然而,采用较为广泛的Sn3Ag0.5Cu焊料合金在服役过程中,钎焊接头处存在因焊缝区及界面区存在粗大的金属间化合物或因各连接材料的热膨胀系数不同而形成裂纹导致断裂,进而失效
[0012]1)本申请高可靠性无铅焊料合金无毒、无污染,是绿色型锡基钎料;
Smart Images

Figure BDA0003673042680000021 
Figure BDA0003673042680000031
Abstract
Description
Technical Field
[0001] The present application relates to a high-reliability lead-free solder alloy, which is mainly suitable for electronic component welding occasions with high requirements for welding strength and high requirements for environmental temperature adaptability. Background Art
[0002] With the rapid development of automotive electronics and the urgent need for 5G applications, the electronics industry has found that automotive electronic products are susceptible to continuous vibration and even impact during service, and require continuous stability of the operating temperature within the range of -40°C to +150°C and dormant energy saving of 5G products, which requires the durability of the joints in the electronic assembly interconnection. However, the widely used Sn3Ag0.5Cu solder alloy has cracks in the brazed joints during service due to the presence of coarse intermetallic compounds in the weld zone and interface zone or the different thermal expansion coefficients of the connecting materials, leading to fracture and failure.
[0003] Patent publication CN110430968A proposes to add Bi, Sb, Co, and Ni elements to SnAgCu to optimize the alloy structure in the joint to improve the vibration resistance of the joint, but there are still shortcomings such as high reflow peak temperature. Summary of the invention
[0004] The technical problem solved by the present application is to overcome the above-mentioned deficiencies in the prior art and provide a high-reliability lead-free solder alloy with good wettability, moderate melting point, good solder joint quality and long-lasting durability.
[0005] The technical solution adopted by the present application to solve the above technical problems is: a high-reliability lead-free solder alloy, characterized in that the mass percentages of the components of the high-reliability lead-free solder alloy are: Ag: 1.5%~4%, Cu: 0.4%~1%, Ni: 0.1%~0.6%, Bi: 2%~4%, Sb: 1%~4%, P: 0.01%~0.3%, In: 0%~0.3%, trace element Re: 0.001%~0.1%, Sn: balance; the trace element Re is composed of one or more of Ce, Ga, and La.
[0006] Preferably, the mass percentages of the components of the high-reliability lead-free solder alloy are: Ag: 2.5% to 3.8%, Cu: 0.5% to 0.8%, Ni: 0.15% to 0.3%, Bi: 2.5% to 4%, Sb: 2% to 3%, P: 0.01% to 0.3%, In: 0% to 0.3%, trace elements Re: 0.001% to 0.1%, Sn: balance.
[0007] The melting temperature of the high reliability lead-free solder alloy described in the present application is between 214°C and 231°C.
[0008] The high-reliability lead-free solder alloy of the present application adds a variety of elements to the main body of the tin alloy, among which the addition of Ag element can form a granular Ag3Sn phase-reinforced alloy with Sn and improve the wettability of the solder; the addition of Cu element improves the mechanical properties of the alloy when forming a CuSn intermetallic compound phase, while reducing the diffusion of Cu elements from the Cu substrate, and the role of Ni is basically the same as that of Cu; the element Bi can greatly reduce the solidus and liquidus temperature of the alloy, but because Bi and its alloys are relatively brittle and need to be strictly controlled, appropriate melting point-reducing elements In and P are added, and P can also form compounds with Sn to disperse and precipitate, refine the structure and thus improve the mechanical properties; the addition of trace elements further refines the alloy structure and thereby stabilizes the evolution of the microstructure of the solder joint during service and slows down the growth of intermetallic compounds.
[0009] The preparation method of the high reliability lead-free solder alloy of the present application is as follows: each master alloy is mixed with Sn ingot and In ingot in proportion and put into a melting furnace for melting. Attention should be paid to the order of adding materials, and the low melting point, easy to burn and trace elements Re or alloy wrapped with tin foil should be added last to ensure the final alloy composition.
[0010] The high reliability lead-free solder alloy of the present application can be used for solder ingots, solder wires, preforms, solder balls, solder powder, solder paste, etc.
[0011] The high reliability lead-free solder alloy of the present application has the following beneficial effects:
[0012] 1) The high-reliability lead-free solder alloy of the present application is non-toxic, non-polluting, and is a green tin-based solder;
[0013] 2) The high reliability lead-free solder alloy of the present application has a suitable melting point, which can reduce deformation caused by excessive temperature during soldering;
[0014] 3) The high-reliability lead-free solder alloy of the present application has good hot and cold processing performance and high reliability, and is suitable for durable application scenarios in the field of electronic packaging. DETAILED DESCRIPTION
[0015] The present application is further described in detail below through examples, which are provided to explain the present application but are not limited to the following examples. Trace elements are represented by Re.
[0016] The components and mass percentage contents of the alloying elements are prepared according to the embodiment, the intermediate alloy is mixed with Sn ingots and In ingots (if containing In) in proportion and put into a tin melting furnace for smelting at a smelting temperature of 450°C-500°C for 20min-30min. Finally, the Sn-P and Sn-Re intermediate alloys wrapped with tin foil are added to the melt using a stainless steel bell jar, and then fully stirred until uniform. The molten alloy is cast into a tin-based master alloy, and then processed into welding wires, preforms, solder balls, solder powder, solder paste, etc.
[0017] The composition and performance-related data of the script in each embodiment are shown in the table. The element content values in the table are mass percentages. The relevant data of Examples 1-9 are as follows.
[0018]
[0019]
[0020] Note: The combination of trace element Re in each embodiment is as follows: Embodiment 1 and 4 are Ce, Embodiment 2 and 7 are Ga, Embodiment 4 and 8 are La, Embodiment 3 and 5 use Ce and Ga with a Ce:Ga ratio of 7:3, Embodiment 6 and 9 use Ga and L with a Ga:La ratio of 3:2.
[0021] The formula design in this embodiment is reasonable, and the lead-free solder applied for is non-toxic, non-polluting, has good processing performance, a suitable melting temperature range, and good mechanical properties, and can be applied to durable solder joints in the field of electronic packaging.
Claims
1. A high reliability lead-free solder alloy, characterized in that The mass percentages of the components of the high-reliability lead-free solder alloy are: Ag: 1.5% to 4%, Cu: 0.4% to 1%, Ni: 0.1% to 0.6%, Bi: 2% to 4%, Sb: 1% to 4%, P: 0.3%, In: 0% to 0.3%, trace element Re: 0.001% to 0.1%, Sn: balance; the trace element Re is composed of one or more of Ce, Ga, and La.
2. The high reliability lead-free solder alloy according to claim 1, characterized in that: The mass percentages of the components of the high reliability lead-free solder alloy are: Ag: 2.5% to 3.8%, Cu: 0.5% to 0.8%, Ni: 0.15% to 0.3%, Bi: 2.5% to 4%, Sb: 2% to 3%, P: 0.3%, In: 0% to 0.3%, trace element Re: 0.001% to 0.1%, Sn: balance.