A wafer-level package structure for a filter with device layer sidewall protection and its fabrication method.

By setting a filling part and a thin film layer to cover the composite film in the filter wafer-level packaging structure, the warpage and delamination problems are solved, and the reliability and yield of the product are improved.

CN116505909BActive Publication Date: 2026-11-17XIAMEN SKY SEMICON TECH CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202310453379.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-04-25
Publication Date
2026-11-17
Estimated Expiration
2043-04-25

AI Technical Summary

Technical Problem

Existing wafer-level packaging structures for filters suffer from significant warpage and low reliability, especially the double-layer film structure, which is prone to delamination, resulting in low product yield.

Method used

A filter wafer-level packaging structure with device layer sidewall protection is adopted. By setting a filling part in the exposed area and forming a first thin film layer to cover the composite film, and combining it with a second thin film layer to form a resonant cavity, the packaging reliability is improved.

Benefits of technology

It effectively reduces the risk of delamination in composite films, improves product process yield and reliability, and enhances resistance to external environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116505909B_ABST
    Figure CN116505909B_ABST
Patent Text Reader

Abstract

A filter wafer-level packaging structure with device layer sidewall protection is disclosed, comprising a wafer, a substrate of the wafer having at least one effective region and at least one exposed region, the effective region being covered with a composite film, and the exposed region having an inwardly recessed filling portion near the edge where the exposed region meets the effective region; a first thin film layer being formed on at least a portion of the exposed region and the composite film, and the first thin film layer filling the filling portion. Accordingly, the present invention also provides a method for fabricating the filter wafer-level packaging structure with device layer sidewall protection, solving the problems of delamination, low packaging reliability, and easy wafer warpage that may exist in existing double-layer film structures.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of filter chip packaging, and in particular to a filter wafer-level packaging structure with device layer sidewall protection and its fabrication method. Background Technology

[0002] Surface acoustic wave (SAW) filters utilize the excitation, propagation, and reception of SAW waves on piezoelectric materials to achieve their filtering characteristics. SAW waves have wavelengths in the range of 100 μm to 2 μm and are mechanical waves that are highly sensitive to their propagation surface. To allow SAW waves in the acoustic wave element to propagate without interference, a cavity must be present above the chip surface in the package.

[0003] Currently, the main packaging technologies for filters are still lead-bonded ceramic, metal, and plastic packages, as well as flip-chip packaging, such as the wafer-level packaging structure for an acoustic filter disclosed in CN201910039927.9. Existing wafer-level packaging structures for filters suffer from significant warpage and low product yield. Furthermore, the double-layer film structure of existing wafer-level packaging structures may exhibit delamination, resulting in low packaging reliability and consequently, low overall reliability. Summary of the Invention

[0004] To address the key technical problems of large warpage and low reliability in the wafer-level packaging structure of filters in the prior art, this application proposes a wafer-level packaging structure for filters with device layer sidewall protection and its fabrication method, which solves the problems of delamination, low packaging reliability and easy wafer warpage that may exist in the existing double-layer film structure.

[0005] A filter wafer-level package structure with device layer sidewall protection includes:

[0006] The wafer has a substrate having at least one effective region and at least one exposed region. The effective region is covered with a composite film, and the exposed region has an inwardly recessed filling portion near the edge where the exposed region meets the effective region.

[0007] A first thin film layer is formed on at least a portion of the exposed area and the composite film, and the first thin film layer fills the fill portion.

[0008] In the above technical solution, the first thin film layer covers the composite film, reducing the possibility of delamination of the double-layer film structure of the composite film; in addition, only the effective area is covered by the composite film, which is less prone to warping than the structure in which the entire substrate is covered by the composite film. Through the combination of the above technical means, the filter wafer-level packaging structure with device layer sidewall protection provided by this application has high packaging reliability and product yield.

[0009] In one possible implementation, the filling portion is located at the edge between the exposed area and the effective area and is in contact with the composite film. Through this approach, the first film layer achieves a tighter coating of the composite film.

[0010] In one possible implementation, the filter wafer-level package structure with device layer sidewall protection further includes a second thin film layer. This second thin film layer is formed on the side of the first thin film layer away from the substrate. The composite thin film, the opening in the first thin film layer, and the second thin film layer form a resonant cavity. In the above technical solution, the resonant cavity is formed through the composite thin film, the opening in the first thin film layer, and the second thin film layer, resulting in a simple structure.

[0011] In one possible implementation, the depth of the filling portion is 0.5μm-20μm.

[0012] The above technical solution enables the first film layer to form a better coating on the composite film after entering the filling part, resulting in higher reliability.

[0013] In one possible implementation, the substrate cutouts and at least a portion of the chip edge are exposed areas.

[0014] The above technical solutions make the wafer-level packaging structure easier to cut during subsequent processing, which helps to improve product reliability.

[0015] In addition, this application also provides a method for fabricating a filter wafer-level package structure with device layer sidewall protection, including the following steps:

[0016] S1. Form a composite thin film on the substrate surface;

[0017] S2. Remove part of the composite film to form at least one effective area and at least one bare area on the substrate surface. The effective area is the area covered by the composite film, and the bare area is the area where the composite film is removed.

[0018] S3. Set pads and resonators on the composite film;

[0019] S4. An inwardly recessed filling portion is formed in the exposed area, the filling portion being close to the edge where the exposed area meets the effective area;

[0020] S5. A first thin film layer is formed on at least a portion of the exposed area and the composite film. The first thin film layer fills the fill portion and has a portion of the surface of the pad exposed and an opening of the resonator exposed, wherein the area of ​​the opening of the resonator exposed is larger than the area of ​​the resonator.

[0021] S6. A second thin film layer is formed on the side of the first thin film layer away from the substrate. The second thin film layer has an opening. The opening is located above the opening on the exposed surface of the pad and the area of ​​the opening is greater than or equal to the area of ​​the opening on the exposed surface of the pad. The composite thin film, the opening of the exposed resonator, and the second thin film layer form a resonant cavity.

[0022] S7. Set a terminal block on the pad, with the terminal block passing through the opening and aperture on the exposed part of the pad surface. Then, form a solder part at the end of the terminal block away from the pad. The solder part is a solder ball or electroless nickel-gold plating.

[0023] Through the above technical solutions, the first thin film layer forms a good coating on the composite film in both the longitudinal and transverse directions, reducing the possibility of delamination of the double-layer film structure of the composite film; in addition, only the effective area is covered by the composite film, which is less prone to warping than the structure in which the entire substrate is covered by the composite film. Through the combination of the above technical means, the filter wafer-level packaging structure with device layer sidewall protection provided in this application has high packaging reliability and product yield.

[0024] In one possible implementation, the filling portion is located at the edge between the exposed area and the effective area and is in contact with the composite film.

[0025] Through the above technical solution, the first thin film layer achieves a tighter coating of the composite film.

[0026] In one possible implementation, the depth of the filling portion is 0.5μm-20μm.

[0027] The above technical solution enables the first film layer to form a better coating on the composite film after entering the filling part, resulting in higher reliability.

[0028] In one possible implementation, the substrate cutouts and at least a portion of the chip edge are exposed areas.

[0029] The above technical solutions make the wafer-level packaging structure easier to cut during subsequent processing, which helps to improve product reliability.

[0030] This invention provides a wafer-level package structure for filters with device layer sidewall protection and its fabrication method. By partially removing the composite thin film, the wafer-level package structure exhibits less warpage, improving product process yield. Furthermore, by providing a filling portion in the exposed area, covering the composite thin film with a first thin film layer and filling the filling portion, the composite thin film is wrapped both laterally and longitudinally, effectively protecting the substrate structure, avoiding the risk of composite thin film delamination, improving the device's resistance to external environments, and thus significantly enhancing product reliability. Attached Figure Description

[0031] The accompanying drawings are included to provide a further understanding of the embodiments and are incorporated in and constitute a part of this specification. The drawings illustrate embodiments and, together with the description, serve to explain the principles of the invention. Other embodiments and many anticipated advantages of the embodiments will be readily recognized as they become better understood through reference to the following detailed description. Elements in the drawings are not necessarily to scale. The same reference numerals refer to corresponding similar parts.

[0032] Figure 1 A schematic diagram of a conventional filter wafer-level package structure with device layer sidewall protection is shown.

[0033] Figure 2 A schematic diagram of a filter packaging structure according to an embodiment of the present invention is shown;

[0034] Figures 3-8 This is a schematic diagram of an intermediate structure during the fabrication process of a filter packaging structure according to an embodiment of the present invention.

[0035] 100 - Wafer, 110 - Substrate, 120 - Effective area, 130 - Exposed area, 131 - Filled portion, 140 - Composite film, 140' - Composite film in the prior art, 141 - Pad, 142 - Resonator, 200 - First thin film layer, 200' - First thin film layer in the prior art, 201 - Opening, 300 - Second thin film layer, 301 - Opening, 400 - Resonant cavity, 500 - Terminal, 501 - Solder portion. Detailed Implementation

[0036] The present application will now be described in further detail with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the invention and not intended to limit it. Furthermore, it should be noted that, for ease of description, only the parts relevant to the invention are shown in the accompanying drawings.

[0037] It should be noted that, unless otherwise specified, the embodiments and features described in this application can be combined with each other. This application will now be described in detail with reference to the accompanying drawings and embodiments.

[0038] In wafer-level packaging structures, composite films are typically double-layer structures (not shown). These double-layer structures may delaminate due to external environmental influences during actual use, leading to a decrease in product reliability. For example... Figure 1 The existing filter wafer-level packaging structure with device layer sidewall protection shown can be seen that in the prior art, the first thin film layer 200' is only covered on the upper surface of the composite film and does not achieve the encapsulation of the composite film 140'. Therefore, the composite film 140' is more prone to delamination.

[0039] To address the aforementioned issues, this application provides a filter wafer-level packaging structure with device layer sidewall protection and its fabrication method.

[0040] Figure 2 This application illustrates a filter wafer-level package structure with device layer sidewall protection provided by one embodiment of the present application, including a wafer 100, a first thin film layer 200, a second thin film layer 300, and terminals 500.

[0041] The substrate 110 of wafer 100 includes an effective region 120 covered by a composite film 140 and an exposed region 130 not covered by the composite film 140. Pads 141 and a resonator 142 are disposed on the side of the composite film 140 away from the substrate 110 of wafer 100. The exposed region 130 is provided with dicing channels (not shown). In subsequent processing, the wafer-level package structure can be cut into multiple chips by cutting the dicing channels. The exposed region 130 also includes an inwardly recessed filling portion 131, and at least a portion of the filling portion 131 is disposed around the effective region 120.

[0042] In this embodiment, the dicing channel divides the wafer 100 into multiple squares. After packaging and dicing the wafer 100, a square chip can be obtained. In other possible implementations, the dicing channel can also divide the wafer 100 into other polygonal patterns.

[0043] The first thin film layer 200 is formed on the composite film 140 and the exposed area and fills the filling portion 131 of the exposed area 130. By filling the filling portion 131 and covering the composite film 140, the first thin film layer 200 achieves the encapsulation of the composite film 140, making the composite film 140 less prone to delamination and improving the reliability of the wafer-level packaging structure.

[0044] In this embodiment, the filling portions 131 are all formed at the edge where the exposed area 130 and the effective area 120 meet and are in close contact with the effective area 120, making the first thin film layer 200 more tightly wrap the composite film 140 and further improving the encapsulation reliability. Furthermore, in this embodiment, the filling portions 131 are arranged around the edge where the exposed area 130 and the effective area 120 meet, forming a closed linear pattern around the composite film 140. In other possible implementations, the filling portions 131 can also be open elongated strips. In this embodiment, the depth of the filling portions 131 is 1 μm. In other possible implementations, the depth of the filling portions 131 can be 0.5 μm-20 μm.

[0045] The second thin film layer 300 is formed on the side of the first thin film layer 200 away from the substrate 110 and has an opening 301 that exposes the terminal 500. The first thin film layer 200 forms openings 201 at the positions of the pad 141 and the resonator 142, respectively, exposing part of the surface of the pad 141 and the resonator 142. The area of ​​the opening 201 exposing the resonator 142 is larger than the area of ​​the resonator 142. The composite thin film 140, the opening 201 of the first thin film layer 200 exposing the resonator 142 and the second thin film layer 300 together constitute the resonant cavity 400.

[0046] In this embodiment, the filling portion 131 is triangular in shape. In other possible implementations, the shape of the filling portion 131 is not limited, as long as it can form a recess to fill the first film layer 200, so that the first film layer 200 can wrap the composite film 140 in the longitudinal direction. By providing an opening 301 in the second film layer 300 that is larger than the opening 201 in the first film layer 200, it is beneficial to set the terminal 500 and improve the product yield.

[0047] The first thin film layer 200 and the second thin film layer 300 are respectively selected from polymer materials, silicon, ceramics, or glass. If the material is a polymer material, the opening 201 or aperture 301 is formed by exposure. If other materials are selected, the opening 201 or aperture 301 is formed by laser. The area of ​​the aperture 301 in the second thin film layer 300 is greater than or equal to the area of ​​the opening 201 on the exposed surface of the first thin film layer 200 on the pad 141.

[0048] One end of the terminal 500 is connected to the pad 141, and the other end is used for soldering. The soldering end of the terminal 500 can form a solder joint 501, which can be made of solder balls or electroless nickel-gold plating. Furthermore, the terminal 500 can be solid or hollow.

[0049] The substrate 110 can be made of silicon or spinel; the composite film 140 can be a silicon oxide film and a lithium tantalate film, or the composite film 140 can be a silicon oxide film and a lithium niobate film.

[0050] In this embodiment, the composite film 140 is a silicon oxide film and a lithium tantalate film, both with a thickness of 1 μm. In other possible implementations, the thickness of the silicon oxide film can be 0.1 μm-5 μm, and the thickness of the lithium tantalate film or the lithium niobate film can be 0.5 μm-10 μm.

[0051] See Figures 2-8 The fabrication method of the filter wafer-level packaging structure with device layer sidewall protection in this embodiment includes the following steps:

[0052] S1, such as Figure 3 As shown, a composite thin film 140 is formed on the surface of the substrate 110.

[0053] S2, such as Figure 4 As shown, removing a portion of the composite film 140 forms at least one effective region 120 and at least one exposed region 130 on the surface of the substrate 110. The effective region 120 is the area covered by the composite film 140, and the exposed region 130 is the area where the composite film 140 has been removed. In the above steps, the removal of the portion of the composite film 140 can be achieved by laser or etching.

[0054] S3, such as Figure 5 As shown, pads 141 and resonators 142 are disposed on the composite film 140.

[0055] S4, such as Figure 6 As shown, an inwardly recessed filling portion 131 is formed in the exposed area 130, and the filling portion 131 is close to the edge where the exposed area 130 meets the effective area 120.

[0056] S5, such as Figure 7 As shown, a first thin film layer 200 is formed on the composite thin film 140 and the exposed area 130. The first thin film layer 200 fills the filling portion 131. The first thin film layer 200 is subjected to exposure drilling or laser drilling so that it has a portion of the surface of the pad 141 exposed and an opening 201 of the resonator 142 exposed, wherein the area of ​​the opening 201 exposing the resonator 142 is larger than the area of ​​the resonator 142.

[0057] S6, such as Figure 8 As shown, a second thin film layer 300 is formed on the side of the first thin film layer 200 away from the substrate 110. The second thin film layer 300 has an opening 301, which is disposed above the opening 201 on the exposed surface of the pad 141, and the area of ​​the opening 301 is equal to the area of ​​the opening on the exposed surface of the pad 141. The composite thin film 140, the opening 201 exposing the resonator 142, and the second thin film layer 300 form a resonant cavity 400, resulting in... Figure 4 The structure shown is as follows. In this embodiment, the area of ​​the opening 301 is the same as the area of ​​the opening 201 that exposes a portion of the surface of the pad 141. In other possible implementations, the area of ​​the opening 301 may also be larger than the area of ​​the opening 201 that exposes a portion of the surface of the pad 141.

[0058] S7. A terminal 500 is provided on the pad 141. The terminal 500 passes through the opening 201 and the aperture 301 that expose a portion of the surface of the pad 141. Then, a solder part 501 is formed at the end of the terminal 500 away from the pad 141. The solder part 501 is a solder ball or electroless nickel-gold plating, resulting in... Figure 2The filter shown is a wafer-level package structure.

[0059] In other possible implementations, the order of operations S6 and S7 can be interchanged.

[0060] The composite film 140 consists of at least two thin films. In the conventional fabrication method of a filter wafer-level package structure with device layer sidewall protection, the first thin film layer 200 is directly covered on the composite film 140, and then the chip is obtained by cutting. In this fabrication method, the first thin film layer 200 can only cover one surface of the composite film 140, and does not form a complete encapsulation of the composite film 140. Separation may occur between the different films of the composite film 140. However, in the fabrication method provided in this application, a portion of the non-functional area (i.e., the effective area 120 referred to in this application) of the composite film 140 is first removed. By setting a filling portion 131 at the edge of the composite film 140 and filling the filling portion 131 with the first thin film layer 200, the first thin film layer 200 further achieves longitudinal protection of the composite film 140, reduces the possibility of delamination of the composite film 140, and thus improves the product yield.

[0061] The specific embodiments of this application have been described above, but the scope of protection of this application is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this application should be included within the scope of protection of this application. Therefore, the scope of protection of this application should be determined by the scope of the claims.

[0062] In the description of this application, it should be understood that the terms "upper," "lower," "inner," "outer," etc., indicating orientation or positional relationships based on the orientation or positional relationships shown in the accompanying drawings, are used only for the convenience of describing this application and for simplification, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this application. The word "comprising" does not exclude the presence of elements or steps not listed in the claims. The word "a" or "an" preceding an element does not exclude the presence of a plurality of such elements. The simple fact that certain measures are recited in mutually different dependent claims does not indicate that combinations of these measures cannot be used for improvement. Any reference signs in the claims should not be construed as limiting the scope.

Claims

1. A filter wafer level package structure with device layer sidewall protection, characterized in that, include: A wafer, wherein the substrate of the wafer has at least one effective region and at least one exposed region, the effective region is covered with a composite film, and the exposed region is provided with an inwardly recessed filling portion near the edge where the exposed region meets the effective region; A first thin film layer is formed on at least a portion of the exposed area and the composite film, and the first thin film layer fills the filler portion.

2. The filter wafer level package structure with device layer side wall protection of claim 1, wherein, The filling portion is located at the edge of the exposed area and the effective area and is in contact with the composite film.

3. The filter wafer level package structure with device layer side wall protection of claim 1 or 2, wherein, The composite film has a pad and a resonator on the side of the substrate away from the wafer. The first thin film layer covers a portion of the surface of the pad and around the resonator and has openings that expose a portion of the surface of the pad and the resonator, respectively, wherein the area of ​​the opening exposing the resonator is larger than the area of ​​the resonator.

4. The filter wafer level package structure with device layer side wall protection of claim 3, wherein, It also includes a second thin film layer, which is formed on the side of the first thin film layer away from the substrate. The composite film, the first thin film layer exposing the opening of the resonator, and the second thin film layer form a resonant cavity.

5. The filter wafer level package structure with device layer side wall protection of claim 1 or 2, wherein, The depth of the filling portion is 0.5μm-20μm.

6. The filter wafer level package structure with device layer side wall protection of claim 1 or 2, wherein, The exposed area is defined as the dicing grooves on the substrate and at least a portion of the chip edge.

7. A method for fabricating a filter wafer-level package structure with device layer sidewall protection, characterized in that, Includes the following steps: S1. Form a composite thin film on the substrate surface; S2. Removing part of the composite film to form at least one effective area and at least one exposed area on the substrate surface, wherein the effective area is the area covered by the composite film, and the exposed area is the area where the composite film is removed; S3. A pad and a resonator are disposed on the composite film; S4. An inwardly recessed filling portion is formed in the exposed area, the filling portion being close to the edge where the exposed area meets the effective area; S5. A first thin film layer is formed on at least a portion of the exposed area and the composite film. The first thin film layer fills the filling portion and has openings that expose a portion of the surface of the pad and the resonator, respectively. The area of ​​the opening exposing the resonator is larger than the area of ​​the resonator. S6. A second thin film layer is formed on the side of the first thin film layer away from the substrate. The second thin film layer has an opening. The opening is disposed above the opening on the surface of the portion of the pad exposed, and the area of ​​the opening is greater than or equal to the area of ​​the opening on the surface of the pad exposed. The composite thin film, the opening exposing the resonator, and the second thin film layer form a resonant cavity. S7. A terminal block is provided on the pad, the terminal block passes through the opening and the aperture that expose a portion of the surface of the pad, and then a solder part is formed at the end of the terminal block away from the pad, the solder part being a solder ball or electroless nickel-gold plating.

8. The method for fabricating a filter wafer-level package structure with device layer sidewall protection according to claim 7, characterized in that, The filling portion is located at the edge of the exposed area and the effective area and is in contact with the composite film.

9. The method for fabricating a filter wafer-level package structure with device layer sidewall protection according to claim 7, characterized in that, The depth of the filling portion is 0.5μm-20μm.

10. The method of making a filter wafer level package structure with device layer sidewall protection of claim 7, wherein, The exposed area is defined as the dicing grooves on the substrate and at least a portion of the chip edge.

Citation Information

Patent Citations

  • A wafer level packaging structure of a filter and a process thereof

    CN109728790A

  • Fan-out wafer-level chip packaging structure and method

    CN107946249A

  • Method of forming monolithic CMOS-MEMS hybrid integrated, packaged structures

    US20110003422A1