A kind of refining and purification method of aluminum glycolate
By controlling the pH value and precipitation method in glycol-hydroxy aluminum, and using alkali-soluble acid deposition or acid-soluble alkali deposition technology for purification, the problems of unstable particle size and small bulk density of glycol-hydroxy aluminum are solved, and high purity and stable molecular weight are achieved The glycosylic aluminum enhances the performance and market competitiveness of gel paste.
Patent Information
- Application Number
- CN202211595155.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-12
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-12-12
AI Technical Summary
In the prior art, the particle size of glycol-hydroxyl aluminum is unstable, the bulk density is small, and the fluidity is poor. There are differences between domestic products and Japanese products, making it difficult to achieve domestic substitution, resulting in limited application of domestic glycol-hydroxyl aluminum in the gel paste market.
By making glycol-hydroxy aluminum into salt compounds dissolved in water, the pH value is accurately adjusted and the precipitation method is controlled, and alkali-soluble acid precipitation or acid-soluble alkali precipitation process is used for purification and purification, combining liquid phase reaction and vacuum drying to improve the product uniformity and stability.
It achieves high purity and stable molecular weight of glycol-hydroxy aluminum, improves the bulk density and activity of the product, is close to the international advanced technology level, reduces production costs, and improves the viscosity and performance of gel paste.
Smart Images

Figure CN116003458B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of compound purification, and in particular relates to a method for refining and purifying aluminum glycolate. Background Art
[0002] Gel patch (original gel paste or Babu paste) refers to a patch made by mixing the raw material drug with a suitable hydrophilic matrix and then coating it on a backing material. The gel patch consists of a backing layer, a paste layer and a protective layer, among which the paste layer is the key to the gel patch and determines the quality of the gel patch. The matrix of the paste layer can be divided into non-cross-linked and cross-linked matrices. Commonly used hydrophilic gel skeletons include synthetic, semi-synthetic and natural polymers. Commonly used cross-linking agents are mainly some high-valent metal ions, with aluminum salts being more commonly used, including aluminum glycolate, aluminum chloride, aluminum hydroxide, etc.
[0003] Most of the Chinese medicine rubber plasters in the domestic patch market are currently only available in the market with original research and no generic drugs. Aluminum glycolate is a commonly used hydrogel matrix crosslinker. Due to production technology reasons, domestic aluminum glycolate does not meet the standards for crosslinkers for gel patches. Therefore, it has not been used on a large scale in my country. It is only used as a crosslinker in Evodia rutaecarpa, compound analgesic plaster, and antihypertensive plaster. At present, Japan's gel patches are in an international leading position, and the domestic market is also rising, showing an upward trend year by year.
[0004] As an important cross-linking agent in gel patches, my country lags behind slightly in the research and application of aluminum glycolate. At present, Japan is in an international leading position in the research and application of aluminum glycolate and gel patches. The aluminum glycolate produced by Kyowa Chemical Industry Co., Ltd. has a more stable molecular weight and stronger aluminum ion activity, so the viscosity of the gel is also better, so the aluminum glycolate it produces is widely used in hydrogel patches. Therefore, in order to promote the healthy and sustainable development of the domestic gel patch market, so that the various indicators of domestic aluminum glycolate can reach or exceed those of similar international products, realize the domestic substitution of aluminum glycolate as a cross-linking agent for gel patches, and reduce costs, the key technology and industrialization research of aluminum glycolate has become the most urgent issue.
[0005] In the current prior art, the method for synthesizing aluminum hydroxide is to use a process in which sodium hydroxide is dissolved in water and then aluminum chloride is added to make an active aluminum hydroxide suspension, which is then added dropwise to a glycine aqueous solution. In this process, aluminum chloride reacts violently with water, releases heat significantly, and easily and quickly forms agglomerates to precipitate solids, resulting in unstable precipitate particle size and a large fluctuation range. In addition, the reaction is a solid-liquid reaction, and uneven contact between the two reaction substrates will also lead to unstable product crystal forms, and the final product has polycrystalline and mixed crystals.
[0006] Therefore, in actual production, our company optimized and changed the process route, dissolved aluminum isopropoxide in toluene, and then added it dropwise to the aqueous solution of glycine. The reaction time was controlled by controlling the reaction temperature. This reaction is a liquid phase reaction, which is mild and basically heat-free. The reaction substrate contact area is large, the reaction is fast, and the product purity is high, and the purity almost meets the requirements of oral tablets.
[0007] However, the currently optimized process still has the following problems:
[0008] 1. Using optimized technology, the aluminum glycolate produced by our company is similar to that produced in Japan, but with poor uniformity;
[0009] 2. The aluminum glycolate produced by the existing domestic technology has large particle size, small bulk density and poor fluidity. Although our company's products are better than the existing domestic technology, there are still some differences with Japan Kyowa's products;
[0010] 3. The molecular weight of aluminum glycolate produced by Kyowa in Japan is more stable, the aluminum ion activity is stronger, and the viscosity of the gel produced is also better. There is a certain gap between the aluminum glycolate products produced by other domestic manufacturers and our company's conventional methods;
[0011] 4. Many domestic aluminum glycolates are insoluble in water and conventional organic solvents for their own reasons. This leads to the failure to control the reaction conditions during the reaction and the impure product cannot be refined and purified.
[0012] Therefore, how to purify and refine aluminum glycolate to obtain an aluminum glycolate crosslinking agent product with a higher bulk density, a stable molecular weight and strong activity while reducing costs is a technical problem that needs to be solved urgently. Summary of the invention
[0013] The present invention aims to solve the problems in the prior art by making aluminum glycolate into a water-soluble salt compound, and then precipitating aluminum glycolate by accurately adjusting the pH value, controlling the precipitation mode and time, so as to achieve the purpose of controlling the particle size and purifying aluminum glycolate. Based on the quality evaluation of the gel patch after molding, the quality standard control technology of aluminum glycolate is studied to make the product fully meet the crosslinking agent requirements of the gel patch.
[0014] In order to achieve the above technical objectives, the technical solution adopted by the present invention is:
[0015] A method for refining and purifying aluminum glycolate, wherein the aluminum glycolate is refined and purified by an alkali dissolution and acid precipitation process or an acid dissolution and alkali precipitation process.
[0016] Preferably, aluminum glycolate is prepared by liquid phase reaction, and then the crude aluminum glycolate is refined and purified by alkali dissolution and acid precipitation process or acid dissolution and alkali precipitation process.
[0017] The method for preparing aluminum glycolate by liquid phase reaction is: dissolving aluminum isopropoxide in toluene, then dropping it into an aqueous solution of glycine, and after the reaction is completed, undergoing post-treatment processes such as centrifugal separation, water washing, drying, crushing, and mixing to obtain aluminum glycolate. The reaction principle is as follows:
[0018]
[0019] Preferably, the alkali dissolution and acid precipitation process comprises the following steps: adding 3 to 5 times the mass of water to the finished aluminum glycolate to form a suspension, adding a strong alkali solution with a mass concentration of 10% at 50 to 60°C and stirring at 100 to 200 r / min until the aluminum glycolate is completely dissolved, cooling to 20 to 30°C, adding 2 mol / L strong acid solution to pH 6.5 to 7.5 at 100 to 200 r / min stirring, continuing stirring for 1 to 2 hours, and completing crystallization, then centrifuging at 1500 to 3000 r / min, adding 3 to 5 times the volume of water of the mixed solution, washing 3 times, vacuum drying, and ball milling at 300 to 500 r / min for 30 to 60 minutes to obtain refined aluminum glycolate.
[0020] Preferably, the acid dissolution and alkali precipitation process comprises the following steps: adding 3 to 5 times the mass of water to the finished aluminum glycolate to form a suspension, adding 2 mol / L strong acid solution at 50 to 60°C and stirring at 100 to 200 r / min until the aluminum glycolate is completely dissolved, cooling to 20 to 30°C, adding a 10% strong alkali solution at a mass concentration of 10% to pH 6.5 to 7.5 at 100 to 200 r / min stirring, continuing stirring for 1 to 2 hours, and completing crystallization, then centrifuging at 1500 to 3000 r / min, adding 3 to 5 times the volume of water of the mixed solution, washing 3 times, vacuum drying, and ball milling at 300 to 500 r / min for 30 to 60 minutes to obtain refined aluminum glycolate.
[0021] More preferably, the vacuum drying method is: temperature 50-60°C, vacuum degree -0.08 to -0.09 MPa, and drying time 6 hours.
[0022] More preferably, the strong acid is one or more of hydrochloric acid, sulfuric acid, nitric acid and perchloric acid.
[0023] More preferably, the strong base is sodium hydroxide and / or potassium hydroxide.
[0024] More preferably, the ball milling adopts a planetary ball mill.
[0025] Beneficial Effects
[0026] 1. The process of the present invention is simple to operate, and the technical purpose can be achieved through a simple acid-base titration reaction process, with low cost and high efficiency;
[0027] 2. The present invention can achieve precise control of the reaction by operating under certain process conditions, and the product has high purity and good crystal uniformity;
[0028] 3. The present invention strictly controls the crystal water content of the product through vacuum drying and ball mill crushing, the molecular weight of the product is more stable, and the bulk density is significantly improved;
[0029] 4. The present invention realizes the secondary refining of aluminum glycolate without destroying the activity of aluminum glycolate; the physical and chemical indicators and product performance of the final product are close to foreign advanced technologies, and the performance is greatly improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 These are the crystal forms of aluminum glycolate of Example 1, Comparative Example 1 and Comparative Example 3. DETAILED DESCRIPTION
[0031] The technical solution of the present invention is further described below in conjunction with specific embodiments, but is not limited thereto.
[0032] Example 1
[0033] Weigh 100g of the finished aluminum glycolate and add it to a 2000ml three-necked flask, add 300ml of water and stir to make a suspension, place it in a 50℃ constant temperature water bath, and slowly add 10% NaOH solution at 100r / min stirring until the aluminum glycolate is completely dissolved at a flow rate of 5ml / min. Cool to 20-30℃, and slowly add 2mol / L hydrochloric acid solution at 100r / min stirring to pH 6.5-7.5 at a flow rate of 5ml / min. Continue stirring for 1h to crystallize, centrifuge at 3000r / min, add 3-5 times the volume of the mixed solution of pure water, wash 3 times, temperature 55±5℃, vacuum degree -0.08~-0.09Mpa, drying time 6h, ball milling in a micro planetary ball mill, speed 300r / min, ball milling time 60min, to obtain the finished product.
[0034] Example 2
[0035] Weigh 100g of the finished aluminum glycolate and add it to a 2000ml three-necked flask, add 500ml of water and stir to make a suspension, place it in a constant temperature water bath at 60°C, and slowly add 10% KOH solution at 200r / min stirring until the aluminum glycolate is completely dissolved at a flow rate of 10ml / min. Cool to 20-30°C, and slowly add 2mol / L sulfuric acid solution at 200r / min stirring to pH 6.5-7.5 at a flow rate of 10ml / min. Continue stirring for 2h to crystallize, centrifuge at 1500r / min, add 3-5 times the volume of the mixed solution of pure water, wash 3 times, temperature 55±5°C, vacuum degree -0.08~-0.09Mpa, drying time 6h, ball milling in a micro planetary ball mill at a speed of 500r / min for 30min to obtain the finished product.
[0036] Example 3
[0037] Weigh 100g of the finished aluminum glycolate and add it to a 2000ml three-necked flask, add 400ml of water and stir to make a suspension, place it in a 50℃ constant temperature water bath, and slowly add 10% NaOH solution under stirring at 150r / min until the aluminum glycolate is completely dissolved at a flow rate of 10ml / min. Cool to 20-30℃, and slowly add 2mol / L nitric acid solution to pH 6.5-7.5 under stirring at 150r / min at a flow rate of 10ml / min. Continue stirring for 2h to crystallize, centrifuge at 2000r / min, add 3-5 times the volume of the mixed solution of pure water, wash 3 times, temperature 55±5℃, vacuum degree -0.08~-0.09Mpa, drying time 6h, ball milling in a micro planetary ball mill at a speed of 300r / min and a ball milling time of 30min to obtain the finished product.
[0038] Example 4
[0039] Weigh 100g of the finished aluminum glycolate and add it to a 2000ml three-necked flask, add 300ml of water and stir to form a suspension, place it in a 50°C constant temperature water bath, and slowly add 2mol / L perchloric acid solution at a stirring rate of 100-200r / min until the aluminum glycolate is completely dissolved, with a flow rate of 5ml / min, cool to 20-30°C, and slowly add 10% NaOH solution at a stirring rate of 100r / min to pH 6.5-7.5, with a flow rate of 5ml / min. Continue stirring for 1h to crystallize, centrifuge at 2500r / min, add 3-5 times the volume of the mixed solution of pure water, wash 3 times, temperature 55±5°C, vacuum degree -0.08-0.09Mpa, drying time 6h, ball milling in a micro planetary ball mill, rotation speed 400r / min, ball milling time 50min, to obtain the finished product.
[0040] Example 5
[0041] Weigh 100g of the finished aluminum glycolate and add it to a 2000ml three-necked flask, add 300ml of water and stir to make a suspension, place it in a constant temperature water bath at 60°C, and slowly add 2mol / L hydrochloric acid solution under stirring at 100r / min until the aluminum glycolate is completely dissolved at a flow rate of 5ml / min. Cool to 20-30°C, and slowly add 10% NaOH solution under stirring at 100r / min to pH 6.5-7.5 at a flow rate of 5ml / min. Continue stirring for 1h to crystallize, centrifuge at 3000r / min, add 3-5 times the volume of the mixed solution of pure water, wash 3 times, temperature 55±5°C, vacuum degree -0.08~-0.09Mpa, drying time 6h, ball milling in a micro planetary ball mill, speed 500r / min, ball milling time 30min, to obtain the finished product.
[0042] Example 6
[0043] Weigh 100g of the finished aluminum glycolate and add it to a 2000ml three-necked flask, add 500ml of water and stir to make a suspension, place it in a 50℃ constant temperature water bath, and slowly add 2mol / L hydrochloric acid solution at 200r / min stirring until the aluminum glycolate is completely dissolved at a flow rate of 10ml / min. Cool to 20-30℃, and slowly add 10% NaOH solution at 200r / min stirring to pH 6.5-7.5 at a flow rate of 10ml / min. Continue stirring for 1h to crystallize, centrifuge at 3000r / min, add 3-5 times the volume of the mixed solution of pure water, wash 3 times, temperature 55±5℃, vacuum degree -0.08~-0.09Mpa, drying time 6h, ball milling in a micro planetary ball mill, speed 300r / min, ball milling time 40min, to obtain the finished product.
[0044] Comparative Example 1
[0045] The commercially available aluminum glycolate product, pharmaceutical grade aluminum glycolate, was purchased from Xi'an Tianzheng Pharmaceutical Excipients Co., Ltd.
[0046] Comparative Example 2
[0047] Our company sells aluminum glycolate products on the market, pharmaceutical grade aluminum glycolate, produced by Renhetang Pharmaceutical Co., Ltd.
[0048] Comparative Example 3
[0049] Aluminum glycolate produced by Kyowa Chemical Industry Co., Ltd.
[0050] Performance Testing
[0051] Detection method:
[0052] Indicators such as pH value, nitrogen content, C2H6AlNO4 content, loss on drying, etc., referenced standards: Ministry-issued standard WS1-(X-013)-92Z and ChP 2020 edition Part IV.
[0053] pH value: Take 1.0g of this product, add 25ml of water, stir evenly, the pH value of the suspension should be 6.5-7.5.
[0054] Nitrogen content: Take about 0.25g of this product, weigh accurately, and determine it according to the nitrogen determination method (General Rule 0704 Method 1). Calculated on the basis of the dry product, the nitrogen content should be 9.90-10.60%.
[0055] C2H6AlNO4 content (% on dry basis): Take about 2.5g of sample, weigh accurately, add 30ml of hydrochloric acid solution (1→2), heat slightly to dissolve, transfer to a 500ml volumetric flask, dilute to scale with water, shake well; accurately measure 20ml, add 25.0ml of disodium ethylenediaminetetraacetic acid solution (0.05mol / L) and 20ml of acetic acid-ammonium acetate buffer (pH4.5), shake well, boil for 5 minutes, cool, add 50ml of ethanol and 2ml of diphenylthiocarbazone indicator solution, titrate with zinc solution (0.05mol / L) until the solution changes from purple-green to rose-red, and correct the titration result with a blank test to obtain the result. Each 1ml of disodium ethylenediaminetetraacetic acid solution (0.05mol / L) is equivalent to 6.753mg of C2H6AlNO4.
[0056] calculate:
[0057]
[0058] Where:
[0059] V——Volume of zinc solution (0.05mol / L) consumed by the test sample, ml T——Titer, 6.753mg / ml
[0060] Vempty——the volume of blank consumed zinc solution (0.05mol / L), ml F——correction factor, i.e. F=Mactual / Mtheoretical
[0061] Mactual——actual concentration of zinc solution (0.05mol / L), mol / LN——dilution factor is 25
[0062] M——theoretical concentration of zinc solution (0.05mol / L), mol / LW——accurately weigh the test sample, g
[0063] Note: Preparation of diphenylthiocarbazone indicator solution: Take 0.1g of diphenylthiocarbazone, add 100ml of ethanol and shake to dissolve.
[0064] Loss on drying: Take a sample and dry it at 130°C to constant weight. The weight loss shall not exceed 14.5%.
[0065] Bulk density: Weigh 10 g of aluminum glycolate sample and put it into a glass measuring cylinder of known mass. Then lift it up and drop it vertically onto a rubber pad from a height of 2.5 cm. Repeat this 50 times and measure the final volume of the sample powder.
[0066] Particle size: Determine by dry method with laser particle size analyzer. Take 1.0 g of aluminum glycolate powder and spread it evenly in the sample injector of dry method laser particle size analyzer. Set the dispersion pressure to 2 bar and the injection speed to 1. Measure according to the method. Repeat 6 times and calculate the average value and RSD.
[0067] Preparation of plaster:
[0068] Accurately weigh the prescription amount of glycerol 70g, 1,2-propylene glycol 20g, azone 2g, sodium polyacrylate NP700 20g, and aluminum glycolate 0.4g, stir evenly until no particles are visible to the naked eye, as phase A; weigh the prescription amount of purified water, tartaric acid 0.4g, and potassium sorbate 0.2g, after tartaric acid and potassium sorbate are completely dissolved, add 2.5g of carbomer 981, let it stand, and after carbomer 981 is completely swollen, it is used as phase B. Add phase A to phase B, stir at low speed for 30min with a stirrer, take out a part of the paste after mixing is complete, place it at room temperature for 24h, and use it for rheological testing; the remaining paste samples are moved to the coating machine to be coated into a patch, and cut to prepare a patch sample with a certain specification, seal it with an aluminum-plastic bag, and place it at room temperature for 7d for subsequent quality evaluation.
[0069] Initial adhesion: Use the method for determining initial adhesion in the general rules of the fourth part of the Pharmacopoeia of the People's Republic of China (2020 Edition) to take out a gel patch sealed in the aluminum-plastic bag, peel off the anti-adhesive layer, and lay the patch flat at an angle of 30° and 2 cm away from the steel ball. Fix the patch with a clip, place steel balls of different specifications in the steel ball chamber and let them slide freely on the surface of the patch, and record the maximum steel ball number that the patch can stick to. The maximum ball number is 10 points, and 1 point is subtracted for each difference in ball number.
[0070] Thixotropy evaluation standard: after 7 days of placement, the patch is intact with no "cold flow" phenomenon, and the score is 10 points; after 7 days of placement, "cold flow" occurs at the edge of the patch, and the score is 6 to 9 points depending on the degree of "cold flow" at the edge; after 7 days of placement, the "cold flow" phenomenon of the patch is more serious, and the score is 0 to 5 points.
[0071] Table 1 Aluminum glycolate performance test results
[0072]
[0073] According to the requirements of the ministerial standard WS1-(X-013)-92Z and the fourth part of the ChP2020 edition, the products of Examples 1 to 6 and Comparative Examples 1 to 3 are all qualified.
[0074] Table 2 Plaster performance test results
[0075] sample Bulk density (g / ml) Particle size (μm) Initial adhesion Thixotropy Example 1 0.57 6.73 10 10 Example 2 0.56 7.05 10 10 Example 3 0.50 7.01 9 10 Example 4 0.60 6.52 10 10 Example 5 0.54 6.78 9 10 Example 6 0.50 6.86 9 10 Comparative Example 1 0.24 138.05 6 5 Comparative Example 2 0.33 22.40 8 8 Comparative Example 3 0.63 5.69 10 10
[0076] The product obtained by the present method embodiment is significantly improved in terms of particle size, bulk density, initial adhesion, thixotropy, etc. compared with domestic commercial products and the conventional process products of the company. From the crystal diagrams of the present invention embodiment and the comparative example ( Figure 1 ) It can also be seen that the aluminum glycolate purified and refined by the method of the present invention has a uniform and distinct crystal form and its comprehensive performance exceeds the international advanced level.
[0077] It should be noted that the above embodiments are only partial embodiments of the preferred methods of implementing the present invention, rather than all embodiments. Obviously, based on the above embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.
Claims
1. A method for refining and purifying aluminum glycolate, characterized in that: The finished aluminum glycolate is refined and purified by an alkali dissolution and acid precipitation process or an acid dissolution and alkali precipitation process; The alkali dissolution and acid precipitation process comprises the following steps: adding 3 to 5 times the mass of water to the finished aluminum glycolate to prepare a suspension, dripping a strong alkali solution with a mass concentration of 10% at 50 to 60° C. and stirring at 100 to 200 r / min until the aluminum glycolate is completely dissolved, cooling to 20 to 30° C. and stirring at 100 to 200 r / min, dripping a 2 mol / L strong acid solution to pH 6.5 to 7.5, continuing stirring for 1 to 2 hours, and completing crystallization; centrifuging at 1500 to 3000 r / min, adding 3 to 5 times the volume of water of the mixed solution, washing 3 times, vacuum drying, and ball milling at 300 to 500 r / min for 30 to 60 minutes to obtain refined aluminum glycolate; The acid dissolution and alkali precipitation process comprises the following steps: adding 3 to 5 times the mass of water to the finished aluminum glycolate to prepare a suspension, adding 2 mol / L of a strong acid solution at 50 to 60° C. and stirring at 100 to 200 r / min until the aluminum glycolate is completely dissolved, cooling to 20 to 30° C. and stirring at 100 to 200 r / min, adding a 10% strong alkali solution to a pH of 6.5 to 7.5, continuing stirring for 1 to 2 hours, and completing crystallization, centrifuging at 1500 to 3000 r / min, adding 3 to 5 times the volume of water of the mixed solution, washing 3 times, vacuum drying, and ball milling at 300 to 500 r / min for 30 to 60 minutes to obtain refined aluminum glycolate; The strong acid is one or more of hydrochloric acid, sulfuric acid, nitric acid and perchloric acid; The strong base is sodium hydroxide and / or potassium hydroxide.
2. The method for refining and purifying aluminum glycolate according to claim 1, characterized in that: The vacuum drying method is: temperature 50-60°C, vacuum degree -0.08~-0.09Mpa, and drying time 6h.