A method for preventing and controlling spontaneous combustion of coal in goaf during shutdown of working face in coal seam prone to spontaneous combustion
Through the regional prevention and control of high-risk areas for coal self-ignition disasters, concrete canvas, high-retaining shisha bubbles and expansion and curing foams, the problems of poor prevention and control and carbon emissions in the existing technology have been solved, and the coal self-ignition disasters have been achieved. efficient prevention and control and low cost effect.
Patent Information
- Application Number
- CN202211127800.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-16
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2042-09-16
AI Technical Summary
The existing technology fails to effectively consider the semi-closed air leakage characteristics of the goaf and the risk of coal self-ignition disasters in different areas in the prevention and control of coal self-ignition disasters, resulting in poor targeted prevention and control and low efficiency, and easy to cause carbon when using liquid carbon dioxide to treat it. Emissions have increased, and the effective utilization of waste flue gas in power plants has not been achieved.
The working surface is divided into different areas, using measures such as hanging concrete canvas, press-injection of high-water-retaining glow bubbles and cooling power plant flue gas, filling expansion and curing foam and lightweight curing filling materials to divide coal spontaneous combustion hazards in different areas. Prevent and control, form flexible compressive windshield walls and sealing walls, and use cooling flue gas to inert and seal.
It significantly improves the prevention and control efficiency of coal spontaneous combustion disasters, reduces the possibility of coal spontaneous combustion disasters, reduces carbon emissions, realizes long-lasting storage and efficient prevention and control of goafs, and reduces prevention and control costs.
Smart Images

Figure CN115355041B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of methods for preventing and controlling coal spontaneous combustion disasters in mines, and in particular to a method for preventing and controlling coal spontaneous combustion in goaf areas during shutdown of a working face in a coal seam prone to spontaneous combustion. Background Art
[0002] Coal is currently the most important energy source in my country. As of 2020, there are still more than 4,700 coal mines across the country, of which 49% are affected by the combined thermal-dynamic disasters of coal spontaneous combustion and gas; in addition, with the increase in coal mining depth, the geological conditions of the mines and the coal seam occurrence conditions are complex, and high gas and high ground temperature make coal seam mining face serious threats of thermal-dynamic disasters such as coal spontaneous combustion.
[0003] Especially in the mining process of high-gas and self-igniting coal seams, due to air leakage in the working face, it is very easy to cause coal spontaneous combustion disasters in the hidden area of the goaf behind the support, thereby inducing thermal dynamic disasters such as gas explosion in the goaf. Especially when the working face needs to be shut down for a long time due to fault crossing, equipment maintenance, holiday adjustment, and support withdrawal, gas accumulation areas are easily formed in the goaf. At the same time, the coal left in the goaf is very easy to oxidize and accumulate heat under air leakage conditions, eventually causing coal spontaneous combustion and other accidents, which seriously threatens the safety of the working face of the self-igniting coal seam during the shutdown period.
[0004] In terms of methods and technologies for preventing and controlling coal spontaneous combustion disasters in goafs, water, yellow mud, inert gas (N2, CO2), plugging materials, inhibitors, three-phase foam, fine water mist, etc. are currently mainly used. For example, CN110173294A discloses a method for controlling hidden disasters in coal mine goafs, which uses a method of spraying an aqueous solution of CaCl2 and perfusing an inert gas, and at the same time perfusing N2 and atomized CaCl2 aqueous solution in combination with the method of pre-buried pipelines in the goafs, so that the goafs of coal mines eventually do not meet the conditions of spontaneous combustion of coal and gas explosion. The above invention uses inhibitors and inert gas technology to control hidden disasters in goafs, but does not take into account the semi-enclosed air leakage characteristics of goafs, and the different roof collapse and compaction degrees in different areas of the goafs behind the working face, resulting in a high probability of coal spontaneous combustion disasters in the two sides of the areas close to the air inlet and return tunnels, while the possibility of coal spontaneous combustion disasters in the goafs behind the middle of the working face is relatively small, which ultimately leads to poor pertinence and low implementation efficiency of the applied technology in the process of preventing and controlling coal spontaneous combustion disasters. At the same time, the current application of liquid carbon dioxide to control coal spontaneous combustion disasters in goafs can easily cause carbon dioxide to escape with the wind and eventually flow into the atmosphere, resulting in increased carbon emissions from mines, which is not in line with the country's strategic goals of solid waste utilization and carbon emission reduction. Therefore, how to achieve the prevention and control of coal spontaneous combustion disasters by CO2 inert gases such as waste flue gas from power plants and their long-term storage in underground spaces is the focus of future field research and application. Summary of the invention
[0005] The purpose of the present invention is to provide a method for preventing and controlling coal spontaneous combustion in the goaf during the shutdown of a working face in a coal seam prone to spontaneous combustion. According to the different degrees of coal spontaneous combustion disaster dangers in different areas of the goaf behind the working face, targeted prevention and control measures are taken in different areas, such as hanging concrete canvas to reduce air leakage, injecting high-water-retaining flue gas foam to cover and isolate oxygen, injecting cooling power plant flue gas to cool and inertate, injecting expanding and solidifying foam to fill and plug leaks, and injecting lightweight solidifying filling materials to condense and reinforce. This can significantly improve the prevention and control efficiency of thermal dynamic disasters such as coal spontaneous combustion during the shutdown of a working face in a coal seam prone to spontaneous combustion.
[0006] To achieve the above object, the present invention provides a method for preventing and controlling spontaneous combustion of coal in goaf during shutdown of a working face of a self-igniting coal seam, and the specific steps are as follows:
[0007] Step 1), along the inclination direction of the coal mining face, the face is divided into three sections based on the inclination length when production is stopped, and are respectively recorded as section A1, section A2 and section A3; section A1 is close to the air inlet lane of the coal mining face, section A3 is close to the air return lane of the coal mining face, and section A2 is the middle area of the coal mining face;
[0008] Step 2), a concrete canvas is hung at the wind inlet corner of the A1 section and a windbreak wall is formed after water spraying and solidification; furthermore, no more than 5 brackets are spaced apart at a time in the A1 section, and a high-level measure drilling hole for injecting high-water-retaining flue gas foam and cooling the flue gas of the power plant is constructed in the goaf behind the bracket, the drilling hole is perpendicular to the inclination of the working face, and the final hole position is designed to be within the fracture zone of the goaf and the horizontal distance from the bracket is within 15-20 meters; in addition, using the gaps between the brackets in the A1 section, a plurality of 1-inch steel pipes with a length of 3-5 meters are inserted into the rear goaf at a 45° angle perpendicular to the inclination of the working face and with the bracket base, and the steel pipes are used as plugging holes to inject expanding and solidifying foam behind the bracket; no more than 2 brackets are allowed between the two inserted steel pipes;
[0009] Step 3), using the gaps between the supports in the A2 section, insert multiple 1-inch steel pipes of 3-5 meters in length into the rear goaf at a 45° angle perpendicular to the inclination of the working face and with the support base, and use the steel pipes as plugging holes to pour lightweight solidified filling materials into the broken rock mass in the goaf behind the supports to form a plugging wall; no more than 2 supports are allowed between the 2 inserted steel pipes;
[0010] Step 4), pre-buried inert gas and grouting 4-inch pipelines in the air inlet corner area of the A3 section, and hung concrete canvas at the return air corner of the A3 section and formed a windbreak wall after water spraying and solidification; furthermore, in the A3 section, no more than 5 brackets are spaced apart at a time, and a high-level measure drilling hole for injecting high-water-retaining flue gas foam and cooling the flue gas of the power plant is constructed in the goaf behind the bracket. The drilling hole is perpendicular to the inclination of the working face, the final hole position needs to be designed in the fracture zone of the goaf, and the horizontal distance from the bracket is within 15-20 meters; in addition, using the gaps between the brackets in the A3 section, a plurality of 3-5 meter long 1-inch steel pipes are inserted into the rear goaf at a 45° angle perpendicular to the inclination of the working face and with the bracket base, and the steel pipes are used as plugging holes to inject expanding and solidifying foam behind the bracket; no more than 2 brackets are allowed between the two inserted steel pipes;
[0011] Step 5), hang flame-retardant air duct cloth to wrap all the supports in the A1 section and the A3 section to reduce air leakage from the coal mining working surface to the rear goaf.
[0012] As a preferred embodiment of the present invention, in step 2) and step 4), the upper fabric layer and the lower fabric layer of the concrete canvas are both highly flame retardant polyphenylene sulfide fibers, the middle fiber layer is flame retardant antistatic polyester fibers, and the cement filled in the middle fiber layer is aluminate refractory cement.
[0013] As a preferred embodiment of the present invention, the high water retention flue gas foam and power plant flue gas in step 2) and step 4) are both cooled low-temperature flue gas treated by a mine-specific air cooler, and the treated flue gas temperature is lower than 25°C.
[0014] As a preferred embodiment of the present invention, the high water retention flue gas foam described in step 2) and step 4) is prepared by using water, animal protein foaming agent, sodium bicarbonate, and water glass as raw materials, and the mass ratios are 72-86, 1-3, 8-15, and 5-10, and the mixture is introduced into the cooling power plant flue gas after being dissolved and stirred once and mixed sufficiently. Among them, the animal protein foaming agent is prepared by using keratin from the hoof and horn of cattle, horses, etc. as raw material; the water retention period of the high water retention flue gas foam can reach more than 6 months, and after the foam loses water and breaks, the flue gas CO2 wrapped in the bubbles will be released to achieve the inerting of the goaf, and at the same time, the high water retention gel formed by the foam can permanently adhere to the coal and isolate oxygen.
[0015] As a preferred embodiment of the present invention, the expansion solidification foam in step 2) and step 4) is prepared from water, ordinary silicate cement, sodium carboxymethyl cellulose, sodium bicarbonate, and aluminum sulfate in a mass ratio of 35-40:45-50:2-5:3-5:5-10, and is dissolved once and rapidly stirred and expanded for 5-10 minutes. The expansion solidification foam has a foaming multiple of up to 5 times, does not release heat during the injection filling process, has a good bonding and solidification effect on loose coal and rock, and the solidification time is 10-30 minutes.
[0016] As a preferred embodiment of the present invention, the lightweight solidifying filling material in step 3) is prepared from water, ordinary Portland cement, grade tertiary fly ash, ceramsite and water glass as raw materials, and is mixed at a mass ratio of 50-60:20-30:2-5:3-10:5-15 and quickly stirred for 3-5 minutes. The bonding and solidification time of the lightweight solidifying filling material to the broken rock mass is 5-15 minutes.
[0017] Compared with the prior art, the present invention has the following beneficial effects:
[0018] 1. The present invention divides the working face of the self-igniting coal seam into three disaster prevention and control sections, A1, A2 and A3, according to the different degrees of coal spontaneous combustion hazards during the shutdown period. Since the A1 and A3 areas are adjacent to the air inlet and return tunnels, resulting in large air leakage and the highest possibility of coal spontaneous combustion disasters, a flexible and compressive permanent windbreak wall is constructed by hanging concrete canvas, which can effectively reduce the problems of windbreak wall fracturing and secondary air leakage caused by mine pressure or roof disturbance; at the same time, the concrete canvas has high strength and good density after curing, which can effectively prevent the toxic and harmful gases inside the goaf from gushing to the working face. In addition, in view of the problem that the roof in the goaf behind the supports in the A1 and A3 sections is not fully collapsed, resulting in large porosity and many air leakage channels in the goaf behind, in order to reduce the possibility of high temperature hazards caused by oxidation and heat accumulation of residual coal in the goaf behind these two dangerous sections, high-level construction measures are taken to drill holes and inject high-water-retaining flue gas foam within 15-20 meters of the goaf behind the supports. The strong diffusivity and high water retention of the foam can achieve wetting coverage of the residual coal within 5-30m behind the goaf for up to 6 months. After the foam loses water and bursts, it will release the flue gas CO2 wrapped in the bubbles to achieve inerting of the goaf. At the same time, the high-water-retaining gel formed by the foam can permanently adhere to the residual coal and isolate oxygen, preventing the oxidation and spontaneous combustion of the residual coal from causing gas in the goaf and other thermal dynamic disasters. In addition, when there is a high-temperature hazard of coal spontaneous combustion in the goaf behind the support, the high-level construction measures can also be used to drill holes and inject a large flow of cooled power plant flue gas to quickly cool down the high-temperature hazard and eliminate the high-temperature point of coal spontaneous combustion. Next, in order to prevent the cracks behind the supports in the A1 and A3 sections of the working face from leaking into the goaf, a plugging borehole was formed by inserting a pipe to inject non-heat-releasing, non-combustible expanding solidifying foam behind the supports, thereby achieving a large-scale, full-area plugging of the air leakage cracks within 3-5 meters behind the supports. Finally, all the supports in the A1 and A3 sections were wrapped with hanging flame-retardant wind tube cloth, thus completely eliminating air leakage in the goaf and fundamentally eliminating the possibility of coal spontaneous combustion disasters in the A1 and A3 sections.
[0019] 2. The high water-retention flue gas foam proposed in the present invention uses the waste flue gas of the power plant as the foam gas source, which not only reduces the high cost of nitrogen generators and high foam application costs caused by the traditional mine using nitrogen as the gas source, but also uses a special air cooler in the mine to treat the flue gas from the power plant to obtain cooled low-temperature flue gas with a temperature below 25°C, which is used as inert gas to fill and inertify the goaf, thereby achieving the cooling and inerting of the goaf, and realizing the dual functions and effects of preventing and controlling coal spontaneous combustion disasters in mines and sealing CO2 in flue gas in underground goafs. In addition, the present invention proposes to use sodium bicarbonate, water glass, animal protein foaming agent and the like as raw materials for high water-retention flue gas foam, wherein the addition of sodium bicarbonate significantly reduces the solubility of major acid gases such as CO2 in flue gas in the bubble liquid film, delaying processes such as bubble coarsening and decay; at the same time, sodium bicarbonate and water glass cross-link in the foam liquid film to form a high water-retention gel material, thereby achieving the locking of moisture and long-term wrapping of flue gas, and the cooled low-temperature flue gas with a temperature below 25°C helps to reduce the thermodynamic drainage of the foam liquid film, enhance the stability of the high water-retention flue gas foam, and extend the water retention time of the high water-retention flue gas foam to more than 6 months, thereby achieving long-term coverage and moistening of the coal left in the goaf, and having the function and effect of long-term prevention and control of spontaneous combustion of coal in the goaf.
[0020] 3. The present invention proposes a method for preventing and controlling spontaneous combustion of coal in goaf areas in sections during shutdown of the working face, which realizes effective division and classification of high-risk areas and low-risk areas for efficient prevention and control. For the high-risk A1 and A3 sections, a method combining high-level construction measures of drilling holes and inserting pipes to form short holes is adopted to achieve complete wetting coverage and efficient oxygen isolation of the remaining coal within 5-30 meters of the goaf behind the supports in these two areas, as well as complete blocking of air leakage cracks within 3-5 meters. After the supports in the two sections are completely wrapped with flame-retardant wind tube cloth, the possibility of spontaneous combustion of coal in the goaf behind these two dangerous areas is completely eliminated. In addition, for the A2 section where the possibility of thermal dynamics occurring during the shutdown of the working face is relatively small, a 3-5 meter long 1-inch steel pipe is inserted into the rear goaf at a 45° angle perpendicular to the inclination of the working face and to the base of the support through the gaps between the supports in the A2 section as a plugging drill hole, and the inserted steel pipe is used to pour a fast-setting lightweight solidifying filling material made of water, ordinary Portland cement, grade tertiary fly ash, expanded clay, and water glass into the broken rock mass in the goaf behind the support. The material has low cost and fast curing time. Low-cost, fast-curing lightweight solidifying filling materials are used to seal and bond the broken rocks in the goaf behind the supports in the A2 section to seal the tiny air leakage cracks in this area. The lightweight solidifying filling material has a small extrusion force on the support, and the support is subjected to a small external load, which can protect the support well. In addition, since the filling material contains lightweight expanded clay, which has extremely strong acid and alkali resistance and a porosity of 50-75%, an isolation zone with high porosity and good thermal insulation can be formed after the filling material is solidified. Once thermal dynamic disasters such as spontaneous combustion of coal occur in the goaf of the A2 section, it can effectively isolate the heat from surging to the working face, showing excellent leak-proofing, oxygen isolation and high-efficiency thermal insulation effects.
[0021] 4. The present invention adopts different technologies to carry out zoning management for different areas with different risk levels. According to the characteristics of coal spontaneous combustion disasters in each section, a targeted prevention and control method with multiple measures coordinated can effectively reduce the waste and consumption of manpower, material resources and resources caused by blind construction drilling and large-scale use of high-cost materials, greatly reducing the cost of prevention and control of coal spontaneous combustion disasters in coal mines, and significantly improving the efficiency of prevention and control of coal spontaneous combustion disasters during the shutdown of the working face. At the same time, the present invention uses a flexible, pressure-resistant permanent windbreak wall formed by concrete canvas, and a blocking wall formed by expanded solidified foam and lightweight solidified filling materials, etc., which can effectively block the goaf to form a closed space, and confine the inert gas such as cooling power plant flue gas in the goaf to prevent it from being lost in the air, so as to achieve the effect of long-term inerting the goaf and reducing carbon emissions. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a schematic diagram of the division of dangerous sections of a method for preventing and controlling spontaneous combustion of coal in goaf during shutdown of a working face of a self-igniting coal seam according to the present invention;
[0023] In the figure: 1- coal mining working face; 2- air inlet tunnel; 3- air inlet corner; 4- concrete canvas one; 5- goaf; 6- concrete canvas two; 7- return air corner; 8- support; 9- return air tunnel; 10- A1 section; 11- A2 section; 12- A3 section. DETAILED DESCRIPTION
[0024] The present invention will be further described below in conjunction with the embodiments and drawings.
[0025] Implementation background: A mine in Pingmei is a high-gas, self-igniting mine. 16-17 The coal seam is low in sulfur, low in ash, high in calorific value, 1 / 3 coking coal, raw coal ash content is 13-16%, moisture content is 1.53%, apparent density is 1.36m 3 / t, belongs to oneself 16-17 The coal seam is prone to spontaneous combustion, with an ignition period of 1-3 months. The coal seam is explosive, with an explosion index of 32.32%. A fully mechanized mining face in this coal seam has a mineable strike length of 620m and an inclined width of 126.3m, with a total of 93 hydraulic supports. A large amount of residual coal is left in the goaf of the face. At the same time, the advancement speed of the face is slow during the fault, and the residual coal in the goaf is fully oxidized and heat is stored. The face was shut down on December 16, 2020, and was ready to start making rack space. It is expected to be shut down for 45 days until it is closed. When the face was shut down, the CO concentration in the return air corner reached more than 80ppm, and the CO concentration still had a trend of continuing to increase, indicating that the residual coal in the goaf behind the support has begun to oxidize to form heat accumulation. If it develops further, it may form a high-temperature oxidation point of coal, which will eventually lead to thermal disasters such as coal spontaneous combustion and gas explosion.
[0026] In order to effectively prevent and control the spontaneous combustion of coal in the goaf of the working face, the mine adopts a method for preventing and controlling spontaneous combustion of coal in the goaf during the shutdown of the working face of the self-igniting coal seam proposed by the present invention. The specific steps are as follows:
[0027] Step 1) Figure 1 As shown, the width of the coal mining face 1 along the inclination direction is 126.3m, which is equally divided into three sections, each of which is 42.1m. According to the serial number of the support 8 of the face (#1 to #93), the area where the 30 supports 8 of #1-#31 are located is recorded as A1 section 10, the area where the 30 supports 8 of #32-#62 are located is recorded as A2 section 11, and the area where the 30 supports 8 of #63-#93 are located is recorded as A3 section 12. Among them, the A1 section 10 is close to the coal mining face air intake lane 2, the A3 section 12 is close to the coal mining face return air lane 9, and the A2 section 11 is the middle area of the coal mining face. On this basis, according to the different degrees of risk of coal spontaneous combustion disasters in the goaf behind the three sections of the coal mining face, targeted coal spontaneous combustion disaster prevention and efficient control measures are taken.
[0028] Step 2) A concrete canvas 4 is hung at the wind inlet corner 3 in the A1 section 10 and sprayed with water and solidified to form a windbreak wall with flexible pressure resistance effect; furthermore, 5 supports 8 are spaced apart in the A1 section 10 each time, and a high-position measure borehole for injecting high-water-retaining flue gas foam and cooling the flue gas of the power plant is constructed in the goaf 5 behind the support 8. The borehole is perpendicular to the inclination of the working face, and the final hole position needs to be designed in the fracture zone of the goaf 5, and the horizontal distance from the support 8 is within 18 meters. A total of 6 high-position measure boreholes are constructed in the A1 section 10; in addition, by utilizing the gaps between the supports 8 in the A1 section 10, a 5-meter-long 1-inch steel pipe is inserted into the rear goaf 5 at a 45° angle to the inclination of the working face for every 2 supports 8, and the steel pipe is used as a plugging borehole to inject non-exothermic, non-combustible expanding and solidifying foam behind the support 8. A total of 15 plugging boreholes are formed in the A1 section 10 by inserting pipes.
[0029] Step 3), utilizing the gaps between the supports 8 in the A2 section 11, insert a 5-meter-long 1-inch steel pipe into the rear goaf 5 at a 45° angle to the base of the support 8, perpendicular to the inclination of the working face, for every three supports 8, and use the steel pipe as a plugging borehole to pour fast-setting lightweight solidifying filling material into the broken rock mass of the goaf 5 behind the support 8. A total of 15 plugging boreholes are formed by inserting pipes in the A2 section 11.
[0030] Step 4), pre-buried inert gas and grouting 4-inch pipelines in the air inlet corner 3 area in the A3 section 12, and hung concrete canvas 2 6 at the return air corner 7 in the A3 section 12 and formed a windbreak wall with flexible pressure resistance after water spraying and curing; furthermore, in the A3 section 12, 5 brackets 8 are spaced each time, and a high-level measure drilling hole for pressurizing high-water-retaining flue gas foam and cooling the flue gas of the power plant is constructed in the goaf 5 behind the bracket 8. The drilling hole is perpendicular to the inclination of the working face and the final hole position needs to be designed. A total of 6 high-position measure boreholes were constructed in the A3 section 12 within the fracture zone of the goaf 5 and within a range of 18 meters horizontally away from the support 8. In addition, utilizing the gaps between the supports 8 in the A3 section 12, a 5-meter-long 1-inch steel pipe was inserted into the rear goaf 5 perpendicular to the inclination of the working face and at an angle of 45° to the support base for every 3 supports 8. The steel pipe was used as a plugging borehole and non-exothermic, non-combustible expanding and curing foam was injected behind the support 8. A total of 15 plugging boreholes were formed in the A3 section 12.
[0031] Step 5), hang flame retardant wind duct cloth to wrap all the supports 8 in the A1 section 10 and the A3 section 12 to reduce air leakage from the coal mining working surface to the rear goaf; the flame retardant wind duct cloth should be hung with the bottom and top visible, and needs to be wrapped from the bottom end of the support 8 to the front beam of the support 8.
[0032] Among them, the upper fabric layer and the lower fabric layer of the concrete canvas 1 4 described in step 2) and the concrete canvas 2 6 described in step 4) are both highly flame retardant polyphenylene sulfide fibers, the middle fiber layer is flame retardant antistatic polyester fiber, and the cement filled in the middle fiber layer is aluminate refractory cement.
[0033] The high water retention flue gas foam is prepared from water, animal protein foaming agent, sodium bicarbonate and water glass as raw materials, in a mass ratio of 72:3:15:10, after being dissolved once, stirred and introduced into the cooling power plant flue gas for sufficient mixing. Among them, the animal protein foaming agent is prepared from keratin from cow hoof horns; the water retention period of the high water retention flue gas foam can reach more than 6 months, and after the foam loses water and breaks, the flue gas CO2 wrapped in the bubbles will be released to inertify the goaf, and the high water retention gel formed by the foam can permanently adhere to the coal and isolate oxygen.
[0034] The expansion solidification foam is prepared from water, ordinary silicate cement, sodium carboxymethyl cellulose, sodium bicarbonate and aluminum sulfate in a mass ratio of 40:50:2:3:5, after one-time dissolution and rapid stirring and expansion for 5-10 minutes. The expansion solidification foam has an expansion multiple of up to 5 times, does not release heat during the injection filling process, has a good bonding and solidification effect on loose coal and rock, and has a solidification time of 10-30 minutes.
[0035] The lightweight solidifying filling material described in step 3) is prepared from water, ordinary silicate cement, tertiary fly ash, ceramsite and water glass as raw materials, and is mixed at a mass ratio of 60:30:2:3:5 and quickly stirred for 3-5 minutes. The bonding and solidification time of the lightweight solidifying filling material to the broken rock mass is 5-15 minutes.
[0036] After utilizing the method for preventing and controlling coal spontaneous combustion in the goaf during the shutdown of a working face in a coal seam prone to spontaneous combustion proposed by the present invention, targeted multi-measure coordinated prevention and control methods are adopted according to the characteristics of coal spontaneous combustion disasters in the three sections of the working face, so that the CO concentration at the return air corner position of the working face of the coal seam prone to spontaneous combustion is reduced from 80ppm to below 20ppm, and finally stabilized at 0ppm, indicating that the oxidation of residual coal and high temperature hazards in the goaf behind the support during the shutdown of the working face were effectively suppressed, thereby completely eliminating the possibility of coal spontaneous combustion disasters during the 45-day shutdown of the working face. Finally, all equipment of the working face was safely evacuated smoothly, and no thermal dynamic disasters such as coal spontaneous combustion occurred during the shutdown period.
[0037] The above is only a preferred implementation method of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A method for preventing and controlling spontaneous combustion of coal in goaf during shutdown of a self-igniting coal seam working face, characterized in that: The specific steps are as follows: Step 1), along the inclination direction of the coal mining face, the working face is divided into three sections based on the inclination length at the time of shutdown, which are respectively recorded as Section A1, Section A2 and Section A3; Section A1 is close to the air inlet lane of the coal mining face, Section A3 is close to the air return lane of the coal mining face, and Section A2 is the middle area of the coal mining face; Step 2), hang concrete canvas at the wind inlet corner in the A1 section and form a windbreak wall after spraying water and curing; furthermore, no more than 5 brackets are spaced apart at a time in the A1 section, and a high-level measure drilling hole for injecting high-water-retaining flue gas foam and cooling the flue gas of the power plant is constructed in the goaf behind the bracket. The drilling hole is perpendicular to the inclination of the working face, and the final hole position is designed to be within the fracture zone of the goaf and within the horizontal distance of 15-20 meters from the bracket; in addition, using the gaps between the brackets in the A1 section, insert multiple 3-5 meter long 1-inch steel pipes into the rear goaf at a 45° angle to the inclination of the working face and the bracket base, and use the steel pipes as a plugging borehole to inject expanding and curing foam behind the bracket; no more than 2 brackets are allowed between the two inserted steel pipes; Step 3), using the gaps between the supports in the A2 section, insert multiple 3-5 meter long 1-inch steel pipes into the rear goaf at a 45° angle perpendicular to the inclination of the working face and with the support base, and use the steel pipes as plugging holes to pour lightweight solidified filling materials into the broken rock mass in the goaf behind the supports to form a plugging wall; no more than 2 supports are allowed between the 2 inserted steel pipes; Step 4), in the air inlet corner area of the A3 section, a 4-inch pipeline for inert gas and grouting is pre-buried, and a concrete canvas is hung at the return air corner in the A3 section, and a windbreak wall is formed after water spraying and solidification; furthermore, in the A3 section, no more than 5 brackets are spaced each time, and a high-level measure drilling hole for injecting high-water-retaining flue gas foam and cooling the flue gas of the power plant is constructed in the goaf behind the bracket. The drilling hole is perpendicular to the inclination of the working face, and the final hole position needs to be designed in the fracture zone of the goaf, and the horizontal distance from the bracket is within 15-20 meters; in addition, using the gaps between the brackets in the A3 section, a number of 3-5-meter-long 1-inch steel pipes are inserted into the rear goaf at a 45° angle perpendicular to the inclination of the working face and with the bracket base, and the steel pipes are used as plugging holes to inject expanding and solidifying foam behind the bracket; no more than 2 brackets are allowed between the two inserted steel pipes; The high water retention flue gas foam in step 2) and step 4) is prepared by using water, animal protein foaming agent, sodium bicarbonate and water glass as raw materials, in a mass ratio of 72-86, 1-3, 8-15 and 5-10, and is dissolved at one time, stirred and introduced into the cooling power plant flue gas for sufficient mixing; Step 5) Hang flame-retardant air duct cloth to wrap all supports in Section A1 and Section A3 to reduce air leakage from the coal mining working surface to the rear goaf.
2. According to the method for preventing and controlling spontaneous combustion of coal in goaf during shutdown of coal seam working face prone to spontaneous combustion according to claim 1, it is characterized in that: The upper fabric layer and the lower fabric layer of the concrete canvas in step 2) and step 4) are both highly flame-retardant polyphenylene sulfide fibers, the middle fiber layer is flame-retardant antistatic polyester fibers, and the cement filled in the middle fiber layer is aluminate refractory cement.
3. The method for preventing and controlling spontaneous combustion of coal in goaf during shutdown of a self-igniting coal seam working face according to claim 1 is characterized in that: The high water-retention flue gas foam and power plant flue gas in step 2) and step 4) are both cooled low-temperature flue gases treated by a mine-specific air cooler, and the treated flue gas temperature is lower than 25°C.
4. The method for preventing and controlling spontaneous combustion of coal in goaf during shutdown of a self-igniting coal seam working face according to claim 1 is characterized in that: The expansion solidification foam in step 2) and step 4) is prepared from water, ordinary silicate cement, sodium carboxymethyl cellulose, sodium bicarbonate and aluminum sulfate as raw materials in a mass ratio of 35-40:45-50:2-5:3-5:5-10, and is dissolved once and rapidly stirred and expanded for 5-10 minutes.
5. The method for preventing and controlling spontaneous combustion of coal in goaf during shutdown of a self-igniting coal seam working face according to claim 1 is characterized in that: The lightweight solidifying filling material in step 3) is prepared from water, ordinary silicate cement, grade tertiary fly ash, ceramsite and water glass as raw materials, and is mixed at a mass ratio of 50-60:20-30:2-5:3-10:5-15 and quickly stirred for 3-5 minutes. The bonding and solidification time of the lightweight solidifying filling material to the broken rock mass is 5-15 minutes.