A surface milling method for automobile steering wheel transmission shaft
Through multi-pass milling and shot peening combined with heat treatment, the problem of insufficient surface accuracy of the automobile steering wheel transmission shaft is solved, and high-precision and long-life processing effects are achieved.
Patent Information
- Application Number
- CN202211373072.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-03
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2042-11-03
AI Technical Summary
After the casting processing of the existing automobile steering wheel transmission shaft, the surface accuracy of the internal cavity is insufficient, resulting in a short service life. Simple internal milling cannot meet the requirements of the cavity surface.
Multi-pass milling is used combined with shot peening and heat treatment, including clamping and positioning, rough milling, fine milling, shot peening, heat treatment and fine grinding. The structural strength and fatigue resistance are improved through multi-pass heat treatment to ensure surface accuracy and quality.
The processing accuracy and service life of the transmission shaft surface are improved. The cavity surface is further strengthened through shot peening and multi-pass heat treatment to ensure that the surface roughness is ≤ Ra0.6 microns, which improves the processing quality and structural strength.
Smart Images

Figure CN115502674B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of part surface milling, and in particular relates to a surface milling method for a vehicle steering wheel transmission shaft. Background Art
[0002] The steering column mechanism is used to connect the steering wheel and the steering gear. Through the steering column mechanism, the vehicle driver transmits the torque to the steering gear, driving the steering gear to achieve steering. For example, Chinese patent CN201410519792.3 discloses an output shaft for a steering column of a car steering wheel, which belongs to the field of automobile technology. It includes a transmission shaft with a hollow structure, a torsion bar passing through the hollow part of the transmission shaft, and the torsion bar is fixed to the transmission shaft through a cylindrical pin. A pin hole is opened on the torsion bar at the matching position of the torsion bar and the transmission shaft. The opening direction of the pin hole is consistent with the length direction of the torsion bar. An expansion pin is arranged in the pin hole. Bolts for fixing the torsion bar are arranged on the transmission shaft on the right side of the cylindrical pin, corresponding to the same position of the torsion bar, in front, behind, left and right of the position.
[0003] The hollow structure transmission shaft of the steering column of the car steering wheel is processed by casting. After the processing is completed, the internal cavity of the transmission shaft needs to be milled to improve the processing accuracy, so as to avoid easy wear on the cavity surface and shorten the service life. However, simply milling the internal cavity of the transmission shaft, the processing accuracy can no longer meet the requirements of the cavity surface, and the cavity surface needs to be further strengthened. Summary of the invention
[0004] The purpose of the present invention is to provide a surface milling method for a steering wheel transmission shaft of an automobile, which ensures the surface processing accuracy through multi-pass milling processing and further strengthens the cavity surface through shot peening processing.
[0005] In order to achieve the above object, the present invention adopts the following technical scheme: a surface milling method for a steering wheel transmission shaft of an automobile, comprising the following steps:
[0006] S1. Clamp and position the transmission shaft casting, and calculate the milling depth of the internal cavity of the transmission shaft casting;
[0007] S2. Rough milling is performed on the internal cavity of the transmission shaft casting, and a machining allowance of 1 mm is reserved after the machining is completed;
[0008] S3, flattening the inner cavity of the transmission shaft casting after rough milling, and performing fine milling;
[0009] S4, after fine milling, the transmission shaft casting is subjected to shot peening treatment on the inner cavity of the transmission shaft casting by using a shot peening device;
[0010] S5. After shot peening, the transmission shaft casting is placed in a heat treatment furnace for heat treatment, heated to 650-750 degrees, kept warm for 1-3 hours, and cooled to room temperature;
[0011] S6. After the heat treatment, the internal cavity of the transmission shaft casting is finely polished. After fine polishing, the surface roughness of the internal cavity surface of the transmission shaft casting is ≤Ra0.6 microns.
[0012] As a further description of the above technical solution:
[0013] In step S4, before the drive shaft casting is shot peened, the drive shaft casting is re-clamped and positioned, the outer surface of the drive shaft casting is polished, and then the inner cavity of the drive shaft casting and the outer surface of the drive shaft casting are shot peened.
[0014] As a further description of the above technical solution:
[0015] In step S4, the outer surface of the transmission shaft casting is roughly ground for multiple times.
[0016] As a further description of the above technical solution:
[0017] In step S3, after the transmission shaft casting is fine-milled, a surface detection method is used to detect the surface machining accuracy, and the fine machining is repeated until the surface machining accuracy meets the preset requirements.
[0018] As a further description of the above technical solution:
[0019] In step S1, before clamping and positioning the transmission shaft casting, the surface of the transmission shaft casting is pickled.
[0020] As a further description of the above technical solution:
[0021] In step S1, before clamping and positioning the transmission shaft casting, the pickled transmission shaft casting is first placed in a heat treatment furnace for heat treatment, heated to 560-640 degrees, kept warm for 1-3 hours, and cooled to room temperature.
[0022] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are:
[0023] 1. In the present invention, after the casting process of the transmission shaft is completed, on the one hand, multi-pass milling is used to ensure the surface processing accuracy and processing efficiency to avoid easy wear of the cavity surface. On the other hand, the internal cavity of the transmission shaft and the outer surface of the transmission shaft are strengthened by shot peening to further strengthen the cavity surface. Finally, the internal cavity of the transmission shaft is finely polished to further improve the processing accuracy.
[0024] 2. In the present invention, the strength and fatigue resistance of the structure are improved by preliminary heat treatment before rough milling, so as to ensure the quality of milling. At the same time, heat treatment is performed again before fine grinding of the internal cavity of the transmission shaft casting to fully ensure the grinding quality. The multi-pass heat treatment process effectively improves the processing quality of the transmission shaft casting. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.
[0026] Figure 1 The present invention is a flow chart of a surface milling method for a vehicle steering wheel transmission shaft. DETAILED DESCRIPTION
[0027] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0028] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0029] See also Figure 1 The present invention provides a technical solution: a surface milling method for a steering wheel transmission shaft of an automobile, comprising the following steps:
[0030] S1. Clamp and position the transmission shaft casting, and calculate the milling depth of the internal cavity of the transmission shaft casting;
[0031] S2. Rough milling is performed on the internal cavity of the transmission shaft casting, and a machining allowance of 1 mm is reserved after the machining is completed;
[0032] S3, flattening the inner cavity of the transmission shaft casting after rough milling, and performing fine milling;
[0033] S4, after fine milling, the transmission shaft casting is subjected to shot peening treatment on the inner cavity of the transmission shaft casting by using a shot peening device;
[0034] S5. After shot peening, the transmission shaft casting is placed in a heat treatment furnace for heat treatment, heated to 680 degrees, kept warm for 1.5 hours, stress-relief annealed for 3 hours, and then air-cooled to room temperature;
[0035] S6. After the heat treatment, the internal cavity of the transmission shaft casting is finely polished. After fine polishing, the surface roughness of the internal cavity surface of the transmission shaft casting is ≤Ra0.6 microns.
[0036] In step S4, before the drive shaft casting is shot peened, the drive shaft casting is re-clamped and positioned, and the outer surface of the drive shaft casting is polished. Then, the internal cavity of the drive shaft casting and the outer surface of the drive shaft casting are shot peened, and the outer surface of the drive shaft casting is also strengthened to improve the quality of the outer surface of the drive shaft casting.
[0037] In step S4, the outer surface of the transmission shaft casting is rough-grinded for multiple times. After each rough-grinding, the grinding quality and the wear of the grinding equipment are tested. The grinding time and rotation speed are adjusted according to the above test results, and the grinding is continued until the surface roughness meets the requirements.
[0038] In step S3, after the transmission shaft casting is fine-milled, a surface detection method is used to detect the surface machining accuracy, and fine machining is repeated until the surface machining accuracy meets the preset requirements, thereby fully ensuring the machining quality of the milling process.
[0039] In step S1, before clamping and positioning the transmission shaft casting, the surface of the transmission shaft casting is pickled to make the surface of the transmission shaft casting clean, and hydrochloric acid pickling can be used to clean the surface of the transmission shaft casting after pickling, and then drying.
[0040] In step S1, before clamping and positioning the transmission shaft casting, the pickled transmission shaft casting is first placed in a heat treatment furnace for heat treatment, heated to 600 degrees, kept warm for 2 hours, and stress-relief annealed for 3 hours and then air-cooled to room temperature. The preliminary heat treatment is used to improve the strength and fatigue resistance of the structure and ensure the quality of milling processing.
[0041] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A surface milling method for a steering wheel transmission shaft of an automobile, characterized in that: The following steps are involved: S1. Clamp and position the transmission shaft casting, calculate the milling depth of the internal cavity of the transmission shaft casting, pickle the surface of the transmission shaft casting before clamping and positioning the transmission shaft casting, put the pickled transmission shaft casting into a heat treatment furnace for heat treatment, heat it to 560-640 degrees, keep it warm for 1-3 hours, and cool it to room temperature; S2. Rough milling is performed on the internal cavity of the transmission shaft casting, and a machining allowance of 1 mm is reserved after the machining is completed; S3, flattening the inner cavity of the transmission shaft casting after rough milling, and performing fine milling; S4, after fine milling, the transmission shaft casting is subjected to shot peening treatment on the inner cavity of the transmission shaft casting by using a shot peening device, before the transmission shaft casting is subjected to shot peening treatment, the transmission shaft casting is re-clamped and positioned, the outer surface of the transmission shaft casting is polished, and then the inner cavity of the transmission shaft casting and the outer surface of the transmission shaft casting are subjected to shot peening treatment; S5. After shot peening, the transmission shaft casting is placed in a heat treatment furnace for heat treatment, heated to 650-750 degrees, kept warm for 1-3 hours, and cooled to room temperature; S6. After the heat treatment, the internal cavity of the transmission shaft casting is finely polished. After fine polishing, the surface roughness of the internal cavity surface of the transmission shaft casting is ≤Ra0.6 microns.
2. The surface milling method of a vehicle steering wheel transmission shaft according to claim 1, characterized in that: In step S4, the outer surface of the transmission shaft casting is roughly ground multiple times.
3. The surface milling method of a vehicle steering wheel transmission shaft according to claim 1, characterized in that: In step S3, after the transmission shaft casting is fine-milled, a surface detection method is used to detect the surface machining accuracy, and fine-machining is repeated until the surface machining accuracy meets the preset requirements.
Citation Information
Patent Citations
Output shaft for steering column of steering wheel of vehicle
CN105438245A
Transmission shaft manufacturing process
CN106425345A
Motorcycle starting lever machining technology
CN108480932A
New energy automobile front and rear axle surface roughness treatment method
CN112296764A
Thermal spraying pretreatment method for casting
JP2009183961A