Assembly process of a supercooler for upward continuous casting
By designing graphite filter, multi-row pores and joint graphite casing in the upper-induction continuous casting crystallizer, combined with cone connection, the problem of low circulating cooling water pressure and scale of the inner copper tube wall is solved, and small dense grains are achieved and efficient cooling improve product quality and production efficiency.
Patent Information
- Application Number
- CN202211179382.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-27
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2042-09-27
AI Technical Summary
The existing upper-induction continuous casting crystallizers have low circulating cooling water pressure, insufficient cooling, lots of scale on the inner copper pipe wall, easy to block, large grains, segregation of components, poor surface quality, slow lead speed, low yield and graphite molds. Crack problems caused by threaded connection with medium copper pipe.
Using an assembly process of an ultra-cooler for continuous casting, including the design of outer steel pipe, medium copper pipe and inner copper pipe. The outer steel pipe is equipped with graphite filter and handle, multiple rows of holes are installed at the bottom of the middle copper pipe, and inner copper pipe is installed. A joint graphite casing is installed on the surface, and the cooling area is increased through conical connections to avoid traditional thread grooves and ensure uniform and stable cooling.
The ultra-strength uniform cooling of liquid metal in the primary cooling zone is achieved, and the rapid and stable flow of the secondary cooling zone is improved, which improves the fine and dense grains of the product, the unsegregated alloy content, the surface quality and production efficiency, and extends the service life of the crystallizer. .
Smart Images

Figure CN115533512B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of upward vertical casting of copper and copper alloys, and in particular to an assembly process of a supercooler for upward continuous casting. Background Art
[0002] The copper alloy upward continuous casting crystallizer adopts a double-layer water-cooled jacket structure. It is mainly composed of inner, middle and outer cooling water pipes, graphite molds, graphite protective sleeves, thermal insulation materials, etc. The outer water pipe is made of alloy steel, and the inner and middle water pipes are made of copper. The quality and service life of the inner water pipe during upward continuous casting are directly related to the quality of the continuous casting rod blank. The cooling cavity formed between the inner and middle water pipes is divided into two parts: the primary cooling zone and the secondary cooling zone. The cooling cavity is connected to the water outlet, and the primary cooling zone is particularly important and directly related to the quality of the upward rod blank. The water delivery cavity formed between the middle and outer water pipes is connected to the water inlet. The water delivery quality of the water delivery cavity directly affects the cooling and crystallization of the liquid metal in the primary cooling zone inside the graphite mold by the cooling cavity, and the two complement each other.
[0003] The existing upward continuous casting crystallizer has the following defects: the circulating cooling water pressure is low and the cooling is insufficient; there is a lot of scale on the inner copper tube wall, which is easy to block the outlet space, the grains produced by the upward continuous casting are coarse, the components are segregated, the surface quality is poor, the casting speed is slow, and the output is low; the graphite mold and the middle copper tube are connected by threads, which causes cracks and fissures in the primary cooling zone of the crystallizer, that is, the external thread interface of the graphite mold, which seriously affects the internal quality of the upper lead rod. Summary of the invention
[0004] The purpose of the present invention is to overcome the above-mentioned shortcomings and provide an assembly process for a supercooler for upward continuous casting, so that during upward continuous casting, the liquid metal is subjected to ultra-high-intensity uniform cooling and crystallization in the primary cooling zone to obtain fine and dense grains, while the rapid and stable circulating flow cooling effect in the secondary cooling zone is enhanced, thereby greatly improving the safety production efficiency, and ensuring that the product crystallization, alloy content, performance and surface quality are free of segregation.
[0005] The object of the present invention is achieved in that:
[0006] An assembly process of an ultracooler for upward continuous casting comprises the following steps:
[0007] Step 1: Clamp the outer steel pipe firmly on the bench vise;
[0008] Step 2: Remove the cold end cap, put each graphite sleeve on the outer wall of the inner copper tube one by one, and adjust the size between the graphite sleeve and the inner copper tube wall;
[0009] Step 3: After the outer steel tube, middle copper tube and inner copper tube are installed, reinstall the cold end convex cap;
[0010] Step 4: Make a graphite crystallization mold, with a conical end at one end and an external thread at the other end;
[0011] Step 5: Hot pressing of graphite crystallization mold and inner copper tube;
[0012] Step 6: After the press-fitting is completed, install the thermal insulation protective layer at the hot end of the inner copper tube;
[0013] Step 7: Tighten the graphite cap with the copper liquid hole and the external thread of the graphite crystallization mold, and the supercooler is assembled.
[0014] Preferably, in the fifth step, before the graphite crystallization mold and the inner copper tube are press-fitted, the surface finish to be press-fitted is polished.
[0015] Preferably, in the sixth step, the hot end of the inner copper tube is wrapped with thermal insulation cotton, and the laminated graphite protective sleeve passes through the graphite crystallization mold sleeve and is pressed onto the outside of the laminated thermal insulation cotton.
[0016] Preferably, graphite mud is used to fill the gap between the graphite crystallization mold and the fitted graphite protective sleeve, and the graphite mud is pushed into the gap with a scraper to completely seal it.
[0017] Preferably, in the third step, a ring column water inlet cavity is formed between the outer steel tube and the middle copper tube and communicates with the water inlet, and a graphite mesh is provided at the water inlet.
[0018] Preferably, multiple rows of holes are provided at the bottom of the middle copper tube.
[0019] Preferably, a handle is provided outside the outer steel tube.
[0020] The beneficial effects of the present invention are:
[0021] 1. A graphite filter is installed at the water inlet of the outer steel pipe to filter impurities in the circulating cooling water and pressurize the incoming water; a handle is installed on the wall of the outer steel pipe to facilitate the furnace workers to safely load and unload the supercooler;
[0022] 2. Set multiple rows of holes at the bottom of the middle copper tube to increase the water pressure in the primary cooling zone and increase the flow rate; strengthen the cooling of the primary cooling zone;
[0023] 3. A segmented graphite sleeve is set on the surface of the inner copper tube to increase the secondary cooling area; prevent scale and corrosion from forming on the outer wall of the inner copper tube; and extend the life of the crystallizer;
[0024] 4. A conical mouth is set at the bottom of the inner copper tube to connect with the conical crystallization graphite mold. The conical shape increases the cooling area; the casting cooling crystallization is uniform without the traditional thread groove; the alloy content inside the ingot is stable without segregation; the cooling is sufficient; the electromechanical properties of the ingot are stable; the conical connection upper continuous casting is seamlessly connected with the inner copper tube; it is suitable for upper vertical casting technology.
[0025] In summary, the present invention can effectively solve the quality problems of the upper lead rod blank, such as cracks, fissures, coarse grains, dark color, broken rods, unstable electromechanical performance, etc., to ensure the overall quality of the copper rod, while appropriately increasing the lead speed, improving production efficiency, and extending the service life of the crystallizer. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a structural schematic diagram of the present invention.
[0027] Figure 2 for Figure 1 A partial enlarged view of .
[0028] Figure 3 It is a schematic diagram of the appearance of the present invention.
[0029] Figure 4 Schematic diagram of the structure of the outer steel pipe.
[0030] Figure 5 for Figure 4 Side view of.
[0031] Figure 6 It is a schematic diagram of the structure of the copper tube.
[0032] Figure 7 Schematic diagram of the structure of the inner copper tube.
[0033] Figure 8 Schematic diagram of the structure of the graphite crystallization mold.
[0034] Among them: 1. Cold end convex cap; 2. Water outlet; 3. Graphite mesh; 4. Water inlet; 5. Inner copper tube; 6. Graphite sleeve; 7. Outer steel tube; 8. Handle; 9. Middle copper tube; 10. Laminated graphite protective sleeve; 11. Laminated insulation cotton; 12. Graphite crystallization mold; 13. Graphite cap; 14. Threaded mouth; 15. Conical end of inner copper tube; 16. Conical end of graphite crystallization mold; 17. Multiple rows of holes; 18. Connecting threads; 19. Copper liquid hole. DETAILED DESCRIPTION
[0035] See also Figure 1-8The present invention relates to an ultracooler for upward continuous casting, which comprises an inner copper tube 5, a middle copper tube 9, an outer steel tube 7 and a graphite crystallization mold 12. The inner copper tube 5 is provided with a graphite sleeve 6, and the graphite sleeve 6 is multi-sectioned. The bottom of the inner copper tube 5 is provided with an inner copper tube conical end 15. One end of the graphite crystallization mold 12 is provided with a graphite crystallization mold conical end 16 matching the inner copper tube conical end 15, and the other end is screwed with a graphite cap 13 through a connecting thread 18. The graphite cap 13 is provided with a copper liquid hole 19. The inner copper The conical end 15 of the tube is hot-pressed with the conical end 16 of the graphite crystallization mold. The connection area between the conical end 15 of the inner copper tube and the conical end 16 of the graphite crystallization mold is a primary cooling (crystallization) zone, and the upper part of the primary cooling zone is a secondary cooling zone. The top and bottom of the outer steel tube 7 are both provided with threaded openings 14. The top of the outer steel tube 7 is threadedly connected to the top of the middle copper tube 9. The bottom of the middle copper tube 9 is provided with multiple rows of holes 17. The bottom of the inner copper tube 9 is extended outwardly with a rim, and the bottom of the outer steel tube 7 is threadedly connected to the rim of the bottom of the inner copper tube 9.
[0036] A fitted graphite protective sleeve 10 is provided on the outside of the bottom of the inner copper tube 5, and the upper part of the inner copper tube 5 is positioned by a cold end convex cap 1. An annular column water inlet cavity is formed between the outer steel tube 7 and the middle copper tube 9 and is communicated with the water inlet 4. A graphite mesh 3 is provided on the water inlet 4. A circulating cooling cavity is formed between the middle copper tube 9 and the inner copper tube 5 and is communicated with the water outlet 2.
[0037] The outer steel pipe 7 is provided with a handle 8 to facilitate furnace workers to safely load and unload the supercooler.
[0038] The outer steel tube 7 is made of heat-resistant alloy steel.
[0039] An assembly process of an ultracooler for upward continuous casting comprises the following steps:
[0040] Step 1: Clamp the outer steel pipe 7 firmly on the bench vise;
[0041] Step 2: Remove the cold end convex cap 1, and put each graphite sleeve 6 on the outer wall of the inner copper tube 5 one by one, and adjust the size matching between the graphite sleeve 6 and the wall of the inner copper tube 5;
[0042] Step 3: After the outer steel tube 7, the middle copper tube 9 and the inner copper tube 5 are installed, reinstall the cold end convex cap 1;
[0043] Step 4: Making a graphite crystallization mold 12, wherein one end of the graphite crystallization mold 12 is provided with a tapered end and the other end is provided with an external thread;
[0044] Step 5: hot pressing the graphite crystallization mold 12 and the inner copper tube 5;
[0045] Step 6: After the press-fitting is completed, install the thermal insulation protective layer at the hot end of the inner copper tube; wrap the hot end of the inner copper tube 5 with the thermal insulation cotton 11, and pass the laminated graphite protective sleeve 10 through the graphite crystallization mold 12 and press it on the outside of the laminated thermal insulation cotton 11; use graphite mud to fill the gap between the graphite crystallization mold 12 and the laminated graphite protective sleeve 10, and use a scraper to push the graphite mud into the gap to completely seal it.
[0046] Step 7: Tighten the graphite cap 13 with the copper liquid hole 19 and the external thread of the graphite crystallization mold 12, and the supercooler is assembled.
[0047] After the supercooler is completed, it can be fixed on the continuous casting upper lead frame through the symmetrical protrusions arranged on the outer steel pipe 7 after pressure testing and baking.
[0048] In the fifth step, before the graphite crystallization mold 12 is press-fitted with the inner copper tube 5, the surface finish to be press-fitted is polished; the hot end inner copper tube 5 is polished and cleaned with fine sandpaper, that is, the inner hole of the tapered end of the inner copper tube is polished to remove debris that may remain in the previous casting operation, and then the graphite crystallization mold tapered end 16 of the graphite crystallization mold is inserted into the tapered end of the inner copper tube, and pushed inward while rotating, and then rotated and withdrawn in the same direction; the raised parts of the outer surface of the tapered end 16 of the withdrawn graphite crystallization mold will be highlighted, and these raised parts are carefully polished with a fine sand polishing pad; the operation is repeated until a good polished bonding surface is obtained, and the surface of the inserted section of the polished and matched graphite crystallization mold 12 is uniformly bright, but it should be noted that the polishing should not be excessive.
[0049] The hot pressing device uses boiling water to heat the supercooler, and uses a kettle to inject hot water through the water inlet 4 to operate or configure facilities such as water heaters, water pumps and water pipes. When the surface of the cooler is heated to an appropriate temperature, the graphite crystallization mold 12 can be inserted and installed; the graphite crystallization mold 12 is slowly pushed into the head of the hot end, keeping it straight and slowly pushed in.
[0050] Here’s how it works:
[0051] A graphite filter is arranged at the water inlet of the outer steel pipe to filter impurities in the cooling circulating water and pressurize the inlet water at the same time; a handle is designed on the wall of the outer steel pipe to facilitate furnace workers to safely load and unload the upward continuous casting supercooler; multiple rows of holes are arranged at the bottom of the middle copper pipe to secondary pressurize the cooling water and strengthen the cooling and crystallization of the primary cooling zone; a node-shaped graphite sleeve is arranged on the surface of the inner copper pipe to protect the scale and corrosion products on the surface of the inner copper pipe, and at the same time, the cooling area of the secondary cooling zone is increased, the cooling is strengthened, and the cooling effect of the secondary cooling zone is ensured; the tapered mouth at the bottom of the inner copper pipe is connected with the tapered mouth of the crystallization graphite mold, the cooling area of the primary cooling crystallization zone is increased, sufficient cooling is provided, and the crystallization zone is uniformly cooled, so as to keep the alloy content of the casting billet stable without segregation and the electromechanical properties stable, and at the same time, the upward continuous casting principle is used to achieve a seamless connection effect between the crystallization mold and the cooling inner copper pipe during the casting process, thereby ensuring the surface and performance quality of the rod billet.
[0052] In addition to the above embodiments, the present invention also includes other implementation modes. Any technical solutions formed by equivalent transformation or equivalent replacement should fall within the protection scope of the claims of the present invention.
Claims
1. An assembly process of an upward continuous casting supercooler, characterized in that: The following steps are involved: Step 1: Clamp the outer steel pipe firmly on the bench vise; Step 2: Remove the cold end cap, put each graphite sleeve on the outer wall of the inner copper tube one by one, and adjust the size between the graphite sleeve and the inner copper tube wall; Step 3: After the outer steel tube, middle copper tube and inner copper tube are installed, reinstall the cold end convex cap; Step 4: Make a graphite crystallization mold, with a conical end at one end and an external thread at the other end; Step 5: Hot pressing of graphite crystallization mold and inner copper tube; Step 6: After the press-fitting is completed, install the thermal insulation protective layer at the hot end of the inner copper tube; Step 7: Tighten the graphite cap with the copper liquid hole and the external thread of the graphite crystallization mold, and the supercooler is assembled.
2. The assembly process of the supercooler for upward continuous casting according to claim 1 is characterized in that: In the fifth step, before the graphite crystallization mold and the inner copper tube are press-fitted, the surface finish to be press-fitted is polished.
3. The assembly process of the supercooler for upward continuous casting according to claim 1 is characterized in that: In the sixth step, the hot end of the inner copper tube is wrapped with thermal insulation cotton, and the laminated graphite protective sleeve passes through the graphite crystallization mold sleeve and is pressed onto the outside of the laminated thermal insulation cotton.
4. The assembly process of the supercooler for upward continuous casting according to claim 3 is characterized in that: Use graphite mud to fill the gap between the graphite crystallization mold and the fitted graphite protective sleeve, and use a scraper to push the graphite mud into the gap to completely seal it.
5. The assembly process of the upward continuous casting supercooler according to claim 1, characterized in that: In the third step, a ring column water inlet cavity is formed between the outer steel tube and the middle copper tube and communicates with the water inlet, and a graphite mesh is provided at the water inlet.
6. The assembly process of the supercooler for upward continuous casting according to claim 5 is characterized in that: A plurality of rows of holes are arranged at the bottom of the middle copper tube.
7. The assembly process of the supercooler for upward continuous casting according to claim 5 is characterized in that: A handle is arranged outside the outer steel pipe.
Citation Information
Patent Citations
Ultra-cooler for up-drawing continuous casting
CN218395860U