A method for olefin hydroformylation reaction

By using cobalt-phosphine catalyst solution in the hydroformylation reaction of olefins, the cobalt concentration and reaction conditions are controlled, the problem of decreasing cobalt concentration of the catalyst is solved, the reaction stability and alcohol selectivity are improved, and the processing cost and environmental impact are reduced.

CN116063168BActive Publication Date: 2024-12-06CHINA PETROLEUM & CHEMICAL CORP +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111273789.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-10-29
Publication Date
2024-12-06
Estimated Expiration
2041-10-29

AI Technical Summary

Technical Problem

The concentration of the catalyst cobalt in the existing olefin hydroformylation reaction has severely decreased, resulting in poor catalyst stability, low reaction efficiency and high processing costs.

Method used

Use cobalt-phosphine catalyst solution in the autoclave to control the initial cobalt concentration in the range of 110-1200PPM, carry out contact reaction between C8-C30 olefin and synthesis gas, and control the temperature at 100-145°C and the pressure at 1-12Mpa. Treat and recycle catalyst solutions to reduce cobalt loss and deposition.

Benefits of technology

Enhance the stability of the catalyst, extend the continuous operation time of the device, reduce catalyst losses and processing costs, improve alcohol selectivity, and reduce environmental protection burden.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0003329558480000091
    Figure BDA0003329558480000091
Patent Text Reader

Abstract

The present invention relates to the technical field of olefin hydroformylation, and discloses a method for olefin hydroformylation reaction, which comprises: in the presence of a cobalt-phosphine catalyst, 30 The olefin and the synthesis gas are introduced into the reactor for contact reaction. The method of the present invention can enhance the stability of the catalyst, reduce the loss of the cobalt-phosphine catalyst, reduce the deposition of the catalyst in the reaction device, extend the continuous operation time of the device, reduce the loss of the catalyst in the product separation process, and reduce the processing cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of olefin hydroformylation, and in particular to a method for olefin hydroformylation reaction. Background Art

[0002] Olefins react with carbon monoxide and hydrogen in the presence of a catalyst to undergo a hydroformylation reaction. The hydroformylation process includes contacting an olefinic unsaturated compound with carbon monoxide and hydrogen in the presence of a catalyst under reaction conditions to produce one or more aldehydes, which are hydrogenated to form alcohols. The catalyst used in the hydroformylation reaction in industrial production is generally a cobalt (Co)-based or rhodium (Rh)-based catalyst.

[0003] CN102123978A discloses a method for hydroformylating alpha-olefins to produce two or more aldehydes comprising normal aldehydes and one or more isomeric aldehydes, wherein the target molar ratio of the normal aldehyde to the one or more isomeric aldehydes is within a selectable range of 3 / 1-60 / 1. The method uses a transition metal-ligand complex catalyst comprising a symmetrical calixarene diphosphite ligand. The target N / I ratio is selected by controlling the carbon monoxide partial pressure.

[0004] CN108586219A discloses a method for preparing aldehyde by hydroformylation of olefins, which relates to the technical field of preparing aldehydes. The preparation method is as follows: step 1: C2-C4 olefins are subjected to hydroformylation reaction with carbon monoxide and hydrogen in the presence of a catalyst in a first reactor to continuously prepare aldehydes, while the temperature is 90°C and the pressure is 2.5MPa; step 2: heating is performed in a second reactor at a temperature of 70-80°C, and an inert gas is introduced into the second reactor; step 3: the first reactor is connected to the second reactor, and the aldehyde prepared in the first reactor is introduced into the second reactor; step 4: during the introduction in step 3, the aldehyde is introduced under isobaric and unequal temperature conditions, and a secondary introduction is performed after the introduction; the invention can realize rapid preparation, improve utilization, save time during preparation, and is easy to operate; it is not easy to pollute the environment during use, and has a high yield.

[0005] Compared with cobalt catalysts, Rh complexes have higher reaction activity and can react at milder temperatures and pressures. However, rhodium catalysts have poor high temperature resistance and are difficult to use for advanced olefin carbonylation. Existing rhodium catalysts have good catalytic effects on terminal olefins, but have low activity on internal olefins. The catalyst is oil-soluble and product separation is also difficult, making post-processing more complicated. Rhodium is a precious metal resource that is scarce and expensive, and its recovery and reuse costs are high.

[0006] CN1454218A discloses a method for the continuous hydroformylation of polyolefins having 30 to 700 carbon atoms and being essentially monounsaturated. The method of the invention comprises: i) preparing a cobalt carbonyl catalyst active for hydroformylation from a catalyst precursor dissolved in an aqueous phase in the absence of the polyolefin, ii) hydroformylating the polyolefin with synthesis gas in the presence of the cobalt carbonyl catalyst in a reaction zone, and iii) separating the cobalt carbonyl catalyst from the output of the reaction zone, while at least partially regenerating the catalyst precursor, and recycling the catalyst precursor to the step.

[0007] CN1370137A discloses a continuous process for the hydroformylation of olefins having 6 to 20 carbon atoms, wherein: a) an aqueous solution of a cobalt (II) salt is brought into contact with hydrogen and carbon monoxide to form a hydroformylation active cobalt catalyst, and then an aqueous phase containing the cobalt catalyst is brought into contact with olefins and optionally an organic solvent as well as hydrogen and carbon monoxide in at least one reaction zone, wherein the cobalt catalyst is extracted into the organic phase and the olefins are hydroformylated, b) the effluent from the reaction zone is treated with oxygen in the presence of an acidic aqueous solution of a cobalt (II) salt, wherein the cobalt catalyst decomposes to form cobalt (II) salts and these are stripped into the aqueous phase; and the phases are subsequently separated, c) the aqueous solution of the cobalt (II) salt is recycled to step a) in unchanged form, wherein the concentration of the aqueous solution of the cobalt (II) salt, calculated as cobalt, is 1.1 to 1.7% by weight and is continuously maintained under conditions not exceeding the solubility limit of cobalt (II) formate in water. The process can be operated stably and without failure for a long period of time.

[0008] EP2881173A4 discloses a catalyst composition and a method for hydroformylating olefins using the catalyst composition, wherein the catalyst composition uses a specific ligand of a transition metal catalyst and a ligand stabilizer in the hydroformylation process of olefins, thereby improving the stability of the catalyst to maintain the catalyst activity, reduce the amount of the ligand, and improve the selectivity for iso-aldehydes. Stability is a common problem of hydroformylation catalysts, and the activity of hydroformylation catalysts decreases significantly as the reaction time increases.

[0009] DE59704070D1 discloses a method for preparing alcohols having 7-18 carbon atoms, comprising hydroformylating the corresponding olefins with synthesis gas in the presence of an organic phase containing a cobalt catalyst at a temperature of 50-220°C and a pressure of 100-400 bar, followed by hydrogenating the aldehydes obtained thereby, wherein an aqueous solution of a cobalt salt is reacted with the synthesis gas in the presence of an organic solvent that is not miscible with water or only a small amount of water to form a cobalt catalyst, and the organic phase containing the cobalt catalyst is prepared by extracting the formed cobalt catalyst from the aqueous phase with an organic extractant that is not miscible with water or only a small amount of water. The formation of the cobalt catalyst, the extraction of the formed cobalt catalyst in the organic phase and the hydroformylation of the corresponding olefins are carried out in a one-step process. The oxo alcohol prepared by the method of the present invention is used to prepare carboxylic acid esters as plasticizers for plastics. The reaction time is generally more than 10 hours.

[0010] When using cobalt-phosphine catalyst, the catalyst concentration is generally high. At higher reaction temperatures, there is a problem of catalyst cobalt concentration decreasing. Summary of the invention

[0011] The purpose of the present invention is to overcome the problem of serious decrease in catalyst cobalt concentration in olefin hydroformylation reaction in the prior art.

[0012] In order to achieve the above object, the present invention provides a method for olefin hydroformylation reaction, which comprises:

[0013] In the presence of cobalt-phosphine catalyst solution I, C8-C 30 The olefin and the synthesis gas are contacted and reacted at a temperature not higher than 180° C., and the amount of the cobalt-phosphine catalyst solution I is such that the initial cobalt concentration in the system for the contact reaction is 110-750 PPM; or

[0014] In the presence of cobalt-phosphine catalyst solution II, C8-C 30 The olefin and the synthesis gas are contacted and reacted at a temperature of 100-145°C, preferably 120-145°C, more preferably 130-145°C, and the amount of the cobalt-phosphine catalyst solution II used is such that the initial cobalt concentration in the system for the contact reaction is 800-1200 PPM.

[0015] The method of the present invention can enhance catalyst stability, reduce cobalt-phosphine catalyst loss, reduce catalyst deposition in a reaction device, extend the continuous operation time of the device, reduce catalyst loss during product separation, and reduce processing costs.

[0016] The present invention adopts a catalyst solution with a low cobalt content, undergoes a hydroformylation reaction, separates the product, and recycles the catalyst solution. During the circulation process, the cobalt content in the catalyst solution can remain substantially unchanged or the cobalt content decreases significantly. In addition, the cobalt concentration decreases steadily during the catalyst circulation process, thereby reducing the amount of deactivated catalyst thrown out, being environmentally friendly, and being conducive to reducing olefin selectivity and significantly improving the alcohol selectivity of the entire process. DETAILED DESCRIPTION

[0017] The endpoints and any values ​​of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of each range, the endpoint values ​​of each range and the individual point values, and the individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.

[0018] As mentioned above, the present invention provides a method for olefin hydroformylation reaction, which comprises:

[0019] In the presence of cobalt-phosphine catalyst solution I, C8-C 30 The olefin and the synthesis gas are contacted and reacted at a temperature not higher than 180° C., and the amount of the cobalt-phosphine catalyst solution I is such that the initial cobalt concentration in the system for the contact reaction is 110-750 PPM; or

[0020] In the presence of cobalt-phosphine catalyst solution II, C8-C 30 The olefin and the synthesis gas are contacted and reacted at a temperature of 100-145°C, preferably 120-145°C, more preferably 130-145°C, and the amount of the cobalt-phosphine catalyst solution II used is such that the initial cobalt concentration in the system for the contact reaction is 800-1200 PPM.

[0021] Preferably, the method further comprises, before carrying out the contact reaction: introducing synthesis gas into the autoclave, so that the synthesis gas is pretreated with the cobalt-phosphine catalyst to obtain a cobalt-phosphine catalyst solution.

[0022] Preferably, C8-C 30 The olefin and the synthesis gas are contacted and reacted at a temperature of 100° C. to 150° C., more preferably 110° C. to 145° C., more preferably 120° C. to 145° C. The inventors have found that in this preferred case, the catalyst is more stable during the reaction.

[0023] Preferably, the pressure of the contact reaction is 1 MPa-12 MPa; more preferably 1 MPa-10 MPa, preferably 2 MPa-8 MPa, and more preferably 5 MPa-8 MPa.

[0024] Preferably, the contact reaction is carried out under stirring conditions, and the stirring speed is 300-600 rpm.

[0025] Preferably, the amount of the cobalt-phosphine catalyst solution I is such that the initial cobalt concentration in the system for the contact reaction is 110-700 PPM; more preferably 200-550 PPM.

[0026] Preferably, the cobalt-phosphine catalyst in solution is mixed with the C8-C 30 The mass ratio of olefin usage is (1-10):1; preferably (2-5):1, and more preferably (2-4):1.

[0027] Preferably, the solvent of the cobalt-phosphine catalyst in solution is selected from xylene, toluene, benzene, methanol, ethanol, C4-C 10 at least one of alcohols.

[0028] According to a particularly preferred embodiment, the method further comprises preparing the cobalt-phosphine catalyst by an operation comprising the following steps:

[0029] (a) mixing a cobalt-containing raw material and a phosphine ligand in the presence of a solvent to obtain a mixed solution I;

[0030] (b) in the presence of a catalyst synthesis gas, subjecting the mixed solution I to a mixed reaction to obtain a cobalt phosphine complex catalyst.

[0031] Preferably, in step (b), the conditions of the mixed reaction include: temperature of 100° C.-150° C., and time of 0.4-10 h.

[0032] Preferably, the contact reaction is carried out under stirring conditions, and the stirring speed is 300-600 rpm.

[0033] Preferably, in step (a), the cobalt-containing raw material is selected from at least one of cobalt carbonate, cobalt acetate, cobalt formate, cobalt stearate, cobalt oxide, cobalt metal, and dicobalt octacarbonyl.

[0034] Preferably, in step (a), the solvent is selected from xylene, toluene, benzene, methanol, ethanol, C4-C 10 at least one of alcohols.

[0035] Preferably, the synthesis gas and the catalyst synthesis gas are each independently a mixed gas containing CO and H2; in the mixed gas, the molar ratio of the CO and H2 is 4:1 to 1:4; preferably 3:1 to 1:3; more preferably 2:1 to 1:2.

[0036] Preferably, the pretreatment conditions include at least: a reaction temperature of 70-180°C, preferably 90-150°C, more preferably 90-110°C; a pressure of 1Mpa-12Mpa. Preferably, the pressure is 2Mpa-8Mpa. Preferably, the reaction residence time is 0.4-40h, preferably 0.4-20h, more preferably 0.4-10h.

[0037] Preferably, the contact reaction conditions at least include: a reaction residence time of 0.4-20 h, preferably 0.4-10 h, more preferably 0.4-4 h.

[0038] Preferably, the reactor is an autoclave or a tubular reactor. 30 The olefins are derived from Fischer-Tropsch synthesis products.

[0039] Preferably, the C8-C 30 Olefins are obtained by polymerization of mixed carbon tetramers.

[0040] Preferably, the mixed C4 is at least one of the C4 produced by a catalytic cracking unit in a refinery, the C4 produced by cracking to produce ethylene, and the C4 produced as a by-product of methanol to olefins.

[0041] According to a particularly preferred embodiment, the method further comprises: introducing the catalyst-containing solvent obtained by separating the product of the contact reaction into a regeneration reactor for regeneration treatment (also known as the pretreatment of the present invention), and circulating the regenerated catalyst solution back to the reactor.

[0042] The present invention has no particular limitation on the specific operations of the separation and the regeneration treatment, and known operations may be used. The present invention will not be described in detail herein, and those skilled in the art should not interpret this as a limitation on the present invention.

[0043] The present invention will be described in detail below by way of examples. In the following examples, unless otherwise specified, all the raw materials or reagents used are commercially available.

[0044] C8 olefins: commercially available, composed of 2,4,4-trimethyl-1-pentene (75.1 wt%), 2,4,4-trimethyl-2-pentene (21.2 wt%), and the rest are multi-branched olefins;

[0045] Cobalt naphthenate and triphenylphosphine are both common commercial products.

[0046] Preparation Example 1

[0047] This preparation example is used to illustrate the preparation of cobalt-phosphine catalyst. The specific preparation method is as follows:

[0048] (a) dissolving cobalt cyclopentaneate and triphenylphosphine in isononyl alcohol at 25° C. to obtain a mixed solution I, wherein the cobalt content in the mixed solution I is 0.13 wt % and the phosphine content is 0.06 wt %;

[0049] (b) The air is replaced with synthesis gas H2 / CO (volume ratio 2:1), CO and H2 gas (the volume ratio of CO and H2 is 1:2) are filled to a pressure of 2 MPa, and the mixed solution I is mixed and reacted at a stirring condition of 400 rpm. The temperature of the mixed reaction is 140° C. and the time is 9 hours to obtain a cobalt phosphine complex catalyst.

[0050] The catalysts used in the following examples of the present invention are prepared by a process similar to that of Preparation Example 1, except that the amount of the raw materials is adaptively adjusted to obtain the catalysts with the corresponding original cobalt concentrations in each example. The present invention will not be described in detail here, and those skilled in the art should not be construed as limiting the present invention.

[0051] Example 1

[0052] A cobalt-phosphine catalyst and isononanol which had been recycled 11 times for olefin hydroformylation reaction were added to an autoclave to obtain 296 g of a cobalt-phosphine catalyst in solution. Syngas (CO / H2 volume ratio of 1:2) was continuously introduced into the autoclave until the pressure reached 3 MPa. The temperature was raised to 150°C and pre-treated under stirring conditions of 600 rpm. The reaction lasted for 1 h. 30 g of C8 olefin was added. The cobalt concentration in the solution was 240 PPM at the beginning of the reaction. A contact reaction was carried out (temperature of 150°C and pressure of 8 MPa). The reaction lasted for 4 h. The solution after the reaction was S1.

[0053] Example 2

[0054] The process flow of this embodiment is the same as that of embodiment 1, except that:

[0055] The cobalt concentration at the beginning of the reaction was 340 PPM, the contact reaction time was 4 h, and the solution after the reaction was S2.

[0056] Example 3

[0057] The process flow of this embodiment is the same as that of embodiment 1, except that:

[0058] The cobalt concentration at the beginning of the reaction was 399 PPM, the contact reaction time was 4 h, and the solution after the reaction was S3.

[0059] Example 4

[0060] The process flow of this embodiment is the same as that of embodiment 1, except that:

[0061] The cobalt concentration at the beginning of the reaction was 365 PPM, the pretreatment temperature was 100° C., and the solution after the reaction was S4.

[0062] Example 5

[0063] The process flow of this embodiment is the same as that of embodiment 1, except that:

[0064] The cobalt concentration at the beginning of the reaction was 502 PPM, and the solution was S5 after the contact reaction.

[0065] Example 6

[0066] The process flow of this embodiment is the same as that of embodiment 1, except that:

[0067] A cobalt-phosphine catalyst that had been recycled seven times for olefin hydroformylation reaction was added to the autoclave to obtain 37 g of a liquid cobalt-phosphine catalyst solution. The initial cobalt concentration was 1158 PPM, and the contact reaction temperature was 132°C. The solution after the contact reaction was S7.

[0068] Comparative Example 1

[0069] A cobalt-phosphine catalyst was added to an autoclave to obtain 59.9 g of a catalyst solution. The solution was stirred at 600 rpm under a synthesis gas pressure of 8 MPa and a CO / H2 molar ratio of 1:2. The temperature was raised to 180°C. After pretreatment for 1 h, 30 g of a C8 olefin raw material was added to carry out a contact reaction. The initial cobalt concentration of the contact reaction system was 1344 PPM. The reaction was carried out at 180°C, a pressure of 8 MPa, and stirring at 600 rpm for 4 hours. After the contact reaction, the cobalt content in the solution was 1161 PPM.

[0070] Test example: Test the difference in cobalt content

[0071] The cobalt content in each reaction product in the above examples was measured, and the specific results are shown in Table 1.

[0072] The test method for cobalt content is: emission spectroscopy

[0073] Table 1

[0074]

[0075] From the results in Table 1, it can be seen that the cobalt content in the olefin hydroformylation reaction of the present invention is significantly reduced and the catalyst is more stable.

[0076] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.

Claims

1. A method for olefin hydroformylation, characterized in that: The method includes: In the presence of cobalt-phosphine catalyst solution I, C8-C 30 The olefin and the synthesis gas are contacted and reacted at a temperature of 100° C. to 150° C., and the amount of the cobalt-phosphine catalyst solution I is such that the initial cobalt concentration in the system for the contact reaction is 110-750 PPM; or In the presence of cobalt-phosphine catalyst solution II, C8-C 30 The olefin and the synthesis gas are contacted and reacted at a temperature of 130-145° C., and the amount of the cobalt-phosphine catalyst solution II is such that the initial cobalt concentration in the system for the contact reaction is 800-1200 PPM; Before the contact reaction is carried out: a catalyst synthesis gas is introduced into the autoclave so that the catalyst synthesis gas and the cobalt-phosphine catalyst are pretreated to obtain a cobalt-phosphine catalyst solution; the phosphine ligand in the cobalt-phosphine catalyst is triphenylphosphine.

2. The method according to claim 1, wherein: The pressure of the contact reaction is 1Mpa-12Mpa.

3. The method according to claim 1, wherein: The pressure of the contact reaction is 2Mpa-10Mpa.

4. The method according to any one of claims 1 to 3, wherein: The amount of the cobalt-phosphine catalyst solution I is such that the initial cobalt concentration in the system for the contact reaction is 110-700 PPM.

5. The method according to claim 4, wherein: The amount of the cobalt-phosphine catalyst solution I is such that the initial cobalt concentration in the system for the contact reaction is 200-550 PPM.

6. The method according to claim 4, wherein: The cobalt-phosphine catalyst in solution and the C8-C 30 The mass ratio of olefin usage is (1-10):

1.

7. The method according to any one of claims 1 to 3, wherein: The method also includes preparing the cobalt-phosphine catalyst by an operation comprising the following steps: (a) mixing a cobalt-containing raw material and a phosphine ligand in the presence of a solvent to obtain a mixed solution I; (b) in the presence of a catalyst synthesis gas, subjecting the mixed solution I to a mixed reaction to obtain a cobalt phosphine complex catalyst.

8. The method according to claim 7, wherein: In step (b), the conditions of the mixed reaction include: temperature of 100° C.-150° C., and time of 0.4-10 h.

9. The method according to claim 7, wherein: In step (a), the cobalt-containing raw material is selected from at least one of cobalt carbonate, cobalt acetate, cobalt formate, cobalt stearate, cobalt oxide, cobalt metal, and dicobalt octacarbonyl.

10. The method according to claim 7, wherein: In step (a), the solvent is selected from xylene, toluene, benzene, methanol, ethanol, C4-C 10 at least one of alcohols.

11. The method according to any one of claims 1 to 3, wherein: The synthesis gas and the catalyst synthesis gas are each independently a mixed gas containing CO and H2; in the mixed gas, the molar ratio of the content of CO and H2 is 4:1 to 1:

4.

12. The method according to claim 11, wherein: The synthesis gas and the catalyst synthesis gas are each independently a mixed gas containing CO and H2; in the mixed gas, the molar ratio of the content of CO and H2 is 3:1 to 1:

3.

13. The method according to claim 12, wherein: The synthesis gas and the catalyst synthesis gas are each independently a mixed gas containing CO and H2; in the mixed gas, the molar ratio of the content of CO and H2 is 2:1 to 1:

2.

14. The method according to claim 1, wherein: The pretreatment conditions at least include: a reaction temperature of 70-180° C.; and a reaction residence time of 0.4-40 h.

15. The method according to claim 14, wherein: The pretreatment conditions at least include: a reaction residence time of 0.4-20h.

16. The method according to claim 15, wherein: The pretreatment conditions at least include: a reaction residence time of 0.4-10h.

17. The method according to claim 1, wherein: The conditions of the contact reaction at least include: a reaction residence time of 0.4-20h.

18. The method according to claim 17, wherein: The conditions of the contact reaction at least include: a reaction residence time of 0.4-10h.

19. The method according to claim 18, wherein: The conditions of the contact reaction at least include: a reaction residence time of 0.4-4h.

20. The method according to any one of claims 1 to 3, wherein: The C8-C 30 The olefins are derived from Fischer-Tropsch synthesis products.

21. The method according to any one of claims 1 to 3, wherein: The C8-C 30 Olefins are obtained by polymerization of mixed carbon tetramers.