Ideal radiation parameter testing method, system, 3D printing method and printing equipment
By using a combination of test patterns and connection patterns in 3D printing, the ideal radiation parameters of the energy radiation device are determined, which solves the problem of insufficient molding or over-curing of printing materials, improves printing quality and efficiency, and simplifies the parameter correction process.
Patent Information
- Application Number
- CN202210867862.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-07-22
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2042-07-22
AI Technical Summary
During the 3D printing process, it is difficult to determine the ideal radiation parameters, resulting in insufficient molding or over-curing of the printed material, affecting the quality and mechanical properties of the component.
By sequentially radiating different test patterns and connection patterns on the printing surface, an integrated molding structure is formed, and the ideal radiation parameters of the energy radiation device are determined based on the molding parameters of the molded block, including using the test images and connection patterns to adjust the radiation parameters with different grayscale values. .
It improves the molding effect of printing materials, simplifies the testing process of radiation parameters, avoids repeated printing and pickup operations, and can correct the power of energy radiation devices without the need for professional equipment and personnel.
Smart Images

Figure CN115256938B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of 3D printing technology, and specifically to an ideal radiation parameter testing method for an energy radiation device, an ideal radiation parameter testing system for an energy radiation device, a 3D printing method, a 3D printing device, an image generation method, and an image generation system. Background Art
[0002] 3D printing is a technology that uses digital model files as the basis and uses powdered metal, plastic, resin and other printing materials to construct objects by printing layer by layer. During printing, it uses radiation energy to shape the printing materials.
[0003] In a photocuring printing device, light energy is radiated to the printing surface through an energy radiating device so that the printing material to be cured on the printing surface is cured and formed after light radiation. Since the molding characteristics of each printing material are different, in order to improve the printing quality, it is necessary to determine how much light energy needs to be provided to the printing material during printing. If the light energy provided is insufficient, it will affect the normal molding, causing printing failure or insufficient strength of the printed component; conversely, if the light energy provided is excessive, it will also lead to over-curing, which will also affect the mechanical properties of the 3D printed component. Summary of the invention
[0004] In view of the shortcomings of the above-mentioned related technologies, the purpose of the present application is to provide a method for overcoming the technical problem of how to determine ideal radiation parameters existing in the above-mentioned related technologies.
[0005] To achieve the above-mentioned purpose and other related purposes, the first aspect disclosed in the present application provides a method for testing ideal radiation parameters of an energy radiation device, comprising the following steps: allowing the energy radiation device to radiate energy to different positions on a printing surface in sequence according to a test pattern, so that the printed material at the corresponding positions on the printing surface is solidified and formed, thereby correspondingly obtaining a plurality of formed blocks; wherein the formed blocks at different positions have different test radiation parameters during radiation; allowing the energy radiation device to radiate energy to the printing surface according to a connection pattern, so that the printed material at the corresponding positions on the printing surface is solidified and formed, thereby correspondingly obtaining a connection block; wherein the connection pattern is used to connect the test patterns, so that the cured connection block connects the plurality of formed blocks to form a pattern solidification layer, and the pattern solidification layer is an integrated molding structure; based on the molding parameters of each molding block in the pattern solidification layer, determining the ideal radiation parameters of the energy radiation device.
[0006] The second aspect disclosed in the present application provides a method for testing ideal radiation parameters of an energy radiation device, comprising the following steps: allowing the energy radiation device to radiate energy onto a printing surface according to a test image to obtain a pattern solidification layer corresponding to the test image on the printing surface, wherein the pattern solidification layer is an integrally formed structure; wherein the test image includes a plurality of test patterns and connecting patterns, wherein the connecting patterns are used to connect the test patterns, and the grayscale values of the test patterns are different; wherein the pattern solidification layer includes a plurality of forming blocks and connecting blocks, wherein the forming blocks are connected by connecting blocks; and determining the ideal radiation parameters of the energy radiation device based on the forming parameters of the forming blocks in the pattern solidification layer and the conversion relationship between the radiation intensity and the grayscale value of the energy radiation device.
[0007] The third aspect disclosed in the present application provides an ideal radiation parameter testing system for an energy radiation device, characterized in that it includes: an interface module, connected to a control device in a 3D printing device, so that the ideal radiation parameter testing system controls the energy radiation device through the control device; a storage module, storing at least one program; a processing module, connected to the interface module and the storage module, for calling the at least one program to control the energy radiation device to determine the ideal radiation parameters of the energy radiation device based on the ideal radiation parameter testing method for the energy radiation device described in any one of the first aspect or the second aspect of the present application.
[0008] The fourth aspect disclosed in the present application provides a 3D printing method for printing an ideal radiation parameter test piece of an energy radiation device in a 3D printing device, wherein the 3D printing device also includes a container for holding printing materials, and the 3D printing method includes the following steps: allowing the energy radiation device to radiate energy to different positions on the printing surface in sequence according to a test pattern, so that the printing materials at the corresponding positions on the printing surface are solidified and formed, thereby correspondingly obtaining a plurality of forming blocks; wherein the forming blocks at different positions have different test radiation parameters during radiation; allowing the energy radiation device to radiate energy to the printing surface according to a connection pattern, so that the printing materials at the corresponding positions on the printing surface are solidified and formed, thereby correspondingly obtaining a connection block; wherein the connection pattern is used to connect the test patterns, so that the connection block after solidification connects the plurality of forming blocks to form a pattern solidification layer, and the pattern solidification layer is an integrally formed structure; taking out the pattern solidification layer from the container to obtain the ideal radiation parameter test piece.
[0009] The fifth aspect disclosed in the present application provides a 3D printing method for printing an ideal radiation parameter test piece of an energy radiation device in a 3D printing device, wherein the 3D printing device also includes a container for holding printing materials, and the 3D printing method includes the following steps: allowing the energy radiation device to radiate energy to a printing surface according to a test image to obtain a pattern solidification layer corresponding to the test image on the printing surface, wherein the pattern solidification layer is an integrally formed structure; wherein the test image includes a plurality of test patterns and a connecting pattern, wherein the connecting pattern is used to connect each test pattern, and each test pattern has a different grayscale value; the pattern solidification layer includes a plurality of forming blocks and connecting blocks, and each forming block is connected by a connecting block; and taking out the pattern solidification layer from the container to obtain the ideal radiation parameter test piece.
[0010] The sixth aspect disclosed in the present application provides a 3D printing device, including: a container for holding printing materials; a component platform, located in the container during a printing operation, for accumulating a solidified layer of an attached pattern layer by layer to form a corresponding 3D component; a Z-axis drive mechanism, connected to the component platform, for adjusting the height of the component platform in the Z-axis direction, so as to adjust the distance from the component platform to a printing surface during a printing operation; an energy radiation device, located above or below the container, for radiating energy to the printing surface in the container; a control device, connected to the energy radiation device and the Z-axis drive mechanism, for controlling the energy radiation device and the Z-axis drive mechanism during a printing operation, so as to accumulate a solidified layer on the component platform to obtain a corresponding 3D component; and, for controlling the energy radiation device to perform a 3D printing method as described in any one of the fourth aspect or the fifth aspect during a test operation.
[0011] In summary, the present application can help determine the ideal radiation parameters when using printing materials, so that the printing materials can exert better performance and the molding effect meets expectations. In addition, the technical solution provided in the present application can avoid repeating the printing, picking up, cleaning, measuring and other processes for each test piece printed when testing the radiation parameters. By connecting the printed test pieces into an integrated structure, each test piece can be taken out in one picking process. In addition, the energy radiation device of the 3D printing equipment may have energy attenuation during use. With the help of the technical solution in the present application, the power of the energy radiation device can be calibrated by the molding parameters of the printed test piece without the need for professional equipment and professionals.
[0012] Those skilled in the art can easily perceive other aspects and advantages of the present application from the detailed description below. In the detailed description below, only exemplary embodiments of the present application are shown and described. As will be appreciated by those skilled in the art, the content of the present application enables those skilled in the art to modify the disclosed specific embodiments without departing from the spirit and scope of the invention to which the present application relates. Accordingly, the description in the drawings and specification of the present application is merely exemplary and not restrictive. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] The specific features of the invention involved in this application are shown in the attached claims. The features and advantages of the invention involved in this application can be better understood by referring to the exemplary embodiments and drawings described in detail below. A brief description of the drawings is as follows:
[0014] Figure 1 It is a schematic diagram showing an ideal radiation parameter testing method of an energy radiation device in the present application in one embodiment;
[0015] Figure 2 It is a simplified structural schematic diagram of a pattern solidification layer in one embodiment of the present application;
[0016] Figure 3 It is a simplified structural schematic diagram of another embodiment of the patterned solidified layer in the present application;
[0017] Figure 4 It is a simplified structural schematic diagram of a pattern solidification layer in another embodiment of the present application;
[0018] Figure 5 It is a simplified structural schematic diagram showing the connection state of the connecting block and the forming block in the present application in one embodiment;
[0019] Figure 6a to Figure 6f Shown is a schematic diagram of the radiation image and the formed patterned cured layer during testing in one embodiment of the present application;
[0020] Figure 7 Shown is a simplified schematic diagram of the hardware architecture of an ideal radiation parameter testing system in one embodiment of the present application;
[0021] Figure 8 It is a schematic diagram showing another embodiment of the ideal radiation parameter testing method in the present application;
[0022] Fig. 9 Shown is a schematic diagram of a 3D printing method in one embodiment of the present application;
[0023] Fig.10 Shown is a simplified structural schematic diagram of a 3D printing device in one embodiment of the present application;
[0024] Fig.11 Shown is a simplified structural schematic diagram of another embodiment of the 3D printing device in this application;
[0025] Fig.12 Shown is a schematic diagram of another embodiment of the 3D printing method in the present application;
[0026] Fig.13 Shown is a schematic diagram of an image generation method in one embodiment of the present application;
[0027] Fig.14 Shown is a schematic diagram of the hardware architecture of an image generation system in one embodiment of the present application. DETAILED DESCRIPTION
[0028] The following is an explanation of the implementation of the present application by means of specific embodiments. People familiar with the art can easily understand other advantages and effects of the present application from the contents disclosed in this specification.
[0029] In the following description, reference is made to the accompanying drawings, which describe several embodiments of the present application. It should be understood that other embodiments may also be used, and that changes in module or unit composition, electrical and operational aspects may be made without departing from the spirit and scope of the present disclosure. The following detailed description should not be considered restrictive, and the scope of the embodiments of the present application is limited only by the claims of the published patents. The terms used herein are only for the purpose of describing specific embodiments and are not intended to limit the present application.
[0030] Furthermore, as used in this article, the singular forms "one", "an" and "the" are intended to include plural forms as well, unless there is an indication to the contrary in the context. It should be further understood that the terms "comprise", "include" indicate the presence of the described features, steps, operations, elements, components, projects, kinds, and / or groups, but do not exclude the presence, occurrence or addition of one or more other features, steps, operations, elements, components, projects, kinds, and / or groups. The terms "or" and "and / or" used herein are interpreted as inclusive, or mean any one or any combination. Therefore, "A, B or C" or "A, B and / or C" means "any of the following: A; B; C; A and B; A and C; B and C; A, B and C". Exceptions to this definition will only occur when the combination of elements, functions, steps or operations is inherently mutually exclusive in some way.
[0031] As described in the background art, in order to improve printing quality, it is necessary to determine how much light energy the energy radiation device needs to provide to the printing material during printing.
[0032] In some embodiments, a radiation parameter can be preset first, and the energy radiation device can be made to project an image onto the printing material in the container based on the preset radiation parameter, so as to obtain a solidified thin layer corresponding to the projected image in the container. After taking out the thin layer, the molding condition of the printing material under the preset radiation parameter can be determined by observing, measuring, etc., so as to adjust the radiation parameters based on the molding condition, and then print another thin layer, repeat observation, measurement, etc., and repeat the process of printing, taking out, observing, measuring, adjusting radiation parameters, etc. until the printed molding condition meets the expected effect.
[0033] However, the testing efficiency is low because the process of printing, picking up, observing, measuring, and adjusting the radiation parameters must be repeated each time a radiation parameter is tested, and the related operation requirements for the operator are also high.
[0034] In view of this, the present application provides a method for testing ideal radiation parameters of an energy radiation device, so as to determine the ideal radiation parameters of the energy radiation device in a simple and easy-to-operate manner.
[0035] The ideal radiation parameter testing method of the energy radiation device can be performed by an ideal radiation parameter testing system of the energy radiation device.
[0036] In an exemplary embodiment, see Figure 7 , which is a brief schematic diagram of the hardware architecture of the ideal radiation parameter testing system in one embodiment of the present application. The ideal radiation parameter testing system 2 includes an interface module 201, a storage module 202, and a processing module 203.
[0037] The interface module 201 determines its interface type according to the connected device, which includes but is not limited to: a universal serial interface, a video interface, an industrial control interface, etc. For example, the interface module 201 may include a USB interface, an HDMI interface, and an RS232 interface, etc. The interface module may be connected to an energy radiation device so as to control the energy radiation device to radiate energy.
[0038] The storage module 202 stores a computer program. Exemplarily, the storage module 202 includes one or more memories, at least part of each of which stores a computer program. Exemplarily, the memory may include a high-speed random access memory, and may also include a non-volatile memory, such as one or more disk storage devices, flash memory devices, or other non-volatile solid-state storage devices. In some embodiments, the memory may also include a memory away from one or more processors, such as a network attached memory accessed via an RF circuit or an external port and a communication network, wherein the communication network may be the Internet, one or more intranets, a local area network, a wide area network, a storage area network, etc., or a suitable combination thereof. The memory controller may control access to the memory by other components of the device, such as a CPU and a peripheral interface.
[0039] The processing module 203 includes: connected to the interface module 201 and the storage module 202, and used to run the computer program to execute the ideal radiation parameter test method of the energy radiation device. Exemplarily, the processing module 203 includes one or more processors coupled to at least one of the storage module and the interface module; the processor may include a general-purpose microprocessor, a dedicated processor, a field programmable logic array, or any combination thereof.
[0040] It should be understood that the 3D printing is a kind of rapid prototyping technology. It is a technology that uses a digital model file as a basis, uses powdered metal or plastic and other bondable materials, and constructs objects by printing layer by layer. When printing, the digital model file is first processed to realize the import of the 3D component model to be printed into the 3D printing device. Here, the 3D component model includes but is not limited to a 3D component model based on a CAD component, which is exemplified by an STL file, and the control device performs layout and layer processing on the imported STL file. The 3D component model can be imported into the control device through a data interface or a network interface. The entity part in the imported 3D component model can be of any shape, for example, the entity part includes a tooth shape, a sphere shape, a house shape, a tooth shape, or any shape with a preset structure. Among them, the preset structure includes but is not limited to at least one of the following: a cavity structure, a structure containing a sudden change in shape, and a structure with preset requirements for the contour accuracy in the entity part. The 3D printing device prints the 3D component by exposing and curing the photocurable material layer by layer and accumulating each cured layer.
[0041] In an exemplary embodiment, the 3D printing device includes a container, an energy radiation device, a component platform, a Z-axis drive mechanism, and a control device. The container is used to hold the printing material to be cured, and the energy radiation device is arranged at a preset position on one side of the top or bottom of the container.
[0042] It should be understood that the 3D printing device described in the present application may include two states: printing operation and testing operation. The printing operation includes the process of solidifying the printing material layer by layer to form a 3D component, and the testing operation includes the process of printing a test piece according to the ideal radiation parameter testing method to determine the ideal radiation parameters of the energy radiation device.
[0043] During the printing operation, the energy radiation device radiates energy to the printing surface located in the container to solidify the material to be solidified located on the printing surface to obtain a solidified layer. The component platform is located in the container during the printing operation, and is used to attach and carry the formed solidified layer so as to accumulate and form a 3D component through the solidified layer. The Z-axis driving mechanism is connected to the component platform and is used to drive the component platform to move in the Z-axis direction. The control device is connected to the energy radiation device and the Z-axis driving mechanism, and is used to control the energy radiation device and the Z-axis driving mechanism during the printing operation to attach and accumulate the solidified layer on the component platform to obtain the corresponding 3D component.
[0044] In the test operation, the energy radiation device radiates energy onto the printing surface located in the container to solidify the printing material on the printing surface. A pattern solidification layer printed in the test operation includes multiple molding blocks. The ideal radiation parameters of the energy radiation device can be determined through the molding parameters of each molding block.
[0045] It should be understood that the radiation parameters include relevant parameters of the energy radiation device when radiating energy, including but not limited to radiation time and radiation intensity. The radiation time is the duration of the energy radiation device radiating energy, and the radiation intensity is the energy value radiated by the energy radiation device per unit time. The radiation intensity can be achieved by adjusting the current of the energy radiation device.
[0046] Among them, the 3D printing device can be classified according to the setting position of the energy radiation device, and can be a 3D printing device with top radiation molding or a 3D printing device with bottom radiation molding. In the 3D printing device with top radiation molding, the energy source, that is, the energy radiation device, is located above the container in the 3D printing device, and radiates energy to the printing material in the container during the printing process; in the 3D printing device with bottom radiation molding, the energy source is located below the container in the 3D printing device, and radiates energy to the printing material in the container during the printing process. Specifically, in the embodiment of the 3D printing device being a 3D printing device with top radiation molding, the energy radiation device is located above the container, and the printing surface is usually located on the liquid surface of the photocurable material in the container. During the printing operation, the energy radiation device radiates energy to the printing surface located in the container to cure the material to be cured located on the printing surface. After printing a layer, the Z-axis drive mechanism controls the component platform to move downward by a printing height to continue printing on the first cured layer. In the embodiment of the 3D printing device with bottom radiation molding, the energy radiation device is located below the container, and the printing surface is usually located on the lower surface of the photocurable material in the container. During the printing operation, the energy radiation device radiates energy to the printing surface in the container to solidify the to-be-solidified material on the printing surface. After printing a layer, the Z-axis driving mechanism controls the component platform to move upward by a certain distance to separate the first solidified layer from the bottom of the container, and controls the Z-axis driving mechanism to control the component platform to move to the next printing height to continue printing on the first solidified layer.
[0047] It should be understood that the printing surface is the horizontal surface of the material to be molded, and in some embodiments is also referred to as the printing reference surface. Typically, the printing surface is located in the container, and the distance between the printing surface and the exit position of the energy radiation device is determined based on the focal length of the energy radiation device. In some embodiments, such as in a 3D printing device for top surface radiation molding, the printing surface is located above the liquid surface of the photocurable material contained in the container; in other embodiments, such as in a 3D printing device for bottom surface radiation molding, the printing surface may also be located at a position below the liquid surface of the photocurable material.
[0048] The 3D printing equipment can be classified into point scanning molding and surface exposure molding printing equipment according to the exposure principle. Examples of point scanning molding printing equipment include but are not limited to SLA (Stereolithography Apparatus) equipment with laser spot scanning, and examples of surface exposure molding printing equipment include but are not limited to DLP (Digital Light Procession, digital light processing, abbreviated as DLP) equipment and LCD (Liquid Crystal Display, liquid crystal surface light source curing, abbreviated as LCD) equipment.
[0049] For SLA printing equipment, the energy radiation device includes a laser emitter, a lens group located on the light path of the laser emitter, and a galvanometer group located on the light output side of the lens group, wherein the laser emitter is controlled to adjust the energy of the output laser beam, for example, the laser emitter is controlled to emit a laser beam of preset power and stop emitting the laser beam, and for another example, the laser emitter is controlled to increase the power of the laser beam and reduce the power of the laser beam. The lens group is used to adjust the focus position of the laser beam, and the galvanometer group is used to controllably scan the laser beam in the two-dimensional space of the top surface of the container, and the light-curable material scanned by the light beam is cured into a corresponding patterned cured layer.
[0050] In the DLP printing device, the energy radiation device includes, for example, a DMD chip, a controller and a storage module. The storage module stores a layered image that layers the 3D component model. After receiving the control signal from the controller, the DMD chip irradiates the light source of each pixel on the corresponding layered image to the top surface of the container. The DMD chip looks like a small mirror, which is encapsulated in a closed space composed of metal and glass. In fact, this mirror is composed of hundreds of thousands or even millions of micromirrors, each of which represents a pixel, and the projected image is composed of these pixels. The DMD chip can be simply described as a semiconductor optical switch and micro-lens corresponding to the pixel point. The controller allows / disables each microchip to reflect light by controlling each optical switch in the DMD chip, thereby irradiating the corresponding layered image to the photocurable material through the transparent top of the container, so that the photocurable material corresponding to the image shape is cured to obtain a patterned cured layer.
[0051] In the LCD printing device, the energy radiation device is an LCD screen light source system. The LCD screen light source system includes an LCD screen located above the container and a light source arranged above the LCD screen. The control chip in the energy radiation device projects the layered image of the slice to be printed onto the printing surface through the LCD screen, and uses the pattern radiation surface provided by the LCD screen to cure the material to be cured in the container into a corresponding pattern cured layer.
[0052] Based on the above description, it can be understood that, for SLA printing equipment, the energy radiated is the laser beam; for surface exposure printing equipment such as DLP and LCD, the energy radiated is the projection image with brightness.
[0053] In an exemplary embodiment, see Figure 1, which is a schematic diagram of an ideal radiation parameter test method of the energy radiation device in the present application in one embodiment. As shown in the figure, in step S110, the energy radiation device is made to radiate energy to different positions on the printing surface in sequence according to the test pattern, so that the printing material at the corresponding position on the printing surface is solidified and formed, thereby correspondingly obtaining a plurality of formed blocks; wherein the test radiation parameters of the formed blocks at different positions during radiation are different.
[0054] Here, the multiple molding blocks are multiple test pieces to be printed, and the shape of each molding block is determined by the test pattern corresponding to each molding block. For SLA printing equipment, after processing each test pattern into a scanning path, the energy radiation device in the 3D printing equipment is scanned based on the scanning path to shape the scanned printing material, thereby forming a molding block corresponding to the test pattern on the printing surface; for surface exposure printing equipment, the energy radiation device is projected onto the printing surface, thereby forming a molding block corresponding to the test pattern on the printing surface.
[0055] The test pattern may be in any shape, such as a square, a circle, a triangle or an irregular shape, as long as the printed molding block can be easily observed or measured. The shapes of different test patterns may be consistent or inconsistent. In some embodiments, test patterns of various shapes may be preset in the ideal radiation parameter test system of the energy radiation device. When the user needs to test the ideal radiation parameters of the energy radiation device, one or more of the preset test patterns may be selected.
[0056] It should be understood that, in this embodiment, each molding block is printed in sequence and then taken out at the same time, so when printing different molding blocks, it is necessary to make the energy radiation device radiate energy to different positions on the printing surface so that the printed materials at these positions are cured and formed after radiation, and corresponding molding blocks are obtained at these positions respectively.
[0057] Here, since the energy radiated by the energy radiation device is determined by multiple factors, it is necessary to adjust the variable parameters corresponding to these factors to observe under which parameters the molding effect is more ideal. Based on this understanding, when printing different molding blocks, printing can be performed according to different radiation parameters. The radiation parameters in this process are defined as test radiation parameters, that is, radiation parameters set only in the test stage to observe the molding effects under different radiation parameters.
[0058] In some embodiments, since the test radiation parameters corresponding to each molding block are different during radiation, after printing a molding block, it is necessary to readjust the test radiation parameters of the energy radiation device to the test radiation parameters corresponding to the next molding block before printing the next molding block. In some embodiments, in the test radiation parameters corresponding to each molding block, the radiation intensity is consistent but the radiation time is different, then the radiation intensity does not need to be adjusted, and only the time of each radiation needs to be adjusted; in other embodiments, in the test radiation parameters corresponding to each molding block, the radiation intensity is different but the radiation time is consistent, then the radiation time does not need to be adjusted, and the intensity of each radiation needs to be adjusted; in some other embodiments, in the test radiation parameters corresponding to each molding block, the radiation intensity and the radiation time are different, then both the radiation time and the radiation intensity need to be adjusted.
[0059] Please continue reading Figure 1 In step S120, the energy radiation device is made to radiate energy to the printing surface according to the connection pattern, so that the printing material at the corresponding position on the printing surface is solidified and formed, thereby obtaining a corresponding connection block; wherein the connection pattern is used to connect each test pattern, so that the connection block after solidification connects the multiple forming blocks to form a pattern solidification layer, and the pattern solidification layer is an integrated molding structure.
[0060] Here, in order to facilitate simultaneous removal of the multiple molding blocks printed in step S110, the molding blocks are connected to form an integrated molding structure, that is, the multiple molding blocks form a whole, so that the multiple molding blocks can be taken out simultaneously when removing.
[0061] Wherein, the connecting block is used to connect each molding block to each other. In some embodiments, each molding block can be connected by a connecting block, for example, molding block a and molding block b are connected only by a connecting block. In other embodiments, each molding block can be connected by multiple connecting blocks, for example, molding block a' and molding block b' are connected by two or more connecting blocks. Of course, in some cases, some molding blocks can be connected by a connecting block, or all molding blocks can be connected by a connecting block, or all molding blocks can be connected by multiple connecting blocks, as long as the molding blocks can be connected to form an integrated molding structure by connecting blocks. After the molding blocks are connected by connecting blocks, a pattern solidification layer is formed.
[0062] It should be understood that the one-piece molding structure includes an integrated structure, which means that multiple components are integrated into one and cannot be physically separated by non-destructive means. In this embodiment, it includes multiple molding blocks and connecting blocks that are printed into one and cannot be physically separated by non-destructive means.
[0063] It is understood that the position and shape of the cured connection block are determined by the position and shape of the connection pattern. Therefore, in order for the connection block to connect multiple molding blocks, the connection pattern needs to connect each test pattern. In some embodiments, each detection pattern can be connected by a connection pattern, for example, the detection pattern a and the detection pattern b are connected by only one connection pattern. In other embodiments, each detection pattern can be connected by multiple connection patterns, for example, the detection pattern a' and the detection pattern b' are connected by two or more connection patterns.
[0064] In an exemplary embodiment, in order to facilitate the connection between the molding blocks, the connection pattern can connect adjacent test patterns, so that the connection block formed after printing can also connect adjacent molding blocks. Figure 2 , which is a simplified structural diagram of the pattern solidification layer in one embodiment of the present application. As shown in the figure, each adjacent molding block 31 is regularly connected by a connecting block 32, thereby forming an integrated molding structure.
[0065] Of course, the connecting blocks do not have to be connected in the same way as the adjacent forming blocks, as long as the forming blocks can be connected into an integral forming structure through the connection of the connecting blocks. Figure 3 , which is a simplified structural diagram of the pattern solidification layer in another embodiment of the present application. As shown in the figure, each forming block 31 is connected by a connecting block 32. Figure 2 The corresponding embodiments adopt a different connection method, but it ensures that each molding block is connected to form an integral molding structure.
[0066] In some embodiments, see Figure 4 , which is a simplified structural schematic diagram of the pattern solidification layer in another embodiment of the present application. As shown in the figure, each forming block 31 is connected by a plurality of connecting blocks 32, and the connecting blocks 32 connect each forming block through an external frame and internal branches, thereby forming an integrated forming structure.
[0067] In this embodiment, by radiating energy between the plurality of forming blocks, the portions between the plurality of forming blocks are also solidified, and a connection relationship is generated between the plurality of forming blocks. Here, the shape of the connection pattern is not specifically limited, as long as the forming blocks can be connected by the connection block to form an integral structure of the dispersed forming blocks, and the connection block can be a long strip, an hourglass shape, etc.
[0068] Here, the obtained pattern solidified layer is usually an integrally formed thin layer structure, which includes the printed forming blocks and connecting blocks. In addition, since the radiation parameters used in the printing of each forming block are different, the thickness of each forming block may also be different.
[0069] In some embodiments, in order to ensure the connection strength between the connecting block and the forming block, there is an overlapping portion between the connecting pattern and the connected test pattern, the overlapping area of the overlapping portion is less than 10% of the area of each connected test pattern, and the overlapping portion is located at the edge of each connected test pattern.
[0070] The overlapped portion refers to the overlapped projection of the connection pattern and the test pattern. To avoid the influence of the connection block on the main structure of the forming block after printing, the overlapped portion can be less than 10% of the area of each connected test pattern and the overlapped portion is located at the edge of each connected test pattern. In other words, for the connection pattern and the test pattern that generate a connection relationship, there is an overlapped portion of less than 10% of the area of the test pattern at the connection between the two.
[0071] See also Figure 5 , which is a simplified structural diagram showing the connection state of the connection block and the forming block in the present application in one embodiment. The connection pattern 42 and the test pattern 41 have an overlapped portion, namely the shaded portion in the figure, which is located at the edge of the test pattern 41.
[0072] In a possible implementation, there is an overlapping portion between the connection pattern and the connected test pattern, the overlapping area of the overlapping portion is less than 10% of the area of each connected test pattern, and the overlapping portion is located at the edge of each connected test pattern, and the connection pattern connects adjacent test patterns, and, in order to avoid the connection structure being too long and easy to break, the spacing between adjacent test patterns is not greater than 1 / 2 of the length or width of any one of the adjacent test patterns.
[0073] Specifically, when two adjacent test patterns are connected by a connection pattern, the length of the connection pattern is not greater than 1 / 2 of the length or width of any one of the connected test patterns. For example, test pattern a and test pattern b are adjacent, the length of test pattern a is L1 and the width is W1, and the length of test pattern b is L2 and the width is W2. When test pattern a and test pattern b are connected by a connection pattern, in order to avoid the connection block from being easily broken, the spacing between test pattern a and test pattern b can be set to be less than or equal to both. Of course, in some embodiments, the length and / or width of the test pattern may be adjusted based on the spacing between adjacent test patterns so that the spacing between adjacent test patterns is not greater than 1 / 2 of the length or width of any of the adjacent test patterns.
[0074] In an exemplary embodiment, in order to avoid the connection failure between the connecting block and the forming block, it is necessary to ensure that the connecting block can be successfully cured. Therefore, when radiating the connecting pattern, it is necessary to ensure that the radiated energy should meet the minimum forming requirements of the printing material. In some embodiments, the connecting pattern can also be directly radiated according to the strongest radiation intensity of the energy radiation device, so as to ensure that the connecting block can be successfully printed. In addition, since the function of the connecting block is mainly to connect the forming blocks, the radiation parameters of each connecting block can be the same. In an embodiment in which the 3D printing device is a surface exposure printing device, part of the connecting pattern can be projected at the same time. In an embodiment in which the 3D printing device is an SLA printing device, since the laser spot needs to scan and cure while moving, although it is impossible to project simultaneously like a surface exposure device, scanning and curing can also be completed in continuous movement, that is, there is no need to adjust the radiation parameters and then scan again.
[0075] Please continue reading Figure 1 In step S130, based on the molding parameters of each molding block in the pattern solidification layer, the ideal radiation parameters of the energy radiation device are determined.
[0076] Here, the molding parameters of each molding block in the pattern curing layer symbolize the molding conditions of the printed material under the corresponding radiation parameters, so the ideal radiation parameters can be determined based on the comparison between the molding parameters of each molding block and the desired molding parameters. For example, the molding parameters of molding block a are closest to the desired molding parameters, but the thickness still differs by 10%. Then, the radiation intensity or radiation time can be appropriately increased based on the test radiation parameters corresponding to molding block a during radiation to serve as the ideal radiation parameters.
[0077] In one embodiment, according to the comparison between the actual molding parameters of each molding block and the expected molding parameters, the test radiation parameters corresponding to the molding block with the closest comparison result can be used as the ideal radiation parameters of the energy radiation device. The actual molding parameters are the molding parameters actually presented by the printed molding blocks, and the expected molding parameters are the molding parameters presented by the expected molding blocks. For example, among the printed molding blocks a, molding blocks b, molding blocks c, molding blocks d, and molding blocks e, the actual molding parameters of molding block d are closest to the expected molding parameters, and the test radiation parameters of molding block d during radiation can be used as the ideal radiation parameters of the energy radiation device.
[0078] In an exemplary embodiment, the radiation parameters include radiation time and radiation intensity, and therefore the test radiation parameters also include radiation time and radiation intensity, that is, when radiating energy according to each test pattern, the test radiation parameters include control of radiation time and radiation intensity, and the ideal radiation parameters finally determined also include radiation time and radiation intensity.
[0079] It should be understood that for SLA printing equipment, the energy it radiates is the laser beam, its radiation intensity is the energy of the laser beam, and the radiation time is the residence time of the laser beam at each scanning point; for surface exposure printing equipment such as DLP and LCD, its radiation energy is the projected image with brightness, and the radiation time is the projection duration of the projected image.
[0080] The ideal radiation parameters refer to radiation parameters suitable for making the printed material meet the molding requirements. The ideal radiation parameters can be a certain interval, for example, the radiation time is between T1 and T2, and the radiation intensity is between P1 and P2. In some cases with higher precision, the ideal radiation parameters can also be a specific value, for example, the radiation time = T3, the radiation intensity = P3.
[0081] In an exemplary embodiment, the degree of curing can generally be reflected in the thickness, strength, color, etc. of the printed material after molding. Therefore, in some embodiments, the molding parameters of the molding block include one or more of the molding thickness, molding color, and molding hardness of the molding block. For example, in some embodiments, the penetration (radiation depth) of the printed material is different under different radiation energies, so the molding parameters of each molding block can be determined by measuring the molding thickness of each molding block; for example, in other embodiments, the printed material will show different colors under different degrees of curing, and the molding parameters of each molding block can be determined by comparing the colors of each molding block; for example, in some other embodiments, the printed material will show different structural stresses under different degrees of curing, so the molding parameters of each molding block can be determined by comparing the hardness of each molding block; of course, in some embodiments, the molding parameters of each molding block can also be determined by combining the molding thickness, molding color, and molding hardness at the same time.
[0082] It should be understood that in some cases, different printing materials have different components, and the molding effects after being irradiated with the same light energy are also different. Therefore, in some embodiments, each printing material has its own corresponding ideal radiation parameters. Through the ideal radiation parameter testing method in this application, the most ideal radiation parameters for a certain energy radiation device can be determined for each printing material, so that when the energy radiation device is used to print the printing material, a more ideal printing effect can be achieved.
[0083] In an exemplary embodiment, each test pattern has a different identification mark to distinguish each molding block and / or indicate each corresponding test radiation parameter.
[0084] Here, each molding block may have a different identification mark, and the identification mark may be a number, a letter, etc., so that each printed molding block can be easily identified; or the identification mark may also be a test radiation parameter corresponding to the molding block. For example, a number and / or letter mark is provided on the test pattern to distinguish each printed molding block, so that it is easy to find the test radiation parameter corresponding to each molding block. In other possible implementations, the test radiation parameter during printing may also be directly displayed on each corresponding test pattern, that is, each test pattern carries its radiation parameter during radiation, so that the corresponding radiation parameter can be directly read on the printed molding block.
[0085] In other embodiments, each test pattern may also have a different shape, so that each printed forming block also has a different shape, so as to facilitate distinguishing different forming blocks.
[0086] In an exemplary embodiment, the forming blocks are arranged in an array, so that the forming blocks can be easily connected through connecting blocks.
[0087] Here, the array arrangement can be one row with multiple columns, one column with multiple rows, or multiple columns with multiple rows. Considering that the pattern solidified layer is usually thin, in order to avoid accidental breakage when taking out the items, the overall structure of the pattern solidified layer can be made more solid by adjusting the aspect ratio of the pattern solidified layer. In one example, when the array is multiple columns and multiple rows, the aspect ratio of the pattern solidified layer can be between 1:1 and 2:1. It should be understood that the aspect ratio is the comparison value of the length and width of the pattern solidified layer.
[0088] The above-mentioned ideal radiation parameter testing method in the present application can avoid repeating the printing, picking up, cleaning, measuring and other processes every time a test piece is printed when testing the radiation parameters. By connecting the printed test pieces into an integrated structure, each test piece can be taken out in one picking up process.
[0089] In an exemplary embodiment, the ideal radiation parameter test system in the present application may also have an input module, through which the user can input a test instruction, thereby triggering the execution of the ideal radiation parameter test method based on the user's test instruction. To this end, the interface module of the ideal radiation parameter test system may also obtain the test instruction input by the user to generate multiple test patterns. In some embodiments, the user may also select the desired test pattern type in the system before testing.
[0090] In a possible implementation, the user may also input desired molding parameters through the input module, and the system may assign test radiation parameters to each test pattern according to the desired molding parameters input by the user. Alternatively, the user may also assign different test radiation parameters to each test pattern.
[0091] The system also generates a connection pattern for connecting the test patterns. In some embodiments, the radiation parameters of the connection pattern can be assigned by the system. In other embodiments, the radiation parameters of the connection pattern can also be assigned by user input. As mentioned above, the radiation parameters of each connection pattern can be the same.
[0092] In an exemplary embodiment, the energy radiation device may have energy attenuation during use. After a period of use, the power of the energy radiation device needs to be calibrated. Through the ideal radiation parameter test method in this application, the power of the energy radiation device can be calibrated by the molding parameters of the printed test piece without the need for professional equipment and professionals. In a specific example, the correction value can be determined by comparing the molding parameters that should be achieved when the energy radiation device is normally printed at the original power with the molding parameters achieved under the same radiation parameters after energy attenuation. In other possible embodiments, when the power of the energy radiation device is attenuated due to use, the standard material can be solidified using prefabricated radiation parameters. Due to the attenuation, the radiation energy at this time is only the preset theoretical radiation energy, not the actual radiation energy. Since the theoretical molding parameters of the standard material under the radiation energy are known, after measuring the actual molding parameters of the standard material under the radiation energy, the numerical matrix of the actual molding parameters is input into the ideal radiation parameter test system. Here, the molding parameter is the molding thickness as an example. The program of the ideal radiation parameter test system can calculate the difference between the actual energy radiated by the energy radiation device and the theoretical value based on the fitting comparison of the output thickness matrix and the theoretical thickness curve, and quickly calibrate the power of the energy radiation device. In this case, the user does not need to use a professional power measuring instrument to calibrate the power of the energy radiation device.
[0093] In an exemplary embodiment, see Figure 6a to Figure 6f , which shows a schematic diagram of the radiation image and the pattern solidified layer formed during the test in one embodiment of the present application. For the convenience of explanation, four test patterns are taken as an example. In a specific application, the number of projected test patterns is not limited to this. In this embodiment, it is assumed that four test pieces need to be printed, and the test patterns corresponding to the four test pieces are 41a, 41b, 41c, and 41d respectively. First, the energy radiation device is sequentially arranged according to the following Figure 6a to Figure 6d The test patterns 41a, 41b, 41c, 41d and their corresponding test radiation parameters are used to radiate energy to the printing surface to obtain the molding blocks corresponding to each test pattern on the printing surface, and then the energy radiation device is controlled according to the following Figure 6e The connection pattern 42 shown radiates energy to the printing surface to connect the molding blocks into an integrated structure through the connection blocks, and finally obtains the following Figure 6f The pattern solidified layer shown includes forming blocks 31a, 31b, 31c, 31d and connecting blocks 32. After the pattern solidified layer is taken out, the forming parameters of each forming block can be measured to determine the ideal radiation parameters of the energy radiation device.
[0094] The flow chart and block diagram in the above-mentioned accompanying drawings of the present application illustrate the possible architecture, function and operation of the system, method and computer program product according to various embodiments of the present application. Based on this, each box in the flow chart or block diagram can represent a module, a program segment or a part of a code, and the module, the program segment or a part of the code contains one or more executable instructions for realizing the specified logical function. It should also be noted that in some implementations as replacements, the functions marked in the box can also occur in a sequence different from that marked in the accompanying drawings. For example, two boxes represented in succession can actually be executed substantially in parallel, and they can sometimes be executed in the opposite order, depending on the functions involved. Specifically in the present application, for example, it is also possible to radiate energy to the print surface first according to the connection pattern, and then radiate energy to the print surface according to the test pattern to finally form a pattern solidification layer. It should also be noted that each box in the block diagram and / or the flow chart, and the combination of the boxes in the block diagram and / or the flow chart can be realized by a dedicated hardware-based system that performs a specified function or operation, or can be realized by a combination of dedicated hardware and computer instructions.
[0095] In an exemplary embodiment, for the energy radiation device for surface exposure, since the brightness of the picture projected by the energy radiation device is related to the light output power of the energy radiation device and the grayscale of the projected image, the radiation energy of each test pattern during projection can be adjusted by changing the grayscale value of the image, so that the energy radiation device can project an image with both a connecting pattern and a test pattern during projection, and each test pattern can have a different radiation energy during projection by changing the grayscale value of each test pattern.
[0096] To this end, the present application also provides another ideal radiation parameter testing method, which can be performed by an ideal radiation parameter testing system. The architecture of the ideal radiation parameter testing system is similar to Figure 1 The ideal radiation parameter test systems shown are the same, only the execution methods are different, so the system architecture will not be described in detail.
[0097] See also Figure 8, which is a schematic diagram of another embodiment of the ideal radiation parameter test method in the present application. As shown in the figure, in step S210, the energy radiation device is made to radiate energy to the printing surface according to the test image to obtain a pattern solidification layer corresponding to the test image on the printing surface, and the pattern solidification layer is an integrated molding structure. Among them, the test image includes a plurality of test patterns and connecting patterns, and the connecting patterns are used to connect the test patterns, and the grayscale values of the test patterns are different; the pattern solidification layer includes a plurality of molding blocks and connecting blocks, and the molding blocks are connected by connecting blocks.
[0098] Here, the energy radiation device is configured to project a test image onto the printing surface, wherein the test image includes a plurality of test patterns and connection patterns, wherein each connection pattern connects each test pattern, and in the test image, each test pattern has a different grayscale value. After the energy radiation device projects the test image, the printing material on the printing surface is solidified and formed accordingly, forming a pattern solidification layer corresponding to the test image, wherein the pattern solidification layer includes a forming block corresponding to the test pattern and a connecting block corresponding to the connection pattern, wherein the connecting block connects each forming block to form an integrated structure. Since the grayscale values of each test pattern are different, although the light intensity of the energy radiation device during projection remains unchanged, the energy received at the corresponding position of each test pattern projected on the printing surface is still different.
[0099] Here, the multiple molding blocks are multiple test pieces to be printed, and the shape of each molding block is determined by the test pattern corresponding to each molding block. For SLA printing equipment, after processing each test pattern into a scanning path, the energy radiation device in the 3D printing equipment is scanned based on the scanning path to shape the scanned printing material, thereby forming a molding block corresponding to the test pattern on the printing surface; for surface exposure printing equipment, the energy radiation device is projected onto the printing surface, thereby forming a molding block corresponding to the test pattern on the printing surface.
[0100] The test pattern may be in any shape, such as a square, a circle, a triangle or an irregular shape, as long as the printed molding block can be easily observed or measured. The shapes of different test patterns may be consistent or inconsistent. In some embodiments, test patterns of various shapes may be preset in the ideal radiation parameter test system of the energy radiation device. When the user needs to test the ideal radiation parameters of the energy radiation device, one or more of the preset test patterns may be selected.
[0101] Please continue reading Figure 8 In step S220, based on the molding parameters of each molding block in the pattern solidification layer and the conversion relationship between the radiation intensity and the grayscale value of the energy radiation device, the ideal radiation parameters of the energy radiation device are determined.
[0102] Here, since the molding parameters of each molding block in the pattern curing layer represent the molding conditions of the printed material under the corresponding radiation parameters, the ideal radiation parameters can be determined based on the comparison between the molding parameters of each molding block and the desired molding parameters. In particular, since a uniform radiation intensity is used to radiate energy in order to project a test image with a connection pattern and a test pattern at one time during projection, when determining the ideal radiation energy of the energy radiation device, it is necessary to convert the grayscale value of each test pattern into a corresponding radiation intensity based on the conversion relationship between the radiation intensity of the energy radiation device and the grayscale value of the projected image.
[0103] In an exemplary embodiment, since the energy projected by the energy radiation device per unit time under different radiation intensities can be obtained through detection, that is, the conversion relationship between radiation intensity and radiation energy. Then, under the condition that the radiation intensity remains unchanged, by changing the gray value of the projected image, the change of radiation energy projected by the energy radiation device under different gray values is detected. Thus, through the conversion relationship between radiation intensity and radiation energy, and the change of radiation energy projected by the energy radiation device under different gray values, the conversion relationship between the radiation intensity and gray value of the energy radiation device can be determined.
[0104] In an exemplary embodiment, the radiation time and radiation intensity of the energy radiation device when projecting the test image are consistent, while the grayscale values of each test pattern are different. Therefore, based on the comparison between the actual molding parameters of each molding block in the pattern solidification layer and the expected molding parameters, the grayscale value of the test pattern corresponding to the molding block with the closest comparison result can be determined. Then, the grayscale value is converted into the corresponding radiation intensity based on the conversion relationship between the radiation parameters of the energy radiation device and the grayscale value of the projected image. At the same time, since the radiation time is preset, the ideal radiation intensity and radiation time can be determined, thereby determining the ideal radiation parameters. Among them, the actual molding parameters are the molding parameters actually presented by the printed molding block, and the expected molding parameters are the molding parameters presented by the expected molding block.
[0105] In an exemplary embodiment, the degree of curing can generally be reflected in the thickness, strength, color, etc. of the printed material after molding. Therefore, in some embodiments, the molding parameters of the molding block include one or more of the molding thickness, molding color, and molding hardness of the molding block. For example, in some embodiments, the penetration (radiation depth) of the printed material is different under different radiation energies, so the molding parameters of each molding block can be determined by measuring the molding thickness of each molding block; for example, in other embodiments, the printed material will show different colors under different degrees of curing, and the molding parameters of each molding block can be determined by comparing the colors of each molding block; for example, in some other embodiments, the printed material will show different structural stresses under different degrees of curing, so the molding parameters of each molding block can be determined by comparing the hardness of each molding block; of course, in some embodiments, the molding parameters of each molding block can also be determined by combining the molding thickness, molding color, and molding hardness at the same time.
[0106] In an exemplary embodiment, the radiation parameters include radiation time and radiation intensity, and therefore the test radiation parameters also include radiation time and radiation intensity, that is, when radiating energy according to each test pattern, the test radiation parameters include control of radiation time and radiation intensity, and the ideal radiation parameters finally determined also include radiation time and radiation intensity.
[0107] It should be understood that for SLA printing equipment, the energy it radiates is the laser beam, its radiation intensity is the energy of the laser beam, and the radiation time is the residence time of the laser beam at each scanning point; for surface exposure printing equipment such as DLP and LCD, its radiation energy is the projected picture with brightness, the radiation time is the brightness of the projected picture, and the radiation time is the projection duration of the projected picture.
[0108] The ideal radiation parameters refer to radiation parameters suitable for making the printed material meet the molding requirements. The ideal radiation parameters can be a certain interval, for example, the radiation time is between T1 and T2, and the radiation intensity is between P1 and P2. In some cases with higher precision, the ideal radiation parameters can also be a specific value, for example, the radiation time = T3, the radiation intensity = P3.
[0109] In an exemplary embodiment, in order to facilitate the connection between the molding blocks, the connection pattern can connect adjacent test patterns, so that the connection block formed after printing can also connect the adjacent molding blocks. Of course, the connection block does not have to be connected in the same way as the adjacent molding blocks, as long as the molding blocks can be connected into an integrated molding structure through the connection of the connection block.
[0110] Here, the shape of the connection pattern is not specifically limited, as long as the forming blocks can be connected by the connection block to form the dispersed forming blocks into an integral structure. The connection block can be a long strip, an hourglass shape, etc.
[0111] Here, the obtained pattern solidified layer is usually an integrally formed thin layer structure, which includes the printed forming blocks and connecting blocks. In addition, since the grayscale values corresponding to the forming blocks are different during printing, the thickness of the forming blocks may also be different.
[0112] In some embodiments, in order to ensure the connection strength between the connecting block and the forming block, there is an overlapping portion between the connecting pattern and the connected test pattern, the overlapping area of the overlapping portion is less than 10% of the area of each connected test pattern, and the overlapping portion is located at the edge of each connected test pattern.
[0113] The overlapped portion refers to the overlapped projection of the connection pattern and the test pattern. To avoid the influence of the connection block on the main structure of the forming block after printing, the overlapped portion can be less than 10% of the area of each connected test pattern and the overlapped portion is located at the edge of each connected test pattern. In other words, for the connection pattern and the test pattern that generate a connection relationship, there is an overlapped portion of less than 10% of the area of the test pattern at the connection between the two.
[0114] In a possible implementation, there is an overlapping portion between the connection pattern and the connected test pattern, the overlapping area of the overlapping portion is less than 10% of the area of each connected test pattern, and the overlapping portion is located at the edge of each connected test pattern, and the connection pattern connects adjacent test patterns, and, in order to avoid the connection structure being too long and easy to break, the spacing between adjacent test patterns is not greater than 1 / 2 of the length or width of any one of the adjacent test patterns.
[0115] Specifically, when two adjacent test patterns are connected by a connection pattern, the length of the connection pattern is not greater than 1 / 2 of the length or width of any one of the connected test patterns. For example, test pattern a and test pattern b are adjacent, the length of test pattern a is L1 and the width is W1, and the length of test pattern b is L2 and the width is W2. When test pattern a and test pattern b are connected by a connection pattern, in order to avoid the connection block from being easily broken, the spacing between test pattern a and test pattern b can be set to be less than or equal to both. Of course, in some embodiments, the length and / or width of the test pattern may be adjusted based on the spacing between adjacent test patterns so that the spacing between adjacent test patterns is not greater than 1 / 2 of the length or width of any of the adjacent test patterns.
[0116] In an exemplary embodiment, in order to avoid the connection failure between the connection block and the molding block, it is necessary to ensure that the connection block can be successfully cured. Therefore, when irradiating the connection pattern, it is necessary to ensure that the irradiated energy should meet the minimum molding requirements of the printing material. To this end, the grayscale value of the connection pattern can be adjusted to the maximum, thereby ensuring that the connection block can be successfully printed. In addition, since the function of the connection block is mainly to connect the molding blocks, the grayscale values of the connection patterns can be the same.
[0117] In an exemplary embodiment, each test pattern has a different identification mark to distinguish each molding block and / or indicate each corresponding test radiation parameter.
[0118] Here, each molding block may have a different identification mark, and the identification mark may be a number, a letter, etc., so that each printed molding block can be easily identified; or the identification mark may also be a test radiation parameter corresponding to the molding block. For example, a number and / or letter mark is provided on the test pattern to distinguish each printed molding block, so that it is easy to find the test radiation parameter corresponding to each molding block. In other possible implementations, the test radiation parameter during printing may also be directly displayed on each corresponding test pattern, that is, each test pattern carries its radiation parameter during radiation, so that the corresponding radiation parameter can be directly read on the printed molding block.
[0119] In other embodiments, each test pattern may also have a different shape, so that each printed forming block also has a different shape, so as to facilitate distinguishing different forming blocks.
[0120] In an exemplary embodiment, the forming blocks are arranged in an array, so that the forming blocks can be easily connected through connecting blocks.
[0121] Here, the array arrangement can be one row with multiple columns, one column with multiple rows, or multiple columns with multiple rows. Considering that the pattern solidified layer is usually thin, in order to avoid accidental breakage when taking out the items, the overall structure of the pattern solidified layer can be made more solid by adjusting the aspect ratio of the pattern solidified layer. In one example, when the array is multiple columns and multiple rows, the aspect ratio of the pattern solidified layer can be between 1:1 and 2:1. It should be understood that the aspect ratio is the comparison value of the length and width of the pattern solidified layer.
[0122] The ideal radiation parameter test method in this application can avoid the need to repeat the printing, taking out, cleaning, measuring and other processes for each test piece printed when testing radiation parameters. By connecting the printed test pieces into an integrated structure, each test piece can be taken out in one take-out process. In addition, all connection patterns and test patterns can be projected in one projection, thereby effectively improving the test efficiency.
[0123] The present application also provides a 3D printing method for printing an ideal radiation parameter test piece of an energy radiation device in a 3D printing device, so as to determine the ideal radiation parameters through the test piece.
[0124] See also Fig. 9 , which is a schematic diagram of the 3D printing method in one embodiment of the present application. As shown in the figure, in step S310, the energy radiation device is allowed to radiate energy to different positions on the printing surface in sequence according to the test pattern, so that the printed material at the corresponding position on the printing surface is solidified and formed, thereby correspondingly obtaining a plurality of formed blocks; wherein, the test radiation parameters of the formed blocks at different positions during radiation are different. In step S320, the energy radiation device is allowed to radiate energy to the printing surface according to the connection pattern, so that the printed material at the corresponding position on the printing surface is solidified and formed, thereby correspondingly obtaining a connection block; wherein, the connection pattern is used to connect each test pattern, so that the cured connection block connects the plurality of formed blocks to form a pattern solidification layer, and the pattern solidification layer is an integrated molding structure.
[0125] Here, the steps S310 and S320 are Figure 1 The principles of step S110 and step S120 in the corresponding embodiment are similar, and the technical details are the same as Figure 1 to Figure 6f The technical details in the corresponding embodiments are similar, so they will not be repeated in this embodiment.
[0126] In step S330, the patterned cured layer is taken out from the container to obtain the ideal radiation parameter test piece.
[0127] Here, after printing the pattern solidified layer, in the top projection printing device, the pattern solidified layer floats on the printing material level of the container, and in the bottom projection printing device, the pattern solidified layer is suspended below the printing material level in the container. After taking out the pattern solidified layer, a test piece with ideal radiation parameters is obtained. In other words, each molding block is a test piece. By measuring the molding parameters of each test piece, the ideal radiation parameters of the energy radiation device can be determined.
[0128] In another exemplary embodiment, for the energy radiation device for surface exposure, since the brightness of the image projected by the energy radiation device is related to the light output power of the energy radiation device and the grayscale of the projected image, the radiation energy of each test pattern during projection can be adjusted by changing the grayscale value of the image, so that the energy radiation device can project an image having both a connection pattern and a test pattern during projection, and each test pattern has different radiation energy during projection by changing the grayscale value of each test pattern. Therefore, the present application also provides another 3D printing method.
[0129] See also Fig.12 , which is a schematic diagram of another embodiment of the 3D printing method in the present application. As shown in the figure, in step S410, the energy radiation device is made to radiate energy to the printing surface according to the test image to obtain a pattern solidification layer corresponding to the test image on the printing surface, and the pattern solidification layer is an integrated molding structure; wherein the test image includes a plurality of test patterns and connecting patterns, and the connecting patterns are used to connect the test patterns, and the grayscale values of the test patterns are different; the pattern solidification layer includes a plurality of molding blocks and connecting blocks, and the molding blocks are connected by connecting blocks. Here, the step S410 is Figure 8 The principle of step S210 in the corresponding embodiment is similar, and the technical details are the same as Figure 8 The technical details in the corresponding embodiments are similar, so they will not be repeated in this embodiment.
[0130] In step S420, the patterned cured layer is taken out from the container to obtain the ideal radiation parameter test piece.
[0131] Here, after printing the pattern solidified layer, in the top projection printing device, the pattern solidified layer floats on the printing material level of the container, and in the bottom projection printing device, the pattern solidified layer is suspended below the printing material level in the container. After taking out the pattern solidified layer, a test piece with ideal radiation parameters is obtained. In other words, each molding block is a test piece. By measuring the molding parameters of each test piece, the ideal radiation parameters of the energy radiation device can be determined.
[0132] In an exemplary embodiment, the 3D printing method may be performed by a 3D printing device.
[0133] The 3D printer can be a top exposure printing device or a bottom exposure printing device. The working state of the 3D printing device includes at least a printing operation and a test operation. The printing operation includes the process of solidifying the printing material layer by layer to form a 3D component, and the test operation includes the process of printing a test piece according to the ideal radiation parameter test method to determine the ideal radiation parameters of the energy radiation device. In some embodiments, the working state of the 3D printing device may also include a filtering operation for filtering the printing material residue in the container, a coating operation for uniformly coating the printing material on the printing surface, etc. Since the main invention of this application does not involve these operations, they will not be described in detail.
[0134] In an exemplary embodiment, taking a bottom surface exposure printing device as an example, see Fig.10, which is a simplified structural diagram of a 3D printing device in one embodiment of the present application. As shown in the figure, the 3D printing device includes a frame (not shown), a container 12, a component platform 13, a Z-axis driving mechanism 14, an energy radiation device 11, and a control device 15.
[0135] The frame is used to carry the container 12 , the Z-axis driving mechanism 14 , and the energy radiation device 11 .
[0136] The container 12 is used to hold the photocurable material, which includes any liquid material or powder material that is easy to photocurable. Examples of liquid materials include: photocurable resin liquid, or resin liquid doped with mixed materials such as ceramic powder, color additives, etc. The material of the container includes but is not limited to: glass, plastic, resin, etc. The capacity of the container 12 depends on the type of 3D printing equipment or the overall format of the energy radiation device in the 3D printing equipment. In some cases, the container may also be called a resin tank. The container may be transparent as a whole or only the bottom of the container may be transparent. For example, the container is a glass container, and light-absorbing paper (such as black film, or black paper, etc.) is attached to the container wall to reduce the interference of light scattering on the curing of the photocurable material during projection. In some embodiments, for bottom surface exposure molding printing equipment, a transparent flexible film (not shown) is also laid on the inner bottom surface of the container to facilitate the peeling of the printed solidified layer from the bottom surface of the container. The transparent flexible film that is easy to peel off is, for example, an FEP release film. The FEP release film is a hot melt extrusion cast film made of ultra-high purity FEP resin (fluorinated ethylene propylene copolymer). The FEP release film has excellent non-stickiness, high temperature resistance, electrical insulation, mechanical properties, wear resistance, etc.
[0137] In an exemplary embodiment, the Z-axis driving mechanism 14 in the 3D printing device is used to connect the component platform 13 .
[0138] The Z-axis driving mechanism 14 includes a driving unit and a Z-axis moving unit, wherein the driving unit is used to drive the Z-axis moving unit so that the Z-axis moving unit drives the component platform 13 to move axially along the Z-axis. For example, the driving unit is a driving motor. The driving unit is controlled by a control instruction. Among them, the control instruction includes: a directional instruction for indicating that the component platform 13 rises, falls or stops, and may even include parameters such as speed / speed acceleration, or torque / torque. This is conducive to accurately controlling the rising distance of the Z-axis moving unit to achieve precise adjustment of the Z-axis. Here, the Z-axis moving unit includes, for example, a fixed rod fixed at one end on the component platform and an interlocking moving component fixed to the other end of the fixed rod, wherein the interlocking moving component is driven by the driving unit to drive the fixed rod to move axially along the Z-axis, and the interlocking moving component is exemplified by a limit moving component engaged by a toothed structure, such as a rack. For another example, the Z-axis moving unit includes: a screw and a positioning moving structure screwed to the screw, wherein both ends of the screw are screwed to the drive unit, and the outer end of the positioning moving structure is fixedly connected to the component platform 13, and the positioning moving structure can be, for example, a ball screw.
[0139] The component platform 13 is a component for attaching and carrying the formed solidified layer. The component platform is used to attach and carry the formed cross-sectional layers, and the cross-sectional layers on the component platform are accumulated layer by layer to form a three-dimensional object. In some embodiments, the component platform is also called a component plate.
[0140] In the print job, for top exposure printing devices, see Fig.11 , which is a simplified structural diagram of another embodiment of the 3D printing device in the present application. As shown in the figure, the Z-axis driving mechanism 14 is used to controllably move and adjust the position of the component platform 13 along the Z-axis direction so that the upper surface of the component platform 13 and the liquid surface of the printing material in the container form a printing surface; for the bottom exposure printing device, the Z-axis driving mechanism 14 is used to controllably move and adjust the position of the component platform 13 along the Z-axis direction so that the lower surface of the component platform 13 and the lower surface in the container form a printing surface. The component platform 13 is used to adhere the photocurable material on the irradiated printing surface to cure and form a patterned cured layer.
[0141] During the testing operation, the component platform may or may not be removed.
[0142] In the embodiment where the component platform is not removed, it is necessary to move the component platform to a position where the test operation will not be affected. Specifically, for a top exposure printing device, if the component platform is not removed, the Z-axis drive mechanism can move the component platform to a position below the container, and when the energy radiation device radiates energy to the printing surface located in the container at a position above the container, the curing depth of the printed material on the printing surface in the Z-axis direction (i.e., the depth direction) is free, that is, it is not affected by the component platform, so that in some embodiments, the ideal radiation parameters of the energy radiation device are determined by the molding thickness of each test piece (molding block); for a bottom exposure printing device, if the component platform is not removed, the Z-axis drive mechanism can move the component platform to a position above the printing surface and keep a certain distance from the printing surface, such as being located at an upper position in the container, or being located above the container, etc., so that when the energy radiation device radiates energy to the printing surface located in the container at a position below the container, the curing depth of the printed material at the bottom of the container in the Z-axis direction (i.e., the depth direction) is free, that is, it is not affected by the component platform, so that in some embodiments, the ideal radiation parameters of the energy radiation device are determined by the molding thickness of each test piece (molding block).
[0143] In some embodiments, the component platform can also help to take out the parts during the test operation. Specifically, for a top exposure printing device, when the printed pattern solidified layer needs to be taken out after the test operation is completed, if the component platform is located at the lower position in the container, the component platform can be directly raised, so that when it rises to the position of the pattern solidified layer, it can drive the pattern solidified layer to rise together and leave the container to complete the removal.
[0144] Of course, in other embodiments, when it is not possible to take out the components with the help of the component platform during the test operation, they can also be taken out manually. Since the forming blocks are connected into an integrated structure by the connecting blocks in the present application, they can be taken out as a whole when taking out the components, which reduces the difficulty of taking out the components.
[0145] In an exemplary embodiment, please refer to Fig.10 The control device 15 is connected to the energy radiation device 11 and the Z-axis driving mechanism 14, and is used to control the multiple energy radiation devices 11 and the Z-axis driving mechanism 14 to accumulate the attached pattern solidified layer on the component platform 13 in the printing operation to obtain the corresponding 3D component, and control the energy radiation device to perform as described in the present application in the test operation. Fig. 9 or Fig.12 The specific principle of the 3D printing method in the corresponding embodiment has been explained in detail above and will not be described again here.
[0146] In an exemplary embodiment, the present application also provides an image generation method, so that the test pattern and connection pattern required by the 3D printing device in the test operation can be automatically generated based on the user's input instructions.
[0147] In summary, the present application may provide the following embodiments, in which different embodiments are represented by serial numbers, for example, 1, 2, 3, ..., etc. represent embodiment 1, embodiment 2, embodiment 3, ..., and these embodiments include:
[0148] 1. A method for generating an image, comprising the following steps:
[0149] After receiving the test instruction input by the user, a plurality of test patterns are generated;
[0150] Assigning different test radiation parameters to each test pattern according to the molding parameters input by the user, or assigning different test radiation parameters to each test pattern based on the different test radiation parameters input by the user;
[0151] A connection pattern is generated, wherein the connection pattern is used to connect various test patterns.
[0152] 2. According to the image generation method described in embodiment 1, each test pattern has a different identification mark to distinguish each molding block and / or mark each corresponding test radiation parameter.
[0153] 3. According to the image generation method described in embodiment 1, the test radiation parameters include radiation time and radiation intensity.
[0154] 4. According to the image generation method described in embodiment 1, each test pattern is arranged in an array.
[0155] 5. According to the image generation method described in Example 4, when the array is multi-row and multi-column, the connection pattern and the test pattern together form a test image, and the aspect ratio of the test image is between 1:1 and 2:1.
[0156] 6. An image generating method according to embodiment 1, wherein there is an overlapping portion between the connecting pattern and the connected test pattern, the overlapping area of the overlapping portion is less than 10% of the area of each connected test pattern, and the overlapping portion is located at the edge of each connected test pattern.
[0157] 7. The image generating method according to embodiment 1 or 6, wherein the connection pattern connects adjacent test patterns.
[0158] 8. The image generating method according to embodiment 7, wherein the length of the connecting pattern is not greater than 1 / 2 of the length or width of any one of the two connected test patterns.
[0159] 9. The image generation method according to embodiment 1, wherein the radiation parameters of each of the connection patterns are the same.
[0160] 10. An image generation system, wherein the image generation system is used for a 3D printing device, the image generation system comprising:
[0161] A communication module, which is in communication with a control device in the 3D printing device;
[0162] An input module, used for receiving test instructions and molding parameters input by a user;
[0163] A storage module storing at least one program;
[0164] a processing module connected to the communication module, the input module and the storage module, for calling the at least one program to send a plurality of test patterns, test radiation parameters and connection patterns generated by the image generation method described in any one of embodiments 1 to 9 to the control device, so that the control device causes the energy radiation device in the 3D printing device to generate the test patterns, the test radiation parameters and the connection patterns according to the image generation method described in any one of embodiments 1 to 9.
[0165] The plurality of test patterns and connection patterns and the corresponding test radiation parameters radiate energy onto the printing surface once or in batches. 11. A 3D printing device, comprising:
[0166] A container for holding printing materials;
[0167] A component platform, located in the container during the printing operation, for accumulating the attached pattern solidified layers layer by layer to form a corresponding 3D component;
[0168] A Z-axis driving mechanism connected to the component platform and used to adjust the height of the component platform in the Z-axis direction so as to adjust the distance from the component platform to the printing surface during the printing operation;
[0169] an energy radiation device, located above or below the container, for radiating energy to a printing surface in the container;
[0170] A control device is connected to the energy radiation device and the Z-axis drive mechanism, and is used to control the energy radiation device and the Z-axis drive mechanism in a printing operation to accumulate a solidified layer on the component platform to obtain a corresponding 3D component; and is used to generate a plurality of test patterns and connection patterns based on the image generation method as described in any one of Examples 1 to 9 in a test operation, so that the energy radiation device prints the plurality of test patterns and connection patterns on the printing surface once or in batches.
[0171] The image generation method can be performed by an image generation system. Fig.14, which is a schematic diagram of the hardware architecture of the image generation system in one embodiment of the present application.
[0172] The image generation system can be applied to a 3D printing device so as to enable a control device in the 3D printing device to control the energy radiation device to work.
[0173] The image generation system 3 comprises:
[0174] The communication module 301 is used for communicating with the outside. Exemplarily, the communication module 301 includes one or more communicators, and the communicator includes one or more wired or wireless communication circuits. The wired communication circuit includes, for example, a wired Ethernet card, USB, etc., and the wireless communication circuit includes, for example, a wireless network card (WiFi), a 2G / 3G / 4G / 5G mobile communication module, Bluetooth, infrared, etc. In this embodiment, the communication module is connected to the control device in the 3D printing device so as to control the energy radiation device in the 3D printing device to work through the control device.
[0175] Input module 304, which enables a user to interact with the image generation system. The input module may include buttons, keyboards, mice, touch pads, etc., and may also include an electronic display with a touch component that facilitates user input by detecting the occurrence and / or location of an object touching its screen.
[0176] The storage module 302 stores a computer program. Exemplarily, the storage module 302 includes one or more memories, at least part of each of which stores a computer program. Exemplarily, the memory may include a high-speed random access memory, and may also include a non-volatile memory, such as one or more disk storage devices, flash memory devices, or other non-volatile solid-state storage devices. In some embodiments, the memory may also include a memory away from one or more processors, such as a network attached memory accessed via an RF circuit or an external port and a communication network, wherein the communication network may be the Internet, one or more intranets, a local area network, a wide area network, a storage area network, etc., or a suitable combination thereof. The memory controller may control access to the memory by other components of the device, such as a CPU and a peripheral interface.
[0177] The processing module 303 is communicatively connected to the communication module 301 and the storage module 302, and is used to run the computer program to execute the image generation method. The specific steps of the image generation method will be described in detail later. Exemplarily, the processing module 303 includes one or more processors coupled to at least one of the memory and the communicator; the processor may include a general-purpose microprocessor, a dedicated processor, a field programmable logic array, or any combination thereof.
[0178] See also Fig.13 , which is a schematic diagram of an image generation method in an embodiment of the present application. As shown in the figure, in step S510, after receiving a test instruction input by a user, a plurality of test patterns are generated.
[0179] Here, the user may generate a plurality of test patterns through the input module 304. For example, a plurality of test pattern templates for selection are preset in the image generation system, and the user may select the required test pattern and the corresponding quantity according to actual needs.
[0180] In step S520, different test radiation parameters are assigned to each test pattern according to the molding parameters input by the user.
[0181] Here, the user can also input the desired molding parameters, such as the desired molding hardness, molding thickness, etc., through the input module 304. After the image generation system receives the molding parameter instruction input by the user, it can assign different test radiation parameters to each test pattern generated in step S510 according to the molding parameters. The assignment includes defining the test radiation parameter value corresponding to each test pattern when radiating. In some embodiments, the operator can set the test radiation parameters corresponding to each test pattern separately, or use the parameters pre-made by the system.
[0182] In step S530 , a connection pattern is generated, wherein the connection pattern is used to connect the test patterns.
[0183] Here, the test patterns are connected by the connection pattern, so that after printing, the forming blocks corresponding to the test patterns can be connected by the connection blocks corresponding to the connection pattern, thereby forming an integrated pattern solidification layer.
[0184] The order of step S520 and step S530 may also be interchanged, that is, after the connection pattern is generated, different test radiation parameters are assigned to each test pattern according to the forming parameters input by the user.
[0185] In some embodiments, the radiation parameters of the connection pattern may be constant, for example, when the connection pattern is generated, the corresponding radiation parameters are automatically assigned to the connection pattern. Since the connection pattern is mainly used to connect the test patterns, when there are multiple connection patterns, it is not necessary to set the radiation parameters of the connection patterns to different values. In some other embodiments, in addition to assigning values to the test patterns, values may also be assigned to the connection patterns.
[0186] The test pattern may be in any shape, such as a square, a circle, a triangle or an irregular shape, as long as the printed molding block can be easily observed or measured. The shapes of different test patterns may be consistent or inconsistent. In some embodiments, test patterns of various shapes may be preset in the ideal radiation parameter test system of the energy radiation device. When the user needs to test the ideal radiation parameters of the energy radiation device, one or more of the preset test patterns may be selected.
[0187] In an exemplary embodiment, the radiation parameters include radiation time and radiation intensity, and therefore the test radiation parameters also include radiation time and radiation intensity, that is, when radiating energy according to each test pattern, the test radiation parameters include control of radiation time and radiation intensity, and the ideal radiation parameters finally determined also include radiation time and radiation intensity.
[0188] It should be understood that for SLA printing equipment, the energy it radiates is the laser beam, its radiation intensity is the energy of the laser beam, and the radiation time is the residence time of the laser beam at each scanning point; for surface exposure printing equipment such as DLP and LCD, its radiation energy is the projected picture with brightness, the radiation time is the brightness of the projected picture, and the radiation time is the projection duration of the projected picture.
[0189] The ideal radiation parameters refer to radiation parameters suitable for making the printed material meet the molding requirements. The ideal radiation parameters can be a certain interval, for example, the radiation time is between T1 and T2, and the radiation intensity is between P1 and P2. In some cases with higher precision, the ideal radiation parameters can also be a specific value, for example, the radiation time = T3, the radiation intensity = P3.
[0190] In some embodiments, in order to ensure the connection strength between the connecting block and the forming block, there is an overlapping portion between the connecting pattern and the connected test pattern, the overlapping area of the overlapping portion is less than 10% of the area of each connected test pattern, and the overlapping portion is located at the edge of each connected test pattern.
[0191] The overlapped portion refers to the overlapped projection of the connection pattern and the test pattern. To avoid the influence of the connection block on the main structure of the forming block after printing, the overlapped portion can be less than 10% of the area of each connected test pattern and the overlapped portion is located at the edge of each connected test pattern. In other words, for the connection pattern and the test pattern that generate a connection relationship, there is an overlapped portion of less than 10% of the area of the test pattern at the connection between the two.
[0192] In a possible implementation, there is an overlapping portion between the connection pattern and the connected test pattern, the overlapping area of the overlapping portion is less than 10% of the area of each connected test pattern, and the overlapping portion is located at the edge of each connected test pattern, and the connection pattern connects adjacent test patterns, and, in order to avoid the connection structure being too long and easy to break, the spacing between adjacent test patterns is not greater than 1 / 2 of the length or width of any one of the adjacent test patterns.
[0193] Specifically, when two adjacent test patterns are connected by a connection pattern, the length of the connection pattern is not greater than 1 / 2 of the length or width of any one of the connected test patterns. For example, test pattern a and test pattern b are adjacent, the length of test pattern a is L1 and the width is W1, and the length of test pattern b is L2 and the width is W2. When test pattern a and test pattern b are connected by a connection pattern, in order to avoid the connection block from being easily broken, the spacing between test pattern a and test pattern b can be set to be less than or equal to both. Of course, in some embodiments, the length and / or width of the test pattern may be adjusted based on the spacing between adjacent test patterns so that the spacing between adjacent test patterns is not greater than 1 / 2 of the length or width of any of the adjacent test patterns.
[0194] In an exemplary embodiment, each test pattern has a different identification mark to distinguish each molding block and / or indicate each corresponding test radiation parameter.
[0195] Here, each test pattern may have different identification marks, and the identification marks may be numbers, letters, etc., so as to facilitate identification of each printed molding block; or the identification marks may also be the test radiation parameters corresponding to the molding block. For example, the test pattern may have numbers and / or letters to distinguish each printed molding block, so as to facilitate finding the test radiation parameters corresponding to each molding block. In other possible implementations, the test radiation parameters during printing may also be directly displayed on each corresponding test pattern, that is, each test pattern carries its radiation parameters during radiation, so that the corresponding radiation parameters can be directly read on the printed molding block.
[0196] In other embodiments, each test pattern may also have a different shape, so that each printed forming block also has a different shape, so as to facilitate distinguishing different forming blocks.
[0197] In an exemplary embodiment, the test patterns are arranged in an array, so that the forming blocks corresponding to the test patterns can be connected through the connecting blocks corresponding to the connecting patterns after printing.
[0198] Here, the array arrangement may be one row and multiple columns, one column and multiple rows, or multiple columns and multiple rows.
[0199] The image after the connection patterns and the test patterns are superimposed is called the test image. Considering that the pattern solidified layer after printing is usually thin, in order to avoid accidental breakage during the removal of the item, the overall structure of the pattern solidified layer can be made more solid by adjusting the aspect ratio of the test image. In one example, when the array is multi-column and multi-row, the aspect ratio of the test image can be between 1:1 and 2:1. It should be understood that the aspect ratio is the comparison value of the length and width of the test image.
[0200] It should be noted that, although the connection pattern and the test pattern are used together to form a test image, in actual projection, after the test pattern and the connection pattern are generated, the test image can be formed based on the connection pattern. Figure 1 to Figure 6f The ideal radiation parameter test method in each embodiment can also be used for testing. Figure 8 The ideal radiation parameter testing method in the corresponding embodiment is used for testing.
[0201] In some embodiments, in order to ensure the connection strength between the connecting block and the forming block after printing, there is an overlapping portion between the connecting pattern and the connected test pattern, the overlapping area of the overlapping portion is less than 10% of the area of each connected test pattern, and the overlapping portion is located at the edge of each connected test pattern.
[0202] The overlapped portion refers to the overlapped projection of the connection pattern and the test pattern. To avoid the influence of the connection block on the main structure of the forming block after printing, the overlapped portion can be less than 10% of the area of each connected test pattern and the overlapped portion is located at the edge of each connected test pattern. In other words, for the connection pattern and the test pattern that generate a connection relationship, there is an overlapped portion of less than 10% of the area of the test pattern at the connection between the two.
[0203] In a possible implementation, there is an overlapping portion between the connection pattern and the connected test pattern, the overlapping area of the overlapping portion is less than 10% of the area of each connected test pattern, and the overlapping portion is located at the edge of each connected test pattern, and the connection pattern connects adjacent test patterns, and, in order to avoid the connection structure being too long and easy to break, the spacing between adjacent test patterns is not greater than 1 / 2 of the length or width of any one of the adjacent test patterns.
[0204] Specifically, when two adjacent test patterns are connected by a connection pattern, the length of the connection pattern is not greater than 1 / 2 of the length or width of any one of the connected test patterns. For example, test pattern a and test pattern b are adjacent, the length of test pattern a is L1 and the width is W1, and the length of test pattern b is L2 and the width is W2. When test pattern a and test pattern b are connected by a connection pattern, in order to avoid the connection block from being easily broken, the spacing between test pattern a and test pattern b can be set to be less than or equal to both. Of course, in some embodiments, the length and / or width of the test pattern may be adjusted based on the spacing between adjacent test patterns so that the spacing between adjacent test patterns is not greater than 1 / 2 of the length or width of any of the adjacent test patterns.
[0205] In an exemplary embodiment, in order to facilitate the connection between the molding blocks, the connection pattern can connect adjacent test patterns, so that the connection block formed after printing can also connect the adjacent molding blocks. Of course, the connection block does not have to be connected in the same way as the adjacent molding blocks, as long as the molding blocks can be connected into an integrated molding structure through the connection of the connection block.
[0206] Here, the shape of the connection pattern is not specifically limited, as long as the forming blocks can be connected by the connection block to form the dispersed forming blocks into an integral structure. The connection block can be a long strip, an hourglass shape, etc.
[0207] Here, the obtained pattern solidified layer is usually an integrally formed thin layer structure, which includes the printed forming blocks and connecting blocks. In addition, since the grayscale values corresponding to the forming blocks are different during printing, the thickness of the forming blocks may also be different.
[0208] In an exemplary embodiment, in order to avoid the connection failure between the connecting block and the forming block, it is necessary to ensure that the connecting block can be successfully cured. Therefore, when radiating the connecting pattern, it is necessary to ensure that the radiated energy should meet the minimum forming requirements of the printing material. In some embodiments, the connecting pattern can also be directly radiated according to the strongest radiation intensity of the energy radiation device to ensure that the connecting block can be successfully printed. In addition, since the function of the connecting block is mainly to connect the forming blocks, the radiation parameters of each connecting pattern can be the same. In an embodiment in which the 3D printing device is a surface exposure printing device, parts of the connecting pattern can be projected at the same time. In an embodiment in which the 3D printing device is an SLA printing device, since the laser spot needs to scan and cure while moving, although it is impossible to achieve simultaneous projection like a surface exposure device, scanning and curing can also be completed during continuous movement, that is, there is no need to adjust the radiation parameters and then scan again.
[0209] In an exemplary embodiment, the image generation system receives the test instructions and molding parameters input by the user through the input module, and then generates multiple test patterns, connection patterns and corresponding test radiation parameters based on the image generation method after being processed by the processing module, and then sends these data to the control device in the 3D printing device so that the control device controls the energy radiation device to work. Fig. 9 The 3D printing method in each corresponding embodiment prints the test piece, that is, the energy radiation device radiates energy to the printing surface in stages based on each test pattern and the connection pattern, so as to determine the ideal radiation parameters of the energy radiation device; it can also be based on Fig.12 The 3D printing method in the corresponding embodiment prints the test piece, that is, the energy radiation device radiates energy to the printing surface once according to each test pattern and the connection pattern, and simultaneously prints the forming blocks and the connection blocks corresponding to each test pattern and the connection pattern, so as to determine the ideal radiation parameters of the energy radiation device.
[0210] In an exemplary embodiment, the image generation system may also be integrated into a 3D printing device.
[0211] Based on this understanding, the present application also provides a 3D printing device, the basic hardware architecture of the 3D printing device is similar to Figure 10-11 The corresponding embodiments are the same, including a container, a component platform, a Z-axis drive mechanism, an energy radiation device, and a control device, so they are not described here in detail. In this embodiment, the 3D printing device also includes an input device, which is connected to the control device, and the input device enables the user to interact with the 3D printing device. The input device may include a button, a keyboard, a mouse, a touch pad, etc., and may also include an electronic display with a touch component, which facilitates user input by detecting the occurrence and / or position of an object touching its screen.
[0212] Here, the user can generate multiple test patterns through the input device. For example, multiple optional test pattern templates are preset in the control device of the 3D printing device, and the user can select the required test pattern and the corresponding quantity according to actual needs.
[0213] Then, different test radiation parameters are assigned to each test pattern according to the molding parameters input by the user.
[0214] Here, the user can also input desired molding parameters, such as desired molding hardness, molding thickness, etc., through the input device. After the control device receives the molding parameter instruction input by the user, it can assign different test radiation parameters to each generated test pattern according to the molding parameters. The assignment includes defining the test radiation parameter value corresponding to each test pattern during radiation.
[0215] Next, a connection pattern is generated, wherein the connection pattern is used to connect the test patterns.
[0216] Here, the test patterns are connected by the connection pattern, so that after printing, the forming blocks corresponding to the test patterns can be connected by the connection blocks corresponding to the connection pattern, thereby forming an integrated pattern solidification layer.
[0217] It is also possible to generate the connection pattern first, and then assign different test radiation parameters to each test pattern according to the forming parameters input by the user.
[0218] In some embodiments, the radiation parameters of the connection pattern may be constant, for example, when the connection pattern is generated, the corresponding radiation parameters are automatically assigned to the connection pattern. Since the connection pattern is mainly used to connect the test patterns, when there are multiple connection patterns, it is not necessary to set the radiation parameters of the connection patterns to different values. In some other embodiments, in addition to assigning values to the test patterns, values may also be assigned to the connection patterns.
[0219] The image generation methods in this embodiment are Fig.13 The principles and details of the methods in the corresponding embodiments are similar, so they will not be repeated here. Figure 1 to Figure 6f The ideal radiation parameter test method in each embodiment can also be used for testing. Figure 8 The ideal radiation parameter testing method in the corresponding embodiment is used for testing.
[0220] The 3D printing device provided in the present application can generate a test pattern and a connection pattern based on user input, thereby reducing the difficulty of operation for the user.
[0221] In one or more exemplary aspects, the functions described by the computer program of the method described in the present application can be implemented in hardware, software, firmware, or any combination thereof. When implemented in software, these functions can be stored or transmitted as one or more instructions or codes on a computer-readable medium. The steps of the method or algorithm disclosed in the present application can be embodied in a processor-executable software module, wherein the processor-executable software module can be located on a tangible, non-temporary computer-readable and writable storage medium. A tangible, non-temporary computer-readable and writable storage medium can be any available medium that a computer can access.
[0222] The flow chart and block diagram in the above-mentioned accompanying drawings of the present application illustrate the possible architecture, function and operation of the system, method and computer program product according to various embodiments of the present application. Based on this, each box in the flow chart or block diagram can represent a module, a program segment or a part of a code, and the module, the program segment or a part of the code contains one or more executable instructions for realizing the specified logical function. It should also be noted that in some implementations as replacements, the functions marked in the box can also occur in a different order from the order marked in the accompanying drawings. For example, two boxes represented in succession can actually be executed substantially in parallel, and they can sometimes be executed in the opposite order, depending on the functions involved. It should also be noted that each box in the block diagram and / or flow chart, and the combination of the boxes in the block diagram and / or flow chart can be realized by a dedicated hardware-based system that performs a specified function or operation, or can be realized by a combination of dedicated hardware and computer instructions.
[0223] The above embodiments are merely illustrative of the principles and effects of the present application and are not intended to limit the present application. Anyone familiar with the technology may modify or change the above embodiments without violating the spirit and scope of the present application. Therefore, all equivalent modifications or changes made by a person of ordinary skill in the art without departing from the spirit and technical ideas disclosed in the present application shall still be covered by the claims of the present application.
Claims
1. A method for testing ideal radiation parameters of an energy radiation device, characterized in that: The following steps are involved: The energy radiation device is made to radiate energy to different positions on the printing surface in sequence according to the test pattern, so that the printing material at the corresponding position on the printing surface is solidified and formed, thereby obtaining a plurality of corresponding forming blocks; wherein the forming blocks at different positions have different test radiation parameters during radiation; the energy radiation device is a DLP projection system or an LCD liquid crystal screen light source system for curing the liquid resin material by surface exposure; The energy radiation device is made to radiate energy to the printing surface according to the connection pattern, so that the printing material at the corresponding position on the printing surface is solidified and formed, thereby obtaining a corresponding connection block; wherein the connection pattern is used to connect each test pattern, so that the connection block after solidification connects the multiple forming blocks to form a pattern solidification layer, and the pattern solidification layer is an integrally formed structure; the radiation parameters of each connection pattern are the same, and the radiation intensity of the connection pattern is the strongest radiation intensity of the energy radiation device; there is an overlapping part between the connection pattern and the connected test pattern, the overlapping area of the overlapping part is less than 10% of the area of each connected test pattern, and the overlapping part is located at the edge of each connected test pattern; the part of the connection pattern is projected simultaneously by the energy radiation device; Based on the molding parameters of each molding block in the pattern solidification layer, the ideal radiation parameters of the energy radiation device are determined; the ideal radiation parameters and the test radiation parameters each include radiation time and radiation intensity.
2. The ideal radiation parameter testing method of the energy radiation device according to claim 1, characterized in that: Each test pattern has a different identification mark to distinguish each molding block and / or indicate each corresponding test radiation parameter.
3. The ideal radiation parameter testing method of the energy radiation device according to claim 1, characterized in that: The step of determining the ideal radiation parameters of the energy radiation device based on the molding parameters of each molding block in the pattern solidification layer includes: according to the comparison between the actual molding parameters of each molding block and the expected molding parameters, the test radiation parameters corresponding to the molding block with the closest comparison result are taken as the ideal radiation parameters of the energy radiation device.
4. The ideal radiation parameter testing method of the energy radiation device according to claim 1, characterized in that: The molding parameters of the molding block include the molding thickness of the molding block and / or the molding color of the molding block and / or the molding hardness of the molding block.
5. The ideal radiation parameter testing method of the energy radiation device according to claim 1, characterized in that: The forming blocks are arranged in an array.
6. The ideal radiation parameter testing method of the energy radiation device according to claim 5, characterized in that: When the array has multiple rows and columns, the aspect ratio of the patterned solidified layer is between 1:1 and 2:
1.
7. The ideal radiation parameter testing method of the energy radiation device according to claim 1, characterized in that: The connection pattern connects adjacent test patterns.
8. The ideal radiation parameter testing method of the energy radiation device according to claim 7, characterized in that: The spacing between adjacent test patterns is no greater than 1 / 2 of the length or width of any one of the adjacent test patterns.
9. The ideal radiation parameter testing method of the energy radiation device according to claim 1, characterized in that: The method for generating the test pattern and the connection pattern comprises: generating a plurality of test patterns based on the test instructions received from the user; Assigning different test radiation parameters to each test pattern based on the molding parameters input by the user; or assigning different test radiation parameters to each test pattern based on the different test radiation parameters input by the user; A connection pattern is generated and a radiation parameter is assigned to the connection pattern; wherein the connection pattern is used to connect each test pattern.
10. A method for testing ideal radiation parameters of an energy radiation device, characterized in that: The following steps are involved: The energy radiation device is made to radiate energy to the printing surface according to the test image, so as to obtain a pattern solidification layer corresponding to the test image on the printing surface, wherein the pattern solidification layer is an integrally formed structure; wherein the test image includes a plurality of test patterns and connection patterns, the connection patterns are used to connect the test patterns, and the grayscale values of the test patterns are different; the pattern solidification layer includes a plurality of molding blocks and connection blocks, and the molding blocks are connected by the connection blocks; the molding blocks at different positions have different test radiation parameters during radiation; the radiation parameters of the connection patterns are the same, and the radiation intensity of the connection patterns is the strongest radiation intensity of the energy radiation device; there is an overlapped portion between the connection pattern and the connected test pattern, the overlapped area of the overlapped portion is less than 10% of the area of each connected test pattern, and the overlapped portion is located at the edge of each connected test pattern; the energy radiation device is a DLP projection system or an LCD liquid crystal screen light source system for curing liquid resin materials by surface exposure; the portion of the connection pattern is simultaneously projected by the energy radiation device; Based on the molding parameters of each molding block in the pattern solidification layer and the conversion relationship between the radiation intensity and grayscale value of the energy radiation device, the ideal radiation parameters of the energy radiation device are determined; the ideal radiation parameters and the test radiation parameters each include radiation time and radiation intensity.
11. The ideal radiation parameter testing method of the energy radiation device according to claim 10, characterized in that: Each test pattern has a different identification mark to distinguish each molding block and / or indicate each corresponding test radiation parameter.
12. The ideal radiation parameter testing method of the energy radiation device according to claim 10, characterized in that: The step of determining the ideal radiation parameters of the energy radiation device based on the molding parameters of each molding block in the pattern solidification layer and the conversion relationship between the radiation intensity and the grayscale value of the energy radiation device includes: according to the conversion relationship and the comparison between the actual molding parameters of each molding block and the expected molding parameters, the ideal radiation parameters determined by the grayscale value of the test pattern corresponding to the molding block with the closest comparison result are used as the ideal radiation parameters of the energy radiation device.
13. The ideal radiation parameter testing method of the energy radiation device according to claim 10, characterized in that: The test patterns in the test image are arranged in an array.
14. An ideal radiation parameter test system for an energy radiation device, characterized in that: include: An interface module connected to a control device in a 3D printing device so that the ideal radiation parameter test system controls the energy radiation device through the control device; A storage module storing at least one program; A processing module, connected to the interface module and the storage module, is used to call the at least one program to control the energy radiation device to determine the ideal radiation parameters of the energy radiation device based on the ideal radiation parameter testing method of the energy radiation device as described in any one of claims 1 to 9 or 10 to 13.
15. The ideal radiation parameter testing system of the energy radiation device according to claim 14, characterized in that: It also includes an input module for receiving test instructions and molding parameters input by a user, or for receiving test instructions and different test radiation parameters input by a user.
16. A 3D printing method, characterized in that: The method is used to print an ideal radiation parameter test piece of an energy radiation device in a 3D printing device, wherein the 3D printing device also includes a container for containing printing materials, and the 3D printing method includes the following steps: The energy radiation device is made to radiate energy to different positions on the printing surface in sequence according to the test pattern, so that the printing material at the corresponding position on the printing surface is solidified and formed, thereby obtaining a plurality of corresponding forming blocks; wherein the forming blocks at different positions have different test radiation parameters during radiation; the energy radiation device is a DLP projection system or an LCD liquid crystal screen light source system for curing the liquid resin material by surface exposure; The energy radiation device is made to radiate energy to the printing surface according to the connection pattern, so that the printing material at the corresponding position on the printing surface is solidified and formed, thereby obtaining a corresponding connection block; wherein the connection pattern is used to connect each test pattern, so that the connection block after solidification connects the multiple forming blocks to form a pattern solidification layer, and the pattern solidification layer is an integrally formed structure; the radiation parameters of each connection pattern are the same, and the radiation intensity of the connection pattern is the strongest radiation intensity of the energy radiation device; there is an overlapping part between the connection pattern and the connected test pattern, the overlapping area of the overlapping part is less than 10% of the area of each connected test pattern, and the overlapping part is located at the edge of each connected test pattern; the part of the connection pattern is projected simultaneously by the energy radiation device; The patterned solidified layer is taken out from the container to obtain the ideal radiation parameter test piece; the ideal radiation parameters and the test radiation parameters respectively include radiation time and radiation intensity.
17. The 3D printing method according to claim 16, characterized in that: Each test pattern has a different identification mark to distinguish each forming block and / or indicate each corresponding ideal radiation parameter.
18. The 3D printing method according to claim 16, characterized in that: The molding parameters of the molding block include the molding thickness of the molding block and / or the molding color of the molding block and / or the molding hardness of the molding block.
19. The 3D printing method according to claim 16, characterized in that: The forming blocks are arranged in an array.
20. The 3D printing method according to claim 19, characterized in that: When the array has multiple rows and columns, the aspect ratio of the patterned solidified layer is between 1:1 and 2:
1.
21. The 3D printing method according to claim 16, characterized in that: The connection pattern connects adjacent test patterns.
22. The 3D printing method according to claim 21, characterized in that: The spacing between adjacent test patterns is no greater than 1 / 2 of the length or width of any one of the adjacent test patterns.
23. A 3D printing method, characterized in that: The method is used to print an ideal radiation parameter test piece of an energy radiation device in a 3D printing device, wherein the 3D printing device also includes a container for containing printing materials, and the 3D printing method includes the following steps: The energy radiation device is made to radiate energy to the printing surface according to the test image, so as to obtain a pattern solidification layer corresponding to the test image on the printing surface, wherein the pattern solidification layer is an integrally formed structure; wherein the test image includes a plurality of test patterns and connection patterns, the connection patterns are used to connect the test patterns, and the grayscale values of the test patterns are different; the pattern solidification layer includes a plurality of molding blocks and connection blocks, and the molding blocks are connected by the connection blocks; the molding blocks at different positions have different test radiation parameters during radiation; the radiation parameters of the connection patterns are the same, and the radiation intensity of the connection patterns is the strongest radiation intensity of the energy radiation device; there is an overlapped portion between the connection pattern and the connected test pattern, the overlapped area of the overlapped portion is less than 10% of the area of each connected test pattern, and the overlapped portion is located at the edge of each connected test pattern; the energy radiation device is a DLP projection system or an LCD liquid crystal screen light source system for curing liquid resin materials by surface exposure; the portion of the connection pattern is simultaneously projected by the energy radiation device; The patterned solidified layer is taken out from the container to obtain the ideal radiation parameter test piece; the ideal radiation parameters and the test radiation parameters respectively include radiation time and radiation intensity.
24. The 3D printing method according to claim 23, characterized in that: Each test pattern has a different identification mark to distinguish each forming block and / or indicate each corresponding ideal radiation parameter.
25. The 3D printing method according to claim 23, characterized in that: Each test pattern is arranged in an array.
26. A 3D printing device, characterized in that: include: A container for holding printing materials; A component platform, located in the container during the printing operation, for accumulating the attached pattern solidified layers layer by layer to form a corresponding 3D component; A Z-axis driving mechanism connected to the component platform and used to adjust the height of the component platform in the Z-axis direction so as to adjust the distance from the component platform to the printing surface during the printing operation; an energy radiation device, located above or below the container, for radiating energy to a printing surface in the container; A control device is connected to the energy radiation device and the Z-axis drive mechanism, and is used to control the energy radiation device and the Z-axis drive mechanism during a printing operation to accumulate an attached solidified layer on the component platform to obtain a corresponding 3D component; and is used to control the energy radiation device during a test operation to perform the 3D printing method as described in any one of claims 16 to 22 or 23 to 25.