Reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells

By designing an offline chemical vapor deposition coating reaction device with large ventilation capabilities under normal temperature environment, fine temperature control of intake and exhaust gas is achieved, and the problems of poor film density and low carrier mobility in the prior art are solved. , suitable for the production of transparent electrode glass for solar cells, improving coating quality and production efficiency.

CN116121732BActive Publication Date: 2024-11-15ZHEJIANG UNIV +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202211598656.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-12-12
Publication Date
2024-11-15
Estimated Expiration
2042-12-12

AI Technical Summary

Technical Problem

The existing chemical vapor deposition coating process is carried out on the high-temperature float glass production line, resulting in poor film density, low carrier mobility, and limited gas volume of the online coating device, which cannot meet the needs of transparent conductive films of solar cells.

Method used

A glass offline chemical vapor deposition coating reaction device with a large ventilation capability that can be used in a normal temperature environment is designed to realize independent temperature control of the intake chamber and exhaust chamber, and pass through the intake preheating channel, reaction air duct and exhaust channel. The fine temperature control is used to achieve gradient temperature control using electric heating module, which is suitable for the production of high-gas volume tin dioxide films.

Benefits of technology

It improves the electrical performance and production efficiency of coating products, ensures the density of the film layer and carrier mobility, and is suitable for the production of transparent electrode glass for solar cells, avoids gas overflow and pollution, and improves the coating quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116121732B_ABST
    Figure CN116121732B_ABST
Patent Text Reader

Abstract

The present invention discloses a reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells, comprising a large-flux air intake chamber that can be independently temperature-controlled and can evenly distribute the reaction gas in the width direction of the reaction device, a reaction channel that can control the interface temperature of the reaction gas in different zones, a large-flux exhaust chamber that can independently temperature-control and can evenly distribute the reaction waste gas in the width direction of the reaction device, and an exhaust gas recovery and treatment device that can generate negative pressure to forcibly extract the reaction waste gas in the exhaust chamber. The present invention realizes independent temperature control of the air intake chamber and the exhaust chamber, as well as fine and precise temperature control of the interfaces of the air intake preheating channel, the reaction gas channel, and the exhaust channel, and can perform ultra-large-volume chemical vapor deposition, greatly improving the quality and production efficiency of chemical vapor deposition glass coating products.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of off-line coating production of flat glass, and in particular to a reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells. Background Art

[0002] Coated glass is not only a very important building energy-saving material, but also an important electrode material in the solar cell industry. Coated glass used in buildings can not only meet the lighting requirements, but also play a role in heat insulation. In summer, it can block some unnecessary solar heat from entering the room. In winter, it can also reflect the people and objects in the room, especially the mid- and far-infrared radiation emitted by the heating equipment, back to the room to play a role in keeping warm. The solar cell industry, especially thin-film solar cells, including cadmium telluride solar cells, perovskite solar cells, and amorphous silicon solar cells all require transparent electrodes, and coated glass is an indispensable material.

[0003] There are usually two manufacturing processes for transparent electrode coated glass for solar cells, chemical vapor deposition coating and magnetron sputtering deposition coating. The material deposited by magnetron sputtering coating is generally indium-doped tin oxide, namely ITO. The deposition of ITO thin film on the glass surface by magnetron sputtering has the advantages of uniform film layer and mature and controllable process. However, since metal indium is a rare precious metal, the resource is limited and the production cost is high. At the same time, due to the characteristics of the magnetron sputtering process itself, there is no chemical bond between the film layer and the glass body, the adhesion of the film layer is poor, and the film layer is easy to fall off at high temperatures. Therefore, it is not easy to use in the production of thin-film solar cells that require repeated heating. Chemical vapor deposition usually undergoes a chemical reaction under high temperature conditions to generate doped metal oxides deposited on the glass surface. There is a chemical bond between the film layer and the glass, so it has a very strong bonding force, and the film layer can withstand repeated heating and cooling without being destroyed. The commonly used film material is fluorine-doped tin oxide, namely FTO.

[0004] The current mainstream chemical vapor deposition coating method adopts online coating, that is, the coating equipment is installed in the A0 area of ​​the tin bath or annealing furnace entrance of the float glass production line, and the coating production is carried out when the glass is still at a high temperature of 500℃~700℃. The biggest advantage of this process is that it utilizes the heat energy in the glass production process. The glass does not need to be cleaned and reheated, which saves energy. However, due to the characteristics of the float glass production line itself, the plate speed of the glass online production process is relatively high, and the scale of the online coating device is limited by the production line. In order to meet the requirements of the transparent conductive film block resistance, the film formation rate must also be high, resulting in poor film density, more defects, and low carrier mobility. To solve this problem, the float glass production line must significantly reduce production and reduce the glass plate speed, which leads to a sharp increase in energy consumption and other costs of the production line.

[0005] The core equipment of chemical vapor deposition coating is the coating reaction device. The chemical reaction is carried out in the reaction device. The reaction device should have good thermal stability and uniform gas distribution and exhaust capabilities.

[0006] Chinese patent application CN112777943A introduces a reaction device for float on-line chemical vapor deposition coating. The patent specification details the main structure and temperature control method of the reaction device. The reaction device is designed based on the float on-line coating method and is used in a high temperature environment. It can produce energy-saving coated glass used in buildings and is suitable for a maximum total gas volume of no more than 50NM 3 / h, generally practical total gas volume 4NM 3 / h~18NM 3 / h, which cannot meet the total gas volume of 200NM in the production of transparent conductive films for solar cells. 3 / h or more, the electrical properties of the film layer cannot meet the requirements of thin-film solar cells. Summary of the invention

[0007] In view of the above technical problems and the shortcomings in the art, the present invention provides a reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells, which is a reaction device for off-line chemical vapor deposition coating of glass with large ventilation capacity that can be used in a room temperature environment. The present invention realizes independent temperature control of the air inlet chamber and the exhaust chamber, as well as fine and precise temperature control of the interface of the air inlet preheating channel, the reaction gas channel, and the exhaust channel, and can perform ultra-large volume chemical vapor deposition, greatly improving the quality and production efficiency of chemical vapor deposition glass coating products.

[0008] A reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells, comprising a large-flux gas inlet chamber which is connected in sequence and can independently control the temperature and can evenly distribute the reaction gas in the width direction of the reaction device, a reaction channel which can control the interface temperature of the reaction gas in different areas, a large-flux exhaust chamber which can independently control the temperature and can evenly distribute the reaction waste gas in the width direction of the reaction device, and a waste gas recovery and treatment device which can generate negative pressure to forcibly extract the reaction waste gas in the exhaust chamber;

[0009] The air intake chamber includes a stainless steel cavity for uniform air distribution and an external heating and temperature control device; multiple air intake choke steel plates for uniform air distribution are arranged in a staggered manner in the stainless steel cavity for uniform air distribution, and the spacing between the air intake choke steel plates changes in steps to form an S-shaped pressure-equalizing air intake channel with gradually increasing fluid resistance;

[0010] The reaction channel includes a steel vertical air inlet preheating channel connected to the air inlet chamber, two steel horizontal reaction air channels parallel to the glass ribbon, two steel vertical exhaust channels connected to the exhaust chamber, and a heating and temperature control device on the outside of each air channel;

[0011] The exhaust chamber includes a uniform pressure-controlled stainless steel cavity, a trapezoidal gas collecting hood, and a heating temperature control device surrounded by the uniform pressure-controlled stainless steel cavity and the outside of the trapezoidal gas collecting hood, which can control the temperature of the reaction exhaust gas in the uniform pressure-controlled stainless steel cavity and the trapezoidal gas collecting hood above the dew point; a plurality of exhaust choke steel plates for uniform exhaust are staggered and evenly arranged in the uniform pressure-controlled stainless steel cavity, forming an S-shaped airflow channel with uniform airflow resistance.

[0012] The present invention realizes full electric temperature control of the entire reaction device, and a simple structure of uniform large-flux gas distribution and large-flux exhaust in the wide direction of the glass plate, which can realize zoned and segmented precise temperature control, can effectively improve the controllability of the glass chemical vapor deposition coating process and the electrical properties of the coated products, and is suitable for the production of transparent electrodes for solar cells.

[0013] Existing chemical vapor deposition technology and coating reaction devices are only suitable for online coating of float glass production lines. The tin bath and annealing furnace A0 zone of the float glass production line are both hot environments with temperatures reaching 500℃~700℃. The environmental heat energy has a great impact on the coating reaction device. The temperature control medium in the reaction device is mainly water or heat transfer oil, and its main function is to take away the heat conducted from the environment into the reaction device. This temperature control method responds slowly to fluctuations in ambient temperature and cannot adjust the temperature of the reaction device in time. Therefore, it cannot be used for offline chemical vapor deposition coating; at the same time, the air inlet chamber and exhaust chamber of the coating reaction device of the existing online chemical vapor deposition technology are designed according to the small flow deposition method, and the general maximum flow does not exceed 50NM 3 / h, the total practical gas volume is generally 4NM 3 / h~18NM 3 / h, suitable for the production of silicon dioxide, titanium dioxide, silicon and other thin films, not suitable for total gas volume exceeding 200NM 3 / h of thin film production of tin dioxide and the like. The reaction device of the present invention is different from the known chemical vapor deposition reaction device. The air inlet chamber, reaction channel and exhaust chamber are all controlled by an electric heating module (i.e., an electric heating temperature control device). Gradient temperature control and zone temperature control can be realized in each module, and precise temperature control of the coating precursor before it reaches the glass surface for chemical reaction can be realized. It is necessary to ensure that the coating precursor has a sufficiently high temperature before reaching the glass surface for decomposition reaction, and to prevent the coating precursor from reacting in advance before reaching the glass surface for decomposition reaction to form powder that falls on the glass surface. The reaction device of the present invention has large-throughput gas distribution and exhaust capabilities, simple structure, and uniform gas distribution, and is suitable for the production of coatings such as tin dioxide.

[0014] In a preferred example, in the reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells, the air inlet chamber, reaction channel, and exhaust chamber are all made of stainless steel plate folded or machined, connected by bolts, and each heating and temperature control device is directly attached to the surface of the steel plate, and the temperature is electrically controlled by a control system. The thickness of the stainless steel plate constituting the air inlet chamber and the exhaust chamber is preferably not less than 2 mm.

[0015] In a preferred example, the reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells has a uniform gas distribution stainless steel cavity with a width of 120mm to 180mm, a height of 500mm to 800mm, and a length of 3450mm to 4550mm.

[0016] In a preferred example, the reaction device for offline chemical vapor deposition coating of transparent electrode glass for solar cells has 4-8 air inlet choke steel plates arranged in a uniformly distributed stainless steel cavity, with the net spacing between the air inlet choke steel plates varying from 4mm to 100mm. The spacing between the air inlet choke steel plates at the gas inlet end is the largest, and the spacing between the air inlet choke steel plates at the gas outlet end is the smallest.

[0017] In a preferred example, the reaction device for offline chemical vapor deposition coating of transparent electrode glass for solar cells has an entire reaction channel surrounded by a stainless steel plate with a thickness of not less than 5 mm, and a heating module (i.e., a heating temperature control device) is provided on the outside of the stainless steel plate.

[0018] In a preferred example, the reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells, the steel vertical air inlet preheating channel is surrounded by a preheating stainless steel plate with a thickness of not less than 5 mm, a heating temperature control device is arranged on the outer side of the steel plate, and the control temperature of the heating temperature control device gradually increases from top to bottom along the direction of gas travel;

[0019] The steel horizontal reaction gas channel is composed of a central stainless steel plate with a thickness of not less than 5mm and the glass to be coated. The central stainless steel plate is placed horizontally, and a heating and temperature control device is arranged above the steel plate.

[0020] The steel vertical exhaust duct is surrounded by a stainless steel plate with a thickness of not less than 5mm, and a heating temperature control device is provided on the outside of the steel plate.

[0021] In a preferred example, in the reaction device for offline chemical vapor deposition coating of transparent electrode glass for solar cells, the temperature control range of the steel vertical air inlet preheating channel is 180°C to 400°C, the width of the steel vertical air inlet preheating channel is 10mm to 30mm, more preferably 12mm to 25mm, and the height of the steel vertical air inlet preheating channel is 80mm to 300mm, more preferably 120mm to 240mm.

[0022] In a preferred example, in the reaction device for offline chemical vapor deposition coating of transparent electrode glass for solar cells, the width of the central stainless steel reaction zone in the steel horizontal reaction gas channel (along the direction of glass travel) is 120mm to 500mm, and more preferably 150mm to 450mm.

[0023] In a preferred example, in the reaction device for offline chemical vapor deposition coating of transparent electrode glass for solar cells, the temperature control range of the steel vertical exhaust duct is 200℃~350℃, more preferably 220℃~280℃, the width of the steel vertical exhaust duct is 15mm~40mm, more preferably 20mm~30mm, and the height of the steel vertical exhaust duct is consistent with the height of the steel vertical air intake preheating duct.

[0024] In a preferred example, the reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells has a uniform pressure-controlled stainless steel cavity with a width of 120 mm to 200 mm, a height of 600 mm to 1500 mm, and a length of 3450 mm to 4550 mm.

[0025] In a preferred example, in the reaction device for offline chemical vapor deposition coating of transparent electrode glass for solar cells, 4-8 exhaust choke steel plates are arranged in a uniformly pressure-controlled stainless steel cavity, and the net spacing between the exhaust choke steel plates is 10mm to 100mm, and more preferably 20mm to 80mm.

[0026] In a preferred example, in the reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells, the acute angle of the trapezoidal gas collecting hood is not less than 45°, and more preferably not less than 55°.

[0027] In a preferred example, in the reaction device for offline chemical vapor deposition coating of transparent electrode glass for solar cells, the air inlet chamber, the reaction channel and the exhaust chamber are connected by bolts, and insulation materials are provided at the connection points, and the insulation materials include aluminum silicate fiber felt.

[0028] In a preferred example, the waste gas recovery and treatment device of the off-line chemical vapor deposition coating reaction device for transparent electrode glass for solar cells is connected to the trapezoidal gas collecting hood, which can generate a negative pressure of 50 to 300 Pa, and forcibly extract the reaction waste gas in the trapezoidal gas collecting hood. Since the online coating reaction device disclosed in the prior art has a small gas volume, it is not necessary to set up a waste gas recovery and treatment device with a forced exhaust function, and only rely on the self-flow of gas for exhaust. In the present invention, since it is used for an off-line chemical vapor deposition coating reaction device for transparent electrode glass for solar cells that requires a large gas volume, it is not enough to rely on the self-flow of gas for exhaust, which can easily cause the reaction waste gas to overflow from the gap between the reaction device and the glass plate, pollute the glass plate surface and the coating environment, and reduce the coating quality.

[0029] The present invention mainly relates to a reaction device for off-line coating on flat glass by chemical vapor deposition method, in particular, coating transparent electrode glass for solar cells. By using this equipment and method, transparent electrode glass for solar cells with excellent performance can be produced.

[0030] The reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells of the present invention is used. After being preheated in a large-flux air inlet chamber and uniformly distributed in the width direction of a glass plate, the reaction gas enters an air inlet preheating channel for further preheating to a temperature before the reaction occurs. After the reaction gas flows vertically to the glass plate surface, it is divided into two parts. One part enters a front reaction channel in the opposite direction of the travel of the glass plate, and the other part enters a rear reaction channel in the direction of the travel of the glass plate. The reaction gas is further heated to a temperature above the reaction temperature by the glass plate and the central stainless steel plate in the front and rear reaction channels. After a chemical deposition reaction occurs on the glass surface, a film is formed. Reaction by-products and part of unreacted gas enter a large-flux exhaust chamber through an exhaust channel, and finally reach an exhaust gas recovery and treatment device. The exhaust gas recovery and treatment device generates a negative pressure of 50 to 300 Pa, and the exhaust gas in the trapezoidal gas collecting hood is forced to be extracted, so as to avoid a large amount of reaction exhaust gas from overflowing from the gap between the reaction device and the glass plate, avoid pollution of the glass plate surface and the coating environment, and ensure the coating quality.

[0031] Compared with the prior art, the present invention has the following beneficial effects:

[0032] The high-flux air inlet chamber, air inlet preheating channel, reaction channel, exhaust channel, and high-flux exhaust chamber in the reaction device of the present invention are all independently electrically temperature-controlled, which can achieve precise reaction gas temperature control, meet the temperature requirements of more different coating precursors, improve the utilization rate of raw materials, and can be used in a room temperature environment. When producing transparent electrode glass for solar cells, products with dense film layers and higher carrier mobility can be produced.

[0033] In order to ensure the uniformity and consistency of the film layer structure, electro-optical and optical properties in the width direction of the glass plate, the flow rate, density, temperature and pressure of the reaction gas flow are required to be uniform. The present invention designs an air distribution structure and an exhaust structure adapted to the large air volume. Specifically, a plurality of air intake choke steel plates for uniform air distribution are staggered in a stainless steel cavity for uniform air distribution, and the spacing between the air intake choke steel plates changes in steps to form an S-shaped equalizing pressure air intake channel with gradually increasing fluid resistance. A plurality of exhaust choke steel plates for uniform exhaust are staggered and evenly arranged in a stainless steel cavity for uniform pressure control to form an S-shaped airflow channel with uniform airflow resistance. The airflow is forced to be organized in the exhaust chamber through the design of the exhaust choke steel plates, and at the same time, there is a large negative pressure at the rear end to forcibly guide and extract the gas, so as to prevent the gas from overflowing from the gap between the reaction device and the glass and thereby polluting the glass plate surface and the entire coating environment. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Figure 1 It is a schematic diagram of the cross-sectional structure of a reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells in a specific implementation manner;

[0035] Figure 2 It is a schematic diagram of the cross-sectional structure of the air inlet chamber in a specific implementation manner;

[0036] Figure 3 It is a schematic diagram of the cross-sectional structure of the reaction channel in a specific implementation manner;

[0037] Figure 4 is a schematic diagram of the cross-sectional structure of the exhaust chamber in a specific implementation manner;

[0038] Figure 5 It is a side view of a trapezoidal air collecting hood in a specific implementation manner. DETAILED DESCRIPTION

[0039] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments. It should be understood that these embodiments are only used to illustrate the present invention and are not used to limit the scope of the present invention. In the present invention, unless otherwise specified, the width generally refers to the direction along the travel of the glass ribbon, and the length generally refers to the width direction of the glass plate.

[0040] like Figure 1 to Figure 5 As shown, one of the main components of the reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells is an air inlet chamber 1, which includes a uniform air distribution stainless steel cavity, which is formed by bending a 316L stainless steel plate with a thickness of not less than 2 mm, with a width of 150 mm, a height of 600 mm, and a length of 3810 mm. Six L-shaped flow-blocking steel plates 6 are arranged inside, and the spacing between the steel plates gradually decreases from the air flow inlet to the air flow outlet, and the spacing is 100 mm, 80 mm, 60 mm, 40 mm and 15 mm respectively. The gas flow resistance gradually increases, which plays a role in uniform air distribution. There are heating modules 7 and 8 outside the uniform air distribution stainless steel cavity, and the heating modules 7 and 8 can step-heat the uniform air distribution stainless steel cavity, so that the temperature of the air flow gradually increases after entering the uniform air distribution stainless steel cavity.

[0041] Connected to the air inlet chamber 1 is the gas preheating channel 15 (i.e., a steel vertical air inlet preheating channel) of the reaction channel 2. The gas preheating channel 15 is composed of stainless steel plates 14 and 16 with a thickness of not less than 5 mm. The channel is 20 mm wide, 150 mm high, and 3810 mm long. There are heating modules 13 and 17 outside the steel plates. The gas preheating channel further heats the reaction gas to the temperature before the reaction occurs.

[0042] After passing through the gas preheating channel 15, the reaction gas hits the glass plate 5 and is divided into two air flows that pass through the reaction channel 24 (i.e., the steel horizontal reaction gas channel) composed of the central stainless steel plates 21, 23 and glass. The reaction zone of the central stainless steel plate is 400 mm wide and 3810 mm long. There are heating modules 18, 19 above the central stainless steel plate.

[0043] After the reaction is completed, the gas enters the exhaust channel 20 (i.e., a steel vertical exhaust channel). The exhaust channel is composed of stainless steel plates 10 and 11 with a thickness of not less than 5 mm. The channel is 30 mm wide, 150 mm high, and 3810 mm long. There are heating modules 9 and 12 outside the steel plates. The heating modules 9 and 12 can ensure that no condensate is generated in the exhaust channel 20 after the reaction.

[0044] After coming out of the exhaust channel 20, the reaction gas enters the exhaust chamber 4. The exhaust chamber 4 includes a uniform pressure-controlled stainless steel cavity and a trapezoidal gas collecting hood. The uniform pressure-controlled stainless steel cavity is composed of a 316L stainless steel plate with a thickness of not less than 2 mm, with a width of 150 mm, a height of 1000 mm, and a length of 3810 mm. There are 4 L-shaped flow-blocking steel plates 26 in the exhaust chamber. The flow-blocking steel plates are spaced 80 mm apart and are evenly distributed. There are heating modules 25 and 27 outside the uniform pressure-controlled stainless steel cavity.

[0045] After passing through the uniform pressure-controlled stainless steel chamber, the reaction gas enters the trapezoidal gas collecting hood 3. The function of the trapezoidal gas collecting hood 3 is to uniformly collect the long strip-shaped gas into the circular or square pipe, and to minimize the uneven distribution of the exhaust negative pressure at the outlet of the exhaust chamber 4. The main body of the trapezoidal gas collecting hood 3 is composed of four 316L steel plates with a thickness of not less than 2 mm, of which the acute angle of the two trapezoidal stainless steel plates 28 is 60°.

[0046] The exhaust end of the trapezoidal gas collecting hood 3 is connected to a waste gas recovery and treatment device (not shown) which can generate a negative pressure of 50 to 300 Pa, thereby forcibly extracting the reaction waste gas in the trapezoidal gas collecting hood 3, thereby preventing a large amount of reaction waste gas from overflowing from the gap between the reaction device and the glass plate 5, avoiding contamination of the glass plate surface and the coating environment, and ensuring the coating quality.

[0047] The air inlet chamber 1, the reaction channel 2 and the exhaust chamber 4 are connected by bolts, and the connection is provided with a heat insulating material aluminum silicate fiber felt.

[0048] The above-mentioned reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells is used. The reaction device is installed on an off-line coating production line. There are glass cutting, glass cleaning and drying, and glass heating equipment in front of the reaction device, and glass annealing equipment behind the coating reactor. The glass is heated to 550℃~620℃, and the reaction device is placed at a position where the bottom surface is 8mm away from the upper surface of the glass. The temperature of the air inlet chamber is controlled to gradually increase from 180℃ at the inlet to 240℃ at the outlet. The temperature of the steel plate of the reaction air inlet channel is controlled to gradually increase from 240℃ at the inlet to 320℃ at the outlet. The temperature of the central steel plate above the reaction channel is kept at 320℃, and the temperature of the exhaust channel steel plate and the exhaust chamber is kept at 260℃.

[0049] Monobutyltin trichloride (MBTC), trifluoroacetic acid (TFA) and water (H2O) are vaporized by bubbling or thin film vaporization, nitrogen is used as carrier gas and diluent gas, and oxygen is used as oxidant. After being mixed evenly, it is transported to the gas inlet chamber, with a total gas volume of 218NM 3 / h, of which MBTC dosage is 35g / m 2 Glass, TFA dosage 0.2g / m 2 Glass.

[0050] Under this condition, the glass plate runs at a speed of 1.2 m / min, and a 400 nm thick fluorine-doped tin oxide film is deposited at a deposition rate of 10 nm / s. The film resistivity is 4.2×10 -4 Ω·cm, the carrier concentration is 4.05×10 20 cm -3 , the carrier mobility is 35.5cm 2 V -1 s -1 .

[0051] In addition, it should be understood that after reading the above description of the present invention, those skilled in the art may make various changes or modifications to the present invention, and these equivalent forms also fall within the scope defined by the claims attached to this application.

Claims

1. A reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells, characterized in that: It includes a large-flux air inlet chamber which is connected in sequence and can independently control the temperature and evenly distribute the reaction gas in the width direction of the reaction device, a reaction channel which can control the interface temperature of the reaction gas in different zones, a large-flux exhaust chamber which can independently control the temperature and evenly distribute the reaction waste gas in the width direction of the reaction device, and a waste gas recovery and treatment device which can generate negative pressure to forcibly extract the reaction waste gas in the exhaust chamber; The air intake chamber includes a stainless steel cavity for uniform air distribution and an external heating and temperature control device; multiple air intake choke steel plates for uniform air distribution are arranged in a staggered manner in the stainless steel cavity for uniform air distribution, and the spacing between the air intake choke steel plates changes in steps to form an S-shaped pressure-equalizing air intake channel with gradually increasing fluid resistance; The reaction channel includes a steel vertical air inlet preheating channel connected to the air inlet chamber, two steel horizontal reaction air channels parallel to the glass ribbon, two steel vertical exhaust channels connected to the exhaust chamber, and a heating and temperature control device on the outside of each air channel; The exhaust chamber includes a uniform pressure-controlled stainless steel cavity, a trapezoidal gas collecting hood, and a heating temperature control device surrounded by the uniform pressure-controlled stainless steel cavity and the outside of the trapezoidal gas collecting hood, which can control the temperature of the reaction exhaust gas in the uniform pressure-controlled stainless steel cavity and the trapezoidal gas collecting hood above the dew point; a plurality of exhaust choke steel plates for uniform exhaust are staggered and evenly arranged in the uniform pressure-controlled stainless steel cavity, forming an S-shaped airflow channel with uniform airflow resistance.

2. The reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells according to claim 1, characterized in that: The air inlet chamber, reaction channel and exhaust chamber are all made of stainless steel plate folding or machining, connected by bolts, and each heating and temperature control device is directly attached to the surface of the steel plate, and all use control system electrical temperature control.

3. The reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells according to claim 1, characterized in that: 4 to 8 air intake choke steel plates are arranged in the uniformly distributed stainless steel cavity. The net spacing between the air intake choke steel plates ranges from 4mm to 100mm. The spacing between the air intake choke steel plates at the gas inlet end is the largest, and the spacing between the air intake choke steel plates at the gas outlet end is the smallest.

4. The reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells according to claim 1, characterized in that: The steel vertical air inlet preheating channel is surrounded by a preheating stainless steel plate with a thickness of not less than 5 mm. A heating temperature control device is set on the outside of the steel plate. The control temperature of the heating temperature control device gradually increases from top to bottom along the direction of gas travel; The steel horizontal reaction gas channel is composed of a central stainless steel plate with a thickness of not less than 5 mm and the glass to be coated. The central stainless steel plate is placed horizontally, and a heating and temperature control device is arranged above the steel plate. The steel vertical exhaust duct is surrounded by a stainless steel plate with a thickness of not less than 5 mm, and a heating temperature control device is installed on the outside of the steel plate.

5. The reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells according to claim 1, characterized in that: The temperature control range of the steel vertical air inlet preheating channel is 180°C~400°C, the width of the steel vertical air inlet preheating channel is 10 mm~30 mm, and the height of the steel vertical air inlet preheating channel is 80 mm~300 mm.

6. The reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells according to claim 4, characterized in that: The width of the central stainless steel reaction zone in the steel horizontal reaction gas channel is 120 mm~500 mm.

7. The reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells according to claim 1, characterized in that: The temperature control range of the steel vertical exhaust duct is 200℃~350℃, the width of the steel vertical exhaust duct is 15 mm~40 mm, and the height of the steel vertical exhaust duct is consistent with the height of the steel vertical air intake preheating duct.

8. The reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells according to claim 1, characterized in that: 4-8 exhaust choke steel plates are arranged in the uniform pressure-controlled stainless steel cavity, and the net spacing between the exhaust choke steel plates is 10 mm~100 mm.

9. The reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells according to claim 1, characterized in that: The acute angle of the trapezoidal air hood shall not be less than 45°.

10. The reaction device for off-line chemical vapor deposition coating of transparent electrode glass for solar cells according to claim 1, characterized in that: The air inlet chamber, the reaction channel and the exhaust chamber are connected by bolts, and heat insulating materials are arranged at the connection points, wherein the heat insulating materials include aluminum silicate fiber felt.

Citation Information

Patent Citations

  • Reactor for preparation of coated glass via chemical vapor deposition method

    CN112777943A

  • Method for coating films with large area offline

    CN103121798A

  • Online normal-pressure chemical vapor deposition film-plating reactor through floatation process

    CN104561938A

  • Bluish grey coated glass's coating film ware structure

    CN207659524U

  • Apparatus for atomic layer deposition

    US20070228470A1