A bidirectional coupling simulation method for dynamic growth of corrosion defects in offshore equipment under external forces
Through the calculation method of mechanic-electrochemical bidirectional coupling, the problem of the dynamic evolution of corrosion damage and the unpredictable mechanical failure risks of marine engineering equipment under the action of external forces is solved, and the accurate analysis of corrosion defects and mechanical damage is achieved, providing marine engineering Equipment safety and lifespan assessment guidance.
Patent Information
- Application Number
- CN202310215749.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-08
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2043-03-08
AI Technical Summary
The prior art is difficult to effectively predict the dynamic evolution of corrosion damage and the risk of mechanical failure of marine engineering equipment under external forces, especially in complex marine environments. Traditional experimental tests are difficult to repeat and the impact of corrosion defects on mechanical distribution cannot be accurately analyzed.
Using the calculation method of mechanics-electrochemical bidirectional coupling, basic electrochemical data is obtained through electrochemical workstation testing, tensile testing machine obtains mechanical data, build a galvanic corrosion model, combines deformation geometric physics and solid mechanical physics to calculate the effect of external forces stress distribution and corrosion behavior changes under the stress concentration coefficient and mechanical damage.
It realizes accurate prediction of the growth of corrosion defects in marine engineering equipment under different time scales, evaluates corrosion sensitive location and mechanical damage, provides theoretical support for the failure risk detection and material design of marine engineering equipment, and optimizes the safety of equipment use and life.
Smart Images

Figure CN116429673B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of marine engineering equipment corrosion simulation, and relates to a bidirectional coupling simulation method for dynamic growth of corrosion defects under the action of external forces. Background Art
[0002] Corrosion is a phenomenon of deterioration and destruction that all substances in nature have to face, which has a great negative impact on industrial production and the national economy. According to the 2014 "Research on my country's Corrosion Status and Control Strategy", the total cost of corrosion in my country accounts for about 3.34% of GDP, exceeding 2.1 trillion yuan. Due to the diversity, complexity and variability of the marine environment, marine equipment such as ships, offshore platforms and other marine facilities suffer from severe corrosion, which has become an important factor restricting the development of the marine industry.
[0003] Based on the demand for lightweight and high strength ratio, in addition to traditional steel, the use of metals such as aluminum alloys, titanium alloys and copper alloys for marine engineering is gradually increasing, and the galvanic corrosion problem caused by the contact of different metals is becoming increasingly prominent. In addition, the environment in which marine engineering equipment is in service is different, and the factors affecting galvanic corrosion are also very complex, such as external loads, temperature and hydrostatic pressure. In particular, when the equipment is in service in the marine environment and is subjected to external loads, stress concentration will occur at the corrosion defects. The stress accelerates the corrosion of the material by affecting the cathode and anode reactions of galvanic corrosion. At the same time, the growth of corrosion defects will cause stress redistribution. When the stress exceeds the yield stress of the material, microcracks will be generated at the defects. The development and extension of the cracks will cause mechanical failure. The dual effects of corrosion defects and mechanical failure seriously affect the safety of use and service life of marine engineering equipment.
[0004] At present, there are many studies on material mechanics-electrochemistry. Usually, the effect of external force on corrosion is evaluated by slow stress stretching combined with electrochemical testing. This traditional experimental test not only requires precise material dimensions, but also has difficulty in setting up the test platform, making it impossible to conduct repeated experiments. In addition, it is difficult to experimentally determine the influence of corrosion defects on mechanical distribution. Therefore, by using the finite element method to couple the multi-physical fields of solid mechanics, electrochemistry, and deformation geometry, a dynamic prediction of the evolution of corrosion damage of structural parts under external forces can be achieved. Summary of the invention
[0005] The purpose of the present invention is to provide a mechanical-electrochemical bidirectional coupling calculation method, a simulation technology for accurately predicting the dynamic evolution of corrosion damage under external forces. It can predict the corrosion-sensitive position of galvanic corrosion under external forces, analyze the growth of corrosion defects at different time scales, and evaluate the stress concentration factor and mechanical damage at the corrosion defects. It provides theoretical and technical support for the failure risk detection of marine engineering equipment and optimizes the material and structural design of marine engineering equipment.
[0006] To achieve the above object, the technical solution of the present invention is as follows:
[0007] Step 1: Test the open circuit potential and polarization curve of the metal material through an electrochemical workstation to obtain the basic electrochemical data required for simulation;
[0008] Step 2: Perform a tensile test on the metal material using a tensile testing machine to obtain basic mechanical data of the material.
[0009] Step 3: Construct a galvanic corrosion model for the generation and development of corrosion defects when dissimilar metals come into contact.
[0010] The mass transfer process of electrochemical corrosion is described by using the secondary current distribution field, and the anodic dissolution process of galvanic corrosion is described by combining the deformation geometry physics field with transient calculation.
[0011] Step 4: construct the stress distribution at the coating defect under the external load. Establish a formula to realize the promotion or inhibition of stress on electrochemical corrosion, and calculate the changes in corrosion behavior at different time scales under the action of external force.
[0012] The Von Mises stress of the entire structure and its defects is calculated using the solid mechanics physical field. The influence of Von Mises stress on the cathode and anode equilibrium potential and exchange current density of the electrochemical reaction is calculated using the Gutman theory.
[0013] Step 5: Calculate the variation of mechanical damage over time in combination with the oxide film thickness. Perform simulation analysis on stress distribution based on the corrosion defect shape calculated in step 4, and evaluate the severity of stress damage in combination with the stress concentration factor.
[0014] Step 6: realize the bidirectional coupling of mechanics and electrochemistry under the action of external force and derive the calculation results, including: corrosion potential of structural parts, corrosion current density distribution, growth of corrosion defects, stress distribution and changes in mechanical damage.
[0015] Furthermore, the specific process of step 1 is as follows:
[0016] (1) Preparation of working electrode: Use laser wire cutting technology to cut the metal material into 10×10×5mm test blocks, use alcohol to clean the surface, and remove impurities such as oil. Use a welding gun to connect the back of the sample to the copper wire, and use a multimeter to test the conductivity of the welded sample. When the conductivity is good, put the sample connected to the copper wire into a rubber mold, fill it with two-component epoxy resin, and take it out after curing for 24 hours. Use 80#-200#-600#-1000#-1500# sandpaper to polish the electrode test surface in turn. After polishing, put it in acetone solution for ultrasonic cleaning for 10 minutes. After ultrasonic cleaning, use a hair dryer to blow dry, put it in a sealed bag and vacuum it for use.
[0017] (2) Open circuit potential and polarization curve test: The test was conducted using an electrochemical workstation. The test system was a three-electrode system, with the sample to be tested as the working electrode, calomel as the standard electrode, and a carbon rod as the counter electrode. The open circuit potential test time was 30 minutes, the polarization curve test range was ±250 mV based on the measured open circuit potential, and the scan rate was 0.333 mV / s.
[0018] (3) Corrosion data acquisition: The exchange current density of the cathode and anode reactions was obtained by the Tafel fitting method, and the equilibrium potential of the cathode and anode reactions was calculated using the Nernst equation.
[0019] Furthermore, an interpolation function is established in the simulation software, and the stretching data is imported.
[0020] Furthermore, the specific process of step 3 is as follows:
[0021] (1) In the parameter setting of the secondary current distribution electrode surface, the electrochemical parameters are input to simulate the galvanic corrosion kinetics process.
[0022] The dynamic changes of the galvanic corrosion interface are calculated using a deformed geometry field that obeys the arbitrary Lagrange-Euler equations to track the galvanic corrosion anode dissolution process.
[0023] (2) The simulated galvanic corrosion kinetics process is verified by the galvanic current density tested by a zero-resistance ammeter.
[0024] Furthermore, the specific process of step 4 is as follows:
[0025] (1) Establish a geometric model based on the actual forces acting on the structural parts;
[0026] (2) After the metal wire elastic material enters the plastic stage, as the strain increases, its anti-deformation ability increases as the hardening function process is:
[0027] σ hard =σ exp (ε eff )-σ s0
[0028] where σ exp is the fitting function of the measured stress and strain curve, ε eff is the total effective strain, σ s0 is the initial yield strength.
[0029] (3) Construct a variable formula based on the hardening function formula, and determine the boundary loads and fixed constraints on the structural parts when calling the plastic subnode.
[0030] (4) Combined with the anode dissolution deformation formula, the transient physical field is used to calculate the changes in the influence of mechanics on the corrosion field on the time scale.
[0031] Furthermore, the specific process of step 5 is as follows:
[0032] (1) Based on the geometric model established in step 3 and combined with the diffusion law of the cathode reaction, the thickness of the anodic oxide layer at different time scales was obtained by numerical calculation.
[0033] (2) Based on the relationship between the thickness of the oxide layer and the average area strain, damage modeling of linear elastic materials is carried out to intuitively predict the influence of corrosion on the occurrence and development of structural cracks.
[0034] (3) Using the theoretical stress concentration factor K t Indicates the severity of stress concentration and realizes the change in the impact of corrosion on the mechanical field.
[0035] Compared with the prior art, the present invention has the following beneficial effects:
[0036] Previous simulation technologies only considered the destructive effects of corrosion. However, in the actual marine service of marine engineering equipment, due to the complex and changeable external environment, there are usually static loads or alternating loads on the surface of the material, and a single electrochemical factor cannot reflect the true service status of marine engineering equipment. The present invention provides a mechanical-electrochemical bidirectional coupling calculation method, a simulation technology that accurately predicts the dynamic evolution of corrosion damage under external forces. It can predict the corrosion-sensitive positions of galvanic corrosion under external forces, analyze the growth of corrosion defects at different time scales, and evaluate the stress concentration coefficient and mechanical damage at the corrosion defects. It provides theoretical and technical support for the failure risk detection of marine engineering equipment and optimizes the material and structural design of marine engineering equipment. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1 It is a flow chart of a specific implementation mode of the present invention.
[0038] Figure 2 Polarization curves of aluminum alloy and 316 stainless steel in simulated seawater solution in the embodiment
[0039] Figure 3 Schematic diagram of the corrosion model of aluminum alloy / 316 stainless steel in the embodiment
[0040] Figure 4 The stress analysis diagram of aluminum alloy / 316 stainless steel in the embodiment
[0041] Figure 5 This is the dynamic change diagram of the galvanic corrosion defect profile
[0042] Figure 6The surface stress distribution and corrosion potential of the structural parts under external force
[0043] Figure 7 Figure 2 shows the development and change of mechanical damage at different time scales. DETAILED DESCRIPTION
[0044] like Figure 1 As shown, the present invention includes the following steps.
[0045] Step 1: Test the open circuit potential and polarization curve of the metal material through an electrochemical workstation to obtain the basic electrochemical data required for simulation;
[0046] Furthermore, the specific implementation method of step 1 is:
[0047] (1) Preparation of working electrode: Use laser wire cutting technology to cut the metal material into 10×10×5mm test blocks, use alcohol to clean the surface, and remove impurities such as oil. Use a welding gun to connect the back of the sample to the copper wire, and use a multimeter to test the conductivity. When the conductivity is good, put the sample connected to the copper wire into a rubber mold, fill it with two-component epoxy resin, and take it out after curing for 24 hours. Use 80#-200#-600#-1000#-1500# sandpaper to polish the electrode test surface in turn. After polishing, put it in acetone solution for ultrasonic cleaning for 10 minutes. After ultrasonic cleaning, blow it dry with a hair dryer and put it in a sealed bag for later use.
[0048] (2) Open circuit potential and polarization curve test: The test was conducted using an electrochemical workstation. The test system was a three-electrode system, with the sample to be tested as the working electrode, calomel as the standard electrode, and a carbon rod as the counter electrode. The open circuit potential test time was 30 minutes, the polarization curve test range was ±250 mV based on the measured open circuit potential, and the scan rate was 0.333 mV / s.
[0049] (3) Corrosion data acquisition: The exchange current density of the cathode and anode reactions was obtained by the Tafel fitting method, and the equilibrium potential of the cathode and anode reactions was calculated using the Nernst equation. The polarization curves and fitting methods are shown in Figure 2 .
[0050] Step 2: Perform a tensile test on the metal material using a tensile testing machine to obtain basic mechanical data of the material.
[0051] Furthermore, an interpolation function is established in the simulation software through the stretching data obtained in step 2, and the stress-strain curve obtained by stretching is imported, wherein strain is the independent variable and stress is the dependent variable.
[0052] Step 3: Construct a galvanic corrosion model for the generation and development of corrosion defects when dissimilar metals come into contact.
[0053] The mass transfer process of electrochemical corrosion is described by using the secondary current distribution field, and the anodic dissolution process of galvanic corrosion is described by combining the deformation geometry physics field with transient calculation.
[0054] Step 3 further includes:
[0055] (1) In the parameter setting of the secondary current distribution electrode surface, the equilibrium potential, exchange current density and anode-cathode transfer coefficient are input to simulate the galvanic corrosion kinetics process.
[0056] The dynamic changes of the galvanic corrosion interface are calculated using a deformed geometry field that obeys the arbitrary Lagrange-Euler equations to track the galvanic corrosion anode dissolution process.
[0057] The galvanic corrosion model and boundary conditions are shown in Figure 3 .
[0058] (2) The simulated galvanic corrosion kinetics process is verified by the galvanic current density tested by a zero-resistance ammeter.
[0059] Step 4: construct the stress distribution at the coating defect under the external load. Establish a formula to realize the promotion or inhibition of stress on electrochemical corrosion, and calculate the changes in corrosion behavior at different time scales under the action of external force.
[0060] The Von Mises stress at the defects of structural parts is calculated using the solid mechanics physics field, and the influence of Von Mises stress on the cathode and anode equilibrium potential and exchange current density of electrochemical reactions is calculated using the Gutman theory.
[0061] Furthermore, the specific implementation of step 4 is as follows:
[0062] (1) Establish a geometric model based on the actual forces of the structural parts, see Figure 4 ;
[0063] (2) After the metal wire elastic material enters the plastic stage, as the strain increases, its anti-deformation ability increases as the hardening function process is:
[0064] σ hard =σ exp (ε eff )-σ s0
[0065] Among them, σ exp is the fitting function of the measured stress and strain curve, ε eff is the total effective strain, σ s0 is the initial yield strength.
[0066] (3) Construct the hardening function variable formula and call the hardening function formula in the Solid Mechanics-Elastic-Plastic Material-Plasticity subnode. Select the boundary load and fixed constraint nodes and set the conditions according to the force analysis.
[0067] (4) Construct the Gutman formula at the variable node and modify the original parameters at the secondary current distribution-electrode surface-equilibrium potential node, and then re-perform the steady-state and transient calculations.
[0068] (5) The influence of mechanics on electrochemical corrosion is calculated based on the Gutman formula constructed above, and combined with the anode dissolution deformation formula, the influence of mechanics on the corrosion field on the time scale is calculated using the transient physical field.
[0069] Step 5: Calculate the variation of mechanical damage over time in combination with the oxide film thickness. Perform simulation analysis on stress distribution based on the corrosion defect shape calculated in step 4, and evaluate the severity of stress damage in combination with the stress concentration factor.
[0070] Furthermore, the specific implementation of step 5 is as follows:
[0071] (1) Based on the geometric model established in step 3 and combined with the diffusion law of the cathode reaction, the dissolution-deposition node is selected in the secondary current distribution node, the material density and the number of transferred electrons are input, and the thickness of the anodic oxide layer at different time scales is obtained through numerical calculation.
[0072] (2) Based on the relationship between the thickness of the oxide layer and the average area strain, damage modeling of linear elastic materials is carried out to intuitively predict the influence of corrosion on the occurrence and development of structural cracks.
[0073] (3) Using the theoretical stress concentration factor K t Indicates the severity of stress concentration and realizes the change in the impact of corrosion on the mechanical field.
[0074] (4) Edit the stress concentration factor formula in the post-processing module to complete the calculation of the stress concentration factor.
[0075] Step 6: realize the bidirectional coupling of mechanics and electrochemistry under external force and derive the calculation results. Including: the growth of corrosion defects ( Figure 5 ), corrosion potential and corrosion current density distribution under external force ( Figure 6 ), stress distribution and changes in mechanical damage ( Figure 7 )wait.
[0076] This study constructs a contact model of dissimilar materials and combines it with a single galvanic corrosion model to build a corrosion and stress simulation model of mechanical-electrochemical bidirectional coupling under external forces. It not only predicts the sensitive positions of galvanic corrosion, but also predicts the changes in corrosion behavior under external forces, analyzes the growth of corrosion defects at different time scales, and evaluates the stress concentration factor and mechanical damage at the corrosion defects. It solves the problem of difficult prediction of corrosion defects and mechanical damage of marine engineering equipment under external forces, reduces the risk of corrosion and mechanical failure of equipment, and has guiding significance for life assessment, equipment maintenance and anti-corrosion design of marine engineering equipment.
[0077] Although the content of the present invention has been described in detail through the above preferred embodiments, it should be appreciated that the above description should not be considered as a limitation of the present invention. After reading the above content, it will be apparent to those skilled in the art that various modifications and substitutions of the present invention will occur. Therefore, the protection scope of the present invention should be limited by the appended claims.
Claims
1. A bidirectional coupling simulation method for the dynamic growth of corrosion defects in offshore equipment under external forces. It is characterized in that The following steps are involved: Step 1, testing the open circuit potential and polarization curve of the metal material by an electrochemical workstation to obtain basic electrochemical data required for simulation, wherein the basic electrochemical data is the exchange current density and equilibrium potential of the cathode and anode reactions; Step 2, performing a tensile test on the metal material by a tensile testing machine to obtain basic mechanical data of the material, wherein the basic mechanical data is a stress-strain curve, wherein step 2 further comprises: An interpolation function is established in the simulation software, and the stress-strain curve data obtained from the tensile test is imported, where strain is the independent variable and stress is the dependent variable; Step 3, constructing a galvanic corrosion model for the generation and development of corrosion defects when dissimilar metals are in contact, using a secondary current distribution field to describe the mass transfer process of electrochemical corrosion, and describing the anodic dissolution process of galvanic corrosion by combining a deformation geometry physical field with transient calculation, wherein step 3 specifically includes: (1) In the parameter setting of the secondary current distribution electrode surface, the electrochemical parameters are input to simulate the kinetic process of galvanic corrosion. The dynamic changes of the galvanic corrosion interface are calculated using the deformation geometry field obeying the arbitrary Lagrange-Euler equation to track the galvanic corrosion anode dissolution process; (2) The simulated galvanic corrosion dynamics process is verified by the galvanic current density tested by a zero-resistance ammeter; Step 4, constructing the stress distribution at the coating defect under the action of external load, establishing a formula to realize the promotion or inhibition of stress on electrochemical corrosion, and calculating the changes in corrosion behavior at different time scales under the action of external force; using the solid mechanics physical field to calculate the Von Mises stress at the defect of the structural part, and calculating the influence of the Von Mises stress on the equilibrium potential of the cathode and anode and the exchange current density of the electrochemical reaction by Gutman theory, wherein the step 4 specifically includes: (1) Establish a geometric model based on the actual forces acting on the structural parts; (2) Construct a variable formula based on the hardening function formula, call the hardening function formula in the plasticity subnode, and determine the boundary load and fixed constraints of the structural component; (3) Construct the Gutman formula at the variable node and modify the original parameters at the secondary current distribution-electrode surface-equilibrium potential node, and then re-perform steady-state and transient calculations; (4) According to the Gutman formula constructed above, the results of the influence of mechanics on electrochemical corrosion are calculated. Combined with the anode dissolution deformation formula, the influence of mechanics on the corrosion field under the time scale of transient physical field calculation is used; Step 5, combining the oxide film thickness to calculate the change law of mechanical damage over time, reversely calculating the stress distribution of corrosion defects calculated at different time scales, and evaluating the severity of stress damage in combination with the stress concentration factor, wherein step 5 specifically includes: (1) Combining the diffusion law of the cathode reaction, the thickness of the anodic oxide layer at different time scales was obtained through numerical calculation; (2) Based on the relationship between the thickness of the oxide layer and the average area strain, damage modeling of linear elastic materials is performed to intuitively predict the influence of corrosion on the occurrence and development of structural cracks; (3) Using the theoretical stress concentration factor K t Indicates the severity of stress concentration and realizes the change of the influence of corrosion on the mechanical field; (4) Edit the stress concentration factor formula in the post-processing module to complete the calculation of the stress concentration factor; Step 6: realize the bidirectional coupling of mechanics and electrochemistry under the action of external force, and derive the calculation results, including: corrosion potential of structural parts, corrosion current density distribution, growth of corrosion defects, stress distribution and changes in mechanical damage.
2. A bidirectional coupling simulation method for dynamic growth of corrosion defects of marine equipment under external force as claimed in claim 1, Its characteristics are: The step 1 specifically includes: (1) preparing a working electrode and detecting the conductivity of the electrode; (2) Use an electrochemical workstation to test the open circuit potential and potentiodynamic polarization curve of the sample; (3) Obtain basic electrochemical data for modeling.
3. A bidirectional coupling simulation method for dynamic growth of corrosion defects of marine equipment under external force as claimed in claim 2, Its characteristics are: The step of preparing the working electrode and detecting the conductivity of the electrode specifically includes: (1) Use laser wire cutting technology to cut the metal material into test blocks of 10×10×5 mm, and use alcohol to clean the surface to remove oil and impurities; (2) Use a welding gun to connect the back of the sample to the copper wire, and use a multimeter to test the conductivity of the welded sample. If the conductivity is good, put the sample connected to the copper wire into a rubber mold, fill it with a two-component epoxy resin, and take it out after curing for 24 hours; (3) Use 80#-200#-600#-1000#-1500# sandpaper to polish the electrode test surface in turn. After polishing, put it into acetone solution for ultrasonic cleaning for 10 minutes. After ultrasonic cleaning, use a hair dryer to dry it, put it into a sealed bag and evacuate it for use.
4. A bidirectional coupling simulation method for dynamic growth of corrosion defects of marine equipment under external force as claimed in claim 2, Its characteristics are: The use of an electrochemical workstation to perform open circuit potential and potentiodynamic polarization curve testing on the sample specifically includes: (1) The test was carried out using an electrochemical workstation. The test system was a three-electrode system, the sample to be tested was the working electrode, calomel was the standard electrode, and the carbon rod was the counter electrode. The test time of the open circuit potential was 30 minutes, and the polarization curve test range was ±250 mV based on the measured open circuit potential. The scan rate was 0.333 mV / s. (2) The exchange current density of the cathode and anode reactions is obtained by the Tafel fitting method, and the equilibrium potential of the cathode and anode reactions is calculated using the Nernst equation to complete the collection of basic electrochemical data.