A method for supplying oxygen-enriched gas to an oxygen-consuming process

By supplying CO2 feed gas to the anode side of the solid oxide electrolytic cell, an oxygen-rich stream with low nitrogen content is generated, which solves the problems of nitrogen oxide formation and high energy consumption in oxygen combustion and oxygen calcining furnaces, improves flame temperature and CO2 capture efficiency reduces costs.

CN115087762BActive Publication Date: 2024-10-01HALDOR TOPSOE AS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202180012763.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-02-06
Filing Date
2021-02-05
Publication Date
2024-10-01
Estimated Expiration
2041-02-05

AI Technical Summary

Technical Problem

Existing oxy-combustion and oxy-calciner equipment rely on expensive low-temperature air separation units (ASU) to provide oxygen-rich streams, resulting in high energy consumption and high costs. At the same time, the high nitrogen content in the flue gas affects the efficiency of CO2 capture and storage.

Method used

By supplying a feed gas containing CO2 to the anode side of a solid oxide electrolyzer (SOEC), electrochemical reduction generates an oxygen-rich gas, replacing traditional air separation methods to provide a low nitrogen content oxygen-rich stream for oxy-combustion or Oxygen calcination process.

Benefits of technology

Reduces the formation of nitrogen oxides during oxy-combustion and oxy-calcination, reduces nitrogen content in the flue gas, increases flame temperature, reduces energy consumption, avoids reliance on expensive ASUs, and improves CO2 capture and storage efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115087762B_ABST
    Figure CN115087762B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for supplying an oxygen-rich gas to an oxygen-consuming process, wherein an oxygen-rich gas with a low nitrogen content is produced by supplying an anode-side feed gas containing CO2 to the anode side of a solid oxide electrolysis cell, and oxygen is produced on the anode side of the solid oxide electrolysis cell. In this way, an anode-side product gas is formed, at least a portion of which contains an oxygen-rich gas. The oxygen-rich gas has a low nitrogen content, and the temperature of the oxygen-rich gas leaving the solid oxide electrolysis cell is 600° C. to 1000° C. The method has a number of advantages, the first of which is energy saving.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to a method for supplying an oxygen-enriched gas to an oxygen-consuming process, wherein an oxygen-enriched gas having a low nitrogen content is produced by supplying an anode-side feed gas comprising CO2 to the anode side of an operating solid oxide electrolysis cell (SOEC). The present invention also relates to a solid oxide electrolysis cell supplied with a feed gas comprising CO2, wherein the anode side of the electrolysis cell is fluidly connected to the oxygen-consuming process.

[0002] Oxyfuel combustion is the process of burning hydrocarbon fuels in a nitrogen-poor environment, usually in a stream of nearly pure oxygen or a mixture of oxygen and carbon dioxide. The main purpose of using oxyfuel combustion in, for example, a coal-fired power plant is to produce flue gas with very high concentrations of CO2 and water vapor, so that CO2 can be separated or captured from the flue gas while avoiding the expensive separation of CO2 from gaseous nitrogen. It is important to note that even when oxycombustion is used, the flue gas still contains impurities such as residual nitrogen, unburned oxygen, SO2, nitrogen oxides and particulate material. Most of these still have to be removed in order to produce sufficiently pure carbon dioxide for carbon capture and storage or for other downstream uses.

[0003] Oxyfuel combustion for CO2 capture consists of four major components: 1) an air separation unit (ASU), which provides an oxygen-rich oxidant stream for combustion; 2) a boiler or gas turbine, where the fuel is burned and heat is produced; 3) a flue gas treatment unit, where undesirable substances such as ash, most sulfur and nitrogen oxides are removed from the flue gas; and 4) a CO2 processing unit (CPU), where final purification of the CO2 for transport, storage and / or utilization occurs.

[0004] When hydrocarbon fuels are burned in pure oxygen, the flame temperature is much higher than when they are burned in air. Peak temperatures can reach 2500°C, compared to 1700°C in conventional supercritical boilers. In a typical gas turbine cycle, combustion temperatures are limited to about 1300-1400°C; in oxygen-fuel coal-fired boilers using current technology, combustion temperatures are limited to about 1900°C. To alleviate material corrosion problems, which can eventually lead to boiler failure, some of the CO2-rich flue gas leaving the boiler is typically mixed with an oxygen-rich stream supplied to the burner. This dilutes the oxygen and reduces the flame temperature to levels similar to those found in conventional air-blown equipment.

[0005] For the combustion of pulverized coal, pilot-scale tests by Croiset and Thambimuthu have reported that when the feed gas used in oxy-fuel combustion has a composition of approximately 35 vol% O2 and 65 vol% dry recycled CO2, the flame temperature and heat capacity of the gas match the combustion of the fuel in air (see, 21 vol% O2 in the air, the remainder N2).

[0006] Another important aspect in oxyfuel combustion power plants is the understanding of nitrogen oxides (NO x ) pathways, as these nitrogen oxides contribute to the undesirable formation of HNO3 during flue gas compression in CO2 processing units. x Three main pathways for the formation of NO are known: 1) thermal NO x 2) Rapid NO x formation; and 3) conversion of fuel nitrogen to NO x In oxyfuel combustion, since there is no N2 from the air, the N2 concentration is very low and thermal NO can usually be ignored. x and fast NO x Therefore, NO from fuel nitrogen x The formation is the most important pathway in boilers using oxyfuel combustion. Approximately 95% of the total NO x It is composed of nitric oxide (NO), the rest is composed of nitrogen dioxide (NO2) and small amounts of nitrous oxide (N2O) and other nitrogen oxides.

[0007] Oxygen-enriched streams are also beneficial in oxy-calciners or oxygen calciners. In fact, oxy-calciners have gained wider attention due to their potential use in, for example, direct air capture devices involving calcium cycles. For example, David W. Keith et al. describe a process for capturing CO2 from the atmosphere (Joule 2, 1573-1594 (2018)). More specifically, a device for capturing 1 megaton of CO2 per year directly from the air from the atmosphere is described. The process chemistry of the device is based on two loops: an alkali loop (CO2+KOH to K2CO3 to KOH) and a calcium loop (CaCO3 to CaO+CO2 to Ca(OH)2 to CaCO3). CO2 is captured by reacting with KOH to generate K2CO3. The K2CO3 reacts with Ca(OH)2 to regenerate KOH and produce CaCO3, which is then calcined in an oxy-calciner to release CO2 and regenerate Ca species. Importantly, the calcination step needs to be carried out in a nitrogen-depleted atmosphere, as CO2 (released during calcination) and N2 are difficult to separate once mixed. In more detail, the calcium carbonate (CaCO3) formed in the calcium loop is directed to the calciner, where this solid material is regenerated into CaO and CO2, the latter of which is directed out of the reactor for purification and compression. The calciner requires an additional heat source to raise the temperature to around 900°C, which is necessary to meet the heat demand of the endothermic calcination reaction. The most obvious way to generate this heat is to use oxyfuel combustion, which, as mentioned earlier, produces flue gases that contain mainly CO2. Again, oxyfuel combustion requires an ASU. The efficiency of an oxycalciner depends on the oxygen concentration of the oxygen-rich stream used for the calcination process: the higher the oxygen concentration, the higher the efficiency. The advantage of a higher O2 concentration is a lower total gas flow to the furnace, thereby reducing the heat demand of the furnace. A smaller heat demand means a smaller fuel input, which reduces the required oxygen flow rate. A smaller furnace reduces the investment cost of the equipment, which is important, especially in the calcium cycle process, where the calciner is an insulated reactor.

[0008] Prior art oxy-combustion and oxy-calciner plants use an ASU, typically a low temperature ASU, for providing an oxygen-rich gas stream for a boiler or calciner chamber. ASUs are very expensive (in terms of capital expenditure (CAPEX) as well as operating expenses (OPEX)). ASUs consume about 225 kWh of energy per ton of O2 produced and are one of the most expensive units in oxy-fuel combustion plants and oxy-calciner plants. An object of the present invention is to provide an alternative method for supplying an oxygen-rich gas to an oxygen-consuming process, such as the above-mentioned oxy-combustion or oxy-calciner process. More specifically, the present invention proposes to produce an oxygen-rich stream with a low nitrogen content by supplying an anode side feed gas comprising CO2 to the anode side of an operating solid oxide electrolysis cell (SOEC), thereby obtaining an oxygen-rich anode side product gas.

[0009] Solid oxide electrolyzers (SOECs) can be used to reduce HO to H, CO to CO, or a combination of HO and CO to syngas (H and CO). This conversion occurs on the cathode (fuel) side of the solid oxide electrolyzer. On the anode (oxygen) side of the electrolyzer, oxygen is electrochemically generated. In the context of the present invention, the term "electrochemically generated" means that the chemical species is formed by an electrochemical process (i.e., a chemical process involving the transfer of electrons). Such methods include, for example, the oxygen evolution reaction (2O 2- =O2+4e - ), water reduction reaction (H2O+2e - =H2+O2 - ) and carbon dioxide reduction reaction (CO2+2e - =CO+O 2- ). Note that the water-gas shift or reverse water-gas shift reactions do not involve electrochemical steps.

[0010] In the context of the present invention, the terms "stream", "gas" and "gas flow" are used interchangeably.

[0011] In the context of the present invention, the term "at least a portion" of a certain gas stream is to be understood as using a portion of the entire gas stream or stream. The gas stream can be simply divided into parts of the same composition. This does not mean to separate the components of the gas. For example, this can involve if it is desired to recycle a portion of the gas stream to the solid oxide electrolysis cell. The portion fed to the oxygen / H2 / CO consumption process can be, for example, 5% to an upper limit of 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, 90% or 100% of an oxygen-rich gas or a gas rich in H2 and / or CO.

[0012] The cathode side feed gas stream may also be referred to as fuel feed and the anode side feed gas stream may also be referred to as flush feed.

[0013] Unless otherwise stated, any given percentage of gas phase is volume %.

[0014] When a cathode side feed gas comprising H2O is fed to the cathode side of an operating SOEC, at least a portion of the H2O is electrochemically reduced to H2 (i.e., electrochemically generating H2), thereby forming a cathode side product gas rich in hydrogen. In the context of the present invention, the term "enriched in X" is understood as "the concentration of X in the stream is increased compared to the concentration of X in the corresponding feed gas". In other words, the cathode side gas stream rich in hydrogen (leaving the electrolyzer) has a higher hydrogen concentration than the cathode side feed gas (entering the solid oxide electrolyzer). Similarly, if a cathode side feed gas comprising CO2 is supplied to the cathode side of an operating SOEC, at least a portion of CO2 is electrochemically reduced to CO (i.e., electrochemically generating CO), thereby forming a cathode side product gas rich in CO. In addition, if a cathode side feed gas comprising a mixture of H2O and CO2 is supplied to the cathode side of an operating SOEC, at least a portion of H2O or CO2 or both is electrochemically reduced, thereby forming a cathode side product gas rich in hydrogen and CO. Similarly, the O2-rich anode side gas stream (leaving the electrolysis cell) has a higher O2 concentration than the anode side feed gas stream (entering the solid oxide electrolysis cell). Note that according to this definition, if the anode side feed gas stream has an oxygen content of less than 10%, then the anode side product gas stream with 10% O2, 90% CO2 can be considered to be O2-rich. Similarly, according to this definition, the anode side product gas stream with 10% O2, 90% CO2 is considered to be O2-rich, even though the oxygen content of this gas is lower than that of the atmosphere.

[0015] Typical operating temperatures for SOECs are between about 600°C and 1000°C: high temperatures are required in order to achieve sufficient oxide ion conductivity in the ceramic membrane used as the electrolyte. Commonly used electrolyte materials include stabilized zirconia, such as yttria-stabilized zirconia (YSZ), doped ceria, doped lanthanum gallate, etc. Commonly used oxygen electrode materials include perovskite materials, such as Sr-doped LaMnO3 (LSM); Sr-doped LaFeO3 (LSF); Sr-doped LaCoO3 (LSC); Sr-doped La(Co,Fe)O3 (LSCF); Sr-doped SmCoO3, etc. The perovskite material is further mixed with doped ceria to form a composite oxygen electrode (SOEC anode). Dopants other than Sr, such as Ca and Ba, are known materials, and in addition to perovskites, Ruddlesden-Popper phases are also known.

[0016] Applicant's WO 2013 / 131778 A2 and US 10,494,728 B2 both describe the production of high purity CO by electrolysis of CO 2 in a solid oxide electrolysis cell or SOEC stack.

[0017] Typically, air (N2 / O2) is used as flushing gas on the anode side of the SOEC. The concentration of O2 in the gas stream leaving the anode side of the solid oxide electrolysis cell depends on the flow rate of the anode side feed gas and the operating current of the SOEC. In principle, if no feed gas is used, or if pure oxygen is used as feed, close to 100% oxygen can be produced on the anode side. However, due to the high risk of degradation of various stack components at high oxygen partial pressures and high temperatures, this is not usually done. However, the advantages obtained here are more important than the disadvantages.

[0018] In the method of the present invention, a stream containing CO2 with a low nitrogen content is used as a feed gas (sometimes also referred to as a flushing gas) on the anode side of the SOEC instead of air. The resulting product gas is rich in oxygen and is suitable for use as an oxidant in many oxygen-consuming processes. In the context of the present invention, the term "oxygen-consuming process" refers to a process in which oxygen reacts with other chemical substances to oxidize the latter substances. Examples of oxygen-consuming processes include oxygen combustion, oxygen calcination, and gasification.

[0019] More specifically, the present invention relates to a method for supplying an oxygen-rich gas to an oxygen-consuming process, wherein at least one operating solid oxide electrolysis cell having a cathode side and an anode side is provided, and

[0020] a) supplying a cathode side feed gas stream comprising steam or CO2 or a mixture thereof to the cathode side of at least one solid oxide electrolysis cell,

[0021] b) electrochemically reducing at least a portion of the cathode side feed gas stream in a solid oxide electrolysis cell to form a cathode side product gas stream rich in hydrogen, carbon monoxide or a mixture thereof,

[0022] c) supplying at least a portion of the cathode-side product gas stream to a hydrogen and / or carbon monoxide consumption process,

[0023] d) supplying an anode side feed gas stream comprising CO2 to the anode side of the solid oxide electrolysis cell; and

[0024] e) electrochemically generating oxygen on the anode side of the solid oxide electrolysis cell to form an oxygen-rich anode side product gas stream, wherein

[0025] - feeding an oxygen-rich gas comprising at least a portion of the oxygen-rich anode-side product gas stream to an oxygen-consuming process,

[0026] - the oxygen-rich gas has a low nitrogen content, which is less than 10% by volume, and

[0027] - the oxygen-rich gas leaving the solid oxide electrolysis cell has a temperature of 600° C. to 1000° C.; and

[0028] The oxygen-consuming process is an oxygen combustion process or an oxygen calcination process.

[0029] In the context of the present invention, the term "hydrogen- and / or carbon monoxide-consuming process" refers to a process in which hydrogen or carbon monoxide or both react to form other chemical species. Examples of hydrogen- and / or carbon monoxide-consuming processes include methanol production, ammonia production, hydroprocessing, methanation, hydrogenation, carbonylation, hydroformylation (oxo synthesis) and oxidative carbonylation.

[0030] The anode side feed gas stream comprising CO2 may, for example, comprise 0-100 vol% CO2, such as 20-100, 40-100, 50-100, 60-100, 70-100, 80-100 vol% CO2.

[0031] In this article, oxygen combustion or oxygen combustion process refers to a process using essentially pure oxygen as an oxidant, and importantly, the process is carried out in the presence of a small amount of nitrogen (N). The oxygen combustion refers to the complete combustion of the fuel, thereby producing a non-reducing product gas. There is no residual heating value in the product gas.

[0032] Gasification refers to the substoichiometric combustion of a fuel. The product gas will be reducing and there will be residual heating value in the product gas.

[0033] In this context, oxygen calcination refers to an oxygen combustion process in which solid carbonates are decomposed to the corresponding oxides, such as CaCO3 to CaO, to produce cement.

[0034] The term "combustion" means that a chemical species can be oxidized to produce heat (an exothermic oxidation reaction).

[0035] According to an embodiment of the present invention, the anode side feed gas and / or the cathode side feed gas are heated before being fed to the solid oxide electrolysis cell. In another embodiment of the present invention, the oxygen-rich gas is not heated before being fed to the oxygen-consuming process. Since the outlet temperature of the oxygen-rich gas from the solid oxide electrolysis cell is high, typically above 600°C, or even above 700, 800 or 900°C, heating can be omitted.

[0036] The present invention also relates to a solid oxide electrolysis cell, wherein the anode side of the electrolysis cell is connected to an oxygen-consuming process fluid, and wherein the electrolysis cell is operated according to the above method.

[0037] The method of the present invention has several advantages.

[0038] First, as long as an anode-side feed gas having a low nitrogen content is provided to the anode side of a solid oxide electrolysis cell, the oxygen-rich stream exiting the cell also has a low nitrogen content, making it very suitable for use as an oxidant in an oxy-combustion or oxy-calciner.

[0039] According to an embodiment of the present invention, the nitrogen content in the oxygen-rich stream is less than 10 vol%, such as less than 5 vol%, 3 vol%, 2 vol%, 1 vol% or 0.1 vol%. The less nitrogen, the better.

[0040] If, instead of air, a gas stream rich in oxygen and at the same time low in nitrogen is used as the oxidant, the hot NO x Formation and rapid NO x The formation pathways are minimized. Secondly, the flue gas leaving the oxygen-consuming process has a lower nitrogen (N2) content. The technically challenging task of separating CO2 from N2, for example for carbon capture, storage or utilization purposes, will thereby be made easier. Note that even if the oxygen-enriched stream is nitrogen-free, if the fuel used in the oxycombustion or oxycalcination process contains nitrogen, the flue gas may still contain some N2 or NO x. Third, due to the low nitrogen content in the oxygen-rich stream compared to the nitrogen content in the air, the energy requirement (i.e., fuel consumption) for heating the stream to the inlet temperature of the oxygen-consuming process is significantly reduced because the nitrogen component of the air is not heated. Fourth, the use of an oxygen-rich stream with a low nitrogen content allows higher flame temperatures to be achieved in oxygen combustion and oxygen calcining kilns. Fifth, by using a SOEC to supply the oxygen-rich gas, a low-temperature ASU or other ASU is no longer required for air separation. As mentioned above, ASUs are expensive, both in terms of capital costs and in terms of operating expenses. Sixth, since the operating temperature of the SOEC is approximately between 600°C and 1000°C, the oxygen-rich stream leaving the anode side of the solid oxide electrolysis cell does not require (or only requires very little) preheating before entering the oxygen combustion or oxygen calcining kiln, making the process more efficient. It should be noted that the oxygen produced using low-temperature air separation will require very significant preheating. Seventh, although the anode side feed gas containing CO2 in the anode side feed of the solid oxide electrolysis cell needs to be preheated, the heating requirements are lower than those of the prior art solutions without SOEC. This is because the oxygen generated electrochemically and forming part of the oxygen-rich stream can be at least partially heated using the Joule heat generated by the SOEC. Eighth, the oxygen generated electrochemically and generally considered to be a low-value by-product of the electrolysis process can be utilized instead of being discharged, thereby improving the efficiency and profitability of the electrolysis process. Therefore, it is particularly advantageous if two product gases from the SOEC are utilized, that is, the oxygen-rich anode side product gas for the oxygen-consuming process, and the cathode side product gas rich in H2 and / or CO is used in the hydrogen and / or carbon monoxide use process. Ninth, the method provides a simple way to control the oxygen content in the oxygen-rich stream entering the oxygen-consuming process. This is because the O2 concentration in the gas stream can be easily and quickly changed by changing the flow rate of the anode side feed gas or the operating current of the SOEC. Tenth, if a portion of the hydrogen and / or carbon monoxide rich stream exiting the cathode side of the SOEC is used as fuel for an oxyfuel combustion or oxycalcination process, and the oxygen rich stream exiting the anode side of the SOEC is simultaneously used as an oxidant for the same oxyfuel combustion or oxycalcination process, then the process can potentially be carried out without the need for additional fuel. If renewable or other low carbon energy sources are used to generate the electrical energy used to operate the SOEC, the process of the present invention can be carried out with very low CO2 emissions.

[0041] The O2 concentration (in this article, concentration is the same as content) in the oxygen-enriched carbon dioxide gas is 0<[O2]≤100 volume%. According to one embodiment, the lower limit of the oxygen concentration is 0.1 volume%. In another embodiment, the oxygen concentration is between 10% and 60%, more preferably between 20% and 40%. Whenever two molecules of CO and / or H2 are electrochemically produced, one molecule of O2 is produced.

[0042] Accordingly, hydrogen or carbon monoxide or a mixture of hydrogen and carbon monoxide is electrochemically produced at the cathode side of at least one solid oxide electrolyzer, and oxygen is electrochemically produced at the anode side of at least one solid oxide electrolyzer in a (H2+CO):O2 molar ratio of 2:1.

[0043] In the field of solid oxide fuel cells and electrolysis, it is well-known that CO2 negatively affects Sr-containing anode materials (such as LSC, LSCF, and LSM). More specifically, it has been shown that in the presence of CO2, such materials decompose and form SrCO3 and other phases. For example, V. Esposito et al., Solid State Ionics, 227 (2012) 46-56 have demonstrated that when exposed to pure CO2 at 800 °C, LSC with the composition of La 0.6 Sr 0.4 CoO 3-δ decomposes into La 0.6 Sr 0.4-x O 3-δ” +x SrCO3+0.5(δ’+δ”)O2+x CoO. Here, δ’ and δ” refer to the oxygen non-stoichiometry in the perovskite, and x refers to the degree of decomposition (0 < x ≤ 0.4). The decomposition was confirmed by X-ray diffraction and thermogravimetric analysis. When the membrane was exposed to pure CO2 at 780 °C, the oxygen flux (i.e., performance) through the LSC membrane decreased by more than 4 times. Esposito et al. concluded that "the use of CO2 is particularly harmful below 800 °C".

[0044] S. Darvish et al. (Journal of Power Sources, 336 (2016) 351-359) also studied the variation of SrCO3 formation probability with temperature, CO2 partial pressure, O2 partial pressure, and LSCF composition using thermodynamic and electrochemical calculations. They proposed that the decomposition of LSCF under CO2-enriched conditions occurs through the following reaction:

[0045] LSCF (reactant) + CO2 = LSCF (product) + SrCO3 + (Co,Fe)3O4 + Fe2O3,

[0046] where LSCF(reactant) is the LSCF sample before CO2 exposure, LSCF(product) is the sample after CO2 exposure (which may have a different composition than LSCF(reactant) due to the formation of new phases), (Co,Fe)3O4 is a cobalt-iron mixed oxide with a spinel structure in which the Co:Fe ratio may vary, and Fe2O3 is corundum. Darvish et al. demonstrated that high CO2 partial pressure and low O2 partial pressure increase the thermodynamic probability of SrCO3 formation. More specifically, they demonstrated that: 1) at temperatures above 427°C, SrCO3 becomes stable at lower oxygen partial pressures at all temperatures studied; 2) the higher the temperature, the greater the effect of any change in oxygen partial pressure on the stability of SrCO3. Even more specifically, they demonstrated that more than 50% La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O3(LSCF) should be heated at 727℃ under reducing conditions (10 -5 atm oxygen partial pressure) when exposed to 30 vol% CO2. In addition, SrCO3 becomes more stable when the Sr concentration in the LSCF increases and / or the Fe concentration in the LSCF decreases. They also compared (La 0.8 Sr 0.2 ) 0.98 MnO3(LSM) and La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O3(LSCF), and concluded that LSM is more stable than LSCF in CO2-rich gas.

[0047] It has now been surprisingly demonstrated that under some conditions, the problem of perovskite decomposition in CO2-rich gases is much less severe than expected. More specifically, when the perovskite is subjected to pure CO2 (i.e., at a CO2 partial pressure of nearly 1 and an oxygen partial pressure of approximately 10) at typical SOEC operating temperatures, the decomposition of the perovskite is significantly reduced. -5 Atm) fed to the anode side of an operating electrolytic cell or stack, we observed very little or no degradation of the LSCF-based electrodes. Although the formation of SrCO3 is thermodynamically strongly favored in a gas with such a composition, the driving force for SrCO3 formation is significantly reduced by the constant flow of oxygen ions supplied to the anode through the electrolyte. Therefore, despite the exposure of the SOEC anode to a feed gas containing CO2, the SOEC can operate without significant performance degradation.

[0048] With respect to the prior art, oxy-calciners have received more extensive attention due to their potential uses, such as direct air capture devices involving calcium cycles. For example, as mentioned above, David W. Keith et al. described a process for capturing CO2 from the atmosphere (Joule 2, 1573-1594 (2018)).

[0049] Typically, oxygen for oxycalciners is obtained by cryogenic air separation, as mentioned in David W. Keith et al. However, as mentioned earlier, ASUs are very expensive (in terms of CAPEX and OPEX), so it would be very advantageous if oxygen could be provided at a lower energy requirement while reducing the nitrogen content of the gas mixture.

[0050] US 9.975.100 teaches the importance of using an oxygen-rich gas stream substantially free of nitrogen to calcine CaCO3 crystal aggregates. Such a gas stream can be obtained by a low temperature ASU, but is expensive, especially for smaller scale applications. Therefore, US 9.975.100 confirms the necessity of avoiding the presence of nitrogen in the oxidant stream fed to the oxy-fuel calciner.

[0051] WO 2008 / 039783 describes another calcium cycle process for high purity hydrogen production, comprising the steps of: (a) gasifying a fuel into a raw synthesis gas comprising CO, hydrogen and steam, and sulfur and halide contaminants in the form of H2S, COS and HX, wherein X is a halogen; (b) passing the raw synthesis gas through a water gas shift reactor (WGSR) injected with CaO and steam, the CaO reacting with the shifted gas to remove CO2, sulfur and X from a solid phase calcium-containing product comprising CaCO3, CaS and CaX2; (c) separating the solid phase calcium-containing product from an enriched gaseous hydrogen product, and (d) regenerating the CaO by calcining the solid phase calcium-containing product in the presence of steam, in the presence of CO2, in the presence of synthesis gas, in the presence of H2 and O2, under partial vacuum, and combinations thereof. The CaO may have a carbon content of at least 12.0 m 2 / g and a surface area of ​​at least 0.015 cm 3 / g of pore volume, CaO has an adsorption capacity of at least about 70 grams of CO2 per kilogram of CaO.

[0052] US 2010 / 0239924 describes a fuel cell system with partial recirculation of the anode exhaust gas. The document only mentions a solid oxide fuel cell system and some recirculation systems, but does not involve the production of O2 in a stream containing CO2 on the oxygen side. In addition, the anode of a solid oxide fuel cell refers to the fuel electrode, i.e., an electrode that usually contains metallic Ni.

[0053] US 9.637.393 teaches a calcium circulation system including a calciner. CaCO3 crystal aggregates react to reform calcium oxide, which is used in the previous step of the process and releases a gas stream containing CO2 by the reaction CaCO3(s)->CaO(s)+CO2(g).

[0054] The reaction takes place at about 900°C, requires heat energy as input, and is carried out in a unit commonly called a calciner. Heat can be supplied to the calciner by the combustion of hydrocarbons, such as natural gas, fuel oil, coal or biomass, or by using solar energy, electricity or a combination thereof. The calciner used can be a rotary kiln, a shaft kiln, a flash calciner or a fluidized bed calciner. The necessary heat is provided when the fuel stream is burned with oxygen in the gas stream, which may consist of air or oxygen from an ASU.

[0055] US 9.284.651 belonging to the applicant discloses an apparatus for producing high-purity CO by electrolysis of CO2 in a stack of solid oxide electrolysis cells followed by the use of a gas separation unit.

[0056] WO 2014 / 154253, also belonging to the applicant, teaches the possibility of using different flushing gases on the anode side. Specifically, it discloses a method for producing CO from CO2 in a SOEC stack. CO2 is directed to the fuel side of the stack by an applied electric current, and excess oxygen is transported to the oxygen side of the stack, optionally flushing the oxygen side with air or nitrogen. The product stream from the SOEC stack (containing CO mixed with CO2) is subjected to separation.

[0057] With regard to the above-mentioned documents belonging to the applicant, it has been shown that CO2 can be used on the oxygen side of SOEC. However, in these documents, the reason for using CO2 instead of air on the anode side is to avoid N2 leaking to the fuel (cathode) side of the electrolyzer through small defects and pinholes that are inevitably present in the SOEC electrolyte. If the goal of the SOEC is to produce high-purity CO on the product side, N2 leakage is undesirable because once present, it is difficult and expensive to remove N2 from the CO gas. In the present invention, the idea is to deliberately use a gas containing CO2 as an anode side feed gas to obtain a mixture of CO2 and O2 for use in an oxygen calciner or other oxygen-consuming process downstream.

[0058] A SOEC or SOEC stack can produce H2 from H2O and / or CO from CO2 on the cathode side. This means that any process that requires H2 and / or CO can use SOEC for these purposes. Through the present invention, it is now also easier to utilize the oxygen produced on the anode side of the SOEC. This in turn means that the SOEC can now be better integrated into various processes or systems that require H2 and / or CO and O2 / CO2 mixtures. Examples of such different processes include biomass gasification and oxyfuel (non-fossil fuel) processes, among others. In various upstream emission sources of CO2, such as cement and steel mills, CO2 can now be recycled with the help of the present invention to obtain CO and O2 / CO2 mixtures. Importantly, the effluent stream of CO2-rich gas leaving the gasifier (e.g., oxygen-fired) can be used as the anode side feed stream of the SOEC.

[0059] According to one aspect of the invention, there is provided an apparatus comprising a solid oxide electrolysis cell (17) having an anode side (17A) and a cathode side (17C), wherein the anode side (17A) of the electrolysis cell is fluidly connected to an oxygen consumption unit (10, 20) selected from an oxygen combustion unit or an oxygen calcination unit, and the cathode side of the electrolysis cell is fluidly connected to a hydrogen and / or carbon monoxide consumption unit (18), and wherein the apparatus is configured to operate the method of any of the preceding claims. An oxygen combustion unit is a unit comprising the associated hardware for carrying out an oxygen combustion process, such as the aforementioned oxygen combustion process. An oxygen calcination unit is a unit comprising the associated hardware for carrying out an oxygen calcination process (such as the aforementioned oxygen calcination process).

[0060] In this context, "fluid connection" means ensuring free fluid passage both in operation and out of operation unless active action is or has been taken to close the connection. There may be control means configured to control or divert gas flows to the oxygen consumption unit and / or to the hydrogen and / or carbon monoxide consumption unit.

[0061] According to one embodiment of the invention, the oxygen consuming unit of the apparatus may be an oxygen calcination unit, and the hydrogen and / or carbon monoxide consuming unit may be one and the same oxygen calcination unit.

[0062] According to one embodiment of the invention, the apparatus comprises a control device configured to control the flow from the anode side of the solid oxide electrolysis cell to the oxygen consumption unit. Such a control device comprises a valve or other hardware for reducing or diverting the gas flow.

[0063] According to one embodiment of the present invention, the apparatus comprises a control device configured to control the flow from the cathode side of the solid oxide electrolysis cell to the hydrogen and / or carbon monoxide consumption unit. Such a control device comprises a valve or other hardware for reducing or diverting the gas flow.

[0064] The present invention is described in more detail in the following examples.

[0065] Example 1 (Comparative Example)

[0066] exist Figure 1 In the present invention, a method (1) according to the state of the art is presented, wherein an oxygen-rich gas (104) is fed to an oxygen calciner (10) and the oxygen-rich gas (104) originates from a cryogenic air separation unit (11). More specifically, an air stream (101) is fed to a cryogenic air separation unit (11) and is thereby separated into an oxygen-rich gas stream (102) and an oxygen-deficient gas stream (103). The gas stream (102) is preheated (e.g. to about 650° C.) using a preheater (12), and the preheated gas stream (104) is then fed to the oxygen calciner (10). At the same time, a fuel stream (105) is fed to the oxygen calciner (10), and the stream is optionally preheated (not shown). A solid material stream (106) containing calcium carbonate is preheated (e.g. to about 650° C.) using a second preheater (13), and the preheated solid material stream (107) is fed to the oxygen calciner (10). The fuel (105) reacts with the oxygen in the oxygen-rich gas stream (104), and the exothermic combustion reaction raises the temperature in the oxygen calciner (10) to about 900°C, which causes the calcium carbonate in the solid material (107) to decompose into calcium oxide and carbon dioxide in the oxygen calciner (10). A suitable oxygen calciner design for this purpose is a circulating fluidized bed (CFB) calciner. The output stream (108) from the oxygen calciner (comprising calcium oxide, carbon dioxide and steam) is fed to a first separator (14), such as a cyclone separator, where the stream is separated into a stream (109) comprising calcium oxide and a stream (110) comprising carbon dioxide and steam. The stream (110) is further fed to a second separator (15), such as a water separation vessel, where the stream (110) is separated into a stream (111) comprising H2O and a stream (112) comprising carbon dioxide.

[0067] Assuming that the oxygen content in the oxygen-rich streams (102, 104) is about 95%, an oxygen calciner with a capacity to calcine 300 tons of calcium carbonate per hour requires about 13 tons of methane or natural gas per hour as fuel and about 60 tons of oxygen-rich gas per hour as oxidant. The main impurity in the oxygen-rich streams (102, 104) originating from the air separation unit (11) is nitrogen. The higher the required oxygen content in the oxygen-rich stream (102), the lower the efficiency of the air separation unit (11). The output streams from the 300 tons / hour oxygen calciner are, for example, a stream (109) containing calcium oxide with a flow rate of 165 tons / hour, a stream (111) containing H2O with a flow rate of 30 tons / hour and a stream (112) containing carbon dioxide with a flow rate of about 170 tons / hour. The composition of the stream (112) containing carbon dioxide is, for example, 97% CO2, 1% O2, 1.5% N2 and 0.01% H2O. Although the preheater (12, 13) and separator unit (14, 15) are Figure 1 , but preheating and separation can be performed in a unit that combines the functions of a preheater and a separator, such as a solid-gas cyclone separator. For example, preheating of the oxygen-rich stream (102) can be performed in a cyclone separator in the presence of a calcium oxide product from an oxygen calciner.

[0068] Example 2

[0069] exist Figure 2 In, a preferred embodiment (2) of the method according to the present invention is presented, wherein an oxygen-rich gas (206) is fed into an oxygen calciner (10), the oxygen-rich gas (206) being obtained by flushing the anode (oxygen) side (17A) of at least one operating solid oxide electrolysis cell (17) with a feed gas (205) comprising CO2, and wherein at least part of the first cathode side product gas (203) comprising carbon monoxide and / or hydrogen is supplied to a hydrogen and / or carbon monoxide consumption process (18). More specifically, a first cathode side feed stream (201) comprising water or steam or CO2 or a mixture thereof is preheated using a cathode side preheater (16), and thereafter the preheated first cathode side feed stream (202) is supplied to the cathode side (17C) of at least one solid oxide electrolysis cell (17).

[0070] At the same time, the first anode side feed gas (204) containing carbon dioxide is preheated using an anode side preheater (19), and the preheated first anode side feed gas (205) is supplied to the anode (oxygen) side (17A) of the solid oxide electrolysis cell. An external voltage is applied to the solid oxide electrolysis cell (17) to provide a driving force for electrochemically reducing at least part of the carbon dioxide and / or steam in the first cathode side feed stream (202) to carbon monoxide and / or hydrogen, thereby forming a first cathode side product gas (203) rich in hydrogen, carbon monoxide or a mixture thereof. Part (not shown) or all of the first cathode side product gas (203) is supplied to a hydrogen and / or carbon monoxide consumption process (18), such as a methanol production process, an ammonia production process, a hydroprocessing process, a methanation process, a hydrogenation process, a carbonylation process, a hydroformylation (carbonylation) process or an oxidative carbonylation process. An externally applied voltage drives the electrochemical oxidation reaction on the anode side (17A) of the solid oxide electrolysis cell, whereby oxygen ions (O - ) is converted into molecular oxygen (O2). The electrochemically produced O2 is mixed with the preheated first anode side feed gas (205) containing carbon dioxide to form a first anode side product gas with a low nitrogen content, an oxygen-rich gas (206). The operating temperature of the solid oxide electrolysis cell (17) is generally between 600°C and 1000°C, preferably between 600°C and 900°C, 700°C and 850°C. Due to the high operating temperature of the solid oxide electrolysis cell, the oxygen-rich stream (206) does not need to be further heated before being sent to the oxygen calciner (10), but can pass through a heat exchanger (not shown). It is further understood that the other above-mentioned streams can pass through a heat exchanger to achieve better heat integration.

[0071] At the same time, a fuel stream (105) is fed to the oxygen calciner (10) and the stream is optionally preheated (not shown). A solid material stream (106) containing calcium carbonate is preheated (e.g. to about 650°C) using a preheater (13), such as a solid-gas cyclone separator, and is fed into the oxygen calciner (10) using the preheated solid material stream (107). The fuel (105) reacts with oxygen in the oxygen-rich stream (206), and the exothermic combustion reaction raises the temperature in the oxygen calciner (10) to about 900°C, which causes the calcium carbonate (107) in the solid material to decompose into calcium oxide and carbon dioxide in the oxygen calciner (10). The output stream (108) from the oxygen calciner (comprising calcium oxide, carbon dioxide and steam) is fed into a first separator (14), such as a cyclone separator, where the stream is separated into a stream (109) containing calcium oxide and a stream (110) containing carbon dioxide and steam. The stream (110) is further fed to another separator (15), such as a water separation vessel, where the stream is separated into a stream (111) comprising H2O and a stream (112) comprising carbon dioxide.

[0072] Assuming that the oxygen content in the oxygen-rich stream (206) is 95% by volume, with the remainder being CO2, an oxygen calciner with a capacity to calcine 300 tons of calcium carbonate per hour requires about 13 tons of methane or natural gas per hour as fuel and about 61 tons of oxygen-rich gas per hour as oxidant. The required flow rate of the first anode side feed stream (204) depends on the required oxygen content in the oxygen-rich stream (206). In order to feed 61 tons of oxygen-rich gas (206) containing 95% by volume of O2 in CO2 to the oxygen calciner, approximately 4 tons of CO2 must be supplied to the anode side (17A) of the electrolysis unit (17). The amount of oxygen produced by the solid oxide electrolysis cell (17) is determined by Faraday's law: in order to produce 57 tons of oxygen per hour, the required current through the electrolysis cell is about 191,000,000 A. Typically, the current range of the solid oxide electrolysis cell is 0.5 A / cm 2 Up to 1A / cm 2 Therefore, under the above conditions, the electrode area required for the electrolysis unit (17) is between 19100m 2 Up to 38200m 2 When pure water or steam is used as the first cathode side feed stream (201) of the electrolysis cell, such an electrolysis unit will produce about 7 tons of hydrogen per hour on the cathode side of the electrolysis cell; or, when pure CO2 is used as the first cathode side feed stream (201) of the electrolysis cell, such an electrolysis unit will produce about 100 tons of CO per hour on the cathode side of the electrolysis cell. The system efficiency is highest when the electrolysis unit (17) is operated at a voltage close to the thermoneutral voltage.

[0073] The nitrogen content of the oxygen-enriched gas stream (206) is determined by the nitrogen content of the first anode side feed gas stream (204). For example, if the first anode side feed gas stream (204) has a nitrogen content of 1% by volume, and the desired oxygen content in the oxygen-enriched gas stream (206) is 95% by volume, the nitrogen content in the resulting oxygen-enriched gas stream (206) is approximately 0.05% by volume.

[0074] Example 3

[0075] exist Figure 3In the embodiment of the present invention, a preferred embodiment (3) of the method according to the present invention is presented, wherein an oxygen-rich gas (312) is fed into an oxygen calciner (10), the oxygen-rich gas (312) being obtained by flushing the anode (oxygen) side (17A) of at least one solid oxide electrolyzer - solid oxide electrolyzer (17) with an anode-side feed gas (308, 309) comprising CO2, and wherein at least part of the first cathode-side product gas (304, 305) rich in carbon monoxide and / or hydrogen is supplied to a hydrogen and / or carbon monoxide consumption process (18), wherein part or all of the product gas stream (304, 310) of the solid oxide electrolyzer (17) is recycled back to the electrolyzer. More specifically, the first cathode-side feed stream (301) comprising water or steam or CO2 or a mixture thereof is preheated using a cathode-side preheater (16). The preheated first cathode side feed stream (302) is optionally mixed with a first cathode side recycle stream (306) to obtain a second cathode side feed stream (303), which is fed to the cathode side (17C) of at least one solid oxide electrolysis cell (17). An external voltage is applied to the solid oxide electrolysis cell (17) to provide a driving force for electrochemically reducing at least a portion of the carbon dioxide and / or steam in the second cathode side feed stream (303) to carbon monoxide and / or hydrogen, thereby forming a first cathode side product gas (304) rich in hydrogen, carbon monoxide or a mixture thereof. Optionally, a portion of the first cathode side product gas (304) is recycled back to the electrochemical cell (17) as a first cathode side recycle stream (306). The remainder of the first cathode side product gas (305) is supplied to the hydrogen and / or carbon monoxide consumption process (18). Although in Figure 3 It is not specifically shown in the figure, but the splitting of the first cathode side product gas (304) into streams (305) and (306) can be carried out in a separation unit, such as a pressure swing adsorber or a temperature swing adsorber or a separation membrane. An additional blower or compressor can be included to increase the pressure of stream (304).

[0076] At the same time, the first anode side feed stream (307) containing carbon dioxide is preheated using the anode side preheater (19). The preheated first anode side feed stream (308) is optionally mixed with the first anode side recycle stream (311) to obtain a second anode side feed stream (309), which is fed to the anode side (17C) of at least one solid oxide electrolysis cell (17). The externally applied voltage drives the electrochemical oxidation reaction on the anode side (17A) of the solid oxide electrolysis cell, thereby converting oxygen ions (O2 -) is converted into molecular oxygen (O2). The electrochemically produced O2 is mixed with the second anode side feed gas (309) containing carbon dioxide to form a first anode side product gas (310) with a low nitrogen content. Optionally, part of the first anode side product gas (310) rich in oxygen is recycled back to the electrochemical electrolysis cell (17) as a first anode side recycle stream (311). The remaining part of the first anode side product gas, i.e., the oxygen-rich gas (312), is an oxygen calciner + SOEC, wherein the CO2 recycled from the flue gas to the SOEC is fed into the oxygen calciner (10). Although in Figure 3 Not specifically shown, the first anode side product gas (310) is split into streams (311) and (312), which can be carried out in a separation unit, such as a pressure swing adsorber or a temperature swing adsorber or a separation membrane. An additional blower or compressor may be included to increase the pressure of stream (310). Due to the high operating temperature of the solid oxide electrolysis cell, the oxygen-rich stream (312) does not need to be further heated, but can pass through a heat exchanger (not shown). It should also be understood that the other above-mentioned streams can pass through a heat exchanger or an additional preheater to achieve better heat integration.

[0077] Example 4

[0078] exist Figure 4In the embodiment of the present invention, a preferred embodiment (4) of the method according to the invention is presented, wherein an oxygen-rich gas (312) is fed to an oxyfuel combustor (20), the oxygen-rich gas (312) being obtained by flushing the anode (oxygen) side (17A) of at least one solid oxide electrolysis cell (17) with an anode side feed gas (308, 309) comprising CO2, and wherein at least part of the first cathode side product gas (304, 305) rich in carbon monoxide and / or hydrogen is supplied to a hydrogen and / or carbon monoxide consumption process (18), wherein a part or all of the output gas stream from the solid oxide electrolysis cell is recycled back to the electrolysis cell, as described in Example 3. Advantageously, the oxygen content in the first anode side product gas (310, 312) is between 20% and 40% by volume, for example 35% by volume, in order to match the heat capacity of air and obtain a flame temperature similar to that in an air-blown kiln. It will be appreciated that the above streams may be passed through a heat exchanger or an additional preheater to achieve better heat integration. For this purpose, a suitable oxy-fuel combustor design is a pulverized fuel kiln or a circulating fluidized bed (CFB) kiln. At the same time, a solid fuel stream (401), including, for example, coal, wood or biomass, may optionally be preheated using a preheater (21) to obtain a preheated solid fuel stream (402). The preheated solid fuel stream (402) is fed to the oxy-fuel combustor (20). In the combustor (20), the solid fuel (402) reacts with the oxygen in the oxygen-rich gas stream (312), and the exothermic combustion reaction raises the flame temperature near the burner (1 to 4 meters from the burner) to above 1100°C and up to 1900°C.

[0079] The output stream (403) from the oxyfuel combustor (20) comprising solid combustion residues, carbon dioxide and steam is fed to a first separator (22), such as a cyclone separator, wherein the stream is separated into a stream (405) comprising solid combustion residues (404) and a stream (405) comprising carbon dioxide and steam. The stream (405) is further fed to a second separator (23), such as a water separation vessel, wherein the stream is separated into a stream (406) comprising H2O and a stream (407) comprising carbon dioxide. Further separation steps may be required and are known to those skilled in the art.

[0080] Assuming an oxygen content of 35% by volume in the oxygen-enriched stream (312), the balance being CO2 and an excess of 5% oxygen, a 0.21 MW pilot scale coal-oxygen combustion unit requires 31 kg per hour of solid fuel (coal) stream (401) and 233 kg per hour of oxygen-enriched stream (312). The output stream (403) from the oxy-fuel combustor (20) contains less nitrogen oxides (NO x ). NO xThe concentration varies with flame temperature and therefore increases when an oxygen-enriched stream (312) with a higher oxygen content is used. The nitrogen content in the solid fuel streams (401, 402) also affects the NO in stream (403). x concentration.

[0081] Example 5

[0082] exist Figure 5 In the embodiment of the present invention, another preferred embodiment (5) of the method according to the invention is presented, wherein an oxygen-rich gas (206) is fed into the oxygen calciner (10), the oxygen-rich gas (206) being obtained by flushing the anode (oxygen) side (17A) of at least one solid oxide electrolysis cell (17) with a first anode-side feed gas (205) comprising CO2, wherein at least part of the gas (203) containing carbon monoxide and / or hydrogen is supplied to a hydrogen and / or carbon monoxide consumption process (18), wherein a flue gas stream (503) containing carbon dioxide is recycled, i.e., wherein at least part of one or both feed gas streams (201, 204) fed to the electrolysis unit comprises at least part of the flue gas stream (503) containing carbon dioxide. In particular, the flue gas stream (501) containing carbon dioxide is split into two equal or unequal parts, wherein a first part (502) of the stream containing carbon dioxide is led out of the process, and a second part (503) of the stream containing carbon dioxide is used to supply feed gas to the electrolysis stack. More specifically, the stream (503) is divided into two equal or unequal parts (504, 505), wherein the stream (504) is optionally mixed with a supplementary cathode side feed stream (506) comprising water or steam or CO2 or a mixture thereof, thereby obtaining a first cathode side feed stream (201). The stream (505) is optionally mixed with a supplementary anode side feed stream (507) comprising CO2, thereby obtaining a first anode side feed gas (204). In one embodiment of the method according to the present invention, the supplementary gas stream (506) comprises steam and has a low CO2 content. It should be understood that the stream (503) comprising carbon dioxide can be supplied to either or both sides of the solid oxide electrolysis cell (17).

[0083] Example 6

[0084] exist Figure 6In the embodiment of the present invention, another preferred embodiment (6) of the method according to the present invention is presented, wherein an oxygen-rich gas (206) is fed into the oxygen calciner (10), the oxygen-rich gas (206) being obtained by flushing the anode (oxygen) side (17A) of at least one solid oxide electrolysis cell (17) with a feed gas (205) comprising CO2, and wherein at least part of the first cathode side product gas (203) comprising carbon monoxide and / or hydrogen is supplied to the hydrogen and / or carbon monoxide consumption process (18), and wherein at the same time part of the first cathode side product gas (203) containing carbon monoxide and / or hydrogen is supplied to the oxygen calciner (10) as a fuel stream (602). More specifically, the first cathode side product gas (203) is split into two equal or unequal parts (601, 602). The stream (601) is supplied to the hydrogen and / or carbon monoxide consumption process (18), while the stream (602) is used as fuel in the oxygen calciner (10). The hydrogen and / or carbon monoxide rich stream (602) may be mixed with additional fuel (603), such as methane, natural gas, hydrogen, carbon monoxide, etc., to obtain a mixed fuel stream (604) which is fed into the oxygen calciner (10). It should be understood that part of the stream (203, 206) may be recycled back to the respective side of the solid oxide electrolysis cell, as described in Examples 3 and 4 and not in Figure 6 Clearly shown in.

[0085] Example 7

[0086] exist Figure 7 In, a preferred embodiment (7) of the method according to the invention is presented, wherein an oxygen-enriched gas (703) is fed to an oxyfuel combustor (20), wherein the oxygen-enriched gas (703) is obtained by mixing (in equal or unequal parts) the following gas streams: an oxygen-enriched first anode side product gas (312) obtained by flushing the anode (oxygen) side (17A) of at least one solid oxide electrolyzer (17) with an anode side feed gas (308, 309) containing CO2; and a flue gas stream (701) obtained by dividing a flue gas stream (407) containing CO2 into two equal or unequal parts (701, 702). Stream (702) is led out of the system, while stream (701) is recycled, as described above. Advantageously, the oxygen content in the first anode side product gas (310, 312) is between 90% and 100% by volume, for example 95% by volume, to minimize the total gas flow rate through the anode chamber of the solid oxide electrolyzer. Advantageously, the oxygen content in the oxygen-enriched gas (703) is between 20 and 40 volume %, for example 35 volume %, to match the heat capacity of air and obtain a flame temperature similar to that in an air-blown kiln.

[0087] Example 8

[0088] Two identical solid oxide electrolysis cell stacks, each consisting of 75 cells with a total active area of ​​approximately 8250 cm 2 , operated in electrolysis mode for 120 hours ( Figure 8 ). The first cathode side feed stream (301) containing ≥99.9% CO2 is mixed with the first cathode side recycle stream (306) containing CO and CO2 to obtain a second cathode side feed stream (303). The second cathode side feed stream (303) is introduced into the cathode side compartments of the two stacks at a temperature of 800°C simultaneously ( Figure 8 a). The electrolysis current passes through the two stacks, causing a portion of the CO2 in the cathode side feed stream to be electrochemically converted into CO, thereby enriching the first cathode side product stream (304) leaving the stack with CO. The temperature of the stream (304) leaving the stack is 751-753°C. The gas is compressed and sent to a pressure swing adsorber unit. The CO-rich outlet stream (305) from the pressure swing adsorber unit is collected as a product for use in, for example, a phosgene plant, while the CO-depleted outlet stream (306) from the pressure swing adsorber unit is mixed with the first cathode side feed stream (301) as described above. The first anode side feed stream (204) containing ≥99.9% CO2 is preheated to 785°C, and the resulting preheated first anode side feed stream (205) is fed to the anode side of the two stacks. As the electrolysis current passes through the stack, gaseous O2 is electrochemically generated on the anode side of the electrolytic cell in the stack, thereby obtaining an oxygen-rich first anode side product gas (206). The first anode side product gas (206) contains CO2 and O2 and has a significantly low nitrogen content. The exact nitrogen content was not measured, but it is estimated to be less than 50 ppm. During the experiment, the temperature of the first anode side product gas (206) leaving the stack was 791-793°C. The stack voltage required to maintain an electrolysis current of approximately 45A was between 97V and 103V ( Figure 8 b). Surprisingly, no significant performance drop was observed when operating the solid oxide electrolysis cell with an anode side stream containing ≥ 99.9% CO2.

Claims

1. A method for supplying an oxygen-rich gas (206, 312) to an oxygen calcination process as an oxygen-consuming process (10), wherein at least one operating solid oxide electrolysis cell having a cathode side and an anode side is provided, and a) supplying a cathode side feed gas stream (202, 303) comprising steam or CO2 or a mixture thereof to the cathode side (17C) of at least one solid oxide electrolysis cell (17), b) electrochemically reducing at least a portion of the cathode side feed gas stream (202, 303) in the solid oxide electrolysis cell to form a cathode side product gas stream (203, 304) rich in hydrogen, carbon monoxide or a mixture thereof, c) supplying at least a portion of the cathode side product gas stream (203, 304) to a hydrogen and / or carbon monoxide consumption process (18), d) supplying an anode side feed gas stream (205, 309) comprising CO2 to the anode side (17A) of the solid oxide electrolysis cell (17); and e) electrochemically generating oxygen on the anode side of the solid oxide electrolysis cell to form an oxygen-rich anode side product gas stream (206, 310), wherein - feeding an oxygen-rich gas comprising at least a portion of the oxygen-rich anode side product gas stream (206) to the oxygen-consuming process, - the oxygen-rich gas has a low nitrogen content, the nitrogen content being less than 10% by volume, and - The oxygen-rich gas leaving the solid oxide electrolysis cell has a temperature of 600°C to 1000°C.

2. The method of claim 1, wherein the temperature of the oxygen-rich gas leaving the at least one solid oxide electrolysis cell is from 600°C to 900°C.

3. The process of claim 1, wherein the temperature of the oxygen-rich gas leaving the at least one solid oxide electrolysis cell is from 700°C to 850°C.

4. The method according to any one of claims 1 to 3, wherein hydrogen or carbon monoxide or a mixture of hydrogen and carbon monoxide is electrochemically produced on the cathode side of the at least one solid oxide electrolysis cell, and oxygen is electrochemically produced at the anode side of the at least one solid oxide electrolysis cell in a (H2+CO):O2 molar ratio of 2:

1.

5. The method according to any one of claims 1 to 3, wherein the oxygen-rich anode-side product gas (206, 310) has an oxygen content of 0<[O2]≤100%.

6. The method according to any one of claims 1 to 3, wherein the oxygen-rich anode-side product gas (206, 310) has an oxygen content [O2] of 80% to 100%.

7. The method according to any one of claims 1 to 3, wherein the oxygen-rich anode-side product gas (206, 310) has an oxygen content [O2] of 95% to 100%.

8. The method according to any one of claims 1 to 3, wherein at least a portion of the anode side product gas (206, 310) is recycled and used as at least a portion of the anode side feed gas (205, 309).

9. The method according to any one of claims 1 to 3, wherein at least a portion of the cathode side product gas (203, 304) is recycled and used as at least a portion of the cathode side feed stream (202, 303).

10. A method according to any one of claims 1 to 3, wherein the flue gas stream (112, 407, 503) obtained from the oxygen calcination process contains carbon dioxide and is recycled and used as at least a part of the cathode side feed stream (202, 303) and / or anode side feed gas (205, 309) fed to the solid oxide electrolysis cell.

11. The method according to any one of claims 1 to 3, wherein the hydrogen and / or carbon monoxide consuming process (18) comprises a methanol production process, an ammonia production process, a hydrotreating process, a methanation process, a hydrogenation process, a carbonylation process, a hydroformylation (carbonyl synthesis) process or an oxidative carbonylation process.

12. The method according to any one of claims 1 to 3, wherein the cathode side feed stream (201, 301, 506) comprises CO2, and at least a portion of the CO2 in the cathode side feed gas stream (201, 301, 506) and / or the anode side feed gas stream (204, 307, 507) is derived from one or more of the following: Metallurgical processes; cement production; carbon capture processes; direct air capture processes and carbon-based fuel combustion processes, including the combustion of non-fossil fuels; or other processes that generate CO2 in one or more streams.

13. The method according to any one of claims 1 to 3, wherein the nitrogen content in the oxygen-rich stream (206, 312) is less than 1%.

14. The method according to any one of claims 1 to 3, wherein the nitrogen content in the oxygen-rich stream (206, 312) is less than 0.1%.

15. The method of any one of claims 1 to 3, wherein the solid oxide electrolysis cell is operated at a thermoneutral voltage or at ±0.2 V / cell of the thermoneutral voltage.

16. An apparatus comprising: A solid oxide electrolysis cell (17) having an anode side (17A) and a cathode side (17C); an oxygen consuming unit which is an oxygen calcining unit (10); and a hydrogen and / or carbon monoxide consumption unit (18), wherein the anode side (17A) of the electrolysis cell is fluidly connected to the oxygen consumption unit and the cathode side of the electrolysis cell is fluidly connected to the hydrogen and / or carbon monoxide consumption unit (18), and wherein the apparatus is configured to operate a method as claimed in any one of the preceding claims.

17. The apparatus according to claim 16, wherein the oxygen consumption unit and the hydrogen and / or carbon monoxide consumption unit are one and the same oxygen calcination unit.

18. Apparatus according to claim 16 or 17, wherein the apparatus comprises control means configured to control flow from the anode side of the solid oxide electrolysis cell to the oxygen consumption unit.

19. The apparatus of claim 16 or 17, wherein the apparatus comprises a control device configured to control the flow from the cathode side of the solid oxide electrolysis cell to the hydrogen and / or carbon monoxide consumption unit.