A device for pressing a gradient density charge column and a design method thereof
By designing a gradient-density charge column suppression device in the military projectile, and utilizing the matching relationship between the punch, guide barrel and die barrel, a distribution of powder density is formed from low at the edge to high in the middle, which solves the problem of the easy generation of explosive charge under impact load. The problem of cracks is improved, the stability and impact resistance are improved, the damage power is enhanced and the production efficiency and safety are improved.
Patent Information
- Application Number
- CN202310067400.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-01-20
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2043-01-20
Smart Images

Figure CN115950313B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of blasting equipment and explosives, and in particular relates to a gradient density charge column suppression device and a design method thereof. Background Art
[0002] When a penetrating warhead is attacking a target, its internal charge is subjected to a strong impact load. Only when the charge explodes at a predetermined depth can the target be damaged to the greatest extent. Therefore, charge stability is a key factor in determining whether a penetrating warhead is effective. One of the important factors affecting the stability of a penetrating warhead is charge quality.
[0003] At present, in military projectiles, press-packed explosives are mainly obtained by axially pressing the explosive powder with upper and lower punches. The advantages of this method are good charge density and high elastic modulus. At the same time, the design of the press mold is relatively simple and can be designed based on experience. The disadvantage is that when the projectile undergoes a large deformation, the explosive column is subjected to the tensile and compressive stress of the shell, and the single modulus explosive column is difficult to buffer the high stress during use, and is prone to cracks and hot spots, and even causes the explosive column to explode prematurely, posing a safety hazard. Summary of the invention
[0004] In view of the deficiencies in the prior art, the purpose of the present invention is to provide a gradient density drug column compression device and a design method thereof to solve the problems of the prior art.
[0005] In order to solve the above technical problems, the present invention adopts the following technical solutions to achieve the above problems:
[0006] A device for pressing a drug column with a gradient density includes a punch, a guide cylinder, a mold cylinder and a base. The guide cylinder is sleeved at one end of the mold cylinder. The punch is slidably arranged in the guide cylinder and can extend into the mold cylinder. The base is sleeved at the other end of the mold cylinder. The base, the mold cylinder and the guide cylinder form a pharmaceutical cavity. Drug powder is placed in the pharmaceutical cavity.
[0007] The outer diameter of the punch is smaller than the inner diameter of the die barrel, d is the outer diameter of the punch, L is 1 / 2 of the difference between the inner diameter of the die barrel and the outer diameter of the punch, and L and d satisfy the following relationship:
[0008]
[0009] Where k is the ratio of the minimum compressive load ρ1 and the maximum tensile load ρ0 to which the explosive charge is subjected during penetration.
[0010] Preferably, the gradient density drug column pressing device further comprises:
[0011] The cushion block is arranged on the side of the die barrel away from the punch. The cushion block is composed of two semi-arc plates, and the base is arranged in the cushion block.
[0012] Preferably, the center lines of the punch, guide cylinder, die cylinder, base and cushion block are coaxially arranged.
[0013] Preferably, the guide cylinder, the mold cylinder and the outer wall of the cushion block are all provided with horizontally arranged positioning pins.
[0014] A design method for a gradient density charge pressing device, the design method comprising:
[0015] Step 1: Determine the effect of charge density on charge impact safety
[0016] The relationship between mechanical properties and density of the selected explosives was tested, and large drop hammer stress loading was performed on charges of different densities to obtain the charge stress-strain curve. Dynamic mechanical performance parameters such as elastic modulus E of the explosives were calculated based on the stress-strain curve.
[0017] Step 2: Determine the requirements for the gradient density charge design
[0018] Using LS-Dyna software and the dynamic mechanical performance parameters obtained in step 1, a simulation model of the warhead penetrating the target plate is established, and the maximum compression load and maximum tensile load on the explosive charge during the penetration process are calculated to determine the maximum theoretical design density ρ0 and the minimum theoretical design density ρ1 of the gradient density column.
[0019] Step 3: Determine the matching relationship between the mold cylinder (4) and the guide cylinder (2)
[0020] According to the position of the powder in the die barrel (4), based on the size matching relationship between the punch (1) and the die barrel (4), the powder is divided into a Q1 area and a Q2 area, the stress conditions of the powder in the Q1 area and the Q2 area are calculated, and according to the law between the density distribution of the powder and the stress conditions, the matching relationship between the die barrel (4) and the guide barrel (2) is designed, and a progressive density drug column pressing system is established;
[0021] When the punch (2) applies pressure to the powder with force F, the powder in region Q1 expands and deforms radially due to the force F. Assuming that the force in region Q2 remains balanced and unchanged, according to the Poisson's ratio of the drug column ν = 0.5, the stress generated by the powder in region Q1 due to the expansion of the powder in region Q2 is:
[0022]
[0023] Among them, S1 is the force-bearing area of the powder in the Q1 region, that is, the bottom area of the punch, ε1 is the strain of the powder in the Q1 region, E is the elastic modulus of the powder, and d is the punch diameter;
[0024] Since the Q2 area is distributed in a circular ring, the radial compressive force exerted by the mold barrel on the outside of the Q2 area should be equal to the compressive force exerted by the Q2 area on the inside. Therefore, the stress magnitude σ on the outside of the Q2 area is 2W The calculation process is as follows:
[0025] σ 2W ·S 2W =σ 2N ·S 2N
[0026]
[0027] The force area of the inner side of the powder in the Q2 region is S 2N =πdh, outer force area S 2W =π(d+2L)h, d is the punch diameter, L is 1 / 2 of the difference between the inner diameter of the die barrel and the outer diameter of the punch; h is the height of the die barrel;
[0028] The density of the drug column is linearly related to the stress on the drug powder, that is, Therefore, there is
[0029]
[0030] The ratio of the maximum theoretical design density ρ0 and the minimum theoretical design density ρ1 obtained in step 2 is k, then If k≤0.9, then k=0.9 to avoid the influence of large density difference on charge stability. The calculation results are
[0031] According to the design of the warhead shell
[0032] L+d=D
[0033]
[0034]
[0035]
[0036] Where D is the diameter of the charge determined according to the warhead shell design.
[0037] Compared with the prior art, the present invention has the following technical effects:
[0038] (I) The gradient density charge pressing device and its design method of the present invention adopt the method that the bottom diameter of the punch is smaller than the pressing diameter of the charge, reasonably controls the edge density of the charge, overcomes the problem that the existing charge edge elastic modulus is high and easy to produce cracks, effectively reduces the edge elastic modulus of the charge, can reduce the stress peak when subjected to impact stress, can adapt to the large degree of shell deformation, effectively improves the charge stability, and at the same time, the density of the middle part of the charge is relatively high, which can ensure the destructive power, and the edge density of the charge can be adjusted by adjusting the powder quality and the pressing density; at the same time, the charge processing procedures can be reduced, and the production efficiency and production safety can be greatly improved. The result of the combined effect of stress and stress duration during charge ignition is that when the charge density is low, its elastic modulus is small. When subjected to impact load, the charge is first compacted, resulting in a smaller stress peak and a longer stress rise time, thereby reducing the stress rate and reducing the risk of premature charge ignition. Therefore, the use of gradient density charge can improve the charge's ability to resist impact and enhance the charge's adaptability to shell deformation. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1 It is a schematic structural diagram of a device for pressing a gradual density medicine column according to the present invention;
[0040] Figure 2 It is an analysis diagram of the gradient density medicine column pressing device of the present invention;
[0041] Figure 3 The present invention is an impact stress curve diagram of PBX explosives at different densities.
[0042] The meaning of each number in the figure is:
[0043] 1-punch, 2-guide tube, 3-progressive density charge, 4-mold tube, 5-base, 6-spacer, 7-positioning pin.
[0044] The specific contents of the present invention are further explained in detail below in conjunction with embodiments. DETAILED DESCRIPTION
[0045] Specific embodiments of the present invention are given below. It should be noted that the present invention is not limited to the following specific embodiments, and all equivalent changes made on the basis of the technical solution of this application fall within the protection scope of the present invention.
[0046] The directional terms mentioned in this article, such as "circumferential direction", "inner diameter" and "outer diameter", are consistent with the specific directions on the paper of the drawings in the specification or the corresponding directions in the space shown in the drawings.
[0047] Example:
[0048] A device for pressing a gradient density drug column, such as Figure 1As shown, it includes a punch 1, a guide cylinder 2, a mold cylinder 4 and a base 5. The guide cylinder 2 is sleeved at one end of the mold cylinder 4. The punch 1 is slidably arranged in the guide cylinder 2 and can extend into the mold cylinder 4. The base 5 is sleeved at the other end of the mold cylinder 4. The base 5, the mold cylinder 4 and the guide cylinder 2 form a pharmaceutical space. The pharmaceutical space is filled with powder. The invention is characterized in that:
[0049] The outer diameter of the punch 1 is smaller than the inner diameter of the die barrel 4, d is the outer diameter of the punch 1, L is 1 / 2 of the difference between the inner diameter of the die barrel 4 and the outer diameter of the punch 1, and L and d satisfy the following relationship:
[0050] The gradient density charge pressing device and design method of the present embodiment adopt a method in which the bottom diameter of the punch is smaller than the charge pressing diameter, so as to reasonably control the edge density of the charge, overcome the problem that the existing charge edge elastic modulus is low and prone to cracks, effectively reduce the edge elastic modulus of the charge, reduce the stress peak when subjected to impact stress, adapt to a large degree of deformation of the shell, and effectively improve the charge stability. At the same time, the density of the middle part of the charge is relatively high, which can ensure the destructive power, and the edge density of the charge can be controlled by adjusting the powder quality and the pressing density. At the same time, the charge processing procedures can be reduced, and the production efficiency and production safety can be greatly improved.
[0051] The guide tube 2 of this embodiment is clearance-matched with the punch 1. By changing the matching relationship, the density distribution of the formed powder column is adjusted to form a gradient density powder column with low edge density and high middle density. When subjected to impact stress, the low-density powder column at the edge buffers the stress, avoiding the occurrence of cracks that may cause premature ignition or even premature explosion of the powder column.
[0052] As a preferred solution of this embodiment, the gradient density drug column pressing device further includes:
[0053] The cushion block 6 is arranged on a side of the die barrel 4 away from the punch 1 . The cushion block 6 is composed of two semi-arc plates, and the base 5 is arranged inside the cushion block 6 .
[0054] The purpose of providing the cushion block 6 is to separate the cushion block 6 from the mold barrel 4 after the drug column is pressed, so as to facilitate demoulding of the progressive density drug column 3 from the mold barrel 4.
[0055] As a preferred solution of this embodiment, the center lines of the punch 1, guide cylinder 2, mold cylinder 4, base 5 and pad 6 are coaxially arranged, which can ensure the overall stability of the device and further improve the safety of the compressed progressive density medicine column 3.
[0056] As a preferred solution of this embodiment, positioning pins 7 are provided on the outer walls of the guide cylinder 2, the mold cylinder 4 and the cushion block 6 to facilitate assembly and the use of tools such as cranes.
[0057] Embodiment 2:
[0058] A design method for the explosive column pressing device described in Example 1, the explosive type of this embodiment is PBX, such as Figure 1-3 As shown, the design method includes:
[0059] Step 1: Determine the effect of PBX charge density on charge impact safety
[0060] The relationship between mechanical properties and density of PBX explosives was tested. Large drop hammer stress loading was applied to charges with different densities to obtain the stress-strain curves of the charges, and the dynamic mechanical properties parameters such as elastic modulus E were calculated.
[0061] like Figure 3 As shown, it is the impact stress curve diagram of the PBX explosive of this embodiment at different densities;
[0062] According to the stress-strain relationship, we can calculate:
[0063] ρ1=1.70g / cm 3 When the charge elastic modulus
[0064] ρ0=1.84g / cm 3 When the charge elastic modulus
[0065] σ1 = ρ1 = 1.70 g / cm 3 The maximum stress borne by the grain column, ε1 is the grain column strain corresponding to the maximum stress.
[0066] σ2 = ρ0 = 1.84 g / cm 3 The maximum stress borne by the grain column, ε2 is the grain column strain corresponding to the maximum stress.
[0067] Step 2: Determine the requirements for the gradient density charge design
[0068] The commercial software LS-Dyna was used to establish a simulation model of the warhead penetrating the target plate using the mechanical property parameters obtained in step 1. The maximum compression load and maximum tensile load on the explosive charge during the penetration process were calculated, and the maximum theoretical design density of the gradient density column was determined to be 1.84 g / cm 3 And minimum density 1.70g / cm 3 .
[0069] Step 3: Calculation of the matching relationship between the mold cylinder (4) and the guide cylinder (2)
[0070] According to the position of the powder in the die, based on the size matching relationship between the punch and the die barrel, the pressed powder is divided into two parts, Q1 and Q2. By analyzing the relationship between the density distribution of the two regions Q1 and Q2 and the matching relationship between the die barrel and the guide barrel, we can get
[0071]
[0072] Substituting the maximum theoretical design density ρ0 and the minimum density ρ1 obtained in step 2, we can obtain The k value is within the usable range. According to the warhead shell design, the diameter of the charge column is determined to be 400mm, so it is substituted into the calculation to obtain
[0073]
[0074]
[0075] The use process of the pressing device of this embodiment:
[0076] The drug column pressing device of the embodiment is assembled from bottom to top except for the punch 1, and after assembly, graphite powder or talcum powder is applied inside the mold barrel 4 to prevent the drug column from sticking to the mold barrel when the mold is removed, causing defects on the drug column surface, and the required amount of drug is calculated and slowly poured into the mold barrel 4;
[0077] The punch 1 is placed in the guide cylinder 2 and pressed down slowly until the bottom of the punch 1 is 2-4 mm lower than the die cylinder 4 to prevent the drug column from rebounding after decompression. The drug powder directly below the punch 2 is subjected to vertical compressive stress, forming a drug column with higher density, while the drug powder close to the side wall of the die cylinder 4 is mainly squeezed laterally, forming a drug column with lower density. After the punch 2 is pressed into place, the pressure is maintained for 15 minutes and then the pressure is slowly released.
[0078] The following methods can be used to adjust the lateral density of the drug column:
[0079] After calculating the required amount of medicine and placing it into the pharmaceutical cavity, the punch 2 is pressurized to 1 to 2 mm below the die barrel and the pressure is maintained to remove the medicine column.
Claims
1. A device for pressing a drug column with a gradient density, comprising a punch (1), a guide cylinder (2), a mold cylinder (4) and a base (5), wherein the guide cylinder (2) is sleeved on one end of the mold cylinder (4), the punch (1) is slidably arranged in the guide cylinder (2) and can extend into the mold cylinder (4), the base (5) is sleeved on the other end of the mold cylinder (4), the base (5), the mold cylinder (4) and the guide cylinder (2) form a drug preparation cavity, and drug powder is placed in the drug preparation cavity, characterized in that: The outer diameter of the punch (1) is smaller than the inner diameter of the die barrel (4), d is the outer diameter of the punch (1), L is 1 / 2 of the difference between the inner diameter of the die barrel (4) and the outer diameter of the punch (1), and L and d satisfy the following relationship: Where k is the minimum compression load on the explosive charge during penetration. ρ 1 and maximum tensile load ρ 0 ratio; D It is the diameter of the charge determined according to the warhead shell design.
2. The drug column pressing device according to claim 1, characterized in that: The gradient density drug column pressing device also includes: The cushion block (6) is arranged on a side of the die barrel (4) away from the punch (1), the cushion block (6) is composed of two semi-arc plates, and the base (5) is arranged inside the cushion block (6).
3. The drug column pressing device according to claim 2, characterized in that: The center lines of the punch (1), the guide cylinder (2), the die cylinder (4), the base (5) and the cushion block (6) are coaxially arranged.
4. The drug column pressing device according to claim 3, characterized in that: Positioning pins (7) are horizontally arranged on the outer walls of the guide cylinder (2), the mold cylinder (4) and the cushion block (6).
5. The design method of the gradient density drug column pressing device according to any one of claims 1 to 4, characterized in that: The design approach includes: Step 1: Determine the effect of charge density on charge impact safety The relationship between mechanical properties and density of the selected explosives was tested, and the charges with different densities were subjected to large drop weight stress loading to obtain the charge stress-strain curve, and the elastic modulus E of the explosives was calculated based on the stress-strain curve; Step 2: Determine the requirements for the gradient density charge design Using LS-Dyna software and the dynamic mechanical performance parameters obtained in step 1, a simulation model of the warhead penetrating the target plate is established, and the maximum compression load and maximum tensile load of the explosive charge during the penetration process are calculated to determine the maximum theoretical design density of the gradient density column. ρ 0 and minimum theoretical design density ρ 1, Step 3: Determine the matching relationship between the mold cylinder (4) and the guide cylinder (2) According to the position of the powder in the die barrel (4), based on the size matching relationship between the punch (1) and the die barrel (4), the powder is divided into a Q1 area and a Q2 area, the stress conditions of the powder in the Q1 area and the Q2 area are calculated, and according to the law between the density distribution of the powder and the stress conditions, the matching relationship between the die barrel (4) and the guide barrel (2) is designed, and a progressive density drug column pressing system is established; When the punch (1) applies force F to the powder, the powder in region Q1 expands and deforms radially due to the force F. Assuming that the force in region Q2 remains balanced and unchanged, according to the Poisson's ratio of the drug column ν=0.5, the stress generated by the powder in region Q1 due to the expansion of the powder in region Q2 is: Among them, S1 is the force-bearing area of the powder in the Q1 region, that is, the bottom area of the punch. is the strain of the powder in the Q1 region, E is the elastic modulus of the powder, and d is the punch diameter; Since the Q2 area is distributed in a circular ring, the radial compressive force applied by the mold barrel on the outside of the Q2 area should be equal to the compressive force applied by the Q2 area on the inside. Therefore, the stress magnitude on the outside of the Q2 area is The calculation process is as follows: The force-bearing area of the inner side of the powder in the Q2 region , outer force area , d is the punch diameter, L is 1 / 2 of the difference between the inner diameter of the die barrel and the outer diameter of the punch; h is the height of the die barrel; The density of the drug column is linearly related to the stress on the drug powder, that is, , so there is The maximum theoretical design density obtained in step 2 ρ 0 and minimum theoretical design density ρ The ratio of 1 is k, then If k≤0.9, then k=0.9 is used to avoid the large density difference affecting the stability of the charge. ; According to the warhead shell design: in, D It is the diameter of the charge determined according to the warhead shell design.
Citation Information
Patent Citations
Missile body charge friction environment simulating device
CN103322869A
Payload for cannon and missile weapon platform
CN105115368A
Explosive molding powder pressing system
CN105272780A
Technology for pressing explosive column with preset density gradient
CN108484340A
Prefabricated density gradient explosive molding powder press mold
CN108707054A