A method for recovering toluenediamine from toluenediamine tar

Through modified activated carbon adsorption and ultrasonic synergistic degradation technology, the problem of processing heavy components in toluenediamine tar has been solved, efficient recovery and resource utilization of toluenediamine has been achieved, environmental pollution and resource waste have been reduced, and economic benefits and environmental benefits have been achieved. goal of protection.

CN115246776BActive Publication Date: 2024-10-29LANZHOU UNIVERSITY OF TECHNOLOGY
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202111541214.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-16
Publication Date
2024-10-29
Estimated Expiration
2041-12-16

AI Technical Summary

Technical Problem

It is difficult to effectively recover and process the heavy components in toluenediamine tar with existing technology, resulting in resource waste and environmental pollution, and there is a lack of low-cost, easy-to-operate treatment methods.

Method used

Modified activated carbon is used for selective adsorption of toluenediamine, and ultrasonic waves are combined with Fe2+ and H2O2 to collaboratively generate hydroxyl radicals to degrade the azo dimer heavy components in tar, and then use extraction agents and analytical regeneration steps to recover toluenediamine. .

Benefits of technology

The efficient recovery of toluenediamine in toluenediamine tar is achieved, with the degradation rate of heavy components reaching 75.4% to 79.8%. The process is simple and the conditions are easy to control, which reduces environmental pollution and resource waste, and achieves the goals of economic benefits and environmental protection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0003414253330000031
    Figure BDA0003414253330000031
  • Figure BDA0003414253330000051
    Figure BDA0003414253330000051
  • Figure BDA0003414253330000111
    Figure BDA0003414253330000111
Patent Text Reader

Abstract

The present invention provides a method for recovering toluenediamine from toluenediamine tar, the method comprising: dissolving the toluenediamine tar with acetone a, adsorbing free toluenediamine with modified activated carbon, filtering to obtain filtrate A and filter residue A; adjusting the pH value of filtrate A to 0.5-6.5, adding ferrous nitrate aqueous solution and H2O2, and performing ultrasonic degradation reaction at 20°C-50°C, filtering to obtain filtrate B; extracting filtrate B with an extractant, evaporating acetone in the extraction phase, and obtaining toluenediamine product A; adding acetone b to filter residue A at 20°C-50°C, regenerating by analysis, filtering to obtain filtrate C, evaporating acetone, and obtaining toluenediamine product B; combining toluenediamine products A and B to obtain toluenediamine product. The present invention recovers free toluenediamine in toluenediamine tar, and degrades and recycles heavy components in toluenediamine tar, has simple process, simple operation, easily controllable conditions, low environmental pollution risk, and is conducive to resource utilization, reduction, and harmless recovery of tar residues.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of toluenediamine tar recovery, and in particular relates to a method for recovering toluenediamine from toluenediamine tar. Background Art

[0002] In the production process of preparing toluenediamine (TDA) by hydrogenating dinitrotoluene, due to factors such as dehydration and condensation between molecules, high-boiling tar substances (commonly known as TDA tar) will be generated. Such substances have high viscosity and freezing point. In order to ensure the fluidity of the slurry, the tar usually contains 30-50wt% of m-toluenediamine. People usually divide the composition of TDA tar into two parts: light components and heavy components. The light components are mainly toluenediamine to ensure the fluidity of the tar slurry, and the heavy components are mainly azo dimers formed by dehydration condensation of m-toluenediamine and diamino-dimethyl-phenazine substances generated by dehydration of o-toluenediamine. For the recovery of light components in tar, the toluenediamine tar is usually sent to an evaporator, and the toluenediamine is recovered by flash evaporation. The toluenediamine tar at the bottom of the evaporator is disposed of by high-temperature incineration. Conventional flash evaporation recovery methods can reduce the toluenediamine content in tar to less than 15wt%, but as the concentration process proceeds, the viscosity of the tar increases greatly and the fluidity decreases, causing the tar to form a solid state and unable to further recover toluenediamine. U.S. Patent No. 5,728,880 proposes to use low-value-added o-toluenediamine to replace m-toluenediamine in tar, which can reduce the m-toluenediamine in tar to 2.4wt.%, but it also causes a waste of o-toluenediamine resources. The thin film evaporation process proposed by patent CN103896780 can reduce the toluenediamine content in tar to 2-5%, but this method also faces problems such as reduced tar fluidity after evaporation and blockage of the device outlet. Patent CN101875614A discloses a method for recovering meta-diaminotoluene from dinitrotoluene hydrogenated tar using molecular sieve as adsorbent, and the toluenediamine recovery rate can reach about 70%. Patent CN203222566U discloses a dinitrotoluene hydrogenated tar recovery system using a bifunctional resin as an adsorbent. None of the above methods involve the treatment of heavy components in toluenediamine tar. In view of the resource utilization of heavy components in tar, patent CN103524356A proposes a method for converting TDA and heavy components in TDA tar into methylcyclohexylamine and methylcyclohexyl diamine using supported metal-based catalysts such as Ni, Co, Pd, and Pt. The product composition of this method is complex, and the product separation and purification are difficult. At present, there is still a lack of effective means for the recycling of heavy components. Therefore, a new process technology is developed to achieve the controlled degradation of azo compounds in TDA tar, which has the characteristics of mild experimental conditions and simple experimental equipment, in order to provide a low-cost and easy-to-operate new approach for the utilization of TDA tar. Summary of the invention

[0003] The technical problem to be solved by the present invention is to provide a method for recovering toluenediamine from toluenediamine tar in view of the deficiencies of the above-mentioned prior art. The method recovers free toluenediamine in TDA tar on the one hand, and degrades and recovers heavy components in TDA tar on the other hand. The process is simple, the operation is simple, the conditions are easy to control, the risk of environmental pollution is small, and the resource utilization, reduction and harmless recovery of tar residues are beneficial, so as to achieve the goals of economic benefits and environmental protection.

[0004] In order to solve the above technical problems, the technical solution adopted by the present invention is: a method for recovering toluenediamine from toluenediamine tar, the method comprising:

[0005] S1. Dissolving toluenediamine tar with acetone a, adsorbing free toluenediamine with modified activated carbon, and filtering to obtain filtrate A and filter residue A;

[0006] S2, adjusting the pH value of the filtrate A obtained in S1 to 0.5-6.5 with a 98% sulfuric acid aqueous solution, then adding a 72g / L ferrous nitrate aqueous solution and a 30% H2O2 aqueous solution, performing a degradation reaction under ultrasonic conditions at a temperature of 20°C-50°C, and filtering to obtain a filtrate B;

[0007] The filtrate A containing the heavy component of toluenediamine tar was subjected to ultrasonic and Fe 2+ , H2O2 synergistically produce hydroxyl radicals, which degrade the azo dimer heavy components in toluenediamine tar into toluenediamine through hydroxyl radicals. The reaction mechanism is as follows:

[0008] Fe 2+ +H2O2→Fe 3+ +OH - + OH R1

[0009] H2O2+Fe 3+ →Fe 2+ +O2+2H + R2

[0010]

[0011] S3, extracting the filtrate B obtained in S2 with an extractant three times, collecting the extract phase, and evaporating the extractant in the extract phase to obtain a toluenediamine product A;

[0012] S4, adding acetone b to the filter residue A obtained in S1 at a temperature of 20°C to 50°C for analytical regeneration, filtering to obtain a filtrate C, and evaporating the acetone to obtain a toluenediamine product B;

[0013] S5. Combine the toluenediamine product A described in S3 and the toluenediamine product B described in S4 to obtain a toluenediamine product.

[0014] Preferably, the dosage ratio of toluenediamine tar, acetone a and modified activated carbon in S1 is 10g:50mL:12g.

[0015] Preferably, the modified activated carbon in S1 is acetic acid modified activated carbon, nitric acid modified activated carbon, sodium hydroxide modified activated carbon or ammonia modified activated carbon.

[0016] Preferably, the mass ratio of the ferrous nitrate aqueous solution with a mass concentration of 72 g / L and the H2O2 aqueous solution with a mass fraction of 30% in S2 is 1:(5-35).

[0017] Preferably, the ultrasonic frequency in the degradation reaction in S2 is 20kHz to 80kHz, and the degradation reaction time is 0.5h to 2h.

[0018] Preferably, the extractant in S3 is dichloromethane, chloroform or carbon tetrachloride.

[0019] Preferably, the evaporation temperature in S3 is 20°C to 50°C.

[0020] Preferably, the usage ratio of the filter residue A and acetone b in S4 is 1 g:5 mL.

[0021] Preferably, the time of the analytical regeneration in S4 is 40 min to 60 min.

[0022] Preferably, the evaporation temperature in S4 is 20°C to 70°C.

[0023] Compared with the prior art, the present invention has the following advantages:

[0024] The invention firstly utilizes the selective chemical adsorption characteristics of modified activated carbon to remove free toluenediamine in toluenediamine tar. The pore structure of the activated carbon mainly affects the total adsorption capacity of the activated carbon to toluenediamine tar, while the surface functional groups of the activated carbon affect the selectivity of toluenediamine. The modified activated carbon can not only increase the specific surface area of ​​the activated carbon, but also correspondingly change the distribution of the surface groups, which has a favorable effect on the adsorption selection of toluenediamine. Under the optimal conditions, the selectivity of the acetic acid modified activated carbon to toluenediamine reaches 90.10% to 98.48%.

[0025] 2. The present invention removes the free heavy components of toluenediamine tar from toluenediamine by using ultrasound, Fe 2+, H2O2 synergistically produce hydroxyl radicals, which degrade the azo dimer heavy components in toluenediamine tar into toluenediamine through hydroxyl radicals. The degradation effect of hydroxyl radicals is used to break the -N=N- bond of the toluenediamine tar heavy components to obtain toluenediamine, thereby recovering toluenediamine from the toluenediamine tar heavy components. The degradation rate of the toluenediamine tar heavy components can reach 75.4% to 79.8%, and the experiment has the characteristics of mild experimental conditions and simple operation.

[0026] 3. The present invention recovers free toluenediamine in toluenediamine tar on the one hand, and degrades and recovers heavy components in toluenediamine tar on the other hand, which is beneficial to the resource utilization, reduction and harmless recovery of toluenediamine tar, achieves the goals of economic benefits and environmental protection, and provides a new way for resource utilization and reduction of toluenediamine tar.

[0027] The present invention is further described in detail below in conjunction with embodiments. DETAILED DESCRIPTION

[0028] Example 1

[0029] The method for recovering toluenediamine from toluenediamine tar of the present embodiment is as follows:

[0030] S1. Dissolve toluenediamine tar with acetone a, adsorb free toluenediamine with modified activated carbon (acetic acid modified activated carbon), and obtain filtrate A and filter residue A after filtering; the amount ratio of toluenediamine tar, acetone a and modified activated carbon is 10g:50mL:12g;

[0031] S2, adjusting the pH value of the filtrate A obtained in S1 to 0.5 with a 98% sulfuric acid aqueous solution, then adding a 72g / L ferrous nitrate aqueous solution and a 30% H2O2 aqueous solution, performing a degradation reaction under ultrasonic conditions of a temperature of 30°C and an ultrasonic frequency of 20kHz for 0.5h, and filtering to obtain a filtrate B; the mass ratio of the 72g / L ferrous nitrate aqueous solution to the 30% H2O2 aqueous solution is 1:5;

[0032] The filtrate A containing the heavy component of toluenediamine tar was subjected to ultrasonic and Fe 2+ , H2O2 synergistically produce hydroxyl radicals, which degrade the azo dimer heavy components in toluenediamine tar into toluenediamine through hydroxyl radicals. The reaction mechanism is as follows:

[0033] Fe 2+ +H2O2→Fe 3+ +OH - + OH R1

[0034] H2O2+Fe 3+ →Fe 2+ +O2+2H + R2

[0035]

[0036] S3, extracting the filtrate B obtained in S2 with an extractant (dichloromethane) three times, collecting the extract phase, evaporating it at a temperature of 30° C., and evaporating the dichloromethane in the extract phase to obtain a toluenediamine product A;

[0037] S4, adding acetone b to the filter residue A obtained in S1 at a temperature of 30°C, performing analytical regeneration for 40 minutes, filtering, obtaining a filtrate C, evaporating at a temperature of 30°C, and obtaining a toluenediamine product B after evaporating the acetone; the usage ratio of the filter residue A to acetone b is 1 g:5 mL;

[0038] S5. Combine the toluenediamine product A described in S3 and the toluenediamine product B described in S4 to obtain a toluenediamine product.

[0039] The filter residue A obtained in S1 is weighed to calculate the unit adsorption capacity of the modified activated carbon (the mass of the filter residue A minus the mass of the modified activated carbon, the total adsorption capacity of the obtained adsorbent, the total adsorption capacity of the adsorbent divided by the mass of the modified activated carbon, that is, the unit adsorption capacity); the toluenediamine product A obtained in S3 is weighed, and the toluenediamine product B obtained in S4 is weighed, and the sum of the mass of the two parts of the product is divided by the mass of the toluenediamine tar used to calculate the total yield of the toluenediamine product; the analytical solution (filtrate C) obtained in S4 in Example 1 is used with p-nitrotoluene as the internal standard, and the gas chromatography internal standard method is used to determine the adsorption selectivity of toluenediamine. The experimental results are shown in Table 1. The types and distribution of functional groups on the surface of the modified activated carbon are determined by Bohem titration analysis, and the results are shown in Table 2.

[0040] Example 2

[0041] The method for recovering toluenediamine from toluenediamine tar of the present embodiment is as follows:

[0042] S1. After dissolving toluenediamine tar with acetone a, free toluenediamine is adsorbed with modified activated carbon (nitric acid modified activated carbon), and after filtering, filtrate A and filter residue A are obtained; the amount ratio of toluenediamine tar, acetone a and modified activated carbon is 10g:50mL:12g;

[0043] S2, adjusting the pH value of the filtrate A obtained in S1 to 2 with a 98% sulfuric acid aqueous solution, then adding a 72g / L ferrous nitrate aqueous solution and a 30% H2O2 aqueous solution, performing degradation reaction under ultrasonic conditions of a temperature of 20°C and an ultrasonic frequency of 40kHz for 1 hour, and filtering to obtain a filtrate B; the mass ratio of the 72g / L ferrous nitrate aqueous solution to the 30% H2O2 aqueous solution is 1:10;

[0044] S3, extracting the filtrate B obtained in S2 with an extractant (chloroform) three times, collecting the extract phase, evaporating it at a temperature of 40° C., evaporating the acetone in the extract phase, and obtaining a toluenediamine product A;

[0045] S4, adding acetone b to the filter residue A obtained in S1 at a temperature of 20°C, performing analytical regeneration for 50 minutes, filtering, obtaining a filtrate C, evaporating at a temperature of 40°C, and obtaining a toluenediamine product B after evaporating the acetone; the usage ratio of the filter residue A to acetone b is 1 g:5 mL;

[0046] S5. Combine the toluenediamine product A described in S3 and the toluenediamine product B described in S4 to obtain a toluenediamine product.

[0047] The calculation method of unit adsorption capacity, adsorption selectivity and total yield of toluenediamine is the same as that of Example 1. The experimental results are shown in Table 1. The types and distribution of functional groups on the surface of modified activated carbon were determined by Bohem titration analysis, and the results are shown in Table 2.

[0048] Example 3

[0049] The method for recovering toluenediamine from toluenediamine tar of the present embodiment is as follows:

[0050] S1. Dissolve toluenediamine tar with acetone a, adsorb free toluenediamine with modified activated carbon (sodium hydroxide modified activated carbon), and obtain filtrate A and filter residue A after filtering; the amount ratio of toluenediamine tar, acetone a and modified activated carbon is 10g:50mL:12g;

[0051] S2, adjusting the pH value of the filtrate A obtained in S1 to 4 with a 98% sulfuric acid aqueous solution, then adding a 72g / L ferrous nitrate aqueous solution and a 30% H2O2 aqueous solution, performing degradation reaction under ultrasonic conditions of a temperature of 40°C and an ultrasonic frequency of 60kHz for 1.5h, and filtering to obtain a filtrate B; the mass ratio of the 72g / L ferrous nitrate aqueous solution to the 30% H2O2 aqueous solution is 1:15;

[0052] S3, extracting the filtrate B obtained in S2 with an extractant (carbon tetrachloride) three times, collecting the extract phase, evaporating it at a temperature of 50° C., and evaporating the carbon tetrachloride in the extract phase to obtain a toluenediamine product A;

[0053] S4, adding acetone b to the filter residue A obtained in S1 at a temperature of 40°C, performing analytical regeneration for 60 minutes, filtering, obtaining a filtrate C, evaporating at a temperature of 70°C, and obtaining a toluenediamine product B after evaporating the acetone; the usage ratio of the filter residue A to acetone b is 1 g:5 mL;

[0054] S5. Combine the toluenediamine product A described in S3 and the toluenediamine product B described in S4 to obtain a toluenediamine product.

[0055] The calculation method of unit adsorption capacity, adsorption selectivity and total yield of toluenediamine is the same as that of Example 1. The experimental results are shown in Table 1. The types and distribution of functional groups on the surface of modified activated carbon were determined by Bohem titration analysis, and the results are shown in Table 2.

[0056] Example 4

[0057] The method for recovering toluenediamine from toluenediamine tar of the present embodiment is as follows:

[0058] S1. Dissolve toluenediamine tar with acetone a, adsorb free toluenediamine with modified activated carbon (ammonia modified activated carbon), and obtain filtrate A and filter residue A after filtering; the amount ratio of toluenediamine tar, acetone a and modified activated carbon is 10g:50mL:12g;

[0059] S2, adjusting the pH value of the filtrate A obtained in S1 to 6.5 with a 98% sulfuric acid aqueous solution, then adding a 72g / L ferrous nitrate aqueous solution and a 30% H2O2 aqueous solution, performing degradation reaction under ultrasonic conditions of a temperature of 50°C and an ultrasonic frequency of 80kHz for 2 hours, and filtering to obtain a filtrate B; the mass ratio of the 72g / L ferrous nitrate aqueous solution to the 30% H2O2 aqueous solution is 1:20;

[0060] S3, extracting the filtrate B obtained in S2 with an extractant (carbon tetrachloride) three times, collecting the extract phase, evaporating it at a temperature of 20° C., and evaporating the carbon tetrachloride in the extract phase to obtain a toluenediamine product A;

[0061] S4, adding acetone b to the filter residue A obtained in S1 at a temperature of 50°C, performing analytical regeneration for 40 minutes, filtering to obtain a filtrate C, evaporating at a temperature of 20°C, and obtaining a toluenediamine product B after evaporating the acetone; the usage ratio of the filter residue A to acetone b is 1 g:5 mL;

[0062] S5. Combine the toluenediamine product A described in S3 and the toluenediamine product B described in S4 to obtain a toluenediamine product.

[0063] The calculation method of unit adsorption capacity, adsorption selectivity and total yield of toluenediamine is the same as that of Example 1. The experimental results are shown in Table 1. The types and distribution of functional groups on the surface of modified activated carbon were determined by Bohem titration analysis, and the results are shown in Table 2.

[0064] Example 5

[0065] The method for recovering toluenediamine from toluenediamine tar of the present embodiment is as follows:

[0066] S1. After dissolving toluenediamine tar with acetone a, free toluenediamine is adsorbed with modified activated carbon (acetic acid modified activated carbon), and after filtering, filtrate A and filter residue A are obtained; the amount ratio of toluenediamine tar, acetone a and modified activated carbon is 10g:50mL:12g;

[0067] S2, adjusting the pH value of the filtrate A obtained in S1 to 2 with a 98% sulfuric acid aqueous solution, then adding a 72g / L ferrous nitrate aqueous solution and a 30% H2O2 aqueous solution, performing degradation reaction under ultrasonic conditions of a temperature of 30°C and an ultrasonic frequency of 40kHz for 1 hour, and filtering to obtain a filtrate B; the mass ratio of the 72g / L ferrous nitrate aqueous solution to the 30% H2O2 aqueous solution is 1:35;

[0068] S3, extracting the filtrate B obtained in S2 with an extractant (chloroform) three times, collecting the extract phase, evaporating it at a temperature of 50° C., and evaporating the chloroform in the extract phase to obtain a toluenediamine product A;

[0069] S4, adding acetone b to the filter residue A obtained in S1 at a temperature of 30°C, performing analytical regeneration for 60 minutes, filtering, obtaining a filtrate C, evaporating at a temperature of 50°C, and obtaining a toluenediamine product B after evaporating the acetone; the usage ratio of the filter residue A to acetone b is 1 g:5 mL;

[0070] S5. Combine the toluenediamine product A described in S3 and the toluenediamine product B described in S4 to obtain a toluenediamine product.

[0071] The calculation method of unit adsorption capacity, adsorption selectivity and total yield of toluenediamine is the same as that of Example 1. The experimental results are shown in Table 1. The types and distribution of functional groups on the surface of modified activated carbon were determined by Bohem titration analysis, and the results are shown in Table 2.

[0072] Comparative Example 1

[0073] The method for recovering toluenediamine from toluenediamine tar of this comparative example is as follows:

[0074] S1. Dissolve toluenediamine tar with acetone a, adsorb free toluenediamine with unmodified activated carbon, and obtain filtrate A and filter residue A after filtering; the amount ratio of toluenediamine tar, acetone a and modified activated carbon is 10g:50mL:12g;

[0075] S2, adjusting the pH value of the filtrate A obtained in S1 to 2 with a 98% sulfuric acid aqueous solution, then adding a 72g / L ferrous nitrate aqueous solution and a 30% H2O2 aqueous solution, performing degradation reaction at a temperature of 30°C without ultrasonic assistance for 1 hour, and filtering to obtain a filtrate B; the mass ratio of the 72g / L ferrous nitrate aqueous solution to the 30% H2O2 aqueous solution is 1:10;

[0076] S3, extracting the filtrate B obtained in S2 with an extractant (dichloromethane) three times, collecting the extract phase, evaporating it at a temperature of 40° C., and evaporating the dichloromethane in the extract phase to obtain a toluenediamine product A;

[0077] S4, adding acetone b to the filter residue A obtained in S1 at a temperature of 20°C, performing analytical regeneration for 50 minutes, filtering, obtaining a filtrate C, evaporating at a temperature of 50°C, and obtaining a toluenediamine product B after evaporating the acetone; the usage ratio of the filter residue A to acetone b is 1 g:5 mL;

[0078] S5. Combine the toluenediamine product A described in S3 and the toluenediamine product B described in S4 to obtain a toluenediamine product.

[0079] The calculation method of unit adsorption capacity, adsorption selectivity and total yield of toluenediamine is the same as that of Example 1. The experimental results are shown in Table 1. The types and distribution of functional groups on the surface of modified activated carbon were determined by Bohem titration analysis, and the results are shown in Table 2.

[0080] Comparative Example 2

[0081] The method for recovering toluenediamine from toluenediamine tar of this comparative example is as follows:

[0082] S1. Dissolve toluenediamine tar with acetone a, adsorb free toluenediamine with unmodified activated carbon, and obtain filtrate A and filter residue A after filtering; the amount ratio of toluenediamine tar, acetone a and modified activated carbon is 10g:50mL:12g;

[0083] S2, adjusting the pH value of the filtrate A obtained in S1 to 2 with a 98% sulfuric acid aqueous solution, performing a degradation reaction under ultrasonic conditions of a temperature of 20° C. and an ultrasonic frequency of 40 kHz for 1 hour, and filtering to obtain a filtrate B;

[0084] S3, extracting the filtrate B obtained in S2 with an extractant (dichloromethane) three times, collecting the extract phase, evaporating it at a temperature of 40° C., and evaporating the dichloromethane in the extract phase to obtain a toluenediamine product A;

[0085] S4, adding acetone b to the filter residue A obtained in S1 at a temperature of 20°C, performing analytical regeneration for 50 minutes, filtering, obtaining a filtrate C, evaporating at a temperature of 40°C, and obtaining a toluenediamine product B after evaporating the acetone; the usage ratio of the filter residue A to acetone b is 1 g:5 mL;

[0086] S5. Combine the toluenediamine product A described in S3 and the toluenediamine product B described in S4 to obtain a toluenediamine product.

[0087] The calculation method of unit adsorption capacity, adsorption selectivity and total yield of toluenediamine is the same as that of Example 1. The experimental results are shown in Table 1. The types and distribution of functional groups on the surface of modified activated carbon were determined by Bohem titration analysis, and the results are shown in Table 2.

[0088] Table 1 Experimental results of Examples 1-5 and Comparative Examples 1-2

[0089]

[0090] Table 2 Types and quantities of functional groups on the surface of activated carbon in Examples 1-5 and Comparative Examples 1-2

[0091]

[0092] In Examples 1-5, the selective chemical adsorption characteristics of modified activated carbon are first used to remove free toluenediamine from toluenediamine tar. The pore structure of the activated carbon mainly affects the total adsorption capacity of the activated carbon for toluenediamine tar, while the surface functional groups of the activated carbon affect the selectivity of toluenediamine. The modified activated carbon can not only increase the specific surface area of ​​the activated carbon, but also change the distribution of the surface groups accordingly, which has a favorable effect on the adsorption selection of toluenediamine. Under the optimal conditions, the selectivity of the acetic acid-modified activated carbon for toluenediamine reaches 90.10% to 98.48%.

[0093] Example 1-5: Toluenediamine tar free heavy components were removed by using ultrasound, Fe 2+ , H2O2 synergistically generate hydroxyl radicals, and the heavy components of azo dimers in toluenediamine tar are degraded into toluenediamine through hydroxyl radicals. The degradation effect of hydroxyl radicals is used to break the -N=N- bond of the heavy components of toluenediamine tar to obtain toluenediamine, thereby recycling toluenediamine from the heavy components of toluenediamine tar. The degradation rate of the heavy components of toluenediamine tar can reach 75.4% to 79.8%, and the method has the characteristics of mild experimental conditions and simple operation. On the one hand, the free toluenediamine in toluenediamine tar is recycled, and on the other hand, the heavy components in toluenediamine tar are degraded and recycled, which is beneficial to the recycling, reduction and harmless recycling of toluenediamine tar, and the goals of economic benefits and environmental protection are achieved, providing a new way for the resource utilization and reduction of toluenediamine tar.

[0094] The above is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any simple modification, change and equivalent change made to the above embodiment according to the technical essence of the invention still falls within the protection scope of the technical solution of the present invention.

Claims

1. A method for recovering toluenediamine from toluenediamine tar, characterized in that: The method is: S1. Dissolve toluenediamine tar with acetone a, adsorb free toluenediamine with modified activated carbon, and obtain filtrate A and filter residue A after filtering; the modified activated carbon in S1 is acetic acid modified activated carbon, nitric acid modified activated carbon, sodium hydroxide modified activated carbon or ammonia modified activated carbon; S2, adjusting the pH value of the filtrate A obtained in S1 to 0.5-6.5 with a 98% sulfuric acid aqueous solution, then adding a 72g / L ferrous nitrate aqueous solution and a 30% H2O2 aqueous solution, performing a degradation reaction under ultrasonic conditions at a temperature of 20°C-50°C, and filtering to obtain a filtrate B; S3, extracting the filtrate B obtained in S2 with an extractant three times, collecting the extract phase, and evaporating the extractant in the extract phase to obtain a toluenediamine product A; S4, adding acetone b to the filter residue A obtained in S1 at a temperature of 20°C to 50°C for analytical regeneration, filtering to obtain a filtrate C, and evaporating the acetone to obtain a toluenediamine product B; S5. Combine the toluenediamine product A described in S3 and the toluenediamine product B described in S4 to obtain a toluenediamine product.

2. A method for recovering toluenediamine from toluenediamine tar according to claim 1, characterized in that: The dosage ratio of toluenediamine tar, acetone a and modified activated carbon in S1 is 10g:50mL:12g.

3. According to the method for recovering toluenediamine from toluenediamine tar described in claim 1, the mass ratio of the ferrous nitrate aqueous solution with a mass concentration of 72g / L and the H2O2 aqueous solution with a mass fraction of 30% in S2 is 1:(5-35).

4. A method for recovering toluenediamine from toluenediamine tar according to claim 1, characterized in that: The ultrasonic frequency in the degradation reaction in S2 is 20kHz to 80kHz, and the degradation reaction time is 0.5h to 2h.

5. A method for recovering toluenediamine from toluenediamine tar according to claim 1, characterized in that: The extractant in S3 is dichloromethane, chloroform or carbon tetrachloride.

6. A method for recovering toluenediamine from toluenediamine tar according to claim 1, characterized in that: The evaporation temperature in S3 is 20°C to 50°C.

7. A method for recovering toluenediamine from toluenediamine tar according to claim 1, characterized in that: The usage ratio of the filter residue A and acetone b in S4 is 1 g:5 mL.

8. A method for recovering toluenediamine from toluenediamine tar according to claim 1, characterized in that: The time for the analytical regeneration in S4 is 40 min to 60 min.

9. A method for recovering toluenediamine from toluenediamine tar according to claim 1, characterized in that: The evaporation temperature in S4 is 20°C to 70°C.

Citation Information

Patent Citations

  • Method for manufacturing toluylendiamines through catalytic hydration of dinitrotoluols

    CN103524356A

  • Dinitrotoluene hydrogenated tar recycling system

    CN203222566U

  • Process for the separation of high-boiling materials from the reaction mixture generated during the production of diaminotoluene

    US5728880A

  • Method for recovering m-diaminotoluene from dinitrotoluene hydrogenated tar

    CN101875614A

  • Method for recycling meta-toluenediamine from dinitrotoluene hydrogenated tar

    CN104058973A