A device, method and application for preparing polymer drag reducing solution

By designing a device for preparing drag-reducing blocks from polymer powder in underwater vehicles, and using water flow stirring and filtration modules to increase the dissolution rate, the space and power consumption limitations of polymer solution preparation and flocculation in underwater vehicles are solved. problem, achieving efficient and pure drag reduction effect.

CN116212709BActive Publication Date: 2024-10-22NORTHWESTERN POLYTECHNICAL UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310166693.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-02-26
Publication Date
2024-10-22
Estimated Expiration
2043-02-26

AI Technical Summary

Technical Problem

The existing technology for preparing polymer drag reduction solutions in underwater vehicles has space and power consumption limitations. The dissolution time is long and impurities are introduced, resulting in poor drag reduction effect. Direct dissolution of polymer powder will cause flocculation.

Method used

Design a device that uses polymer powder to prepare drag reduction blocks, and accelerates dissolution through the stirring auxiliary module in the water flow. The filter module and plastic beads are used to increase the dissolution speed and purity, avoid the introduction of impurities, and achieve efficient preparation of polymer drag reduction blocks. solution.

Benefits of technology

It realizes the rapid preparation of polymer drag reduction solution, increases the configuration amount, avoids the introduction of impurities, improves the solubility and drag reduction effect, and the drag reduction rate can reach 27% and is maintained for 10 minutes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116212709B_ABST
    Figure CN116212709B_ABST
Patent Text Reader

Abstract

The present invention discloses a device, method and application for preparing a polymer drag reduction solution, belonging to the field of underwater drag reduction technology; the device comprises a water inlet pipe, a cylinder, a filter module, a drag reduction block, a stirring auxiliary module and a water outlet pipe; a plurality of drag reduction blocks are arranged in the cylinder, and the drag reduction solution is obtained by being dissolved by water flow; the filter module is arranged in the cylinder, and is used to filter the incoming water and the outgoing drag reduction solution; the stirring auxiliary module is arranged in the cylinder, and is used to increase the dissolution rate of the drag reduction block. The water inlet pipe is connected with the input end of the cylinder, and water flow is introduced into the cylinder; the water outlet pipe is connected with the output end of the cylinder, and the drag reduction solution in the cylinder is output. The present invention adopts the drag reduction block prepared by polymer powder as the raw material for configuring the drag reduction solution, and the stirring auxiliary module can play a stirring role under the action of water flow to accelerate the dissolution rate; the device and method can increase the configuration amount of the drag reduction solution, and at the same time avoid the introduction of other impurities, so that the residual material can be recycled and reused.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of underwater drag reduction, and in particular relates to a device, a method and an application of preparing a polymer drag reduction solution. Background Art

[0002] Among the resistances experienced by underwater vehicles, friction resistance accounts for the largest proportion. Therefore, reducing friction resistance is of great significance for increasing the speed and range of underwater vehicles. Currently, common underwater friction resistance reduction technologies include: superhydrophobic drag reduction, groove surface drag reduction, microbubble drag reduction and polymer additive drag reduction. Among them, polymer additive drag reduction only requires dissolving a small amount of high molecular polymer in the turbulent flow field to achieve a significant drag reduction effect. It has been widely used in the fields of oil pipeline transportation, heating pipelines, etc. In addition, injecting polymer solution into the working fluid in the pipeline through slit injection and wall blowing also has a drag reduction effect, and even has a better drag reduction effect than the polymer solution at the same concentration. Therefore, some scholars have proposed that spraying polymer solution on the surface of underwater vehicles can produce a drag reduction effect.

[0003] Spraying is an effective method for releasing drag-reducing mucus, and the drag-reducing effect is affected by the mucus concentration, spraying angle and rate. The mucus drag-reducing device disclosed in the prior art uses a pre-prepared polymer solution for spraying. It is necessary to consider the power consumption and space limitations of the aircraft, and it is not advisable to carry too much drag-reducing mucus. In the prior art, there is a dilution technology for polymer concentrated mucus, which uses a storage chamber, a mixing section, and a bend section. The polymer concentrated mucus is stored in the storage chamber, and the polymer dilute solution is evenly output by mixing in the mixing section and further blending in the bend section, but the bend section will cause greater local losses. The method for dissolving polymer drag-reducing powder in the prior art is that the polymer solid drag-reducing powder is composed of citric acid powder, sodium bicarbonate powder and polyethylene oxide powder. The powder is generated by the reaction of citric acid, sodium bicarbonate and water in water to form carbon dioxide bubbles, so that the polyethylene oxide powder is quickly and fully diffused in the water to form a polymer solution. This method introduces other substances into the solution, which will affect the drag reduction effect of the polymer solution. In addition, when the polymer powder is directly dissolved in water, flocculation will occur, reducing its solubility.

[0004] It is inconvenient for underwater vehicles to carry too much polymer solution due to space and power consumption issues. Carrying polymer solid particles to prepare the solution instantly can increase the carrying capacity, but the existing dissolution method takes a long time to dissolve, introduces other substances, has a complex reaction process, and causes flocculation. Therefore, a device for preparing polymer drag reduction solution is designed, which can quickly prepare polymer solution without introducing impurities and can stably maintain the drag reduction effect for a period of time. Summary of the invention

[0005] Technical issues to be solved:

[0006] In order to avoid the shortcomings of the prior art, the present invention provides a device, method and application for preparing a polymer drag reducing solution. The device for preparing a polymer drag reducing solution uses a drag reducing block prepared from a polymer powder as a raw material for configuring the drag reducing solution. The stirring auxiliary module arranged in the device can fully stir the solution under the action of water flow, thereby accelerating the solution preparation speed. The use of the device and method can increase the configuration amount of the drag reducing solution, while avoiding the introduction of other impurities, thereby achieving the recycling and reuse of the surplus material.

[0007] The technical solution of the present invention is: a device for preparing a polymer drag-reducing solution, characterized in that it comprises a water inlet pipe, a cylinder, a filter module, a drag-reducing block, a stirring auxiliary module and a water outlet pipe;

[0008] A plurality of the drag reduction blocks are arranged in the cylinder and dissolved by water flow to obtain a drag reduction solution;

[0009] The filtering module is disposed in the cylinder and is used to filter the incoming water and the outgoing drag reduction solution;

[0010] The stirring auxiliary module is arranged in the cylinder body and is used to increase the dissolution speed of the drag reducing block.

[0011] The water inlet pipe is connected to the input end of the cylinder to introduce water into the cylinder; the water outlet pipe is connected to the output end of the cylinder to output the drag reducing solution in the cylinder.

[0012] A further technical solution of the present invention is that the drag reduction block is prepared by melting polymer powder, pouring it into a square mold and cooling it, and the side length ranges from 3 to 5 mm.

[0013] A further technical solution of the present invention is: the cylinder body is composed of a cylindrical section, a contraction section, and an expansion section; the cylindrical section is a cylindrical structure with two ends open; the expansion section and the contraction section are coaxially installed at two ends of the cylindrical section as an input end and an output end respectively;

[0014] The small diameter end of the expansion section is connected to the water inlet pipe, and the large diameter end is connected to one end of the cylindrical section; the small diameter end of the contraction section is connected to the water outlet pipe, and the large diameter end is connected to the other end of the cylindrical section.

[0015] A further technical solution of the present invention is: the filtration module includes a honeycomb net, a filter fiber board, and a partition net; the expansion section is provided with a honeycomb net and a filter fiber board in sequence along the incoming flow direction; the contraction section is provided with a filter fiber board and a honeycomb net in sequence along the incoming flow direction; the partition net is provided in the middle of the cylindrical section to prevent undissolved drag reduction blocks from accumulating downstream.

[0016] A further technical solution of the present invention is: the filter fiber board is fireproof cotton; the material of the honeycomb net and the partition net is aluminum alloy.

[0017] A further technical solution of the present invention is that the stirring auxiliary module is composed of a plurality of plastic beads.

[0018] A further technical solution of the present invention is that the plastic beads have a particle size range of 2-5 mm and are arranged in layers in an alternating manner with the drag reduction blocks in the cylindrical section.

[0019] A further technical solution of the present invention is: the water inlet pipe is provided with a water inlet valve and a flow meter, the opening and closing is controlled by the water inlet valve, and the flow rate is monitored by the flow meter.

[0020] A method for preparing a polymer drag reducing solution, characterized in that the specific steps are as follows:

[0021] Step 1: Use an electronic balance to weigh a certain amount of fusible polymer powder, heat it to completely melt it, then pour the molten polymer into a square mold, and take it out after cooling and solidification to obtain a drag reduction block;

[0022] Step 2: First, fix the partition net in the middle of the cylindrical section and place it vertically, put the drag reduction block in from the upper port, spread a layer of the drag reduction block on the partition net, then pour a layer of plastic beads, then put in the filter fiber board and honeycomb net, then tighten the contraction section and connect the water outlet pipe; then, place the cylindrical section horizontally, put the drag reduction block, plastic beads, filter fiber board, honeycomb net in sequence from the water inlet end, then tighten the expansion section and connect the water inlet pipe; finally, connect the water inlet pipe to the flow meter and the water inlet valve;

[0023] Step 3: Open the water inlet valve, and water flows through the drag reduction block in the cylindrical section to dissolve it, and then the polymer drag reduction solution flows out from the outlet pipe;

[0024] Step 4: After the drag reduction solution is prepared, the drag reduction blocks are recovered; the drag reduction block recovery method is to disassemble the device, take out the undissolved drag reduction blocks, rinse them with water, and immerse them in an alcohol solution to disperse them, and then take them out and dry them before continuing to use them.

[0025] An application of a device for preparing a polymer drag-reducing solution, characterized in that the device for preparing a polymer drag-reducing solution is installed in an underwater vehicle, a water inlet hole and a spray hole are arranged on the surface of the vehicle, water flow is introduced into a water inlet pipe through the water inlet hole, and the prepared drag-reducing solution is sprayed onto the surface of the underwater vehicle through the spray hole.

[0026] Beneficial Effects

[0027] The beneficial effects of the present invention are as follows: the device for preparing a polymer drag reduction solution proposed by the present invention is composed of a water inlet valve, a flow meter, a honeycomb net, a drag reduction block, a cylindrical section, a contraction section, a water inlet pipe, an expansion section, a filter fiber board, plastic beads, a partition net, and a water outlet pipe. The flow rate is controlled by opening and closing the water inlet valve; an expansion section is set at the entrance of the cylindrical section, and a honeycomb net is placed after the expansion section to ensure uniform incoming flow. The filter fiber board is placed after the honeycomb net, which is used to increase the flow resistance of water to slow down the water flow speed and filter some impurities in the water. After filtration, the water flows through the drag reduction block in the cylindrical section, which is mixed with plastic beads to increase the dissolution rate; a partition net is set in the middle of the cylindrical section, which can effectively prevent the smaller-sized drag reduction blocks from accumulating downstream. The filter fiber board at the outlet of the cylindrical section can prevent the smaller-sized drag reduction blocks from entering the pipeline, and the honeycomb net and the contraction section can ensure that the polymer drag reduction solution sprayed from the water outlet pipe is uniform. Therefore, when the water flows through the solid mixture in the cylindrical section, a polymer drag reduction solution can be obtained.

[0028] The present invention proposes a device for preparing a polymer drag-reducing solution, which has a simple overall structure, is easy to implement and has a low production cost. Compared with a concentrated polymer drag-reducing solution, polymer powder is prepared into a drag-reducing block, which is easy to carry and store and has high purity without introducing other impurities. At the same time, the flocculation phenomenon caused by direct stirring and dissolving of the polymer powder can be avoided, thereby improving the solubility of the polymer.

[0029] The present invention adds a honeycomb mesh to the water inlet and outlet of the device to play a rectifying role and ensure the smooth flow. Adding a filter fiber board can filter impurities in the water and ensure the water quality to improve the drag reduction effect.

[0030] The present invention adds plastic beads to the drag reducing block, which has a good mixing effect, improves the dissolution speed and avoids the problem of damage caused by mechanical stirring. At the same time, it can avoid the problem of the drag reducing block particles adhering to each other after dissolution. After the solution is prepared, the remaining drag reducing block can be recycled and reused, thereby improving the utilization rate.

[0031] The polymer drag reduction solution prepared by the present invention is sprayed into the experimental pipeline. As the spraying time increases, the drag reduction rate gradually increases, reaching a maximum drag reduction rate of 27% after 5 minutes of spraying, and can maintain this drag reduction rate for 10 minutes of continuous spraying. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 The present invention is a schematic diagram of a device for preparing a polymer drag reducing solution.

[0033] Figure 2 Schematic diagram of cellular network structure.

[0034] Figure 3 Schematic diagram of the isolation net structure.

[0035] Figure 4This is the law of drag reduction rate changing with time in the test section.

[0036] Explanation of the reference numerals: 1. Water inlet valve 2. Flow meter 3. Water inlet pipe 4. Honeycomb mesh 5. Drag reduction block 6. Cylindrical section 7. Contraction section 8. Expansion section 9. Filter fiber board 10. Plastic beads 11. Partition mesh 12. Water outlet pipe. DETAILED DESCRIPTION

[0037] The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, but should not be construed as limiting the present invention.

[0038] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0039] The present embodiment provides a device for preparing a polymer drag-reducing solution, which uses drag-reducing blocks prepared from polymer powder as raw materials for preparing the drag-reducing solution. The stirring auxiliary module arranged in the device can fully stir the solution under the action of water flow, thereby accelerating the solution preparation speed. The use of this device and method can increase the preparation amount of the drag-reducing solution, while avoiding the introduction of other impurities, thereby achieving the recycling and reuse of the remaining material.

[0040] The device for preparing the polymer drag-reducing solution is installed in an underwater vehicle, a water inlet hole and a spray hole are arranged on the surface of the vehicle, water flow is introduced into the water inlet pipe through the water inlet hole, and the prepared drag-reducing solution is sprayed onto the surface of the underwater vehicle through the spray hole to produce a drag-reducing effect.

[0041] Embodiment 1:

[0042] Reference Figure 1 As shown, a device for preparing a polymer drag-reducing solution in this embodiment includes a water inlet valve 1, a flow meter 2, a water inlet pipe 3, a cylinder, a honeycomb net 4, a drag-reducing block 5, a filter fiber board 9, plastic beads 10, a spacer net 11, and a water outlet pipe 12; the water inlet pipe 3 is connected to the input end of the cylinder to introduce water into the cylinder; the water outlet pipe 12 is connected to the output end of the cylinder to output the drag-reducing solution in the cylinder.

[0043] The cylinder body includes a cylindrical section 6, a contraction section 7, and an expansion section 8. The cylindrical section 6 is a cylindrical structure with openings at both ends; the expansion section 8 and the contraction section 7 are coaxially installed at both ends of the cylindrical section 6 as input ends and output ends respectively; the small diameter end of the expansion section 8 is connected to the water inlet pipe 3, and the large diameter end is connected to one end of the cylindrical section 6; the small diameter end of the contraction section 7 is connected to the water outlet pipe 12, and the large diameter end is connected to the other end of the cylindrical section 6.

[0044] The expansion section 8 is provided with a honeycomb net 4 and a filter fiber board 9 in sequence along the incoming flow direction. Figure 2 As shown, the honeycomb net 4 is used to ensure uniform incoming flow; the filter fiber board 9 is used to increase the flow resistance of water to slow down the water flow speed, and at the same time can filter some impurities in the water. After filtration, the water flows through the drag reduction block 4 in the cylindrical section 6, in which the mixed plastic beads 10 can increase the dissolution rate. A partition net 11 is set in the middle of the cylindrical section 6, as shown in FIG. Figure 3 As shown, it can effectively prevent the smaller drag reduction blocks from accumulating downstream. The contraction section 7 is provided with a filter fiber board 9 and a honeycomb net 4 in sequence along the incoming flow direction. The filter fiber board 9 can prevent the smaller drag reduction blocks from entering the pipeline, and the honeycomb net 4 and the contraction section 7 can ensure that the polymer drag reduction solution sprayed from the outlet pipe is uniform.

[0045] Preferably, the drag reduction block is prepared by melting polymer powder, pouring it into a square mold and cooling it, and its side length ranges from 3 to 5 mm. Water flows through the drag reduction block in the device to dissolve it, and a polymer drag reduction solution can be obtained from the water outlet pipe.

[0046] Preferably, the filter fiber board 9 is fireproof cotton.

[0047] Preferably, the plastic beads 10 have a particle size of 2-5 mm and are arranged in layers in an alternating manner with the drag reduction blocks 4 in the cylindrical section.

[0048] Preferably, the expansion section 8, the contraction section 7 and the cylindrical section 6 are connected by threads.

[0049] Preferably, the expansion section 8, the cylindrical section 6 and the contraction section 7 are made of polyvinyl chloride.

[0050] Preferably, the partition net 11 is fixed to the inner wall of the cylindrical section 6 by screws.

[0051] Preferably, the honeycomb mesh 4 and the partition mesh 11 are made of aluminum alloy.

[0052] Embodiment 2:

[0053] The specific process of a method for preparing a polymer drag reducing solution in this embodiment is as follows:

[0054] Step 1: Use an electronic balance to weigh 100 g of polyethylene oxide powder, put the weighed 100 g of polyethylene oxide powder into an oven and heat it at 100°C for 3 hours to completely melt it, then pour the melted polyethylene oxide into a square mold, which has 400 closely arranged 5 mm×5 mm×5 mm cavities, and take out the drag reduction block 5 after cooling and solidifying for 10 minutes.

[0055] Step 2: Place the cylindrical end 6 vertically with the water outlet facing upward, put in the drag reduction block 5 prepared in step 1, pour in 300g of plastic beads 10 with a diameter of 3mm, then put in the filter fiberboard 9, and then put in the honeycomb mesh 4 with a pore size of 1mm, then screw in the contraction section 7 and connect the water outlet pipe 12; then place the cylindrical section 6 horizontally, and then put in the drag reduction block 5, plastic beads 10, filter fiberboard 9 and honeycomb mesh 4 with the same mass as the water outlet in turn, screw in the expansion section 8, connect the water inlet pipe 3, and connect the water inlet pipe 3 to the flow meter 2 and the water inlet valve 1.

[0056] Step 3: Open the water inlet valve 1, read the indication of the flow meter 2 to make it discharge water at a speed of 100L / h. After the water is dissolved in the drag reduction block 5 in the cylindrical section 6, the polymer drag reduction solution flows out from the outlet pipe 12.

[0057] Step 4: After the solution is prepared, the device can be disassembled, and the undissolved drag reduction block 5 can be taken out, rinsed with water, and immersed in an alcohol solution to disperse it. After being taken out and dried, it can be used again.

[0058] Reference Figure 4 As shown, the polymer drag reduction solution prepared in this embodiment is sprayed into the experimental pipeline. As the spraying time increases, the drag reduction rate gradually increases, reaching a maximum drag reduction rate of 27% after 5 minutes of spraying, and can maintain this drag reduction rate for 10 minutes of continuous spraying. After the experiment is over, the undissolved drag reduction blocks can be taken out, cleaned and dried for next use.

[0059] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations on the present invention. A person skilled in the art may change, modify, replace and modify the above embodiments within the scope of the present invention without departing from the principles and intent of the present invention.

Claims

1. A device for preparing a polymer drag reducing solution, characterized in that: It includes a water inlet pipe, a cylinder, a filter module, a drag reduction block, a stirring auxiliary module and a water outlet pipe; the drag reduction block is prepared by melting polymer powder, pouring it into a square mold and cooling it, and its side length ranges from 3 to 5 mm; the stirring auxiliary module is composed of a plurality of plastic beads, and the particle size of the plastic beads ranges from 2 to 5 mm, and is arranged in layers in a staggered manner with the drag reduction block in the cylinder section; A plurality of the drag reduction blocks are arranged in the cylinder and dissolved by water flow to obtain a drag reduction solution; The filtering module is arranged in the cylinder and is used to filter the incoming water and the outgoing drag reduction solution; The stirring auxiliary module is arranged in the cylinder body and is used to increase the dissolution speed of the drag reduction block; The water inlet pipe is connected to the input end of the cylinder to introduce water into the cylinder; the water outlet pipe is connected to the output end of the cylinder to output the drag reduction solution in the cylinder, and the maximum drag reduction rate reaches 27% after 5 minutes of spraying, and can maintain this drag reduction rate for 10 minutes of continuous spraying; The cylinder body is composed of a cylindrical section, a contraction section, and an expansion section; the cylindrical section is a cylindrical structure with two ends open; the expansion section and the contraction section are coaxially installed at the two ends of the cylindrical section as the input end and the output end respectively; the small diameter end of the expansion section is connected to the water inlet pipe, and the large diameter end is connected to one end of the cylindrical section; the small diameter end of the contraction section is connected to the water outlet pipe, and the large diameter end is connected to the other end of the cylindrical section; The filter module includes a honeycomb net, a filter fiber board, and a partition net. The expansion section is provided with a honeycomb net and a filter fiber board in sequence along the incoming flow direction; the contraction section is provided with a filter fiber board and a honeycomb net in sequence along the incoming flow direction; the partition net is provided in the middle of the cylindrical section to prevent undissolved drag reduction blocks from accumulating downstream.

2. The device for preparing a polymer drag reducing solution according to claim 1, characterized in that: The filter fiberboard is fireproof cotton; the honeycomb net and the partition net are made of aluminum alloy.

3. The device for preparing a polymer drag reducing solution according to claim 1, characterized in that: The water inlet pipe is provided with a water inlet valve and a flow meter, the opening and closing of which is controlled by the water inlet valve, and the flow rate is monitored by the flow meter.

4. A method for preparing a polymer drag reducing solution, which is implemented based on the device for preparing a polymer drag reducing solution according to any one of claims 1 to 3, characterized in that The specific steps are as follows: Step 1: Use an electronic balance to weigh a certain amount of fusible polymer powder, heat it to completely melt it, then pour the molten polymer into a square mold, and take it out after cooling and solidification to obtain a drag reduction block; Step 2: First, fix the partition net in the middle of the cylindrical section and place it vertically, put the drag reduction block in from the upper port, lay a layer of the drag reduction block on the partition net, then pour a layer of plastic beads, then put in the filter fiber board and honeycomb net, then tighten the contraction section and connect the water outlet pipe; then, place the cylindrical section horizontally, put the drag reduction block, plastic beads, filter fiber board, honeycomb net in sequence from the water inlet end, then tighten the expansion section and connect the water inlet pipe; finally, connect the water inlet pipe to the flow meter and the water inlet valve; Step 3: Open the water inlet valve, and water flows through the drag reduction block in the cylindrical section to dissolve it, and then the polymer drag reduction solution flows out from the outlet pipe; Step 4: After the drag reduction solution is prepared, the drag reduction blocks are recovered; the drag reduction block recovery method is to disassemble the device, take out the undissolved drag reduction blocks, rinse them with water, and immerse them in an alcohol solution to disperse them, and then take them out and dry them before continuing to use them.

5. Application of a device for preparing a polymer drag reducing solution, characterized in that: The device for preparing the polymer drag-reducing solution according to any one of claims 1 to 3 is installed in an underwater vehicle, a water inlet hole and a spray hole are arranged on the surface of the vehicle, water flow is introduced into the water inlet pipe through the water inlet hole, and the prepared drag-reducing solution is sprayed onto the surface of the underwater vehicle through the spray hole.