A method for recycling low-quality glyphosate materials
By dissolving low-quality glyphosate materials in liquid alkali and using nano-sustained-release decolorizer and acidification treatment, the dilemma of processing low-quality glyphosate materials has been successfully solved, and the recycling of high-quality glyphosate raw powder has been achieved to meet environmental protection and economic needs. Benefit requirements.
Patent Information
- Application Number
- CN202211055991.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-31
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-08-31
AI Technical Summary
Because low-quality glyphosate materials contain industrial salts and mechanical impurities, they are difficult to crush or dry, making them impossible to process and causing accumulation difficulties. Moreover, traditional methods cannot meet environmental protection requirements and quality assurance.
Dissolve the low-quality glyphosate material in liquid alkali, remove mechanical impurities through filtration, use a decolorizing agent for decolorization, and then extract high-quality glyphosate raw powder through acidification and crystallization, using nano-sustained release decolorizing agents and appropriate acidification to ensure Product purity and whiteness.
Efficient recycling of low-quality glyphosate materials has been achieved. The quality of the glyphosate raw powder produced is no different from that of normal production. It has considerable economic benefits and meets environmental protection and quality requirements.
Smart Images

Figure CN115368409B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of glyphosate low-quality material processing methods, and specifically is a method for producing glyphosate raw powder by recycling glyphosate low-quality materials. Background Art
[0002] Glyphosate is the largest and fastest growing systemic herbicide in the world. With the continuous consumption of oil in the world, the rise of bio-alternative energy, and the successful promotion and use of genetically modified crops resistant to glyphosate, it provides a good opportunity for glyphosate production. Glyphosate production mainly includes the alkyl aminoacetate method and the IDA method. The alkyl aminoacetate method is the most common in China. The raw materials for the alkyl aminoacetate method are polyformaldehyde (formaldehyde), aminoacetic acid, dimethyl phosphite, triethylamine, methanol, hydrochloric acid, and sodium hydroxide. The depolymerization of polyformaldehyde is catalyzed by triethylamine. After depolymerization, addition, condensation, and hydrolysis reactions, and after removing the solvent and excess hydrochloric acid, glyphosate crystals are precipitated, filtered and washed, and the filter cake is glyphosate acid. The filtrate is called glyphosate acid mother liquor, and the mother liquor output is about 2-6 tons / raw powder. The filtrate, i.e. the mother liquor, is immediately pumped into the mother liquor tank for static precipitation. After 1-2 months of static precipitation, the upper mother liquor is extracted for other comprehensive utilization treatments. The bottom of the glyphosate low-quality tank powder agglomerated, the precipitation amount is 65 tons / 10,000 tons of raw powder, the production capacity of 150,000 tons of equipment produces 1,000 tons of tank powder per year, the low-quality material contains 60%-70% glyphosate, industrial salt (sodium chloride) 5%-10%, water 5%-10%, and the rest is mechanical impurities, COD, N-NH3, microorganisms and algae, etc. Since the glyphosate low-quality material contains industrial salt and is in block form, it is not easy to crush or dry. It does not meet environmental protection requirements and quality assurance to dissolve it through ammonia or drop isopropylamine to prepare glyphosate ammonium salt solution or isopropylamine salt solution, so it has been piled up and cannot be processed. Summary of the invention
[0003] In view of the dilemma of the accumulation of low-quality glyphosate materials that cannot be processed, the purpose of the present invention is to design and provide a technical solution for a method for extracting high-quality glyphosate raw powder by dissolving low-quality glyphosate materials in liquid alkali, reducing and decolorizing, and acidifying and crystallizing glyphosate by utilizing the characteristic that glyphosate acid can be dissolved in liquid alkali. The glyphosate powder is firstly dissolved in liquid alkali, mechanical impurities in the low-quality materials are removed by filtering, the low-quality material solution is decolorized by using a decolorizer, and finally hydrochloric acid is added to acidify and crystallize glyphosate crystals, and high-quality glyphosate raw powder is obtained after filtering.
[0004] The method for producing glyphosate raw powder by recycling low-quality glyphosate materials is characterized by comprising the following process steps:
[0005] (1) Add block or granular low-quality materials and water into reactor A, and add liquid alkali while stirring to neutralize until the low-quality materials in the reactor are completely dissolved. The resulting solution is glyphosate solution A.
[0006] The glyphosate low-quality material refers to the liquid remaining after the glyphosate crystals are filtered out by acidification and crystallization during the production of glyphosate by the glycine method, which is the glyphosate mother liquor. The glyphosate mother liquor is first stored in a mother liquor tank for cooling and standing, and the solid matter is deposited at the bottom of the mother liquor tank. The main components of the solid matter are glyphosate 60%-70%, industrial salt 5%-10%, water 5%-10%, and the rest includes mechanical impurities, COD, N-NH3, and microbial algae.
[0007] The liquid alkali includes sodium hydroxide solution, potassium hydroxide solution, ammonia water or dimethylamine solution, and flake alkali or caustic soda can also be added.
[0008] The concentration of the sodium hydroxide solution is 30% to 55%, preferably 30% to 40%, and more preferably 32%; the concentration of the caustic soda is 20% to 99%, preferably 80% to 90%.
[0009] The concentration of potassium hydroxide solution is 40% to 55%, preferably 40% to 45%; the concentration of caustic soda flakes is 80% to 95%, preferably 90% to 95%.
[0010] The dimethylamine solution is a 40% aqueous solution.
[0011] The concentration of ammonia water is 25% to 28%, preferably 25%.
[0012] (2) filtering the glyphosate solution A obtained in step (1) through a plate and frame filter press, and the solution obtained after filtration is glyphosate solution B;
[0013] Here, glyphosate solution B is a turbid liquid, showing green or light yellow color.
[0014] (3) The glyphosate solution B obtained in step (2) is pressed into a reaction kettle B, and 0.6-1‰ of a decolorizing agent is poured into the reaction kettle while stirring. After continuing to stir for 10 minutes, the solution in the kettle is taken for colorimetry. When the color of the solution becomes clear and transparent, a glyphosate solution C is obtained;
[0015] The amount of decolorizer added here will depend on the amount of impurities contained in the low-quality material. Generally, 0.6‰ of the solution volume is added first, and then gradually added as needed after color comparison.
[0016] After sampling here, the solution should be placed in a test tube with a diameter of 2.5 cm and compared with the color of the standard solution in the same test tube. It is feasible to achieve the same color and clarity. Otherwise, decolorizing agent needs to be added.
[0017] The decolorizing agent is a nano slow-release decolorizing agent formed by ferrous sulfate and Bacillus subtilis.
[0018] The preparation method of the nano slow-release decolorizer formed by ferrous sulfate and Bacillus subtilis comprises the following steps: immersing silicon-based nano microcapsules in a mixed aqueous solution formed by a ferrous sulfate solution and Bacillus subtilis in a supergravity reactor, stirring the mixed aqueous solution at a speed of 500-800 r / min for 2-4 hours, so that the mixed aqueous solution is fully infused into the silicon-based nano microcapsules; and vacuum filtration, water injection cleaning, and drying to obtain the nano slow-release decolorizer.
[0019] As a preferred embodiment, a method for preparing a nano slow-release decolorizing agent formed by ferrous sulfate and Bacillus subtilis is provided, which comprises the following steps: immersing a dilute solution of ferrous sulfate and Bacillus subtilis in a silicon-based nano microcapsule through a supergravity device, stirring the mixture at a speed of 800 r / min for 2 hours in a supergravity reactor, allowing the mixture to be fully infused into the microcapsule, and then separating the microcapsule from the mixture through a vacuum suction filter tank. After turning off the vacuum, adding clean water to the suction filter tank to cover the upper layer of the microcapsule by 3 to 5 cm, soaking for 20 minutes, turning on the vacuum, sucking away the soaking solution, loading the cleaned microcapsule into a tray and moving it to a vacuum drying oven, and drying it at a temperature of about 40°C for 4 hours. The powdery state after drying is the nano slow-release decolorizing agent.
[0020] The silicon-based nano-microcapsules are hollow porous SiO2 nanoparticles activated for 3-6 hours under vacuum conditions; wherein the average particle size of the hollow porous nano-SiO2 is 100-150 nm, the wall thickness is about 10-15 nm, and the pore size is about 3.5-6.5 nm.
[0021] The mass concentration of ferrous sulfate solution is 36-40%, and the mass concentration of Bacillus subtilis is 8-10%; at the same time, the mass ratio of ferrous sulfate, Bacillus subtilis and silicon-based nano-microcapsules is controlled to be 24-28:4-6:66-72.
[0022] The mixture of ferrous sulfate and Bacillus subtilis in which the silicon-based nano-microcapsules are soaked is an aqueous solution, in which the concentration of ferrous sulfate is 36~40%, and the concentration of Bacillus subtilis is 8~10%. In view of the biological properties of Bacillus subtilis, in order to maintain its activity, the operating temperature is required to be maintained at an appropriate temperature of 32~38℃, the tolerance temperature does not exceed 40℃, and the death temperature is 45℃.
[0023] The nano slow-release decolorizer has a decolorizing effect on low-quality materials containing 5-10% industrial salt (sodium chloride), mechanical impurities, COD, N-NH3, and microorganisms and algae. It mainly uses nano microcapsules to adsorb fine mechanical impurities, microorganisms and algae in the aqueous solution, and uses ferrous sulfate and Bacillus subtilis therein to inhibit and inactivate the microorganisms and algae, so that the impurities in the aqueous solution are removed, and the nano microcapsules are filtered out together with the mechanical impurities.
[0024] The amount of the nano-release decolorant added to the alkali-dissolved aqueous solution is 0.6‰~1‰. If an excessive amount of decolorant is added, such as an amount of 2‰, although it has no effect on the decolorization effect, an unpleasant odor will be generated when hydrochloric acid is subsequently added to adjust the pH value; and if too little decolorant is added, such as an amount of 0.1‰, the decolorization effect is not good, the clarity of the alkali-dissolved aqueous solution does not meet the requirements, and the whiteness of the raw material washed with crystallization water does not meet the requirements of more than 85, and is only 70~75 degrees.
[0025] (4) Adjust the temperature of the reactor to 0°C~10°C, and slowly drip hydrochloric acid liquid into glyphosate solution C while stirring to acidify and neutralize until pH=2;
[0026] When hydrochloric acid is added dropwise to the reaction kettle, the temperature needs to be lowered to adjust the reaction temperature, and the temperature is required to be adjusted to 0°C to 15°C, preferably 0°C to 10°C, and more preferably 0°C to 4°C.
[0027] The concentration of hydrochloric acid here is 10% to 37%, preferably 20% to 30%, more preferably 20% to 25%.
[0028] Here, the pH value is adjusted to between 1.5 and 2.5, preferably between 1.5 and 2.
[0029] (5) Continue stirring the glyphosate solution C. White crystals gradually precipitate from the solution C, and a milky white turbid liquid D appears.
[0030] Hydrochloric acid may be added dropwise here to adjust the pH value to 1.5-2.5, preferably 1.5-2.
[0031] (6) Pour the turbid liquid D into a suction filter tank for filtration. The filtrate is pumped into the mother liquid tank for storage as the mother liquid. The white crystals are filtered and then sent to an air flow dryer for drying. After drying, the glyphosate raw powder is obtained and sampled for inspection.
[0032] When filtering the glyphosate crystals here, the filtrate can be recycled to wash the glyphosate crystals in the filter tank.
[0033] After drying, glyphosate crystals can be used as glyphosate raw powder for preparation or sale as technical drug.
[0034] The purpose of the present invention can also be achieved like this:
[0035] A method for producing glyphosate raw powder by recycling glyphosate low-quality materials, wherein the glyphosate low-quality materials are solids deposited at the bottom of the mother liquid tank after the acid mother liquid obtained in the process of producing glyphosate by the glycine method is stored in the mother liquid tank and cooled and left to stand. The method comprises the following steps:
[0036] (1) Put the crushed low-quality materials into the reactor A, add water to cover the low-quality materials, and introduce ammonia gas into the water while stirring to neutralize it until the low-quality materials in the reactor are completely dissolved. The resulting solution is glyphosate solution A. The ammonia gas is obtained by gasifying liquid ammonia.
[0037] (2) filtering the glyphosate solution A obtained in step 1) through a plate and frame filter press, and the solution obtained after filtration is glyphosate solution B;
[0038] (3) The glyphosate solution B obtained in step 2) is pressed into a reaction kettle B, and 0.6-1‰ of a decolorizing agent is poured into the reaction kettle while stirring. After stirring for 10 minutes, the solution in the kettle is taken for colorimetry. When the color of the solution becomes clear and transparent, a glyphosate solution C is obtained;
[0039] (4) Adjust the temperature of the reactor to 0°C~4°C, and slowly drip hydrochloric acid liquid into glyphosate solution C while stirring to acidify and neutralize until the pH is 2~2.5;
[0040] (5) Continue stirring the glyphosate solution C. White crystals gradually precipitate from the solution C, and a milky white turbid solution D appears.
[0041] (6) Pour the turbid liquid D into a suction filter tank for filtration. The filtrate is pumped into the mother liquid tank for storage as the mother liquid. The white crystals are filtered and sent to an air flow dryer for drying. After drying, the glyphosate raw powder is obtained and samples are taken for inspection.
[0042] Steps (2), (3), (4), (5) and (6) are the same or substantially the same as the process of the aforementioned method. Step 1) requires that the reactor A has an ammonia supply device, and safety devices such as a liquid ammonia cylinder and a pressure reducing valve are required to be installed in the workshop.
[0043] The above method of recycling low-quality glyphosate materials to produce glyphosate raw powder makes full use of low-quality glyphosate resources, maintains the normal production of glyphosate, and the quality of the recycled glyphosate raw powder is no different from that of glyphosate produced by the normal glycine method, and can be sold as a genuine product, which has considerable economic benefits.
[0044] Unless otherwise specified, all percentages involved in this patent application are by weight. BRIEF DESCRIPTION OF THE DRAWINGS
[0045] Figure 1 This is a picture of the glyphosate product in Example 1 without any decolorization.
[0046] Figure 2 This is a picture of the glyphosate product obtained in Example 2.
[0047] Figure 3 This is a picture of the glyphosate product obtained in Example 3.
[0048] Figure 4 This is a picture of the glyphosate product obtained in Example 5. DETAILED DESCRIPTION
[0049] The present invention is further described below in conjunction with specific embodiments.
[0050] The glyphosate low-quality material used in this embodiment refers to the liquid remaining after the glyphosate crystals are filtered out by acidification and crystallization during the production of glyphosate by the glycine method, which is the glyphosate mother liquor. The glyphosate mother liquor is first stored in a mother liquor tank, cooled and allowed to stand, and the solid matter deposited at the bottom of the mother liquor tank, the main components of which are glyphosate 62.5%, industrial salt (NaCl) 7.8%, water 8.5%, and the rest includes mechanical impurities, COD, N-NH3, and microbial algae.
[0051] The preparation method of the nano slow-release decolorizing agent used in this embodiment is as follows: a diluent of ferrous sulfate with a mass concentration of 38% and 8.5% Bacillus subtilis (purchased from the Institute of Biological Sciences of Hubei Academy of Agricultural Sciences, BWCC30260) is used to immerse the diluted solution in the silicon-based nano-microcapsules through a supergravity reactor (the mass ratio of ferrous sulfate, Bacillus subtilis and silicon-based nano-microcapsules is 26.8:4.2:69), and the mixture is stirred at a speed of 800r / m for 2hr in a supergravity reactor (purchased from Beijing Zhongchao Haiqi Technology Co., Ltd.), and the temperature in the supergravity reactor is controlled to be 32~38°C. The mixed liquid is fully infused into the microcapsules, and then the microcapsules are separated from the mixed liquid through a vacuum suction filter tank. After turning off the vacuum, add clean water to the suction filter tank to cover the upper layer of the microcapsules by 3 to 5 cm. After soaking for 20 minutes, turn on the vacuum to suck away the soaking liquid. The cleaned microcapsules are loaded into a tray and moved to a vacuum drying oven, and dried at a temperature of about 40°C for 4 hours. The powder after drying is the nano slow-release decolorizer.
[0052] The silicon-based nano-microcapsules are hollow porous SiO2 nanoparticles activated for 3-6 hours under vacuum conditions; wherein the average particle size of the hollow porous nano-SiO2 is 100 nm, the wall thickness is about 15 nm, and the pore size is about 4.5 nm.
[0053] Example 1
[0054] 300g of glyphosate low-quality tank powder was put into a 3-mouth beaker, and then 393g of clean water was poured in and stirred. During the process of adding dropwise while stirring, 357g of 32% liquid alkali was dripped in. No decolorizing agent was added. The aqueous solution after the alkali was dissolved was directly filtered through a sand core filter to remove mechanical impurities. The filtrate was poured into a 3-mouth beaker and 301g of 30% concentrated hydrochloric acid was dripped in while stirring until the pH value reached 1.97. A turbid liquid of glyphosate crystals appeared in the beaker. The turbid liquid was poured into a sand core funnel for filtration, and the crystals in the funnel were rinsed with 200g of clean water. After drying, the glyphosate crystals were taken out and placed in a tray and dried in a 100°C oven for 12 hours to obtain 194g of off-white crystals with a whiteness of 65 and a purity of 89.6%. The color was as follows: Figure 1 shown.
[0055] Example 2
[0056] Put 250g of low-quality material tank powder into a 3-mouth beaker, then pour in 250g of clean water and start stirring. While stirring and dropping, drop in 250g of 32% liquid alkali. After the low-quality material is completely dissolved, add 5g of Al2O3 flocculation decolorizer and continue stirring for 2m until Al2O3 is completely dissolved. Then pour the solution in the beaker into a sand core filter to filter out mechanical impurities. Pour the filtrate into a 3-mouth beaker and continue to drop 290g of 30% concentrated hydrochloric acid while stirring until the pH value reaches 0.41. A glyphosate crystal turbid liquid appears in the beaker. Pour the turbid liquid into a sand core funnel for filtration, and rinse the crystals in the funnel with 180g of clean water. After drying, take out the glyphosate crystals, put them in a tray and send them to a 100℃ oven for drying for 12 hours to obtain 196g of grayish white crystals with a whiteness of 80 and a purity of 88.8%. The color is as follows Figure 2 shown.
[0057] Example 3
[0058] 400g of low-quality tank powder was put into a 3-mouth beaker, and then 401g of clean water was poured in and stirred. During the process of adding dropwise while stirring, 462g of 32% liquid alkali was dripped in. After the low-quality material was completely dissolved, 0.8g of the nano slow-release decolorizer prepared above was added. Stirring was continued for 2 minutes. The color of the aqueous solution did not change significantly. Then the solution in the beaker was poured into a sand core filter to filter out mechanical impurities. The filtrate was poured into a 3-mouth beaker and 512g of 30% concentrated hydrochloric acid was dripped in while stirring until the pH value reached 1.45. A turbid liquid of glyphosate crystals appeared in the beaker. The turbid liquid was poured into a sand core funnel for filtration, and the crystals in the funnel were rinsed with 200g of clean water. After drying, the glyphosate crystals were taken out and placed in a tray and sent to a 100°C oven for drying for 12 hours to obtain 298g of glyphosate crystals with the color as above. Figure 3 As shown, the whiteness is 75 and the purity is 92.6%.
[0059] Example 4
[0060] 400g of low-quality material tank powder was put into a 3-mouth beaker, and then 401g of clean water was poured in and stirred. During the process of adding dropwise while stirring, 462g of 32% liquid alkali was dripped in. After the low-quality material was completely dissolved, 4.8g of the nano slow-release decolorizer prepared above was added. Stirring was continued for 2 minutes. The aqueous solution gradually changed from oil tea color to clear and transparent color. Then the solution in the beaker was poured into a sand core filter to filter out mechanical impurities. The filtrate was poured into a 3-mouth beaker and 512g of 30% concentrated hydrochloric acid was dripped in while stirring until the pH value reached 0.23. A milky white glyphosate crystal turbid liquid appeared in the beaker. The turbid liquid was poured into a sand core funnel for filtration, and the crystals in the funnel were rinsed with 200g of clean water. After drying, the glyphosate crystals were taken out and placed in a tray and sent to a 100°C oven for drying for 12 hours to obtain 290g of pure white crystals. The color was as follows: Figure 4 As shown, the whiteness is 88 and the purity is 92.9%.
[0061] Example 5
[0062] 500g of low-quality tank powder was put into a 3-mouth beaker, and then 536g of clean water was poured in and stirred. During the process of dropping with stirring, 637g of 32% liquid alkali was dropped in. After the low-quality material was completely dissolved, 10g of the nano slow-release decolorizer prepared above was added. Stirring was continued for 2m, and the aqueous solution gradually changed from oil tea color to clear and transparent color. Then the solution in the beaker was poured into a sand core filter to filter out mechanical impurities. The filtrate was poured into a 3-mouth beaker and 492g of 30% concentrated hydrochloric acid was continued to be dropped in while stirring until the pH value reached 2.66. During the dropwise addition of concentrated hydrochloric acid, an unpleasant odor continuously escaped from the beaker with stirring, and a milky white glyphosate crystal turbid liquid appeared in the beaker. The turbid liquid was poured into a sand core funnel for filtration, and the crystals in the funnel were rinsed with 200g of clean water. After drying, the glyphosate crystals were taken out and placed in a tray and sent to a 100°C oven for drying for 12 hours to obtain 325.4g of pure white crystals with the same color as Figure 4 Similar, whiteness is 92 and purity is 93.1%.
Claims
1. A method for recycling low-quality glyphosate materials, characterized in that: The steps include: (a) adding low-quality glyphosate into an alkali solution and gradually dissolving it to obtain a glyphosate solution A, wherein the low-quality glyphosate refers to the liquid remaining after the glyphosate crystals are filtered out by acidification and crystallization during the production of glyphosate by the glycine method, namely the glyphosate mother liquor, the glyphosate mother liquor is first stored in a mother liquor tank, cooled and allowed to stand, and the solid matter deposited at the bottom of the mother liquor tank, the solid matter mainly comprising 60%-70% glyphosate, 5%-10% industrial salt, 5%-10% water, and the remainder comprising mechanical impurities, COD, N-NH3, and microorganisms and algae; (b) filtering the glyphosate solution A through a plate and frame filter to remove mechanical impurities and fine sand and soil in the solution to obtain a glyphosate solution B; (c) adding a decolorizing agent to the glyphosate solution B obtained by filtering in step (b) for decolorization to obtain a glyphosate solution C, so that the turbid green solution gradually becomes pure and transparent, wherein the decolorizing agent is a nano slow-release decolorizing agent formed by ferrous sulfate and Bacillus subtilis, and the preparation method of the nano slow-release decolorizing agent formed by ferrous sulfate and Bacillus subtilis is as follows: in a supergravity reactor, immersing silicon-based nano-microcapsules in a mixed aqueous solution formed by ferrous sulfate solution and Bacillus subtilis, stirring at a speed of 500-800 r / min for 2-4 hours, so that the mixed aqueous solution is fully infused into the silicon-based nano-microcapsules; The nano slow-release decolorizing agent is obtained through vacuum filtration, water injection washing and drying; (d) adding hydrochloric acid to the decolorized glyphosate solution C in step (c) to reduce the pH value of the solution to less than pH 2.4; (e) Continue to add dilute hydrochloric acid to solution C, and white crystals gradually precipitate from the solution to form a turbid solution D; (g) The chaotic liquid D is injected into a centrifuge for centrifugal filtration to obtain glyphosate wet powder, which is then dried to obtain glyphosate raw powder with a whiteness of more than 85 and a content of more than 95%.
2. The method for recycling low-quality glyphosate materials according to claim 1, characterized in that: The mass concentration of ferrous sulfate solution is 36-40%, and the mass concentration of Bacillus subtilis is 8-10%; at the same time, the mass ratio of ferrous sulfate, Bacillus subtilis and silicon-based nano-microcapsules is controlled to be 24-28:4-6:66-72.
3. The method for recycling low-quality glyphosate materials according to claim 1, characterized in that: The silicon-based nano-microcapsules are hollow porous SiO2 nanoparticles activated for 3-6 hours under vacuum conditions; The average particle size of the hollow porous nano-SiO2 is 100-150 nm, the wall thickness is 10-15 nm, and the pore size is 3.5-6.5 nm.
4. The method for recycling low-quality glyphosate materials according to claim 1, characterized in that: The stirring speed was 800 r / min, the stirring time was 2 h, and the temperature in the ultragravity reactor was controlled at 32~38 °C.
5. The method for recycling low-quality glyphosate materials according to claim 1, characterized in that: The alkali in step (a) is aqueous ammonia, 32-40% sodium hydroxide aqueous solution, 40-55% potassium hydroxide aqueous solution, or 30-40% dimethylamine aqueous solution.
6. The method for recycling low-quality glyphosate materials according to claim 1, characterized in that: When hydrochloric acid is added dropwise to the glyphosate solution C for acidification in step (e) or step (d), the temperature is controlled at 0-15°C.
7. The method for recycling low-quality glyphosate materials according to claim 1, characterized in that: After the turbid liquid D in step (g) or (f) is filtered by suction, the filtered liquid is the glyphosate mother liquor, which is returned to the mother liquor tank for subsequent treatment as the glyphosate mother liquor.
Citation Information
Patent Citations
Method for recycling glyphosate raw powder from glyphosate mother liquid
CN101805371A
Method for immobilized culture of salt-tolerant bacillus strains and application
CN105969759A