A method for recovering CO2 by multi-stage pressure swing adsorption
Through the method of recovering CO2 through multi-stage pressure swing adsorption cascades, the CO2 analyzer is used to detect and recover different concentrations of CO2 in real time, which solves the problems of different CO2 concentration requirements and device complexity in the existing technology, and realizes efficient and low-cost CO2 capture.
Patent Information
- Application Number
- CN202211713252.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-29
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-12-29
AI Technical Summary
The existing pressure swing adsorption method mainly focuses on improving the purity of the product gas in CO2 capture, which cannot meet the different CO2 concentration requirements of different industrial applications. The device is complex and energy consumption is high.
A multi-stage pressure swing adsorption cascade method is used to recover CO2, and the purity changes of the desorbed gas are detected in real time through a CO2 analyzer. The high-concentration desorbed gas is recycled as a product, and the low-concentration desorbed gas is used as the raw material gas for adsorption in the lower stage, reducing the amount of subsequent processing. , achieving low-cost capture of CO2.
It achieves precise recovery of CO2 at multiple concentrations, reduces energy consumption, simplifies the device structure, improves capture efficiency, and reduces investment and operating costs.
Smart Images

Figure CN115738592B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of adsorption technology and relates to a method for recovering CO2 from industrial flue gas by pressure swing adsorption, and in particular to a method for recovering CO2 by using multi-stage pressure swing adsorption steps. Background Art
[0002] In recent years, the global greenhouse effect has further intensified, and CO2 is the main gas causing the greenhouse effect. CO2 emissions mainly come from industrial emissions. The power, steel, cement and other industries are the main sources of CO2 emissions. CO2 emissions mainly come from fuel combustion, raw material decomposition and other processes in the production process.
[0003] For the reduction of industrial CO2 emissions, adsorption capture is a carbon reduction technology with good prospects. The adsorption method mainly includes three categories: pressure swing adsorption (PSA / VPSA), temperature swing adsorption (TSA), and electroswing adsorption (ESA). Pressure swing adsorption is a method that uses the characteristics of solid particle adsorbents under the same conditions to achieve alternating adsorption and desorption processes through periodic pressure changes according to the different adsorption capacities of different gas components, thereby achieving gas separation or purification. The substance adsorbed on the surface of the solid adsorbent is the adsorption phase. Most pressure swing adsorption is a physical process that can be achieved at room temperature. Pressure swing adsorption has the advantages of short operating cycle, high degree of automation, and low energy consumption. There are corresponding commercial demonstrations in the field of gas capture, and it is currently a research hotspot.
[0004] At present, the research on capturing CO2 by pressure swing adsorption is mainly focused on improving the purity of product gas and large-scale application. At present, CO2 gas is mainly purified to industrial grade standards (concentration ≥ 99%) or food grade standards (concentration ≥ 99.9%), and then applied to industry or food industry. However, there are differences in the concentration requirements of CO2 in actual applications. For example, microalgae carbon fixation, concrete CO2 mineralization maintenance, etc. do not require high CO2 concentration.
[0005] Therefore, a method for multi-stage pressure swing adsorption cascade recovery of CO2 is developed specifically, and the changing characteristics of the desorbed gas purity during the desorption process are rationally utilized for segmented collection to obtain CO2 of different purities. Summary of the invention
[0006] The object of the present invention is to provide a method for recovering CO2 in stages by multi-stage pressure swing adsorption, wherein the desorbed gas is recovered in stages according to concentration, the product gas can be used in different ways, and the gas processing amount of the lower stage adsorption is reduced, thereby achieving simplification of the CO2 capture device and low-cost capture of CO2.
[0007] In order to achieve the purpose of the invention, the present invention adopts the following technical solutions:
[0008] The present invention provides a method for recovering CO2 by multi-stage pressure swing adsorption, the method comprising multi-stage pressure swing adsorption, each stage of pressure swing adsorption comprising adsorption, release, desorption and pressure increase in sequence;
[0009] During the desorption process, the purity change is detected in real time by a CO2 analyzer, and the high-concentration desorbed gas is recovered as product gas, and the low-concentration desorbed gas is used as the feed gas for the next stage of pressure swing adsorption.
[0010] The present invention arranges the pressure swing adsorption unit in multiple stages according to the concentration and production requirements of the CO2 utilization end (the method flow diagram is shown in FIG. Figure 1 The CO2 analyzer is used to achieve accurate recovery of the target product gas, while reducing the gas processing volume and purification requirements in the subsequent adsorption stage and reducing energy consumption.
[0011] As a preferred technical solution of the present invention, the adsorption includes: passing the compressed raw gas into an adsorption tower so that CO2 is adsorbed on the adsorbent.
[0012] In the present invention, other gases and a small amount of unabsorbed CO2 gas are discharged from the outlet at the other end of the adsorption tower.
[0013] In the present invention, the valves of the feed pipeline and the exhaust pipeline of the adsorption tower are closed after the adsorption is completed.
[0014] As a preferred technical solution of the present invention, the sequential discharge includes: opening the sequential discharge valve of the adsorption tower after adsorption, and sequentially discharging the gas to another adsorption tower.
[0015] In the present invention, the pressure change during the sequential placement process is monitored in real time by a pressure sensor.
[0016] As a preferred technical solution of the present invention, the desorption includes: closing the downstream valve of the adsorption tower, opening the desorption valve, vacuum desorbing the adsorbent after adsorption, detecting the purity change of CO2 in real time through a CO2 analyzer, recovering the high-concentration desorbed gas as product gas, and using the low-concentration desorbed gas as the feed gas for the lower stage pressure swing adsorption.
[0017] In the present invention, a vacuum pump is provided on the exhaust pipeline connected to the desorbed gas.
[0018] In the present invention, the desorbed gas from the last stage of pressure swing adsorption is recovered as product gas.
[0019] As a preferred technical solution of the present invention, the pressure boosting includes sequential pressure boosting and final pressure boosting.
[0020] Preferably, the pressurized gas discharged in sequence is the downstream gas of another adsorption tower.
[0021] In the present invention, the pressurized gas comes from an adsorption tower that has completed pressure swing adsorption.
[0022] Preferably, the boosted gas whose pressure is finally increased is the feed gas and / or waste gas of each stage of pressure swing adsorption.
[0023] In the present invention, when the final pressure rise reaches the adsorption pressure, the next stage of pressure swing adsorption is carried out.
[0024] As a preferred technical solution of the present invention, each stage of pressure swing adsorption includes at least two adsorption towers.
[0025] Preferably, the adsorption tower is filled with an adsorbent.
[0026] Preferably, the adsorbent comprises any one of activated carbon, molecular sieve, silica gel or activated alumina, or a combination of at least two of them. Typical but non-limiting examples of the combination include: a combination of activated carbon and molecular sieve, a combination of molecular sieve and silica gel, or a combination of silica gel and activated alumina, etc., preferably molecular sieve.
[0027] As a preferred technical solution of the present invention, the adsorption pressure is 120-500kPa, for example, it can be 120kPa, 200kPa, 250kPa, 300kPa, 350kPa, 400kPa, 450kPa or 500kPa, but is not limited to the listed values. Other unlisted values within the numerical range are also applicable, preferably 200-300kPa.
[0028] Preferably, the adsorption temperature is 10-50°C, for example, it can be 10°C, 15°C, 20°C, 25°C, 30°C, 35°C, 40°C, 45°C or 50°C, but is not limited to the listed values. Other unlisted values within the numerical range are also applicable, preferably 10-20°C.
[0029] Preferably, the adsorption time is 1-10 min, for example, 1 min, 3 min, 5 min, 7 min, 9 min or 10 min, etc., but is not limited to the listed values, and other values not listed within the numerical range are also applicable.
[0030] Preferably, the pressure endpoint of the release is 60%-90% of the adsorption pressure, for example, it can be 60%, 65%, 70%, 75%, 80%, 85% or 90%, etc., but is not limited to the listed values. Other unlisted values within the numerical range are also applicable, preferably 60%-70% of the adsorption pressure.
[0031] As a preferred technical solution of the present invention, the pressure of the vacuum desorption is 10-80 kPa, for example, it can be 10 kPa, 20 kPa, 30 kPa, 40 kPa, 50 kPa, 60 kPa, 70 kPa or 80 kPa, but is not limited to the listed values, and other values not listed within the numerical range are also applicable, preferably 10-30 kPa;
[0032] In the present invention, the vacuum desorption time is 1-10 min, for example, it can be 1 min, 3 min, 5 min, 7 min, 9 min or 10 min, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0033] As a preferred technical solution of the present invention, the pressure endpoint of the sequential pressure increase is 20-200kPa, for example, it can be 20kPa, 40kPa, 60kPa, 80kPa, 100kPa, 120kPa, 140kPa, 160kPa, 180kPa or 200kPa, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0034] In the present invention, the pressure endpoint of the sequential release and pressure increase is controlled by the gas volume during the sequential release.
[0035] Preferably, the pressure endpoint of the final pressure rise is 120-500kPa, for example, it can be 120kPa, 200kPa, 250kPa, 300kPa, 350kPa, 400kPa, 450kPa or 500kPa, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0036] In the present invention, the pressure end point of the final pressure rise is the designed adsorption pressure.
[0037] As a preferred technical solution of the present invention, the concentration of CO2 in the product gas is 30.0%-99.9%, for example, it can be 30.0%, 40.0%, 50.0%, 60.0%, 70.0%, 80.0%, 90.0% or 99.9%, etc., but is not limited to the listed values, and other unlisted values within the numerical range are also applicable, preferably 50.0-99.9%.
[0038] Preferably, the concentration of CO2 in the low-concentration desorbed gas is 20.0%-90.0%, for example, it can be 20.0%, 30.0%, 40.0%, 50.0%, 60.0%, 70.0%, 80.0% or 99.0%, etc., but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0039] The numerical range described in the present invention not only includes the point values listed above, but also includes any point values between the above numerical ranges that are not listed. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values included in the range.
[0040] Compared with the prior art, the present invention has the following beneficial effects:
[0041] (1) The method provided by the present invention arranges the pressure swing adsorption unit in multiple stages according to the concentration and output demand standards of the CO2 utilization end, purifies CO2 step by step, and accurately recovers the CO2 product gas at multiple concentrations;
[0042] (2) The method provided by the present invention can produce usable product gas in each stage of pressure swing adsorption, while reducing the gas processing volume and purification requirements of the subsequent adsorption stage, improving the CO2 capture efficiency, reducing energy consumption, and reducing the floor space and investment and operating costs of the adsorption device. BRIEF DESCRIPTION OF THE DRAWINGS
[0043] Figure 1 A flow chart of the arrangement of a multi-stage pressure swing adsorption cascade recovery of CO2 provided by the present invention;
[0044] Figure 2 A schematic diagram of a two-stage pressure swing adsorption system device for stepwise recovery of CO2 provided by the present invention;
[0045] Among them, 1-compression device, 2-control valve (V1-V17), 3-adsorption tower (A, B, C and D), 4-vacuum pump, 5-CO2 analyzer, 6-pressure sensor, 7-buffer tank, 8-first product gas storage tank, 9-second product gas storage tank. DETAILED DESCRIPTION
[0046] The technical solution of the present invention is further described below by specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.
[0047] The present invention provides a system device for recovering CO2 by two-stage pressure swing adsorption cascade, and its structural schematic diagram is as follows: Figure 2 As shown; the system device includes a first pressure swing adsorption unit (PSA-1) and a second pressure swing adsorption unit (PSA-2);
[0048] The first pressure swing adsorption unit comprises a compression device 1, two parallel adsorption towers 3 (A and B), a vacuum pump 4, a CO2 analyzer 5, a pressure sensor 6, a buffer tank 7, a first product gas storage tank 8 and control valves (V1-V9);
[0049] A raw gas inlet is provided at the bottom of the adsorption tower 3-A; a compression device 1 is provided on the pipeline connecting the adsorption tower 3-A and the raw gas inlet;
[0050] A pressure sensor 6 is provided on the pipeline connecting the top of the adsorption tower 3-A and the adsorption tower 3-B;
[0051] The bottoms of the adsorption tower 3-A and the adsorption tower 3-B are connected in sequence with a vacuum pump 4 and a CO2 analyzer 5;
[0052] The CO2 analyzer 5 is connected to two pipelines, one of which is connected to the first product gas storage tank 8, and the other is connected to the buffer tank 7;
[0053] The second pressure swing adsorption unit comprises a compression device 1, two parallel adsorption towers 3 (C and D), a vacuum pump 4, a pressure sensor 6, a second product gas storage tank 9 and control valves (V10-V17);
[0054] The gas outlet of the buffer tank 7 is connected to the gas inlet of the adsorption tower 3-C; a compression device 1 is provided on the pipeline connecting the buffer tank 7 and the adsorption tower 3-C;
[0055] A pressure sensor 6 is provided on the pipeline connecting the adsorption tower 3-C and the top of the adsorption tower 3-D;
[0056] The bottoms of the adsorption tower 3-C and the adsorption tower 3-D are connected to a vacuum pump 4 and a second product gas storage tank 9;
[0057] The tops of the adsorption tower 3-A and the adsorption tower 3-C are both provided with pipelines for exhaust gas discharge.
[0058] The present invention provides a method for recovering CO2 by two-stage pressure swing adsorption cascade. Figure 2 The system device provided includes a first pressure swing adsorption (PSA-1 adsorption) and a first pressure swing adsorption (PSA-2 adsorption):
[0059] PAS-1 adsorption includes the following steps:
[0060] (1) Adsorption: Open the control valves V1, V2, and V6, pressurize the raw gas to the adsorption pressure through the compression device 1, and adsorb after the pressure in the adsorption tower A rises to the adsorption pressure. After the adsorption is completed, close the valves V1, V2, and V6;
[0061] (2) Discharge: Open the control valve V7 to discharge the gas in the adsorption tower 3-A into the adsorption tower 3-B, monitor the pressure change in real time through the pressure sensor 6, and close the valve V7 when the pressure drops to 60%-90% of the adsorption pressure;
[0062] (3) Desorption: Open the control valves V2, V3, and V8, use the vacuum pump 4 to perform vacuum desorption, and monitor the CO2 concentration in the desorbed gas in real time through the CO2 analyzer 5. The low-concentration desorbed gas is stored in the buffer tank 7 as the raw gas for the lower adsorption. When the set concentration target value is reached, close the control valve V8; open the control valve V9, recover the high-concentration desorbed gas as the product gas and store it in the first product gas tank 8. After the desorption is completed, close the control valves V2, V3, and V9;
[0063] (4) Pressure increase: Open the control valve V7, and the gas in the adsorption tower 3-B is discharged into the adsorption tower 3-A (except for the first pressure swing adsorption). The pressure change is monitored in real time by the pressure sensor 6. After reaching the target pressure, the valve V7 is closed. The feed gas and / or waste gas of each stage of pressure swing adsorption is used as the boost gas for the final pressure increase and is pressurized to the designed adsorption pressure;
[0064] PAS-2 adsorption includes the following steps:
[0065] (1) Adsorption: Open the control valves V10, V11, and V16, and pressurize the low-concentration desorbed gas in the buffer tank 7 to the adsorption pressure through the compression device 1. After the pressure in the adsorption tower 3-C rises to the adsorption pressure, adsorption is carried out. After the adsorption is completed, close the valves V10, V11, and V16;
[0066] (2) Discharge: Open the control valve V17 to discharge the gas in the adsorption tower 3-C into the adsorption tower 3-D, monitor the pressure change in real time through the pressure sensor 6, and close the valve V17 when the pressure drops to 60%-90% of the adsorption pressure;
[0067] (3) Desorption: Open the control valves V11, V13 and V15, and use the vacuum pump 4 to perform vacuum desorption. The desorbed gas is stored as product gas in the second product gas tank 9. After the desorption is completed, close the control valves V11, V13 and V15;
[0068] (4) Pressure increase: Open the control valve V17, and the gas in the adsorption tower 3-D is discharged into the adsorption tower 3-C (except for the first pressure swing adsorption). The pressure change is monitored in real time by the pressure sensor 6. After reaching the target pressure, the valve V17 is closed. The feed gas and / or waste gas of each stage of pressure swing adsorption is used as the boost gas for the final pressure increase and is pressurized to the designed adsorption pressure;
[0069] The method of recovering CO2 by pressure swing adsorption cascade with more than two stages is similar to the method of recovering CO2 by pressure swing adsorption cascade with two stages, except that the low-concentration desorbed gas in the buffer tank 7 is repeatedly subjected to PSA-1 adsorption for a cycle.
[0070] Example 1
[0071] This embodiment provides a method for recovering CO2 by two-stage pressure swing adsorption, wherein the pressure swing adsorption process includes a first pressure swing adsorption (PSA-1 adsorption) and a second pressure swing adsorption (PSA-2 adsorption):
[0072] PSA-1 involves the following steps:
[0073] (1) The compressed blast furnace gas is passed into an adsorption tower to adsorb CO2 on the 13X molecular sieve filled in the adsorption tower. The adsorption pressure is 200 kPa, the temperature is 20°C, and the time is 1 min;
[0074] The blast furnace gas comes from a steel plant with a gas volume of 3000 Nm 3 / h, the raw material composition is 55% N2, 17.8% CO2, 25% CO, 1.5% H2, 0.4% CH4 and 0.3% O2;
[0075] (2) Open the discharge valve of the adsorption tower after adsorption and discharge the gas to another adsorption tower. The pressure endpoint of the discharge is 120 kPa;
[0076] (3) The downstream valve of the adsorption tower is closed, and the desorption valve is opened to perform vacuum desorption on the 13X molecular sieve that adsorbs CO2, and the pressure of the vacuum desorption is 10 kPa; the purity change of CO2 is detected by a CO2 analyzer, and the CO2 with a concentration of more than 60% is recovered as product gas 1, and the CO2 with a concentration of less than 60% is used as the feed gas for the second stage pressure swing adsorption;
[0077] (4) The pressure of the vented gas from another adsorption tower into the adsorption tower is raised to 100 kPa;
[0078] PSA-2 includes the following steps:
[0079] (1') Compressing CO2 with a concentration of less than 60% and passing it into an adsorption tower, so that the CO2 is adsorbed on the 13X molecular sieve filled in the adsorption tower, and the adsorption pressure is 150 kPa, the temperature is 20° C., and the time is 1 min;
[0080] (2') Open the discharge valve of the adsorption tower after adsorption, and discharge the gas to another adsorption tower. The pressure endpoint of the discharge is 90 kPa;
[0081] (3') Close the downstream valve of the adsorption tower, open the desorption valve to vacuum desorb the 13X molecular sieve adsorbing CO2, the vacuum desorption pressure is 30 kPa, and the time is 1 min; the desorbed gas is recovered as product gas 2;
[0082] (4') The pressure of the vent gas from another adsorption tower discharged into the adsorption tower is raised to 70 kPa, and the feed gas and waste gas of the second stage pressure swing adsorption are used as the boost gas for the final pressure increase and are pressurized to the designed adsorption pressure.
[0083] The composition of the product gas at each stage obtained by two-stage pressure swing adsorption in this embodiment is shown in Table 1;
[0084] Table 1
[0085]
[0086] By applying the two-stage pressure swing adsorption stepwise recovery method of CO2 provided in this embodiment, two product gases with obvious concentration gradients were obtained. The concentration of CO in the exhaust gas was 36.1%, which was a high calorific value gas and could be recycled.
[0087] Example 2
[0088] This embodiment provides a method for recovering CO2 by three-stage pressure swing adsorption, wherein the pressure swing adsorption process includes a first pressure swing adsorption (PSA-1 adsorption), a first pressure swing adsorption (PSA-2 adsorption) and a third pressure swing adsorption (PSA-3 adsorption):
[0089] PSA-1 involves the following steps:
[0090] (1) The compressed cement kiln flue gas is passed into an adsorption tower to adsorb CO2 on the 13X molecular sieve filled in the adsorption tower. The adsorption pressure is 150 kPa, the temperature is 20°C, and the time is 1 min;
[0091] The cement kiln flue gas comes from a steel plant with a gas volume of 10000Nm 3 / h, the raw material composition is 68.5% N2, 25.0% CO2, 1.0% CO and 5.5% O2;
[0092] (2) Open the discharge valve of the adsorption tower after adsorption and discharge the gas to another adsorption tower. The pressure endpoint of the discharge is 105 kPa;
[0093] (3) The downstream valve of the adsorption tower is closed, and the desorption valve is opened to perform vacuum desorption on the 13X molecular sieve that adsorbs CO2, and the pressure of the vacuum desorption is 20 kPa; the purity change of CO2 is detected by a CO2 analyzer, and the CO2 with a concentration of more than 50% is recovered as product gas 1, and the CO2 with a concentration of less than 50% is used as the feed gas for the second stage pressure swing adsorption;
[0094] (4) The pressure of the vented gas from another adsorption tower into the adsorption tower is raised to 90 kPa;
[0095] PSA-2 includes the following steps:
[0096] (1') CO2 with a concentration of less than 50% is compressed and introduced into an adsorption tower, so that the CO2 is adsorbed on the 13X molecular sieve filled in the adsorption tower, and the adsorption pressure is 120 kPa, the temperature is 20° C., and the time is 1 min;
[0097] (2') Open the discharge valve of the adsorption tower after adsorption, and discharge the gas to another adsorption tower. The end point of the discharge pressure is 80 kPa;
[0098] (3') The downstream valve of the adsorption tower is closed, and the desorption valve is opened to perform vacuum desorption on the 13X molecular sieve adsorbing CO2, and the pressure of the vacuum desorption is 20 kPa; the purity change of CO2 is detected by a CO2 analyzer, and the CO2 with a concentration of more than 80% is recovered as the product gas 2, and the CO2 with a concentration of less than 80% is used as the feed gas for the third stage of pressure swing adsorption;
[0099] (4') The pressure of the vented gas from another adsorption tower into the adsorption tower is raised to 70 kPa;
[0100] PSA-3 includes the following steps:
[0101] (1") CO2 with a concentration of less than 80% is compressed and introduced into an adsorption tower, so that the CO2 is adsorbed on a 13X molecular sieve filled in the adsorption tower, and the adsorption pressure is 120 kPa, the temperature is 20° C., and the time is 1 min;
[0102] (2”) Open the discharge valve of the adsorption tower after adsorption and discharge the gas to another adsorption tower. The end point of the discharge pressure is 72 kPa;
[0103] (3”) Close the downstream valve of the adsorption tower, open the desorption valve to perform vacuum desorption on the 13X molecular sieve adsorbing CO2, the vacuum desorption pressure is 20 kPa, and the time is 1 min; the desorbed gas is recovered as product gas 3;
[0104] (4”) The pressure of the vent gas from another adsorption tower discharged into the adsorption tower is raised to 70 kPa, and the feed gas and waste gas of the second and third stage pressure swing adsorption are used as the boost gas for the final pressure increase and are pressurized to the designed adsorption pressure.
[0105] The composition of the product gas at each stage obtained by three-stage pressure swing adsorption in this embodiment is shown in Table 2;
[0106] Table 2
[0107] <![CDATA[N2(V%)]]> <![CDATA[CO2(V%)]]> CO(V%) <![CDATA[O2(V%)]]> Product gas 1 40.1 52.6 1.2 6.1 Product gas 2 15.6 80.2 0.7 3.5 Product gas 3 0.6 99.1 0.2 0.1 Exhaust 90.5 1.0 1.4 7.1
[0108] By applying the three-stage pressure swing adsorption stepwise recovery method of CO2 provided in this embodiment, three product gases with obvious concentration gradients are obtained. The exhaust gas is mainly N2 and can be directly discharged.
[0109] Comparative Example 1
[0110] This comparative example provides a method for recovering CO2 by two-stage pressure swing adsorption stepwise. Except that a CO2 analyzer is not provided, other conditions are the same as those in Example 1.
[0111] Because there is no CO2 analyzer, the purity of CO2 is judged only by the vacuum desorption time, and it is impossible to achieve accurate recovery of multiple concentrations of CO2 product gas.
[0112] The applicant declares that the present invention illustrates the detailed structural features of the present invention through the above-mentioned embodiments, but the present invention is not limited to the above-mentioned detailed structural features, that is, it does not mean that the present invention must rely on the above-mentioned detailed structural features to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of the components selected by the present invention, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.
Claims
1. A method for recovering CO2 by multi-stage pressure swing adsorption, characterized in that: The method comprises a multi-stage pressure swing adsorption, each stage of which comprises adsorption, discharge, desorption and pressure increase in sequence; each stage of the pressure swing adsorption comprises at least two adsorption towers; the discharge comprises: opening the discharge valve of the adsorption tower after adsorption, and discharging the gas to another adsorption tower; The pressure increase includes sequential pressure increase and final pressure increase; the pressure end point of the sequential pressure increase is 20-200kPa; the pressure end point of the final pressure increase is 120-500kPa; The boosted gas for the downstream pressure increase is the downstream gas from another adsorption tower; the boosted gas for the final pressure increase is the feed gas and / or waste gas of each stage of pressure swing adsorption; During the desorption process, the CO2 purity change is detected in real time by a CO2 analyzer, and the high-concentration desorbed gas is recovered as product gas, and the low-concentration desorbed gas is used as the feed gas for the next stage of pressure swing adsorption.
2. The method according to claim 1, characterized in that The adsorption includes: passing the compressed raw gas into an adsorption tower so that CO2 is adsorbed on the adsorbent.
3. The method according to claim 1, characterized in that The desorption includes: closing the downstream valve of the adsorption tower, opening the desorption valve, vacuum desorbing the adsorbent after adsorption, detecting the purity change of CO2 in real time through a CO2 analyzer, recovering the high-concentration desorbed gas as product gas, and using the low-concentration desorbed gas as the feed gas for the lower stage pressure swing adsorption.
4. The method according to claim 1, characterized in that: The adsorption tower is filled with adsorbent.
5. The method according to claim 4, characterized in that The adsorbent includes any one of activated carbon, molecular sieve, silica gel or activated alumina or a combination of at least two of them.
6. The method according to claim 1, characterized in that The adsorption pressure is 120-500 kPa.
7. The method according to claim 6, characterized in that The adsorption pressure is 200-300 kPa.
8. The method according to claim 1, characterized in that The adsorption temperature is 10-50°C.
9. The method according to claim 8, characterized in that The adsorption temperature is 10-20°C.
10. The method according to claim 1, characterized in that The adsorption time is 1-10 min.
11. The method according to claim 1, characterized in that: The pressure endpoint of the sequential release is 60%-90% of the adsorption pressure.
12. The method according to claim 3, characterized in that The pressure of the vacuum desorption is 10-80 kPa.
13. The method according to claim 12, characterized in that The pressure of the vacuum desorption is 10-30 kPa.
14. The method according to claim 1, characterized in that The concentration of CO2 in the product gas is 30.0%-99.9%.
15. The method according to claim 14, characterized in that The concentration of CO2 in the product gas is 50.0-99.9%.
16. The method according to claim 1, characterized in that The concentration of CO2 in the low-concentration desorbed gas is 20.0%-90.0%.
Citation Information
Patent Citations
Method for multiple-unit coupled vacuum voltage transformation adsorption CO2 between segments
CN101249369A
Variable pressure absorption method for increasing absorption phase product yield
CN102935324A
Method for recovering adsorbed phase product by two stages of PSA
CN104147896A