Method for preparing semiconductor device
By forming a characteristic AlOxNy film layer on the sapphire substrate and etching the hemispherical nano pits on the side wall of the cone, the defects of the LED devices during the growth of GaN materials on the sapphire substrate are solved, and the luminous efficiency of the LED chip is improved. The luminous intensity is particularly suitable for the production of deep ultraviolet LEDs.
Patent Information
- Application Number
- CN202210771793.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-06-30
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2042-06-30
AI Technical Summary
When existing LED devices grow GaN materials on sapphire substrates, due to excessive lattice differences, there are many defects and insufficient luminous efficiency and reliability, especially the luminous efficiency and reliability of deep ultraviolet LEDs and mini/micro-LEDs. promote.
An AlOxNy film layer is formed on a sapphire substrate. By controlling the mole ratio of oxygen and nitrogen, its refractive index is between 1.30 and 1.35, the cone is etched and the hemispherical nano-pit is etched on the side wall to increase the total reflection angle of light and light intensity, and semiconductor layers are grown in MOCVD to enhance epitaxial crystallization quality.
By improving the total reflection and light intensity of light, the luminous efficiency and luminous intensity of LED chips are improved, which is particularly suitable for the production of deep ultraviolet LED chips, while reducing material growth defects and improving epitaxial crystallization quality.
Smart Images

Figure CN115148873B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and more specifically, to a method for preparing a semiconductor device. Background Art
[0002] LED (Light Emitting Diode) is a semiconductor light-emitting device, mainly composed of p-type semiconductor and n-type semiconductor. Among them, the n-type region has many electrons with high mobility, and the p-type region has many holes with low mobility. The transition layer between the p-type semiconductor and the n-type semiconductor is called the pn junction. When a forward voltage is applied to the LED, electrons can recombine with holes and release photons. At present, the optoelectronic performance of LED has been greatly improved, but the luminous efficiency and reliability of high-end LED device products such as deep ultraviolet LED, mini / micro-LED still need to be improved.
[0003] At present, the mainstream method of making LEDs is to grow GaN materials on sapphire substrates. When GaN materials grow on sapphire, many defects will be generated due to the large lattice difference. In order to improve the crystal quality of GaN, people make cone-shaped patterns on sapphire or silicon oxide to reduce the occurrence of defects. However, the cone has sidewall growth, which will reduce the quality of material growth. In addition, since the refractive index of sapphire and silicon oxide is not much different from that of GaN, the light emitted from the quantum well light-emitting layer cannot be reflected well, thus affecting the luminous efficiency of the LED.
[0004] Therefore, it is of great significance to develop a new manufacturing method to improve the luminous efficiency of the device and enhance the quality of material growth. Summary of the invention
[0005] The present invention provides a method for preparing a semiconductor device, which can effectively improve the luminous efficiency and luminous intensity of an LED chip, and is particularly suitable for preparing a deep ultraviolet LED chip.
[0006] The present application provides a method for preparing a semiconductor device, comprising the following steps:
[0007] Providing a sapphire substrate;
[0008] After the sapphire substrate is routinely cleaned, it is placed in an electron beam reaction chamber, and Al material is evaporated in a nitrogen ion-assisted and oxygen atmosphere to form AlO on the surface of the sapphire substrate. x N y The AlO film layer is formed by controlling the molar ratio of oxygen atoms to 5% to 25% and the molar ratio of nitrogen atoms to 12% to 40%. x N y The refractive index of the thin film layer is between 1.30 and 1.35;
[0009] Using stepper lithography on AlO x N y The film layer is coated with photoresist to make a pattern, and then dry-etched with an inductively coupled plasma etcher. x N y A cone is etched out of the thin layer and then cleaned;
[0010] The sapphire substrate with the cone formed thereon is placed in an MOCVD reaction chamber, and hydrogen is introduced to etch the sidewall of the cone into a hemispherical nano-pit;
[0011] The n-type semiconductor layer, the light-emitting layer, and the p-type semiconductor layer are continuously grown by MOCVD until the epitaxial wafer has a complete structure.
[0012] Optionally, along a direction perpendicular to the plane where the sapphire substrate is located, the AlO x N y The thickness of the film layer is 2 to 4 um.
[0013] Optionally, the height of the cone is 1.60-1.9 um, the bottom diameter is 2.5-2.8 um, and the distance between two adjacent cones is 0.2-0.5 um.
[0014] Optionally, the diameter of the hemispherical nano-pits is 60-300 nm, and the distance between two adjacent pits is 20-35 nm.
[0015] Compared with the prior art, the method for preparing a semiconductor device provided by the present invention achieves at least the following beneficial effects:
[0016] The present invention forms AlO on the surface of the sapphire substrate x N y cone, by controlling the molar ratio of oxygen atoms and nitrogen atoms, AlO x N y The refractive index of the thin film layer is between 1.30 and 1.35, and the brightness is improved by changing the total reflection angle of light. Compared with the traditional sapphire cone and SiO2 cone (the refractive index of sapphire is 1.78 and the refractive index of silicon oxide is 1.46), when the light emitted by MQW is emitted from GaN to the sapphire cone, the angle is greater than 46.4° and the angle is greater than 36.4° when it is emitted from GaN to SiO2. x N y When the angle is greater than 30.6°, total reflection can occur, and more light returns and is emitted from the front or side, thereby improving the luminous efficiency of the LED device.
[0017] By making hemispherical nano-pits on the side wall of the cone, when the light emitted from the multi-quantum well light-emitting layer is directed to the hemispherical nano-pits on the side wall of the cone, it will encounter nano-scale windows, and the light can oscillate back and forth at both ends of the window. The light with a wavelength matching the window can be enhanced and propagated from the side wall of the inverted cone pit, effectively improving the luminous intensity of the LED chip, which is particularly suitable for making deep ultraviolet LED chips. In addition, the presence of nano-pits on the side wall of the cone makes it more difficult for gallium nitride materials to nucleate on the side wall of the cone, reducing the growth of the side wall of the pattern, thereby improving the quality of epitaxial crystallization.
[0018] Of course, any product implementing the present invention does not necessarily need to achieve all of the technical effects described above at the same time.
[0019] Further features and advantages of the present invention will become apparent from the following detailed description of exemplary embodiments of the present invention with reference to the attached drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The accompanying drawings, which are incorporated in and constitute a part of the specification, illustrate embodiments of the invention and, together with the description, serve to explain the principles of the invention.
[0021] Figure 1 Shown is a complete structural diagram of a semiconductor diode provided in an embodiment of the present application;
[0022] Figure 2 Shown is a schematic diagram of a cone provided in an embodiment of the present application;
[0023] Figure 3 The figure shows a schematic diagram of a cone with a hemispherical nano-pit etched into a sidewall provided by an embodiment of the present application;
[0024] Among them, 1. sapphire substrate, 2. AlO x N y Film layer, 3. cone, 4. n-type semiconductor layer, 5. multi-quantum well layer, 6. p-type semiconductor layer. DETAILED DESCRIPTION
[0025] Various exemplary embodiments of the present invention will now be described in detail with reference to the accompanying drawings. It should be noted that the relative arrangement of components and steps, numerical expressions and numerical values set forth in these embodiments do not limit the scope of the present invention unless otherwise specifically stated.
[0026] The following description of at least one exemplary embodiment is merely illustrative in nature and is in no way intended to limit the invention, its application, or uses.
[0027] Technologies, methods, and equipment known to ordinary technicians in the relevant art may not be discussed in detail, but where appropriate, the technologies, methods, and equipment should be considered as part of the specification.
[0028] In all examples shown and discussed herein, any specific values should be interpreted as merely exemplary and not limiting. Therefore, other examples of the exemplary embodiments may have different values.
[0029] It should be noted that like reference numerals and letters refer to similar items in the following figures, and therefore, once an item is defined in one figure, it need not be further discussed in subsequent figures.
[0030] The present invention provides a method for preparing a semiconductor device, which can improve the crystal quality of epitaxial materials, effectively improve the luminous efficiency and luminous intensity of LED chips, and is particularly suitable for preparing deep ultraviolet LED chips.
[0031] The following is a detailed description with reference to the accompanying drawings and specific embodiments.
[0032] Figure 1 Shown is a complete structural diagram of a semiconductor diode provided in an embodiment of the present application; Figure 2 Shown is a schematic diagram of a cone provided in an embodiment of the present application; Figure 3 FIG. 1 is a schematic diagram of a cone with a hemispherical nano-pit etched into a sidewall provided by an embodiment of the present application. Figure 1-Figure 3 , the method for preparing a semiconductor device comprises:
[0033] Step 1: Provide a sapphire substrate 1.
[0034] Step 2: After the sapphire substrate 1 is subjected to conventional cleaning treatment, the sapphire substrate 1 is placed in an electron beam reaction chamber, and Al material is evaporated in a nitrogen ion-assisted and oxygen atmosphere to form an AlO layer with a thickness of 2 to 4 μm on the surface of the sapphire substrate. x N y The AlO layer 2 is formed by controlling the molar ratio of oxygen atoms to 5% to 25% and the molar ratio of nitrogen atoms to 12% to 40%. x N y The refractive index of the thin film layer is between 1.30 and 1.35.
[0035] Step 3: Use a stepper lithography machine to x N y A photoresist is applied to the film layer 2 to form a pattern, and then dry etching is performed using an inductively coupled plasma etcher. x N yA plurality of cones 3 are etched on the thin layer 2, wherein the height H of the cone 3 is 1.60-1.9 um, the bottom diameter M is 2.5-2.8 um, and the distance L between two adjacent cones 3 is 0.2-0.5 um, and then the thin layer 2 is cleaned.
[0036] Step 4: Place the sapphire substrate with the cone 3 formed thereon into a MOCVD reaction chamber, introduce hydrogen, and etch the sidewall of the cone 3 into a hemispherical nano-pit, wherein the diameter R of the hemispherical nano-pit is 60 to 300 nm, and the distance D between two adjacent pits is 20 to 35 nm.
[0037] Step 5: Continue to grow the n-type semiconductor layer 4, the light-emitting layer 5, and the p-type semiconductor layer 6 by MOCVD until the epitaxial wafer has a complete structure.
[0038] Although some specific embodiments of the present invention have been described in detail by way of example, it will be appreciated by those skilled in the art that the above examples are for illustration only and are not intended to limit the scope of the present invention. It will be appreciated by those skilled in the art that the above embodiments may be modified without departing from the scope and spirit of the present invention. The scope of the present invention is defined by the appended claims.
Claims
1. A method for preparing a semiconductor device, characterized in that: The following steps are involved: Providing a sapphire substrate; After the sapphire substrate is routinely cleaned, it is placed in an electron beam reaction chamber, and Al material is evaporated in a nitrogen ion-assisted and oxygen atmosphere to form AlO on the surface of the sapphire substrate. x N y The AlO film layer is formed by controlling the molar ratio of oxygen atoms to 5% to 25% and the molar ratio of nitrogen atoms to 12% to 40%. x N y The refractive index of the thin film layer is between 1.30 and 1.35; Using stepper lithography on AlO x N y The film layer is coated with photoresist to make a pattern, and then dry-etched with an inductively coupled plasma etcher. x N y A cone is etched out of the thin layer and then cleaned; The sapphire substrate with the cone formed thereon is placed in an MOCVD reaction chamber, and hydrogen is introduced to etch the sidewall of the cone into a hemispherical nano-pit; The n-type semiconductor layer, the light-emitting layer, and the p-type semiconductor layer are continuously grown by MOCVD until the epitaxial wafer has a complete structure.
2. The method for preparing a semiconductor device according to claim 1, wherein: Along the direction perpendicular to the plane where the sapphire substrate is located, the AlO x N y The thickness of the film layer is 2 to 4 um.
3. The method for preparing a semiconductor device according to claim 1, wherein: The height of the cone is 1.60-1.9 um, the bottom diameter is 2.5-2.8 um, and the distance between two adjacent cones is 0.2-0.5 um.
4. The method for preparing a semiconductor device according to claim 1, wherein: The diameter of the hemispherical nano-pits is 60-300 nm, and the distance between two adjacent pits is 20-35 nm.