A high-precision detection method for optical lens quality
Through the initial inspection and re-inspection method, combined with the use of cooling condensation and colored adhesion liquid, the problem of fingerprint and dust interference in traditional detection is solved, and the efficient and accurate detection of optical lenses is achieved, which significantly improves the detection efficiency.
Patent Information
- Application Number
- CN202210993405.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-18
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2042-08-18
AI Technical Summary
In traditional optical lens detection methods, fingerprints and dust have a great interference to the detection results, especially the minor scratches and fine fingerprints are difficult to distinguish, resulting in low detection efficiency and easy to misjudgment.
The initial inspection and re-examination method are used. The initial inspection obtains the image by irradiating light sources on the cooled and condensed lens to determine the suspected scratches. If there is any suspicion, it will enter the re-examination. During the re-examination, the colored adhesion liquid is scraped on the surface of the lens. To display scratches, shadow contour analysis and traceability analysis are performed in combination with computer image processing.
Effectively avoid fingerprint and dust interference, significantly improve detection efficiency, can quickly and accurately detect scratches on the lens, reduce subsequent inspection workload, and achieve high-precision detection of the lens.
Smart Images

Figure CN115266756B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of lens detection, and in particular to a high-precision detection method for the quality of optical lenses. Background Art
[0002] After optical lenses are manufactured, they need to go through multiple inspection processes, among which scratch inspection is an extremely important part of the inspection process. Traditional scratch detection methods include naked eye inspection, magnified inspection with the help of industrial cameras, etc. However, in traditional inspection methods, fingerprints and dust have a great interference on the inspection results, especially for some fine scratches and fine fingerprints and dust, which are difficult to distinguish quickly even with the help of instrument magnified inspection. On the one hand, it is easy to cause misjudgment of lens quality, and on the other hand, it is also time-consuming. There is a lot of room for improvement in its inspection efficiency. Summary of the invention
[0003] In view of the problems existing in the prior art, the purpose of the present invention is to provide a high-precision detection method for the quality of optical lenses. This high-precision detection method for the quality of optical lenses can avoid the interference of fingerprints and dust on lens detection, and can realize fast and accurate scratch detection on the lenses, which significantly improves the detection efficiency compared with traditional detection methods.
[0004] The above technical objectives of the present invention are achieved through the following technical solutions: a high-precision detection method for the quality of optical lenses, including initial inspection and re-inspection; during the initial inspection, it is determined whether the lens has suspected scratches, if so, it enters the re-inspection, if not, the inspection is completed and a surface-undamaged lens is obtained; scraping a colored attachment liquid on the surface of the lens entering the re-inspection; determining whether the lens has traces of coloring, if so, completing the inspection and obtaining a surface-damaged lens, if not, completing the inspection and obtaining a surface-undamaged lens.
[0005] In some embodiments, the initial inspection step includes: cooling the lens, the cooling temperature is 0℃-10℃; placing the cooled lens in an environment where condensation and fogging can occur, the temperature of the environment where condensation and fogging can occur is 10℃-15℃ higher than the cooling temperature, and the humidity of the environment where condensation and fogging can occur is not less than 75%; directly irradiating the light source onto the lens whose surface has condensed and fogged, and then acquiring an image of the lens through an industrial camera; judging whether the lens has suspected scratches based on the acquired image.
[0006] In some embodiments, the light source is a movable light source. When acquiring the lens image, the light source moves linearly, and each lens is photographed with multiple images by an industrial camera.
[0007] In some embodiments, the lens is dried before the colored adhesive liquid is scraped onto the lens surface.
[0008] In some embodiments, after the lens is completely dried and before the colored attachment liquid is scraped on the surface of the lens, the lens is cooled again at a cooling temperature of 0°C-10°C.
[0009] In some embodiments, the colored attachment liquid is a mixture of glycerin and pigment at a concentration of 35%-50%.
[0010] In some embodiments, after the colored attachment liquid is scraped onto the surface of the lens, an image of the lens is acquired again by an industrial camera, and it is determined whether the lens has any traces of coloring based on the acquired image.
[0011] In some embodiments, reverse checking is also included, and the reverse checking step includes: transferring all images of lenses of the same production batch obtained during the re-inspection process to computer image processing software; reducing the transparency of the image and overlapping all the images to see if there is any shadow. If not, there is no need to continue the reverse checking step. If so, continue with the following reverse checking step; draw the shadow outline on the overlapping image; trace the source and analyze the link where the scratches appear in the shadow according to the size and distribution of these shadow outlines and the depth of the shadows within the outlines.
[0012] In some embodiments, after the shadow outline on the overlapping image is drawn, different colors are filled according to the depth of the shadow within the shadow outline.
[0013] In some embodiments, if it is determined that the lens has tinting marks, the lens is graded based on the number, area, distribution range, and depth of the tinting marks.
[0014] In summary, the present invention has the following beneficial effects:
[0015] This high-precision detection method for the quality of optical lenses performs an initial screening of the lenses through an initial inspection, and selects lenses without even suspected scratches, which greatly reduces the workload of subsequent inspections. During the re-inspection, by scraping the colored attachment liquid on the surface of the lens, on the one hand, fingerprints, dust and other attachments on the lens surface can be scraped clean during the scraping process, and on the other hand, this method can quickly and significantly highlight the scratches on the lens surface, which can not only avoid the interference of fingerprints, dust and other attachments on lens detection, but also realize fast and accurate scratch detection of lenses. Compared with traditional detection methods, this high-precision detection method for the quality of optical lenses has significantly improved the detection efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a flowchart of the present invention. DETAILED DESCRIPTION
[0017] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0018] See also Figure 1 , a high-precision inspection method for the quality of optical lenses, including initial inspection and re-inspection, wherein the initial inspection is used for initial screening of lenses, and lenses with abnormalities on the lens surface that cannot be confirmed to be attachments or scratches are divided into a group, and the lenses in this group are lenses with suspected scratches, and lenses with no abnormalities on the lens surface are divided into another group, and the lenses in this group are lenses without suspected scratches. Lenses with suspected scratches need to be further inspected to determine whether the abnormalities on the lens surface are attachments or scratches, while lenses without suspected scratches do not need to be further inspected, and they have reached the finished product standard. In this way, a large number of lenses that do not need further inspection can be screened out, greatly reducing the workload of subsequent inspections. In general, the initial inspection is used to determine whether the lens has suspected scratches. If so, it will enter re-inspection. If not, the inspection is completed and a lens with a intact surface is obtained.
[0019] The initial inspection can be carried out in the following way: first, cool the lens. The cooling temperature can be adjusted to 10℃. The cooling time can be determined according to the specifications of the lens and the thermal conductivity of the material. During the cooling process, a temperature monitoring mechanism can be used to monitor the temperature of the lens in real time to ensure that the lens can be cooled to the right position. Then put the cooled lens into an environment where condensation and fogging can occur. The ambient temperature where condensation and fogging can occur can be set to 10℃ higher than the cooling temperature. The ambient humidity where condensation and fogging can occur can be set to 75%. When the lens is cooled to the right position, condensation and fogging will occur quickly on the surface of the lens in an environment with a temperature difference of 10℃ and a humidity of 75%. If there is an abnormality on the lens surface, it will be quickly highlighted. Then the light source is directly irradiated on the lens whose surface has condensed and fogged, and the lens image is obtained through the industrial camera. Finally, the technician determines whether the lens has suspected scratches based on the obtained image. The purpose of the industrial camera is to magnify and microscopic the lens surface to clearly observe the outer surface of the lens. It should be noted here that the industrial camera used in this embodiment is a common magnification and microscopy equipment in the field of industrial inspection, which belongs to the existing conventional technology. Therefore, its specific structure, installation position and working principle will not be repeated in this embodiment.
[0020] In the above steps, after the lens is dewed and fogged, the lens surface will change from the original mirror reflection to diffuse reflection, thereby greatly reducing the interference of reflected light when observing the lens, and after the lens is dewed and fogged, the condensation conditions of abnormal areas and normal smooth areas on the lens surface are also different, so that technicians can easily judge whether there are suspected scratches on the lens surface. In order to make the lens dewed and fogged, this embodiment abandons the traditional method of spraying steam or artificial breathing, and instead adopts the method of cooling first and then condensing. One of the reasons is that, after experiments and combined with common sense, it can be known that compared with the method of heating to generate steam and spraying steam onto the lens, the energy consumption of cooling the lens and allowing the lens to condense by itself is relatively small. The method of dewed and fogged lenses in this embodiment can effectively reduce energy consumption. The second reason is that water vapor is dangerous and there is a greater risk of burns during operation, while this embodiment does not require excessive high temperature throughout the process. The third reason is that water vapor needs to be sprayed onto the lens to atomize the lens surface. If the spraying is uneven, the lens atomization will be uneven. In order to achieve uniform spraying of water vapor, the construction cost needs to be increased. The static condensation atomization in the present embodiment is low in cost to construct a cooling and condensation atomization environment. The fourth reason is that continuous spraying of water vapor will be detrimental to the shooting of industrial lenses and may cause obstruction of the field of view. The static condensation atomization method in the present embodiment will not interfere with the shooting of industrial lenses. In addition, the method of atomizing the lens by breathing air is relatively primitive. When there are dozens or hundreds of lenses in a test batch, the method of atomizing by breathing air is obviously not applicable. The atomization method of first cooling the lens and then condensing it in the present embodiment has the advantages of low energy consumption, high safety, uniform atomization and no interference with the shooting of industrial lenses, and is also suitable for large-scale condensation and atomization of lenses.
[0021] In order to show the lens surface more clearly to technicians and reduce omissions, a mobile light source can be used. When acquiring the lens image, the light source moves linearly. Each lens can take multiple images through an industrial camera. In this way, each lens will have clear surface images corresponding to multiple light reflection angles. Technicians can perform a more detailed initial screening of the lenses based on these images to improve the detection effect.
[0022] If the lens that has completed the initial inspection is detected to have suspected scratches on its surface, it will enter the re-inspection. The re-inspection can be carried out in the following methods: first, the lens is dried to remove the condensed droplets on the lens surface. The drying method can be wiped with dry gauze or blown with warm air or a combination of the above two methods, but not limited to this. Then, the colored attachment liquid is scraped on the surface of the lens to make the colored attachment liquid fully and evenly adhere to the surface of the lens. The purpose of drying the lens above is also to reduce the fluidity of the colored attachment liquid on the lens, so as to facilitate the attachment of the colored attachment liquid to the lens. In the process of scraping the colored attachment liquid, on the one hand, the attachments on the surface of the lens (dust, fingerprints, etc.) can be wiped off. , thereby eliminating the interference of attachments on lens scratch detection. On the other hand, if there are scratches on the lens surface, the colored attachment liquid will be scraped into the scratches. Since the lens coating at the scratches has been scraped off, the colored attachment liquid is easily left in the scratches. As the colored attachment liquid is repeatedly and continuously scraped on the lens, the scratches on the lens will become more prominent, thereby showing coloring marks consistent with the scratches. If there are no scratches on the lens surface, the lens will not show coloring marks. The purpose of the above steps is to determine whether the lens has coloring marks. If so, the detection is completed and a lens with damaged surface is obtained. If not, the detection is completed and a lens with intact surface is obtained.
[0023] The colored adhesion liquid can be a mixture of 35% concentration of glycerin and pigment. The color of the pigment is not limited, as long as the color can be easily distinguished by technicians. Glycerin has a certain viscosity, its raw materials are easy to obtain and are non-toxic, non-corrosive, and easily soluble in water. It can adhere to the surface of the lens more firmly and is easy to scrape. After the inspection is completed, the colored adhesion liquid can be washed off by rinsing the lens with clean water, which is very easy to clean.
[0024] In order to further reduce the fluidity of the colored adhesion liquid on the lens, the lens can be cooled again after the lens is completely dried and before the colored adhesion liquid is scraped on the lens surface. The cooling temperature can be set to 0°C. After the lens is cooled, the temperature of the colored adhesion liquid attached to its surface can be reduced, thereby reducing the fluidity of the colored adhesion liquid.
[0025] After the colored attachment liquid is scraped on the surface of the lens, the lens image can be obtained again through the industrial camera, and whether the lens has any traces of coloring can be judged based on the obtained image. If traces of coloring are found on the surface of the lens, it means that the surface of the lens is damaged. If no traces of coloring are found on the surface of the lens, it means that the surface of the lens is intact. It should be noted here that the function and principle of the industrial camera in the re-inspection are the same as those in the initial inspection. Therefore, the relevant content of the industrial camera will not be repeated here.
[0026] The detection method involved in the present invention also includes reverse checking, which can be used to reverse check which processing procedures the scratches on the lens are generated in. The reverse checking can be carried out by the following method: first, all images of the lenses of the same production batch obtained during the re-inspection process are transmitted to the computer image processing software, and then the image transparency is reduced and all the images are overlapped to see whether there is a shadow. If not, there is no need to continue the reverse checking step. If so, continue with the following reverse checking step, then trace the shadow outline on the overlapped image, and finally trace the source and analyze the link where the scratches appear in the shadow according to the size and distribution of the shadow outline and the depth of the shadow within the outline. The smaller the outline (i.e. the more regular the shadow distribution) and the higher the shadow overlap (i.e. the darker the shadow color), the less accidental the scratches are. It can be judged from this that there is a high probability that there is a problem with one or several processing steps of this batch of lenses, resulting in the consistent distribution of scratches on each lens. At this time, traceability and reverse investigation can be carried out to check whether the operation of each process is compliant and whether the equipment of each process is operating normally. During this period, the distribution position of the shadow can be used to specify the processing steps that may cause scratches, thereby achieving more accurate traceability and reverse investigation, so as to achieve timely correction of non-compliant operations or timely repair of problematic equipment.
[0027] In order to more clearly distinguish the depth of the shadow within the shadow outline, after drawing the shadow outline on the overlapping image, different colors can be filled according to the depth of the shadow within the shadow outline.
[0028] Finally, after determining that the lens has traces of coloring, the lens can be graded based on the number, area, distribution range and depth of the coloring traces, and the lens can be reworked or scrapped based on different grading conditions.
[0029] This specific embodiment is merely an explanation of the present invention and is not a limitation of the present invention. After reading this specification, those skilled in the art may make non-creative modifications to the present embodiment as needed. However, as long as they are within the scope of the claims of the present invention, they are protected by the patent law.
Claims
1. A high-precision detection method for optical lens quality, characterized in that: Includes initial inspection and re-inspection; During the initial inspection, determine whether the lens has any suspected scratches. If so, proceed to re-inspection. If not, complete the inspection and obtain a lens with a flawless surface. The initial inspection steps include: Cool the lens at a temperature of 0°C-10°C; Place the cooled lenses in an environment where condensation and fogging can occur. The ambient temperature is 10℃-15℃ higher than the cooling temperature, and the ambient humidity is not less than 75%; Directly shine the light source on the lens whose surface has been condensed and fogged, and then obtain the lens image through an industrial camera; Determine whether the lens has suspected scratches based on the acquired image; Scrape the colored adhesive liquid on the surface of the lens to be re-inspected; Before scraping the colored attachment liquid on the lens surface, first dry the lens. After the lens is completely dried and before scraping the colored attachment liquid on the lens surface, cool the lens again at a cooling temperature of 0°C-10°C. Determine whether the lens has any traces of coloring. If so, complete the test and obtain a lens with damaged surface. If not, complete the test and obtain a lens with intact surface.
2. A high-precision detection method for optical lens quality according to claim 1, characterized in that: The light source is a movable light source. When acquiring the lens image, the light source moves linearly, and each lens is photographed with multiple images by an industrial camera.
3. The method for high-precision detection of optical lens quality according to claim 1, characterized in that: The colored attachment liquid is a mixture of glycerin and pigment in a concentration of 35%-50%.
4. The method for high-precision detection of optical lens quality according to claim 1, characterized in that: After the colored attachment liquid is scraped onto the surface of the lens, the lens image is acquired again through the industrial camera, and the acquired image is used to determine whether the lens has any traces of coloring.
5. The method for high-precision detection of optical lens quality according to claim 4, characterized in that: It also includes reverse checking, and the reverse checking steps include: All images of lenses from the same production batch acquired during the re-inspection process are transferred to computer image processing software; Reduce the image transparency and overlap all images to see if there is a shadow. If not, there is no need to continue the reverse check step. If yes, continue with the following reverse check steps; Outline the shadows on the overlapping images; Based on the size and distribution of these shadow outlines and the depth of the shadows within the outlines, we can trace back and analyze the links where scratches on the shadows appear.
6. A high-precision detection method for optical lens quality according to claim 5, characterized in that: After outlining the shadows on the overlapping images, fill them with different colors depending on the depth of the shadows within the shadow outlines.
7. The method for high-precision detection of optical lens quality according to claim 1, characterized in that: If the lens is determined to have stains, the lens will be graded based on the number, area, distribution range and depth of the stains.