Production of monoethylene glycol
By pretreating wood-based raw materials and multi-step reaction treatment, the problem that monoethylene glycol production in the prior art depends on non-renewable resources, and efficient and environmentally friendly monoethylene glycol production is achieved.
Patent Information
- Application Number
- CN202180009983.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-01-15
- Filing Date
- 2021-01-08
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2041-01-08
AI Technical Summary
The methods for producing monoethylene glycol in the prior art rely mainly on non-renewable resources and lack solutions to use bio-based materials.
Monoethylene glycol is produced by pretreating the wood-based feedstock, including mechanical treatment and multi-step reaction treatment, such as enzymatic hydrolysis and catalytic conversion. The method includes providing a wood-based feedstock, pretreatment to form liquid portions and solid cellulose particles, followed by enzymatic hydrolysis and catalytic conversion, and ultimately recovering monoethylene glycol.
It realizes efficient production of monoethylene glycol from bio-based materials, reduces dependence on non-renewable resources, and provides an environmentally friendly production path.
Smart Images

Figure CN114981234B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a method for producing monoethylene glycol (MEG) from wood-based raw materials. The present disclosure also relates to an apparatus for producing monoethylene glycol (MEG) from wood-based raw materials. The present invention also relates to monoethylene glycol obtained by the method described in this specification. Background Art
[0002] Monoethylene glycol (MEG), also known as ethylene glycol or 1,2-ethylene glycol, is an important liquid raw material that can be used, for example, in the manufacture of polyethylene terephthalate (PET) and polyester resins. Monoethylene glycol can be used in applications requiring resins as chemical intermediates, solvent coupling agents, freezing point depressants, solvents, humectants, and chemical intermediates. The increasing use of monoethylene glycol in the polyester fiber and polyethylene terephthalate industries is driving the growth of the global monoethylene glycol market. Conventional methods for producing ethylene glycol involve the use of non-renewable resources. The inventors therefore recognized the need to provide a method for producing monoethylene glycol using bio-based materials. Summary of the invention
[0003] A method for producing monoethylene glycol from a wood-based feedstock is disclosed. The method may include: i) providing a wood-based feedstock derived from a wood-based feedstock and comprising wood chips, wherein up to 5% by weight of the wood chips in the wood-based feedstock are extra-thick wood chips as specified in SCAN-CM 40:01, subjecting the wood feedstock to at least one pretreatment to form a liquid portion and a portion comprising solid cellulose particles. The method may further include: ii) subjecting the portion comprising solid cellulose particles to enzymatic hydrolysis to form a lignin portion and a carbohydrate portion. The method may further include: iii) subjecting the carbohydrate portion to catalytic conversion to form a liquid composition of glycol. The method may further include: iv) recovering monoethylene glycol from the liquid composition of glycol.
[0004] Further disclosed is an apparatus for producing monoethylene glycol from a wood-based feedstock. The apparatus may include at least one pretreatment unit configured to subject a wood-based feedstock derived from the wood-based feedstock and comprising wood chips to at least one pretreatment to form a liquid portion and a portion comprising solid cellulose particles, wherein up to 5% by weight of the wood chips in the wood-based feedstock are ultra-thick wood chips as specified in SCAN-CM 40:01. The apparatus may also include at least one hydrolysis reactor configured to subject the portion comprising solid cellulose particles to enzymatic hydrolysis to form a lignin portion and a carbohydrate portion. The apparatus may also include a conversion reactor configured to subject the carbohydrate portion to catalytic conversion to form a liquid composition of glycols. The apparatus may also include a distillation unit configured to recover monoethylene glycol from the liquid composition of glycols.
[0005] Further disclosed is monoethylene glycol produced by the process as described in the present specification. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] The accompanying drawings provide a further understanding of the embodiments and constitute a part of this specification, illustrating various embodiments. In the drawings:
[0007] Figure 1 is a flow chart of one embodiment of a method for producing monoethylene glycol;
[0008] Figure 2 One embodiment of an apparatus for producing monoethylene glycol is shown;
[0009] Figure 3 showing the proposed chip grader in SCAN-CM 40:01; and
[0010] Figure 4 and Figure 5 The measurements performed when measuring the geometric specific surface area (GSSA) are shown. DETAILED DESCRIPTION
[0011] A method for producing monoethylene glycol (MEG) from wood-based raw materials is disclosed. The method may include the following steps:
[0012] i) providing a wood-based feedstock derived from a wood-based raw material and comprising wood chips, wherein up to 5 wt. % of the wood chips in the wood-based feedstock are extra thick wood chips as specified in SCAN-CM 40:01, subjecting the wood feedstock to at least one pretreatment to form a liquid fraction and a fraction comprising solid cellulose particles;
[0013] ii) subjecting the fraction comprising solid cellulose particles to enzymatic hydrolysis to form a lignin fraction and a carbohydrate fraction;
[0014] iii) subjecting the carbohydrate portion to a catalytic conversion to form a liquid composition of a diol; and
[0015] iv) recovering monoethylene glycol from the liquid composition of glycols.
[0016] Further disclosed is an apparatus for producing monoethylene glycol (MEG) from wood raw materials. The apparatus may include:
[0017] at least one pretreatment unit configured to subject a wood-based feedstock derived from a wood-based raw material and comprising wood chips to at least one pretreatment to form a liquid portion and a portion comprising solid cellulose particles, wherein at most 5 wt. % of the wood chips in the wood-based feedstock are extra thick wood chips as specified in SCAN-CM 40:01;
[0018] at least one hydrolysis reactor configured to subject the fraction comprising solid cellulose particles to enzymatic hydrolysis to form a lignin fraction and a carbohydrate fraction;
[0019] a conversion reactor configured to subject the carbohydrate portion to catalytic conversion to form a liquid composition of diols; and
[0020] A distillation unit configured to recover monoethylene glycol from the liquid composition of glycols.
[0021] Further disclosed is monoethylene glycol (MEG) obtained by the process described in the present specification.
[0022] Unless otherwise indicated, the expression "pretreatment" or "pretreatment" in this specification should be understood as the process of (a) converting the wood-based feedstock into a portion containing solid cellulose particles. As a result of the pretreatment, in addition to the portion containing solid cellulose particles, a liquid portion may also be formed. The liquid portion may be separated from the portion containing solid cellulose particles. The portion containing solid cellulose particles may further include a certain amount of lignocellulose particles and lignin particles in free form. Lignocellulose comprises lignin chemically bonded to the cellulose particles. The wood-based raw material may be selected from hardwood, softwood and a combination thereof. The wood-based raw material may, for example, be derived from pine, poplar, beech, poplar, spruce, eucalyptus, ash or birch. The wood-based raw material may also be any combination or mixture of these woods. The wood-based raw material may be hardwood. Preferably, the wood-based raw material is hardwood because it has a higher inherent sugar content, but the use of other types of wood is not excluded. Hardwood may be selected from any combination of beech, birch, ash, oak, maple, chestnut, willow, poplar and a mixture thereof.
[0023] Providing the wood-based feedstock in step i) may include subjecting the wood-based feedstock to a mechanical treatment selected from the group consisting of peeling, slicing, splitting, cutting, pulping, grinding, crushing, splitting, sieving and / or washing the wood-based feedstock to form the wood-based feedstock.
[0024] The apparatus may include a mechanical unit configured to mechanically process the wood-based feedstock, the mechanical processing being selected from the group consisting of peeling, slicing, splitting, cutting, beating, grinding, crushing, splitting, screening and / or washing the wood-based feedstock to form the wood-based feedstock.
[0025] Therefore, providing a wood-based feedstock derived from a wood-based raw material can include subjecting the wood-based raw material to a mechanical treatment to form the wood-based feedstock. The mechanical treatment can include peeling, slicing, splitting, cutting, pulping, grinding, crushing, splitting, screening and / or washing the wood-based raw material. During the mechanical treatment, for example, logs can be debarked and / or formed into wood chips of a specific size and structure. The formed wood chips can also be cleaned, for example, with water, to remove materials such as sand, gravel and stone therein. In addition, before the pretreatment step, the structure of the wood chips may be loosened. The wood-based feedstock may contain a certain amount of bark from the logs.
[0026] Providing the wood-based feedstock may include purchasing the wood-based feedstock. The purchased wood-based feedstock may include purchased wood chips or wood shavings derived from wood-based raw materials.
[0027] In one embodiment, the wood chips have a specific surface area (SSA) of 2-35 cm 2 / g, or 4–33 cm 2 / g, or 6–30cm 2 / g, or 10–25 cm 2 / g, or 12–20 cm 2 / g.
[0028] The specific surface area (SSA) of wood chips can be measured by applying water on the surface of the wood chips and measuring the mass of the water (SSA measured by liquid adsorption method). Based on the mass of the applied water, the average specific surface area of the wood chips per specific mass of dry matter can be calculated. The wood chips are soaked before measurement to reach the cell wall saturation point. This prevents the water to be applied from being absorbed into the wood. After soaking, the surface of the multiple wood chips is dehydrated by centrifugation. The mass of the multiple wood chips after centrifugation is weighed. Thereafter, a water film is applied on the surface of the multiple wood chips by immersing the multiple wood chips in water. The multiple wood chips wetted in this way are weighed again. The mass of the applied water can be calculated by the mass difference between the multiple wood chips with a dry surface and the multiple wood chips coated with a water film. After this, the multiple wood chips are dried to obtain the amount of dry matter in the sample. The specific surface area is calculated based on the ratio of the mass of water applied to the surface of the multiple wood chips to the amount of dry matter in the multiple wood chips. Calculation is performed by using the formula given below. Therefore, the specific surface area can be determined in the following way: 100 g wet weight of the well-mixed sample is weighed in a metal basket. The numbered metal basket is placed in a plastic bucket that has been filled with water at room temperature. Make sure that all the multiple wood chips are below the water surface. Soak the sample for at least 8 hours, and most preferably overnight, so that the cell walls and cell cavities of the wood are filled with water. This way, there is no water absorption into the wood chips later to affect the specific surface area results. After soaking, the sample is placed in a centrifuge bag at standard humidity. The humidity of the centrifuge bag is standardized by immersing the centrifuge bag in water and centrifuging for 2 minutes before each sampling point. The sample is centrifuged for 4 minutes. The sample is weighed in the basket (weight 1.) to the nearest 0.01 g. The weighing result is recorded. The weighed sample is re-immersed in water for 2 minutes, making sure that all the multiple wood chips are under water. After this, the sample is drained in the basket above the bucket for 30 seconds. Transfer the wet wood chips to a tared drying container and weigh (weight 2.) to the nearest 0.01 g, and record the weighing result. Dry the sample in a 105±2℃ incubator overnight. After drying, weigh the sample (weight 3.). Record the weighing result. According to the following formula g 水 / g od_木 (grams of water applied per gram of dry matter) Calculation result:
[0029] g 水 / g od_木 =(g 湿 -g 干 ) / g od_木
[0030] Among them, g 干 =Weight 1.(g)
[0031] g 湿 =Weight 2.(g)
[0032] g od_木=Weight 3.(g)
[0033] The result is calculated as the average of two parallel measurements. The measurement result is converted into grams of water applied per gram of dry matter by calculation. The result of grams of water per gram of dry matter (g 水 / g od_木) Convert to specific surface area (SSA):
[0034] SSA[cm 2 / g od_木 ]=26,531*(g 水 / g od_木 ) 2 +113,86*(g 水 / g od_木 )-19,718
[0035] In one embodiment, the wood chips have a geometric specific surface area (GSSA) of 4-40 cm 2 / g, or 5–35 cm 2 / g, or 6–30cm 2 / g, or 10–25 cm 2 / g, or 12–20 cm 2 / g.
[0036] The geometric specific surface area (GSSA) can be measured as follows: First the size distribution of the wood chips is measured according to SCAN-CM 40:01:
[0037] Size Class Fraction% Size class over 45mm% F1 Size grade extra thick 45–8mm% F2 Size grade 8-13mm% F3 Size grade 13-7mm% F4 Size grade 7-3mm% F5 Size grade fine material <3mm% F6
[0038] Then, 50 wood chips were randomly selected from each accepted fraction and the following dimensions of each chip were measured, such as Figure 4 As shown. According to SCAN-CM 48:01 (revised in 2001), the mass-weighted averages of length and width of the wood chips in each fraction are measured. The wood chips are divided into 15 grades within each fraction, and the mass-weighted averages of length and width are calculated:
[0039] Length grade Fraction% <10 L1 10,1-13 L2 13,1-16 L3 16,1-19 L4 19,1-22 L5 22,1-25 L6 25,1-28 L7 28,1-31 L8 31,1-34 L9 34,1-37 L10 37,1-40 L11 40,1-43 L12 43,1-46 L13 46,1-49 L14 >49 L15
[0040] Width Grade Fraction% <10 W1 10,1-13 W2 13,1-16 W3 16,1-19 W4 19,1-22 W5 22,1-25 W6 25,1-28 W7 28,1-31 W8 31,1-34 W9 34,1-37 W10 37,1-40 W11 40,1-43 W12 43,1-46 W13 46,1-49 W14 >49 W15
[0041] Then the wood chip thickness of each wood chip was measured with an accuracy of 0.1 mm, and the wood chips were classified into 15 grades, namely T1, T2...T15, from thinnest to thickest, and the average thickness of each grade and the mass weight of each grade were calculated in the same way as in SCAN-CM 48:01. The mass weighted average of the thickness was calculated.
[0042] Then measure the cutting angles of 10 wood pieces of each fraction, and calculate the average value An of the angles.
[0043] Then measure the angle of each wood piece, such as Figure 5 As shown, take a piece of wood and draw the cutting angle on paper; lengthen the sides of the angle to form a right triangle, the larger the more accurate; measure the opposite side and hypotenuse of the triangle; and calculate the angle according to the equation An = arcsin (A / B). Then the geometric specific surface area (GSSA) of each fraction can be calculated by the following formula:
[0044] GSSAn=20000*(Wn*Ln+Tn*Ln+Wn*Tn / sin(An)) / (Ln*Wn*Tn*BD)
[0045] Where GSSAn = specific surface area of fraction Fn, [cm 2 / g]
[0046] Wn = mass-weighted average width of the wood chips in fraction Fn, [mm]
[0047] Ln = mass-weighted average length of the wood chips in fraction Fn, [mm]
[0048] Tn = mass-weighted average of the thickness of the wood chips in fraction Fn, [mm]
[0049] An = average value of the chip cutting angle in each fraction Fn, [radians]
[0050] BD = basic density of wood, [kg dry wood / m solid of wet wood 3 ]
[0051] Then, the mass-weighted average of the geometric specific surface area (GSSA) can be calculated by the following formula:
[0052] GSSA=(∑(SSAn*Fn)) / 100
[0053] in,
[0054] GSSA = Geometric Specific Surface Area of Wood Chips
[0055] GSSAn = mass-weighted average of the geometric specific surface areas of fractions Fn, [cm 2 / g]
[0056] Fn = mass fraction of chips of each size classified according to standard SCAN-CM 40:01.
[0057] The wood-based feedstock may comprise wood chips, wherein up to 5 wt. % of the wood chips in the wood-based feedstock are extra thick wood chips as defined in SCAN-CM 40:01. Standard SCAN-CM 40:01 (revised in 2001) describes a chip grading method in which a sample of the wood chips is placed on top of a screen consisting of five screen trays and one fines tray (see Figure 3 ). The screen has holes or slits of a specific size, and the stack keeps reciprocating. After a specified time, the screening is stopped and the six grades obtained are weighed separately. The size of each grade is its mass, expressed as a percentage of the total mass of all six grades.
[0058] Unless otherwise stated, in this specification, the characterisation of wood chips in the wood-based feedstock as "extra thick chips" is to be understood as chips which pass through the first screen of a chip grader but are retained on the second screen comprising 8 mm slots when the chips are size graded as specified in SCAN-CM 40:01.
[0059] Unless otherwise stated, in this specification the characterization of wood chips in the wood-based feedstock as "fines" is understood to mean that there are no wood chips retained even on the fifth screen containing 3 mm holes when the wood chips are size graded as specified in SCAN-CM 40:01.
[0060] In one embodiment, at most 3.5 wt%, or at most 3 wt%, or at most 2.5 wt%, or at most 2 wt% of the wood chips in the wood-based feedstock are extra thick wood chips as specified in SCAN-CM 40:01.
[0061] In one embodiment, at most 10 wt%, or at most 6 wt%, or at most 3 wt%, or at most 1.5 wt%, or at most 0.5 wt% of the wood chips in the wood-based feedstock are fines as defined in SCAN-CM40:01.
[0062] In one embodiment, at most 3 wt%, or at most 1 wt%, or at most 0.5 wt%, or at most 0.1 wt%, or substantially 0 wt% of the wood chips in the wood-based feedstock are oversized wood chips as specified in SCAN-CM 40:01. That is, oversized wood chips can be substantially removed from the wood-based feedstock. Unless otherwise specified, in this specification, the feature that wood chips in the wood-based feedstock are "oversized wood chips" should be understood as wood chips that do not pass through the first screen containing 45 mm holes when the wood chip size is classified as specified in SCAN-CM 40:01.
[0063] The inventors have surprisingly found that the impregnation liquid more evenly absorbs and impregnates a feedstock containing chips of a given size, particularly when the amount of oversized chips is minimized and the amount of extra thick chips in the feedstock is controlled.
[0064] The pretreatment of the wood-based feedstock in step i) may comprise one or more different pretreatment processes. In different pretreatment processes, the wood-based feedstock may vary. The purpose of at least one pretreatment process is to form a fraction comprising solid cellulose particles for further processing.
[0065] Pretreatment i) may include pre-steaming the wood-based feedstock. Pretreatment i) may include pre-steaming the wood-based feedstock received from mechanical treatment. The pretreatment in i) may include impregnation treatment and / or steam explosion, and includes pre-steaming the wood-based feedstock before impregnation treatment and / or steam explosion, wherein the pre-steaming of the wood-based feedstock is carried out at atmospheric pressure with steam at a temperature of 100-130°C. During pre-steaming, the wood-based feedstock is treated with low-pressure steam. Pre-steaming may also be carried out with steam at a temperature below 100°C, or below 98°C, or below 95°C. Pre-steaming has the additional effect of reducing or removing air inside the wood-based feedstock.
[0066] Pre-steaming may be performed in at least one pre-steaming reactor. In one embodiment, one of the at least one pre-treatment units is a pre-steaming reactor configured to subject the wood-based feedstock to pre-steaming. In one embodiment, one of the at least one pre-treatment units is a pre-steaming reactor operably disposed before the impregnation reactor and / or the pressurization reactor and configured to subject the wood-based feedstock to pre-steaming with steam at a temperature of 100-130° C. at atmospheric pressure.
[0067] Furthermore, the pretreatment of i) may include subjecting the wood-based feedstock to at least one impregnation treatment with an impregnation liquid. The impregnation treatment may be performed on the wood-based feedstock received from the mechanical treatment and / or from the pre-steaming. The pretreatment in i) may include, prior to steam explosion, subjecting the wood-based feedstock to at least one impregnation treatment with an impregnation liquid selected from water, at least one acid, at least one base, at least one alcohol, or any combination or mixture thereof.
[0068] The inventors have surprisingly found that a specific size range of wood chips in a wood-based feedstock has the added benefit of beneficially affecting the impregnation process. It has surprisingly been found that when using wood chips of a specific size, the impregnation liquid can be more evenly distributed and absorbed into the wood chips.
[0069] A feeder may be used to transfer the wood-based feedstock from the mechanical treatment and / or from the pre-steaming to the impregnation treatment. The feeder may be a screw feeder, such as a plug screw feeder. The feeder may compress the wood-based feedstock during the transfer process. When the wood-based feedstock subsequently enters the impregnation treatment, it may swell and absorb the impregnation liquid.
[0070] The impregnation liquid may include water, at least one acid, at least one base, at least one alcohol, or any combination or mixture thereof. The at least one acid may be selected from the group consisting of an inorganic acid, such as sulfuric acid (H2SO4), nitric acid, phosphoric acid; an organic acid, such as acetic acid, lactic acid, formic acid, carbonic acid; and any combination or mixture thereof. In one embodiment, the impregnation liquid includes sulfuric acid, such as dilute sulfuric acid. The concentration of the acid may be 0.3–5.0% w / w, 0.5–3.0% w / w, 0.6–2.5% w / w, 0.7–1.9% w / w, or 1.0–1.6% w / w. The impregnation liquid may act as a catalyst to affect the hydrolysis of hemicellulose in the wood-based feedstock. In one embodiment, the impregnation is performed using only water, i.e., by autohydrolysis. In one embodiment, the wood-based feedstock may be impregnated by alkaline hydrolysis. NaOH and Ca2(OH)3 may be mentioned as examples of bases used in alkaline hydrolysis.
[0071] One of the at least one pretreatment units may be an impregnation reactor configured to subject the wood-based feedstock to at least one impregnation treatment with an impregnation liquid. One of the at least one pretreatment unit may be an impregnation reactor operably disposed before the pressurized reactor and configured to subject the wood-based feedstock to at least one impregnation treatment with an impregnation liquid selected from water, at least one acid, at least one alcohol, or any combination or mixture thereof. Thus, the impregnation treatment may be performed in at least one impregnation reactor or container. In one embodiment, two or more impregnation reactors are used.
[0072] The transfer from one impregnation reactor to another can be carried out using a feeder, such as a screw feeder. The feeder can, together with the steam, eliminate differences in liquid concentration within the wood chips, so that the impregnation liquid can more easily penetrate the wood chips.
[0073] The impregnation process can be carried out by conveying the wood-based feedstock through at least one impregnation reactor, i.e., the wood-based feedstock can be transferred into the impregnation reactor, spread within the impregnation reactor, and then transferred out of the impregnation reactor so that the wood-based feedstock is uniformly impregnated with the impregnation liquid. The impregnation process can be carried out in a batch process or in a continuous manner.
[0074] The residence time of the wood-based feedstock in the impregnation reactor, i.e. the time the wood-based feedstock is in contact with the impregnation liquid, may be 5 seconds to 5 minutes, or 0.5 to 3 minutes, or about 1 minute. The temperature of the impregnation liquid may be, for example, 20-99°C, or 40-95°C, or 60-90°C. Maintaining the temperature of the impregnation liquid below 100°C has the additional effect of preventing or reducing the dissolution of hemicellulose.
[0075] After the impregnation treatment, the wood-based feedstock may be allowed to remain in, for example, a storage tank or silo for a predetermined period of time to allow the impregnation liquid absorbed into the wood-based feedstock to stabilize. This predetermined period of time may be 15-60 minutes, or for example about 30 minutes.
[0076] Pretreatment i) may include subjecting the wood-based feedstock to steam explosion. Wood-based feedstock from mechanical treatment, pre-steaming step and / or from impregnation treatment may be subjected to steam explosion. In one embodiment, pretreatment i) includes at least one of the following: mechanically treating the wood-based material to form a wood-based feedstock, pre-steaming the wood-based feedstock, impregnating the wood-based feedstock, and steam explosion of the wood-based feedstock. In one embodiment, pretreatment i) includes mechanically treating the wood-based material to form a wood-based feedstock, pre-steaming the wood-based feedstock, impregnating the wood-based feedstock, and steam explosion of the wood-based feedstock. In one embodiment, pretreatment i) includes pre-steaming the wood-based feedstock, impregnating the wood-based feedstock, and steam explosion of the wood-based feedstock. In one embodiment, pretreatment i) includes impregnating the wood-based feedstock, and steam explosion of the wood-based feedstock. That is, the wood-based feedstock that has been impregnated may subsequently be steam exploded. Additionally, the pre-steamed wood-based feedstock may be subsequently subjected to an impregnation process, and then the impregnated wood-based feedstock may be steam exploded.
[0077] The wood-based feedstock may be stored, for example, in chip boxes or silos between different treatments. Alternatively, the wood-based feedstock may be transferred from one treatment to another in a continuous manner.
[0078] The pre-treatment in i) may include subjecting the wood-based feedstock to steam explosion, which is accomplished by treating the wood-based feedstock with steam at a temperature of 130-240°C at a pressure of 0.17-3.25 MPaG, and then suddenly and explosively depressurizing the wood-based feedstock. The wood-based feedstock may be treated with steam for 1-20 minutes, or 1-20 minutes, or 2-16 minutes, or 4-13 minutes, or 3-10 minutes, or 3-8 minutes, and then suddenly and explosively depressurizing the wood-based feedstock.
[0079] In this specification, the term "steam explosion" may refer to a semi-hydrolysis process in which a wood-based feedstock is treated with steam at a temperature of 130-240°C at a pressure of 0.17-3.25 MPaG in a reactor, and then the wood-based feedstock is suddenly and explosively depressurized, resulting in the rupture of the fiber structure of the wood-based feedstock.
[0080] The steam explosion process may be carried out in a pressurized reactor. That is, one of the at least one pretreatment units may be a pressurized reactor configured to subject a wood-based feedstock derived from a wood-based raw material to steam explosion. The steam explosion may be carried out in a pressurized reactor by treating the wood-based feedstock with steam at a temperature of 130-240°C at a pressure of 0.17-3.25 MPaG and then subjecting the wood-based feedstock to a sudden, explosive decompression. The wood-based feedstock may be introduced into the pressurized reactor using a compression conveyor, such as a screw feeder. If a screw feeder is used, a portion of the impregnation liquid absorbed by the wood-based feedstock is removed as a pressurized liquid during conveying using the screw feeder, while a portion of the impregnation liquid remains in the feedstock. The wood-based feedstock may be introduced into the pressurized reactor together with steam and / or gas. The pressure of the pressurized reactor may be controlled by adding steam. The pressurized reactor may be operated in a continuous manner or as a batch process. The wood-based feedstock, such as the wood-based feedstock that has been subjected to an impregnation treatment, may be introduced into the pressure reactor at a temperature of 25-140° C. The residence time of the wood-based feedstock in the pressure reactor may be 0.5-120 minutes. Unless otherwise specified, the term “residence time” in this specification is to be understood as the time between the introduction or entry of the wood-based feedstock into, for example, the pressure reactor and the exit or discharge of the wood-based feedstock therefrom.
[0081] Due to the semi-hydrolysis of the wood-based feedstock affected by the steam treatment in the reactor, the hemicellulose present in the wood-based feedstock may be hydrolyzed or degraded into, for example, xylose oligomers and / or monomers. Therefore, the steam explosion of the wood-based feedstock can lead to the formation of an output stream. The output stream from the steam explosion can be steam separated. The output stream from the steam explosion can be mixed or merged with a liquid. The output stream of the steam explosion can be mixed with a liquid to form a liquid portion and a portion containing solid cellulose particles. The liquid can be pure water or water containing C5 sugars. The water containing C5 sugars can be circulating water from the operation of separating and / or washing the portion containing solid cellulose particles before enzymatic hydrolysis. The output stream can be mixed with a liquid, and the resulting material can be mechanically homogenized to break up the agglomerates.
[0082] The liquid portion may contain sugars from the hydrolyzed hemicellulose as well as soluble lignin and other byproducts. In one embodiment, the liquid portion contains carbohydrates, such as C5 sugars (C5H 10 O5 or (C5(H2O) n The liquid portion may contain carbohydrates, such as monosaccharides (C6H 12 O6 or C5H 10 O5), disaccharide (C 12 H 22 O 11 ), oligosaccharides and / or polysaccharides ((C6H 10 O5)n or (C5H8O4) n In one embodiment, the liquid portion comprises soluble C5 carbohydrates (C5H 10 O5 or C5(H2O) n ) and other carbohydrates. The liquid portion may also contain other components.
[0083] In addition to cellulose, the portion comprising solid cellulose particles may also comprise lignin. In one embodiment, the portion comprising solid cellulose particles comprises carbohydrates, such as solid C6 carbohydrates (C6H 12 O6 or C6(H2O) n ), and lignin. The portion comprising solid cellulose particles may also comprise other carbohydrates and other components.
[0084] The method may comprise separating and recovering the liquid portion and the portion containing solid cellulose particles formed in i) prior to ii). The separated or recovered portion containing solid cellulose particles may be washed prior to the enzymatic hydrolysis in ii). The portion containing solid cellulose particles may be diluted with water and / or other liquids containing at least soluble carbohydrates.
[0085] The step ii) of subjecting the portion containing solid cellulose particles to enzymatic hydrolysis can be carried out at a temperature of 30-70°C, or 35-65°C, or 40-60°C, or 45-55°C, or 48-53°C. The step ii) of subjecting the portion containing solid cellulose particles to enzymatic hydrolysis can be carried out at atmospheric pressure. The pH of the portion containing solid cellulose particles can be maintained at a pH value of 3.5-6.5, or 4.0-6.0, or 4.5-5.5 during ii). The pH of the portion containing solid cellulose particles can be adjusted by adding alkali and / or acid. The step ii) of subjecting the portion containing solid cellulose particles to enzymatic hydrolysis can last for 20-120 hours, or 30-90 hours, or 40-80 hours. The enzymatic hydrolysis of the portion containing solid cellulose particles can be carried out in a continuous manner, or as a batch process, or as a combination of continuous and batch processes.
[0086] In one embodiment, the enzymatic hydrolysis is carried out at a temperature of 30-70°C, or 35-65°C, or 40-60°C, or 45-55°C, or 48-53°C, while the pH of the fraction comprising solid cellulose particles is maintained at a pH value of 3.5-6.5, or 4.0-6.0, or 4.5-5.5, wherein the enzymatic hydrolysis is allowed to continue for 20-120 hours, or 30-90 hours, or 40-80 hours.
[0087] The enzymatic hydrolysis can be carried out in at least one process step.
[0088] In one embodiment, enzymatic hydrolysis can be carried out as a one-step hydrolysis process, and the part that wherein comprises solid cellulose particles carries out enzymatic hydrolysis in at least one first hydrolysis reactor.After hydrolysis, hydrolysate, i.e. hydrolyzate, can be separated, and the solid lignin part that wherein can also comprise unhydrolyzed cellulose except lignin is separated with the liquid carbohydrate part.One-step hydrolysis process can be carried out as a batch process, comprises for example several reactors working in parallel, and wherein each reactor can receive a part in the part that comprises solid cellulose particles.In addition, the independent parallel circuit with parallel reactors can be used.
[0089] In one embodiment, enzymatic hydrolysis can be carried out as a two-step hydrolysis process or as a multi-step hydrolysis process. In a two-step hydrolysis process or in a multi-step hydrolysis process, the part comprising solid cellulose particles can first be subjected to a first enzymatic hydrolysis in at least one first hydrolysis reactor. The liquid carbohydrate part formed can then be separated from the solid lignin part that may also comprise unhydrolyzed cellulose. The solid part can then be subjected to a second or any subsequent enzymatic hydrolysis, for example, in at least one second hydrolysis reactor. At least one of the first enzymatic hydrolysis and the second or any subsequent enzymatic hydrolysis can be carried out as a batch process or as a continuous process, including, for example, one or more reactors working in parallel. After the second or any subsequent enzymatic hydrolysis, the hydrolyzate, i.e., the hydrolyzate, can be separated, wherein the solid lignin part is separated from the liquid carbohydrate part.
[0090] The reaction time in the first hydrolysis reactor may be from 8 to 72 hours.The reaction time in the second and / or any subsequent hydrolysis reactors may be from 8 to 72 hours.
[0091] Enzyme is a catalyst for enzymatic hydrolysis. Enzymatic reaction reduces pH value and can also reduce viscosity by shortening the length of cellulose fibers. Subjecting the part comprising solid cellulose particles to enzymatic hydrolysis can cause cellulose to be converted into glucose monomers by enzyme. The lignin present in the part comprising solid cellulose particles can be substantially kept in solid form.
[0092] At least one enzyme can be used to perform enzymatic hydrolysis. At least one enzyme can be selected from the group consisting of cellulases, hemicellulases, laccases, and lignin decomposing peroxidases. Cellulases are multiprotein complexes consisting of synergistic enzymes with different specific activities and can be divided into exo- and endo-cellulases (glucanases) and beta-glucosidases (cellobiose). The enzyme can be a commercially available cellulase mixture or made on site.
[0093] Cellulose is an insoluble linear polymer of repeating glucose units linked by β-1-4-glycosidic bonds. During enzymatic hydrolysis, the cellulose chains break apart by cleavage of at least one β-1-4-glycosidic bond.
[0094] Enzymatic hydrolysis can result in the formation of a lignin portion and a carbohydrate portion. In one embodiment, the carbohydrate portion comprises C6 sugars (C6H 12 O6 or (C6(H2O) n In one embodiment, the carbohydrate moiety comprises a monosaccharide (C6H 12 O6 or C5H 10 O5), disaccharide (C 12 H 22 O 11 ), oligosaccharides, and / or polysaccharides ((C6H 10 O5) n or (C5H8O4) n In one embodiment, the carbohydrate moiety comprises galactose, glucose, mannose, arabinose, xylose, glucuronic acid and / or galacturonic acid.
[0095] The inventors have surprisingly discovered that a specific size range of wood chips in a wood-based feedstock has the added benefit of influencing the amount of carbohydrate fraction received from enzymatic hydrolysis.
[0096] In one embodiment, the lignin fraction is in solid form. In one embodiment, the carbohydrate fraction is in liquid form. The lignin fraction and the carbohydrate fraction formed in ii) may be separated and recovered prior to iii).
[0097] During the separation carried out before ii) and / or before iii), the solid part can be separated from the liquid part. The separation carried out before ii) and / or before iii) can be carried out by filtration and / or by centrifugation. The filtration can be vacuum filtration, filtration based on the use of negative pressure, filtration based on the use of excess pressure or filter press.
[0098] The carbohydrate fraction recovered from the enzymatic hydrolysis may be purified prior to step iii). The purification of the carbohydrate fraction may be performed using at least one of: membrane filtration, crystallization, sterilization, pasteurization, evaporation, chromatography, ion exchange, passing through activated carbon. The purification of the carbohydrate fraction has the additional utility of providing the desired target sugar quality. The carbohydrate fraction may be subjected to iii) catalytic conversion.
[0099] The catalytic conversion of the carbohydrate moiety iii) may include subjecting the carbohydrate moiety to catalytic hydrogenolysis. That is, in step iii), the carbohydrate moiety may be subjected to a catalyst in the presence of hydrogen. The catalytic conversion may be carried out in the presence of water. In one embodiment, the catalytic conversion of the carbohydrate moiety includes subjecting the carbohydrate moiety to catalytic hydrogenation in the presence of a solvent, preferably water and a catalyst system.
[0100] Catalytic conversion can be carried out in the presence of a catalyst system comprising one or more catalysts. In one embodiment, the catalyst system comprises or consists of a first catalyst. In one embodiment, the catalyst system comprises or consists of at least one first catalyst and at least one second catalyst. In one embodiment, the catalyst system comprises or consists of a first catalyst and a second catalyst. The first catalyst can be a heterogeneous solid catalyst. The second catalyst can be a homogeneous catalyst. In one embodiment, the first and second catalysts can be heterogeneous catalysts, such as catalysts supported on a carrier.
[0101] The first catalyst may include an active metal component selected from the 8th, 9th or 10th families of the IUPAC periodic table, such as iron, cobalt, nickel, ruthenium, rhodium, palladium, iridium and platinum, or a mixture thereof. In one embodiment, the first catalyst includes a heterogeneous nickel alloy such as Raney Nickel or is composed thereof. The active metal component of the first catalyst may be supported by a carrier, and the carrier includes activated carbon, aluminum oxide, silicon dioxide, silicon carbide, zirconium oxide, zinc oxide, titanium dioxide or a mixture thereof. The active metal component of the first catalyst may account for 0.05-70 weight % of the total weight of the catalyst.
[0102] The second catalyst may include at least one active component selected from tungsten oxide, tungsten sulfide, tungsten hydroxide, tungsten oxide bronze, tungstic acid, tungstate, metatungstic acid, metatungstate, paratungstic acid, paratungstate, peroxytungstic acid, peroxytungstate, tungsten-containing heteropolyacid. In one embodiment, the second catalyst includes or consists of homogeneous sodium tungstate.
[0103] The first catalyst may be active in hydrogenation. The second catalyst may be active in cracking.
[0104] In one embodiment, the second catalyst is a homogeneous catalyst, and the second catalyst may be recovered and recycled for reuse in iii).
[0105] The catalytic conversion step iii) of the carbohydrate part can be carried out at a temperature of 120-300°C, or 180-270°C, or 230-270°C. The room temperature initial pressure in iii) can be 1-15MPa or 9-12MPa. The catalytic conversion can be carried out in a continuous manner. The time for the catalytic conversion of the carbohydrate part can be 5 minutes to 3 hours, or 30 minutes to 2.5 hours.
[0106] The catalytic conversion can be carried out in a conversion reactor, for example in a fixed bed or slurry reactor. The catalytic conversion of the carbohydrate portion can occur as a slurry reaction. The hydrogen and carbohydrate portion can be added to the reactor separately or simultaneously using respective pumps and compressors. A second catalyst in liquid form can be added to the reactor separately from the carbohydrate portion or simultaneously. The first catalyst can be provided to the reactor separately from the carbohydrate portion, preferably the first catalyst is provided to the reactor before the carbohydrate portion is fed into the reactor. Liquid and gaseous reaction products comprising diols can be removed from the reactor. The reaction products can be cooled and depressurized. After depressurization, the gaseous product can be subjected to gas / liquid separation to separate the product comprising diols in liquid form.
[0107] Therefore, subjecting the carbohydrate portion to catalytic conversion iii) can produce a liquid composition of diols. The catalytic conversion at least completes hydrogenolysis and hydrocracking reactions to achieve hydrogenolysis and hydrocracking of the carbohydrate portion, thereby forming a liquid composition of diols. The liquid composition of diols may include or consist of the following: monoethylene glycol (MEG, also known as 1,2-ethylene glycol), monopropylene glycol (MPG, also known as 1,2-propylene glycol) and 1,2-butanediol (BDO, also known as butanediol). Based on the total weight of the liquid composition of diols, these diols may be present in a concentration of 0.1-40% by weight. The liquid composition of diols may also include other by-products. The ethylene glycol reaction yield may be at least 60%.
[0108] The recovery of monoethylene glycol from the diol liquid composition in step iv) can be carried out by a separation technique selected from the group consisting of adsorption, evaporation, distillation, extractive distillation, azeotropic distillation, vacuum distillation, atmospheric distillation, membrane separation, filtration, reaction purification or a combination thereof.
[0109] In one embodiment, monoethylene glycol is recovered by distillation. The distillation may be carried out in at least one distillation column. The distillation may be carried out at a temperature of 50-250° C. or 100-200° C. The distillation may be carried out at a pressure of at least 0.1 kPa, or at least 10 kPa, or at least 50 kPa. The pressure may be at most 400 kPa, or at most 200 kPa, or at most 120 kPa. It will be clear to those skilled in the art to vary the temperature and pressure relative to each other to obtain suitable conditions.
[0110] The MEG recovered in iv) can be subjected to an esterification reaction with terephthalic acid to form polyethylene terephthalate (PET). The esterification reaction can be carried out at a pressure of 0.27-0.55 MPa and a temperature of 220-260° C. The water formed during the reaction can be removed by distillation.
[0111] PET can be used to form a resin. The resin can be further processed into a container using, for example, injection molding or stretch blow molding.
[0112] The method disclosed in this specification has the additional utility of utilizing wood chips of a specific size range. Wood chips of a specific size have additional utility in favorably affecting the impregnation process. The specific size of the wood chips has the additional utility of making the impregnation process effective, such as the impregnation liquid is evenly distributed on the wood chips and absorbed therein, so less impregnation liquid may be required. Using wood chips of a specific chip size has the additional utility of making the method easier to control. By limiting the amount of super thick wood chips in the method, the formation of unhydrolyzed fiber bundles (shives) and sticks (sticks) in pretreatment i) can be reduced or minimized, and the yield of the part containing solid cellulose particles from pretreatment i) can be increased. This may then affect the yield of the carbohydrate part received from enzymatic hydrolysis ii), and further affect the yield of the glycol received from catalytic conversion iii). Then, the impregnation process as described in this specification has the additional utility of beneficially affecting steam explosion, so that a part containing solid cellulose particles with a larger surface area can be obtained. Therefore, the entire process of producing monoethylene glycol can be improved.
[0113] Example
[0114] Reference will now be made in detail to embodiments of the present disclosure, examples of which are illustrated in the accompanying drawings.
[0115] The following description discloses some embodiments in such detail that those skilled in the art can utilize the apparatus and its use and method based on the present disclosure. Not all steps of the embodiments are discussed in detail, because many steps will be obvious to those skilled in the art based on the present disclosure.
[0116] For simplicity, in the case of repeated components, the item numbering will be maintained in the following exemplary embodiments.
[0117] Attached Figure 1 and Figure 2 An example of a flow diagram of a process for producing monoethylene glycol and the corresponding apparatus 1 are illustrated in more detail. The figures are not drawn to scale and many components have been omitted for the sake of clarity. Figure 2 The apparatus 1 for producing monoethylene glycol (MEG) from wood-based raw materials comprises at least one pretreatment unit 2 configured to perform at least one pretreatment on a wood-based feedstock originating from the wood-based raw material to form a liquid portion and a portion comprising solid cellulose particles.
[0118] Figure 2The device further comprises a mechanical unit 6 configured to mechanically treat the wood-based raw material. The mechanical treatment may be selected from peeling, slicing, splitting, cutting, pulping, grinding, crushing, splitting, screening and / or washing the wood-based raw material to form a wood-based feedstock. The wood-based feedstock comprises wood chips, wherein at most 5% by weight of the wood chips in the wood-based feedstock are extra-thick wood chips as specified in SCAN-CM40:01.
[0119] One of the at least one pre-treatment unit 2 is a pressurized reactor 2c configured to subject a wood-based feedstock derived from a wood-based raw material to steam explosion.
[0120] Figure 2 The apparatus disclosed in the invention further comprises an impregnation reactor 2b operably arranged before the pressurized reactor 2c. The impregnation unit 2b is configured to subject the wood-based feedstock to at least one impregnation treatment with an impregnation liquid. The impregnation liquid may be selected from water, at least one acid, at least one base, at least one alcohol, or any combination or mixture thereof.
[0121] Figure 2 The apparatus disclosed in further comprises a pre-steaming reactor 2a operatively arranged before the impregnation reactor 2b and the pressurization reactor 2c. The pre-steaming unit is configured to pre-steam the wood-based feedstock.
[0122] At least one pretreatment unit may include at least one of a pre-steaming reactor 2a, an impregnation reactor 2b, and a pressurized reactor 2c. Alternatively, the at least one pretreatment unit may include two of these or all three of them, the two or all three being arranged one after the other.
[0123] After the pretreatment unit is arranged at least one hydrolysis reactor 3. The at least one hydrolysis reactor 3 is configured to subject the fraction comprising solid cellulose particles to enzymatic hydrolysis to form a lignin fraction and a carbohydrate fraction.
[0124] Figure 2 The apparatus disclosed in also comprises a conversion reactor 4 configured to subject the carbohydrate portion to a catalytic conversion to form a liquid composition of diols.
[0125] Figure 2 The apparatus further comprises a distillation unit 5 configured to recover monoethylene glycol from the liquid diol composition.
[0126] Example 1 - Effect of Chip Size in Wood-Based Feedstock
[0127] In this example, the effect of the specific size of the wood chips in the wood-based feedstock was tested. The wood-based feedstock was pre-steamed as described in this specification and then subjected to an impregnation treatment. The impregnation treatment was performed by using H2SO4 with an acid concentration of 13 g / l as the impregnation liquid. The temperature of the impregnation liquid was 90°C. The residence time was 1 minute. The results are shown in Table 1 below.
[0128] Table 1.
[0129]
[0130]
[0131] *The sulfuric acid content is calculated based on the amount of sulfur
[0132] As can be seen from Table 1 above, the sulfur content measured as ICP mg / kg (Inductively Coupled Plasma Optical Emission Spectrometry according to SFS-EN ISO 11885) increases as a result of the impregnation treatment, indicating that the impregnation liquid has been well impregnated.
[0133] It is obvious to a person skilled in the art that, as technology develops, the basic idea can be implemented in various ways. Therefore, the implementations are not limited to the examples described above; instead, they may vary within the scope of the claims.
[0134] The embodiments described above can be used in any combination with each other. Several embodiments can be combined to form another embodiment. The method, device, or monoethylene glycol disclosed herein may include at least one embodiment described above. It should be understood that the above benefits and advantages may relate to one embodiment, or may relate to multiple embodiments. The embodiments are not limited to those embodiments that solve any or all of the problems described or those embodiments that have any or all of the benefits and advantages. It will be further understood that the expression of "one / kind" item refers to one / kind or more / kind of the items. The term "include / comprise" is used in this specification to indicate the inclusion / inclusion of the following features or actions, without excluding the presence of one or more other features or actions.
Claims
1. A method for producing monoethylene glycol from a wood-based feedstock, wherein the method comprises: i) providing a wood based feedstock derived from a wood based raw material and comprising wood chips, wherein at most 5 wt% of the wood chips in the wood based feedstock are extra thick wood chips as defined in SCAN-CM 40:01, and wherein at most 10 wt% of the wood chips in the wood based feedstock are fines as defined in SCAN-CM 40:01, and subjecting the wood feedstock to at least one pretreatment to form a liquid fraction and a fraction comprising solid cellulose particles, wherein extra thick chips are chips which pass through the first screen of a chip grader but are retained on the second screen comprising 8 mm slots when the chips are size graded as specified in SCAN-CM 40:01, and wherein fines are chips which are not retained even on the fifth screen comprising 3 mm holes when the chips are size graded as specified in SCAN-CM 40:01, and wherein the pretreatment comprises subjecting the wood-based feedstock to at least one impregnation treatment with an impregnation liquid selected from a combination of water and at least one acid, wherein the impregnation treatment is carried out in at least one impregnation reactor, wherein the residence time of the wood-based feedstock in the impregnation reactor is 5 seconds to 5 minutes, and the temperature of the impregnation liquid is 20-99°C; ii) subjecting the fraction comprising solid cellulose particles to enzymatic hydrolysis to form a lignin fraction and a carbohydrate fraction; iii) subjecting the carbohydrate portion to a catalytic conversion to form a liquid composition of diols; and iv) recovering monoethylene glycol from the liquid composition of glycols.
2. The method of claim 1, wherein: Up to 3.5 wt. % of the wood chips in the wood-based feedstock are extra thick wood chips as defined in SCAN-CM 40:
01.
3. The method of claim 1, wherein: Up to 3 wt% of the wood chips in the wood-based feedstock are extra thick wood chips as defined in SCAN-CM 40:
01.
4. The method of claim 1, wherein: Up to 2.5 wt. % of the wood chips in the wood-based feedstock are extra thick wood chips as defined in SCAN-CM 40:
01.
5. The method of claim 1, wherein: Up to 2 wt. % of the wood chips in the wood-based feedstock are extra thick wood chips as defined in SCAN-CM 40:
01.
6. The method according to any one of claims 1 to 5, wherein: Up to 6 wt% of the wood chips in the wood-based feedstock are fines as defined in SCAN-CM 40:
01.
7. The method according to any one of claims 1 to 5, wherein: Up to 3 wt% of the wood chips in the wood-based feedstock are fines as defined in SCAN-CM 40:
01.
8. The method according to any one of claims 1 to 5, wherein: Up to 1.5 wt% of the wood chips in the wood-based feedstock are fines as defined in SCAN-CM 40:
01.
9. The method according to any one of claims 1 to 5, wherein: Up to 0.5 wt. % of the wood chips in the wood-based feedstock are fines as defined in SCAN-CM 40:
01.
10. The method according to any one of claims 1 to 5, wherein: The specific surface area of wood chips is 2 – 35 cm 2 / g.
11. The method according to any one of claims 1 to 5, wherein: The specific surface area of wood chips is 4 – 33 cm 2 / g.
12. The method according to any one of claims 1 to 5, wherein: The specific surface area of wood chips is 6 – 30 cm 2 / g.
13. The method according to any one of claims 1 to 5, wherein: The specific surface area of wood chips is 10 – 25 cm 2 / g.
14. The method according to any one of claims 1 to 5, wherein: The specific surface area of wood chips is 12 – 20 cm 2 / g.
15. The method according to any one of claims 1 to 5, wherein: The geometric surface area of wood chips is 4 – 40 cm 2 / g.
16. The method according to any one of claims 1 to 5, wherein: The geometric surface area of wood chips is 5 – 35 cm 2 / g.
17. The method according to any one of claims 1 to 5, wherein: The geometric surface area of wood chips is 6 – 30 cm 2 / g.
18. The method according to any one of claims 1 to 5, wherein: The geometric surface area of wood chips is 10 – 25 cm 2 / g.
19. The method of any one of claims 1 to 5, wherein: The geometric surface area of wood chips is 12 – 20 cm 2 / g.
20. The method of any one of claims 1 to 5, wherein: The wood-based raw material is hardwood.
21. The method of claim 20, wherein: The hardwood is selected from the group consisting of beech, birch, ash, oak, maple, chestnut, willow, poplar and any combination thereof.
22. The method of any one of claims 1 to 5, wherein: Providing the wood-based feedstock includes subjecting the wood-based feedstock to a mechanical treatment selected from the group consisting of debarking, slicing, splitting, cutting, beating, grinding, crushing, splitting, screening and / or washing the wood-based feedstock to form the wood-based feedstock.
23. The method of any one of claims 1 to 5, wherein: The pretreatment in i) comprises subjecting the wood-based feedstock to steam explosion, which is performed by treating the wood-based feedstock with steam at a temperature of 130-240° C. at a pressure of 0.17-3.25 MPaG and then suddenly and explosively decompressing the wood-based feedstock.
24. The method of claim 23, wherein: The pretreatment in i) comprises pre-steaming the wood-based feedstock prior to the impregnation treatment and / or steam explosion, wherein the pre-steaming of the wood-based feedstock is carried out with steam at a temperature of 100-130° C. under atmospheric pressure.
25. The method of any one of claims 1 to 5, wherein: The enzymatic hydrolysis is carried out at a temperature of 30-70°C while the pH of the fraction comprising the solid cellulose particles is maintained at a pH value of 3.5-6.5, wherein the enzymatic hydrolysis is continued for 20-120 hours.
26. The method of claim 25, wherein: The enzymatic hydrolysis is carried out at a temperature of 35-65°C.
27. The method of claim 25, wherein: The enzymatic hydrolysis is carried out at a temperature of 40-60°C.
28. The method of claim 25, wherein: The enzymatic hydrolysis was carried out at a temperature of 45-55°C.
29. The method of claim 25, wherein: The enzymatic hydrolysis was carried out at a temperature of 48-53°C.
30. The method of claim 25, wherein: The pH of the fraction comprising solid cellulose particles is maintained at a pH value of 4.0-6.
0.
31. The method of claim 25, wherein: The pH of the fraction comprising solid cellulose particles is maintained at a pH value of 4.5-5.
5.
32. The method of claim 25, wherein: The enzymatic hydrolysis lasts for 30-90 hours.
33. The method of claim 25, wherein: The enzymatic hydrolysis lasts for 40-80 hours.
34. The method of any one of claims 1 to 5, wherein: The catalytic conversion of the carbohydrate moiety comprises subjecting the carbohydrate moiety to catalytic hydrogenation in the presence of water and a catalyst system.
35. The method of any one of claims 1 to 5, wherein: The recovery of monoethylene glycol from the liquid diol composition is carried out by distilling the liquid diol composition.