Alkaline soil conditioner prepared by using grape juice distillation residue and preparation method thereof
The porous carbon matrix and sugar are modified by distillation of grape juice to form an acid-release core, and combined with cement and zeolite powder shell layer, the problems of high cost and unsatisfactory effects of traditional alkaline soil improvement methods are solved, and the soil alkalinity is effectively reduced and exchange sodium content to prevent alkali reflux and improve soil nutrient structure.
Patent Information
- Application Number
- CN202210861852.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-07-22
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2042-07-22
AI Technical Summary
The traditional alkaline soil improvement method is costly and has poor effect, which can easily lead to the problem of soil alkaline rebate and it is difficult to effectively reduce the content of soil alkaline and exchangeable sodium.
The alkaline soil modification agent prepared with grape juice distillation residue is formed by modifying the porous carbon matrix and the distillation residue of fermented grape juice distillation residue, and the alkalinity of the soil is reduced by using organic acids and sugars. Cement and zeolite powder in the outer shell prevent alkali return.
Effectively reduce the content of alkaline and exchangeable sodium in the soil, prevent the soil from returning alkaline again, and provide minerals such as phosphorus, calcium, and magnesium to improve the nutrient structure of the soil and promote plant growth.
Smart Images

Figure CN115368907B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of alkaline soil improvement, and in particular to an alkaline soil improver prepared by using grape juice distillation residue and a preparation method thereof. Background Art
[0002] Alkaline soil refers to soil solution with OH- concentration greater than H + Concentrated soil generally refers to soil with a pH value greater than 7.3. The higher the pH value, the stronger the alkalinity of the soil. Common alkaline soils are mainly saline soil and alkaline soil. The parent materials of soil formation in the north are mostly montmorillonite, etc., and the soil contains a lot of sodium carbonate. In addition, due to climatic factors and other reasons, with the large accumulation of salts such as sodium carbonate in the soil, a large amount of exchangeable sodium is adsorbed in the soil colloid. These exchangeable sodiums are easily replaced from the soil colloid by calcium and magnesium ions in the soil solution and enter the soil solution to form carbonates. These carbonates are alkaline after hydrolysis, thus leading to soil salinization. When plants live in this kind of soil, it is easy to cause plant cell dehydration, which will seriously affect the healthy growth of plants, and even cause plant death in severe cases. Therefore, it has become an important agricultural measure to reduce the alkali of this type of soil, such as the traditional application of organic fertilizers, water irrigation, application of chemical agents, application of microbial agents, etc. However, these traditional methods generally have the problems of high process costs, unsatisfactory effects, and easy alkali return. Summary of the invention
[0003] In view of the above problems, the present invention provides an alkaline soil conditioner prepared by using grape juice distillation residue and a preparation method thereof. The conditioner uses the residual liquid after fermenting grape juice to distill wine to not only effectively reduce the alkalinity of the soil, but also reduce the content of exchangeable sodium in the soil, thereby alleviating the problem of soil returning to alkalinity. Specifically, the present invention discloses the following technical solutions.
[0004] First, the present invention discloses an alkaline soil conditioner prepared by using grape juice distillation residue, which comprises an acid-releasing core, an isolation layer and an outer shell layer. The acid-releasing core comprises a porous carbon matrix and an acidic component adsorbed in the matrix, and the acidic component comes from the residual liquid after the fermented grape juice is distilled. The isolation layer is coated on the surface of the acid-releasing core, and the isolation layer is a solidified film formed by cross-linking of cellulose under the action of metal ions in the acidic component. The outer shell layer is a porous shell layer formed by bonding cement and zeolite powder and coated on the surface of the isolation layer.
[0005] Furthermore, the solutes in the residual liquid at least include: lactic acid, tartaric acid, citric acid, malic acid, succinic acid, glucose, fructose, sucrose, etc. The present invention finds that the residual liquid remaining after the fermented grape juice is distilled to extract the alcohol component contains a large amount of organic acid, sugar and mineral elements, and is a good alkaline soil conditioner.
[0006] Second, the present invention discloses a method for preparing an alkaline soil conditioner using grape juice distillation residue, comprising the following steps:
[0007] (I) The porous carbon matrix is mixed evenly with residual liquid after distillation of fermented grape juice, and then heated and kept warm in a closed and protective atmosphere to modify the porous carbon matrix, and a modified base material is obtained after completion.
[0008] (II) The modified base material is crushed and mixed again with the residual liquid after distillation of fermented grape juice, and then granulated and dried to obtain the acid-releasing core.
[0009] (III) applying a slurry formed by cellulose and water to the surface of the acid-releasing core, and then allowing it to stand for a certain period of time. After completion, heating and curing it into a film, the isolation layer can be coated on the surface of the acid-releasing core to obtain an isolated acid-releasing core.
[0010] (IV) coating the surface of the isolated acid-releasing inner core with a slurry formed by zeolite powder and cement, and then curing the slurry to obtain an alkaline soil conditioner coated with an outer shell layer.
[0011] In a further embodiment, in step (I), the porous carbon matrix is a porous carbon obtained by pyrolysis and carbonization of agricultural biomass. Agricultural biomass has a large output, abundant sources, and low cost. Using it as a source of porous carbon is not only low in cost, but also can achieve the purpose of waste recycling.
[0012] In a further embodiment, in step (I), the ratio of the porous carbon matrix to the residual liquid is 1 g: 10-18 ml. The porous carbon matrix has excellent adsorption capacity, and the residual liquid can be fully adsorbed therein to infiltrate the porous carbon matrix.
[0013] In a further embodiment, in step (I), the protective atmosphere is nitrogen or an inert gas, so that the heating and heat preservation process is carried out in an oxygen-isolated environment.
[0014] In a further embodiment, in step (I), the heating temperature is 80-90°C and the time is 1-2 hours. By subjecting the porous carbon matrix soaked in the residual liquid containing a large amount of organic acid to high temperature and high pressure heat treatment modification, a large amount of organic functional groups can be loaded on the surface of the porous carbon matrix, thereby improving the ability of the porous carbon matrix to adsorb exchangeable sodium in the soil.
[0015] In a further embodiment, in step (II), the ratio of the modified base material to the residual liquid is 1 g: 6-9 ml. In addition to containing a large amount of organic acid that can be used to neutralize alkaline soil, the residual liquid also contains a large amount of sugar, which gives the residual liquid good bonding properties and facilitates the granulation of the modified base material.
[0016] In a further embodiment, in step (II), the drying temperature is 50-55°C and the drying time is 2-3 hours. Optionally, the particle size of the acid-releasing core is maintained between 5 and 20 mm.
[0017] In a further embodiment, in step (III), the solid content of the slurry formed by the cellulose and water is 25-33% (mass fraction). Optionally, the cellulose includes at least one of hydroxymethyl cellulose, hydroxyethyl carboxymethyl cellulose, carboxymethyl hydroxypropyl cellulose and the like.
[0018] In a further embodiment, in step (III), the standing time is 8 to 15 minutes, so that the water in the slurry enters the surface layer of the acid-releasing inner core and the metal ions therein diffuse into the slurry to participate in the cross-linking reaction.
[0019] In a further embodiment, in step (III), the heating temperature is 50-55° C. and the heating time is 20-40 min. Part of the metal ions in the residual liquid in the acid-releasing core diffuse into the cellulose isolation layer to participate in its cross-linking, which not only accelerates the formation of the isolation layer, but also increases the density and strength of the isolation layer, and prevents the alkaline products generated by the subsequent outer shell during the curing process from entering the acid-releasing core.
[0020] In a further embodiment, in step (IV), the solid content of the slurry formed by the zeolite powder and cement is 30-40% (mass fraction), and the weight ratio of the zeolite powder and cement is 1 part:0.28-0.35 parts. The zeolite powder particles contain a large number of micropores, and the cement can be used as a binder to bind the zeolite powder together, and after curing, a hard porous shell is formed, which is convenient for the discharge of the acidic components in the acid-releasing core.
[0021] In a further embodiment, in step (IV), the curing is natural curing for 5 to 7 days, during which the cement undergoes a hydration reaction and eventually forms the hard outer shell layer with the zeolite powder.
[0022] In a further embodiment, in step (IV), the thickness of the outer shell layer is controlled to be between 3 and 5 mm. The outer shell layer can effectively protect the acid-releasing inner core and maintain a stable state for a long time after the release of the acidic components is completed, serving as an adsorbent of exchangeable sodium in the soil to prevent the soil from returning to alkalinity again.
[0023] Compared with the prior art, the present invention has the following beneficial effects:
[0024] The alkaline soil conditioner of the present invention utilizes the residual liquid after fermenting grape juice to distill wine, which not only effectively reduces the soil alkalinity, but also reduces the content of exchangeable sodium in the soil, thereby alleviating the problem of soil returning to alkalinity. The reason is that:
[0025] First, the present invention utilizes the characteristic that the residual liquid contains a large amount of organic acid, and utilizes the organic acid to modify the inner and outer surfaces of the porous carbon, so that the surface of the porous carbon is loaded with a large amount of organic functional groups, effectively improving the adsorption capacity of the porous carbon to exchangeable sodium in the soil, etc., thereby reducing the content of exchangeable sodium in the soil, and alleviating the problem of soil returning to alkali again. Moreover, when the porous carbon modified by the residual liquid is used to store the residual liquid again, the organic functional groups on the surface of the porous carbon can exist stably, that is, the degradation of the organic functional groups is avoided by the homologous mechanism. In addition, the above process also helps to convert insoluble ash such as phosphates in the porous carbon into soluble organic salts. After the modifier is applied to the soil, these organic salts are released into the soil with water, providing the soil with mineral nutrients such as phosphorus, calcium, magnesium, and iron.
[0026] Secondly, the present invention prepares an acid-releasing core by combining the modified base material obtained after the above modification with the residual liquid again, and utilizes the rich pores of the porous carbon to store the acidic components in the residual liquid therein, so as to release them into the soil later to reduce the alkalinity of the soil. After the acidic components are released, the pores in the acid-releasing core are vacant again, thereby converting the acid-releasing core into an adsorbent. Since it has been modified as mentioned above, it can effectively reduce the content of exchangeable sodium in the soil and alleviate the problem of soil alkali return. In addition, since the residual liquid contains a large amount of sugar and glycerol, the residual liquid has good viscosity, and thus acts as a binder to granulate the porous carbon. After these sugars enter the soil, they work together with the mineral nutrients to improve the soil nutritional structure, which helps promote plant growth.
[0027] Furthermore, in order to keep the acid-releasing core stable in the soil, it can be retained in the soil as an adsorbent for a long time to adsorb and store exchangeable sodium after releasing the acidic components. The present invention prepares an outer shell layer on the surface of the acid-releasing core. Since the cement in the outer shell releases the hydration product calcium hydroxide during the curing process, it will consume the acidic components in the acid-releasing core after entering the acid-releasing core. For this reason, the present invention coats a layer of isolation layer on the surface of the acid-releasing core. At the same time, the present invention also uses the metal ions contained in the acid-releasing core (including those brought by the residual liquid and those converted from the ash, etc.) to promote the cross-linking molding of the isolation layer, increase the density and strength of the isolation layer, and at the same time, the calcium ions generated during the cement hydration process will also react with the isolation layer again to cross-link, further increase the density of the isolation layer, and prevent the hydration products from entering the acid-releasing core. In addition, the present invention uses zeolite powder as the main component of the outer shell, which contains a large number of tiny pores, which is convenient for water in the soil to enter and carry out the acidic components in the acid-releasing core. In addition, since the zeolite powder contains a large amount of active silicon dioxide and aluminum oxide, it can react with the hydration product calcium hydroxide of the cement to form hydrated calcium silicate and aluminate, thereby effectively consuming the hydration product calcium hydroxide and reducing the hydration products entering the acid-releasing core. In addition, the formation of the hydrated calcium silicate and aluminate is also equivalent to promoting the hydration of cement, increasing the strength of the outer shell, and increasing the stability of the modifier. In addition, after the acidic components are released as an adsorbent, the large number of tiny pores contained in the zeolite particles in the outer shell can also adsorb and store exchangeable sodium, playing a role in alleviating the soil from returning to alkalinity again. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. The embodiments of the present invention are described in detail below in conjunction with the accompanying drawings, wherein:
[0029] Figure 1 This is a rendering of the residual liquid after distilling the fermented grape juice used in the following examples to make wine. DETAILED DESCRIPTION
[0030] It should be noted that all professional and scientific terms used herein have the same meanings as those familiar to those skilled in the art, unless otherwise defined. The reagents or raw materials used in the present invention can be purchased through conventional channels. Unless otherwise specified, the reagents or raw materials used in the present invention are used in a conventional manner in the art or in accordance with the product instructions.
[0031] In the following examples, the residual liquid is the residue after the fermented grape juice is distilled to prepare brandy (see the attached figure of the specification Figure 1), the organic acids and other components it contains are shown in the following table, and it also contains some sugars and metal ions.
[0032] lactic acid tartaric acid Citric Acid Malic Acid Succinic acid Acetic acid glycerin Content (g / L) 3.29 1.64 1.16 0.72 0.39 0.05 5.44
[0033] Example 1
[0034] A method for preparing an alkaline soil conditioner using grape juice distillation residue comprises the following steps:
[0035] (I) The porous carbon matrix prepared by pyrolysis of rice husk and the residual liquid after distillation of fermented grape juice were added into a reactor with a liner at a ratio of 1 g:13 ml and mechanically stirred for 30 minutes to uniformly mix the two. The reactor was then closed and heated to 85° C. in a water bath under nitrogen atmosphere for 2 hours, and then cooled naturally to room temperature to obtain a modified base material.
[0036] (II) The modified base material is crushed and mixed with the residual liquid after distillation of fermented grape juice in a ratio of 1g:7ml, and then granulated in a granulator. Then, the mixture is placed in an oven and dried at 55°C for 2.5 hours to obtain granules with a particle size of about 8 to 13 mm, which are the acid-releasing cores for later use.
[0037] (III) Hydroxyethyl carboxymethyl cellulose is added to water to form a slurry with a solid content of 28.73 wt.%, and then the slurry is sprayed on the surface of the acid-releasing core. After standing for 10 minutes, it is kept at 50° C. for 30 minutes to allow the slurry on the surface of the acid-releasing core to solidify into a film, thereby obtaining an isolated acid-releasing core.
[0038] (IV) 300 mesh zeolite powder and silicate cement are added to water to form a slurry with a solid content of 36.34 wt.%, and the weight ratio of the zeolite powder to cement is 1 part:0.31 parts. The slurry is then coated on the surface of the isolated acid-releasing inner core, and then cured at room temperature for 7 days under a natural environment, and after completion, an alkaline soil conditioner coated with an outer shell layer with a thickness of 3 to 5 mm is obtained.
[0039] Example 2
[0040] A method for preparing an alkaline soil conditioner using grape juice distillation residue comprises the following steps:
[0041] (I) The porous carbon matrix prepared by pyrolysis of corn stalks and the residual liquid after distillation of fermented grape juice were added into a reactor with a liner at a ratio of 1 g:10 ml and mechanically stirred for 30 minutes to uniformly mix the two. The reactor was then closed and heated to 80° C. in a water bath under nitrogen atmosphere for 2 hours, and then cooled naturally to room temperature to obtain a modified base material.
[0042] (II) The modified base material is crushed and mixed with the residual liquid after distillation of fermented grape juice in a ratio of 1g:9ml, and then granulated in a granulator. Then, the mixture is placed in an oven and dried at 53°C for 2 hours to obtain granules with a particle size of about 5 to 8 mm, which are the acid-releasing cores for later use.
[0043] (III) Hydroxyethyl carboxymethyl cellulose is added to water to form a slurry with a solid content of 25.04 wt.%, and then the slurry is sprayed on the surface of the acid-releasing core. After standing for 8 minutes, it is kept at 55° C. for 20 minutes to allow the slurry on the surface of the acid-releasing core to solidify into a film, thereby obtaining an isolated acid-releasing core.
[0044] (IV) 400 mesh zeolite powder and silicate cement are added to water to form a slurry with a solid content of 29.97 wt.%, and the weight ratio of the zeolite powder to cement is 1 part:0.28 parts. The slurry is then coated on the surface of the isolated acid-releasing inner core, and then cured at room temperature for 5 days under a natural environment, and after completion, an alkaline soil conditioner coated with an outer shell layer with a thickness of 3 to 5 mm is obtained.
[0045] Example 3
[0046] A method for preparing an alkaline soil conditioner using grape juice distillation residue comprises the following steps:
[0047] (I) The porous carbon matrix prepared by pyrolysis of corn stalks and the residual liquid after distillation of fermented grape juice were added into a reactor with a liner at a ratio of 1 g:18 ml and mechanically stirred for 30 minutes to uniformly mix the two. The reactor was then closed and heated to 90° C. in a water bath under the protection of a nitrogen atmosphere for 1 hour, and then naturally cooled to room temperature to obtain a modified base material.
[0048] (II) The modified base material is crushed and mixed with the residual liquid after distillation of fermented grape juice in a ratio of 1g:6ml, and then granulated in a granulator. Then, the mixture is placed in an oven and dried at 50°C for 3 hours to obtain granules with a particle size of about 16 to 20 mm, which are the acid-releasing cores for later use.
[0049] (III) Carboxymethyl hydroxypropyl cellulose is added to water to form a slurry with a solid content of 33.02 wt.%, and then the slurry is sprayed on the surface of the acid-releasing core. After standing for 15 minutes, it is kept at 50° C. for 40 minutes to allow the slurry on the surface of the acid-releasing core to solidify into a film, thereby obtaining an isolated acid-releasing core.
[0050] (IV) 280 mesh zeolite powder and silicate cement are added to water to form a slurry with a solid content of 40.02 wt.%, and the weight ratio of the zeolite powder to cement is 1 part:0.35 parts. The slurry is then coated on the surface of the isolated acid-releasing inner core, and then cured at room temperature for 7 days under a natural environment, and after completion, an alkaline soil conditioner coated with an outer shell layer with a thickness of 3 to 5 mm is obtained.
[0051] Example 4
[0052] A method for preparing an alkaline soil conditioner using grape juice distillation residue comprises the following steps:
[0053] (I) The porous carbon matrix prepared by pyrolysis of rice husk and the residual liquid after distillation of fermented grape juice were added into a reactor with a liner at a ratio of 1 g:13 ml and mechanically stirred for 30 minutes to uniformly mix the two. The reactor was then closed and heated to 85° C. in a water bath under nitrogen atmosphere for 2 hours, and then cooled naturally to room temperature to obtain a modified base material.
[0054] (II) The modified base material is crushed and mixed with the residual liquid after distillation of fermented grape juice in a ratio of 1g:7ml, and then granulated in a granulator. Then, the mixture is placed in an oven and dried at 55°C for 2.5 hours to obtain granules with a particle size of about 8 to 13 mm, which are the acid-releasing cores for later use.
[0055] (III) 300 mesh zeolite powder and silicate cement are added to water to form a slurry with a solid content of 36.34 wt.%, and the weight ratio of the zeolite powder to cement is 1 part:0.31 parts. The slurry is then coated on the surface of the acid-releasing core, and then cured at room temperature for 7 days under a natural environment, and after completion, an alkaline soil conditioner coated with a shell layer with a thickness of 3 to 5 mm is obtained.
[0056] Example 5
[0057] A method for preparing an alkaline soil conditioner using grape juice distillation residue comprises the following steps:
[0058] (I) The porous carbon matrix prepared by pyrolysis of corn stalks is crushed and mixed with the residual liquid after distillation of fermented grape juice in a ratio of 1g:9ml, and then granulated in a granulator. Then, the mixture is placed in an oven and dried at 53°C for 2 hours to obtain a granular material with a particle size of about 5 to 8 mm, which is the acid-releasing core, and is set aside.
[0059] (II) Hydroxyethyl carboxymethyl cellulose was added into water to form a slurry with a solid content of 25.04 wt.%, and then the slurry was sprayed on the surface of the acid-releasing core. After standing for 8 minutes, the slurry was kept at 55° C. for 20 minutes to solidify into a film, thereby obtaining an isolated acid-releasing core.
[0060] (III) 400 mesh zeolite powder and silicate cement are added to water to form a slurry with a solid content of 29.97 wt.%, and the weight ratio of the zeolite powder to cement is 1 part:0.28 parts. The slurry is then coated on the surface of the isolated acid-releasing inner core, and then cured at room temperature for 5 days under a natural environment, and after completion, an alkaline soil conditioner coated with an outer shell layer with a thickness of 3 to 5 mm is obtained.
[0061] Example 6
[0062] A method for preparing an alkaline soil conditioner using grape juice distillation residue comprises the following steps:
[0063] (I) The porous carbon matrix prepared by pyrolysis of corn stalks and the residual liquid after distillation of fermented grape juice were added into a reactor with a liner at a ratio of 1 g:18 ml and mechanically stirred for 30 minutes to uniformly mix the two. The reactor was then closed and heated to 90° C. in a water bath under the protection of a nitrogen atmosphere for 1 hour, and then naturally cooled to room temperature to obtain a modified base material.
[0064] (II) The modified base material is crushed and granulated, and then placed in an oven and dried at 50° C. for 3 hours to obtain granules with a particle size of about 16 to 20 mm, which are the acid-releasing cores and are set aside.
[0065] (III) Carboxymethyl hydroxypropyl cellulose is added to water to form a slurry with a solid content of 33.02 wt.%, and then the slurry is sprayed on the surface of the acid-releasing core. After standing for 15 minutes, it is kept at 50° C. for 40 minutes to allow the slurry on the surface of the acid-releasing core to solidify into a film, thereby obtaining an isolated acid-releasing core.
[0066] (IV) 280 mesh zeolite powder and silicate cement are added to water to form a slurry with a solid content of 40.02 wt.%, and the weight ratio of the zeolite powder to cement is 1 part:0.35 parts. The slurry is then coated on the surface of the isolated acid-releasing inner core, and then cured at room temperature for 7 days under a natural environment, and after completion, an alkaline soil conditioner coated with an outer shell layer with a thickness of 3 to 5 mm is obtained.
[0067] Example 7
[0068] A method for preparing an alkaline soil conditioner using grape juice distillation residue comprises the following steps:
[0069] (I) The porous carbon matrix prepared by pyrolysis of rice husk and the residual liquid after distillation of fermented grape juice were added into a reactor with a liner at a ratio of 1 g:13 ml and mechanically stirred for 30 minutes to uniformly mix the two. The reactor was then closed and heated to 85° C. in a water bath under nitrogen atmosphere for 2 hours, and then cooled naturally to room temperature to obtain a modified base material.
[0070] (II) The modified base material is crushed and mixed with the residual liquid after distillation of fermented grape juice in a ratio of 1g:7ml, and then granulated in a granulator. Then, the mixture is placed in an oven and dried at 55°C for 2.5 hours to obtain granules with a particle size of about 8 to 13 mm, which are the acid-releasing cores for later use.
[0071] (III) Hydroxyethyl carboxymethyl cellulose is added to water to form a slurry with a solid content of 28.73 wt.%, and then the slurry is sprayed on the surface of the acid-releasing core. After standing for 10 minutes, it is kept at 50° C. for 30 minutes to allow the slurry on the surface of the acid-releasing core to solidify into a film, thereby obtaining an isolated acid-releasing core.
[0072] (IV) Portland cement is added into water to form a slurry with a solid content of 36.34 wt.%, and then the slurry is coated on the surface of the isolated acid-releasing inner core, and then cured at room temperature for 7 days in a natural environment. After completion, an alkaline soil conditioner coated with an outer shell layer with a thickness of 3 to 5 mm is obtained.
[0073] Effect test:
[0074] The alkaline soil conditioner prepared in the above embodiments was added to the cultivated layer of alkaline soil with an average pH value of 8.14 at a ratio of 1000 kg / meal. Then, the pH value of the test soil corresponding to the alkaline soil conditioner in each embodiment was tested by a pH detector at 30 days, 90 days, and 180 days after watering, and the results are shown in Table 1.
[0075] Table 1 pH value of test soil
[0076] Example No. 1 2 3 4 5 6 7 pH value at 30 days 7.22 7.31 7.18 7.36 7.26 7.64 8.06 pH value at 90 days 7.15 7.20 7.06 7.24 7.41 7.77 8.17 pH value at 180 days 7.19 7.26 7.13 7.28 7.73 7.82 8.23
[0077] It can be seen that by applying a suitable proportion in the soil, the alkaline soil conditioner prepared in Examples 1, 2 and 3 can not only effectively improve the pH value of the alkaline soil, making the alkaline soil into a weak alkaline soil, but also the alkaline soil conditioner of Examples 1 to 3 can effectively prevent the soil from returning to alkalinity again by testing the pH of the soil at 180 days. In addition, the soil can be made weakly acidic by further increasing the application ratio, which can be determined according to the characteristics of the crops planted. However, the alkaline soil conditioner prepared in Example 4 does not have an isolation layer coated on the surface of the acid-releasing core, resulting in the alkaline hydration product produced during the preparation of the outer shell layer entering the acid-releasing core and consuming the acidic components therein, resulting in the improvement effect of the alkaline soil conditioner of Example 4 being reduced relative to Example 1. However, Example 5 did not modify the porous carbon matrix, resulting in the decrease in the ability of the alkaline soil conditioner prepared therefrom to prevent the soil from returning to alkalinity, and the phenomenon of late return to alkalinity occurred. Example 6 did not add the residual liquid after the distillation of fermented grape juice to the modified base material again, resulting in the insufficient alkalinity reduction ability of the alkaline soil conditioner prepared therefrom, and the soil pH could not be reduced to a qualified level. The outer shell layer of the alkaline soil conditioner prepared in Example 7 does not have zeolite powder, which makes it difficult for the alkaline soil conditioner to effectively release the acidic components therein to improve the soil. Moreover, as time goes by, the alkalinity of the soil increases, indicating that the conditioner cannot effectively improve the alkaline soil.
[0078] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. An alkaline soil conditioner prepared by using grape juice distillation residue, characterized in that: It comprises an acid-releasing core, an isolation layer and an outer shell; wherein: the acid-releasing core comprises a porous carbon matrix and an acidic component adsorbed in the matrix, the acidic component comes from the residual liquid after the fermented grape juice is distilled, and the residual liquid is the residue after the fermented grape juice is distilled to prepare brandy; the isolation layer is coated on the surface of the acid-releasing core, and the isolation layer is a solidified film formed by cross-linking of cellulose under the action of metal ions in the acidic component; the outer shell is a porous shell layer formed by bonding cement and zeolite powder and coated on the surface of the isolation layer; The alkaline soil conditioner is prepared by the following steps: (I) uniformly mixing the porous carbon matrix with residual liquid after distillation of fermented grape juice, and then heating and preserving the temperature in a closed and protective atmosphere to modify the porous carbon matrix, and after completion, obtaining a modified base material; (II) crushing the modified base material and mixing it again with the residual liquid after distillation of fermented grape juice, and then granulating and drying to obtain the acid-releasing core; (III) applying a slurry formed by cellulose and water to the surface of the acid-releasing core, and then allowing it to stand, and then heating and curing it to form a film, so that the isolation layer can be coated on the surface of the acid-releasing core to obtain an isolated acid-releasing core; (IV) coating the surface of the isolated acid-releasing inner core with a slurry formed by zeolite powder and cement, and then curing the slurry to obtain an alkaline soil conditioner coated with an outer shell layer.
2. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: The solutes in the residual liquid at least include: lactic acid, tartaric acid, citric acid, malic acid, succinic acid, glucose, fructose, and sucrose.
3. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: In step (I), the ratio of the porous carbon matrix to the residual liquid is 1 g: 10-18 ml.
4. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: In step (I), the porous carbon matrix is porous carbon obtained by pyrolysis and carbonization of agricultural biomass.
5. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: In step (I), the heating temperature is 80-90° C. and the heating time is 1-2 hours.
6. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: In step (I), the protective atmosphere is nitrogen or an inert gas.
7. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: In step (II), the ratio of the modified base material to the residual liquid is 1 g: 6-9 ml.
8. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: In step (II), the drying temperature is 50-55° C. and the drying time is 2-3 hours.
9. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: The particle size of the acid-releasing core is maintained between 5 and 20 mm.
10. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: In step (III), the solid content of the slurry formed by the cellulose and water is 25-33% by mass.
11. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: In step (III), the cellulose includes at least one of hydroxymethyl cellulose, hydroxyethyl carboxymethyl cellulose, and carboxymethyl hydroxypropyl cellulose.
12. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: In step (III), the heating temperature is 50-55° C. and the heating time is 20-40 min.
13. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: In step (IV), the solid content of the slurry formed by the zeolite powder and cement is 30-40% by mass, and the weight ratio of the zeolite powder to cement is 1 part:0.28-0.35 parts.
14. The alkaline soil conditioner prepared by using grape juice distillation residue according to claim 1, characterized in that: In step (IV), the curing is natural curing, and the time is 5 to 7 days.
15. The alkaline soil conditioner prepared by using grape juice distillation residue according to any one of claims 1 to 14, characterized in that: In step (IV), the thickness of the outer shell layer is controlled between 3 and 5 mm.