. The method according to claim 6 or 7, characterized in that... During the at least one charging step and the refining step, the first current and the second current have the same intensity.
9. The method according to claim 6 or 7, characterized in that... During the at least one charging step and the refining step, the first current and the second current have different intensities.
10. The method according to claim 9, characterized in that... In the at least one charging step, the first current and the second current have a greater intensity than the first current and the second current in the refining step.