A preparation process for a drug for treating hyperphosphatemia
By improving the synthesis and preparation process of sucrose ferric hydroxide drugs, and using micro-reaction channels and fluidized bed drying technology, immediate-release capsules are prepared, which solves the problems of low phosphate binding rate and inconvenience in taking in the existing technology, and significantly improves The efficacy of the drug and the suitability of the patient for taking it.
Patent Information
- Application Number
- CN202310256281.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-16
- Publication Date
- 2024-09-20
- Estimated Expiration
- 2043-03-16
AI Technical Summary
When treating hyperphosphatemia, the existing technology has low phosphate binding rate, low activity, troublesome administration, poor taste, poor patient compliance, large side effects, complex preparation process, and poor production operability.
By improving the synthesis and preparation process of sucrose ferric hydroxide drugs, using the micro-reaction channel process of ferric chloride hexahydrate and anhydrous sodium carbonate to control the pH value, combined with fluidized bed drying and capsule filling technology, the drug activity is improved and phosphate binding efficiency to prepare immediate-release capsules.
It significantly improves the phosphate binding ability of the drug, enhances the efficacy, improves the patient's suitability for taking it, reduces iron release side effects, and improves the drug's ability to control blood phosphorus.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of drug preparation, and in particular to a preparation process of a drug for treating hyperphosphatemia. Background Art
[0002] Phosphorus is a basic substance in the human body. It participates in the formation of fat, protein, and cell membrane. It is the basic component of energy phosphate complexes. It accounts for about 1% of the human body weight. The adult human body contains about 600-900g, of which 85.7% is concentrated in bones and teeth. Hyperphosphatemia refers to the level of serum phosphorus exceeding 4.5mg / dl. Increased blood phosphorus is closely related to the progression of kidney disease, secondary hyperparathyroidism, renal osteodystrophy, and soft tissue calcification. Hyperphosphatemia is a common complication of chronic renal failure. In recent decades, there have been many improvements in the treatment of hyperphosphatemia in uremic hemodialysis patients, but the control of blood phosphorus is still an important problem that dialysis patients need to solve, because hemodialysis has extremely limited phosphorus removal, dietary restrictions can cause malnutrition and inconvenience in life, and long-term hyperphosphatemia can cause secondary hyperparathyroidism, renal osteodystrophy, vitamin D metabolism disorders, and cardiovascular and cerebrovascular diseases, which seriously reduce the quality of life of patients and are the main reason for the increase in mortality. Therefore, the control of blood phosphorus is the key to reducing cardiovascular complications, improving the quality of life of kidney disease dialysis patients, and reducing morbidity and mortality.
[0003] In order to control the blood phosphorus level in patients with renal failure, in 2013, the US FDA approved the sucrose ferric hydroxide chewable tablets developed by ViforFresenius Medical Care Renal Pharma France. The tablets are chewed while eating, and absorb and bind to phosphate from the diet in the gastrointestinal tract, thereby preventing the stomach and intestine from absorbing phosphate. The phosphate bound to the ferric hydroxide is removed with the bowel movements, thereby achieving the effect of controlling blood phosphorus. The production process of the sucrose ferric hydroxide chewable tablets is to add ferric chloride solution to sodium carbonate solution, wash the obtained hydrogel with deionized water to remove salt, then add sucrose, potato starch and pregelatinized starch to the hydrogel, stir evenly to obtain a suspension, and then spray dry to obtain a raw material powder, and then mix the raw material powder with sweeteners, lubricants, etc., and directly press the mixed powder into tablets to obtain the final product. Chinese patent document CN109223824A discloses a method for preparing a drug for treating hyperphosphatemia in patients with chronic kidney disease undergoing dialysis. The preparation process comprises reacting ferric oxide with hydrochloric acid to generate a ferric chloride solution, reacting the solution with a sodium carbonate solution, adding sucrose and starch to stir, preparing a sucrose ferric hydroxide aqueous solution, freeze-drying the solution to obtain a loose sucrose ferric hydroxide powder, and then mixing the powder with other ingredients to compress chewable tablets by a powder direct tableting method. Chinese patent document CN109331036A discloses the use of polysaccharide iron in the preparation of a drug for treating hyperphosphatemia, comprising mixing ferric chloride with syrup and then adding a sodium carbonate solution, reacting, adding a volume precipitant, centrifuging, washing, and drying to obtain a polysaccharide iron complex. Chinese patent document CN105764492A discloses a pharmaceutical composition comprising phosphate binder particles, wherein the hydroxylated sucrose iron is prepared by fluidized bed drying, spray drying, wet granulation, dry granulation, etc., but the reaction with phosphate in food fails to reach the most ideal state, and the phosphate binding ability is not strong. In summary, these existing technologies often have problems such as low phosphate binding rate, weak activity, inconvenient administration, poor taste, poor patient compliance, large side effects, complex preparation process, and poor production operability. Summary of the invention
[0004] In view of the problems existing in the prior art, the present invention provides a preparation process for a drug for treating hyperphosphatemia. By improving the synthesis and preparation process of the original drug, iron release can be reduced, drug activity can be increased, and phosphate binding efficiency can be improved, thereby greatly enhancing the efficacy of the drug, improving the suitability of the drug for patients, and reducing the side effects of iron release.
[0005] To achieve the above object, the present invention provides a preparation process of a drug for treating hyperphosphatemia, comprising the following steps:
[0006] S1. Synthesis: Weigh ferric chloride hexahydrate and anhydrous sodium carbonate respectively, add water and stir until completely dissolved to obtain ferric chloride hexahydrate solution and anhydrous sodium carbonate solution, mix, add to a reactor, continue stirring, control pH, after the reaction is completed, centrifuge the material, discard the water layer, wash the solid layer with water, then transfer the solid layer to a cup, add water and stir quickly to obtain a suspension; sieve, measure the iron content, add sucrose while stirring, stir quickly to obtain a suspension;
[0007] S2, drying: weighing pregelatinized starch and potato starch, adding them into a fluidized bed as a base material, using the suspension obtained in step S1 as a feed, and then drying the material. After drying, taking out the material and sieving it to obtain the raw material, weighing it, and measuring the iron content;
[0008] S3, mixing the API with the excipients: adding the excipients colloidal silicon dioxide and magnesium stearate to the API obtained in step S2, mixing well and sieving to obtain a mixed powder;
[0009] S4, capsule filling: select gastric juice instant soluble empty capsules of appropriate specifications, fill the empty capsules with the mixed powder obtained in step S3, fill, press and seal to obtain the drug for treating hyperphosphatemia.
[0010] Furthermore, the mass ratio of ferric chloride hexahydrate to anhydrous sodium carbonate in step S1 is (470-480):500.
[0011] Furthermore, the mixing in step S1 is performed by pumping the ferric chloride hexahydrate solution and the anhydrous sodium carbonate solution into a Y-shaped tube using a peristaltic pump, and the two solutions are mixed and reacted in the tube after passing through the Y-shaped tube.
[0012] Furthermore, the pH in step S1 is controlled by adjusting the concentration ratio of the ferric chloride hexahydrate solution to the anhydrous sodium carbonate solution to adjust the pH to between 7 and 10.
[0013] Furthermore, the solid layer in step S1 is washed with water by adding water to the solid layer, crushing it in water and then centrifuging it, and repeating it 3 times.
[0014] Furthermore, the mass ratio of iron content to sucrose in step S1 is 500:750.
[0015] Furthermore, the drying in step S2 is to set the air inlet temperature to 80-100°C, turn on the air inlet, adjust the air inlet volume so that the base material can just be blown up, start feeding at a low speed after the base material temperature reaches above 60°C, and adjust the drying parameters to allow the system to dry stably.
[0016] Furthermore, the mass ratio of the colloidal silicon dioxide and magnesium stearate added in step S3 to the iron content measured in step S2 is 12.5:25:500.
[0017] Furthermore, the order of adding auxiliary materials in step S3 is to first add the colloidal silicon dioxide auxiliary material, mix it in a three-dimensional mixer at 40 rpm for 10-20 minutes, sieve it several times to crush the particles, and then add magnesium stearate and mix it for 5-15 minutes.
[0018] Furthermore, the filling amount of the filled capsules in step S4 is controlled to contain 500 mg of iron per capsule according to the iron content of the mixed powder.
[0019] Compared with the prior art, the present invention has the following beneficial effects:
[0020] 1. The present invention sets a similar micro-reaction channel process in the merging process, prepares equal volumes of ferric chloride hexahydrate solution and anhydrous sodium carbonate solution, merges the two liquids through a Y-thin tube and then enters the reactor. Because the activity of the product is greatly affected by pH, the Y-thin tube is used to merge the two liquids and then enter the reactor to ensure the consistency of the raw material reaction microenvironment and thus keep the product consistent, thereby improving the activity of the product and improving the ability to bind phosphate.
[0021] 2. The present invention sets a different conventional fluidized bed drying operation, first puts the base starch in the fluidized bed, and then sprays the sucrose and iron suspension into it. The obtained particles are in the form of sucrose iron wrapped starch, and the particle size is large. The disintegration of starch in the center of the particle helps to increase the surface area of phosphate binding, improve the drug activity, and enhance the phosphate binding ability.
[0022] 3. The drug for treating hyperphosphatemia prepared by the present invention is a quick-release capsule. Compared with tablets, the capsule is loaded with raw material powder. The characteristics of the capsule, compared with the original chewable tablets, improve the medication compliance of patients with bad teeth. DETAILED DESCRIPTION
[0023] The experimental methods in the following examples of the present invention, where no specific conditions are specified, are usually carried out under conventional conditions or under conditions recommended by the manufacturers. The various commonly used chemical reagents used in the examples are all commercially available products.
[0024] Unless otherwise defined, all technical and scientific terms used in the present invention have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention.
[0025] The present invention is further described in the following examples, but the examples are not intended to limit the scope of protection of the present invention.
[0026] Example 1. Preparation process of the drug for treating hyperphosphatemia of the present invention
[0027] S1, synthesis: weigh 470g of ferric chloride hexahydrate into a plastic cup, add 2 liters of water, stir until completely dissolved, and obtain ferric chloride hexahydrate solution; add 500g of anhydrous sodium carbonate to another cup, add 2 liters of water, stir until completely dissolved, and obtain anhydrous sodium carbonate solution; use a peristaltic pump to pump the above two solutions into a Y-tube, and after passing through the Y-tube, the two solutions are mixed and reacted in the pipeline. The reaction solution enters a glass reactor after passing through a section of the pipeline, and continues to stir. The pH is regulated to 7 by the concentration ratio of ferric chloride hexahydrate solution and anhydrous sodium carbonate solution; stir for 30 minutes to complete the reaction, transfer the material to a centrifuge, centrifuge at 1200rpm for 20 minutes, discard the water layer, wash the solid layer with water, crush it in water and centrifuge it again, and repeat 3 times; after washing, the solid layer is transferred to a cup, 2L of water is added to quickly stir evenly, and the iron content is measured after sieving; then, according to the mass ratio of iron content to sucrose of 500:750, sucrose is added in sequence under stirring, and quickly stirred into a uniform suspension;
[0028] S2, drying: according to the iron content measured in step S1, the mass ratio of potato starch to pregelatinized starch is 500:375:375, weigh pregelatinized starch and potato starch, and add them to the fluidized bed as the base material; stir the suspension obtained in step S1 evenly, use it as feed, then set the air inlet temperature to 80-100°C, turn on the air inlet, adjust the air inlet volume so that the base material can just be blown up, turn on the low speed feed after the base material temperature reaches above 60°C, adjust the drying parameters so that the system is stable for drying, take out the material after drying, pass it through a 20-mesh sieve, obtain the raw material, weigh it, and measure the iron content;
[0029] S3, mixing the API with the excipients: weighing two excipients, colloidal silicon dioxide and magnesium stearate, in a ratio of 500:12.5:25 according to the mass ratio of the iron content measured in step S2 to colloidal silicon dioxide and magnesium stearate, then adding the colloidal silicon dioxide and mixing in a three-dimensional mixer at 40 rpm for 20 minutes, sieving and crushing the particles, then adding magnesium stearate and mixing for 15 minutes, mixing evenly and sieving to obtain a mixed powder for capsule filling;
[0030] S4, capsule filling: select gastric juice instant soluble empty capsules of appropriate specifications, add the mixed powder obtained in step S3 to fill the empty capsules, the filling amount is controlled according to the iron content of the mixed powder, and each capsule contains 500 mg of iron. Fill, press and seal to obtain the drug for treating hyperphosphatemia of this embodiment.
[0031] Example 2: Preparation process of the drug for treating hyperphosphatemia of the present invention
[0032] S1, synthesis: weigh 470g of ferric chloride hexahydrate into a plastic cup, add 2 liters of water, stir until completely dissolved, and obtain ferric chloride hexahydrate solution; add 500g of anhydrous sodium carbonate to another cup, add 2 liters of water, stir until completely dissolved, and obtain anhydrous sodium carbonate solution; use a peristaltic pump to pump the above two solutions into a Y-tube, and after passing through the Y-tube, the two solutions are mixed and reacted in the pipeline. The reaction solution enters a glass reactor after passing through a section of the pipeline, and continues to stir. The pH is regulated to 7.5 by the concentration ratio of ferric chloride hexahydrate solution and anhydrous sodium carbonate solution; stir for 30 minutes to complete the reaction, transfer the material to a centrifuge, centrifuge at 1200rpm for 20 minutes, discard the water layer, wash the solid layer with water, crush it in water and centrifuge it again, and repeat 3 times; after washing, the solid layer is transferred to a cup, 2L of water is added to quickly stir evenly, and the iron content is measured after sieving; then, according to the mass ratio of iron content to sucrose of 500:750, sucrose is added in sequence under stirring, and quickly stirred into a uniform suspension;
[0033] S2, drying: according to the iron content measured in step S1, the mass ratio of potato starch to pregelatinized starch is 500:375:375, weigh pregelatinized starch and potato starch, and add them to the fluidized bed as the base material; stir the suspension obtained in step S1 evenly, use it as feed, then set the air inlet temperature to 80-100°C, turn on the air inlet, adjust the air inlet volume so that the base material can just be blown up, turn on the low speed feed after the base material temperature reaches above 60°C, adjust the drying parameters so that the system is stable for drying, take out the material after drying, pass it through a 20-mesh sieve, obtain the raw material, weigh it, and measure the iron content;
[0034] S3, mixing the API with the excipients: weighing two excipients, colloidal silicon dioxide and magnesium stearate, in a ratio of 500:12.5:25 according to the mass ratio of the iron content measured in step S2 to colloidal silicon dioxide and magnesium stearate, then adding the colloidal silicon dioxide first, mixing in a three-dimensional mixer at 40 rpm for 10 minutes, sieving and crushing the particles, then adding magnesium stearate and mixing for 15 minutes, mixing evenly and sieving to obtain a mixed powder for capsule filling;
[0035] S4, capsule filling: select gastric juice instant soluble empty capsules of appropriate specifications, add the mixed powder obtained in step S3 to fill the empty capsules, the filling amount is controlled according to the iron content of the mixed powder, and each capsule contains 500 mg of iron. Fill, press and seal to obtain the drug for treating hyperphosphatemia of this embodiment.
[0036] Example 3: Preparation process of the drug for treating hyperphosphatemia of the present invention
[0037] S1, synthesis: weigh 470g of ferric chloride hexahydrate into a plastic cup, add 2 liters of water, stir until completely dissolved, and obtain ferric chloride hexahydrate solution; add 500g of anhydrous sodium carbonate to another cup, add 2 liters of water, stir until completely dissolved, and obtain anhydrous sodium carbonate solution; use a peristaltic pump to pump the above two solutions into a Y-tube, and after passing through the Y-tube, the two solutions are mixed and reacted in the pipeline. The reaction solution enters a glass reactor after passing through a section of the pipeline, and continues to stir. The pH is regulated to 8 by the concentration ratio of ferric chloride hexahydrate solution and anhydrous sodium carbonate solution; stir for 30 minutes to complete the reaction, transfer the material to a centrifuge, centrifuge at 1200rpm for 20 minutes, discard the water layer, wash the solid layer with water, crush it in water and centrifuge it again, and repeat 3 times; after washing, the solid layer is transferred to a cup, 2L of water is added to quickly stir evenly, and the iron content is measured after sieving; then, according to the mass ratio of iron content to sucrose of 500:750, sucrose is added in sequence under stirring, and quickly stirred into a uniform suspension;
[0038] S2, drying: according to the iron content measured in step S1, the mass ratio of potato starch to pregelatinized starch is 500:375:375, weigh pregelatinized starch and potato starch, and add them to the fluidized bed as the base material; stir the suspension obtained in step S1 evenly, use it as feed, then set the air inlet temperature to 80-100°C, turn on the air inlet, adjust the air inlet volume so that the base material can just be blown up, turn on the low speed feed after the base material temperature reaches above 60°C, adjust the drying parameters so that the system is stable for drying, take out the material after drying, pass it through a 20-mesh sieve, obtain the raw material, weigh it, and measure the iron content;
[0039] S3, mixing the API with the excipients: weighing two excipients, colloidal silicon dioxide and magnesium stearate, in a ratio of 500:12.5:25 according to the mass ratio of the iron content measured in step S2 to colloidal silicon dioxide and magnesium stearate, then adding the colloidal silicon dioxide first, mixing in a three-dimensional mixer at 40 rpm for 10 minutes, sieving and crushing the particles, then adding magnesium stearate and mixing for 15 minutes, mixing evenly and sieving to obtain a mixed powder for capsule filling;
[0040] S4, capsule filling: select gastric juice instant soluble empty capsules of appropriate specifications, add the mixed powder obtained in step S3 to fill the empty capsules, the filling amount is controlled according to the iron content of the mixed powder, and each capsule contains 500 mg of iron. Fill, press and seal to obtain the drug for treating hyperphosphatemia of this embodiment.
[0041] Comparative Example 1
[0042] Sucrose ferric hydroxide chewable tablets produced by Vifor Fresenius Medical Care Renal Pharma France.
[0043] Comparative Example 2
[0044] The difference between this comparative example and Example 1 lies in step S1, and the remaining steps and parameters are consistent with those of Example 1. Step S1 of this comparative example is: weigh 470g of ferric chloride hexahydrate into a plastic cup, add 2 liters of water, stir until completely dissolved, and obtain ferric chloride hexahydrate solution; add 500g of anhydrous sodium carbonate into another cup, add 2 liters of water, stir until completely dissolved, and obtain anhydrous sodium carbonate solution; the ferric chloride hexahydrate solution is directly dripped into the anhydrous sodium carbonate solution for reaction, and the reaction solution enters the glass reactor after passing through a section of pipeline, and continues to stir, and the pH is regulated to 7 by the concentration ratio of the ferric chloride hexahydrate solution and the anhydrous sodium carbonate solution; the reaction is completed by stirring for 30 minutes, and the material is transferred to a centrifuge, centrifuged at 1200rpm for 20 minutes, the water layer is discarded, the solid layer is washed with water, crushed in water and centrifuged again, and repeated 3 times; the solid layer after washing is transferred to a cup, 2L of water is added until it is quickly stirred evenly, and the iron content is measured after sieving; then, sucrose is added in sequence under stirring according to the mass ratio of iron content to sucrose of 500:750, and quickly stirred into a uniform suspension.
[0045] Comparative Example 3
[0046] The difference between this comparative example and Example 1 is the difference in step S2, and the other steps and parameters are consistent with Example 1. Step S2 of this comparative example is: the suspension obtained in step S1 is atomized by spray drying at a frequency of 25 Hz, and dried under the conditions of hot air temperature of 150°C, exhaust air temperature of 100°C, and cyclone pressure difference of 0.7 kPa, and the feeding speed ensures that the material does not occupy too much of the inner wall (no droplets in the glass viewing hole); after drying, the raw material powder is collected, weighed, and the iron content is measured.
[0047] Comparative Example 4
[0048] The difference between this comparative example and Example 1 is the difference in step S4, and the other steps and parameters are the same as those of Example 1. Step S4 of this comparative example is: after the tablet press is installed, the filling depth is first adjusted so that each tablet contains 500 mg of iron, and then the main tablet pressing pressure (without pre-pressing) is adjusted so that the tablet hardness is about 50-120N. After the tablet parameters are stable, the tablets are continuously pressed, and the mixed powder is pressed to obtain the drug for treating hyperphosphatemia.
[0049] Test example, drug activity test and iron release test
[0050] 1. Test samples: The drugs prepared in Examples 1-3 and Comparative Examples 1-4 were used as test samples.
[0051] 2. Test method: 500 mg of the test sample containing iron was added to the simulated gastrointestinal acidic pH 1.2 and alkaline pH 7.5 phosphorus binding medium, and the paddle method was used to fully react for 4 hours. The residual phosphorus content in the reaction solution before and after the reaction was determined by the molybdenum blue method. Phosphorus binding rate = phosphate concentration after reaction / phosphate concentration before reaction * 100%;
[0052] 3. Test results: see Table 1 below;
[0053] Table 1. Phosphorus binding rate
[0054] Phosphorus binding rate pH1.2 pH7.5 Example 1 75.7% 27.9% Example 2 74.1% 26.9% Example 3 74.8% 27.2% Comparative Example 1 58.3% 22.2% Comparative Example 2 62.9% 23.2% Comparative Example 3 63.2% 23.6% Comparative Example 4 69.6% 24.8%
[0055] As shown in Table 1, the phosphate binding rates of the drugs prepared in Examples 1-3 of the present invention under pH 1.2 are all greater than 73%, and under pH 7.5 are all greater than 26%, which are significantly higher than the original drug in Comparative Example 1, indicating that the drug of the present invention has significantly improved phosphate binding capacity and increased the blood phosphorus control ability of the drug compared with the original drug; among them, Example 1 has the best phosphate binding rate and is the best embodiment of the present invention;
[0056] In Comparative Example 2, since the mixing method of the ferric chloride hexahydrate solution and the anhydrous sodium carbonate solution was changed, the two liquids were not combined through multiple Y-shaped capillaries before entering the reactor, so the phosphate binding capacity decreased. Because the activity of the product is greatly affected by pH, the Y-shaped capillaries can ensure that the reaction microenvironment of the raw materials is consistent and thus the product remains consistent, ensuring the activity of the product, thereby improving the phosphate binding capacity;
[0057] In Comparative Example 3, the phosphate binding capacity decreased due to the change in the drying process and the use of spray drying. This is because the conventional fluidized bed drying was used, in which the starch was placed first and then the sucrose and iron suspension was sprayed in. In this way, the disintegration of the starch in the center of the particles helped to increase the surface area of the bound phosphate, thereby increasing the activity of the product and thus increasing the phosphate binding capacity.
[0058] Comparative Example 4 changes the dosage form of the drug to tablets, which do not have the characteristics of quick-release capsules that can reduce iron release and improve binding efficiency. Therefore, the phosphorus binding rate is slightly lower than that of Example 1, and the phosphate binding capacity is reduced.
[0059] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A process for preparing a drug for treating hyperphosphatemia, characterized in that: The following steps are involved: S1. Synthesis: Weigh ferric chloride hexahydrate and anhydrous sodium carbonate respectively, add water and stir until completely dissolved to obtain ferric chloride hexahydrate solution and anhydrous sodium carbonate solution, mix, add to a reactor, continue stirring, control pH, after the reaction is completed, centrifuge the material, discard the water layer, wash the solid layer with water, then transfer the solid layer to a cup, add water and stir quickly to obtain a suspension; sieve, measure the iron content, add sucrose while stirring, stir quickly to obtain a suspension; S2, drying: weighing pregelatinized starch and potato starch, adding them into a fluidized bed as a base material, using the suspension obtained in step S1 as a feed, and then drying the material. After drying, taking out the material and sieving it to obtain the raw material, weighing it, and measuring the iron content; S3, mixing the API with the excipients: adding the excipients colloidal silicon dioxide and magnesium stearate to the API obtained in step S2, mixing well and sieving to obtain a mixed powder; S4, capsule filling: select gastric juice instant soluble empty capsules of appropriate specifications, fill the empty capsules with the mixed powder obtained in step S3, fill, press and seal to obtain the drug for treating hyperphosphatemia; The mixing in step S1 is to pump the ferric chloride hexahydrate solution and the anhydrous sodium carbonate solution into the Y-shaped tube by a peristaltic pump, and the two solutions are mixed and reacted in the tube after passing through the Y-shaped tube; The drying in step S2 is to set the air inlet temperature to 80-100°C, start the air inlet, adjust the air inlet volume so that the base material can just be blown up, start the low speed feed after the base material temperature reaches above 60°C, and adjust the drying parameters so that the system can dry stably.
2. The preparation process of the drug for treating hyperphosphatemia according to claim 1, characterized in that: The mass ratio of ferric chloride hexahydrate to anhydrous sodium carbonate in step S1 is (470-480):
500.
3. The preparation process of the drug for treating hyperphosphatemia according to claim 1, characterized in that: The pH in step S1 is controlled by adjusting the concentration ratio of the ferric chloride hexahydrate solution to the anhydrous sodium carbonate solution to adjust the pH to between 7 and 10.
4. The preparation process of the drug for treating hyperphosphatemia according to claim 1, characterized in that: The solid layer washing method in step S1 is to wash the solid layer with water, crush it in water and then centrifuge it, and repeat it 3 times.
5. The preparation process of the drug for treating hyperphosphatemia according to claim 1, characterized in that: The mass ratio of the iron content to sucrose in step S1 is 500:
750.
6. The preparation process of the drug for treating hyperphosphatemia according to claim 1, characterized in that: The mass ratio of the colloidal silicon dioxide and magnesium stearate added in step S3 to the iron content measured in step S2 is 12.5:25:
500.
7. The preparation process of the drug for treating hyperphosphatemia according to claim 1, characterized in that: The order of adding auxiliary materials in step S3 is to first add the colloidal silicon dioxide auxiliary material, mix it in a three-dimensional mixer at 40 revolutions per minute for 10-20 minutes, sieve and crush the particles, and then add magnesium stearate and mix for 5-15 minutes.
8. The preparation process of the drug for treating hyperphosphatemia according to claim 1, characterized in that: The filling amount of the filled capsules in step S4 is controlled to contain 500 mg of iron per capsule according to the iron content of the mixed powder.